Amide compound
The use of a specific amide compound as a Lewis base in solid titanium catalyst components addresses the need for high stereoregularity and productivity in propylene polymers, achieving enhanced heat resistance and melting points, and enabling their use in diverse applications.
Patent Information
- Application Number
- PCT/JP2024/013474
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-03-30
- Filing Date
- 2024-04-01
- Publication Date
- 2024-10-03
AI Technical Summary
There is a need for propylene polymers with extremely high stereoregularity and high productivity for use as solid titanium catalyst components in olefin polymerization, which can achieve high melting points and heat resistance while being environmentally friendly and resource-efficient.
An amide compound with a specific structure is used as a Lewis base in the solid titanium catalyst component, enhancing the stereoregularity and productivity of propylene polymers, allowing for high heat resistance and heat of fusion, and can be used as an internal donor in Ziegler-Natta catalysts.
The amide compound achieves high stereoregularity and productivity in propylene polymers, resulting in polymers with improved heat resistance and melting points, and can be used in various applications including as a solvent, drug intermediate, and nylon raw material.
Smart Images

Figure JP2024013474_03102024_PF_FP_ABST
Abstract
Description
Amide compounds
[0001] The present invention relates to novel amide compounds.
[0002] Amide compounds are known to be used as solvents, intermediates for pharmaceuticals, pesticides, and other chemicals, as well as raw materials for nylon, etc. There have also been reports of their use in Mg compound-supported titanium catalysts used in olefin polymerization.
[0003] Olefin polymerization catalysts are one of the technologies that have made great advances since the discovery of the so-called Ziegler-Natta catalyst in 1953, when Ziegler reported that ethylene could be polymerized even at low pressure by combining titanium tetrachloride and an organoaluminum compound. Subsequently, Natta reported the first propylene polymerization using a combination of titanium trichloride and a halogen-containing organoaluminum compound. Among these catalysts, it was discovered that a third-generation catalyst containing titanium tetrachloride, a magnesium compound, and a Lewis base could achieve both high polymerization activity (high productivity) and high stereoregularity in propylene polymerization. This was one of the opportunities for the worldwide spread of propylene polymers (polypropylene).
[0004] Furthermore, it has been discovered that Lewis bases (hereinafter also referred to as "internal donors"), which are one of the main components of the above-mentioned third-generation catalyst components (hereinafter also referred to as "solid titanium catalyst components"), have a significant effect on the catalytic performance, and various Lewis bases have been developed to date.
[0005] Lewis bases reported for use in Ziegler-Natta catalysts include, for example, ethyl benzoate, phthalate esters, 1,3-diketones (Patent Document 1), malonate esters (Patent Document 2), succinate esters (Patent Document 3), 2,4-pentanediol diesters (Patent Document 4), naphthalenediol diesters (Patent Document 5), and catechol diesters (Patent Document 6), and this is still an area where research and development is being actively conducted, primarily by companies. There are also reports that diamide compounds with specific structures are suitable (Patent Documents 7 and 8).
[0006] Japanese Patent Publication No. 2005-226076, Special Publication No. 2000-516987, Special Publication No. 2002-542347, Special Publication No. 2005-517746, Special Publication No. 2011-529888, Special Publication No. 2014-500390, Chinese Patent Publication No. 108570120, Chinese Patent Publication No. 108570119
[0007] Propylene polymers have heat resistance and rigidity similar to those of general-purpose engineering plastics, but because they are composed almost entirely of carbon and hydrogen, they have the advantage of producing less toxic gases when burned.
[0008] Due to recent advances in molding technology, the use of propylene polymers with higher stereoregularity than conventional polymers may enable the development of higher physical properties (such as rigidity and heat resistance). Therefore, there is a demand in the market for propylene polymers with higher stereoregularity. Furthermore, from the viewpoints of resource conservation and environmental protection, there is a demand for a highly productive method for producing propylene polymers.
[0009] Therefore, an object of the present invention is to provide an internal donor component suitable for a solid titanium catalyst component, which, when used in a solid titanium catalyst component, can produce a propylene polymer with extremely high stereoregularity (which can be expected to have a high melting point and a high heat of fusion) with high productivity (high activity).
[0010] As a result of extensive research aimed at solving the above problems, the present inventors have found that an amide compound having a specific structure is suitable as, for example, a Lewis base for a solid titanium catalyst component, and have thus completed the present invention. Examples of the present invention are shown below.
[0011] [1] An amide compound having a structure represented by the following formula (1):
[0012] [In formula (1), C, C 1 and C 2 is a carbon atom, N is a nitrogen atom, R 1 and R 2 are each a hydrocarbon group, and R 11 and R 12 are each a hydrogen atom or a hydrocarbon group, at least one of which is a hydrocarbon group; R 3~R 6 are each a hydrogen atom or a hydrocarbon group, R is a hydrogen atom, and m is an integer of 1 to 5.
[0013] [2] The R 11 and R 12 [3] The amide compound according to item [1], wherein both of R 1 , R 2 , R 4 , R 5 is a hydrocarbon group consisting of carbon and hydrogen.
[0014] The amide compound of the present invention can be used, for example, as a solvent, a pharmaceutical intermediate, a raw material for nylon, a chelating agent, and a raw material for Ziegler-Natta catalysts.
[0015] The amide compound according to the present invention will be described in more detail below. [Amide Compound] The amide compound according to the present invention (hereinafter also referred to as "amide compound (A)") is represented by the following general formula (1).
[0016] In the above formula (1), C, C 1 and C 2 is a carbon atom, and N is a nitrogen atom. A line such as "-" indicates a covalent bond.
[0017] The R 1 and R 2 are each a hydrocarbon group. More specifically, they are each a substituted or unsubstituted hydrocarbon group having 1 to 20 carbon atoms. Examples of the hydrocarbon group include aliphatic hydrocarbon groups, alicyclic hydrocarbon groups, and substituted or unsubstituted hydrocarbon groups having 6 to 20 carbon atoms and an aryl group. Such a substituent may have a structure containing a heteroatom as described below. Examples of heteroatom-containing aryl groups include those having a basic skeleton in which the aryl structure itself contains a heteroatom, such as a pyrrole ring or a pyran ring, and those in which a substituent such as a heteroatom-containing hydrocarbon group, such as an alkoxy group, is bonded to a benzene ring.
[0018] The R 11 and R12 are hydrogen atoms or hydrocarbon groups, and at least one of them is a hydrocarbon group. Specific examples of the hydrocarbon group include the R 1 , R 2 The same substituents as those exemplified in the above R 11 , R 12 Preferably, both of are hydrocarbon groups.
[0019] The H in the amide compound having the above-mentioned "N-H" structure is so-called active hydrogen, which is expected to have high reactivity with titanium and the like in the solid titanium catalyst component for olefin polymerization, and therefore is thought to be highly unsuitable as an electron donor component. However, the amide compound of the present invention may exhibit unexpected properties that make it suitable as the electron donor component.
[0020] The R 1 ~R 12 Among them, R 1 , R 2 is preferably a substituted or unsubstituted hydrocarbon group having 6 to 20 carbon atoms and an aryl group.
[0021] The structure containing a hetero atom is typically a structure having a substituent containing a hetero atom, and a preferred example of such a substituent is a heteroatom-containing aryl group, and a particularly preferred example is an aryl group containing oxygen. 1 , R 2 is preferably a structure in which one of the carbon atoms contained therein is covalently bonded to the adjacent carbonyl carbon.
[0022] The R 3 , R 4 , R 5 , R 6 are each a hydrogen atom or a hydrocarbon group. As described above, the hydrocarbon group is a group that includes an embodiment containing a heteroatom. The heteroatom is preferably a group containing an element selected from the elements of Groups 15, 16, and 17 of the periodic table. 3 , R 4 , R 5 , R 6More specifically, examples of the alkyl group include a group selected from a hydrogen atom, a substituted or unsubstituted hydrocarbon group having 1 to 20 carbon atoms, and a halogen atom.
[0023] The hydrocarbon group will be described in more detail. The hydrocarbon group of the present invention is a substituent essentially containing carbon and hydrogen atoms, and may be partially substituted with atoms selected from the group consisting of elements in Groups 15 to 17 of the periodic table, such as nitrogen atoms, oxygen atoms, phosphorus atoms, and halogen atoms. The heteroatoms may be substituted at one or more positions.
[0024] In the present invention, the expression "atom" such as a halogen atom or a hydrogen atom in the description of a substituent may naturally refer to an embodiment having a bond, such as "H-" or "Cl-", as represented by a structural formula.
[0025] The R is a hydrogen atom. However, in the present invention, "-(CR2)" in formula (1) m Preferably, the R bonded to adjacent carbon atoms of "-(CR)" is bonded to each other to form a double bond. m The "-" structure is a methylene chain structure.
[0026] The above R 1 , R 2 , R 3 , R 4 , R 5 , R 6 , R 11 , R 12 can bond to each other to form a ring structure. Preferred embodiments of these will be described below.
[0027] The R 1 and R 2 can bond to each other to form a ring structure. 1 , R 3 , R 4 , R 11 The substituents selected from can be bonded to each other to form a ring structure. 2 , R 5 , R 6 , R 12 The substituents selected from can be bonded to each other to form a ring structure.
[0028] The R 3 and R 4 and a substituent selected from the group consisting of R 5 and R 6 The substituents selected from the above may be bonded to each other to form a ring structure.
[0029] The R 3 ~R 6 The ring structure formed by bonding the substituents selected from the group consisting of C 1 Carbon or C 2 In consideration of the mobility around the carbon, the alicyclic structure is preferably a 5-membered or larger ring, more preferably a 6-membered or larger ring. On the other hand, the upper limit of the number of members in the ring structure is arbitrary, but is preferably a 10-membered ring, more preferably an 8-membered ring.
[0030] In addition, the above-mentioned R 3 and R 4 Ya, R 5 and R 6 When R forms a ring structure, it also includes an embodiment in which a carbon-carbon double bond is formed (in this case, the carbon-carbon double bond is considered to be a two-membered ring). 3 ~R 6 When the groups bond to form a ring structure, the ring structure is preferably an alicyclic structure. The reason why such a structure is suitable for the present invention will be described later.
[0031] The above R 3 ~R 6 is preferably a relatively low bulky substituent. In the case of a solid titanium catalyst component containing an organic compound (generally referred to as an internal donor), bulky compounds tend to be preferred in many cases. The reason why such low bulky substituents tend to be preferred in the present invention is unclear at present, but as will be described later, it is likely that the amide compound of the present invention tends to stably adopt a relatively preferred conformation as a component of an olefin polymerization catalyst, for example, and therefore, the substituent R on the opposite side of the amide group is preferred. 3 ~R 6It is believed that this is because, when R has a small bulky structure, it is difficult for the coordination of the olefin to the titanium of the solid titanium catalyst component to be disturbed. 3 , R 6 is a hydrogen atom.
[0032] The R 11 and R 12 is a hydrocarbon group, and it may be preferable that these substituents are bonded to each other to form a ring structure. Such a structure can be represented by "-(CR 2 ) m While the structure of the "-" portion exhibits a relatively flexible structure, it has the effect of suppressing the rotation of the amide group and making it easier to adopt a "slightly stable" conformation, such as a conformation that exhibits a relatively large twist-like movement. Therefore, it is thought that in the solid titanium catalyst component, it has a moderate interaction with titanium and is likely to form an active site with high stereoregularity.
[0033] In the amide compound of the present invention, m is an integer of 1 to 5. A preferred lower limit is 2, although it depends on the structure of A. On the other hand, a preferred upper limit is 4. Within this range, the distance between at least two amide groups falls within an appropriate range, and the olefin polymerization performance preferred in the present invention can be expected to be exhibited.
[0034] The above R 1 ~R 12The hydrocarbon group contained in is a monovalent hydrocarbon group having 1 to 20 carbon atoms, preferably 1 to 10, more preferably 2 to 8, even more preferably 3 to 8, still more preferably 4 to 8, and particularly preferably 4 to 6 carbon atoms. Examples of such hydrocarbon groups include aliphatic hydrocarbon groups, alicyclic hydrocarbon groups, and aromatic hydrocarbon groups, such as substituted or unsubstituted aryl groups and substituted or unsubstituted cycloalkenyl groups, such as methyl, ethyl, n-propyl, isopropyl, n-butyl, isobutyl, hexyl, heptyl, octyl, 2-ethylhexyl, decyl, dodecyl, tetradecyl, hexadecyl, octadecyl, eicosyl, cyclohexyl, and phenyl groups. The alicyclic hydrocarbon groups and aromatic hydrocarbon groups may contain a substituent. Among these, n-butyl, isobutyl, hexyl, octyl, and phenyl groups are preferred, with n-butyl, isobutyl, and phenyl being more preferred.
[0035] Furthermore, in the case of a hydrocarbon group containing an element of Groups 15 to 17 of the periodic table, such as nitrogen, oxygen, phosphorus, or a halogen, specific preferred examples include a carboxylic acid ester group, an aldehyde group, an acetyl group, a carbonyl structure-containing group such as an oxycarbonylalkyl group, an alkoxy group, a substituted or unsubstituted alkoxy group, a substituted or unsubstituted alkenyloxy group, a substituted or unsubstituted cycloalkyloxy group, a substituted or unsubstituted cycloalkenyloxy group, a substituted or unsubstituted aryloxy group, a substituted or unsubstituted heteroaryl group, a substituted or unsubstituted heteroaryloxy group, and a siloxy group. The heteroatom is preferably nitrogen or oxygen, more preferably oxygen.
[0036] Among the heteroatom-containing substituents, preferred are aryl groups containing oxygen-containing substituents. Specifically, preferred examples include structures in which an oxygen-containing substituent, such as an alkoxy group, an aryloxy group, an alkoxyalkyl group, or an aryloxyalkyl group, or a substituent in which the oxygen of the substituent is substituted with a carbonyl group or a carboxyl group, is bonded to an aromatic skeleton. Among the above, preferred are substituents in which an alkoxy group or an aryloxy group is bonded to an aromatic skeleton, and more preferred are substituents in which an alkoxy group is bonded to an aromatic skeleton. The number of carbon atoms in the oxygen-containing substituent is preferably 1 to 10, more preferably 1 to 8, and even more preferably 1 to 6. More specifically, preferred examples include the methoxyphenyl group, as well as an ethoxyphenyl group, a propyloxyphenyl group, an isopropyloxyphenyl group, a butoxyphenyl group, and a phenoxyphenyl group.
[0037] In the present invention, R 1 , R 2 , R 4 , R 5 is preferably a hydrocarbon group, more preferably a hydrocarbon group consisting of carbon and hydrogen. In the present invention, the hydrocarbon group consisting of carbon and hydrogen refers to a hydrocarbon group consisting of only carbon and hydrogen, which does not substantially contain heteroatoms. Among such hydrocarbon groups, the R 1 , R 2 is preferably a substituent selected from an alkyl group and an aromatic hydrocarbon group. 4 , R 5 is preferably an aliphatic hydrocarbon group, more preferably an alkyl group. 1 , R 2 , R 3 , R 4 , R 5 , R 6 , R 11 , R 12 are preferably independent (substituent) groups that do not bond to each other.
[0038] The R 11 and R 12When one of the substituents is a hydrogen atom, the other substituent is preferably a hydrocarbon group containing an aromatic structure. More specifically, examples of such substituents include an aliphatic hydrocarbon group or a substituent in which one hydrogen atom of an alicyclic hydrocarbon group is substituted with an aryl group, and an aromatic hydrocarbon group. Examples of such substituents include a benzyl group, a 2-phenylethyl group, a 3-phenylpropyl group, a 2-phenylpropyl group, and a 4-phenylbutyl group, in which an aliphatic hydrocarbon group is partially substituted with an aryl group such as a phenyl group. Other examples include hydrocarbon groups containing an aromatic structure and an alicyclic structure, such as a (phenylcyclohexyl)methyl group, a 2-(phenylcyclohexyl)ethyl group, and a 3-(phenylcyclohexyl)propyl group. Examples of aromatic hydrocarbon groups include a phenyl group, a naphthalyl group, an indenyl group, a fluorenyl group, and the like, as well as substituents in which a portion of the aromatic structure is hydrogenated.
[0039] Examples of such amide compounds include the following structures: The structural formulas of the exemplary compounds below may have stereoisomers, and although some of the isomeric structures are specified, they may also include isomeric structures not shown as examples.
[0040]
[0041]
[0042]
[0043]
[0044]
[0045]
[0046]
[0047] In addition to the above, compounds having an "N--H" type amide structure disclosed in the examples below can also be exemplified.
[0048] In the above structural formulas, a methyl group is represented as "Me", an ethyl group as "Et", a propyl group as "Pr", a butyl group as "Bu", a phenyl group as "Ph", a cyclohexyl group as "Cy", and a benzyl group as "Bn". "n" represents "normal", "i" represents "iso", and "t" represents "tertiary". In the structural formulas, carbon atoms are present at the vertices and ends, and "-" represents a covalent bond. Such compound structural formula formats are well known to those skilled in the art.
[0049] Such compounds can be used in a variety of applications, but are particularly suitable as internal donors for solid titanium catalyst components used in olefin polymerization catalysts. When used as the internal donor, these compounds may be used alone or in combination of two or more. Furthermore, as long as the object of the present invention is not impaired, these amide compounds can also be used in combination with other known internal donor components such as known diamide compounds or ester compounds. Furthermore, the amide compounds can also be formed during the process of preparing the solid titanium catalyst component.
[0050] When an α-olefin such as propylene is polymerized in the presence of an olefin polymerization catalyst using the above-mentioned solid titanium catalyst component, a polymer having a wide molecular weight distribution and a high melting point and heat of fusion tends to be obtained with high activity. The reason for this is unclear at present, but the present inventors, taking into account the above-mentioned facts, have speculated that the amide moiety of the amide compound of the present invention tends to be relatively easily coordinated with titanium and magnesium of the solid titanium catalyst component, while the C bonded to the nitrogen of the amide group in the structural formula (1) in particular tends to be easily coordinated with titanium and magnesium of the solid titanium catalyst component. 1 carbon, C 2 In terms of rigidity around the carbon, the amide compound of the present invention is considered to have a loose structure, and therefore assumes a conformation with limited range of motion, which is thought to facilitate the production of olefin polymers with high stereoregularity and a wide molecular weight distribution (wider toward the high molecular weight side).In this case, since the stereoregularity of the polymer, particularly on the high molecular weight side, is high, it is likely to crystallize relatively easily for its molecular weight, and the nucleating agent effect is also exhibited, which is thought to facilitate the production of polymers with high melting points and heats of fusion.
[0051] The olefin polymers obtained by the process of the present invention are polymers obtained using a catalyst capable of adopting a wide range of conformations to some extent, and therefore can be polymers with a wide range of molecular weights even on the low molecular weight side. Therefore, there may be a large amount of components soluble in hydrocarbon solvents such as decane. Although such soluble components are usually feared to weaken the crystalline structure of the olefin polymer, the heat of fusion of the olefin polymers of the present invention tends to be high. This is probably because the nucleating effect of the high molecular weight components takes precedence.
[0052] <Method for Producing Amide Compound> The method for producing an amide compound is not particularly limited, and for example, the "Synthesis Example" in the Examples described below can be used. Alternatively, an amide compound may be synthesized using a known reaction. An amide compound may be synthesized by synthesizing each moiety using a known synthesis method and then bonding them using a known method. More specifically, the amide compound can be produced using the following reaction.
[0053] The diamide compound shown in the following reaction formula (2) can be synthesized, for example, by reacting an N,N'-dialkyldiamine compound with an acid chloride in the presence of a base. The diamine compound used may be the corresponding hydrochloride. The base used is not particularly limited, but examples thereof include sodium hydroxide, potassium hydroxide, pyridine, N,N-dimethyl-4-aminopyridine (DMAP), and triethylamine.
[0054]
[0055] Furthermore, the diamide compound described in the above reaction formula (2) can also be prepared by a method of reacting an N,N'-dialkyldiamine compound with a carboxylic acid in the presence of an acid catalyst, or by a method using a condensing agent such as N,N'-dicyclohexylcarbodiimide (DCC), as shown in the following reaction formula (3).
[0056]
[0057] Furthermore, the diamide compound represented by the above reaction formula (3) can also be synthesized by reacting the corresponding diamide compound with a base, followed by reaction with an alkyl halide, as shown in the following reaction formula (4): The base to be used is not particularly limited, but examples thereof include an organolithium reagent, sodium hydride, and potassium hydride.
[0058]
[0059] As described above, the amide compound of the present invention can be used in a variety of applications. In particular, as described above, it is suitable as an internal donor component of a solid titanium catalyst component contained in an olefin polymerization catalyst. In addition, it is expected to be used as a special solvent, an intermediate for pharmaceuticals and agricultural chemicals, and a raw material for special polyamides.
[0060] (Method of analyzing compounds) 1 H-NMR spectrum (400 MHz, JEOL Ltd., JNM-ECZ400S / L1 type measuring apparatus) was measured, and peaks were assigned in the usual manner to determine the structure.
[0061] Example 1 Synthesis of Compound 1 Compound 1 shown below was synthesized by the method described below.
[0062]
[0063] In a thoroughly heated and dried 100 mL three-neck flask equipped with a stirrer, 5.05 grams of N,N'-dimethyl-2,4-pentanediamine (38.8 mmol, 1 equivalent) and 39 mL of anhydrous pyridine were added under a nitrogen atmosphere. The reaction solution was cooled in an ice bath, and then 11.7 grams of benzoyl chloride (83.0 mmol, 2.1 equivalents) was slowly added dropwise. After the dropwise addition was complete, the temperature was slowly raised to room temperature, and stirring was continued for 22 hours. After the reaction was complete, the reaction solution was again cooled in an ice bath, and 5 mL of methanol was added. Water and ethyl acetate were added to the resulting reaction solution, and the mixture was extracted three times with ethyl acetate. The collected organic layer was washed once with water and once with saturated brine, dried over magnesium sulfate, and then concentrated using a rotary evaporator. The obtained crude product was purified by NH gel column chromatography (hexane:ethyl acetate = gradient from 90:10 to 40:60), and as a result, 11.7 g (35.1 mmol, yield 90%) of Compound 1 was obtained. 1 The H-NMR data is shown below.
[0064] 1 H NMR (400 MHz, CDCl, TMS as internal standard): δ 0.94–1.32 (m, 6 H), 1.57–1.90 (overlapping with water signals, m, 2 H), 2.37–3.00 (m, 6 H), 3.63–4.96 (m, 2 H), 6.87–7.46 (overlapping with CHCl signals, m, 10 H).
[0065] <Preparation of solid titanium catalyst component [α1]> After thoroughly replacing the atmosphere in a 1 L glass vessel with nitrogen, 85.8 g of anhydrous magnesium chloride, 321 g of decane, and 352 g of 2-ethylhexyl alcohol were added and reacted by heating at 130°C for 3 hours to obtain a homogeneous solution. 241 g of this solution and 6.43 g of ethyl benzoate were added to the glass vessel, and the mixture was stirred and mixed at 50°C for 1 hour.
[0066] The homogeneous solution thus obtained was cooled to room temperature, and 38.3 ml of this homogeneous solution was added dropwise over 45 minutes with stirring to 100 ml of titanium tetrachloride maintained at -20°C. After the addition was complete, the temperature of this mixture was raised to 80°C over 3.8 hours. When the temperature reached 80°C, 1.71 g of Compound 1 was added to the mixture. The temperature was again raised to 120°C over 40 minutes and maintained at the same temperature for 35 minutes with stirring. After the reaction was completed, the solid was collected by hot filtration, resuspended in 100 ml of titanium tetrachloride, and then heated to 120°C for 35 minutes with stirring. After the reaction was completed, the solid was again collected by hot filtration and thoroughly washed with decane at 100°C and room temperature until no free titanium compound was detected in the washings. The solid titanium catalyst component [α1] prepared by the above procedure was stored as a decane slurry, and a portion of this was dried for the purpose of examining the catalyst composition. The solid titanium catalyst component [α1] thus obtained had a composition of 0.66% by mass of titanium, 1.3% by mass of magnesium, and 0.05% by mass of 2-ethylhexyl alcohol residue.
[0067] <Main Polymerization> 500 g of propylene and 1 NL of hydrogen were added to a 2-liter polymerization vessel at room temperature, followed by a mixture of 7 ml of heptane, 0.50 mmol of triethylaluminum, 0.10 mmol of cyclohexylmethyldimethoxysilane, and 0.0040 mmol (titanium atom equivalent) of the solid titanium catalyst component [α1] mixed for 10 minutes at 25°C. The mixture was then added, and the temperature inside the polymerization vessel was quickly raised to 70°C while stirring. After polymerization at 70°C for 1.5 hours, the reaction was terminated with a small amount of methanol, and the propylene was purged. The resulting polymer particles were then dried under reduced pressure at 80°C overnight. The various results are as follows.
[0068] Activity: 13.4 kg-PP / g-catalyst Bulk density: 380 kg / m 3 MFR: 10.1 g / 10 min Decane insoluble content: 9.0 mass % Tm: 163.0°C, 157.6°C Tc: 112.6°C Tmf: 169.0°C ΔH: 89.7 J / g Mw / Mn: 9.1 Mz / Mw: 8.8
[0069] The various analytical methods are as follows: (1) Bulk specific gravity: Measured in accordance with JIS K-6721. (2) Melt flow rate (MFR): Measured in accordance with ASTM D1238E, with a load of 2.16 kg and a temperature of 230° C. for propylene polymers.
[0070] (3) Amount of decane-soluble (insoluble) components: About 3 g (10 -4 The weight was measured to the nearest gram. This weight was represented as b (grams) in the formula below. ), 500 ml of decane, and a small amount of a heat stabilizer soluble in decane were added, and the mixture was heated to 150°C over 2 hours while stirring with a stirrer under a nitrogen atmosphere to dissolve the propylene polymer. After maintaining the temperature at 150°C for 2 hours, the mixture was slowly cooled to 23°C over 8 hours. The resulting liquid containing a precipitate of the propylene polymer was filtered under reduced pressure using a 25G-4 standard glass filter manufactured by Tokyo Glass Instruments Co., Ltd. 100 ml of the filtrate was collected and dried under reduced pressure to obtain a portion of the decane-soluble component, and the weight of this was reduced to 10 -4 The weight was measured to the nearest gram (this weight is represented as a (gram) in the formula below). After this operation, the amount of decane-soluble components was determined using the following formula: Content of decane-soluble components = 100 × (500 × a) / (100 × b) Content of decane-insoluble components = 100 - 100 × (500 × a) / (100 × b)
[0071] (4) Molecular Weight Distribution (MWD): Gel Permeation Chromatograph: HLC-8321 GPC / HT Model, manufactured by Tosoh Corporation. Detector: Differential Refractometer. Column: Two TSKgel GMH6-HT columns and two TSKgel GMH6-HTL columns, manufactured by Tosoh Corporation, were connected in series. Mobile Phase: o-Dichlorobenzene. Flow Rate: 1.0 mL / min. Measurement Temperature: 140°C. Calibration Curve Preparation Method: A standard polystyrene sample was used. Measurements were performed under the following conditions: sample concentration: 0.1% (w / w) and sample solution volume: 0.4 mL. The resulting chromatograms were analyzed using known methods to calculate the weight-average molecular weight (Mw), number-average molecular weight (Mn), Z-average molecular weight (Mz), and the Mw / Mn and Mz / Mw values, which are indicators of molecular weight distribution (MWD). The measurement time per sample was 60 minutes.
[0072] (5) Melting Point (Tm) of Polymer: The melting point (Tm), crystallization temperature (Tc), and heat of fusion (ΔH) of the polymer in the present invention were measured by differential scanning calorimetry (DSC) using a PerkinElmer DSC8000 device. 3 to 10 mg of sample was sealed in an aluminum pan and heated from room temperature to 200°C at 100°C / min. The sample was held at 200°C for 5 minutes and then cooled to 30°C at 10°C / min. The peak temperature observed in this cooling test was taken as the crystallization temperature (Tc), and the calorific value determined by the area of the peak was taken as ΔH. After being left at 30°C for 5 minutes, the sample was heated a second time to 200°C at 10°C / min. The peak temperature observed in this second heating test was taken as the melting point (Tm).
[0073] The final melting point (Tmf) of the polymer in the present invention was measured by differential scanning calorimetry (DSC) using a PerkinElmer DSC8000 instrument. 3 to 10 mg of sample was sealed in an aluminum pan and heated from room temperature to 240°C at 80°C / min. The sample was held at 240°C for 1 minute and then cooled to 0°C at 80°C / min. After holding at 0°C for 1 minute, the sample was heated to 150°C at 80°C / min and held for 5 minutes. Finally, the sample was heated to 180°C at 1.35°C / min, and the intersection of the tangent to the inflection point on the high-temperature side of the peak obtained in this final heating test and the baseline was taken as the final melting point (Tmf).
[0074] Tmf can be considered as one parameter for evaluating the crystal structure of a component that exhibits very high stereoregularity, or the ease of crystallization and crystal structure of a polymer in the ultra-high molecular weight range that is thought to be difficult to crystallize. More specifically, it can be considered that the higher the Tmf value, the more likely the ultra-high molecular weight polymer component is to form crystals with high heat resistance.
[0075] Example 2 Synthesis of Compound 2 Compound 2 shown below was synthesized by the method described below.
[0076]
[0077] In the above synthesis of compound 1, 4.90 g (18.1 mmol, yield 79%) of compound 2 was obtained in accordance with the same procedures and equivalent relationships as in the synthesis of compound 1, except that butyryl chloride was used instead of benzoyl chloride. 1 The H-NMR data is shown below.
[0078] 1 H NMR (400 MHz, CDCl, TMS as internal standard): 0.91–1.00 (m, 6 H), 1.04–1.28 (m, 6 H), 1.38–1.83 (overlapped with H2O signals, m, 6 H), 2.05–2.35 (m, 4 H), 2.75–2.84 (m, 6 H), 3.66–4.85 (m, 2 H).
[0079] <Preparation of solid titanium catalyst component [α2]> A solid titanium catalyst component [α2] was obtained in the same manner as in Example 1, except that 1.37 g of compound 2 was used instead of 1.77 g of compound 1. The composition of the solid titanium catalyst component [α2] thus obtained was 0.64 mass % titanium, 1.4 mass % magnesium, and 0.07 mass % of 2-ethylhexyl alcohol residue.
[0080] <Main Polymerization> Propylene polymerization was carried out in the same manner as in Example 1, except that the solid titanium catalyst component [α2] was used instead of the solid titanium catalyst component [α1]. Various results were as follows.
[0081] Activity: 14.6 kg-PP / g-catalyst Bulk density: 470 kg / m 3 MFR: 13.0 g / 10 min Decane insoluble content: 8.0 mass % Tm: 158.7°C Tc: 114.4°C Tmf: 169.2°C ΔH: 90.3 J / g Mw / Mn: 8.8 Mz / Mw: 8.3
[0082] Example 3 Synthesis of Compound 3 Compound 3 shown below was synthesized by the method described below.
[0083] A 100 mL three-neck flask containing a heat-dried stirrer was prepared and the inside atmosphere was replaced with nitrogen. Under a nitrogen atmosphere, 0.99 g of N-benzyl-1,3-propanediamine (12.1 mmol, 1 equivalent) and 24 mL of pyridine (anhydrous) were added, and the reaction solution was cooled in an ice bath. After confirming that the reaction solution was sufficiently cooled, 3.56 g of benzoyl chloride (25.3 mmol, 2.1 equivalents) was slowly added dropwise. After the addition was complete, the temperature was slowly raised to room temperature and stirring was continued for 20 hours. After tracking the reaction by GC-MS analysis, the mixture was again cooled in an ice bath and quenched by adding 2 mL of methanol. Ethyl acetate and water were added to the quenched reaction solution, and the mixture was extracted three times with ethyl acetate. The collected organic layer was washed sequentially with water, saturated aqueous sodium bicarbonate, and saturated brine. The resulting organic layer was dried over magnesium sulfate and then concentrated using a rotary evaporator. The obtained crude product was purified by NH gel column chromatography (hexane:ethyl acetate = 100:0 to 60:40 gradient), and 4.34 g (11.7 mmol, yield 97%) of TKN-040 was obtained. The product was highly viscous, and a small amount of ethyl acetate remained. 1 The H-NMR data is shown below.
[0084] 1 H-NMR (500 MHz, CDCl, TMS as internal standard): δ 1.80-1.85 (m, 2 H), 3.51-3.55 (m, 2 H), 3.65-3.68 (m, 2 H), 4.54 (s, 2 H), 7.17-7.19 (m, 2 H), 7.29-7.49 (m, 10 H), 7.87 (br s, 1 H), 7.94-7.96 (m, 2 H).
Claims
1. An amide compound having the structure of the following formula (1): [In formula (1), C, C 1 and C 2 is a carbon atom, N is a nitrogen atom, R 1 and R 2 are each a hydrocarbon group, R 11 and R 12 are each a hydrogen atom or a hydrocarbon group, at least one of which is a hydrocarbon group; R 3 ~R 6 are each a hydrogen atom or a hydrocarbon group, R is a hydrogen atom, and m is an integer of 1 to 5.
2. R 11 and R 12 The amide compound according to claim 1, wherein both of are hydrocarbon groups.
3. The above R 1 , R 2 , R 4 , R 5 The amide compound according to claim 1 , wherein is a hydrocarbon group consisting of carbon and hydrogen.
Citation Information
Patent Citations
Components and catalysts for the polymerization of olefins
JP2000516987A
Components and catalysts for olefin polymerization
JP2002542347A
Catalyst component and catalyst for olefin polymerization
JP2005226076A
Solid catalyst component for olefin polymerization, catalyst comprising same, and use thereof
JP2005517746A
Internal donor for olefin polymerization catalyst
JP2011529888A