Method of fabricating electrochromic stack and apparatus thereof

TWI945550BActive Publication Date: 2026-11-11VIEW INC
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
TW113126090
Authority / Receiving Office
TW · TW
Patent Type
Patents
Current Assignee / Owner
Priority Date
2015-11-20
Filing Date
2016-07-13
Publication Date
2026-11-11
Estimated Expiration
2036-07-12

Smart Images

  • Figure TWG2TB001920295_001
    Figure TWG2TB001920295_001
  • Figure TWG2TB001920295_002
    Figure TWG2TB001920295_002
  • Figure TWG2TB001920295_003
    Figure TWG2TB001920295_003
Patent Text Reader

Abstract

The embodiments described herein relate to electrochromic stacks, electrochromic devices, and methods and apparatus for fabricating such stacks and devices. In several embodiments, the anodic coloring layer in the electrochromic stack or device is fabricated to include a heterogeneous structure, such as a heterogeneous composition and / or morphology. Such heterogeneous anodic coloring layers can be used to better tune the characteristics of the device.
Need to check novelty before this filing date? Find Prior Art

Description

Prior Technology

[0001] Electrochromism is a phenomenon in which a material exhibits reversible, electrochemically mediated changes in its optical properties when placed in different electronic states (typically due to voltage variations). These optical properties typically include one or more of color, transmittance, absorbance, and reflectance. A well-known electrochromic material is tungsten oxide (WO3). Tungsten oxide is a cathodic electrochromic material that undergoes a color transition from transparent to blue through electrochemical reduction. Electrochromic materials can be incorporated into, for example, windows and mirrors. The color, transmittance, absorbance, and / or reflectance of such windows and mirrors can be altered by inducing changes in the electrochromic material. A well-known application of electrochromic materials is, for example, rearview mirrors in some vehicles. In these electrochromic rearview mirrors, the change in the mirror's reflectivity at night prevents the headlights of other vehicles from disturbing the driver. Although electrochromism was discovered in the 1960s, electrochromic devices have encountered various problems in the past, which have prevented the technology from realizing its full commercial potential. Summary of the Invention

[0002] The embodiments described herein relate to electrochromic materials, electrochromic stacks, electrochromic devices, and methods and apparatus for preparing such materials, stacks, and devices. In several embodiments, the opposing electrode material may have a heterogeneous composition. In some cases, the opposing electrode may be deposited to comprise multiple sublayers, which may have different compositions and / or morphologies. In these or other cases, the opposing electrode may be deposited to include a gradient in composition. The gradient (if present) is typically along a direction perpendicular to the plane of the opposing electrode. In several embodiments, the composition is heterogeneous with respect to the concentration of one or more metals in the opposing electrode material. The compositional gradient may be distributed throughout the entire thickness of the opposing electrode or only on a portion of the opposing electrode (e.g., a sublayer). In one embodiment of the disclosed invention, an electrochromic device is provided, comprising: a substrate; an electrochromic layer disposed on or above the substrate, the electrochromic layer comprising a cathode-dyed electrochromic material; and a counter electrode layer disposed on or above the substrate, the counter electrode layer comprising (a) a first sublayer comprising a first anode-dyed material, and (b) a second sublayer comprising a second anode-dyed material, wherein the first anode-dyed material and the second anode-dyed material have different compositions, but each comprises an oxide of at least one transition metal, and wherein the first sublayer is disposed between the electrochromic layer and the second sublayer. In some embodiments, the first and second anode dyeing materials may each include at least one transition metal and another non-alkali metal. In some such embodiments, the first and second anode dyeing materials may each include nickel and tungsten. The second anode dyeing material may further include tantalum. The second anode dyeing material may further include niobium. The second anode dyeing material may further include tin. In some embodiments, the second anode dyeing material may include at least one transition metal, another non-alkali metal, and a second non-alkali metal, wherein the first anode dyeing material contains at least one transition metal and another non-alkali metal as its only metal. In some cases, the first and second anode dyeing materials may each include at least one transition metal, another non-alkali metal, and a second non-alkali metal, wherein the second anode dyeing material has a higher atomic concentration of the second non-alkali metal compared to the first anode dyeing material. At least one transition metal may be selected from the group consisting of: tungsten (W), tantalum (Ta), chromium (Cr), manganese (Mn), iron (Fe), cobalt (Co), nickel (Ni), rhodium (Rh), ruthenium (Ru), vanadium (V), iridium (Ir), and combinations thereof. Another non-alkali metal may be selected from the group consisting of: silver (Ag), aluminum (Al), arsenic (As), gold (Ag), boron (B), barium (Ba), beryllium (Be), bismuth (Bi), calcium (Ca), cadmium (Cd), cerium (Ce), cobalt (Co), chromium (Cr), copper (Cu), europium (Eu), iron (Fe), gallium (Ga), thorium (Gd), germanium (Ge), hafnium (Hf), mercury (Hg), indium (In), iridium (Ir), lanthanum (La), magnesium (Mg), manganese (Mn), molybdenum (Mo), niobium (Nb), neodymium (Nd), and osmium. (Os), ruthenium (Pa), lead (Pb), palladium (Pd), ferronium (Pr), protonium (Pm), polonium (Po), platinum (Pt), radium (Ra), rhenium (Re), rhodium (Rh), ruthenium (Ru), antimony (Sb), scandium (Sc), selenium (Se), silicon (Si), samarium (Sm), tin (Sn), strontium (Sr), tantalum (Ta), terbium (Tb), yttrium (Tc), tellurium (Te), thorium (Th), titanium (Ti), thallium (Tl), uranium (U), vanadium (V), tungsten (W), yttrium (Y), zinc (Zn), zirconium (Zr), and combinations thereof. In some embodiments, the other non-alkali metal may be selected from the group consisting of: silver (Ag), arsenic (As), gold (Au), boron (B), cadmium (Cd), copper (Cu), europium (Eu), gallium (Ga), thorium (Gd), germanium (Ge), mercury (Hg), osmium (Os), lead (Pb), palladium (Pd), protonium (Pm), polonium (Po), platinum (Pt), radium (Ra), tektium (Tb), deuterium (Tc), thorium (Th), thallium (Tl), and combinations thereof. In some cases, the other non-alkali metal may be selected from the group consisting of: tantalum (Ta), tin (Sn), and niobium (Nb). In a particular example, the other non-alkali metal is tantalum (Ta). In another example, the other non-alkali metal is tin (Sn). In yet another example, the other non-alkali metal is niobium (Nb). In some embodiments, the first and second anodic dyeing materials may each comprise a first transition metal, a second transition metal, and oxygen, wherein the ratio of the first transition metal to the second transition metal in the first and second anodic dyeing materials is different. In these or other embodiments, the opposing electrode layer may further comprise a third sublayer comprising a third anodic dyeing electrochromic material, wherein the first, second, and third anodic dyeing materials have different compositions, but each comprises at least one transition metal, and wherein the second sublayer is disposed between the first and third sublayers. The first anodic dyeing material may comprise at least one transition metal, a second transition metal (but no other transition metal), and oxygen; the second anodic dyeing material may comprise at least one transition metal, a second transition metal, a third transition metal, and oxygen; and the third anodic dyeing material may comprise at least one transition metal, a second metal, a third transition metal, and oxygen, and the second and third anodic dyeing materials may have different concentrations of the third transition metal. In some embodiments, the first and second sublayers of the opposing electrode layer may be in physical contact with each other. The first and second sublayers of the opposing electrode layers may be separated from each other by a defect-mitigating insulating layer, which in some cases has a resistivity between approximately 1 and 5 × 10¹⁰ ohm-cm. In several embodiments, the first anode coloring material has a first affinity for lithium and the second anode coloring material has a second affinity for lithium, wherein the first affinity for lithium and the second affinity for lithium may be different. Electrochromic devices may possess specific visual characteristics. In some embodiments, when the electrochromic device is in its most transparent state, its transmittance b* value may be about 14 or lower. For example, when the electrochromic device is in its most transparent state, its transmittance b* value may be about 10 or lower. When the electrochromic device is in its most transparent state, its visible light transmittance may be at least about 55%. The counter electrode layer may have a specific total thickness. In some embodiments, the counter electrode layer may have a total thickness between about 50 nm and about 650 nm (e.g., between about 100 nm and about 400 nm or between about 150 nm and about 300 nm). The first and second sublayers of the counter electrode layer may each have a morphology of a mixture of an amorphous phase and a nanocrystalline phase, wherein the nanocrystals have a diameter of less than about 50 nm. In some cases, the second sublayer may be a defect-mitigating insulating layer having a resistivity between about 1 and 5 × 10¹⁰ ohm-cm. The electrochromic device may further include a transparent conductive layer disposed on or above the electrochromic layer and the counter electrode layer. The transparent conductive layer may include doped indium oxide. In some embodiments, at least one of the first and second anodizing materials may include nickel, aluminum, and oxygen. In one example, the first anodizing material includes nickel, tungsten, and oxygen, while the second anodizing material includes nickel, aluminum, and oxygen. In some embodiments, at least one of the first and second anodizing materials includes nickel, silicon, and oxygen. For example, the first anodizing material may include nickel, tungsten, and oxygen, while the second anodizing material may include nickel, silicon, and oxygen. In another embodiment disclosed, an electrochromic device is provided, comprising: a substrate; an electrochromic layer disposed on or above the substrate, the electrochromic layer comprising a cathode-dyed electrochromic material; and an anode-dyed opposing electrode layer also disposed on or above the substrate, the opposing electrode layer comprising (a) a first sublayer comprising a first nickel-tungsten oxide composition, and (b) a second sublayer comprising a second nickel-tungsten oxide composition, wherein the first and second nickel-tungsten oxide compositions have different relative amounts of nickel and / or tungsten, and wherein the first sublayer is disposed between the electrochromic layer and the second sublayer. In some embodiments, the second nickel-tungsten oxide composition may further comprise tantalum, niobium, tin, or a combination thereof. In one example, the second nickel-tungsten oxide composition comprises tantalum. In another example, the second nickel-tungsten oxide composition comprises niobium. In yet another example, the second nickel-tungsten oxide composition comprises tin. In many embodiments, the first nickel-tungsten oxide composition may further comprise tantalum, wherein the second nickel-tungsten oxide composition comprises a greater concentration of tantalum compared to the first nickel-tungsten oxide composition. The first nickel-tungsten oxide composition may further comprise niobium, and the second nickel-tungsten oxide composition may comprise a greater concentration of niobium compared to the first nickel-tungsten oxide composition. In some cases, the first nickel-tungsten oxide composition may further comprise tin, and the second nickel-tungsten oxide composition may comprise a greater concentration of tin compared to the first nickel-tungsten oxide composition. The opposing electrode layer may include a third sublayer. The third sublayer may include a third nickel-tungsten oxide composition. The first, second, and third nickel-tungsten oxide compositions may contain different relative amounts of nickel and / or tungsten. A second sublayer may be disposed between the first and third sublayers. In some embodiments, the third nickel-tungsten oxide composition may further include tantalum, niobium, tin, or combinations thereof. In one example, the third nickel-tungsten oxide composition includes tantalum. In another example, the third nickel-tungsten oxide composition includes niobium. In yet another example, the third nickel-tungsten oxide composition includes tin. In some embodiments, the second and third nickel-tungsten oxide compositions may each include tantalum, and the third nickel-tungsten oxide composition may include a greater concentration of tantalum compared to the second nickel-tungsten oxide composition. In these or other embodiments, the second and third nickel-tungsten oxide compositions may each include niobium, and the third nickel-tungsten oxide composition may include a greater concentration of niobium compared to the second nickel-tungsten oxide composition. In some cases, the second and third nickel-tungsten oxide compositions may each include tin, and the third nickel-tungsten oxide composition may include a greater concentration of tin compared to the second nickel-tungsten oxide composition. In some embodiments, the opposing electrode layer may include a third sublayer comprising a third nickel-tungsten oxide composition, wherein the second nickel-tungsten oxide composition further comprises metal M1, the third nickel-tungsten oxide composition further comprises metal M2, and wherein metal M1 and metal M2 may be different from each other. In some such cases, the second nickel-tungsten oxide composition may be substantially free of metal M2, and the third nickel-tungsten oxide composition may be substantially free of metal M1. The first sublayer of the opposing electrode layer may be a flash layer having a thickness between about 10 nm and about 80 nm. In some cases, the thickness of the flash layer may be limited, for example, between about 10 nm and about 50 nm or between about 10 nm and about 30 nm. The first sublayer may have a specific resistivity, for example, between about 1 and 5 × 10¹⁰ ohm-cm. In some embodiments, the first and second sublayers of the opposing electrode layer may each have a thickness between about 20 nm and about 200 nm. In some such cases, the thickness of the first sublayer may differ from the thickness of the second sublayer by about 50 nm to about 200 nm. In some embodiments, the second nickel-tungsten oxide composition may include about 2-10% atomic tantalum, and the third nickel-tungsten oxide composition may include about 5-20% atomic tantalum. In some embodiments, the first sublayer may be substantially composed of nickel-tungsten oxide, the second sublayer may be substantially composed of nickel-tungsten-tantalum oxide with about 2-10% atomic tantalum, and the third sublayer may be substantially composed of nickel-tungsten-tantalum oxide with about 5-20% atomic tantalum. For example, the nickel-tungsten-tantalum oxide in the second sublayer may be about 4% atomic tantalum, and the nickel-tungsten-tantalum oxide in the third sublayer may be about 8% atomic tantalum. In another example, the second nickel-tungsten oxide composition may include about 2-10% atomic niobium, and the third nickel-tungsten oxide composition may include about 5-20% atomic niobium. The first sublayer may be substantially composed of nickel-tungsten oxide, the second sublayer may be substantially composed of nickel-tungsten-niobium oxide with about 2-10% atomic niobium, and the third sublayer may be substantially composed of nickel-tungsten-niobium oxide with about 5-20% atomic niobium. For example, the nickel-tungsten-niobium oxide in the second sublayer may be about 4% atomic niobium, and the nickel-tungsten-niobium oxide in the third sublayer may be about 8% atomic niobium. In another embodiment, the second nickel-tungsten oxide composition may include about 2-10% atomic tin, and the third nickel-tungsten oxide composition may include about 5-20% atomic tin. The first sublayer may be substantially composed of nickel-tungsten oxide, the second sublayer may be substantially composed of nickel-tungsten-tin oxide with about 2-10% atomic tin, and the third sublayer may be substantially composed of nickel-tungsten-tin oxide with about 5-20% atomic tin. For example, the nickel-tungsten-tin oxide in the second sublayer may be about 4% atomic tin, and the nickel-tungsten-tin oxide in the third sublayer may be about 8% atomic tin. In several embodiments, the second nickel-tungsten oxide composition may further include a metal not present in the first nickel-tungsten oxide composition. In some embodiments, at least one of the first and second sublayers of the opposing electrode layer may include a hierarchical composition. In many embodiments, the first and second sublayers of the opposing electrode layer may each have a morphology of a mixture of an amorphous phase and a nanocrystalline phase, wherein the nanocrystals have a diameter of less than about 50 nm. In another embodiment disclosed, a method for manufacturing an electrochromic device is provided, the method comprising: depositing an electrochromic layer comprising a cathode-colored electrochromic material; and depositing an opposing electrode layer as follows: depositing a first anode-colored sublayer and depositing a second anode-colored sublayer, wherein the first anode-colored sublayer is disposed between the electrochromic layer and the second anode-colored sublayer, and wherein the first and second anode-colored sublayers have different compositions and each comprises an oxide of at least one transition metal. In some embodiments, the second anode coloring sublayer may include one or more metals not present in the first sublayer. For example, the second anode coloring sublayer may include tantalum, while the first anode coloring sublayer may not include tantalum. In many embodiments, the first anode coloring sublayer may be substantially tantalum-free. In some instances, the second anode coloring sublayer may include niobium, while the first anode coloring sublayer may not include niobium. In many embodiments, the first anode coloring sublayer may be substantially niobium-free. In some embodiments, the second anode coloring sublayer may include tin, while the first anode coloring sublayer may not include tin. In many embodiments, the first anode coloring sublayer may be substantially tin-free. In some embodiments, the second anode coloring sublayer may include aluminum, while the first anode coloring sublayer may not include aluminum. The first anode coloring sublayer may be substantially aluminum-free. In these and other cases, the second anode coloring sublayer may include silicon, while the first anode coloring sublayer may not include silicon. The first anode coloring sublayer may be substantially silicon-free. In some embodiments, depositing the relative electrode layer may further include depositing a third anode coloring sublayer comprising an oxide of at least one transition metal, wherein the second anode coloring sublayer is disposed between the first and third anode coloring sublayers. In some such embodiments, the second and third anode coloring sublayers may each comprise a metal not present in the first anode coloring sublayer, and the atomic concentration of the metal not present in the first anode coloring sublayer in the third anode coloring sublayer may be higher than that in the second anode coloring sublayer. For example, the first anode coloring sublayer may be substantially composed of nickel-tungsten oxide, and the second and third anode coloring sublayers may be substantially composed of nickel-tungsten-tantalum oxide, and the concentration of tantalum in the third anode coloring sublayer may be higher than that in the second anode coloring sublayer. In some embodiments, different conditions may be used to deposit different sublayers. For example, a first anodic dyeing sublayer may be deposited at a higher deposition rate than a second anodic dyeing sublayer. In these or other cases, the first anodic dyeing sublayer may be deposited at a lower sputtering power than that used to deposit the second anodic dyeing sublayer. In some embodiments, the first anodic dyeing sublayer may be deposited at a sputtering power between about 5-20 kW / m², while the second sublayer may be deposited at a sputtering power between about 20-45 kW / m². In these or other embodiments, the temperature at which the electrochromic device is partially fabricated during the deposition of the first anodic dyeing sublayer may be lower than that during the deposition of the second anodic dyeing sublayer. The method may also include lithiating one or more layers and / or sublayers. For example, the method may further include lithiating the first anode color sublayer before depositing the second anode color sublayer. In one embodiment, the method further includes depositing lithium on the second anode color sublayer, and then, where appropriate, depositing a third anode color sublayer on the second anode color sublayer. In another embodiment, the method further includes depositing a third anode color sublayer on the second anode color sublayer, and then depositing lithium on the third anode color sublayer. In another embodiment of the disclosed invention, a method for manufacturing an electrochromic device is provided, the method comprising: depositing an electrochromic layer comprising a cathode-colored electrochromic material; and depositing an opposing electrode layer as follows: depositing a first anode-colored sublayer, lithiating the first anode-colored sublayer, and after lithiating the first anode-colored sublayer, depositing a second anode-colored sublayer, wherein the first anode-colored sublayer is disposed between the electrochromic layer and the second anode-colored sublayer, and wherein the first and second anode-colored sublayers have different compositions and each comprises an oxide of at least one transition metal. In another embodiment of the disclosed invention, an apparatus for manufacturing an electrochromic device is provided, the apparatus comprising: (a) an integrated deposition system comprising: (i) a first deposition station including one or more first targets for depositing an electrochromic material layer on a substrate when the substrate is placed in the first deposition station; (ii) a second deposition station including one or more second targets for depositing a first sublayer of a first opposing electrode material on the substrate when the substrate is placed in the second deposition station; (iii) a third deposition station including one or more third targets for depositing a second sublayer of a second opposing electrode material on the substrate when the substrate is placed in the third deposition station, the second opposing electrode material having a composition different from the first opposing electrode material; and (b) a controller including executable program instructions for causing a substrate to pass through the first, second, and third deposition stations in a manner that sequentially deposits a stack on the substrate, the stack including an electrochromic material layer, a first sublayer of the first opposing electrode material, and a second sublayer of the second opposing electrode material. In some embodiments, one or more second targets and one or more third targets may each include at least a pair of rotatable cylindrical targets. The controller may include executable instructions for depositing a first relative electrode material at a sputtering power lower than that used for depositing a second relative electrode material. In some embodiments, the controller may include executable instructions for depositing the first relative electrode material at a sputtering power between about 10-20 kW / m² and for depositing the second relative electrode material at a sputtering power between about 20-45 kW / m². The following will describe in further detail, with reference to the relevant drawings, these and other features and advantages of the disclosed embodiments. Simple Explanation of the Diagram

[0003] The following detailed description can be more fully understood when considered in conjunction with the diagram: Figure 1 is a schematic cross-sectional view of an electrochromic device according to certain embodiments. Figure 2 is a schematic cross-sectional view of an electrochromic device comprising two sub-layers relative to the electrode layer according to certain embodiments. Figure 3 is a schematic cross-sectional view of an electrochromic device comprising three sub-layers relative to the electrode layer according to certain embodiments. Figures 4A-4I show diagrams illustrating the composition of one or more layers in an electrochromic device according to various embodiments. Figure 5 illustrates a method for manufacturing an electrochromic stack as part of an electrochromic device according to certain embodiments. Figure 6A illustrates a rotating sputtering target according to certain embodiments. Figure 6B shows a top-down view of two rotating sputtering targets depositing material on a substrate according to some embodiments. Figures 7A-7C illustrate embodiments of using a secondary sputtering target to deposit material onto a primary sputtering target, which, according to some embodiments, is then deposited onto a substrate. Figure 8 illustrates the hysteresis curves used for depositing various optically switchable materials. Figures 9A-9E illustrate several embodiments of the integrated deposition system. Implementation

[0004] Electrochromic device A schematic cross-sectional view of an electrochromic device 100 according to some embodiments is shown in FIG1. ​​The electrochromic device includes a substrate 102, a conductive layer (CL) 104, an electrochromic layer (EC) 106 (sometimes also referred to as a cathode coloring layer or cathode dyeing layer), an ion-conducting layer (IC) 108, a counter electrode layer (CE) 110, and a conductive layer (CL) 114. The counter electrode layer 110 may be an anode coloring / dyeing layer and is sometimes referred to as an "ion storage" layer because ions reside there when the electrochromic device is not colored. The counter electrode layer is sometimes referred to herein as an anode coloring / dyeing counter electrode layer, or even as an anode coloring / dyeing electrochromic layer. When the counter electrode layer 110 is described as an "electrochromic" layer, it should be understood that the counter electrode layer is colored when driven by an anode potential because ions are expelled from this layer, or becomes clear and substantially transparent when driven by a cathode potential because ions are re-intercalated. Elements 104, 106, 108, 110, and 114 are collectively referred to as electrochromic stack 120. A voltage source 116 operable to apply a potential to the electrochromic stack 120 enables the electrochromic device to transition from, for example, a clear state to a stained state. In other embodiments, the order of the layers is reversed relative to the substrate. That is, the layers are arranged in the following order: substrate, conductive layer, opposing electrode layer, ion-conducting layer, electrochromic material layer, conductive layer. The conductive layer is typically a transparent conductive layer; however, in reflective devices, the conductive layer may be reflective, such as a metal layer. It should be understood that references to the transition between a transparent and stained state are not limiting and merely indicate one of many instances of achievable electrochromic transitions. Unless otherwise stated, whenever a clear-stained transition is mentioned herein, the corresponding apparatus or method encompasses other optical state transitions, such as non-reflective-reflective, transparent-opaque, etc. Furthermore, the terms "clear" and "bleached" refer to optically neutral states, such as unstained, transparent, or translucent. Additionally, unless otherwise specified herein, the "color" or "chroma" of an electrochromic transition is not limited to any particular wavelength or wavelength range. As will be understood by those skilled in the art, appropriate electrochromic properties and the selection of the relative electrode material control the associated optical transition. In several embodiments herein, the relative electrode is deposited to include heterogeneous composition and / or morphology. For example, the relative electrode may comprise two or more sublayers, in some cases having different compositions and / or morphologies. In these or other cases, the entire relative electrode or sublayers of the relative electrode may include a gradient in composition. Although Figure 1 shows the relative electrode layer 110 as a simple layer, it should be understood that many embodiments herein utilize heterogeneous relative electrode layers. In some embodiments, the electrochromic device reversibly cycles between a clear state and a stained state. In the clear state, a potential is applied to the electrochromic stack 120 such that ions available in the stack that can cause the electrochromic material 106 to enter the stained state are primarily residing in the opposing electrode 110. When the potential on the electrochromic stack reverses, ions are transported through the ion-conducting layer 108 to the electrochromic material 106, causing the material to enter the stained state. In some embodiments, all materials used to fabricate the electrochromic stack 120 are inorganic, solid (i.e., solid-state), or both inorganic and solid. Because organic materials tend to degrade over time, inorganic materials offer the advantage of a reliable electrochromic stack that functions over extended periods. Solid-state materials also offer the advantage of not having the containment and leakage problems often present with liquid materials. The individual layers in the electrochromic device are discussed in detail below. It should be understood that any one or more layers in the stack may contain some amount of organic material, but in many embodiments, one or more layers contain very little or no organic matter. The same applies to liquids that may be present in small amounts in one or more layers. It should also be understood that solid materials can be deposited or otherwise formed by methods employing liquid components (such as certain methods using sol-gel or chemical vapor deposition). Referring again to Figure 1, voltage source 116 is typically a low-voltage power supply and can be configured to operate in conjunction with radiation and other environmental sensors. Voltage source 116 can also be configured to connect to an energy management system (e.g., a computer system) that controls the electrochromic device based on factors such as year, day, and measured environmental conditions. Such energy management systems, combined with large-area electrochromic devices (i.e., electrochromic windows), can significantly reduce building energy consumption. Any material with suitable optical, electrical, thermal, and mechanical properties can be used as substrate 102. Such substrates include, for example, glass, plastics, and mirror materials. Suitable plastic substrates include, for example, acrylic, polystyrene, polycarbonate, allyl diethylene glycol carbonate, SAN (styrene-acrylonitrile copolymer), poly(4-methyl-1-pentene), polyester, polyamide, etc. If a plastic substrate is used, a hard film such as a diamond-like protective coating, silica / silicone anti-abrasion coating, or the like, well known in plastic polishing techniques, can be used to provide barrier protection and prevent abrasion. Suitable glass includes clear or tinted soda-lime glass, including soda-lime float glass. The glass can be tempered or untempered. In some embodiments of the electrochromic device 100 using glass (e.g., soda-lime glass) as substrate 102, a sodium diffusion barrier layer (not shown) exists between substrate 102 and conductive layer 104 to prevent sodium ions from diffusing from the glass into conductive layer 104. The substrate may also include alkali-free (e.g., sodium-free) fused glass, such as Corning Incorporated's Gorilla Glass™, Willow Glass™, and similar commercially available products. If such an alkali-free substrate is used, a diffusion barrier is not required; however, a light-adjusting layer can be used between the substrate and the electrochromic device to optimize the color and reflective properties, such as those of a window. In some embodiments, the optical transmittance of substrate 102 (i.e., the ratio of transmitted radiation or spectrum to incident radiation or spectrum) is about 40 to 95%, for example, about 90-92%. The substrate may have any thickness, provided it possesses mechanical properties suitable for supporting the electrochromic stack 120. While substrate 102 may have any size, in some embodiments it is about 0.01 mm to 10 mm thick, and in some cases about 3 mm to 9 mm thick. In some embodiments, the substrate is architectural glass. Architectural glass is glass used as a building material. Architectural glass is typically used in commercial buildings, but can also be used in residential buildings, and typically, but not necessarily, separates indoor and outdoor environments. In some embodiments, the architectural glass is at least 20 inches by 20 inches, and can be much larger, for example, about 72 inches by 120 inches. Architectural glass is typically at least about 2 mm thick. Architectural glass less than about 3.2 mm thick cannot be tempered. In some embodiments using architectural glass as the substrate, the substrate can still be tempered even after an electrochromic stack has been fabricated on it. In some embodiments using architectural glass as the substrate, the substrate is soda-lime glass from a tin float glass production line. A conductive layer 104 is formed on top of the substrate 102. In some embodiments, one or both of conductive layers 104 and 114 are inorganic and / or solid. Conductive layers 104 and 114 can be made of many different materials, including conductive oxides, thin metal coatings, conductive metal nitrides, and composite conductors. Typically, conductive layers 104 and 114 are transparent at least in the wavelength range in which the electrochromic layer exhibits electrochromism. Transparent conductive oxides include metal oxides and metal oxides doped with one or more metals. Examples of such metal oxides and doped metal oxides include indium oxide, indium tin oxide, doped indium oxide, tin oxide, doped tin oxide, zinc oxide, zinc aluminum oxide, doped zinc oxide, ruthenium oxide, doped ruthenium oxide, and the like. Because oxides are often used in these layers, they are sometimes referred to as "transparent conductive oxide" (TCO) layers. The function of the conductive layer is to diffuse the potential provided by voltage source 116 on the surface of electrochromic stack 120 into the interior regions of the stack with almost no ohmic potential drop. Further details and examples relating to TCO layers are provided in U.S. Patent Application No. 12 / 645,111, filed December 22, 2009, entitled "Fabrication of Low Deceptive Electrochromic Devices," which is incorporated herein by reference in its entirety. A cathode-colored layer 106 (also referred to as an electrochromic layer 106) covers the conductive layer 104. In some embodiments, the electrochromic layer 106 is inorganic and / or solid, and in typical embodiments it is both inorganic and solid. The electrochromic layer may contain any one or more of a variety of different cathode-colored electrochromic materials, including metal oxides. Such metal oxides include tungsten oxide (WO3), molybdenum oxide (MoO3), niobium oxide (Nb2O5), titanium oxide (TiO2), vanadium oxide (V2O5), tantalum oxide (Ta2O5), and the like. In some embodiments, the metal oxide is doped with one or more dopants, such as lithium, sodium, potassium, molybdenum, vanadium, titanium, and / or other suitable metals or metal-containing compounds. Mixed oxides (e.g., W-Mo oxide, W-V oxide) are also used in some embodiments. The cathode-colored electrochromic layer 106 containing metal oxides is capable of receiving ions transferred from the anode-colored electrode layer 110. Further details relating to the cathode-colored electrochromic layer are provided in U.S. Patent Application No. 12,645,111, which is incorporated herein by reference above. Generally, in cathode-colored electrochromic materials, the coloring / staining (or any change in optical properties such as absorbance, reflectance, and transmittance) of the electrochromic material is caused by the reversible insertion (e.g., embedding) of ions into the material and the corresponding charge-balanced electron injection. Typically, some of the ions responsible for the optical transition are irreversibly bound within the electrochromic material. As explained below, some or all of these irreversibly bound ions compensate for the "blind charge" in the material. In most electrochromic materials, suitable ions include lithium ions (Li+) and hydrogen ions (H+) (i.e., protons). However, in some cases, other ions will be suitable. These ions include, for example, deuterium ions (D+), sodium ions (Na+), potassium ions (K+), calcium ions (Ca++), barium ions (Ba++), strontium ions (Sr++), and magnesium ions (Mg++). In several embodiments described herein, lithium ions are used to generate the electrochromic phenomenon. Lithium ions are inserted into tungsten oxide (WO3-y (0 < y ≤ ~0.3)) which changes the tungsten oxide from transparent (clear state) to blue (stained state). Referring again to Figure 1, in the electrochromic stack 120, an ion-conducting layer 108 covers the electrochromic layer 106. In some embodiments, this ion-conducting layer 108 is omitted during the deposition of layers in the stack, and the cathode-colored electrochromic layer 106 is deposited in direct physical contact with the anolyte-colored opposing electrode layer 110. As a result of certain processing steps, an interface region can be formed between the cathode-colored electrochromic layer 106 and the anolyte-colored opposing electrode layer 110, thereby allowing the interface region to act as an ion-conducting layer in the completed device. When the electrochromic device transitions between a clear state and a dyed state, the ion-conducting layer 108 acts as a medium for transporting ions (in an electrolyte manner). In various cases, the ion-conducting layer 108 is highly conductive to the associated ions of the electrochromic layer and the opposing electrode layer, but has sufficiently low electronic conductivity that electron transfer occurring during normal operation is negligible. The thin ion-conducting layer (sometimes also referred to as the ion conductor layer) with high ion conductivity allows for rapid ion conduction in high-performance electrochromic devices and thus allows for rapid switching. In some embodiments, the ion-conducting layer 108 is inorganic and / or solid. When manufactured from materials and in a manner that produces relatively few defects, the ion conductor layer can be made very thin to produce a high-performance device. In various embodiments, the ion conductor material has an ion conductivity between approximately 10⁸ Siemens / cm or ohm⁻¹cm⁻¹ and approximately 10⁹ Siemens / cm or ohm⁻¹cm⁻¹ and a resistance of approximately 10¹¹ ohm⁻¹. In other embodiments, the ion conductor layer may be omitted. In such embodiments, no separate ion conductor material is deposited when forming the electrochromic stack for the electrochromic device. Alternatively, in these embodiments, the cathodic-colored electrochromic material may be deposited in direct physical contact with the anodic-colored electrode material. One or both of the anodic and cathodic-colored materials may be deposited to include an oxygen-rich portion compared to the rest of the material. Typically, the oxygen-rich portion is in contact with other types of layers. For example, an electrochromic stack may include an anodic coloring material in contact with a cathode coloring material, wherein the cathode coloring material includes an oxygen-rich portion in direct physical contact with the anodic coloring material. In another example, the electrochromic stack includes an anodic coloring material in contact with a cathode coloring material, wherein the anodic coloring material includes an oxygen-rich portion in direct physical contact with the cathode coloring material. In yet another example, both the anodic and cathode coloring materials include oxygen-rich portions, wherein the oxygen-rich portion of the cathode coloring material is in direct physical contact with the oxygen-rich portion of the anodic coloring material. Oxygen-rich portions of these layers can be provided as different sublayers (e.g., cathode or anode coloring materials include oxygen-rich sublayers and less oxygen-rich sublayers). Oxygen-rich portions of the layers can also be provided in hierarchical layers (e.g., cathode or anode coloring materials may include an oxygen concentration gradient directly perpendicular to the surface of the layer). Embodiments omitting the ion conductor layer and where the anode coloring material is in direct contact with the cathode coloring electrochromic material are further discussed in the following U.S. patents, each of which is incorporated herein by reference in its entirety: U.S. Patent Nos. 8,300,298 and 8,764,950. On top of the ion-conducting layer 108 (when present) is an anodic dyeing layer 110 (also referred to as the relative electrode layer 110). In several embodiments herein, the relative electrode layer is deposited to include a heterogeneous structure. This structure may be heterogeneous in composition and / or morphology. Further details of the disclosed relative electrode structure and composition are provided below. In some embodiments, the relative electrode layer 110 is inorganic and / or solid. The relative electrode layer may contain one or more of a variety of different materials capable of acting as an ion reservoir when the electrochromic device is in a clear state. During an electrochromic transition induced, for example, by the application of an appropriate potential, the anodic dyeing relative electrode layer transfers some or all of its ions to the cathodic dyeing electrochromic layer, thereby causing the electrochromic layer to become dyed. In parallel, the relative electrode layer is dyed in the event of ion loss. In several embodiments, one or more defect mitigation insulating layers (DMILs) may be provided. Such DMILs may be provided between or within the layers depicted in FIG. 1. In some specific embodiments, DMILs may be provided between sublayers of opposing electrode layers, although DMILs may also be provided at alternative or additional locations. DMILs help minimize the risk of manufacturing defective devices. In some embodiments, the insulating layer has a resistivity between about 1 and 5 × 10¹⁰ ohm-cm. In some embodiments, the insulating layer contains one or more of the following metal oxides: cerium oxide, titanium oxide, aluminum oxide, zinc oxide, tin oxide, aluminum silicon oxide, tungsten oxide, nickel tungsten oxide, tantalum oxide, and oxidized indium tin oxide. In some embodiments, the insulating layer contains nitrides, carbides, oxynitrides, or oxycarbides, such as nitrides, carbides, oxynitrides, or oxycarbides of the listed oxides. As an example, the insulating layer includes one or more of the following metal nitrides: titanium nitride, aluminum nitride, silicon nitride, and tungsten nitride. The insulating layer may also contain a mixture or combination of oxide and nitride materials (e.g., silicon oxynitride). DMIL is further described in U.S. Patent No. 9,007,674, which is incorporated herein by reference above. The electrochromic devices in the embodiments described herein can also be scaled down to substrates smaller or larger than architectural glass. Electrochromic stacks can be deposited on substrates ranging in size from approximately 12 inches by 12 inches to as large as 80 inches by 120 inches. In some embodiments, the electrochromic glass is integrated into an insulating glass unit (IGU). The insulating glass unit consists of multiple glass sheets assembled into a single unit, typically intended to maximize the thermal insulation properties of the gas contained within the space formed by the unit while providing clear visibility through it. The insulating glass unit with the electrochromic glass, except for electrical leads for connecting the electrochromic glass to a voltage source, will resemble insulating glass units known in the present art. Since the electrochromic insulating glass unit may experience high temperatures (due to the absorption of radiant energy by the electrochromic glass), a more robust sealant than that used in conventional insulating glass units may be necessary. Examples include stainless steel spacers, high-temperature polyisobutylene (PIB), novel double sealants, foil-coated PIB tape for spacer joints, and the like. In some cases, the electrochromic glass may be incorporated into a laminate; this laminate may be a separate construction or incorporated into the IGU as one of the IGU panels. Relative electrode layer In many embodiments described herein, the anodized relative electrode layer is heterogeneous in composition or physical characteristics (such as morphology). Such heterogeneous relative electrode layers can exhibit improved color, switching behavior, lifetime, uniformity, process window, etc. In some embodiments, the opposing electrode layer comprises two or more sublayers, wherein these sublayers have different compositions and / or morphologies. One or more of such sublayers may also have a hierarchical composition. The compositional and / or morphological gradients can have any form of transition, including linear transitions, S-shaped transitions, Gaussian transitions, etc. Many advantages can be achieved by providing opposing electrodes in the form of two or more sublayers. For example, the sublayers can be different materials with complementary properties. One material may contribute to better color quality, while another material may contribute to high-quality, long-lifetime switching behavior. Combining materials can contribute to a high degree of film quality and uniformity, while simultaneously achieving a high deposition rate (and thus high throughput). Some of the approaches outlined herein can also contribute to better control of lithium distribution throughout the electrochromic device, and in some cases may result in improved morphology of the opposing electrode (e.g., higher transport) and an overall reduction in defects in the electrochromic device. Another benefit that may arise from the embodiments described herein is the availability of one or more intermediate states. The potential difference between the sublayers allows lithium to reside in discrete locations (e.g., to a certain extent within a specific sublayer), thereby enabling the electrochromic device to achieve intermediate color states, such as between a fully dyed device and a fully clear device. In some cases, intermediate states can be achieved by applying different voltages to the device. Including multiple sublayers within opposing electrode layers reduces or eliminates the need to apply different voltages to achieve different intermediate color states. These and other benefits of the disclosed embodiments are further described below. In some cases, the counter electrode includes a first sublayer of a first anodic-colored counter electrode material and one or more additional sublayers of a second anodic-colored counter electrode material. In various cases, the first sublayer of the CE layer may be located closer to the cathode-colored electrochromic material than the second (and, where applicable, additional) sublayers of the CE layer. In some embodiments, the first sublayer is a flash layer, typically characterized as a thin, often rapidly deposited layer with a thickness of no more than about 100 nm, and in various cases no more than about 80 nm. The flash layer may be between about 5 nm and about 100 nm thick, between about 10 nm and about 80 nm thick, or between about 10 nm and about 50 nm thick, or between about 10 nm and about 30 nm thick. In other cases, a separate flash layer (which may be an anodic-colored counter electrode material) may be provided between the electrochromic layer and the first sublayer of the counter electrode. In some embodiments, a flash layer may be provided between the second sublayer and the transparent conductor layer. The flash layer (if present) may or may not exhibit electrochromic properties. In some embodiments, the flash layer is made of a relative electrode material that does not change color with the remaining electrochromic / relative electrode layers (though this layer may have a composition very similar to other layers, such as anodized layers). In some embodiments, the first sublayer (the flash layer or thicker than the flash layer) has a relatively high resistivity (e.g., between about 1 and 5 × 10¹⁰ ohm-cm). Generally speaking, the first and second anodic coloring electrode materials can each be any anodic coloring electrode material independently. The first and / or second electrode materials can be binary metal oxides (e.g., oxides comprising two metals other than lithium or other transport ions, NiWO being an example), ternary metal oxides (e.g., oxides comprising three metals, NiWTaO being an example), or even more complex materials. In many cases, these materials also include lithium, which is mobile to some extent within the device. Specific examples of anodic coloring electrode materials are provided below. As used herein, the term metal is intended to include metals and metalloids (e.g., B, Si, Ge, As, Sb, Te, and Po). In some embodiments, the first anodizing material may include at least one transition metal selected from the group consisting of chromium (Cr), manganese (Mn), iron (Fe), cobalt (Co), nickel (Ni), rhodium (Rh), ruthenium (Ru), vanadium (V), and iridium (Ir). In addition to one or more of the transition metals just listed, the first anodizing material may include at least one or more additional metals (in many cases, at least one non-alkali metal). In some embodiments, the additional metal may be selected from the group consisting of silver (Ag), aluminum (Al), arsenic (As), gold (Ag), barium (Ba), beryllium (Be), bismuth (Bi), calcium (Ca), cadmium (Cd), cerium (Ce), cobalt (Co), chromium (Cr), copper (Cu), europium (Eu), iron (Fe), gallium (Ga), thorium (Gd), germanium (Ge), hafnium (Hf), mercury (Hg), indium (In), iridium (Ir), lanthanum (La), magnesium (Mg), manganese (Mn), molybdenum (Mo), niobium (Nb), and neodymium (Nd). Osmium (Os), ruthenium (Pa), lead (Pb), palladium (Pd), tungsten (Pr), protonium (Pm), polonium (Po), platinum (Pt), radium (Ra), rhenium (Re), rhodium (Rh), ruthenium (Ru), antimony (Sb), scandium (Sc), selenium (Se), silicon (Si), samarium (Sm), tin (Sn), strontium (Sr), tantalum (Ta), terbium (Tb), deuterium (Tc), tellurium (Te), thorium (Th), titanium (Ti), thallium (Tl), uranium (U), vanadium (V), tungsten (W), yttrium (Y), zinc (Zn), zirconium (Zr), and combinations thereof. In these or other embodiments, the second anodic coloring material may be a first anodic coloring material doped or otherwise combined with one or more additional elements. The additional elements may include at least one non-alkali metal in various cases. In some embodiments, the one or more additional elements are selected from the group consisting of: silver (Ag), aluminum (Al), arsenic (As), gold (Ag), barium (Ba), beryllium (Be), bismuth (Bi), calcium (Ca), cadmium (Cd), cerium (Ce), cobalt (Co), chromium (Cr), copper (Cu), europium (Eu), iron (Fe), gallium (Ga), thorium (Gd), germanium (Ge), hafnium (Hf), mercury (Hg), indium (In), iridium (Ir), lanthanum (La), magnesium (Mg), manganese (Mn), molybdenum (Mo), niobium (Nb), and neodymium (Nd). The additional elements include osmium (Os), ruthenium (Pa), lead (Pb), palladium (Pd), tungsten (Pr), protonium (Pm), polonium (Po), platinum (Pt), radium (Ra), rhenium (Re), rhodium (Rh), ruthenium (Ru), antimony (Sb), scandium (Sc), selenium (Se), silicon (Si), samarium (Sm), tin (Sn), strontium (Sr), tantalum (Ta), terbium (Tb), deuterium (Tc), tellurium (Te), thorium (Th), titanium (Ti), thallium (Tl), uranium (U), vanadium (V), tungsten (W), yttrium (Y), zinc (Zn), zirconium (Zr), and combinations thereof. In some embodiments, the additional element may include at least one element selected from the group consisting of tantalum, tin, niobium, zirconium, silicon, aluminum, and combinations thereof. While the additional element may be a dopant in the second anode coloring material, it is not necessarily so. In some compositions, the additional element forms a compound or salt with other elements of the material. In one particular example, the first anode coloring material is NiWO. In these or other examples, the second anode coloring material may be NiWO doped with or otherwise including an additional metal (e.g., a non-alkali metal, transition metal, post-transition metal, or in some cases, a metalloid), wherein the additional metal is selected from the list presented above, and an exemplary material is NiWTaO. Other examples of second anode coloring materials in which the first anode coloring material is NiWO include, but are not limited to, NiWSnO, NiWNbO, NiWZrO, NiWAlO, and NiWSiO. In some similar embodiments, the first anode coloring material may be NiWO and the second anode coloring material may be nickel oxide doped with or otherwise including an additional metal (e.g., a non-alkali metal, transition metal, post-transition metal, or in some cases, a metalloid), wherein the additional metal is selected from the list presented above. Exemplary materials for the second anode coloring material include, but are not limited to, NiTaO, NiSnO, NiNbO, NiZrO, NiAlO, NiSiO, and combinations thereof. In one example, the second anode coloring material may be selected from the group consisting of NiTaO, NiSnO, NiNbO, NiAlO, NiSiO, and combinations thereof. In another example, the second anode coloring material may be selected from the group consisting of NiAlO and NiSiO. In some embodiments, the first and second anodizing materials contain the same elements but in different proportions. For example, the two materials may contain Ni, W, and Ta, but two or three of these elements are present in different masses or atomic ratios. The following examples further illustrate this option. In other embodiments, the first and second sublayers may be more significantly different in composition from each other. For example, the first and second sublayers (and any additional sublayers) may each be any anodizing material, regardless of the composition of the other sublayers. As mentioned, other examples of anodizing materials are provided below. Two or more sublayers may have different physical properties. In various cases, the material used in one or more of the sublayers will not perform as well as the relative electrode material if it is not provided together with the accompanying sublayer (e.g., it will exhibit poor color quality, poor lifetime performance, slow switching speed, slow deposition rate, etc.). Figure 2 provides a cross-sectional view of an electrochromic stack deposited according to one embodiment. The stack includes transparent conductive oxide layers 204 and 214. A cathode-colored electrochromic layer 206 is in contact with the transparent conductive oxide layer 204. An anodic-colored opposing electrode layer 210 is in contact with the transparent conductive oxide layer 214, the anodic-colored opposing electrode layer including two sublayers 210a and 210b. The first sublayer 210a of the opposing electrode is in contact with the electrochromic layer 206, while the second sublayer 210b is in contact with the transparent conductive oxide layer 214. In this embodiment, a separate ion conductor layer is not deposited (however, as described in more detail herein, an interface region acting as an ion conductor layer can be constructed in situ). The first and second sublayers 210a and 210b of the anodic coloring relative electrode layer 210 may have different compositions and / or morphologies. In various examples, the second sublayer 210b includes at least one metal and / or metal oxide not present in the first sublayer 210a. In one particular example, the first sublayer 210a is NiWO and the second sublayer 210b is doped or otherwise combined with another metal of NiWO (e.g., NiWTaO, NiWSnO, NiWNbO, NiWZrO, NiWAlO, NiWSiO, etc.). In another example, the first sublayer 210a is NiWO and the second sublayer 210b is doped or otherwise combined with another metal of nickel oxide (NiO) (e.g., NiTaO, NiSnO, NiNbO, NiZrO, NiAlO, NiSiO, etc.). In another embodiment, the first and second sublayers 210a and 210b include the same element at different relative concentrations. In some embodiments, the first sublayer 210a is a flash layer. The flash layer is typically a thin layer (and therefore it is typically, but not necessarily, deposited relatively quickly). In some embodiments, the first sublayer of the anodic coloring electrode is a flash layer between about 5 nm and about 100 nm thick, between about 10 nm and about 80 nm thick, between about 10 nm and about 50 nm thick, or between about 10 nm and about 30 nm thick. The thickness of the flash layer (or other opposing electrode sublayers not deposited as flash layers) depends on the materials selected for each sublayer. One consideration that may affect the maximum thickness of each sublayer is its color quality compared to the color quality of the remaining sublayers. In many cases, the remaining sublayers will have superior color performance (e.g., a less yellow, clearer appearance) compared to the first sublayer / flash layer. In a specific instance, the NiWTaO sublayer has superior color performance compared to the NiWO sublayer (which can be deposited as a flash layer). Therefore, the NiWO sublayer needs to be relatively thin to achieve the desired overall color performance in the device; for example, a thin flash layer of NiWO will have a less yellow color compared to a thicker NiWO layer. One competing concern related to the thickness of each sublayer is the relative deposition rate of the material within the sublayer. In many embodiments, the first sublayer / flash layer may be a material deposited at a higher deposition rate compared to the materials in the remaining sublayers. Similarly, the first sublayer / flash layer may be deposited at a lower power compared to the remaining sublayers. These factors make it advantageous to use a relatively thick first sublayer to achieve higher throughput and / or reduce the amount of power used. These concerns are balanced by the factors described above to select an appropriate sublayer thickness. In many embodiments, the remaining sublayers may be thicker than the first sublayer 210a. In some embodiments where the opposing electrode layer 210 includes two sublayers (such as 210a and 210b), the second sublayer 210b may be between about 20 nm and about 300 nm thick, for example between about 150 nm and about 250 nm thick, or between about 125 nm and about 200 nm thick. In some embodiments, the second sublayer 210b is homogeneous in composition. Figure 4A presents a graph showing the concentrations of various elements present in the first and second sublayers 210a and 210b of Figure 2 in a specific embodiment where the first sublayer is NiM1O and the second sublayer is a compositionally homogeneous NiM1M2O. The first sublayer 210a is labeled CE1 and the second sublayer 210b is labeled CE2. In this example, the first sublayer has a composition of about 25% nickel, about 8% M1, and about 66% oxygen, while the second sublayer has a composition of about 21% nickel, about 3% M1, about 68% oxygen, and about 8% M2. In several embodiments, M2 may be a metal. In other embodiments, the second sublayer 210b may include a hierarchical composition. The composition may be hierarchical in terms of the relative concentrations of the metals present. For example, in some cases, the second sublayer 210b has a hierarchical composition in terms of metals not present in the first sublayer. In a particular example, the first sublayer is NiWO and the second sublayer is NiWTaO, wherein the concentration of tantalum is hierarchical throughout the second sublayer. The relative concentrations of the remaining elements (excluding tantalum) may be uniform throughout the second sublayer, or they may vary throughout the sublayer. In a particular example, the concentration of oxygen in the second sublayer 210b (and / or in the first sublayer 210a) may also be hierarchical. Figure 4B presents a graph showing the concentration of M2 in the first and second sublayers 210a and 210b of Figure 2, in a specific embodiment where the first sublayer is NiM1O and the second sublayer is a hierarchical NiM1M2O layer. As in Figure 4A, the first sublayer 210a is labeled CE1 and the second sublayer is labeled CE2. In this example, the concentration of M2 increases with the thickness of the second sublayer, reaching approximately 15% (atoms) on the surface of the second sublayer furthest from the EC layer. Other elements are omitted from the figure; however, in one embodiment, it reflects a composition substantially as described with respect to Figures 4A or 4D, which is adjusted where appropriate to accommodate varying M2 concentrations. In some embodiments, the concentration of M2 decreases with the thickness of the second sublayer, i.e., the concentration of M2 is highest and decreases on the surface of the second sublayer closest to the EC layer, reaching its lowest concentration on the surface of the second sublayer furthest from the EC layer. In another embodiment, the concentration of M2 is highest in the middle region of the second sublayer, that is, for example, the concentration of M2 is highest at the center of the second sublayer and decreases towards both sides of the second sublayer. In this embodiment, the concentration of M2 may not be the same on each side of the second sublayer. In some embodiments, the first and second sublayers may have compositions that are more distinct from each other. Figure 4C presents a graph showing the concentrations of various elements present in the first and second sublayers 210a and 210b of Figure 2 in an embodiment where the first sublayer is NiM1O and the second sublayer is NiM2O. In one particular case, M1 is tungsten and M2 is vanadium, but other metals and materials may also be used. Although Figure 4C shows that the concentrations of oxygen and nickel remain constant in the two sublayers of the opposing electrode layers, this is not always the case. The specific compositions described in Figures 4A-4C are provided merely as examples and are not intended to be limiting. Different materials and concentrations / compositions may also be used. Figure 3 shows other examples of electrochromic stacks similar to those shown in Figure 2. The stack in Figure 3 includes transparent conductive oxide layers 304 and 314, a cathode-colored electrochromic layer 306, and an anode-colored counter electrode layer 311. Here, the counter electrode layer 311 is composed of three sublayers 311a-c. The first sublayer 311a may be a flash layer as described above with respect to the first sublayer 210a of Figure 2. Sublayers 311a-c may each have different compositions. In some embodiments, the second and third sublayers 311b and 311c may include the same element at different relative concentrations. In another embodiment, all sublayers 311a-c include the same element at different relative concentrations. An IC layer (not shown in Figure 3) may be present between the electrochromic layer 306 and the counter electrode layer 311. In one example, the first sublayer 311a is a first anodic coloring relative electrode material, while the second and third sublayers 311b and 311c are second anodic coloring relative electrode materials (each deposited with a different composition). Within each sublayer, the composition of the second and third sublayers 311b and 311c can be homogeneous. Figure 4D presents a graph showing the concentration of M2 present in the first, second, and third sublayers 311a-c of Figure 3, where the first sublayer is NiM1O and the second and third sublayers are different compositions of homogeneous NiM1M2O. The first sublayer is labeled CE1, the second sublayer is labeled CE2, and the third sublayer is labeled CE3. Other elements (M1, Ni, and O) are omitted in Figure 4D. In one embodiment, these elements reflect a composition substantially as described with respect to Figures 4A or 4C, which are adjusted where appropriate for varying M2 concentrations. In a related embodiment, the concentration of M2 in the third sublayer may be lower than that in the second sublayer. In other cases, the composition in one or more of the second and third sublayers 311b and 311c may be hierarchical, for example, in terms of the concentration of metals (in some cases, metals not present in the first sublayer 311a). Figure 4E presents a graph showing the concentration of M2 present in the first, second, and third sublayers 311a-c of Figure 3, where the first sublayer (CE1) is NiM1O, the second sublayer (CE2) is NiM1M2O with a hierarchical M2 composition, and the third sublayer (CE3) is compositionally homogeneous NiM1M2O. Other elements (M1, Ni, and O) are omitted in Figure 4E. In one embodiment, these elements reflect a composition substantially as described with respect to Figures 4A or 4C, which is adjusted where appropriate to accommodate varying M2 concentrations. In a related embodiment, the composition may be hierarchical in the opposite direction. For example, the concentration of M2 may decrease rather than increase throughout the second sublayer (when moving from CE1 to CE3). As mentioned, in some embodiments, the second anodic coloring relative electrode material may be the first relative electrode material having an additional metal. In a particular embodiment, the concentration of this additional metal is lower in the second sublayer 311b and higher in the third sublayer 311c. In a particular example, the first sublayer 311a is NiWO, the second sublayer 311b is NiWTaO, the third sublayer 311c is NiWTaO, and the concentration of tantalum in the third sublayer 311c is higher than that in the second sublayer 311b. In a similar example, the first sublayer 311a is NiWO, the second and third sublayers 311b and 311c are NiWSnO, and the concentration of tin in the third sublayer 311c is higher than that in the second sublayer 311b. Many anodic coloring materials and combinations of materials can be used. In a different embodiment, the concentration of the additional metal in the second sublayer may be higher than that in the third sublayer. This trend (increasing or decreasing the concentration of the additional metal) can continue in many sublayers. Referring to Figure 2, in another example, the first sublayer 210a is NiWO, and the second sublayer 210b is NiAlO or NiWAlO. In another example, the first sublayer 210a is NiWO, and the second sublayer 210b is NiSiO or NiWSiO. Referring to Figure 3, in one example, the first sublayer 311a is NiWO, the second sublayer 311b is NiAlO, and the third sublayer 311c is NiAlO, with the aluminum concentration in the third sublayer 311c being higher (or lower) than in the second sublayer 311b. In another example, the first sublayer 311a is NiWO, the second sublayer 311b is NiSiO, and the third sublayer 311c is NiSiO, with the silicon concentration in the third sublayer 311c being higher (or lower) than in the second sublayer 311b. As mentioned above, the trend of increasing concentrations of additional (or different) metals (e.g., aluminum or silicon in these examples) in many sublayers is sustainable. In some cases, the concentration (atomic %) of the additional metal in the third sublayer 311c is at least 1.2 times the concentration of the additional metal in the second sublayer 311b. For example, the concentration of the additional metal in the third sublayer 311c may be at least about 1.5 times, at least about 2 times, or at least about 2.5 times the concentration of the additional metal in the second sublayer 311b. In some embodiments, more than one additional metal not present in the first sublayer 311a may be provided in the second and / or third sublayers 311b / 311c. In some specific embodiments, the third sublayer 311c may include another additional material (e.g., a metal or another element) not present in the first or second sublayers 311a and 311b. Detailing the examples provided above, in one embodiment, the first sublayer 311a may be NiWO (in any suitable composition), the second sublayer 311b may be NiWTaO (having a composition comprising about 7% (atomic) tantalum and any suitable relative composition of nickel, tungsten, and oxygen), and the third sublayer 311c may also be NiWTaO (having a composition comprising about 14% (atomic) tantalum and any suitable relative composition of nickel, tungsten, and oxygen). This example is shown in Figure 4D (where M1 is tungsten and M2 is tantalum). In a similar example, tantalum and / or tungsten may be replaced with different metals. As mentioned, many different materials can be provided for the first sub-layer. In multiple embodiments, the first sub-layer is NiM1O. In the case where the first sub-layer is NiM1O, it can be provided in any suitable composition. In certain embodiments, the NiM1O sub-layer has a composition of Ni xM1 yO z, where 0.2 < x < 0.3, 0.02 < y < 0.1, and 0.5 < z < 0.75. In many embodiments, M1 is tungsten (W), although the embodiments are not limited thereto. In the case where M1 is tungsten and the first sub-layer is NiWO, NiWO can have a composition of Ni xW yO z, where 0.2 < x < 0.3, 0.05 < y < 0.1, and 0.6 < z < 0.7. Similarly, many different materials can be provided for the second (and any additional, if present) sub-layer. As mentioned, these sub-layers will often include the material of the first sub-layer plus an additional metal (M2) and / or metal oxide. In the case where the first sub-layer includes NiM1O and the second / additional sub-layer includes NiM1M2O, the second / additional sub-layer can have a composition of Ni aM1 bM2 cO d, where 0.2 < a < 0.3, 0.05 < b < 0.1, 0.01 < c < 0.1, and 0.5 < d < 0.75. In many embodiments, the subscript c is lower in the sub-layer placed closer to the electrochromic layer and higher in the sub-layer placed farther from the electrochromic layer. The thickness of the sub-layer is generally determined by the total required thickness of the CE layer and the number of sub-layers used. The required total CE layer thickness is at least partially determined by the required charge capacity of the CE layer, and exemplary thicknesses are provided below. In the case where the counter electrode layer is provided in the form of three sub-layers as shown in FIG. 3, the first sub-layer 311a can be a relatively thin flash layer as described above. The second and third sub-layers 311b and 311c can have any relative thickness. For example, the second sub-layer 311b can be thinner, thicker, or approximately the same thickness as compared to the third sub-layer 311c. In some embodiments, additional sublayers may be provided. These additional sublayers may be homogeneous in composition or, as described above, hierarchical. The trends described regarding the first, second, and third sublayers of Figures 2 and 3 may also apply to all additional sublayers in the various embodiments providing such additional sublayers. In one example, the opposing electrode is deposited to include four sublayers, wherein the first sublayer (located closest to the electrochromic layer) comprises a first material (e.g., NiM1O), and the second, third, and fourth sublayers comprise a second material (e.g., NiM1M2O) that includes additional elements (e.g., metals) not present in the first sublayer. The concentration of this additional element may be higher in sublayers farther from the electrochromic layer and lower in sublayers closer to the electrochromic layer. As a specific example, the first sublayer (closest to the electrochromic layer) is NiWO, the second sublayer is NiWTaO with 3% (atomic) Ta, the third sublayer is NiWTaO with 7% (atomic) Ta, and the fourth sublayer (farthest from the electrochromic layer) is NiWTaO with 10% (atomic) Ta. In another embodiment, a counter electrode may be provided in the form of a monolayer, but the composition of the counter electrode layer may be hierarchical. The composition may be hierarchical with respect to one or more elements present in the material. In some embodiments, the counter electrode has a hierarchical composition with respect to one or more metals in the material. In these or other embodiments, the counter electrode may have a hierarchical composition with respect to one or more nonmetals (e.g., oxygen). Figure 4F presents a graph showing the concentration of M2 present in a counter electrode layer provided in the form of a monolayer with a hierarchical composition. In this example, the composition is hierarchical with respect to the metal (M2) therein. Other elements (Ni, M1, and O) are omitted in Figure 4F. In one embodiment, these elements reflect a composition substantially as described with respect to Figures 4A or 4C, which is adjusted where appropriate to accommodate a changing M2 composition. Where it is not desirable to be limited by theories or mechanisms of action, the first sublayer disclosed by Xianxin can help protect the ion-conducting and / or electrochromic layer from damage caused by overheating or other harsh conditions during the deposition of the opposing electrode layer. The first sublayer can be deposited under milder conditions than those used to deposit the remaining sublayers. For example, in some embodiments, the first sublayer can be deposited at a sputtering power between about 5-20 kW / m², while the second sublayer can be deposited at a sputtering power between about 20-45 kW / m². In a particular instance where the first sublayer is NiWO and the second sublayer is NiWTaO, NiWTaO can be deposited using a higher sputtering power than NiWO. If this high-power process is performed to directly deposit the ion-conducting and / or electrochromic layer, in some embodiments, the ion-conducting and / or electrochromic layer may be degraded, for example, due to overheating and premature crystallization of the associated materials and / or due to oxygen loss in the ion-conducting and / or electrochromic layer. However, by providing a thin flash layer of NiWO as the first sublayer, this NiWO layer can be deposited under milder conditions. The NiWO sublayer can then protect the underlying ion-conducting and / or electrochromic layer during the deposition of subsequent NiWTaO sublayers. This protection allows the electrochromic device to function more reliably and effectively. In some embodiments, the electrochromic device includes a tungsten oxide-based electrode layer that is cathode-colored; and a nickel oxide-based counter electrode layer that is anodic-colored; wherein the nickel oxide-based counter electrode layer includes at least a first sublayer and a second sublayer, each of the first and second sublayers having the formula Li aNiW xA yO z, where: a is 1 to 10; x is 0 to 1; y is 0 to 1; and z is at least 1; and where a, x, y, z, and A are selected independently for each of the first and second sublayers of the counter electrode layer. In some embodiments, y may be greater than 0 for at least one of the first and second sublayers of the opposing electrode layer. In some instances, y may be zero in the first sublayer of the opposing electrode layer and greater than zero in the second sublayer of the opposing electrode layer. In these or other embodiments, x may be greater than 0 for at least one of the first and second sublayers of the opposing electrode layer. For example, x may be greater than zero in the first sublayer of the opposing electrode layer and zero in the second sublayer of the opposing electrode layer. In several embodiments, the first and second sublayers have different compositions. For each of the first and second sublayers of the opposing electrode layer, A can be independently selected from the group consisting of: silver (Ag), aluminum (Al), arsenic (As), gold (Ag), boron (B), barium (Ba), beryllium (Be), bismuth (Bi), calcium (Ca), cadmium (Cd), cerium (Ce), cobalt (Co), chromium (Cr), copper (Cu), europium (Eu), iron (Fe), gallium (Ga), thorium (Gd), germanium (Ge), hafnium (Hf), mercury (Hg), indium (In), iridium (Ir), lanthanum (La), magnesium (Mg), manganese (Mn), molybdenum (Mo), niobium (N) b) Neodymium (Nd), osmium (Os), ruthenium (Pa), lead (Pb), palladium (Pd), ilium (Pr), protonium (Pm), polonium (Po), platinum (Pt), radium (Ra), rhenium (Re), rhodium (Rh), ruthenium (Ru), antimony (Sb), scandium (Sc), selenium (Se), silicon (Si), samarium (Sm), tin (Sn), strontium (Sr), tantalum (Ta), terbium (Tb), deuterium (Tc), tellurium (Te), thorium (Th), titanium (Ti), thallium (Tl), uranium (U), vanadium (V), tungsten (W), yttrium (Y), zinc (Zn), zirconium (Zr), and combinations thereof. In many embodiments, A can be a first metal in the first sublayer and a second metal in the second sublayer, the first metal being different from the second metal. In some embodiments, y in the first sublayer can be zero, making the first sublayer LiNiWO. In some embodiments, A in the first and / or second sublayers of the opposing electrode layer may be selected from the group consisting of Ta, Nb, Sn, Al, and Si. In these or other embodiments, A in each of the first and second sublayers of the opposing electrode layer may be selected from the group consisting of Ta, Nb, Sn, Al, and Si, wherein A in the first sublayer of the opposing electrode layer is different from A in the second sublayer of the opposing electrode layer. In some embodiments, y may be between about 0.1 and 1 for at least one of the first and / or second sublayers of the opposing electrode layer. In a particular embodiment, y may be between about 0.1 and 1 for each of the first and second sublayers of the opposing electrode layer. In some embodiments, the first sublayer of the opposing electrode may be NiWO, while the second sublayer of the opposing electrode may be a material selected from the group consisting of: NiWTaO, NiWNbO, NiWSnO, NiWAlO, NiWSiO, NiTaO, NiNbO, NiSnO, NiAlO, NiSiO, and combinations thereof. In some embodiments, the second sublayer of the opposing electrode may be a material selected from the group consisting of: NiWTaO, NiWNbO, NiWSnO, NiWAlO, NiWSiO, and combinations thereof. The second sublayer of the opposing electrode may be a material selected from the group consisting of: NiTaO, NiNbO, NiSnO, NiAlO, NiSiO, and combinations thereof. In various embodiments, the first and second sublayers of the opposing electrode may each be independently selected from the group consisting of: NiWO, NiWTaO, NiWNbO, NiWSnO, NiWAlO, NiWSiO, NiTaO, NiNbO, NiSnO, NiAlO, NiSiO, and combinations thereof, wherein the material of the first sublayer is different from the material of the second sublayer. In some embodiments, the first and second sublayers of the opposing electrode may each be independently selected from the group consisting of: NiWO, NiWTaO, NiWNbO, NiWSnO, NiWAlO, NiWSiO, and combinations thereof, wherein the material of the first sublayer is different from the material of the second sublayer. In some cases, the first and second sublayers of the opposing electrode may each be independently selected from the group consisting of: NiWO, NiTaO, NiNbO, NiSnO, NiAlO, NiSiO, and combinations thereof, wherein the material of the first sublayer is different from the material of the second sublayer. The disclosed embodiments also demonstrate improved performance due to higher quality morphology and improved morphology control within the anodized material. As described herein, the counter electrode material can be crystalline, nanocrystalline, amorphous, or a combination thereof. Often, a relatively low crystallinity is desired, and any existing crystals should be relatively small. By providing counter electrodes in the form of two or more sublayers, one or more additional interfaces (e.g., interfaces where sublayers contact each other) are introduced within the counter electrodes. These interfaces can, for example, interfere with crystal formation due to nucleation and associated grain growth effects. Such effects can prevent crystals from growing larger and limit the size of any crystals formed. This effect on morphology can result in less voids or other defects in the fabrication of the device. Similarly, when the counter electrode is deposited in the form of one or more sublayers, the sublayers can eliminate protrusions / dimples / stripes in the underlying layers. When the counter electrode layer is deposited in a single step as a single homogeneous layer, protrusions / dimples / stripes present in the underlying layers (which in some cases may originate from the substrate) are largely transferred to / through the counter electrode layer. In contrast, by depositing the counter electrode layer in several steps (e.g., using multiple sublayers), the sublayers can contribute to a smoother surface because protrusions / dimples / stripes are less noticeable in the presence of the additional deposited layers. Several benefits can be achieved by reducing the transfer of such surface inhomogeneities through the layers of the device. For example, sealing can be improved, resulting in improved humidity control. Relatedly, queuing time during manufacturing can be reduced, thereby improving throughput. Where it is not desired to be limited by theory or mechanism of action, it is also believed that the disclosed method can be used to achieve improved control over the distribution of lithium within an electrochromic device. Different relative electrode materials exhibit different affinities for lithium, and therefore the choice of relative electrode material affects how lithium ions are distributed within the electrochromic device. By selecting specific materials and combinations of materials, the distribution of lithium within the device can be controlled. In devices fabricated without depositing a separate ion-conducting layer, the distribution of lithium within the device can be particularly important. In such embodiments, the distribution of lithium throughout the device can affect whether an ion-conducting / substantially electronically insulating region is formed in the interface region between the electrochromic and relative electrode layers after the deposition of the electrochromic stack and further processing of the stack. In some embodiments, the sublayer of the relative electrode includes materials with different affinities for lithium. For example, the material of the first sublayer may have a higher or lower affinity for lithium compared to the material of the second (or additional) sublayer of the relative electrode. Accordingly, the disclosed method can be used to achieve improved control over the total amount of lithium used in the manufacture of electrochromic devices. In various cases, lithium can be added during the deposition of the opposing electrode layers. In some embodiments, lithium can be added during the deposition of one or more sub-layers of the opposing electrodes. In these or other embodiments, lithium can be added between subsequent sub-layers of the opposing electrodes. By controlling the distribution and total amount of lithium within the electrochromic device, device uniformity and appearance can be improved. Another benefit of using the disclosed technique is improved color and switching performance. As mentioned above, certain counter electrode materials exhibit superior performance in terms of color (e.g., a clearer, more transparent state, a more attractive colored state, etc.), switching speed, lifespan, and other properties. However, some materials that contribute to high-quality results in one property may have disadvantages in other properties. For example, a material ideal for exhibiting a very transparent and uncolored clear state may have problems associated with slow switching speeds and / or short lifespans. In various embodiments, it is possible to achieve a counter electrode with improved properties by combining this material with another counter electrode material (which may have its own problems such as a relatively yellower clear state). The disadvantages associated with one counter electrode material can be mitigated by the other counter electrode material. For example, in one particular embodiment, the first sublayer / glitter layer may be made of a material having acceptable (but not excellent) color quality in a clear state, while the second sublayer (and any additional sublayers present, if applicable) may be made of a material having excellent color quality in a clear state (compared to the material of the glitter layer). Color quality may be evaluated based on the a* and / or b* values ​​of the material, with higher quality colors typically corresponding to a* and b* values ​​close to zero, and lower quality colors typically corresponding to a* and b* values ​​farther from zero. In several embodiments, the a* and / or b* values ​​of the first and second sublayers (in their clear state) may differ by about 6 or at least about 3. In these or other cases, the a* and / or b* values ​​of the first and second sublayers (in their clear state) may differ by about 10 or less. In some cases, the flash layer can be deposited at a relatively high rate using low sputtering power, while the second sublayer can be deposited at a relatively low rate using even higher sputtering power. The first sublayer can help fabricate devices more quickly, while also protecting the ion-conducting and / or electrochromic layer during the formation of the opposing electrodes (e.g., by preventing the ion-conducting and / or electrochromic layer from being exposed to the high temperatures generated during the high-sputtering-power deposition of the second sublayer), while the second sublayer can help provide high-quality color performance for the device. In some cases, separating the counter electrode into multiple layers can improve reliability or reduce defect rates by adjusting the film stress within the film. Film stress within the counter electrode layer can improve or worsen the adhesion of subsequent layers, which can affect the long-term reliability of the device when subjected to changes in voltage, temperature, humidity, ambient light, etc. Changes in film stress can also affect the apparent defect rate of the device. Particles present on the substrate before or during device deposition can cause short circuits between electrode layers, leading to reduced staining in localized areas. Defect mitigation layers (DMILs) can be used to reduce the occurrence of such short circuits, and some embodiments of DMILs require manipulating the stress within the counter electrode to expel particles before the DMIL is applied. This description is in U.S. Patent Application No. 13 / 763,505, filed February 8, 2013, entitled "DEFECT-MITIGATION LAYERS IN ELECTROCHROMIC DEVICES". Multilayered electrodes may have a high-stress initial layer that allows particles to deform or be expelled, and a low-stress final layer that can fill any open areas created by the expelled particles. In some embodiments, the anolyte-colored counterpart electrode layer (or one or more sublayers thereof) is a material comprising nickel, tungsten, tantalum, and oxygen. These materials may be provided together in the form of NiWTaO in any suitable composition (or combination / arrangement of the composition throughout the counterpart electrode). Nickel-tungsten-tantalum-oxygen-based materials are particularly advantageous as anolyte materials because they can be specifically clear or color-neutral in their clear state. Many counterpart electrode materials are even slightly stained (colored) in their clear state. For example, NiWO typically has a slightly yellowish tint in its clear state. For aesthetic reasons, it is advantageous in various cases for both the cathode and anolyte colors in the electrochromic device to be very clear (transparent) and colorless when the device is in its clear state. Additionally, some anodizing electrode materials exhibit good color quality (i.e., very clear in their clear state) but are unsuitable for commercial use because their ability to undergo rapid optical transitions diminishes over time. In other words, for such materials, the duration of the optical transition increases with the lifespan / use of the device. In this case, a newly manufactured window will exhibit a higher switching rate than the same window that has been used for, for example, six months. One example of anodizing electrode materials exhibiting good color quality but a decreasing switching rate over time is nickel-tantalum oxide (NiTaO). It has been shown that including tungsten in such materials significantly reduces the decrease in switching rate over time. Therefore, NiTaO is a valuable candidate for one or more anodizing electrode materials. NiWTaO can have various compositions when used as an anodizing material. In some embodiments, a specific balance can be formed between the various components of NiWTaO. For example, the atomic ratio of Ni:(W+Ta) in the material can fall between about 1.5:1 and 3:1, for example, between about 1.5:1 and 2.5:1, or between about 2:1 and 2.5:1. In a particular example, the atomic ratio of Ni:(W+Ta) is between about 2:1 and 3:1. The atomic ratio of Ni:(W+Ta) is related to (i) the ratio of the total number of nickel atoms in the material to (ii) the total number of tungsten and tantalum atoms in the material. NiWTaO materials may also have a specific W:Ta atomic ratio. In some embodiments, the W:Ta atomic ratio is between about 0.1:1 and 6:1, for example, between about 0.2:1 and 5:1, or between about 1:1 and 3:1, or between about 1.5:1 and 2.5:1, or between about 1.5:1 and 2:1. In some cases, the W:Ta atomic ratio is between about 0.2:1 and 1:1, or between about 1:1 and 2:1, or between about 2:1 and 3:1, or between about 3:1 and 4:1, or between about 4:1 and 5:1. In some embodiments, specific Ni:(W+Ta) and W:Ta atomic ratios are used. All combinations of the disclosed Ni:(W+Ta) compositions and the disclosed W:Ta compositions are covered, although only certain combinations are explicitly listed herein. For example, the atomic ratio of Ni:(W+Ta) can be between about 1.5:1 and 3:1, where the atomic ratio of W:Ta is between about 1.5:1 and 3:1. In another example, the atomic ratio of Ni:(W+Ta) can be between about 1.5:1 and 2.5:1, where the atomic ratio of W:Ta is between about 1.5:1 and 2.5:1. In yet another example, the atomic ratio of Ni:(W+Ta) can be between about 2:1 and 2.5:1, where the atomic ratio of W:Ta is between about 1.5:1 and 2:1, or between about 0.2:1 and 1:1, or between about 1:1 and 2:1, or between about 4:1 and 5:1. Other exemplary materials for the counter electrode include, but are not limited to, nickel oxide, nickel-tungsten oxide, nickel-vanadium oxide, nickel-chromium oxide, nickel-aluminum oxide, nickel-manganese oxide, nickel-magnesium oxide, chromium oxide, iron oxide, cobalt oxide, rhodium oxide, iridium oxide, manganese oxide, and Prussian blue. These materials (e.g., metals and oxygen) may be provided in different stoichiometric ratios as appropriate for a given application. In other embodiments, the counter electrode material may include titanium cerium oxide, zirconium cerium oxide, nickel oxide, nickel-tungsten oxide, vanadium oxide, and mixtures of oxides (e.g., a mixture of Ni₂O₃ and WO₃). Doped formulations of these oxides may also be used, wherein dopants include, for example, tantalum and tungsten, and other elements listed above. Because the anodic coloring electrode layer contains ions that generate electrochromic phenomena in the cathode coloring electrochromic material when the cathode coloring electrochromic material is in a clear state, the anodic coloring electrode can have high transmittance and neutral color when it has a large number of these ions. When the charge is removed from the anodic coloring electrode (that is, when ions are transported from the electrode to the electrochromic layer), the electrode layer will change from a (more or less) transparent state to a colored state. The morphology of the counter electrode layer or any one or more sublayers therein can be crystalline, amorphous, or a mixture thereof. The crystalline phase can be nanocrystalline. In some embodiments, the counter electrode material layer (or one or more sublayers therein) is amorphous or substantially amorphous. Various substantially amorphous counter electrodes have been found to perform better than their crystalline counterparts under certain conditions. The amorphous state of one or more counter electrode oxide materials can be obtained by using certain processing conditions described below. While not wishing to be limited by any theory or mechanism, it is believed that amorphous counter electrode materials (such as nickel-tungsten oxide or nickel-tungsten-tantalum oxide) are generated by relatively low-energy atoms in a sputtering process. Low-energy atoms are obtained, for example, by using lower target power, higher chamber pressure (i.e., lower vacuum), and / or a larger source-to-substrate distance in the sputtering process. Amorphous films are also more likely to form in the presence of relatively high fractions / concentrations of heavy atoms (e.g., W). Under the process conditions described, films with better stability under UV / thermal exposure are produced. In essence, amorphous materials can possess some crystalline components, typically, but not necessarily, nanocrystalline materials dispersed within an amorphous matrix. The following describes the grain size and amount of such crystalline materials in more detail. In some embodiments, the morphology of the counter electrode or any sublayer therein may include microcrystalline, nanocrystalline, and / or amorphous phases. For example, the counter electrode may be a material having, for instance, an amorphous matrix in which nanocrystalline particles are distributed. In some embodiments, nanocrystalline particles constitute about 50% or less, about 40% or less, about 30% or less, about 20% or less, or about 10% or less of the counter electrode material (by weight or by volume, depending on the embodiment). In some embodiments, the nanocrystalline particles have a maximum diameter of less than about 50 nm, in some cases less than about 25 nm, less than about 10 nm, or less than about 5 nm. In some cases, the nanocrystalline particles have an average diameter of about 50 nm or less, or about 10 nm or less, or about 5 nm or less (e.g., about 1-10 nm). In some embodiments, it is required to have a nanocrystal size distribution in which at least about 50% of the nanocrystals have a diameter within one standard deviation of the average nanocrystal diameter, for example, at least about 75% of the nanocrystals have a diameter within one standard deviation of the average nanocrystal diameter, or at least about 90% of the nanocrystals have a diameter within one standard deviation of the average nanocrystal diameter. It has been found that relative electrode materials comprising amorphous matrices tend to function more effectively than relatively more crystalline relative electrode materials. In some embodiments, a material / additive may form a host matrix in which the crystalline domains of the base anodizing material are found. In various cases, the host matrix is ​​substantially amorphous. In some embodiments, only the crystalline structure in the relative electrode is formed by the base anodizing electrochromic material in, for example, oxide form. An example of a base anodizing electrochromic material in oxide form is nickel tungsten oxide. Additives may contribute to the formation of an amorphous host matrix that is not substantially crystalline, but which incorporates the crystalline domains of the base anodizing electrochromic material (e.g., nanocrystals in some cases). An exemplary additive is tantalum. In other embodiments, the additive, together with the anodizing base material, forms a compound having covalent and / or ionic bonds. This compound may be crystalline, amorphous, or a combination thereof. In other embodiments, the anodizing base material forms the host matrix in which the crystalline domains of the additive exist in discrete phase or capsule form. For example, some embodiments include an amorphous counterpart electrode having an amorphous matrix of a first material, wherein a second material (also amorphous) is distributed throughout the first material in the form of a capsule (e.g., a capsule having the diameter described herein with respect to crystalline material distributed throughout the amorphous matrix). In several embodiments, the sublayers within the opposing electrode layer may have different degrees of crystallinity. For example, the first sublayer may be more crystalline, less crystalline, or have approximately the same crystallinity as the second (or additional) sublayer of the opposing electrode. For example, the first sublayer may have a larger, smaller, or approximately equal average crystal size compared to the second (or additional) sublayer. The first sublayer may also have a larger, smaller, or approximately equal proportion of crystalline material compared to the second (or additional) sublayer. In some embodiments, the thickness of the relative electrode is from about 50 nm to about 650 nm. In some embodiments, the thickness of the relative electrode is from about 100 nm to about 400 nm, sometimes in the range of about 150 nm to 300 nm, or between about 200 nm and 300 nm. The thickness of the relative electrode layer is also substantially uniform. In one embodiment, the substantially uniform relative electrode layer varies only about ±10% within each of the above-described thickness ranges. In another embodiment, the substantially uniform relative electrode layer varies only about ±5% within each of the above-described thickness ranges. In yet another embodiment, the substantially uniform relative electrode layer varies only about ±3% within each of the above-described thickness ranges. The amount of ions present in the opposing electrode layer during the clear state (and correspondingly in the electrochromic layer during the dyed state) and available to drive the electrochromic transition depends on the layer composition, layer thickness, and manufacturing method. The electrochromic layer and opposing electrode layer can support approximately tens of millicoulombs of available charge (in the form of lithium ions and electrons) per square centimeter of layer surface area. The charge capacity of the electrochromic film is the amount of charge that can be reversibly loaded and unloaded per unit area and unit thickness of film by applying an applied voltage or potential. In one embodiment, the WO3 layer has a charge capacity between about 30 and about 150 millicoulombs / cm² / micrometer. In another embodiment, the WO3 layer has a charge capacity between about 50 and about 100 millicoulombs / cm² / micrometer. In one embodiment, the opposing electrode layer has a charge capacity between about 75 and about 200 millicoulombs / cm² / micrometer. In another embodiment, the opposing electrode layer has a charge capacity between about 100 and about 150 millicoulombs / cm² / micrometer. The relative electrode layer and / or electrochromic device may have specific characteristics when all layers / sublayers are considered. For example, in some embodiments, when the relative electrode is in its clearest state (when the relative electrode is held at its most cathode potential and ions are fully residing in the relative electrode layer of the device), the relative electrode will have a b* value between about 2 and 10 or between about 4 and 6. An electrochromic device manufactured according to the disclosed embodiments may have a b* value between about 6 and 14 or between about 9 and 12 when the device is in its clearest state. These values ​​will take into account the color that may be caused by the relative electrode layer and the electrochromic layer. An electrochromic window manufactured according to the disclosed technology may have a b* value between about 6 and 14 or between about 9 and 12 when the electrochromic window is in its clearest state. The b* value of such a window may be less than 10. In various cases, the electrochromic device and / or electrochromic window according to the disclosed embodiments may have a transmittance b* value of about 14 or less, 12 or less, or 10 or less when the device or window is in its clearest state. These values ​​will take into account the colors that may be caused by the opposing electrode layer, the electrochromic layer, the substrate (e.g., glass), the conductive oxide layer, and any other layers present in the window. Similarly, the relative electrode layer and / or electrochromic device may have a specific transmittance when in its clearest state. In some embodiments, the relative electrode layer will have at least about 65% visible light transmittance when in its clearest state. The electrochromic device disclosed herein may have at least about 55% visible light transmittance when in its clearest state. The electrochromic window manufactured as disclosed herein may have at least about 50% visible light transmittance when in its clearest state. In some embodiments, as described with respect to the relative electrode layer, the electrochromic layer may be implemented as two or more sublayers. Details relating to the differences between sublayers and to the variations within the layers may also apply to the electrochromic layer (instead of the relative electrode layer, or other than the relative electrode layer). Other states related to the composition of changes within the EC device The foregoing discussion largely focuses on embodiments involving opposing electrode layers with heterogeneous compositions. The composition of the opposing electrode is often heterogeneous in terms of the metals contained therein. Alternatively or additionally, the opposing electrode (or another layer / region in the electrochromic device) can be fabricated to include a heterogeneous composition in terms of another element (such as oxygen). In several embodiments, for example, the electrochromic and / or opposing electrode layers can be deposited to include oxygen-rich portions. The oxygen-rich portions (in some cases, provided as distinct sublayers, and in others, not provided as distinct sublayers) can be in contact with other electrode layers (e.g., the oxygen-rich portions of the electrochromic layer can be deposited in direct contact with the opposing electrode layer, and / or the oxygen-rich portions of the opposing electrode layer can be deposited in direct contact with the electrochromic layer). The heterogeneous structure of the electrochromic and / or opposing electrode layers can facilitate the formation of an interface region between these two layers, wherein (after further processing) the interface region acts as a region of ion conduction and substantial electronic insulation. The interface region itself can be heterogeneous in terms of composition and / or morphology. Generally, in some embodiments, the interface region may have a heterostructure comprising at least two discrete components represented by different phases and / or compositions. Additionally, the interface region may include a gradient among these two or more discrete components, such as ionicly conductive materials and electrochromic materials (e.g., a mixture of lithium tungstate and tungsten oxide). This gradient can provide, for example, variable compositions, microstructures, resistivity, dopant concentrations (e.g., oxygen concentrations), stoichiometry, density, and / or grain size schemes. The gradient can have many different forms of transition, including linear transitions, sigmoid transitions, Gaussian transitions, etc. Since the interface region can be formed from a portion of the electrochromic and / or opposing electrode layers, these layers can also be deposited to include such heterostructures. In some embodiments, an electrochromic stack can be provided as a hierarchical electrochromic element. The EC element does not have an abrupt transition between the EC layer and the IC layer, or between the IC layer and the CE layer, but is instead a single-layer hierarchical composition with EC regions transitioning to IC regions (interface regions), and IC regions transitioning to CE regions. Because the EC element is a single layer with a hierarchical composition, it can be described in many ways, as follows. The following description is intended to illustrate certain embodiments of the EC element. One embodiment is a monolayer hierarchical EC element comprising EC, IC, and CE regions. In one embodiment, the EC element is purely solid and inorganic. A single EC element can be described in many ways to understand its hierarchical composition. In several embodiments, the monolayer hierarchical EC element does not have abrupt boundaries between EC / IC or IC / CE. More precisely, both of these interfaces are characterized by hierarchical compositions as discussed herein. In some cases, the monolayer hierarchical EC element has a continuously variable composition in all regions of the element. In other cases, the element has at least one or at least two regions with a constant composition. Figures 4G-4I illustrate examples of how the composition of one type of EC element can be measured. In these particular examples, the EC region of the EC element comprises a first transition metal; the IC region comprises an alkali metal; and the CE region comprises a mixed transition metal oxide. IC regions, which may be formed after the EC and CE regions, are deposited in contact with each other. In one particular example, the mixed transition metal oxide comprises a first transition metal and an additional transition metal, while in other examples, the mixed transition metal oxide does not include the first transition metal. In some devices, Figures 4G-4I depict the same EC element, but in different ways. These ways each illustrate how many EC elements can be described according to the embodiments described herein. In this example, some of the components shown in the figures are present throughout the entire hierarchical composition, while others are not. For example, a transition metal is present continuously in a significant concentration throughout the device from the EC region through the CE region. The invention is not limited to this approach. In some embodiments, some or all of these components are present in at least a minimum amount (or even a large amount) throughout the EC element. In some instances, within the scope of Figures 4G-4I, each component is present in at least some of the regions of the EC element. Referring to Figure 4G, the EC element is described by the mole fractions of its constituent elemental composition as the regions EC, IC, or CE in which these components are present. Starting from the beginning and moving graphically from left to right, in the EC region, there is a higher mole fraction of oxygen (O) compared to the first transition metal (TM 1). For example, this could represent tungsten oxide with an oxygen to tungsten ratio of approximately 3:1. Moving further to the right, the mole fraction of the first transition metal begins to decrease at some point in the EC region. At some points in the CE region, the mole fractions of oxygen and the first transition metal are equal. For example, this could represent nickel-tungsten oxide with a stable composition in the CE region. In this example, the second transition metal (TM 2) is present throughout the EC element, and in this particular instance, it has a higher mole fraction in the CE region than in other regions of the EC element. Additionally, alkali metals (M alkalis) are present in the EC element. For the purposes of this specification, "alkali metal" is intended to encompass both neutral alkali metal elements and their cations, whether they are bound to or unbound in the material matrix and thus capable of being embedded / transported during device operation. In this example, the alkali metal has the highest molar fraction in the IC region. This may correspond to lithium in lithium tungstate present in this region in one example. As shown in Figure 4G, the oxygen concentration may also be highest in the IC region. This high oxygen concentration may be a result of the deposited material in the IC region being superstoichiometric relative to oxygen. In some embodiments, the material in the IC region may include the superstoichiometric (relative to oxygen) form of the material in the EC region and / or CE region. It is important to note that the components with molar fractions shown in Figure 4G are those fixed in the EC element, such as the alkali metal component, which does not include mobile lithium ions that can be used to drive the EC element to color or bleach (therefore, the ions are mobile and their position in the EC element will change depending on, for example, the applied charge). This example illustrates how the composition of an EC element can be described. One embodiment includes an EC element comprising: a) a first transition metal having a higher mole fraction in the EC region than a second transition metal (if present) in the EC region; b) an alkali metal having a maximum mole fraction in the IC region compared to both the EC and CE regions; and c) a second transition metal having its maximum mole fraction in the CE region in any region of the EC element. Referring to Figure 4H, if we consider the same EC element composition as described with respect to Figure 4G, but disregard oxygen content, this is another way to describe the embodiments described herein. For example, in this graph, the y-axis is not a mole fraction but a metal concentration; that is, the concentration of each metal TM1, Malkali, and TM2 in each region of the graded composition. In this example, the first transition metal and the alkali metal are each described by their concentration relative to the other two metals. The second transition metal is described by its absolute concentration. Referring to Figure 4H, in the EC region, the first transition metal has its maximum concentration relative to the other metals. The alkali metal has its maximum concentration relative to the other metals in the IC region. The second transition metal has its maximum (absolute) concentration in the CE region. In this example, TM1 and TM2 have substantially the same concentration in the CE region, for example, this could represent NiWO. One embodiment is an EC element, comprising: a) a first transition metal having the highest concentration in the EC region relative to other metals in the EC element; b) an alkali metal having the highest concentration in the IC region relative to other metals in the EC element; and c) a second transition metal having its absolute highest concentration in the CE region of the EC element. Figure 4I depicts the same EC element composition as described in Figures 4G and 4H, but focuses on the actual composition of each region, such as compounds. For example, in this figure, the y-axis represents the percentage composition of the following compounds in each region with a hierarchical composition: oxides of the first transition metal (TM 1-oxide), mixtures of oxides including alkali metals and the first and second transition metals (M alkali-TM 1-TM 2 oxide mixture), and mixed transition metal oxides (TM 1-TM 2 oxide). As mentioned, the mixed transition metal oxide does not necessarily include the first transition metal (e.g., it may include the second and third transition metals), but in this example it does. In this example, TM 1-oxide is most abundant in the EC region and is the major component of the EC region. The M alkali-TM 1-TM 2 oxide mixture is the major component of the IC region, and the TM 1-TM 2 oxide is the major component of the CE region. Note that the M alkali-TM 1-TM 2 oxide mixture may include more than one compound in the material matrix; for example, this oxide mixture may represent a hierarchical mixture of lithium tungstate, tungsten oxide, and nickel tungsten oxide. The morphology of the EC element in the layer can vary, that is, in any one or more of these regions, the hierarchical region can have amorphous portions, crystalline portions, and / or mixed amorphous and crystalline portions. In some embodiments, the CE region is substantially amorphous. One embodiment comprises an EC element including: a) a first transition metal oxide, which is the main component of the EC region; b) a mixed transition metal oxide, which is the main component of the CE region; and c) a mixture comprising a first transition metal and a mixed transition metal oxide, the mixture being the main component of the IC region. Another embodiment comprises an EC element including: a) a first transition metal oxide, which is the main component of the EC region; b) a mixed transition metal oxide, which is the main component of the CE region; and c) a mixture comprising an alkali metal compound, a first transition metal, and a mixed transition metal oxide, the mixture being the main component of the IC region. In one embodiment, the mixed transition metal oxide includes a first transition metal and a second transition metal selected from the group consisting of: nickel, tantalum, titanium, vanadium, chromium, cerium, cobalt, copper, iridium, iron, manganese, molybdenum, niobium, palladium, ruthenium, rhodium, and ruthenium. In one embodiment, the mixed transition metal oxide does not include a first transition metal. In one embodiment, the alkali metal is a lithium cation that associates as a transportable ion with a compound or with a material matrix during EC element operation. One embodiment is a method of manufacturing an electrochromic device, comprising: (a) forming an electrochromic layer comprising an electrochromic material or a counter electrode layer comprising a counter electrode material; (b) forming an intermediate layer on the electrochromic layer or the counter electrode layer, wherein the intermediate layer comprises an oxygen-rich form of at least one of the electrochromic material, the counter electrode material, and additional materials, wherein the additional materials comprise different electrochromic or counter electrode materials, and the intermediate layer is not substantially electronically insulating; (c) exposing the intermediate layer to lithium; and (d) heating the formed stack to transform at least a portion of the intermediate layer into a region co-extending with a region of the intermediate layer, the region comprising an electronically insulating ion-conducting material and the material of the intermediate layer. Since the intermediate layer can be formed from the oxygen-enriched form of EC and / or CE materials, the EC layer and / or CE layer can be understood as being formed to include heterogeneous components (e.g., including both oxygen-enriched and oxygen-depleted portions). Method for manufacturing electrochromic windows Electrochromic stacking deposition As mentioned above, one embodiment is a method for manufacturing an electrochromic window. Broadly, the method includes sequentially depositing (i) a cathode-colored electrochromic layer, (ii) an ion-conducting layer (if present), and (iii) an anolyte-colored opposing electrode layer on a substrate to form a stack, wherein (a) the ion-conducting layer separates the cathode-colored electrochromic layer from the anolyte opposing electrode layer, or (b) the cathode-colored electrochromic layer and the anolyte opposing electrode layer are in physical contact. In several embodiments, the opposing electrode layer is deposited to be heterogeneous in composition and / or morphology. For example, in some cases, the opposing electrode may be deposited to include sublayers. In some embodiments, the opposing electrode layer is deposited to include a hierarchical composition. The gradient may be along a direction perpendicular to the surface of the layer. Sequential deposition can employ a single integrated deposition system with a controlled ambient environment in which pressure, temperature, and / or gas composition are controlled independently of an external environment outside the integrated deposition system, and the substrate remains within the integrated deposition system at any time during the sequential deposition of the electrochromic layer, an ion-conducting layer (if applicable), and the opposing electrode layer. (Examples of integrated deposition systems maintaining a controlled ambient environment are described in more detail below with reference to Figures 9A-9E.) Gas composition can be characterized by the partial pressures of various components within the controlled ambient environment. The controlled ambient environment can also be characterized by particle number or particle density. In some embodiments, the controlled ambient environment contains fewer than 350 particles per cubic meter (having a size of 0.1 micrometers or larger). In some embodiments, the controlled ambient environment meets the requirements of a Class 1000 cleanroom (US FED STD 209E) or a Class 100 cleanroom (US FED STD 209E). In some embodiments, the controlled ambient environment meets the requirements of a Class 10 cleanroom (US FED STD 209E). The substrate can enter and / or leave the controlled surrounding environment of a cleanroom that meets Class 1000, Class 100 or even Class 10 requirements. Typically, but not necessarily, this manufacturing method is integrated into a multi-step process for fabricating electrochromic windows using architectural glass as a substrate, but the method is not limited thereto. Electrochromic mirrors and other devices can be manufactured using some or all of the operations and approaches described herein. Further details relating to the method for manufacturing electrochromic windows are set forth in U.S. Patent Application No. 12 / 645,111, which is incorporated herein by reference above. Methods for depositing electrochromic stacks may include sequentially depositing (i) a cathode-colored EC layer, (ii) an IC layer (if present), and (iii) an anodic-colored CE layer on a substrate to form a stack, wherein (a) the IC layer separates the EC layer from the CE layer, or (b) the EC layer and the CE layer are in physical contact with each other. This method can be performed in a single integrated deposition system with a controlled environment in which pressure and / or gas composition are controlled independently of an external environment outside the integrated deposition system, and the substrate may remain within the integrated deposition system at any time during the sequential deposition of the EC layer, the IC layer (if present), and the CE layer, under various conditions. In one embodiment, the sequentially deposited layers are each deposited by physical vapor deposition. Generally, layers of an electrochromic device can be deposited using a variety of techniques, including (to name only) physical vapor deposition, chemical vapor deposition, plasma-enhanced chemical vapor deposition, and atomic layer deposition. As used herein, the term physical vapor deposition includes the entire range of PVD techniques recognized in this art, including sputtering, evaporation, ablation, and similar techniques. Figure 5 illustrates one embodiment of a method 720 for forming an electrochromic stack. First, a cathode-colored EC layer is deposited on a substrate (process 722). Then, an IC layer, if present, may be deposited (process 724) (as mentioned above, in some embodiments, the IC layer is omitted, and therefore process 724 is omitted). A heterogeneous anode-colored CE layer may then be deposited (process 726). In some cases, the heterogeneous CE layer may be deposited in two or more steps. For example, in cases where the CE layer includes sublayers, the individual sublayers may be deposited using different methods / steps. A reverse order of deposition is also an embodiment, where the CE layer is deposited first, followed by, if present, the IC layer, and then the EC layer. In one embodiment, each of the electrochromic layer, the ion-conducting layer, and the opposing electrode layer, if present, is a solid phase layer. In these or other embodiments, each of the electrochromic layer, the ion-conducting layer, and the opposing electrode layer, if present, may consist only of inorganic materials. It should be understood that although some embodiments are described as relative electrode layers, ion conductor layers, and electrochromic layers, any one or more of these layers may consist of one or more sublayers, which may have different compositions, sizes, morphologies, charge densities, optical properties, etc. Furthermore, any one or more of the device layers may have a hierarchical composition or hierarchical morphology, wherein the composition or morphology varies within at least a portion of the layer thickness. Many of the embodiments described herein are presented in the context of opposing electrode layers including heterogeneous compositions and / or morphologies. The heterogeneous opposing electrode layers described may be used in conjunction with other layers or regions including hierarchical and / or sublayers with different compositions and / or morphologies (e.g., electrochromic layers, interface regions between EC and CE layers, etc.). In one instance, the concentrations of oxygen, dopants, or charge carriers vary within a given layer at least during its fabrication. In another instance, the morphology of the layer varies from crystalline to amorphous. Such hierarchical composition or morphology can be selected to influence the functional characteristics of the device. In some cases, additional layers may be added to the stack. In one instance, a heat dissipation layer is inserted between one or two TCO layers and the EC stack. The heat dissipation layer is made of a material with high thermal conductivity and thus allows heat to diffuse efficiently across the stack. Additionally, as described above, some embodiments of the electrochromic device utilize the movement of ions via an ion-conducting layer between the electrochromic layer and the opposing electrode layer. In some embodiments, this plasma (or its neutral precursor) is introduced into the stack in the form of a final embedding of one or more layers into the stack. Such layers may be deposited before, during, and / or after other layers in the deposition stack (e.g., EC, IC, CE layers). Alternatively (or further), one or more lithiation steps may be performed as intermediate steps between steps performed for electrode deposition. For example, the opposing electrode layer may be deposited by depositing a first sublayer, followed by lithium deposition thereon, and then ending by depositing one or more additional sublayers. In one embodiment, a first sublayer (which may be a flash layer) and a second sublayer are deposited sequentially, followed by lithiation, and then a third sublayer is deposited on the second sublayer. In another embodiment, a first sublayer (which may be a flash layer) and a second sublayer are deposited sequentially, followed by a third sublayer deposited on the second sublayer, and then lithium is deposited on the third sublayer. In some embodiments, a DMIL or capping layer is deposited on the third sublayer. Compared to depositing sublayers after lithiation, depositing sublayers before lithiation can result in sublayers with the same or different composition and / or morphology. Lithiation can also be performed during the deposition of a single sublayer, for example, when the sublayer material includes excess lithium, such that the deposition of that sublayer provides sufficient lithium, for example, for the rest of the electrochromic device stack. This result can be achieved, for example, by co-sputtering lithium with the sublayer material or when the sublayer material already includes lithium. Such approaches can have certain advantages, such as better separation of lithium from indium tin oxide (ITO) or other materials in the conductive layer, improving adhesion and preventing undesirable side reactions. In some embodiments, the ionic system is introduced into the stack in parallel with one or more of the electrochromic layer, the ion-conducting layer, and the opposing electrode layer. In one embodiment, when lithium ions are used, the lithium system is sputtered, for example, together with a material used to prepare one or more of the stacked layers, or as part of a lithium-containing material (e.g., by using a method employing lithium nickel tungsten tantalum oxide or another lithium-containing material). In one embodiment, the IC layer is deposited via sputtering a lithium aluminum silicon oxide target. In another embodiment, the Li-based system is co-sputtered with aluminum silicon to achieve the desired film. Referring again to process 722 in Figure 5, in one embodiment, depositing the electrochromic layer includes depositing WO x, for example, where x is less than 3.0 and at least about 2.7. In this embodiment, WO x has a substantially nanocrystalline morphology. In some embodiments, the electrochromic layer is deposited to a thickness between about 200 nm and 700 nm. In one embodiment, depositing the electrochromic layer includes sputtering tungsten with a self-contained tungsten target. Specific precipitation conditions for forming the WO x electrochromic layer are further discussed in U.S. Patent Application No. 12 / 645,111, which is incorporated herein by reference above. It should be understood that although the deposition of the EC layer is described as self-target sputtering, other deposition techniques are employed in some embodiments. For example, chemical vapor deposition, atomic layer deposition, and similar techniques may be used. As those skilled in the art will know, each of these techniques, as well as PVD, has its own material source form. Referring again to Figure 5 (Operation 724), once the EC layer is deposited, the IC layer, if applicable, can be deposited. Electrochromic devices operating via lithium-ion intercalation are well-suited for the requirements of architectural windows. Suitable lithium-ion conductor layer materials include lithium silicate, lithium aluminum silicate, lithium oxide, lithium tungstate, lithium aluminum borate, lithium borate, lithium zirconium silicate, lithium niobate, lithium borosilicate, lithium phosphosilyl silicate, lithium nitride, lithium oxynitride, lithium aluminum fluoride, lithium phosphooxynitride (LiPON), lithium lanthanum titanate (LLT), lithium tantalum oxide, lithium zirconium oxide, lithium silicon carbon oxynitride (LiSiCON), lithium titanium phosphate, lithium germanium vanadium oxide, lithium zinc germanium oxide, and other ceramic materials that allow lithium ions to pass through while possessing high resistance (preventing electron movement through them). Specific deposition conditions for in-situ formation of IC layers are further discussed in U.S. Patent Application No. 12 / 645,111 and U.S. Patent No. 9,261,751, each of which is incorporated herein by reference above. In some embodiments, the deposition of an ion-conducting layer includes a deposition of an ion-conducting layer with a thickness of about 10 to 100 nm. Referring again to Figure 5 (operation 726), after depositing the IC layer, if present, an anodized CE layer is deposited. In some embodiments where the IC layer is omitted, operation 726 may follow operation 722. As described above, the anodized CE layer may be deposited to include heterogeneous composition and / or morphology. In various cases, operation 726 involves depositing two or more sublayers of the anodized relative electrode material. As described above, one of these sublayers may be a flash layer. In these or other cases, the relative electrode may be deposited to include a hierarchical composition. In one embodiment, depositing the counter electrode layer includes depositing a nickel-tungsten-tantalum oxide (NiWTaO) layer or sublayer. In a particular embodiment, depositing the counter electrode layer includes sputtering a target comprising about 30% (by weight) to about 70% tungsten in nickel and / or tantalum in an oxygen-containing environment to produce a nickel-tungsten-tantalum oxide layer (the tantalum is provided by a tungsten / nickel / tantalum target of suitable composition or by another target or by another source such as an evaporation tantalum source). In another embodiment, the target is tungsten comprising between about 40% and about 60% of nickel (and / or tantalum), in another embodiment, between about 45% and about 55% of nickel (and / or tantalum), and in yet another embodiment, about 51% of nickel (and / or tantalum). In some embodiments where the anodized relative electrode layer comprises a NiWTaO layer or sublayer, a variety of deposition targets or combinations of targets can be used to deposit the NiWTaO material. For example, individual metal targets of nickel, tungsten, and tantalum can be used. In other cases, at least one of the targets comprises an alloy. For example, a nickel-tungsten alloy target can be used with a tantalum target. In another case, a nickel-tantalum alloy target can be used with a tungsten target. In yet another case, a tungsten-tantalum alloy can be used with a nickel target. In yet another case, an alloy target containing a nickel-tungsten-tantalum material can be used. Furthermore, any of the listed targets can be provided in oxide form. Sputtering often occurs in the presence of oxygen, and this oxygen is incorporated into the material. Alternatively, or in addition to an oxygen-containing sputtering atmosphere, an oxygen-containing sputtering target can be used. Sputtering targets used to form anodic-colored relative electrode materials may have compositions that allow the formation of relative electrode layers or sublayers according to any of the compositions described herein. Additionally, sputtering targets used to form anodic-colored relative electrode materials may allow materials to be formed as needed, for example, arranged in a manner as described herein to form heterogeneous relative electrode layers (e.g., having heterogeneous compositions, heterogeneous morphologies, sublayers, hierarchical compositions, etc.). In an example of forming NiWTaO material using a single sputtering target, the sputtering target may have a composition matching any of the NiWTaO materials disclosed herein. In other examples, combinations of sputtering targets are used, and the compositions of the combined targets allow deposition of any of the NiWTaO compositions (or other relative electrode materials) disclosed herein. In one embodiment, the gas composition used when forming the CE (or a sublayer therein) contains between about 30% and about 100% oxygen; in another embodiment, between about 75% and about 100% oxygen; in another embodiment, between about 95% and about 100% oxygen; and in yet another embodiment, about 100% oxygen. In one embodiment, the power density used for sputtering the CE target is between about 2 watts / cm² and about 50 watts / cm² (measured based on the applied power divided by the target surface area); in another embodiment, between about 5 watts / cm² and about 20 watts / cm²; and in yet another embodiment, between about 8 watts / cm² and about 10 watts / cm²; and in yet another embodiment, at about 8 watts / cm². In some embodiments, the power delivered for sputtering is provided via direct current (DC). In other embodiments, pulsed DC / AC reactive sputtering is used. In one embodiment, when using pulsed DC / AC reactive sputtering, the frequency is between about 20 kHz and about 400 kHz, in another embodiment between about 20 kHz and about 50 kHz, in another embodiment between about 40 kHz and about 50 kHz, and in another embodiment about 40 kHz. In one embodiment, the pressure in the deposition station or chamber is between about 1 and about 50 mTorr, in another embodiment between about 20 and about 40 mTorr, in another embodiment between about 25 and about 35 mTorr, and in another embodiment about 30 mTorr. In some cases, a nickel-tungsten oxide (NiWO) ceramic target, such as argon and oxygen sputtering, is used. In one embodiment, NiWO is between about 15% (atomic) and about 60% Ni; between about 10% and about 40% W; and between about 30% and about 75% O. In another embodiment, NiWO is between about 30% (atomic) and about 45% Ni; between about 10% and about 25% W; and between about 35% and about 50% O. In one embodiment, NiWO is about 42% (atomic) Ni, about 14% W, and about 44% O. In another embodiment, depositing the relative electrode layer includes depositing the relative electrode layer to a thickness between about 150 and 350 nm; in another embodiment, it is between about 200 and about 250 nm thick. The above conditions can be combined in any way to achieve the deposition of heterogeneous relative electrode layers. The sputtering process used to form the various portions of the CE layer can utilize one or more sputtering targets. Different sputtering targets can be used to form various CE materials. Generally, the sputtering target used to form the CE layer includes the elements to be present in the deposited CE layer (plus oxygen, whichever is provided in the target itself and / or by the sputtering gas). In some cases, all the elements of the CE layer are provided together in a single target. In other cases, all the elements of the CE layer except oxygen are provided together in a single target. In still other cases, different sputtering targets may include different materials, and the targets can be used together to form the desired CE material. The discussion of sputtering targets herein is largely in the case of forming NiWTaO materials. However, the teachings herein apply to the formation of any of the disclosed materials, provided that the provided target includes the appropriate elements in the appropriate composition. In an example of using a sputtering target to form a NiWTaO layer, the target may include nickel, tungsten, and tantalum. In some cases, the sputtering target also includes oxygen. In some cases, multiple targets may be provided, and the compositions of the targets may be the same or different from each other. In one example of forming a NiWTaO layer, at least one of the materials nickel, tungsten, and tantalum may be provided in a single target. Similarly, in the case of using a sputtering target to form a NiWO layer, the target may include nickel and tungsten, with oxygen added as appropriate. Nickel and tungsten may also be provided in a single target. Other CE materials may similarly be deposited using one or more targets that may have the same or different compositions from each other. Sputtering targets may include grids or other overlapping shapes, wherein different portions of the grid comprise different associated materials (e.g., in the case of forming a NiWTaO layer or sublayer, certain portions of the grid may comprise elemental nickel, elemental tungsten, elemental tantalum, nickel-tungsten alloys, nickel-tantalum alloys, and / or tungsten-tantalum alloys). In some cases, the sputtering target may be an alloy of associated materials (e.g., in the case of forming a NiWTaO layer or sublayer, two or more of nickel, tungsten, and tantalum may be provided in alloy form). When using two or more sputtering targets, each sputtering target may comprise at least one of the associated materials (e.g., in the case of forming a NiWTaO layer or sublayer, each target may contain at least one element and / or alloy of nickel, tungsten, and / or tantalum, any of which may be provided in oxide form). In some cases, sputtering targets may overlap. In some embodiments, sputtering targets may also be rotatable. As mentioned, the opposing electrode layer is typically an oxide material. Oxygen may be provided as part of the sputtering target and / or as the sputtering gas. In some cases, the sputtering target is a substantially pure metal, and the sputtering is carried out in the presence of oxygen to form oxides. In one embodiment, multiple targets are used to normalize the deposition rate of the CE layer, thereby eliminating the need for inappropriately high power (or other inappropriate adjustments to the desired process conditions) used to increase the deposition rate. In one embodiment, the distance between the CE target (cathode or source) and the substrate surface is between about 35 mm and about 150 mm; in another embodiment, it is between about 45 mm and about 130 mm; and in yet another embodiment, it is between about 70 mm and about 100 mm. As mentioned, one or more rotating targets may be used in some cases. In various cases, the rotating target may include an internal magnet. Figure 6A presents a view of a rotating target 900. Inside the rotating target 900 is a magnet 902, which (when appropriate power is supplied to the target) causes material to be sputtered away from the target surface 904 in a sputtering cone 906 (the sputtering cone is sometimes also called a sputtering plasma). The magnet 902 may extend along the length of the sputtering target 900. In several embodiments, the magnet 902 may extend radially outward in a directional manner such that the resulting sputtering cone 906 is ejected from the sputtering target 900 in a direction perpendicular to the target surface 904 (this direction is measured along the central axis of the sputtering cone 906, which typically corresponds to the average direction of the sputtering cone 906). The sputtering cone 906 may be V-shaped when viewed from above and may extend along the height of the target 900 (or the height of the magnet 902, if it is not the same as the height of the target 900). The magnet 902 inside the rotating target 900 can be fixed (i.e., although the surface 904 of the target 900 rotates, the magnet 902 inside the target 900 does not rotate), thus fixing the sputtering cone 906. Small circles / dots depicted in the sputtering cone 906 represent sputtered material ejected from the sputtering target 900. The rotating target can be combined with other rotating targets and / or planar targets as needed. In one example, two rotating targets are used to deposit a NiWTaO anodized CE layer (or a sublayer within an anodized CE layer): the first target comprises nickel and tungsten, while the second target comprises tantalum (either or both in oxide form, depending on the case). Figure 6B presents a top-down view of a deposition system used to deposit an anodized layer or sublayer in this manner. The nickel-tungsten target 910 and the tantalum target 912 each include an internal magnet 914. The magnets 914 are angled toward each other such that sputtering cones 916 and 918 from the nickel-tungsten target 910 and the tantalum target 912, respectively, overlap. Figure 6B also shows a substrate 920 passing in front of the targets 910 and 912. As shown, sputtering cones 916 and 918 overlap closely at their impact points on the substrate 920. In some embodiments, sputtering cones from the respective sputtering targets may overlap closely (e.g., when deposited on a substrate, the non-overlapping area reached by only a single sputtering cone is less than about 10% of the total area reached by either sputtering cone, for example, less than about 5%). In other embodiments, the sputtering cones may be more widely spaced from each other, such that any one or both of the sputtering cones have at least about 10% (e.g., at least about 20%, at least about 30%, or at least about 50%) of the total area reached by any sputtering cone. In embodiments similar to the one shown in Figure 6B, also presenting a NiWTaO CE layer (or sublayer), one sputtering target is tungsten, and the other is an alloy of nickel and tantalum (either one or both targets may be in oxide form). Similarly, one sputtering target may be nickel, and the other may be an alloy of tungsten and tantalum (either one or both targets may be in oxide form). In a related embodiment, three sputtering targets are used: a tantalum target, a nickel target, and a tungsten target (any one of which may be in oxide form). Sputtering cones from each of the three targets may overlap, where appropriate, by forming an angle with a magnet. Additionally, shielding, grids, and / or other additional plasma forming elements may be used to aid in the formation of a suitable plasma mixture to form NiWTaO. Similarly, in cases where other anodic-colored relative electrode materials may be used, including any combination of targets of elemental metals, alloys, and / or oxides, it is assumed that the target comprises the material (other than oxygen) to be incorporated into the related layer or sublayer to be formed. Various sputtering target designs, orientations, and implementation methods are further discussed in U.S. Patent No. 9,261,751, which is incorporated herein by reference above. The density and orientation / shape of the material sputtered from the sputtering target depend on a variety of factors, including, for example, the shape and strength of the magnetic field used to generate the sputtered plasma, pressure, and power density. The distance between adjacent targets and the distance between each target and the substrate also affect how the sputtered plasma mixes and how the resulting material is deposited on the substrate. In some embodiments, two different types of sputtering targets are provided to deposit a single layer or sublayer in an electrochromic stack: (a) a primary sputtering target that sputters material onto a substrate, and (b) a secondary sputtering target that sputters material onto a primary sputtering target. The primary and secondary sputtering targets may include any combination of metals, metal alloys, and metal oxides to achieve the desired composition in the deposited layer. In one particular example, in the case of NiWTaO as the electrode material, the primary sputtering target includes an alloy of nickel and tungsten, while the secondary sputtering target includes tantalum. In another example, the primary sputtering target includes tantalum, while the secondary sputtering target includes an alloy of nickel and tungsten. These sputtering targets can be used together to deposit an anodic coloring layer (or sublayer) of NiWTaO. Other combinations of alloys (e.g., nickel-tantalum, tungsten-tantalum, and other metal alloys) and metals (e.g., nickel, tungsten, and other metals) may also be used, where appropriate, to form NiWTaO or other desired materials. Any sputtering target may be provided in oxide form. Many different configurations are possible when using primary and secondary sputtering targets. Figures 7A and 7B present top-down views of one embodiment of a deposition station for depositing multi-component anodic coloring relative electrode materials. Although presented in the specific case of depositing relative electrode materials, the sputtering target configurations discussed herein can be used to deposit any material in an electrochromic stack, provided that the target has a composition suitable for the desired material in the deposition stack. A primary sputtering target 1001 and a secondary sputtering target 1002 are provided, each having an internal magnet 1003. The sputtering targets in this example are rotating sputtering targets, but planar or other shaped targets can also be used. The targets can rotate in the same direction or in opposite directions. As shown in Figure 7A, when there is no substrate 1004 between the two targets, the secondary sputtering target 1002 sputters material onto the primary sputtering target 1001. This deposits material from the secondary sputtering target 1002 onto the primary sputtering target 1001. Then, as shown in FIG7B, when the substrate 1004 is moved to the position between the two targets, sputtering from the secondary sputtering target 1002 stops and sputtering from the primary sputtering target 1001 to the substrate 1004 begins. When material is sputtered from the primary sputtering target 1001 and deposited onto the substrate 1004, the deposited material includes materials derived from the primary and secondary sputtering targets 1001 and 1002, respectively. In effect, this method involves forming a hybrid sputtering target surface in situ on the primary sputtering target 1001. One advantage of this method is that a fresh coating of material from the secondary sputtering target 1002 is periodically deposited onto the surface of the primary sputtering target 1001. The hybrid materials are then delivered together to the substrate 1004. In a particular example, in the case of forming a NiWTaO relative electrode material, the primary and secondary sputtering targets may each comprise any combination of tantalum, tungsten, nickel, and / or their alloys, in oxide form, as appropriate. In one of the related embodiments shown in FIG7C, the secondary sputtering target 1022 is positioned behind the primary sputtering target 1021, and the substrate 1024 passes in front of the primary sputtering target 1021, such that it does not obstruct the line of sight between the two targets 1021 and 1022. Each sputtering target may include a magnet 1023. In this embodiment, it is not necessary to periodically stop sputtering from the secondary sputtering target 1021 to the primary sputtering target 1022. Alternatively, such sputtering can be performed continuously. When the primary sputtering target 1021 is located between the substrate 1024 and the secondary sputtering target 1022 (e.g., when there is no line of sight between the secondary sputtering target 1022 and the substrate 1024), the primary sputtering target 1021 will rotate, allowing material deposited on the primary sputtering target 1021 to be sputtered onto the substrate 1024. More flexibility exists in the design of the secondary sputtering target 1022. In one related embodiment, the secondary sputtering target may be planar or other non-rotating targets. When using two rotating targets, the targets can rotate in the same direction or in opposite directions. In similar embodiments, the secondary sputtering target (e.g., the secondary target in Figures 7A-7C) can be replaced by another secondary material source. The secondary material source can provide material to the primary sputtering target by means other than sputtering. In one example, the secondary material source provides evaporated material to the primary sputtering target. The evaporated material can be any component of the deposited layer. In various examples, the evaporated material is an elemental metal or a metal oxide. Specific examples of evaporated materials include tantalum, tungsten, and nickel, which can be used to form NiWTaO anodized relative electrode materials. In one embodiment, elemental tantalum is evaporated onto a primary sputtering target comprising a mixture and / or alloy of nickel and tungsten. Other materials can also be provided in this manner to form layers or sublayers of other compositions. When the secondary material source provides the evaporated material, the secondary material source can be provided at any location relative to the primary sputtering target and the substrate. In some embodiments, the secondary material source is provided such that it is located behind the primary sputtering target and deposited primarily on the primary sputtering target, much like the configuration shown in Figure 7C. When using primary and secondary sputtering targets, the secondary sputtering target can operate at a cathode potential compared to the potential of the primary sputtering target (which is already cathode). Alternatively, the target can operate independently. Furthermore, regardless of the relative target potential, neutral material ejected from the secondary target will deposit on the primary target. Neutral atoms will constitute a portion of the flux and will deposit on the cathode primary target regardless of their relative potential. In several embodiments, reactive sputtering can be used to deposit one or more materials in an electrochromic stack. Figure 8 is a graph showing the sputtering deposition rate of a sputtering target as a function of oxygen concentration at a fixed power. As shown in Figure 8, there is a strong hysteresis effect related to the oxygen concentration pattern in which the target has been exposed / operated. For example, when starting from a low oxygen concentration and increasing to a higher oxygen concentration, the deposition rate remains relatively high until the oxygen concentration reaches a point where the sputtering target forms oxides that cannot be removed from the target sufficiently quickly. At this point, the deposition rate decreases, and the sputtering target essentially forms a metal oxide target. Under all other conditions being equal, the deposition rate of an oxide target is generally much lower than that of a metal target. The relatively high deposition rate regions in Figure 8 correspond to metal deposition schemes, while the relatively low deposition rate regions correspond to metal oxide deposition schemes. When the target is initially exposed to / operates at a high oxygen concentration and then exposed to / operates at a relatively low concentration, the deposition rate remains relatively low until the oxygen concentration reaches a point where the deposition rate suddenly rises to a higher level. As shown in Figure 8, the oxygen concentration at which these changes occur varies depending on whether the oxygen concentration increases or decreases. The exact oxygen concentration at which the scheme change occurs can be controlled by altering the target power density and the magnetic field strength of the internal magnet 1003. For example, if a target sputters a substantially higher flux of metal atoms from its surface (due to higher power and / or magnetic field strength) compared to a target sputtering a very low flux of metal atoms, the target is likely to remain in the metal deposition scheme. Such hysteresis effects can be used to facilitate the deposition process. In some embodiments using two or more sputtering targets to deposit material in an electrochromic stack, one target can be operated in a metal deposition scheme while the other target can be operated in a metal oxide deposition scheme. By controlling the target power density, the magnetic field strength of the internal magnet 1003, and the atmosphere in which each target is exposed / operated, it is possible to operate in both schemes simultaneously. In one example, a first nickel-tungsten target is exposed to a relatively low concentration of oxygen followed by a medium concentration, allowing it to operate in a metal deposition scheme. A second tantalum target is exposed to a relatively high concentration of oxygen followed by a medium concentration, allowing it to operate in a metal oxide deposition scheme. The two targets can then be placed together, still exposed to a medium oxygen concentration, where they are used to deposit material onto the substrate in both schemes (the first target continues to operate in the metal deposition scheme, while the second target continues to operate in the metal oxide deposition scheme). In many cases, different atmospheric exposures for each target may not be necessary. Factors other than different historical oxygen exposures can also cause targets to operate under different deposition schemes. For example, targets may have different hysteresis profiles due to different materials within them. Therefore, targets may operate under different schemes, even if they have historically been exposed to the same atmospheric oxygen conditions and are operating under those same conditions. Furthermore, the amount of power applied to each target can significantly affect the deposition scheme experienced by each target. Thus, in one instance, due to different power applied to each target, one target operates under a metal deposition scheme while another operates under a metal oxide deposition scheme. This approach can be easier because it does not require separating the targets to expose them to different oxygen concentrations. One advantage of operating targets at different points in the hysteresis profile is the ability to tightly control the composition of the deposition material. It should be understood that although the deposition sequence shown in Figure 5 is the first EC layer, the second IC layer, and the final CE layer, this sequence can be reversed in several embodiments. In other words, when the "sequential" deposition of stacked layers is described herein, it is intended to encompass the following "reverse" sequence: the first CE layer, the second IC layer, and the third EC layer, as well as the "forward" sequence described above. Both forward and reverse sequences can result in a reliable, high-quality electrochromic device. Furthermore, it should be understood that the conditions described for depositing the various EC, IC, and CE materials described herein are not limited to depositing such materials. In some cases, other materials can be deposited under the same or similar conditions. Additionally, the IC layer can be omitted in some cases. Furthermore, in some embodiments, non-sputtering deposition conditions can be used to produce deposited materials that are the same as or similar to those described herein. Since the amount of charge that the EC and CE layers can safely possess varies depending on the materials used, the relative thicknesses of the individual layers can be controlled as appropriate to match the capacity. In one embodiment, the electrochromic layer comprises tungsten oxide, and the counter electrode comprises nickel-tungsten-tantalum oxide (provided in the counter electrode layer or sublayer), and the thickness ratio of the electrochromic layer to the counter electrode layer is between about 1.7:1 and 2.3:1, or between about 1.9:1 and 2.1:1 (where about 2:1 is a specific example). As mentioned, the EC stack is manufactured in an integrated deposition system in which the substrate does not leave the integrated deposition system at any time during the stacking process. In one embodiment, the second TCO layer is also formed using an integrated deposition system in which the substrate does not leave the integrated deposition system during the deposition of the EC stack and the TCO layer. In one embodiment, all layers are deposited in an integrated deposition system in which the substrate does not leave the integrated deposition system during deposition; that is, in one embodiment, the substrate is a glass sheet, and the stack including the EC layer, and optionally the IC layer and CE layer sandwiched between the first and second TCO layers is manufactured on the glass, wherein the glass does not leave the integrated deposition system during deposition. In another embodiment of this embodiment, the substrate is glass having a diffusion barrier deposited before entering the integrated deposition system. In another embodiment, the substrate is glass, and the diffusion barrier; the stack including the EC layer, and optionally the IC layer and CE layer sandwiched between the first and second TCO layers is entirely deposited on the glass, wherein the glass does not leave the integrated deposition system during deposition. As mentioned above, lithium may be provided together with the EC, CE, and / or IC layers when the EC, CE, and / or IC layers are formed on the substrate. This may involve, for example, co-sputtering lithium with other materials of a given layer (e.g., tungsten and oxygen, with additional or different elements added where appropriate in some cases). In some embodiments, the lithium is delivered via a separate process and allows diffusion or otherwise incorporation into the EC, CE, and / or IC layers. In some embodiments, only a single layer in the electrochromic stack is lithiated. For example, in some instances, only the anodic-colored CE layer (or a sublayer therein) is lithiated. In other cases, only the cathode-colored EC layer is lithiated. In other cases, only the IC layer is lithiated. In other embodiments, two or more of the EC, IC, and CE layers (including sublayers) are lithiated. Specific conditions for lithiation are further discussed in U.S. Patent Application No. 12 / 645,111, which is incorporated herein by reference above. In some embodiments, the electrochromic stack includes a counter electrode layer or sublayer in direct physical contact with the electrochromic layer, without an ion-conducting layer in between. In some such cases, the electrochromic and / or counter electrode layer may include an oxygen-rich portion (e.g., an oxygen-rich sublayer or oxygen-rich portion of a hierarchical layer in various cases) in contact with other such layers. The oxygen-rich portion may include an electrochromic material or counter electrode material having a higher oxygen concentration than in the remainder of the electrochromic and / or counter electrode layer. Further discussion and description of electrochromic devices manufactured according to such designs are found in U.S. Patent No. 8,300,298, filed April 30, 2010, which is incorporated herein by reference. In one embodiment of the disclosed invention, a method for manufacturing an electrochromic device is provided, the method comprising: depositing an electrochromic layer comprising a cathode-colored electrochromic material; and depositing a counter electrode layer comprising: depositing a first anode-colored sublayer comprising Ni aW bA cO d, wherein a, b, and d are greater than zero; and depositing a Ni eW fB gO The second anodic sublayer h is colored, wherein e, f, and h are greater than zero, wherein at least one of c and g is greater than zero, and wherein A and B, when present, are each independently selected from the following groups: silver (Ag), aluminum (Al), arsenic (As), gold (Ag), boron (B), barium (Ba), beryllium (Be), bismuth (Bi), calcium (Ca), cadmium (Cd), cerium (Ce), cobalt (Co), chromium (Cr), copper (Cu), europium (Eu), iron (Fe), gallium (Ga), thorium (Gd), germanium (Ge), hafnium (Hf), mercury (Hg), indium (In), iridium (Ir), lanthanum (La), magnesium (Mg), manganese (Mn), molybdenum (Mo), niobium (Nb), neodymium (Nd), osmium (Os), and arsenic (Pa). Lead (Pb), palladium (Pd), ruthenium (Pr), protonium (Pm), polonium (Po), platinum (Pt), radium (Ra), rhenium (Re), rhodium (Rh), ruthenium (Ru), antimony (Sb), scandium (Sc), selenium (Se), silicon (Si), samarium (Sm), tin (Sn), strontium (Sr), tantalum (Ta), terbium (Tb), deuterium (Tc), tellurium (Te), thorium (Th), titanium (Ti), thallium (Tl), uranium (U), vanadium (V), tungsten (W), yttrium (Y), zinc (Zn), and zirconium (Zr), and lithium-ionizing one or more anode-colored sublayers of opposing electrode layers, wherein a first anode-colored sublayer is disposed between an electrochromic layer and a second anode-colored sublayer, and wherein the first and second anode-colored sublayers have different compositions. The electrochromic device can be manufactured to include any of the materials / material combinations / structures described herein. As mentioned above, in some embodiments, the fabrication of the electrochromic stack is performed in an integrated deposition system. Such integrated systems allow the deposition of individual layers in the stack without disrupting the vacuum. In other cases, one or more layers in the stack may be deposited by methods requiring removal from a protected vacuum environment. For example, in some cases, one or more layers (e.g., a cathode-colored EC layer) are deposited on a substrate using physical vapor deposition under vacuum, the substrate is then removed from the vacuum, and an ion-conducting layer is deposited using a sol-gel (or other non-vacuum) method, and then the substrate is returned to a vacuum environment for deposition of an anode-colored opposing electrode layer. The sol-gel method involves the generation of solid materials from small molecules. Monomers are converted into colloidal solutions that act as precursors for integrated networks of discrete particles or network polymers. Examples of depositable ionic conductor materials include, for example, silicate-based structures; lithium silicate, lithium aluminum silicate, lithium aluminum borate, lithium borate, lithium zirconium silicate, lithium niobate, lithium borosilicate, lithium phosphosilate, lithium nitride, lithium aluminum fluoride, and other such lithium-based ceramic materials; silica or silicon oxide, silicon dioxide, and tantalum oxide. Multi-step thermochemical condition adjustment Once the stack is deposited, the device can be subjected to a multi-step thermochemical conditioning (MTC) process. Therefore, in embodiments where a device without a separate ion-conducting layer is deposited, this conditioning process can facilitate the formation of ion-conducting regions within the device. The MTC process is further described in U.S. Patent Application No. 12 / 645,111, which is incorporated herein by reference above. In some embodiments, different process flows may be used to manufacture the electrochromic device. Alternative process flows are further discussed in U.S. Patent Application No. 14 / 362,863, filed June 4, 2014, entitled "THIN-FILM DEVICES AND FABRICATION," which is incorporated herein by reference in its entirety. Integrated sedimentation system As explained above, integrated deposition systems can be used to fabricate electrochromic devices, for example, on architectural glass. As described above, electrochromic devices are used to fabricate IGUs, which are then used to fabricate electrochromic windows. The term "integrated deposition system" refers to an apparatus used to fabricate electrochromic devices on optically transparent and translucent substrates. This apparatus has multiple stations, each dedicated to specific unit operations, such as depositing specific components (or portions of components) of the electrochromic device, and cleaning, etching, and temperature control of such devices or portions thereof. These multiple stations are fully integrated, allowing the substrate on which the electrochromic device is fabricated to be moved from one station to the next without exposure to the external environment. The integrated deposition system operates in a controlled environment within the system's process stations. A fully integrated system allows for better control over the interface quality between the deposited layers. Interface quality refers to the adhesion quality between layers and the absence of contaminants and other factors in the interface area. The term "controlled environment" refers to a sealed environment separated from the external environment, such as an open atmosphere or a cleanroom. In a controlled ambient environment, at least one of the pressure and gas composition is controlled independently of the conditions in the external environment. Generally (though not always), the controlled ambient environment has a pressure below atmospheric pressure; for example, at least a partial vacuum. The conditions in the controlled ambient environment may remain constant during the processing operation or may vary over time. For example, the layer of an electrochromic device may be deposited in a controlled ambient environment under vacuum, and when the deposition operation is complete, the environment may be backfilled with purging or reagent gas, and the pressure increased to, for example, atmospheric pressure, for processing at another station, and then the vacuum may be restored for the next operation, etc. In one embodiment, the system includes a plurality of deposition stations aligned in series and interconnected, operable to transfer a substrate from one station to the next without exposing the substrate to the external environment. The plurality of deposition stations include (i) a first deposition station containing one or more targets for depositing a cathode-colored electrochromic layer; (ii) a second (if present) deposition station containing one or more targets for depositing an ion-conducting layer; and (iii) a third deposition station containing one or more targets for depositing a counter electrode layer. In some cases, the second deposition station may be omitted. For example, the apparatus may not include any targets for depositing a separate ion-conducting layer. Additionally, any of the stacked layers can be deposited in two or more stations. For example, in the case where the opposing electrode is deposited to include two or more sublayers, the individual sublayers can be deposited in different stations. Alternatively or further, two or more sublayers within a layer can be deposited in the same station, and in some cases, different targets within the same station are used. In one example, the opposing electrode is deposited in a single station and includes sublayers with different compositions (e.g., a NiWO sublayer and one or more NiWTaO sublayers, although other combinations of materials may also be used). Targets with different compositions can be provided in different portions of the station to deposit sublayers as needed. In another example, the opposing electrode can be deposited in two stations: a first station for depositing a first sublayer (e.g., a thin flash layer) of a first opposing electrode material (e.g., NiWO or another anodic-colored opposing electrode material) and a second station for depositing one or more additional sublayers of a second (or additional) opposing electrode material (e.g., one or more sublayers of NiWTaO or another anodic-colored opposing electrode material). In another embodiment, dedicated stations are provided for depositing layers or sublayers with different compositions. For example, a first station may be provided to deposit a first sublayer having a first composition (e.g., NiWO), a second station may be provided to deposit a second sublayer having a second composition (e.g., NiWTaO comprising about 7% tantalum), and a third station may be provided to deposit a third sublayer having a third composition (e.g., NiWTaO comprising about 14% tantalum). The system also includes a controller containing programmed instructions for causing the substrate to pass through the plurality of stations in a manner that sequentially deposits the following layers onto the substrate to form a stack: (i) an electrochromic layer, (ii) (if present) an ion-conducting layer, and (iii) a counter electrode layer (as described herein). In one embodiment, the plurality of deposition stations are operable to transfer the substrate from one station to the next without breaking the vacuum. In another embodiment, the plurality of deposition stations are configured to deposit an electrochromic layer, an ion-conducting layer, and a counter electrode layer, if present, on a building glass substrate. In another embodiment, the integrated deposition system includes a substrate holder and a transport mechanism operable to hold the building glass substrate in a vertical orientation while it is in the plurality of deposition stations. In another embodiment, the integrated deposition system includes one or more load locks for transferring the substrate between an external environment and the integrated deposition system. In another embodiment, the plurality of deposition stations include at least two stations for depositing layers selected from the group consisting of: a cathode-colored electrochromic layer, an ion-conducting layer, and an anodized counter electrode layer. In some embodiments, the integrated deposition system includes one or more lithium deposition stations, each including a lithium-containing target. In one embodiment, the integrated deposition system contains two or more lithium deposition stations. In one embodiment, the integrated deposition system has one or more isolation valves for isolating individual process stations from each other during operation. In one embodiment, one or more lithium deposition stations have isolation valves. In this document, the term "isolation valve" means a means in an integrated deposition system for isolating a deposition or other process in progress at one station from processes at other stations. In one example, the isolation valve is a physical (solid) isolation valve that engages during lithium deposition within the integrated deposition system. A physical solid valve may engage to completely or partially isolate (or shield) lithium deposition from other processes or stations in the integrated deposition system. In another embodiment, the isolation valve may be a gas knife or shield, for example, delivering a partial pressure of argon or other inert gas over the area between the lithium deposition station and other stations to prevent ion flow to other stations. In another example, the isolation valve can be a evacuation zone between the lithium deposition station and other process stations, allowing lithium ions entering the evacuation zone, or ions from other stations, to be diverted to, for example, a waste stream without contaminating adjacent processes. This is achieved, for example, through differential pressure within the lithiation station of the integrated deposition system via controlled flow dynamics in the surrounding environment, thus adequately isolating lithium deposition from other processes within the integrated deposition system. Again, the isolation valve is not limited to lithium deposition stations. Figure 9A schematically illustrates an integrated deposition system 800 according to some embodiments. In this example, system 800 includes a sample loading cavity 802 for introducing a substrate into the system and an exit loading cavity 804 for removing the substrate from the system. The loading cavities allow the substrate to be introduced into and removed from the system without disturbing the controlled environment of the system. The integrated deposition system 800 has a module 806 having a plurality of deposition stations; an EC layer deposition station, an IC layer deposition station, and a CE layer deposition station. In the broadest sense, the integrated deposition system does not need to have loading cavities; for example, module 806 can function as an integrated deposition system on its own. For example, a substrate can be loaded into module 806, a controlled environment can be established, and then the substrate can be processed through the various stations within the system. Individual stations within an integrated deposition system may contain heaters, coolers, various sputtering targets and components for moving them, RF and / or DC power supplies and power delivery mechanisms, etching tools (e.g., plasma etching), gas sources, vacuum sources, glow discharge power supplies, process parameter monitors and sensors, robots, power supplies and the like. Figure 9B shows a perspective view and a more detailed cross-sectional view of a section (or simplified form) of the integrated deposition system 800, including its interior. In this example, the system 800 is modular, with a sample loading chamber 802 and a sample loading chamber 804 connected to a deposition module 806. An inlet 810 is provided for loading, for example, a building glass substrate 825 (the loading chamber 804 has a corresponding outlet). The substrate 825 is supported by a tray 820, which travels along a track 815. In this example, the tray 820 is supported by the track 815 via suspension, but the tray 820 may also be supported on top of a track located near the bottom of the device 800 or, for example, at an intermediate position between the top and bottom of the device 800. The tray 820 can be translated forward and / or backward (as indicated by the double-headed arrows) through the system 800. For example, during lithium deposition, the substrate can be moved forward and backward in front of the lithium target 830, allowing for multiple transfers to achieve the desired lithiation. The tray 820 and substrate 825 are oriented substantially vertically. This substantially vertical orientation is not restrictive, but it helps prevent defects because particulate matter, for example, generated by the aggregation of atoms from sputtering, tends to succumb to gravity and therefore does not deposit on substrate 825. Furthermore, because architectural glass substrates tend to be large, the vertical orientation of the substrate as it traverses the station of the integrated deposition system allows for the coating of thinner glass substrates, as there are fewer sagging issues in thicker hot glass. In this configuration, the target 830 (cylindrical target) is oriented substantially parallel to and in front of the substrate surface where deposition takes place (other sputtering components are not shown here for simplicity). The substrate 825 may translate through the target 830 during deposition and / or the target 830 may move in front of the substrate 825. The movement path of the target 830 is not limited to translation along the path of the substrate 825. The target 830 may rotate along an axis passing through its length, translate along the path of the substrate (forward and / or backward), translate along a path perpendicular to the substrate path, move along a circular path in a plane parallel to the substrate 825, etc. The target 830 does not need to be cylindrical; it can be planar or any shape necessary for depositing a desired layer with the desired characteristics. Furthermore, there may be more than one target in each deposition station and / or the target may move between stations depending on the required process. The integrated deposition system 800 also includes various vacuum pumps, gas inlets, pressure sensors, and the like to establish and maintain a controlled environment within the system. These components are not shown but will be understood by those skilled in the art. System 800 is controlled, for example, via a computer system or other controller represented in Figure 9B by an LCD and keyboard 835. Those skilled in the art will understand that the embodiments described herein can employ various processes involving data stored in or transferred through one or more computer systems. The embodiments also relate to equipment, such computers, and microcontrollers for performing these operations. Such equipment and processes can be used to deposit the methods described herein and electrochromic materials designed for implementing these methods. Control equipment may be specially configured for the desired purpose, or it may be a general-purpose computer selectively activated or reconfigured by computer programs and / or data structures stored in the computer. The processes presented herein are not inherently related to any particular computer or other equipment. Specifically, various general-purpose machines can be used with programs written according to the teachings in this document, or it may be more convenient to construct more specialized devices to perform and / or control the required methods and processes. As mentioned, the individual stations of an integrated deposition system can be modular, but once connected, they form a continuous system in which a controlled environment is established and maintained for substrate processing at each station within the system. Figure 9C shows an integrated deposition system 800a, which is similar to system 800, but in this example, the stations are each modular, specifically EC layer station 806a, IC layer station 806b (if applicable), and CE layer station 806c. In a similar embodiment, IC layer station 806b is omitted. Modularization is not necessary, but it is suitable because, depending on the needs, the integrated deposition system can be assembled according to conventional requirements and emerging methodological advancements. For example, lithium deposition stations (not shown) can be inserted in relevant locations to provide lithium as needed for each layer and sublayer. Figure 9D shows one embodiment of the integrated deposition system 800d. In this embodiment, the integrated deposition system 800d includes a sample loading chamber 802, two stations 850 and 851 for depositing a sublayer of a cathode-colored electrochromic material, two stations 852 and 853 for depositing a sublayer of an anodic-colored opposing electrode material, and an exit loading chamber 804. The first sublayer of the cathode-colored electrochromic material is deposited in station 850. The second sublayer of the cathode-colored electrochromic material is deposited in station 851, and in some cases may be an oxygen-rich form of the electrochromic material deposited in station 850. In this embodiment, there is no separate station for depositing an ion-conducting layer. After depositing the second sublayer of the electrochromic material, the first sublayer of the anodic-colored opposing electrode material may be deposited in station 852. As described herein, the first sublayer may be, for example, a flash layer of NiWO or another anodic-colored material. Then, the second sublayer of the anodic-colored opposing electrode material may be deposited in station 853. This layer may have any composition as described herein, and in one embodiment is NiWTaO. In various cases, the second CE layer station 853 (or any other station configured to deposit CE material) is configured to deposit a sublayer with a hierarchical composition. Figure 9E shows another embodiment of the integrated deposition system 800e. This embodiment is similar to the embodiment shown in Figure 9D, and for simplicity, only the differences will be described. In the deposition system of Figure 9E, a lithiation station 854 is included after the second opposing electrode station 853. In similar embodiments, additional lithiation stations may be provided. Additionally, lithiation stations may be located between the pairs of stations shown in Figure 9E, for example, between stations 850 and 851, between stations 851 and 852, between stations 852 and 853, between stations 853, and / or between stations 855 and 856. Additionally, a capping station 855 is included after the lithiation station 854. The capping station 855 is used to deposit a capping layer. A capping layer is defined as a layer added to the electrochromic device between the EC or CE layer and the TCO. In some embodiments, the capping layer is an anodic coloring material. For example, in some cases, the capping layer includes elements identical to the anodic coloring material in one or more sublayers of the opposing electrode layer (e.g., the capping layer may include the same elements present in the first sublayer, second sublayer, etc.). In one example, the capping layer is made of NiWO, wherein the composition of NiWO in the capping layer may be the same as or different from the composition of NiWO used elsewhere in the device (e.g., in the first sublayer of the opposing electrode layer). In another example, the capping layer may be made of NiWTaO, NiWSnO, NiWNbO, or another anodic coloring opposing electrode material, wherein the composition of the capping layer may be the same as or different from the composition of this material used in other parts of the device (e.g., in the second sublayer of the opposing electrode layer). Although the capping layer may be made of an anodized material, in several embodiments, the capping layer does not exhibit electrochromic behavior in the completed device. In some embodiments, the capping layer may have a resistivity between about 1 and 5 × 10¹⁰ ohm-cm. The integrated deposition system 800e also includes a station 856 for depositing a transparent conductive oxide (TCO) layer. In some embodiments, this layer may be indium tin oxide (ITO). The integrated deposition system, such as those shown in Figures 9A-9E, can also have a TCO layer station for depositing a TCO layer on the EC stack (not shown in 9A-9D). Depending on the method requirements, additional stations can be added to the integrated deposition system, such as stations for heating / annealing processes, cleaning processes, laser etching, rotation processes, capping layers, defect mitigation insulating layers (DMIL), MTC, etc. Although the foregoing embodiments have been described in considerable detail to facilitate understanding, the described embodiments should be considered illustrative rather than restrictive. It will be readily apparent to those skilled in the art that certain changes and modifications can be practiced within the scope of the appended claims.

[0005] 100: Electrochromic device 102:Substrate 104: Conductive Layer (CL) 106: Electrochromic layer (EC) / Cathode-colored layer / Cathode-colored electrochromic layer / Electrochromic material 108: Ion Conducting Layer (IC) 110: Relative Electrode Layer (CE) / Relative Electrode / Anodic Coloring Relative Electrode Layer / Anodic Coloring Layer 114: Conductive Layer (CL) 116: Voltage source 120: Electrochromic stacking 204: Transparent conductive oxide layer 206: Cathode-colored electrochromic layer / Electrochromic layer 210: Anodized Relative Electrode Layer / Relative Electrode Layer 210a: First sublayer 210b: Second sublayer 214: Transparent conductive oxide layer 304: Transparent conductive oxide layer 306: Cathode-colored electrochromic layer / electrochromic layer 311: Anodized Relative Electrode Layer / Relative Electrode Layer 311a: First sublayer 311b: Second Sublayer 311c: Third sublayer 314: Transparent conductive oxide layer 720: Method for forming electrochromic stacks 722: Process (deposition of EC layer) 724: Process (IC layer deposition as needed) 726: Process (Deposition of heterogeneous CE layer) 728: Process (Deposition of TCO layer) 800: Integrated sedimentation system 800a: Integrated sedimentation system 800d: Integrated sedimentation system 800e: Integrated Deposition System 802: Sample loading chamber 804: Sample loading cavity 806: Deposition Module 806a: EC level station 806b: IC layer station 806c: CE layer station 810: Imports 815: Track 820: Pallet 825:Substrate 830: Target 835: Keyboard 850: EC Level Station 1 851: EC Level Station 2 852: CE Layer Station 1 853: CE Level Station 2 854: Lithiumization Station 855: Cover Station 856: TCO Station 900: Rotating Target / Sputtering Target 902: Magnet 904: Target surface 906: Sputtering Cone 910: Nickel-Tungsten Target 912: Tantalum Target 914: Internal magnet 916: Sputtering Cone 918: Sputtering Cone 920:Substrate 1001: Level 1 Sputtering Target 1002: Secondary sputtering target 1003: Internal magnet 1004:Substrate 1021: Level 1 Sputtering Target 1022: Secondary sputtering target 1023: Magnet

Claims

1. An apparatus for manufacturing electrochromic stacks on a substrate, the apparatus comprising: A first electrochromic (EC) layer station configured to deposit a first EC sublayer of an EC layer, the first EC sublayer comprising a cathode-colored electrochromic material; a first lithiation station configured to deposit metallic lithium on the EC layer using a lithium-containing source; a second EC layer station configured to deposit a second EC sublayer of the EC layer, the second EC sublayer comprising a cathode-colored electrochromic material; a first counter electrode (CE) layer station configured to deposit a first CE sublayer of a CE layer, the first CE sublayer comprising an anode-colored electrochromic material; a second CE layer station configured to deposit a second CE sublayer of the CE layer, comprising an anode-colored electrochromic material, the second CE layer station using a higher power than the first CE layer station to deposit the second CE sublayer; and a controller configured to allow the substrate to pass through the stations in the device without breaking a vacuum, and to allow the device to sequentially deposit the electrochromic stacked layers on the substrate.

2. The device of claim 1, further comprising a second lithiation station configured to deposit metallic lithium from a self-contained lithium source onto the CE layer or the first CE sublayer.

3. The apparatus of claim 1, wherein the second CE layer station deposits a graded composition of the metal in the second CE sublayer.

4. A method for manufacturing an electrochromic stack, the method comprising: Depositing an electrochromic (EC) layer of the electrochromic stack; depositing lithium metal on the EC layer; and depositing a CE layer of the electrochromic stack using a counter electrode (CE) target, wherein depositing the CE layer includes: depositing a first CE sublayer; and depositing a second CE sublayer using a higher power than that used to deposit the first CE sublayer.

Citation Information

Patent Citations

  • Electrochromic devices

    TW201211664A