Battery cell, battery and electric device
By setting weak areas on the electrode terminals to destroy at pressure or temperature thresholds, excess gas inside the battery cell is discharged, which solves the problem of the risk of battery cell explosion and improves the stability and assembly efficiency of the battery cell.
Patent Information
- Application Number
- PCT/CN2024/075001
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-12
- Filing Date
- 2024-01-31
- Publication Date
- 2024-10-17
AI Technical Summary
During the discharge process, the battery cell generates gas due to the electrolyte and active material, causing the pressure inside the casing to rise, increasing the risk of explosion.
A weak zone is set on the electrode terminal so that it will be destroyed when the pressure or temperature inside the casing exceeds a threshold, forming a channel to discharge excess gas, thereby reducing the risk of explosion, and improving explosion protection by setting a weak zone in the insertion part or the first flange part Effect.
It effectively reduces the risk of battery cells bursting due to excessive internal pressure, simplifies the assembly process of battery cells, and improves structural stability and safety.
Smart Images

Figure CN2024075001_17102024_PF_FP_ABST
Abstract
Description
Battery cells, batteries and electrical devices
Technical field
[0001] The present application relates to the field of battery technology, and in particular to battery cells, batteries, and electrical devices. [Background Technology]
[0002] With the advancement of battery technology, battery cells are being used in a growing number of fields and are gradually replacing traditional fossil fuels in the automotive powertrain sector. Battery cells store chemical energy and controllably convert it into electrical energy. In recyclable battery cells, after discharge, the active material can be activated by recharging for continued use.
[0003] A battery cell typically consists of an electrode assembly, electrode terminals, and a casing. The electrode assembly is electrically connected to the outside world via the electrode terminals. The casing houses and supports the electrode assembly. The casing contains electrolyte. The electrolyte and the active materials in the electrode assembly can generate gas, causing pressure inside the casing to rise, potentially posing a risk of explosion.
[0004] [Summary of the invention]
[0005] In view of the above problems, the present application provides a battery cell, a battery and an electrical device, which can reduce the risk of battery cell explosion.
[0006] In a first aspect, the present application provides a battery cell comprising a housing and electrode terminals. The housing includes a wall portion having an extraction hole. The electrode terminal is disposed in the extraction hole and has a weakened region configured to be broken when the internal pressure of the housing exceeds a pressure threshold or the temperature exceeds a temperature threshold, thereby allowing communication between the interior of the housing and the exterior of the housing.
[0007] Through this approach, when pressure or temperature exceeds a threshold, the weak zone is destroyed, allowing excess gas inside the casing to escape, thereby reducing the risk of battery cell rupture due to excessive internal pressure. Compared to placing the weak zone in the casing, placing the weak zone at the electrode terminal reduces the possibility of casing deformation and facilitates battery cell assembly.
[0008] In some embodiments, the electrode terminal is provided with a notch groove, and the weak area forms the bottom of the notch groove.
[0009] The above method facilitates the processing of weak areas. When the pressure exceeds the pressure threshold or the temperature exceeds the temperature threshold, the electrode terminal can break or bend along the notched groove under the action of pressure, and the excess gas inside the shell can be discharged, thereby reducing the risk of battery cells exploding due to excessive internal pressure.
[0010] In some embodiments, the electrode terminal includes an insertion portion and a first flange portion connected to each other, the insertion portion is inserted into the lead-out hole along the axial direction of the electrode terminal, and in the radial direction of the electrode terminal, the outer peripheral surface of the first flange portion at least partially exceeds the outer peripheral surface of the insertion portion, and the first flange portion is arranged on the outer periphery of the lead-out hole and is supported on the side of the wall portion facing the interior of the shell, wherein the weak area is arranged on the insertion portion and / or the first flange portion.
[0011] In the above manner, since the pressure inside the shell exerts a relatively large force on the insertion part and the first flange part, by setting the weak area on the insertion part or the first flange part, the weak area can be made more sensitive to the pressure inside the shell and more easily achieve an explosion-proof effect.
[0012] In some embodiments, the electrode terminal is provided with a notch groove, the weak area forms the bottom of the notch groove, and the notch groove is provided on the side surface of the first flange portion facing and / or away from the wall portion.
[0013] The above method facilitates the processing of the weak area on the one hand, and on the other hand, generally speaking, the thickness of the first flange portion in the above axial direction is relatively thin, so the notched groove is more sensitive to the internal pressure of the shell and is more likely to have an explosion-proof effect.
[0014] In some embodiments, the scoring groove is at least partially opposite to the matching gap between the outer peripheral surface of the insertion portion and the hole wall of the lead-out hole along the axial direction.
[0015] By adopting the above-mentioned method, when the electrode terminal is broken or bent along the notched groove, it is easier to escape from the lead-out hole, the pressure can be quickly released, and the explosion-proof effect is more easily achieved.
[0016] In some embodiments, in the radial direction, the radial width of the matching gap is greater than the radial width of the scoring groove.
[0017] By adopting the above-mentioned method, when the electrode terminal is broken or bent along the notched groove, it is easier to escape from the lead-out hole, the pressure can be quickly released, and the explosion-proof effect is more easily achieved.
[0018] In some embodiments, a projection of the radially outermost edge of the score groove along the axial direction falls within the matching gap.
[0019] By adopting the above-mentioned method, when the electrode terminal is broken or bent along the notched groove, it is easier to escape from the lead-out hole, the pressure can be quickly released, and the explosion-proof effect is more easily achieved.
[0020] In some embodiments, in the radial direction, the radial width of the score groove is greater than or equal to 0.5 mm and less than or equal to 2 mm.
[0021] In the radial direction, setting the radial width of the scored groove to be greater than or equal to 0.5 mm facilitates bending or breaking of the first flange along the scored groove when the pressure or temperature inside the housing exceeds a pressure threshold or a temperature threshold. Setting the radial width of the scored groove to be less than or equal to 2 mm allows the first flange to maintain sufficient structural strength, thereby improving the structural stability of the battery cell.
[0022] In some embodiments, in the axial direction, the axial depth of the score groove is greater than or equal to 0.1 times the axial thickness of the first flange portion and less than or equal to 0.9 times the axial thickness of the first flange portion.
[0023] In the axial direction, setting the axial depth of the scored groove to 0.1 times the axial thickness H0 of the first flange portion 230 facilitates bending or breaking of the first flange portion along the scored groove when the pressure or temperature inside the housing exceeds a pressure threshold or a temperature threshold. By setting the axial depth of the scored groove to less than or equal to 0.9 times the axial thickness of the first flange portion, the first flange portion can maintain sufficient structural strength, improving the structural stability of the battery cell.
[0024] In some embodiments, the weakened area is at least partially located on the outer periphery of the insert portion.
[0025] Through the above-mentioned method, on the one hand, the processing of the weak area is facilitated, and on the other hand, the insertion portion is made more likely to break along the weak area.
[0026] In some embodiments, the electrode terminal includes an insertion portion and a sealing portion connected to each other. The insertion portion is inserted into the lead-out hole along the axial direction of the electrode terminal. The insertion portion is cylindrical. The sealing portion is sealed at one end of the insertion portion facing the inside of the shell to form a recessed portion. The weak area is arranged on the sealing portion.
[0027] In this way, since the thickness of the blocking portion in the axial direction is relatively thin, the weak area is more sensitive to the internal pressure of the shell, and is more likely to achieve explosion-proof effect. In addition, the gas inside the shell is allowed to enter the recessed portion and be discharged through the recessed portion.
[0028] In some embodiments, the blocking portion is welded to the inserting portion to form a weld mark, and the weak area is located within the weld mark.
[0029] By using the above method, the weld mark can be used as a weak area, which can simplify the manufacturing process of the battery cell.
[0030] In some embodiments, the weak area is arranged in a ring shape around the central axis of the lead-out hole.
[0031] Through the above method, the weak area can be made more sensitive to the internal pressure of the shell, thereby achieving a better explosion-proof effect.
[0032] In some embodiments, the electrode terminal includes an insertion portion and a sealing portion connected to each other, the insertion portion is inserted into the lead-out hole along the axial direction of the electrode terminal, the insertion portion is cylindrical, and the sealing portion is sealed at one end of the insertion portion facing the inside of the shell to form a recessed portion, and the battery cell includes a sealing piece, which is used to seal the recessed portion, and the battery cell is electrically connected to the outside through the sealing piece.
[0033] In the above manner, the recessed portion is sealed by the sealing member and electrically connected to the outside, thereby increasing the connection area between the battery cell and the external device.
[0034] In some embodiments, the recess is used to inject electrolyte into the interior of the housing.
[0035] Through the above-mentioned manner, the structural complexity of the battery cell can be simplified, the occurrence of electrolyte leakage during the assembly process can be reduced, and the assembly efficiency of the battery cell can be improved.
[0036] In some embodiments, the blocking portion is provided with a liquid injection hole, which connects the interior of the shell with the recessed portion.
[0037] The above method is conducive to sealing after the electrolyte injection is completed, thereby reducing the risk of electrolyte leakage.
[0038] In some embodiments, the battery cell further includes a current collecting plate and an electrode assembly disposed inside the housing. The current collecting plate is used to connect the tabs and electrode terminals of the electrode assembly. The side of the sealing portion facing away from the recessed portion is welded to the current collecting plate.
[0039] In the above manner, the thin thickness of the blocking portion is utilized to be welded to the current collecting plate, thereby facilitating electrical connection between the electrode terminal and the current collecting plate from the side of the electrode terminal facing away from the current collecting plate.
[0040] In some embodiments, the battery cell includes an electrode assembly, the outer shell includes a shell and an end cover, one end of the shell has an opening, the end cover covers the opening, the shell includes a side wall and an end wall, the side wall surrounds the outside of the electrode assembly, the end wall is arranged opposite to the opening, and the wall portion is the end cover or the end wall.
[0041] By arranging the electrode terminals on the end covers or end walls in the above manner, the assembly efficiency of the battery cells can be improved, and the possibility of deformation of the end covers or end walls can be reduced, thereby facilitating the assembly of the battery cells.
[0042] In some embodiments, the melting point of the material of the electrode terminal is lower than the melting point of the material of the housing.
[0043] In the above manner, when welding the electrode terminal to other components, the lower melting point of the material of the electrode terminal is conducive to reducing the welding temperature, while the relatively high melting point of the material of the shell can reduce the adverse effects of the welding process on the shell, thereby reducing the risk of leakage.
[0044] In some embodiments, the difference between the melting point of the material of the housing and the melting point of the material of the electrode terminal is greater than 300°C.
[0045] By adopting the above method, when welding the electrode terminal to other components, it is helpful to reduce the welding temperature and reduce the adverse effects of the welding process on the shell, thereby reducing the risk of leakage.
[0046] In some embodiments, the material of the housing includes steel, and the material of the electrode terminal includes aluminum or copper.
[0047] Using steel as the housing material can lower the thermal expansion coefficient and provide good mechanical strength. Copper or aluminum has a lower melting point than steel, making the electrode terminals easier to weld and easier to process and shape.
[0048] In a second aspect, the present application provides a battery comprising the above-mentioned battery cell.
[0049] In a third aspect, the present application provides an electrical device, which includes the above-mentioned battery.
[0050] The above description is only an overview of the technical solution of the present application. In order to more clearly understand the technical means of the present application, it can be implemented in accordance with the contents of the specification. In order to make the above and other purposes, features and advantages of the present application more obvious and easy to understand, the specific implementation methods of the present application are listed below.
Brief Description of the Drawings
[0051] Various other advantages and benefits will become apparent to those skilled in the art upon reading the detailed description of the preferred embodiment below. The accompanying drawings are for illustration purposes only and are not to be considered as limiting the present application. The same reference numerals are used throughout the drawings to represent the same components. In the drawings:
[0052] FIG1 is a schematic structural diagram of a vehicle according to one or more embodiments;
[0053] FIG2 is a schematic diagram of an exploded structure of a battery according to one or more embodiments;
[0054] FIG3 is a schematic cross-sectional view of a battery cell according to one or more embodiments;
[0055] FIG4 is a schematic diagram of the cross-sectional structure of the battery cell shown in FIG3 with some parts hidden;
[0056] FIG5 is a bottom view of the structure of the battery cell shown in FIG3 with some parts hidden;
[0057] FIG6 is a schematic structural diagram of part A of the battery cell shown in FIG3 with some parts hidden;
[0058] FIG7 is a schematic diagram of a partial structure of a battery cell according to one or more embodiments;
[0059] FIG8 is a schematic diagram of a partial structure of a battery cell according to one or more embodiments;
[0060] FIG9 is a schematic diagram of a partial structure of a battery cell according to one or more embodiments;
[0061] FIG. 10 is a schematic diagram of a partial structure of a battery cell according to one or more embodiments.
[0062] Reference numerals in the specific embodiments are as follows: 1000a vehicle; 100a battery; 200a controller; 300a motor; 10a housing; 11a first portion; 12a second portion; D1 radial width of the notched groove; D2 radial width of the matching gap; H0 axial thickness of the first flange portion; H1 axial depth of the notched groove; 1 battery cell; 100 housing; 101 wall portion; 102 lead-out hole; 200 electrode terminal; 210 notched groove; 211 weak area; 220 insertion portion; 230 first flange portion; 240 matching seam; 250 sealing portion; 260 recessed portion; 270 second flange portion; 300 sealing member; 251 liquid injection hole; 400 collecting plate; 500 electrode assembly; 501 electrode tab; 110 shell; 120 end cover; 111 opening; 112 side wall; 113 end wall; 600 insulating member; 700 weld mark. [Specific implementation method]
[0063] The following embodiments of the technical solution of the present application will be described in detail with reference to the accompanying drawings. The following embodiments are only used to more clearly illustrate the technical solution of the present application and are therefore only examples and are not intended to limit the scope of protection of the present application.
[0064] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by those skilled in the art to which this application belongs; the terms used herein are only for the purpose of describing specific embodiments and are not intended to limit this application; the terms "including" and "having" and any variations thereof in the specification and claims of this application and the above-mentioned figure descriptions are intended to cover non-exclusive inclusions.
[0065] In the description of the embodiments of this application, the technical terms "first" and "second" are used only to distinguish different objects and should not be understood to indicate or imply relative importance or implicitly specify the quantity, specific order, or primary and secondary relationship of the indicated technical features. In the description of the embodiments of this application, the meaning of "plurality" is more than two, unless otherwise clearly and specifically defined.
[0066] References herein to "embodiments" mean that a particular feature, structure, or characteristic described in connection with the embodiments may be included in at least one embodiment of the present application. The appearance of this phrase in various places in the specification does not necessarily refer to the same embodiment, nor does it constitute an independent or alternative embodiment that is mutually exclusive of other embodiments. It is understood, both explicitly and implicitly, by those skilled in the art that the embodiments described herein may be combined with other embodiments.
[0067] In the description of the embodiments of this application, the term "and / or" is simply a description of the association relationship between associated objects, indicating that three relationships can exist. For example, A and / or B can represent the following three situations: A exists alone, A and B exist simultaneously, and B exists alone. In addition, the character " / " in this document generally indicates that the associated objects are in an "or" relationship.
[0068] In the description of the embodiments of the present application, the term "multiple" refers to more than two (including two). Similarly, "multiple groups" refers to more than two groups (including two groups), and "multiple pieces" refers to more than two pieces (including two pieces).
[0069] In the description of the embodiments of the present application, the technical terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", "axial", "radial", "circumferential", etc., indicating the orientation or position relationship, are based on the orientation or position relationship shown in the accompanying drawings, and are only for the convenience of describing the embodiments of the present application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the embodiments of the present application.
[0070] In the description of the embodiments of the present application, unless otherwise expressly specified or limited, technical terms such as "installed," "connected," "connected," and "fixed" should be understood in a broad sense. For example, they can refer to fixed connections, detachable connections, or integration; mechanical connections or electrical connections; direct connections or indirect connections through an intermediate medium; internal connections between two components or interactions between two components. Those skilled in the art can understand the specific meanings of the above terms in the embodiments of the present application based on specific circumstances.
[0071] With the advancement of battery technology, battery cells are being used in a growing number of fields and are gradually replacing traditional fossil fuels in the automotive powertrain sector. Battery cells store chemical energy and controllably convert it into electrical energy. In recyclable battery cells, after discharge, the active material can be activated by recharging for continued use.
[0072] A battery cell typically consists of an electrode assembly, electrode terminals, and a casing. The electrode assembly is electrically connected to the outside world via the electrode terminals. The casing houses and supports the electrode assembly. The casing contains electrolyte. The electrolyte and the active materials in the electrode assembly can generate gas, causing pressure inside the casing to rise, potentially posing a risk of explosion.
[0073] To reduce the risk of battery cell explosion, this application provides a weak zone in the electrode terminal. The weak zone is designed to connect the interior of the housing to the exterior when the internal pressure of the housing exceeds a pressure threshold or the temperature exceeds a temperature threshold. Compared to providing a weak zone in the housing, providing a weak zone in the electrode terminal can reduce the possibility of housing deformation and facilitate battery cell assembly.
[0074] Based on the above considerations, the present application provides a battery cell, a battery, and an electrical device. When the pressure exceeds a pressure threshold or the temperature exceeds a temperature threshold, the electrode terminal can break or bend along the weak zone under the action of pressure or high temperature, allowing excess gas inside the housing to be discharged, thereby reducing the risk of the battery cell bursting due to excessive internal pressure. By providing the weak zone on the insertion portion or the first flange portion, the weak zone can be made more sensitive to the pressure inside the housing, making it easier to achieve an explosion-proof effect. In this way, the risk of battery cell bursting can be reduced.
[0075] The battery cells, batteries, and electrical devices disclosed in the embodiments of the present application can be used in electrical devices that use batteries as power sources or various energy storage systems that use batteries as energy storage elements. The electrical devices can be, but are not limited to, mobile phones, tablets, laptops, electric toys, power tools, battery-powered vehicles, electric vehicles, ships, spacecraft, and the like. Among them, electric toys can include fixed or mobile electric toys, such as game consoles, electric car toys, electric ship toys, and electric airplane toys, and the like, and spacecraft can include airplanes, rockets, space shuttles, and spacecraft, and the like.
[0076] For the convenience of description, the following embodiments are described by taking a vehicle 1000a as an example of an electrical device according to an embodiment of the present application.
[0077] Referring to Figure 1, vehicle 1000a can be a fuel vehicle, a gas vehicle, or a new energy vehicle. The new energy vehicle can be a pure electric vehicle, a hybrid vehicle, or an extended-range vehicle, etc. A battery 100a is provided inside vehicle 1000a. Battery 100a can be provided at the bottom, head, or tail of vehicle 1000a. Battery 100a can be used to power vehicle 1000a. For example, battery 100a can serve as an operating power source for vehicle 1000a. Vehicle 1000a can also include a controller 200a and a motor 300a. Controller 200a is used to control battery 100a to power motor 300a, for example, to meet the power requirements for starting, navigating, and driving the vehicle 1000a.
[0078] In some embodiments of the present application, the battery 100a can serve not only as an operating power source for the vehicle 1000a, but also as a driving power source for the vehicle 1000a, replacing or partially replacing fuel or natural gas to provide driving power for the vehicle 1000a.
[0079] In some embodiments, the battery 100a may be an energy storage device, including an energy storage container, an energy storage cabinet, and the like.
[0080] The battery 100 a mentioned in the embodiments of the present application refers to a single physical module including one or more battery cells 1 to provide higher voltage and capacity.
[0081] In the embodiment of the present application, the battery cell 1 may be a secondary battery, which refers to a battery cell that can be recharged to activate the active material after discharge and continue to be used. Each battery cell 1 may also be a primary battery.
[0082] The battery cell 1 includes, but is not limited to, a lithium-ion battery, a sodium-ion battery, a sodium-lithium-ion battery, a lithium metal battery, a sodium metal battery, a lithium-sulfur battery, a magnesium-ion battery, a nickel-metal hydride battery, a nickel-cadmium battery, a lead-acid battery, etc. The battery cell 1 may be cylindrical, flat, rectangular, or have other shapes.
[0083] In some embodiments, the battery 100 a may be a battery module. When there are multiple battery cells 1 , the multiple battery cells 1 are arranged and fixed to form a battery module.
[0084] In some embodiments, referring to FIG. 2 , the battery 100 a may be a battery pack, which includes a housing 10 a and battery cells 1 . The battery cells 1 or battery modules are housed in the housing 10 a .
[0085] In some embodiments, the box 10a can serve as part of the chassis structure of the vehicle 1000a. For example, a portion of the box 10a can become at least a portion of the floor of the vehicle 1000a, or a portion of the box 10a can become at least a portion of the cross member and longitudinal member of the vehicle 1000a.
[0086] Referring to Figure 2, the battery 100a includes a housing 10a and a battery cell 1, and the battery cell 1 is accommodated in the housing 10a. The housing 10a is used to provide a storage space for the battery cell 1, and the housing 10a can adopt a variety of structures. In some embodiments, the housing 10a can include a first portion 11a and a second portion 12a, and the first portion 11a and the second portion 12a cover each other, and the first portion 11a and the second portion 12a jointly define a storage space for accommodating the battery cell 1. The second portion 12a can be a hollow structure with one end open, and the first portion 11a can be a plate-like structure, and the first portion 11a covers the open side of the second portion 12a, so that the first portion 11a and the second portion 12a jointly define a storage space; the first portion 11a and the second portion 12a can also be hollow structures with one side open, and the open side of the first portion 11a covers the open side of the second portion 12a. Of course, the box body 10a formed by the first part 11a and the second part 12a can be in various shapes, such as a cylinder, a cuboid, etc.
[0087] In battery 100a, there may be multiple battery cells 1, which may be connected in series, in parallel, or in a hybrid configuration. A hybrid configuration refers to a combination of series and parallel connections within the battery cells 1. Multiple battery cells 1 may be directly connected in series, in parallel, or in a hybrid configuration, and then the entire battery cell 1 may be housed within the housing 10a. Alternatively, battery 100a may comprise multiple battery cells 1 connected in series, in parallel, or in a hybrid configuration to form a battery module, which is then further connected in series, in parallel, or in a hybrid configuration to form a single unit housed within the housing 10a. Battery 100a may also include other structures, such as a busbar assembly for electrically connecting the multiple battery cells 1.
[0088] 3 , a battery cell 1 is the smallest unit of a battery 100a. In this embodiment, a cylindrical battery cell 1 is used as an example for description. The battery cell 1 includes a housing 100, an electrode assembly 500, and other functional components.
[0089] In some embodiments, the housing 100 is used to encapsulate the electrode assembly 500 and the electrolyte and other components. The housing 100 can be a steel shell, an aluminum shell, a plastic shell (such as polypropylene), a composite metal shell (such as a copper-aluminum composite shell), or an aluminum-plastic film.
[0090] The outer shell 100 may include an end cap 120 and a shell 110. The end cap 120 refers to a component that covers the opening 111 of the shell 110 to isolate the internal environment of the battery cell 1 from the external environment. Without limitation, the shape of the end cap 120 can be adapted to the shape of the shell 110 to match the shell 110. Optionally, the end cap 120 can be made of a material with a certain hardness and strength (such as aluminum alloy), so that the end cap 120 is not easily deformed when squeezed or collided, so that the battery cell 1 can have a higher structural strength and improved safety performance. Functional components such as electrode terminals 200 can be provided on the end cap 120. The electrode terminal 200 can be used to electrically connect to the electrode assembly 500 for outputting or inputting electrical energy of the battery cell 1. In some embodiments, the end cap 120 can also be provided with a pressure relief mechanism for releasing internal pressure when the internal pressure or temperature of the battery cell 1 reaches a threshold. The end cap 120 may be made of a variety of materials, including but not limited to copper, iron, aluminum, stainless steel, aluminum alloy, and plastic. In some embodiments, an insulating material may be disposed inside the end cap 120 to isolate the electrical connection components within the housing 110 from the end cap 120, thereby reducing the risk of short circuits. For example, the insulating material may be plastic, rubber, or the like.
[0091] The housing 110 is a component that cooperates with the end cap 120 to form the internal environment of the battery cell 1. This internal environment can be used to accommodate the electrode assembly 500, electrolyte, and other components. The housing 110 and end cap 120 can be separate components. An opening 111 can be provided in the housing 110, and the end cap 120 is placed over the opening 111 to form the internal environment of the battery cell 1. Alternatively, the end cap 120 and housing 110 can be integrated. Specifically, the end cap 120 and housing 110 can form a common connection surface before other components are inserted into the housing. When the interior of the housing 110 is to be enclosed, the end cap 120 is placed over the housing 110. The housing 110 can be of various shapes and sizes, such as a rectangular parallelepiped, a cylinder, or a hexagonal prism. Specifically, the shape of the housing 110 can be determined based on the specific shape and size of the electrode assembly 500. The housing 110 can be made of a variety of materials, including but not limited to copper, iron, aluminum, stainless steel, aluminum alloy, and plastic.
[0092] The electrode assembly 500 is a component where electrochemical reactions occur in the battery cell 1. One or more electrode assemblies 500 may be contained in the housing 110.
[0093] In some embodiments, the electrode assembly 500 includes a positive electrode, a negative electrode, and a separator. During the charge and discharge process of the battery cell, active ions (e.g., lithium ions) are intercalated and released between the positive and negative electrodes. The separator is positioned between the positive and negative electrodes to prevent short circuits between the positive and negative electrodes while allowing the active ions to pass through.
[0094] In some embodiments, the positive electrode may be a positive electrode sheet, which may include a positive electrode current collector and a positive electrode active material disposed on at least one surface of the positive electrode current collector.
[0095] As an example, the positive electrode current collector has two surfaces facing each other in its thickness direction, and the positive electrode active material is provided on either or both of the two facing surfaces of the positive electrode current collector.
[0096] As an example, the positive electrode current collector may be a metal foil or a composite current collector. For example, as the metal foil, aluminum or stainless steel with a silver surface treatment, stainless steel, copper, aluminum, nickel, carbon electrode, carbon, nickel or titanium, etc. may be used. The composite current collector may include a polymer material base layer and a metal layer. The composite current collector may be formed by forming a metal material (aluminum, aluminum alloy, nickel, nickel alloy, titanium, titanium alloy, silver and silver alloy, etc.) on a polymer material substrate (such as a substrate of polypropylene, polyethylene terephthalate, polybutylene terephthalate, polystyrene, polyethylene, etc.).
[0097] As an example, the positive electrode active material may include at least one of the following materials: lithium-containing phosphates, lithium transition metal oxides and their respective modified compounds. However, the present application is not limited to these materials, and other traditional materials that can be used as battery positive electrode active materials may also be used. These positive electrode active materials may be used alone or in combination of two or more. Among them, examples of lithium-containing phosphates may include but are not limited to at least one of lithium iron phosphate (such as LiFePO4 (also referred to as LFP)), a composite material of lithium iron phosphate and carbon, lithium manganese phosphate (such as LiMnPO4), a composite material of lithium manganese phosphate and carbon, lithium iron manganese phosphate, and a composite material of lithium iron manganese phosphate and carbon. Examples of lithium transition metal oxides may include but are not limited to lithium cobalt oxide (such as LiCoO2), lithium nickel oxide (such as LiNiO2), lithium manganese oxide (such as LiMnO2, LiMn2O4), lithium nickel cobalt oxide, lithium manganese cobalt oxide, lithium nickel manganese oxide, lithium nickel cobalt manganese oxide (such as LiNi 1 / 3 Co 1 / 3 Mn 1 / 3 O2 (also referred to as NCM 333 ), LiNi 0.5 Co 0.2 Mn 0.3 O2 (also referred to as NCM 523 ), LiNi0.5 Co 0.25 Mn 0.25 O2 (also referred to as NCM 211 ), LiNi 0.6 Co 0.2 Mn 0.2 O2 (also referred to as NCM 622 ), LiNi 0.8 Co 0.1 Mn 0.1 O2 (also referred to as NCM 811 ), lithium nickel cobalt aluminum oxide (such as LiNi 0.85 Co 0.15 Al 0.05 O2) and at least one of its modified compounds, etc.
[0098] In some embodiments, the negative electrode may be a negative electrode sheet, and the negative electrode sheet may include a negative electrode current collector.
[0099] As an example, the negative electrode current collector may be a metal foil, a metal foam, or a composite current collector. For example, the metal foil may be silver-surface-treated aluminum or stainless steel, stainless steel, copper, aluminum, nickel, a carbon electrode, carbon, nickel, or titanium. The metal foam may be nickel foam, copper foam, aluminum foam, alloy foam, or carbon foam. The composite current collector may include a polymer base layer and a metal layer. The composite current collector may be formed by forming a metal material (copper, copper alloy, nickel, nickel alloy, titanium, titanium alloy, silver, and silver alloy, etc.) on a polymer substrate (such as a substrate made of polypropylene, polyethylene terephthalate, polybutylene terephthalate, polystyrene, polyethylene, etc.).
[0100] As an example, the negative electrode sheet may include a negative electrode current collector and a negative electrode active material disposed on at least one surface of the negative electrode current collector.
[0101] As an example, the negative electrode current collector has two surfaces facing each other in its thickness direction, and the negative electrode active material is provided on either or both of the two facing surfaces of the negative electrode current collector.
[0102] As an example, the negative electrode active material may adopt the negative electrode active material for battery cells that is well known in the art. As an example, the negative electrode active material may include at least one of the following materials: artificial graphite, natural graphite, soft carbon, hard carbon, silicon-based materials, tin-based materials, lithium titanate, etc. The silicon-based material may be selected from at least one of elemental silicon, silicon oxide compounds, silicon-carbon composites, silicon-nitrogen composites, and silicon alloys. The tin-based material may be selected from at least one of elemental tin, tin oxide compounds, and tin alloys. However, the present application is not limited to these materials, and other traditional materials that can be used as negative electrode active materials for batteries may also be used. These negative electrode active materials may be used alone or in combination of two or more.
[0103] In some embodiments, the material of the positive electrode current collector may be aluminum, and the material of the negative electrode current collector may be copper.
[0104] In some embodiments, the electrode assembly 500 further includes a separator disposed between the positive electrode and the negative electrode.
[0105] In some embodiments, the separator is a separator. The present application has no particular limitation on the type of separator, and any known separator with a porous structure having good chemical and mechanical stability can be selected.
[0106] As an example, the primary material of the separator can be selected from at least one of glass fiber, non-woven fabric, polyethylene, polypropylene, polyvinylidene fluoride, and ceramic. The separator can be a single-layer film or a multi-layer composite film, without particular limitation. When the separator is a multi-layer composite film, the materials of each layer can be the same or different, without particular limitation. The separator can be a separate component positioned between the positive and negative electrodes, or it can be attached to the surfaces of the positive and negative electrodes.
[0107] In some embodiments, the separator is a solid electrolyte, which is disposed between the positive electrode and the negative electrode and serves to transport ions and isolate the positive and negative electrodes.
[0108] In some embodiments, the battery cell also includes an electrolyte, which acts as a conductor of ions between the positive and negative electrodes. This application does not specifically limit the type of electrolyte, and the electrolyte can be selected based on needs. The electrolyte can be liquid, gel, or solid.
[0109] The liquid electrolyte includes an electrolyte salt and a solvent.
[0110] In some embodiments, the electrolyte salt may be selected from at least one of lithium hexafluorophosphate, lithium tetrafluoroborate, lithium perchlorate, lithium hexafluoroarsenate, lithium bis(fluorosulfonyl)imide, lithium bis(trifluoromethanesulfonyl)imide, lithium trifluoromethanesulfonate, lithium difluorophosphate, lithium difluorooxalatoborate, lithium dioxalatoborate, lithium difluorodioxalatophosphate, and lithium tetrafluorooxalatophosphate.
[0111] In some embodiments, the solvent can be selected from at least one of ethylene carbonate, propylene carbonate, ethyl methyl carbonate, diethyl carbonate, dimethyl carbonate, dipropyl carbonate, methylpropyl carbonate, ethylpropyl carbonate, butylene carbonate, fluoroethylene carbonate, methyl formate, methyl acetate, ethyl acetate, propyl acetate, methyl propionate, ethyl propionate, propyl propionate, methyl butyrate, ethyl butyrate, 1,4-butyrolactone, cyclopentane, dimethyl sulfone, methyl ethyl sulfone and diethyl sulfone. The solvent can also be an ether solvent. Ether solvents can include one or more of ethylene glycol dimethyl ether, ethylene glycol diethyl ether, diethylene glycol dimethyl ether, triethylene glycol dimethyl ether, tetraethylene glycol dimethyl ether, 1,3-dioxolane, tetrahydrofuran, methyltetrahydrofuran, diphenyl ether and crown ether.
[0112] Among them, the gel electrolyte includes a skeleton network with a polymer as the electrolyte, combined with an ionic liquid-lithium salt.
[0113] Among them, solid electrolytes include polymer solid electrolytes, inorganic solid electrolytes, and composite solid electrolytes.
[0114] As an example, the polymer solid electrolyte may be polyether (polyethylene oxide), polysiloxane, polycarbonate, polyacrylonitrile, polyvinylidene fluoride, polymethyl methacrylate, a single ion polymer, polyionic liquid-lithium salt, cellulose, or the like.
[0115] As an example, the inorganic solid electrolyte can be an oxide solid electrolyte (crystalline perovskite, sodium superconducting ion conductor, garnet, amorphous LiPON film), a sulfide solid electrolyte (crystalline lithium superion conductor (lithium germanium phosphosulfide, silver germanium sulfide), amorphous sulfide) and one or more of a halide solid electrolyte, a nitride solid electrolyte and a hydride solid electrolyte.
[0116] As an example, a composite solid electrolyte is formed by adding an inorganic solid electrolyte filler to a polymer solid electrolyte.
[0117] In some embodiments, the electrode assembly 500 is a wound structure in which the positive electrode sheet and the negative electrode sheet are wound into a wound structure.
[0118] In some embodiments, the electrode assembly 500 is provided with tabs 501 that conduct current from the electrode assembly 500. Tabs include positive and negative tabs. The positive and negative tabs can be located together at one end of the main body or separately at opposite ends of the main body. During the charge and discharge process of the battery 100a, the positive and negative active materials react with the electrolyte, and the tabs 501 connect to the electrode terminals to form a current loop.
[0119] According to some embodiments of the present application, as shown in Figures 3 to 5, the battery cell 1 of the present application includes a housing 100 and an electrode terminal 200. The housing 100 includes a wall portion 101, and the wall portion 101 is provided with an extraction hole 102. The electrode terminal 200 is provided in the extraction hole 102, and the electrode terminal 200 is provided with a weak area 211. The weak area 211 is configured to be broken when the internal pressure of the housing 100 exceeds a pressure threshold or the temperature exceeds a temperature threshold, thereby connecting the interior of the housing 100 with the exterior of the housing 100.
[0120] The electrode terminal 200 can be installed in the housing 100 by being inserted into the lead-out hole 102. Specifically, one end of the electrode terminal 200 is disposed toward the interior of the housing 100 and can be used to electrically connect to the electrode assembly 500 disposed within the housing 100. The other end of the electrode terminal 200 is disposed toward the exterior of the housing 100 and can be connected to the outside world, thereby enabling charging and discharging of the electrode assembly 500.
[0121] The interior of the housing 100 can contain an electrolyte and active materials. These materials can generate gas, causing the pressure inside the housing 100 to rise. This accumulation of gas can cause the pressure inside the housing 100 to exceed a threshold pressure. By providing a weak area 211 on the electrode terminal 200, when the pressure exceeds the threshold pressure or the temperature exceeds the threshold temperature, the weak area 211 is destroyed, allowing the interior of the housing 100 to communicate with the exterior, allowing excess gas inside the housing 100 to escape.
[0122] When the battery cell 1 releases energy too quickly, it often causes the temperature inside the housing 100 to rise, which can promote pressure increase. When the temperature exceeds the temperature threshold, the weak area 211 can be destroyed, which helps to alleviate the pressure increase inside the housing 100.
[0123] This configuration can suppress the continuous increase in pressure inside the housing 100 and reduce the risk of the battery cell 1 exploding.
[0124] Alternatively, the weak area 211 may be destroyed due to a pressure greater than the load that the weak area 211 can withstand. The weak area 211 may also be destroyed due to high temperature, for example, due to high temperature causing the weak area 211 to become weaker, or due to high temperature causing the weak area 211 to melt or deform.
[0125] In some embodiments, the electrode terminal 200 may be completely broken along the weak region 211, and the broken portion may move away from the interior of the housing 100 under the pressure inside the housing 100. In other embodiments, the electrode terminal 200 may be partially broken along the weak region 211, and the broken portion may bend away from the interior of the housing 100 under the pressure inside the housing 100.
[0126] If the weak area 211 is positioned on the housing 100, for example, on the wall 101, it would weaken the structural strength of the housing 100, reducing its ability to withstand loads and making it susceptible to deformation under stress, hindering the assembly of the battery cell 1. For example, the housing 100 may support the electrode assembly 500, and deformation of the housing 100 would make assembly of the electrode assembly 500 difficult. Therefore, positioning the weak area 211 on the electrode terminal 200 can reduce the possibility of deformation of the housing 100 and facilitate assembly of the battery cell 1.
[0127] According to some embodiments of the present application, optionally, as shown in FIG. 6 , the electrode terminal 200 is provided with a notch groove 210 , and the weak area 211 forms the bottom of the notch groove 210 .
[0128] A weak area 211 can be formed on the electrode terminal 200 by forming a notch 210. When the pressure exceeds a pressure threshold or the temperature exceeds a temperature threshold, the electrode terminal 200 can break or bend along the notch 210 under the pressure or high temperature, allowing excess gas inside the housing 100 to be discharged, thereby reducing the risk of the battery cell 1 exploding due to excessive internal pressure.
[0129] According to some embodiments of the present application, optionally, as shown in Figure 6, the electrode terminal 200 includes an insertion portion 220 and a first flange portion 230 connected to each other, and the insertion portion 220 is inserted into the lead-out hole 102 along the axial direction of the electrode terminal 200. In the radial direction of the electrode terminal 200, the outer peripheral surface of the first flange portion 230 at least partially exceeds the outer peripheral surface of the insertion portion 220, and the first flange portion 230 is arranged on the outer periphery of the lead-out hole 102 and is supported on the side of the wall portion 101 facing the interior of the shell 100, wherein the weak area 211 is arranged on the insertion portion 220 and / or the first flange portion 230.
[0130] The axial direction of the electrode terminal 200 refers to the distance between one end of the electrode terminal 200 facing the interior of the housing 100 and the other end facing away from the interior of the housing 100, while the radial direction of the electrode terminal 200 refers to the direction perpendicular to the axial direction of the electrode terminal 200. With respect to the axial and radial directions described below, any unspecified references refer to the axial and radial directions of the electrode terminal 200.
[0131] By positioning the insertion portion 220 so that it is inserted into the lead-out hole 102 along the axial direction of the electrode terminal 200, the electrode terminal 200 can be installed. By supporting the first flange portion 230 on the wall portion 101, the connection stability between the electrode terminal 200 and the wall portion 101 can be improved. In the radial direction of the electrode terminal 200, by positioning the outer circumference of the first flange portion 230 at least partially beyond the outer circumference of the insertion portion 220 and positioning the first flange portion 230 inside the housing 100, the wall portion 101 can block the first flange portion 230, thereby preventing the electrode terminal 200 from being removed from the interior of the housing 100.
[0132] The weak area 211 can be provided on the insertion portion 220, the first flange portion 230, or both. By providing the weak area 211 on the insertion portion 220, when the pressure inside the housing 100 exceeds a pressure threshold or the temperature exceeds a temperature threshold, the insertion portion 220 can break or bend along the weak area 211, allowing excess gas inside the housing 100 to be discharged. By providing the weak area 211 on the first flange portion 230, when the pressure inside the housing 100 exceeds a pressure threshold or the temperature exceeds a temperature threshold, the first flange portion 230 can break or bend along the weak area 211, allowing excess gas inside the housing 100 to be discharged.
[0133] Since the pressure inside the shell 100 exerts a relatively large force on the insertion part 220 and the first flange part 230, by setting the weak area 211 on the insertion part 220 or the first flange part 230, the weak area 211 can be made more sensitive to the pressure inside the shell 100 and more easily achieve an explosion-proof effect.
[0134] According to some embodiments of the present application, optionally, as shown in Figures 6 to 8, the electrode terminal 200 is provided with a notched groove 210, the weak area 211 forms the bottom of the notched groove 210, and the notched groove 210 is arranged on the side surface of the first flange portion 230 facing and / or away from the wall portion 101.
[0135] The side surface of the first flange portion 230 facing the wall portion 101 and the side surface of the first flange portion 230 facing away from the wall portion 101 may be spaced apart in the axial direction. The scored groove 210 may be provided on the side surface of the first flange portion 230 facing the wall portion 101, or on the side surface of the first flange portion 230 facing away from the wall portion 101, or on both the side surface of the first flange portion 230 facing the wall portion 101 and the side surface of the first flange portion 230 facing away from the wall portion 101. The weak area 211 may be formed by the scored groove 210.
[0136] This arrangement facilitates the machining of the scored groove 210. Furthermore, since the first flange portion 230 is generally thinner in the axial direction, the scored groove 210 is more sensitive to the internal pressure of the housing 100 and more likely to provide explosion-proofing. When the pressure or temperature inside the housing 100 exceeds a pressure threshold or a temperature threshold, the first flange portion 230 can break or bend axially along the scored groove 210, thereby achieving the explosion-proofing function of the scored groove 210.
[0137] Furthermore, in the radial direction, the first flange portion 230 partially overlaps and is connected to the insertion portion 220 , and the notched groove 210 can be set at the non-overlapping portion of the first flange portion 230 and the insertion portion 220 , which is conducive to realizing the anti-explosion function of the notched groove 210 .
[0138] According to some embodiments of the present application, optionally, as shown in FIG. 6 , the notched groove 210 is at least partially arranged opposite to a matching gap 240 between an outer peripheral surface of the insertion portion 220 and a hole wall of the lead-out hole 102 along the axial direction.
[0139] By arranging the notched groove 210 at least partially opposite to the matching seam 240 along the axial direction, when the electrode terminal 200 breaks or bends along the notched groove 210, it will not be blocked by the wall 101 and will be more easily released from the lead-out hole 102, thereby being able to quickly release pressure and more easily achieve an explosion-proof effect.
[0140] Furthermore, the battery cell 1 includes an insulating member 600, which is used to fill the mating gap 240 and provide insulation and sealing. When the pressure or temperature inside the housing 100 exceeds a pressure threshold or a temperature threshold, the electrode terminal 200 may break or bend along the scored groove 210, loosening the insulation member 600's filling of the mating gap 240, thereby allowing gas to escape from the mating gap 240.
[0141] According to some embodiments of the present application, optionally, as shown in FIG. 6 , in the radial direction, a radial width D2 of the matching slit 240 is greater than a radial width D1 of the scoring groove 210 .
[0142] By setting the radial width D2 of the matching gap 240 to be larger than the radial width D1 of the notch groove 210 in the radial direction, the electrode terminal 200 is more likely to be released from the lead-out hole 102 when it breaks or bends along the notch groove 210, thereby quickly releasing pressure and achieving an explosion-proof effect.
[0143] Specifically, when the pressure inside the housing 100 exceeds a pressure threshold or the temperature exceeds a temperature threshold, the first flange portion 230 may be split axially along the score groove 210 to form a connecting groove that penetrates the first flange portion 230. After the connecting groove is formed, gas accumulated inside the housing 100 may be discharged sequentially through the connecting groove and the matching seam 240.
[0144] According to some embodiments of the present application, optionally, as shown in FIG. 6 , the projection of the outermost edge of the scoring groove 210 in the radial direction along the axial direction falls within the matching gap 240 .
[0145] In the radial direction, the scored groove 210 and the matching gap 240 may partially overlap. When the pressure inside the housing 100 exceeds a pressure threshold or the temperature exceeds a temperature threshold, the first flange portion 230 is subjected to pressure. The pressure acts on the housing 100 in a direction away from the interior of the housing 100, and the bottom of the scored groove 210 may deform away from the interior of the housing 100 until the first flange portion 230 breaks or bends along the scored groove 210.
[0146] By arranging the axial projection of the radially outermost edge of the scored groove 210 to fall within the matching gap 240, the wall portion 101 can escape through the matching gap 240 when the bottom of the scored groove 210 deforms. When the electrode terminal 200 breaks or bends along the scored groove 210, it can more easily escape from the lead-out hole 102, enabling rapid pressure relief and more effective explosion prevention.
[0147] Furthermore, the projection of the innermost edge of the scoring groove 210 in the radial direction along the axial direction may fall within the matching slot 240 or outside the matching slot 240 .
[0148] According to some embodiments of the present application, optionally, in the radial direction, the radial width D1 of the score groove 210 is greater than or equal to 0.5 mm and less than or equal to 2 mm. For example, the radial width D1 of the score groove 210 can be set to 0.6 mm, 0.8 mm, 1.0 mm, 1.4 mm, 1.6 mm, etc.
[0149] In the radial direction, by setting the radial width D1 of the score groove 210 to be greater than or equal to 0.5 mm, the first flange portion 230 is facilitated to break or bend along the score groove 210 when the pressure or temperature inside the housing 100 exceeds a pressure threshold or a temperature threshold. By setting the radial width D1 of the score groove 210 to be less than or equal to 2 mm, the first flange portion 230 can maintain sufficient structural strength, thereby improving the structural stability of the battery cell 1.
[0150] According to some embodiments of the present application, optionally, in the axial direction, the axial depth H1 of the score groove 210 is greater than or equal to 0.1 times the axial thickness H0 of the first flange portion 230 and less than or equal to 0.9 times the axial thickness H0 of the first flange portion 230. For example, the axial depth H1 of the score groove 210 may be equal to 0.1 times, 0.2 times, 0.3 times, 0.5 times, or 0.7 times the axial thickness H0 of the first flange portion 230. For another example, when the axial thickness H0 of the first flange portion 230 is equal to 1 mm, the radial width D1 of the score groove 210 may be set to 0.2 mm, 0.4 mm, 0.5 mm, 0.6 mm, 0.8 mm, etc.
[0151] In the axial direction, by setting the axial depth H1 of the score groove 210 to 0.1 times the axial thickness H0 of the first flange portion 230, it is beneficial to promote the first flange portion 230 to break or bend along the score groove 210 when the pressure inside the housing 100 exceeds a pressure threshold or the temperature exceeds a temperature threshold. By setting the axial depth H1 of the score groove 210 to be less than or equal to 0.9 times the axial thickness H0 of the first flange portion 230, the first flange portion 230 can maintain sufficient structural strength, which is beneficial to improving the structural stability of the battery cell 1.
[0152] According to some embodiments of the present application, optionally, as shown in FIG. 9 , the weak area 211 is at least partially located on the outer circumferential surface of the insertion portion 220 .
[0153] Such a configuration, on the one hand, facilitates the processing of the weak area 211 , and on the other hand, makes it easier for the insertion portion 220 to break along the weak area 211 .
[0154] When the internal pressure of the housing 100 exceeds a pressure threshold or the temperature exceeds a temperature threshold, the insertion portion 220 may break or bend along the weak area 211 from the outer circumference, thereby reducing the risk of the battery cell 1 exploding.
[0155] For example, the weak area 211 can be formed at the bottom of the notch groove 210, the notch of the notch groove 210 can be opened on the outer peripheral surface of the insertion portion 220, and the weak area 211 can be located at the first flange portion 230. When the internal pressure of the shell 100 exceeds the pressure threshold or the temperature exceeds the temperature threshold, the insertion portion 220 and the weak area 211 can be synchronously broken or bent along the notch groove 210.
[0156] According to some embodiments of the present application, optionally, as shown in Figure 10, the electrode terminal 200 includes an insertion portion 220 and a sealing portion 250 connected to each other, the insertion portion 220 is inserted into the lead-out hole 102 along the axial direction of the electrode terminal 200, and the insertion portion 220 is arranged in a cylindrical shape. The sealing portion 250 is sealed at one end of the insertion portion 220 facing the inside of the shell 100 to form a recessed portion 260, and the weak area 211 is arranged on the sealing portion 250.
[0157] The recessed portion 260 may be formed on a side of the blocking portion 250 facing away from the interior of the housing 100. When the weak area 211 is disposed on a side surface of the blocking portion 250 facing the recessed portion 260, the weak area 211 may be in communication with the recessed portion 260.
[0158] The weak area 211 is arranged on the side surface of the sealing part 250 facing the recessed part 260, or on the side surface of the sealing part 250 facing away from the recessed part 260, or on both the side surface of the sealing part 250 facing the recessed part 260 and the side surface of the sealing part 250 facing away from the recessed part 260.
[0159] The side surface of the sealing portion 250 facing the recessed portion 260 and the side surface of the sealing portion 250 facing away from the recessed portion 260 may be spaced apart in the axial direction. By providing the weak area 211 on the side surface of the sealing portion 250 facing and / or away from the recessed portion 260, when the pressure inside the housing 100 exceeds a pressure threshold or the temperature exceeds a temperature threshold, the sealing portion 250 may break or bend along the weak area 211, thereby allowing gas inside the housing 100 to enter the recessed portion 260 and be discharged through the recessed portion 260.
[0160] By providing the recessed portion 260, the thickness of the blocking portion 250 in the axial direction can be smaller than the thickness of the inserting portion 220. Since the blocking portion 250 is relatively thin in the axial direction, the weak area 211 is more sensitive to the internal pressure of the housing 100 and is more likely to achieve an explosion-proof effect.
[0161] According to some embodiments of the present application, optionally, as shown in FIG. 10 , the blocking portion 250 is welded to the inserting portion 220 to form a weld mark 700 , and the weak area 211 is located within the weld mark 700 .
[0162] By controlling the welding process, the weld mark 700 can be used as the weak area 211. When the pressure inside the housing 100 exceeds a pressure threshold or the temperature exceeds a temperature threshold, the weak area 211 can be destroyed. This configuration can simplify the manufacturing process of the battery cell 1.
[0163] In some embodiments, the battery cell 1 further includes a current collecting plate 400 disposed within the housing 100. The sealing portion 250 and the current collecting plate 400 are welded together to form a weld mark 700, electrically connecting the sealing portion 250 and the current collecting plate 400. When the pressure or temperature within the housing 100 exceeds a pressure threshold or a temperature threshold, the sealing portion 250 may rupture along the weak region 211, thereby blocking the current path between the electrode terminal 200 and the electrode assembly 500 and delaying the release of electrical energy.
[0164] In other embodiments, the weak area 211 is provided on the sealing portion 250 and surrounds the weld mark 700. This configuration allows the sealing portion 250 to break along the weak area 211 when the pressure inside the housing 100 exceeds a pressure threshold or the temperature exceeds a temperature threshold, thereby blocking the current path between the electrode terminal 200 and the electrode assembly 500 and delaying the release of electrical energy.
[0165] According to some embodiments of the present application, optionally, as shown in FIG. 5 , the weak area 211 is arranged in a ring shape around the central axis of the outlet hole 102 .
[0166] This configuration makes the weak zone 211 more sensitive to the internal pressure of the housing 100, providing a better explosion-proof effect. Specifically, when the internal pressure or temperature of the housing 100 exceeds a pressure threshold or a temperature threshold, the electrode terminal 200 may fracture along the weak zone 211. In the radial direction, the portion of the electrode terminal 200 located within the weak zone 211 may separate from the portion located outside the weak zone 211. Alternatively, the portion of the electrode terminal 200 located within the weak zone 211 may bend away from the interior of the housing 100.
[0167] According to some embodiments of the present application, optionally, as shown in Figures 3 and 6, the electrode terminal 200 includes an insertion portion 220 and a blocking portion 250 connected to each other. The insertion portion 220 is inserted into the lead-out hole 102 along the axial direction of the electrode terminal 200. The insertion portion 220 is cylindrical. The blocking portion 250 blocks one end of the insertion portion 220 facing the interior of the housing 100 to form a recessed portion 260. The battery cell 1 includes a blocking member 300, which is used to block the recessed portion 260. The battery cell 1 is electrically connected to the outside through the blocking member 300.
[0168] By providing the blocking member 300 to block the recessed portion 260 , the blocking member 300 can be used to increase the connection area between the battery cell 1 and external devices, and alleviate leakage of electrolyte inside the battery cell 1 .
[0169] Specifically, by providing a fixed connection between the blocking piece 300 and the electrode terminal 200, a current path can be formed between the electrode assembly 500, the electrode terminal 200, and the blocking piece 300. The electrode assembly 500 can be electrically connected to the outside through the electrode terminal 200 and the blocking piece 300 in sequence. For example, a battery cell 1 can be connected to a busbar through the blocking piece 300. A busbar is a connecting bar with a multi-layer composite structure that can connect multiple battery cells 1 in series or in parallel by welding or bolting.
[0170] Furthermore, a second flange portion 270 may be formed at one end of the electrode terminal 200 facing away from the interior of the housing 100. The opening of the recessed portion 260 is located at the second flange portion 270. A sealing member 300 may be connected to the second flange portion 270 to seal the recessed portion 260. The electrode terminal 200 may be electrically connected to the outside through the sealing member 300. The wall portion 101 may be constrained between the first flange portion 230 and the second flange portion 270 to limit relative movement between the electrode terminal 200 and the housing 100.
[0171] According to some embodiments of the present application, optionally, as shown in FIG. 3 , the recess 260 is used to inject electrolyte into the interior of the housing 100 .
[0172] During the production process of the battery cell 1, the recessed portion 260 can communicate with the interior of the outer shell 100, thereby allowing electrolyte to be injected into the inner portion of the outer shell 100 through the recessed portion 260. By providing the recessed portion 260, the electrolyte can be injected through the recessed portion 260 after the electrode terminal 200 and the outer shell 100 are assembled and connected, and then sealed using the sealing member 300. This can simplify the structural complexity of the battery cell 1, reduce the occurrence of electrolyte leakage during the assembly process, and improve the assembly efficiency of the battery cell 1.
[0173] According to some embodiments of the present application, optionally, as shown in FIG. 3 , the blocking portion 250 is provided with a liquid injection hole 251 , and the liquid injection hole 251 connects the interior of the housing 100 with the recessed portion 260 .
[0174] During assembly of the battery cell 1, electrolyte injection can flow sequentially through the recessed portion 260 and the injection hole 251 before entering the interior of the housing 100. The provision of the injection hole 251 facilitates sealing after electrolyte injection, reducing the risk of electrolyte leakage. The sealing portion 250 is thinner than the insertion portion 220. By placing the injection hole 251 within the sealing portion 250, the formation of the injection hole 251 is facilitated, facilitating the injection of electrolyte.
[0175] Optionally, two ends of the liquid injection hole 251 along the axial direction may be connected to the recessed portion 260 and the interior of the housing 100 respectively.
[0176] When the blocking portion 250 is provided with a weak area 211, to achieve the function of the weak area 211, the blocking of the liquid injection hole 251 is configured to be impervious to pressure within a pressure threshold range or temperature within a temperature threshold range within the housing 100. Of course, in some embodiments, the electrode terminal 200 may not be provided with a liquid injection hole 251.
[0177] According to some embodiments of the present application, optionally, as shown in Figure 3, the battery cell 1 also includes a collecting plate 400 and an electrode assembly 500 arranged inside the outer shell 100, the collecting plate 400 is used to connect the electrode tab 501 and the electrode terminal 200 of the electrode assembly 500, and the sealing portion 250 is welded to the collecting plate 400 on the side facing away from the recessed portion 260.
[0178] The current collecting plate 400 can be disposed between the electrode terminal 200 and the electrode assembly 500, forming a current path between the electrode terminal 200 and the electrode assembly 500. The provision of the current collecting plate 400 facilitates electrical connection between the electrode terminal 200 and the electrode assembly 500. By utilizing the thinness of the sealing portion 250 for welding to the current collecting plate 400, electrical connection between the electrode terminal 200 and the current collecting plate 400 is facilitated from the side of the electrode terminal 200 facing away from the current collecting plate 400.
[0179] According to some embodiments of the present application, optionally, as shown in Figure 3, the battery cell 1 includes an electrode assembly 500, the outer shell 100 includes a shell 110 and an end cover 120, one end of the shell 110 has an opening 111, the end cover 120 covers the opening 111, the shell 110 includes a side wall 112 and an end wall 113, the side wall 112 surrounds the outside of the electrode assembly 500, the end wall 113 is arranged opposite to the opening 111, and the wall portion 101 is the end cover 120 or the end wall 113.
[0180] In the above embodiment, the wall portion 101 is the end wall 113 . In other embodiments, the wall portion 101 may also be the end cover 120 .
[0181] Since the end cover 120 or the end wall 113 is flatter than the side wall 112 , the assembly efficiency of the battery cell 1 can be improved by disposing the electrode terminal 200 on the end cover 120 or the end wall 113 .
[0182] The electrode assembly 500 can be supported within the housing 100 by the end cap 120 or the end wall 113. If the weak area 211 were located in the end cap 120 or end wall 113, it would weaken the structural strength of the end cap 120 or end wall 113, reducing its ability to withstand loads. This would make the end cap 120 or end wall 113 susceptible to deformation, hindering the assembly of the battery cell 1. Therefore, the weak area 211 located in the electrode terminal 200 can reduce the possibility of deformation of the end cap 120 or end wall 113, facilitating assembly of the battery cell 1.
[0183] According to some embodiments of the present application, optionally, the melting point of the material of the electrode terminal 200 is lower than the melting point of the material of the housing 100 .
[0184] When welding the electrode terminal 200 to other components, the lower melting point of the material of the electrode terminal 200 is conducive to reducing the welding temperature, while the relatively high melting point of the material of the shell 100 can reduce the adverse effects of the welding process on the shell 100, thereby reducing the risk of leakage.
[0185] According to some embodiments of the present application, optionally, the difference between the melting point of the material of the housing 100 and the melting point of the material of the electrode terminal 200 is greater than 300° C.
[0186] Such a configuration is beneficial for lowering the welding temperature when welding the electrode terminal 200 to other components, and can also reduce damage to the housing 100 during the welding process, thereby reducing the risk of leakage.
[0187] According to some embodiments of the present application, optionally, the material of the housing 100 includes steel, and the material of the electrode terminal 200 includes aluminum or copper.
[0188] Using steel as the material for the housing 100 can lower the thermal expansion coefficient of the housing 100 and provide good mechanical strength. Copper or aluminum has a lower melting point than steel, so using copper or aluminum as the material for the electrode terminal 200 can make the electrode terminal 200 easier to weld and is also easier to process and shape.
[0189] According to some embodiments of the present application, optionally, as shown in Figures 3 to 10, the battery cell 1 includes a housing 100 and an electrode terminal 200. The housing 100 includes a wall portion 101, and the wall portion 101 is provided with an extraction hole 102. The electrode terminal 200 is provided in the extraction hole 102, and the electrode terminal 200 is provided with a weak area 211. The weak area 211 is configured to be broken when the internal pressure of the housing 100 exceeds a pressure threshold or the temperature exceeds a threshold, so that the interior of the housing 100 is connected to the exterior of the housing 100. The electrode terminal 200 is provided with a notch 210, and the weak area 211 forms the bottom of the notch 210. The electrode terminal 200 includes a connected insertion portion 220 and a first flange portion 230. The insertion portion 220 is inserted into the lead-out hole 102 along the electrode terminal 200's axial direction. In the radial direction of the electrode terminal 200, the outer circumference of the first flange portion 230 at least partially extends beyond the outer circumference of the insertion portion 220. The portion of the first flange portion 230 disposed outside the lead-out hole 102 is supported on the side of the wall portion 101 facing the interior of the housing 100. A weakened area 211 is provided on the insertion portion 220 and / or the first flange portion 230. The electrode terminal 200 is provided with a notched groove 210. The weakened area 211 forms the bottom of the notched groove 210. The notched groove 210 is provided on the side surface of the first flange portion 230 facing toward and / or away from the wall portion 101. The notched groove 210 is axially disposed at least partially opposite a matching gap 240 between the outer circumference of the insertion portion 220 and the wall of the lead-out hole 102. In the radial direction, the radial width D2 of the matching slit 240 is greater than the radial width D1 of the scored groove 210. The axial projection of the radially outermost edge of the scored groove 210 falls within the matching slit 240. In the radial direction, the radial width D1 of the scored groove 210 is greater than or equal to 0.5 mm and less than or equal to 2 mm. In the axial direction, the axial depth H1 of the scored groove 210 is greater than or equal to 0.1 times the axial thickness H0 of the first flange portion 230 and less than or equal to 0.9 times the axial thickness H0 of the first flange portion 230. The weak area 211 is at least partially located on the outer circumferential surface of the insertion portion 220. The electrode terminal 200 includes an interposed portion 220 and a sealing portion 250. The interposed portion 220 is inserted into the lead-out hole 102 along the axial direction of the electrode terminal 200. The interposed portion 220 is cylindrical in shape. The sealing portion 250 seals the end of the interposed portion 220 facing the interior of the housing 100 to form a recessed portion 260. A weak region 211 is provided on the sealing portion 250. The sealing portion 250 is welded to the interposed portion 220, forming a weld mark 700. The weak region 211 is located within the weld mark 700. The weak region 211 is arranged in an annular shape around the central axis of the lead-out hole 102.The electrode terminal 200 includes an insertion portion 220 and a sealing portion 250 connected to each other. The insertion portion 220 is inserted into the lead-out hole 102 along the axial direction of the electrode terminal 200. The insertion portion 220 is cylindrical in shape. The sealing portion 250 seals the end of the insertion portion 220 facing the interior of the housing 100 to form a recessed portion 260. The battery cell 1 includes a sealing member 300, which is used to seal the recessed portion 260. The battery cell 1 is electrically connected to the outside through the sealing member 300. The recessed portion 260 is used to inject electrolyte into the interior of the housing 100. The sealing portion 250 is provided with an injection hole 251, which connects the interior of the housing 100 with the recessed portion 260. The battery cell 1 also includes a current collecting plate 400 and an electrode assembly 500 disposed within the outer casing 100. The current collecting plate 400 is used to connect the tab 501 of the electrode assembly 500 to the electrode terminal 200. The sealing portion 250 is welded to the current collecting plate 400 on the side facing away from the recessed portion 260. The battery cell 1 includes the electrode assembly 500. The outer casing 100 includes a housing 110 and an end cap 120. One end of the housing 110 has an opening 111, and the end cap 120 covers the opening 111. The housing 110 includes a sidewall 112 and an end wall 113. The sidewall 112 surrounds the outer side of the electrode assembly 500, and the end wall 113 is disposed opposite the opening 111. The wall 101 serves as the end cap 120 or the end wall 113. The melting point of the material of the electrode terminal 200 is lower than that of the outer casing 100. The difference between the melting points of the outer casing 100 and the electrode terminal 200 is greater than 300°C. The housing 100 is made of steel, and the electrode terminal 200 is made of aluminum or copper.
[0190] According to some embodiments of the present application, as shown in FIG2 , a battery 100a includes the battery cell 1. This configuration can improve the stability and reliability of the battery cell 1 during operation by reducing the risk of explosion of the housing 100, thereby improving the stability and reliability of the battery 100a during operation.
[0191] According to some embodiments of the present application, as shown in FIG1 , an electrical device includes the battery 100a described above. This configuration can improve the stability and reliability of the battery 100a during operation by improving the stability and reliability of the battery cell 1, thereby improving the stability and reliability of the electrical device during operation.
[0192] In summary, the embodiments of the present application can achieve that when the pressure exceeds the pressure threshold or the temperature exceeds the temperature threshold, the electrode terminal 200 can be broken or bent along the weak area 211 under the action of pressure, so that the interior of the shell 100 is connected with the outside of the shell 100, and the excess gas inside the shell 100 can be discharged, reducing the risk of the battery cell 1 exploding due to excessive internal pressure. At the same time, it can reduce the possibility of deformation of the shell 100, thereby facilitating the assembly of the battery cell 1.
[0193] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present application, rather than to limit them. Although the present application has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some or all of the technical features therein. These modifications or replacements do not deviate the essence of the corresponding technical solutions from the scope of the technical solutions of the embodiments of the present application, and they should all be included in the scope of the claims and specification of the present application. In particular, as long as there is no structural conflict, the various technical features mentioned in the various embodiments can be combined in any way. The present application is not limited to the specific embodiments disclosed herein, but includes all technical solutions that fall within the scope of the claims.
Claims
1. A battery cell, characterized in that: The battery cell comprises: A housing, the housing comprising a wall portion, the wall portion being provided with a lead-out hole; An electrode terminal is disposed at the lead-out hole, and the electrode terminal is provided with a weak area, and the weak area is configured to be destroyed when the internal pressure or temperature of the shell exceeds a pressure threshold, so that the inside of the shell is connected with the outside of the shell.
2. The battery cell according to claim 1, characterized in that: The electrode terminal is provided with a notch groove, and the weak area forms the bottom of the notch groove.
3. The battery cell according to claim 1, characterized in that: The electrode terminal includes an insertion portion and a first flange portion connected to each other, the insertion portion is inserted into the lead-out hole along the axial direction of the electrode terminal, and in the radial direction of the electrode terminal, the outer circumferential surface of the first flange portion at least partially exceeds the outer circumferential surface of the insertion portion, and the first flange portion is arranged on the periphery of the lead-out hole and is supported on a side of the wall portion facing the interior of the outer shell, wherein the weak area is arranged on the insertion portion and / or the first flange portion.
4. The battery cell according to claim 3, characterized in that: The electrode terminal is provided with a notch groove, the weak area forms the bottom of the notch groove, and the notch groove is arranged on the side surface of the first flange portion facing and / or away from the wall portion.
5. The battery cell according to claim 4, characterized in that: The notched groove is at least partially disposed opposite to a matching gap between an outer peripheral surface of the insertion portion and a hole wall of the lead-out hole along the axial direction.
6. The battery cell according to claim 5, characterized in that: In the radial direction, the radial width of the matching slot is greater than the radial width of the notch groove.
7. The battery cell according to claim 6, characterized in that: A projection of an outermost edge of the notch groove in the radial direction along the axial direction falls within the matching gap.
8. The battery cell according to claim 7, characterized in that: In the radial direction, the radial width of the notch groove is greater than or equal to 0.5 mm and less than or equal to 2 mm.
9. The battery cell according to claim 8, characterized in that: In the axial direction, an axial depth of the notch groove is greater than or equal to 0.1 times the axial thickness of the first flange portion and less than or equal to 0.9 times the axial thickness of the first flange portion.
10. The battery cell according to claim 3, characterized in that: The weakened area is at least partially located on the outer peripheral surface of the insertion portion.
11. The battery cell according to claim 1, characterized in that: The electrode terminal includes an insertion portion and a blocking portion connected to each other, the insertion portion is inserted into the lead-out hole along the axial direction of the electrode terminal, the insertion portion is cylindrical, and the blocking portion blocks one end of the insertion portion toward the inside of the shell to form a recessed portion, and the weak area is arranged on the blocking portion.
12. The battery cell according to claim 11, characterized in that: The blocking portion is welded to the inserting portion to form a weld mark, and the weak area is located in the weld mark.
13. The battery cell according to claim 1, characterized in that: The weak area is arranged in a ring shape around the central axis of the outlet hole.
14. The battery cell according to claim 1, characterized in that: The electrode terminal includes an insertion portion and a sealing portion connected to each other, the insertion portion is inserted into the lead-out hole along the axial direction of the electrode terminal, the insertion portion is cylindrical, and the sealing portion is sealed at one end of the insertion portion facing the inside of the shell to form a recessed portion, the battery cell includes a sealing piece, and the sealing piece is used to seal the recessed portion, and the battery cell is electrically connected to the outside through the sealing piece.
15. The battery cell according to claim 14, characterized in that: The recessed portion is used to inject electrolyte into the interior of the shell.
16. The battery cell according to claim 15, characterized in that: The blocking portion is provided with a liquid injection hole, and the liquid injection hole connects the interior of the shell with the recessed portion.
17. The battery cell according to claim 14, characterized in that: The battery cell further comprises a current collecting plate and an electrode assembly disposed inside the shell, the current collecting plate is used to connect the electrode tab of the electrode assembly and the electrode terminal, and the side of the sealing portion away from the recessed portion is welded to the current collecting plate.
18. The battery cell according to any one of claims 1 to 17, characterized in that: The battery cell includes an electrode assembly, the outer shell includes a shell and an end cover, one end of the shell has an opening, the end cover covers the opening, the shell includes a side wall and an end wall, the side wall surrounds the outside of the electrode assembly, the end wall is arranged opposite to the opening, and the wall portion is the end cover or the end wall.
19. The battery cell according to claim 1, characterized in that: The melting point of the material of the electrode terminal is lower than the melting point of the material of the outer shell.
20. The battery cell according to claim 19, characterized in that: The difference between the melting point of the material of the housing and the melting point of the material of the electrode terminal is greater than 300°C.
21. The battery cell according to claim 1, characterized in that: The material of the shell includes steel, and the material of the electrode terminal includes aluminum or copper.
22. A battery, characterized in that: Comprising a battery cell as claimed in any one of claims 1 to 21.
23. An electrical device, characterized in that: The electrical device comprises the battery as claimed in claim 22.
Citation Information
Patent Citations
Nonaqueous Electrolyte Secondary Battery
CN106486637A
Multi-functional lithium battery cap sealing structure and manufacturing method thereof
CN112397819A
Electrochemical device and electric equipment
CN115149073A
Battery pack
CN207097909U
Battery monomer, battery and electric equipment
CN218602700U