Method for manufacturing glass spacer, glass spacer, and hard disk drive device
Patent Information
- Application Number
- LAP856
- Authority / Receiving Office
- LA · LA
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2020-03-06
- Filing Date
- 2021-03-08
- Publication Date
- 2026-02-27
AI Technical Summary
In hard disk drive devices, glass spacers used with glass magnetic disks face issues of static electricity accumulation and dust generation due to friction, leading to potential damage from discharges and foreign matter attraction, and existing film-coating methods are inefficient and costly.
A method of manufacturing a ring-shaped glass spacer with a conductive film covering the entire surface, including thicker films on the end surfaces, using a rotating shaft and spray nozzle system to evenly apply a mist of conductive materials like tin oxide, zinc oxide, or titanium oxide, ensuring uniform thickness and reduced dust generation.
The solution effectively suppresses static electricity and dust generation, maintaining the integrity of the magnetic head and reducing operational issues in hard disk drives while minimizing manufacturing costs.
Smart Images

Figure 00000000_0001_ABST 
Figure 00000000_0000_ABST
Abstract
Description
Method for manufacturing a glass spacer, glass spacer, and hard disk drive device The present invention relates to a method for manufacturing a ring-shaped glass spacer provided in contact with a magnetic disk within a hard disk drive device, a glass spacer, and a hard disk drive device equipped with this glass spacer. With the recent rise of cloud computing, many hard disk drives (hereinafter also referred to as HDDs) are being used in data centers for the cloud to increase storage capacity. HDD devices are equipped with ring-shaped spacers between magnetic disks to hold them apart. These spacers function to ensure that the magnetic disks do not touch each other and are positioned precisely spaced apart in predetermined locations. Conventionally, metal materials with low manufacturing costs have been used as the material for these spacers. Incidentally, when a glass substrate is used as the substrate for a magnetic disk, the spacer and the magnetic disk are in contact with each other. As a result, changes in temperature within the HDD device cause a difference in thermal expansion between the metal spacer and the glass magnetic disk, causing the magnetic disk to bend. This, in turn, worsens the levitation of the magnetic head. Poor levitation of the magnetic head is undesirable from the standpoint of reading and writing data in the hard disk drive. For this reason, in recent years, the use of glass spacers (hereinafter referred to as glass spacers) has been considered in response to the use of glass substrates for magnetic disks. However, since glass is generally an insulator, static electricity tends to accumulate on the magnetic disk or glass spacer due to friction between the rapidly rotating magnetic disk and glass spacer and the air. When the magnetic disk or spacer becomes charged, it easily attracts foreign matter and fine particles, and the discharge of the accumulated static electricity to the magnetic head can damage the recording and playback elements of the magnetic head, which is undesirable. In contrast, a glass spacer is known in which at least the contact surface with the magnetic disk and the inner circumferential surface of the glass spacer are coated with a conductive ceramic film with a thickness of 0.1 to 3 μm (Patent Document 1). This allows for efficient dissipation of static electricity accumulated on the magnetic disk, resulting in virtually no wear on the contact surface. Japanese Patent Application Publication No. 9-44969 However, when brittle materials such as glass or ceramics were used as the material for the spacer body, even if a conductive coating was formed on the surface of the spacer body, there were cases where some of the brittle material of the spacer body became fine particles and generated dust. Therefore, the present invention aims to provide a glass spacer that can suppress the charging of magnetic disks and glass spacers in order to suppress the discharge of static electricity from magnetic heads charged on magnetic disks within an HDD device, and further suppress dust generation, a hard disk drive device using this glass spacer, and a method for manufacturing the glass spacer. One aspect of the present invention is a method for manufacturing a ring-shaped glass spacer that is provided in contact with a magnetic disk within a hard disk drive device. The aforementioned glass spacer is constructed by forming a film on the glass spacer body. The manufacturing method includes a process of forming the film on the surface of the glass spacer body, The process involves forming the film by rotating the outer peripheral end face of the glass spacer body in the circumferential direction while passing it through areas where the components of the film are sprayed. It is preferable to rotate the outer circumferential end surface by passing a rotating shaft, which is loosely fitted into the hole of the ring-shaped glass spacer body, through the hole, bringing a part of the inner circumferential end surface of the hole into contact with the rotating shaft, and rotating the rotating shaft. Preferably, the rotating shaft is mounted on a moving mechanism so as to move in one direction while rotating. Preferably, the area in the sprayed state is formed by misting the components of the film from both sides of the transport path of the glass spacer body. Preferably, the process includes heating the film formed on the glass spacer body. The arithmetic mean roughness Ra of the surface of the film is preferably 1 μm or less. The surface resistivity of the aforementioned film at 22°C is 10 -4 ~10 6 It is preferable that the value is [Ω / sq]. The aforementioned film includes, for example, one of tin oxide, zinc oxide, and titanium oxide. Another aspect of the present invention is an apparatus for forming a film on the surface of a spacer for a hard disk drive device, which includes a housing that incorporates a spacer transport means comprising at least a drive motor and a spray nozzle, and having a rotating shaft spanning a pair of moving mechanisms. Another aspect of the present invention is a ring-shaped glass spacer provided in contact with a magnetic disk within a hard disk drive device. The entire surface of the glass spacer, including its main surface and end faces, is covered with a film containing one of tin oxide, zinc oxide, and titanium oxide, wherein the thickness of the film on the end face of the glass spacer is greater than the thickness of the film on the main surface of the glass spacer. Preferably, the difference between the maximum and minimum film thickness of the film on the entire surface of the glass spacer is less than half of the maximum film thickness. Preferably, the entire surface of the glass spacer is covered with the film, which has a thickness of less than 100 nm. Preferably, the arithmetic mean roughness Ra at the end face of the glass spacer is greater than the arithmetic mean roughness Ra at the main surface of the glass spacer. The surface resistivity of the aforementioned film at 22°C is 10 -4 ~10 6 It is preferable that the value is [Ω / sq]. Another aspect of the present invention is a hard disk drive device comprising the glass spacer and the magnetic disk. According to the glass spacer, hard disk drive device, and method for manufacturing the glass spacer described above, it is possible to suppress the charging of magnetic disks and glass spacers and suppress dust generation. This is an external perspective view of a spacer according to one embodiment. This is a diagram illustrating the arrangement of a spacer and a magnetic disk according to one embodiment. This is a cross-sectional view of a main part illustrating an example of the structure of an HDD device into which the spacer according to one embodiment is incorporated. This is a cross-sectional view of an example of a glass spacer according to one embodiment. This is a diagram illustrating an example of film formation in a manufacturing method of a glass spacer according to one embodiment. This is a diagram illustrating an example of a spacer transport means used in a manufacturing method of a glass spacer according to one embodiment. The following describes in detail the glass spacer, hard disk drive device, and method for manufacturing the glass spacer according to the present invention. Figure 1 is an external perspective view of a glass spacer (hereinafter sometimes simply referred to as a spacer) 1 according to one embodiment, and Figure 2 is a diagram illustrating the arrangement of the spacer 1 and the magnetic disk 5. Figure 3 is a cross-sectional view of a key part illustrating an example of the structure of an HDD device into which the spacer 1 is incorporated. Figure 4 is a cross-sectional view of an example of the spacer 1. As shown in Figure 2, the spacers 1 are incorporated into the HDD device by stacking the magnetic disks 5 and spacers 1 alternately. As shown in Figure 3, multiple magnetic disks 5 are fitted onto a spindle 14 that rotates connected to a motor 12 via the spacers 1, and then fixed on top of them with screws via top clamps 16, thereby mounting them at predetermined intervals. As shown in Figure 2, the spacer 1 is positioned between the two magnetic disks 5, with the spacer 1 and the magnetic disks 5 being arranged alternately to maintain a predetermined gap between adjacent magnetic disks 5. In the following embodiments, the spacer 1 described refers to a spacer provided between the two magnetic disks 5 so as to be in contact with the magnetic disks 5, but the spacer targeted by the present invention also includes a spacer that is in contact only with the uppermost or lowermost magnetic disk 5. Depending on the specifications of the HDD device, a spacer 1 that is in contact only with the uppermost or lowermost magnetic disk 5 may not be provided. As shown in Figure 1, the spacer 1 has a ring shape and comprises an outer peripheral end face 2, an inner peripheral end face 3, and two opposing main surfaces 4. The inner circumferential end surface 3 is the surface that contacts the spindle 14 and is the wall surface surrounding a hole with an inner diameter slightly larger than the outer diameter of the spindle 14. The dimensions of the annular spacer 1 can be appropriately changed depending on the specifications of the HDD to be mounted, but for a nominal 3.5-inch HDD device, the outer diameter is, for example, 30 to 34 mm, the inner diameter is, for example, 24 to 26 mm, the radial width is, for example, 2 to 5 mm, and the thickness is, for example, 0.5 to 3 mm. In addition, a chamfered surface may be appropriately provided at the connection between the outer peripheral end face 2 and the inner peripheral end face 3 and the main surface 4. The chamfered surface may be a straight line or an arc in cross-sectional shape. The dimensions of the chamfered surface are, for example, 0.01 to 0.5 mm in the radial and thickness directions. The main surface 4 consists of two parallel surfaces that are in contact with the magnetic disk 5. The spacer 1 is in close contact with the magnetic disk 5 and fixes it in place by friction. As the spacer 1 and the magnetic disk 5 are in contact with each other in this way, changes in temperature inside the HDD device cause differences in thermal expansion between the spacer 1 and the magnetic disk 5, resulting in displacement and friction. This makes it easy for static electricity to be generated on the glass, which is an insulator. Also, static electricity is easily generated on the spacer 1 due to friction between the rapidly rotating spacer 1 and the air. When static electricity is generated on the spacer 1 and the spacer 1 becomes charged, it easily attracts foreign matter and fine particles, and the discharge of accumulated static electricity to the magnetic head can damage the recording and playback elements of the magnetic head, so static electricity is undesirable. In addition, some of the glass may be released from the surface of the spacer 1 as fine particles and become dust. Due to dust generation, fine particles float in the sealed space of the HDD device and adhere to the main surface of the magnetic disk 5, hindering reading from and writing to the magnetic disk 5 by the magnetic head, so dust generation is undesirable. Such dust generation is particularly likely to occur from the outer peripheral end face of the spacer 1. This is because the outer peripheral end face is constantly exposed during the operation of the HDD device and is close to the main surface of the magnetic disk 5. In addition, dust may be generated from the inner peripheral end face of the spacer 1 when it is attached to the spindle due to friction. This dust generation is undesirable because it may transfer to the main surface of the magnetic disk 5 during rework, which is the process of replacing the magnetic disk 5. Therefore, in order to prevent static electricity buildup and dust generation, the entire surface of the spacer 1 is covered with a conductive film 22 containing tin oxide or zinc oxide. That is, as shown in Figure 4, the spacer 1 has a ring-shaped glass spacer body (hereinafter referred to as the spacer body) 20 and a film 22. The film 22 is, for example, tin oxide (SnO 2 The conductive film can contain ) or zinc oxide (ZnO). Film 22 may also be a film containing titanium oxide. FTO, which is tin oxide doped with fluorine, or zinc oxide doped with aluminum oxide (Al 2 O 3 AZO doped with ) may also be used. The thickness of the film 22 covering the entire surface of the spacer 1 is preferably less than 100 nm. Conventionally, methods such as sputtering, PVD (Physical Vapor Deposition), CVD (Chemical Vapor Deposition), or spraying have been used for film deposition. However, when these deposition methods are used in a general manner, there is a fundamental problem that film cannot be deposited on the parts of the spacer that are in contact with the holding member (support member) that holds the spacer. As a result, a portion of the spacer's surface is not deposited and remains exposed due to being held by the holding member, which can cause glass fragments to be released as fine particles and generate dust. It is also possible to remove the spacer, which has been deposited while being held by the holding member, from the deposition apparatus and perform a second deposition while the deposited area is held by the holding member, in order to completely eliminate the exposed area. However, since two depositions are performed, there is approximately twice the film thickness unevenness between the area in contact with the holding member and the other areas, and the deposition process becomes complicated, leading to increased costs. In this embodiment, instead of using the conventional retaining member described above, the entire surface of the spacer 1 is covered with a film 22 containing tin oxide. The thickness of the film 22 covering the entire surface of the spacer 1 is preferably 200 nm or less, and more preferably less than 100 nm. If the thickness exceeds 200 nm, the manufacturing cost may become excessive. If the thickness exceeds 100 nm, the surface irregularities of the film 22 become large, and when the protruding parts of the film 22 come into contact with the magnetic disk 5, they are pressed, and some of these protrusions may detach from the surface of the film 22 and become fine particles, which may generate dust. These generated fine particles may transfer to the main surface of the magnetic disk during rework, which is undesirable. Furthermore, it is preferable that the thickness of the film 22 on the outer peripheral end face 2 and the inner peripheral end face 3 of the spacer 1 is greater than the thickness of the film 22 on the main surface 4 of the spacer 1. The film 22 on the outer peripheral end face 2 is exposed to the sealed space of the HDD device, so dust generation from the outer peripheral end face 2 must be suppressed. For this reason, the thickness of the film 22 on the outer peripheral end face 2 is made greater than the thickness of the film 22 on the main surface 4 of the spacer 1 so that the glass of the spacer body 20 is not exposed to the sealed space. On the other hand, the film 22 on the inner peripheral end face 3 rubs against the spindle 14, so dust generation is likely. For this reason, the thickness of the film 22 on the inner peripheral end face 3 is made greater than the thickness of the film 22 on the main surface 4 of the spacer 1. For example, the thickness of the film 22 on the main surface 4 of the spacer 1 can be 30 nm or more and 190 nm or less, but it is more preferable to have a thickness of 30 nm or more and 90 nm or less. Furthermore, the thickness of the film 22 on the outer peripheral end face 2 and the inner peripheral end face 3 can be, for example, 40 nm or more and 200 nm or less, but it is more preferable to have a thickness of 40 nm or more and less than 100 nm. In one embodiment, it is preferable that the arithmetic mean roughness Ra of the outer peripheral end face 2 and the inner peripheral end face 3 of the spacer 1 is greater than the arithmetic mean roughness Ra of the main surface 4 of the spacer 1. By increasing the arithmetic mean roughness Ra of the outer peripheral end face 2 and the inner peripheral end face 3 of the spacer 1, the adhesion of the film 22 can be improved. In this way, even if the film thickness of the film 22 at the end face is thicker than that of the main surface, film peeling due to film stress becomes less likely to occur. For example, by polishing the main surface 4 of the spacer 1 before forming the film, the arithmetic mean roughness Ra of the main surface 4 of the spacer 1 can be made smaller than that of the outer peripheral end face 2 and the inner peripheral end face 3. It is preferable that the arithmetic mean roughness Ra of the main surface 4 of the spacer 1 be 1.0 μm or less. It is also preferable that the arithmetic mean roughness Ra of the outer peripheral end face 2 and the inner peripheral end face 3 of the spacer 1 be 0.5 μm or more. Furthermore, according to one embodiment, it is preferable that the difference between the maximum and minimum film thickness of the film 22 on the entire surface of the spacer 1 is less than half of the maximum film thickness. More preferably, this difference is less than one-quarter of the maximum film thickness. If there are no areas on the surface of the spacer 1 where the film thickness of the film 22 is extremely thin due to holding by a holding jig or the like, this difference can be calculated from the film thickness of each surface: the main surface, the inner circumferential end surface, and the outer circumferential end surface of the spacer 1. The film thickness of each surface can be, for example, the film thickness at the center of each surface. By doing so, the variation in the film thickness of the film 22 on the entire surface of the spacer 1 can be reduced, thereby preventing the film thickness from becoming extremely thin in a part of the surface when a predetermined film thickness is formed, which would make it impossible to suppress dust generation. The manufacturing of a spacer 1 equipped with such a film 22 includes a process of forming the film 22 on the surface of a ring-shaped spacer body 20 that forms the basis of the spacer 1. In this process, the film 22 is formed by rotating the outer peripheral end face 2 of the spacer body 20 in the circumferential direction and passing it through areas where the components of the film 22 are in a sprayed state. Figure 5 is a diagram illustrating an example of film formation in a manufacturing method of a spacer 1 according to one embodiment. In this way, by rotating the outer peripheral end face 2 of the spacer body 20 in the circumferential direction and passing it through the area where the components of the film 22 are sprayed 23, the film 22 can be efficiently and evenly formed on the entire surface of the spacer body 20. Conventionally, when the outer end face of the spacer body 20 is held by a holding member, the film 22 is not formed on the holding portion. After forming the film 22, it is possible to change the holding portion to a different location and form the film 22 a second time, but this results in unevenness in the thickness of the film 22. On the other hand, with the film formation method of the present invention, there is no need to change the holding member, and the film 22 can be formed evenly in a single film formation process. As one embodiment of the method for forming the film 22, it is preferable to loosely fit the rotating shaft 50 into the hole of the ring-shaped spacer body 20, that is, to pass a rotating shaft 50, whose outer diameter is smaller than the inner diameter of the hole, through the hole, bringing a part of the inner circumferential surface of the hole (the inner circumferential end surface of the spacer body 20) into contact with the rotating shaft 50, and rotating the rotating shaft 50 to rotate the outer circumferential end surface 2. In this method, the spacer body 20 is rotated by the rotation of the rotating shaft 50. Therefore, the surface roughness and material of the rotating shaft 50 should be appropriately designed so that there is appropriate friction between the rotating shaft 50 and the inner circumferential end surface of the spacer body 20. In addition, recesses (grooves) or protrusions may be provided on the surface of the rotating shaft 50 to prevent the rotating shaft from shifting position in the axial direction during rotation. By providing recesses or protrusions, it becomes easier to increase the number of ring-shaped spacer bodies that can be attached to a single rotating shaft, thereby improving production efficiency. By rotating the spacer body 20 in the spray state 23, the components of the film 22 can be efficiently attached to the entire surface of the spacer body 20 (main surface 4, outer peripheral end surface 2, and inner peripheral end surface 3). According to one embodiment, it is preferable that the rotating shaft 50 is provided on the moving mechanism 52 so as to move in one direction while rotating. With this spacer conveying means, the spacer body 20 can be rotated and conveyed in the spray state 23, and a film 22 can be formed on the entire surface of the spacer body 20. The moving mechanism 52 includes, for example, a pair of spirally wound rotating members 54 and a drive motor (not shown), as shown in Figure 6. Figure 6 is a diagram illustrating an example of a spacer transport means used in a glass spacer manufacturing method according to one embodiment. As the rotating member 54 shown in Figure 6 rotates due to the drive of the drive motor, the rotating shaft 50, which is stretched between the rotating members 54 on both sides, rotates and moves in the X direction. Therefore, the rotating member 54 is positioned along the transport path of the spacer body 20. According to one embodiment, by providing multiple locations where the spray state 23 is maintained, and transporting the spacer body 20 with the moving mechanism 52, passing it through each of the locations where the spray state 23 is maintained, the film 22 can be reliably formed over the entire surface of the spacer body 20. According to one embodiment, it is preferable that the area of the sprayed state 23 is formed by misting the components of the film 22 from a plurality of spray nozzles provided so as to surround the transport path of the spacer body 20. For example, the plurality of spray nozzles can be provided on both sides, left and right, top and bottom, top and bottom left and right, etc. of the transport path. Alternatively, the plurality of spray nozzles may be provided along the transport path of the spacer body 20. By appropriately combining these, thickness unevenness of the film 22 can be suppressed. The process of forming the film 22 may include heating the film 22 formed on the spacer body 20 using heating means during and / or after the formation of the film 22. Note that the spacer body 20 may be heated before the formation of the film 22, and the film 22 may be heated by the residual heat. That is, the film 22 can be heated by appropriately combining heating before, during, and after the formation of the film 22. For example, when fine droplets adhere to the surface of the spacer body 20 in the spray state 23 where fine droplets scatter and a liquid film 22 is formed, by heat-treating this film 22, a chemical reaction is caused to solidify the film 22. The film 22 is preferably a conductive oxide or ceramic. For example, when forming tin oxide as the film 22, a spray state 23 of a liquid in which an organotin compound such as dibutyltin diacetate or dimethyltin dichloride is dissolved in a solvent such as ethanol is formed, the film 22 is formed on the surface of the spacer body 20 in this spray state 23, and then, for example, heated at 400 to 600 °C to form tin oxide. Note that as described above, the spray may be performed after and / or while heating the spacer body 20. As the heating means, conventionally known heating devices such as various heaters and heating plates can be used. Note that the spacer conveying means as illustrated in FIG. 6 as an example is not limited to glass spacers and can be used for forming a film on the surface of any spacer. Therefore, a device for forming a film incorporated in a housing including at least a drive motor, a spray port, and optionally a heating means can form a film on the surface of a spacer for a hard disk drive device made of any material. The arithmetic mean roughness Ra of the surface of the film 22 is preferably 1 μm or less. The surface resistivity of the film 22 at 22 [°C] is 10 -4 to 10 6It is preferable that the resistivity is [Ω / sq]. By using such a material, even if the spacer 1 or magnetic disk 5 becomes charged, the surface resistivity of the spacer 1 is small, so charge can flow from the spacer 1 through the spindle 14, or from the magnetic disk 5 through the spacer 1 and spindle 14, to the outside of the spacer 1 and magnetic disk 5, thereby suppressing the charging of the spacer 1 and magnetic disk 5. The surface resistivity can be measured, for example, using a four-probe resistivity meter. The material of the film 22 is, for example, tin-containing ceramics containing tin oxide, or zinc-containing ceramics containing zinc oxide. Alternatively, a material containing titanium oxide may be used. Furthermore, materials doped with fluorine or aluminum oxide may be used. Since the film 22 formed from these materials is conductive, the surface resistivity of the spacer 1 having the film 22 at 22°C is set to 10 -4 ~10 6 It can be expressed as [Ω / sq]. Thus, in the manufacturing method of the spacer 1, the film 22 is formed by rotating the outer peripheral end surface of the spacer body 20 in the circumferential direction while passing it through the area where the components of the film 22 are sprayed 23. This allows the film 22 to be formed over the entire surface of the spacer body 20, ensuring uniform film formation. Furthermore, since the entire surface is covered by the film 22, there are no exposed glass areas, thus suppressing dust generation. Moreover, because the process can be carried out under atmospheric pressure, the film 22 can be formed at a lower cost compared to PVD, CVD, etc. The manufacturing method of the spacer 1 described above is not limited to the method of forming a film 22 by rotating the outer peripheral end surface of the spacer body 20 in the circumferential direction while passing it through the area where the spray is applied 23, but other manufacturing methods can also be used. For example, the spacer body 20 may be placed on a stand such as a heating plate, and the film 22 may be formed on the entire surface by performing multiple sprays while appropriately changing the way it is placed and the spraying method. [Example 1] A glass spacer with an outer diameter of 32 mm, an inner diameter of 25 mm, and a thickness of 2 mm was prepared. The arithmetic mean roughness Ra of the main surface, inner circumferential end surface, and outer circumferential end surface of the glass spacer was set to 0.3 μm, 0.8 μm, and 0.8 μm, respectively. The film formation apparatus has a rectangular parallelepiped housing (chamber) structure containing a pair of rotating members (helical) equipped with a rotating shaft and a drive motor. Multiple spray nozzles and lamp heaters are provided at predetermined intervals on the upper and lower surfaces. The spray nozzles and lamp heaters are positioned to ensure sufficient film formation even as the glass spacer is transported. The glass spacer is passed through the rotating shaft inside the housing, and the rotating shaft is placed over the pair of rotating members. The output of the lamp heater is set so that the glass spacer is heated to 400°C, and an ethanol solution of dibutyltin diacetate is sprayed into a specific area inside the housing every 5 seconds to create a sprayed state in a part of the housing. Next, the transport speed of the glass spacer in the X direction (see Figure 6) is set to 10 cm / min, and the drive motor and other conditions are set so that the workpiece rotates at 3 rpm. The rotating shaft then moves while rotating on the rotating members, passing through the sprayed state. In this way, a film is formed on the surface of the glass spacer while it is heated and transported in the sprayed state. The thicknesses of the tin oxide films formed on the main surface, inner end face, and outer end face of the glass spacer were 70 nm, 82 nm, and 90 nm, respectively. Here, the film thickness on the end faces was thicker than that on the main surface. Furthermore, the difference between the maximum and minimum film thicknesses was 20 nm, and the maximum film thickness was 90 nm. Therefore, the difference between the maximum and minimum film thicknesses of the film 22 on the entire surface of spacer 1 satisfies the conditions of being less than half and less than one-quarter of the maximum film thickness, indicating very small variation in film thickness. The arithmetic mean roughness Ra of these surfaces was 0.3 μm, 0.8 μm, and 0.8 μm, respectively. The surface resistivity of the glass spacer after tin oxide film formation was 10 at 22 [°C]. -4 ~10 6 It was within the range of [Ω / sq]. [Example 2] Using a glass spacer of the same size as described above, the formation of a film on the glass spacer was repeated in the same manner as described above. By reducing the transport speed in the X direction during the spraying process, a film with a greater thickness than in Example 1 was formed. The thicknesses of the tin oxide films formed on the main surface, inner circumferential end surface, and outer circumferential end surface of the glass spacer were 140 nm, 170 nm, and 188 nm, respectively. Here, the film thickness on the end surfaces was thicker than the film thickness on the main surface. Furthermore, the difference between the maximum and minimum film thickness of the film 22 on the entire surface of the spacer 1 was less than half of the maximum film thickness, indicating that the film thickness variation was small. The arithmetic mean roughness Ra of these surfaces was 0.4 μm, 0.9 μm, and 1.0 μm, respectively. [Example 3] Using a glass spacer of the same size as described above, the formation of a film on the glass spacer was repeated in the same manner as described above. By increasing the transport speed in the X direction during the spraying process, a film with a smaller thickness than that of Example 1 was formed. The thicknesses of the tin oxide films formed on the main surface, inner circumferential end surface, and outer circumferential end surface of the glass spacer were 40 nm, 47 nm, and 51 nm, respectively. Here, the film thickness on the end surfaces was thicker than the film thickness on the main surface. Furthermore, the difference between the maximum and minimum film thickness of the film 22 on the entire surface of the spacer 1 was less than half and less than one-quarter of the maximum film thickness, indicating that the film thickness variation was very small. The arithmetic mean roughness Ra of these surfaces was 0.3 μm, 0.8 μm, and 0.8 μm, respectively. [Reference example] The same glass spacer as in Example 1 was placed on a heating plate and heated to 400°C. While maintaining this temperature, a solution of dibutyltin diacetate in ethanol was sprayed from above so that the film thickness on the main surface became 70 nm. Next, the glass spacer was turned over and placed on the heating plate, heated to 400°C, and then the solution of dibutyltin diacetate in ethanol was sprayed in the same manner. The thicknesses of the tin oxide films formed on the main surface, inner peripheral end face, and outer peripheral end face of the obtained glass spacer were 70 nm, 140 nm, and 140 nm, respectively. Although the film thickness on the end face was thicker than that on the main surface, the difference between the maximum film thickness and the minimum film thickness did not satisfy less than half of the maximum film thickness. That is, it was found that the film thickness variation of the film 22 on the entire surface of the spacer 1 was very large. Also, the arithmetic mean roughness Ra of these surfaces was 0.3 μm, 0.9 μm, and 0.9 μm, respectively. Two spacers produced in Example 1 were sandwiched between three magnetic disks (the main surface roughness Ra is 0.3 nm or less) as shown in FIG. 3 to produce an HDD device, and operation confirmation such as signal recording and reproduction by a magnetic head was performed. As a result, no particular problem was found. Similarly, HDD devices were produced for the spacers produced in Example 2, Example 3, and the reference example, and operation confirmation was performed. As a result, no particular problem was found. As described above, the glass spacer, hard disk drive device, and method for manufacturing the glass spacer of the present invention have been described in detail. However, the present invention is not limited to the above-described embodiments, and various improvements and modifications may be made without departing from the gist of the present invention. 1 Spacer 2 Outer peripheral end face 3 Inner peripheral end face 4 Main surface 5 Magnetic disk 10 Hard disk drive device 12 Motor 14 Spindle 16 Top clamp 20 Spacer body 22 Film 23 Spraying state 50 Rotating shaft 52 Moving mechanism 54 Rotating member
Claims
1. A method for manufacturing a ring-shaped glass spacer that is provided in contact with a magnetic disk within a hard disk drive device, wherein the glass spacer is formed by forming a film on the glass spacer body, and the method includes a process for forming the film on the surface of the glass spacer body, wherein the process forms the film by rotating the outer peripheral end face of the glass spacer body in a circumferential direction and passing it through a location where the components of the film are in an atomized state.
2. The method for manufacturing a glass spacer according to claim 1, wherein a rotating shaft that fits loosely into the hole of the ring-shaped glass spacer body is passed through the hole, and the rotating shaft is brought into contact with a part of the inner peripheral end face of the hole, thereby rotating the rotating shaft, thereby rotating the outer peripheral end face. 。 3. The method for manufacturing glass spacers according to claim 2, wherein the rotating shaft is mounted on a moving mechanism so as to move in one direction while rotating. Law.
4. The method for manufacturing a glass spacer according to any one of claims 1 to 3, wherein the sprayed area is formed by spraying the components of the film in mist form from both sides of the conveying path of the glass spacer body. method.
5. The method for manufacturing a glass spacer according to any one of claims 1 to 4, wherein the treatment includes heating the film formed on the glass spacer body. Construction method.
6. The glass spacer according to any one of claims 1 to 5, wherein the arithmetic mean roughness Ra of the surface of the film is 1 μm or less. Manufacturing method.
7. The surface resistivity of the film at 22°C is 10 -4 ~10 6 The glass spacer according to any one of claims 1 to 6, wherein the glass spacer has a thickness of [Ω / sq]. Manufacturing method.
8. The glass spacer according to any one of claims 1 to 7, wherein the film contains any one of tin oxide, zinc oxide, and titanium oxide. Manufacturing method of sa 9. A method for forming a film on the surface of a spacer for a hard disk drive device, comprising: a housing having at least a drive motor and a spray nozzle, and incorporating a spacer transport means in which a rotary shaft is hung between a pair of moving mechanisms. A device for doing this.
10. A ring-shaped glass spacer that is provided in contact with a magnetic disk in a hard disk drive device, wherein the entire surface of the glass spacer, including the main surface and end faces, is covered with a film containing one of tin oxide, zinc oxide, and titanium oxide, and the thickness of the film on the end faces of the glass spacer is thicker than the thickness of the film on the main surface of the glass spacer. Glass spacer.
11. The method according to claim 10, wherein the difference between the maximum and minimum thicknesses of the film on the entire surface of the glass spacer is less than half of the maximum thickness. Glass spacer.
12. The method according to claim 10 or 11, characterized in that the entire surface of the glass spacer is covered with the film having a thickness of less than 100 nm. The glass spacer described above.
13. Any one of claims 10 to 12, wherein the arithmetic mean roughness Ra of the end faces of the glass spacer is greater than the arithmetic mean roughness Ra of the main surfaces of the glass spacer. The glass spacer according to claim 1.
14. The surface resistivity of the film at 22°C is 10 -4 ~10 6 Any one of claims 10 to 13, wherein [Ω / sq] Item 2. A glass spacer according to item 1.
15. A magnetic disk comprising the glass spacer according to any one of claims 10 to 14. Hard disk drive device.