New photocatalyst with surface-modified plasmonic materials

Surface-modified metal plasmonic nanoparticles on semiconductor layers with energy filters facilitate efficient single-electron transfer reactions, overcoming the limitations of traditional photoredox catalysis by stabilizing charge carriers and reducing heat, resulting in scalable and sustainable chemical synthesis.

WO2024213779A1PCT designated stage expired Publication Date: 2024-10-17DE PAIVA SA JACINTO
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
PCT/EP2024/060100
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-12
Filing Date
2024-04-12
Publication Date
2024-10-17

AI Technical Summary

Technical Problem

Photoredox catalysis faces limitations due to the overreliance on traditional transition metal complexes, with challenges in enabling single-electron transfer (SET) reactions using plasmonic materials due to multiple charges and ultrafast carrier relaxation, which hinders scalability and sustainability.

Method used

A catalytic system comprising surface-modified metal plasmonic nanoparticles deposited on a semiconductor layer, utilizing ligands to stabilize charge carriers and facilitate SET reactions, with an energy filter to prolong charge separation states and reduce local heating, enabling redox-neutral and efficient chemical synthesis.

Benefits of technology

This approach enhances the stability and efficiency of photocatalysts, allowing for scalable and sustainable single-electron transfer reactions with improved selectivity and flexibility, while minimizing waste and environmental impact.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure EP2024060100_17102024_PF_FP_ABST
    Figure EP2024060100_17102024_PF_FP_ABST
Patent Text Reader

Abstract

The invention relates to a catalytic system for use in photoredox catalysis, comprising plasmonic nanoparticles, preferably deposited on a semiconductor layer wherein a surface of the metal nanoparticles is modified with at least one ligand, a photoelectrochemical cell comprising the catalytic system, a method of obtaining the catalytic system and a method of synthesizing a molecule through a photoredox catalytical reaction with a single electron transfer mechanism by using the catalytic system.
Need to check novelty before this filing date? Find Prior Art

Description

New photocatalyst with surface-modified plasmonic materials

[0001] Photoelectrocatalysis is a promising strategy for sustainable chemical synthesis, particularly for the production of chemicals and fuels. While electrocatalysis has relatively high efficiencies, it suffers from long charge transfer pathways, high cost, and narrow substrate scope. Photocatalysis offers shorter charge transfer pathways, broad substrate scope, and comparatively low cost, but has complex recyclability processes and low efficiency. Additionally, photocatalysis is more suitable for singleelectron transfer reactions, which are fundamental for organic synthesis. The complementary nature of electro- and photo-catalysis allows for the merging of concepts to mitigate each other's limitations. This approach allows for direct control of redox events to the surface of the electrolyte media, providing handles to optimize efficiency, selectivity, and flexibility unattainable by individual approaches.

[0002] Photoredox catalysis uses light as a reactant to initiate and direct desirable chemistry through single-electron transfer transformation. A photoredox catalyst is a molecule that can be excited by light to initiate redox reactions. The excited photoredox catalyst generates electrical charges (electrons and holes), which are subsequently transferred to a substrate or catalyst that initiates cascade reactions. This mechanism produces versatile but unstable radicals in situ, allowing for unique chemical transformations. The photon energy is used to reduce power consumption and control selectivity.

[0003] However, the overreliance on traditional transition metal complexes as photocatalysts remains a bottleneck for photoredox catalysis scale-up. This issue calls for alternative approaches that differ fundamentally from conventional means of initiating photochemical reactions. Although photoelectrocatalysis is a qualified approach to creating new synthetic routes, the sustainability and commercial credentials of single-electron redox chemistry need to be improved to make it scalable.

[0004] Plasmons are highly effective materials for light absorption and hot carrier generation, which is why they have been applied to photocatalysis. The excitation of its localised surface plasmon resonance creates a non-thermal distribution of multiple carriers that could be harnessed for chemical reactions. However, multi-charge makes its adaptation to photoredox catalysis difficult because, in photoredox catalysis, singleelectron transfer (SET) is the primary mechanism of the reaction. The fact is exacerbated by the ultrafast relaxation of the carriers of about 1 ps.

[0005] SET is a chemical reaction in which an electron is transferred from one molecule (the electron donor) to another molecule (the electron acceptor) in a single step, often a system consisting of a photosensitiser and a substrate or catalyst. This process typically occurs through intermediate steps involving forming transient species, such as radicals. The rate of SET reactions is governed by the energy difference between the donor and acceptor drives electron transfer (Marcus's theory). According to Marcus's theory, the rate of an electron transfer reaction depends on the electronic coupling between the donor and acceptor, the reorganisation of the solvent and the energy difference between the donor and acceptor. Examples include biological systems, e.g. enzyme-catalyzed reactions, photosynthesis and respiration, and inorganic systems, e.g. electrochemical cells and solar energy conversion. Importantly, these processes occur at moderate temperatures and involve single electrical charges. However, enabling SET in plasmonic materials is very challenging, due to multiple charges and their ultrafast relaxations.

[0006] It is an aim of the current invention to provide novel universal photocatalytic systems, which enable control of photocatalysts’ redox states and lifetime, and which leads to simplified, scalable, sustainable and selective chemical synthesis.

[0007] In a first aspect, it is provided a catalytic system for use in photoredox catalysis, comprising metal plasmonic nanoparticles, preferably deposited on a semiconductor layer or ultrathin insulating layer acting as an energy filter, wherein the plasmonic nanoparticles surface is modified with at least one ligand.

[0008] It has been found by the present inventor that surface modification of the metal nanoparticles with a ligand enables SET chemical reactions in solid electrodes, which are redox-neutral. The provenience of the carriers could be traced to the plasmon resonance decay by ultrafast infrared spectroscopy. The findings establish plasmons as a viable photosensitiser or photocatalyst for photoredox catalysis, keeping their inherent advantages, such as intense light absorption, chemical stability and extensive redox window while offering easy design and tunability by simple ligand surface modification. When the metal nanoparticles are deposited on a semiconductor, the lifetime of the charge is increased.

[0009] Redox neutrality is a strategy for improved catalytic output and catalyst stability while avoiding the use of sacrificial agents that increase cost and waste. According tothe green chemistry principles and UN sustainable development goal 12, ‘responsible consumption and production’ existent and novel chemical reactions should be catalyzed (to increase atoms efficiency and rates while decreasing waste and unselective pathways) by easily separable catalysts, enabling their reuse and minimize their components leaching to the environment. In the context of SET reactions, they should be performed in a redox-neutral approach, namely that both electrons and holes are consumed equally and lead to product(s) generation. Any metal nanoparticles may be used, as long as they provide a plasmonic effect. More particularly, the metal nanoparticles should provide optical absorption in the optical range defined as electromagnetic spectrum ranging from UV to near Infrared (300- 1200 nm), measured by UV-Vis optical absorption and reflectance. In a preferred embodiment, the plasmonic nanoparticles are selected from copper, gold, silver and aluminium and are, more preferably, gold nanoparticles due to their chemical stability under organic synthesis conditions.

[0010] In another preferred embodiment, the metal plasmonic nanoparticles have an average size of 200nm or less, 100nm or less, 50nm or less or 10nm or less, as measured by Dynamic Light Scattering (DLS)

[0011] In another preferred embodiment, the metal plasmonic nanoparticles are situated at a distance of at least 10 nm from each other. Even more preferably, the metal plasmonic nanoparticles have a concentration in the layer deposited on the semiconductor of between 10-20% of a compact layer.

[0012] In another preferred embodiment the metal plasmonic nanoparticles are deposited on an n-type semiconductor (ETL layer). Due to the semiconductor's electronic structure, it can trap charge carriers more effectively, increasing the probability of their participation in chemical reactions before they recombine. The n- type semiconductor is preferably chosen from TiO2, ZnO, SnO2, SrTiO3, BrTiO3, Sb2O5, doped ZnO (eg AI:ZnO, ln:ZnO), doped Sb2O5 (eg. Sn-Sb2O5) and combinations thereof. Preferably, the n-type semiconductor is TiO2, SnO2 or a combination thereof.

[0013] The n-type semiconductor may have a thickness of about 200 nm or less, preferably 150 nm or less, more preferably 120 nm or less, e.g. 100 nm, 80 nm, 70 nm or less, as measured by Scanning Electron Microscopy (SEM). More preferably, the n-type semiconductor layer is transparent.

[0014] According to the present invention, by “transparent” it is meant the quality an object or substance has when you can see through it, or when it does not significantly influence the perception of the underlying material. Different degrees of transparency are required depending on the intended use.

[0015] Even more preferably, the n-type semiconductor layer is transparent and colourless, to minimize light scattering, absorption and / or reflection that reduces the quantum yield of the process. Quantum yield is the ratio between the amount of light directly used to form the product and the light uptake by the photosystem. The term “colourless” as used herein refers to a colour-neutral layer that does not have a distinguishable colour, as measured using the CIE 1931 RGB colour space developed by the International Commission on Illumination (CIE) in 1931.

[0016] In an alternative preferred embodiment, the metal plasmonic nanoparticles are deposited on a p-type semiconductor (HTL layer) and is chosen from NiO, CuSCN, AgSCN, Cui, CuBr, CuXO2 (wherein X is for example Cr, B, Al, Ga, In, Sc, Fe), PEDOT.PSS (poly(3,4-ethylenedioxythiophene) polystyrene sulfonate), Spiro: OMeTAD (2,2',7,7'-Tetrakis[N,N-di(4-methoxyphenyl)amino]-9,9'- spirobifluorene), PTAA (Poly[bis(4-phenyl)(2,4,6-trimethylphenyl)amine), and combinations thereof. Preferably, the p-type semiconductor materials are Spiro: OMeTAD, PEDOTPSS and PTAA.

[0017] The p-type semiconductor may have an average thickness of about 700 nm or less, preferably 400 nm or less, more preferably 150 nm or less, e.g. 120 nm, 100 nm, 50 nm or less, as measured by Scanning Electron Microscopy (SEM). More preferably, the p-type semiconductor layer is transparent. Even more preferably, the p-type semiconductor layer is transparent and colourless.

[0018] In a preferred embodiment, the plasmonic nanoparticles are modified with at least one ligand such that the nanoparticles are functionalized with ligand molecules. The ligand acts as a charge acceptor prolonging the plasmon carriers’ lifetime. If a semiconductor is present, it will act as the opposite charge acceptor, also prolonging the charge lifetime. The ligand must selectively accept a single charge and should preferably stabilize it for more than a 1 ns. Also, the ligand should have a higher redox potential than the redox potential of the SET reaction, ensuring the necessary driving force for a spontaneous transformation. The ligand can also contain additional functionalities such as acid or base to promote concerted proton-coupled electron transfers, which decrease the energetics of the chemical transformation.

[0019] In one embodiment, the ligand molecules can be covalently attached to the metal nanoparticle’s surface.

[0020] For example, the ligand has the general formula RX-Acceptor, or RX-Spacer- Acceptor, wherein X is a group that is used to selectively coordinate to the plasmonic surface, which can be, for example, selected from an amino group or a thiol group, more preferably a thiol group. R may be selected from hydrogen atoms, or a substituted or unsubstituted alkyl group. The Spacer serves as a separating element between the coordinating group X on the plasmonic surface and a charge atom accepting unit (Acceptor), which can be substituted or unsubstituted alkyl groups or substituted or unsubstituted triazole groups. The Acceptor is a group designed to receive charge from the plasmonic material, which may be coordinated directly to the X group or to the Spacer linked to X. The acceptor can be one or more substituted or unsubstituted aromatic groups or substituted or unsubstituted methyl viologen groups. Examples of aromatic groups are phenyl, benzyl, naphthyl, phenanthroline or anthracenyl. Examples of substituents are an alkyl, alkoxy, halo, nitro, cyano, carboxyl, ester, amide or hydroxyl groups.

[0021] For example, the ligand is 1 -naphthylmethylamine, thiophenol, 4- methoxythiophenol, 1 -naphthalenethiol, 1 -aminoperylene, 3-aminoperylene, perylene diimide with perylene units from 0-3, i.e Naphthalene Diimide (NDI), Perylene Diimide (PDI), Terrylene Diimide (TDI) and Quarterrylene Diimide (QDI).

[0022] In another preferred embodiment, the catalytic system further comprises a conductive substrate and is preferably chosen from indium tin oxide, fluorinated tin oxide (FTO) or conductive polymers.

[0023] In yet another preferred embodiment, an energy filter is interposed between the charge collector (i.e. the conductive substrate) and plasmonic structure, to prolong the lifetimes of charge separation states and reduce local heating. Usually, when light is absorbed to generate hot carriers, some of the energy inevitably converts into heat, raising the temperature of the system. This heating can influence the chemical processes, which is particularly problematic in reactions involving single-electron transfers. For example, heat can promote unwanted side reactions or lead to the decomposition of sensitive reactants or catalysts, which can obscure or interfere with the desired photocatalytic processes. Thermal effects can obscure redox potentials due to local heating, pushing reactions towards double reduction or oxidationprocesses instead of radical formation via a single-electron transfer process, which is fundamental to many synthetic chemical processes. According to this preferred embodiment in which an energy filter layer is provided in the catalytic system, the efficiency and selectivity of plasmonic catalysis may be enhanced by prolonging the lifetimes of charge separation states and reducing local heating.

[0024] This energy filter is an ultrathin non-crystalline semiconductor (amorphous) layer characterized by a specific transmission function (T(E)), with the role of enhancing hot electron or hole extraction and charge-separated state lifetime. The energy filters are categorised after the shape of their transmission function T(E): deltashaped , box-shaped, or step-shaped. Exemplary ways to choose and calculate T(E) may be found in Fast, J., 2022, Hot-carrier extraction in nanowires, Department of Physics, Lund University

[0025] Examples of the energy filter layer are represented by pinhole-free noncrystalline semiconductors, which may be chosen from TiO2, ZnO, SnO2, SrTiO3, BrTiO3, Sb2O5, doped ZnO, NiO, CuSCN, AgSCN, Cui, CuBr, CuXO2, and combinations thereof. In a preferred embodiment, the energy filter is a layer of amorphous TiO2 (to extract hot electrons) or amorphous NiO (to extract hot holes).

[0026] The energy filter layer may have an average thickness of about 20 nm or less, more preferably 10 nm or less, e.g. 8 nm, 7 nm, 5 nm or less, as measured by Scanning Electron Microscopy (SEM). More preferably, the non-crystalline semiconductor layer is transparent. Even more preferably, the non-crystalline semiconductor layer is transparent and colourless.

[0027] In a preferred embodiment, the energy filter is a layer of amorphous TiO2 (to extract hot electrons) or amorphous NiO (to extract hot holes), with a thickness of up to 10nm.

[0028] The catalytic system according to the invention may be in the form of an electrode for use in an electrochemical cell, comprising the conductive substrate as described above and plasmonic nanoparticles deposited directly on the conductive substrate, wherein the surface of the metal nanoparticles is modified with the at least one ligand. Alternatively, the plasmonic nanoparticles are deposited on a p-type or n- type semiconductor, which is in direct contact with the conductive substrate. Even more preferred, an energy filter as described above is interposed between the conductive substrate and the metal nanoparticles, wherein the metal nanoparticles are deposited directly on the energy filter.

[0029] According to another aspect, the invention relates to a photoelectrochemical cell comprising a working electrode comprising a catalytic system as described above; a counter electrode; optionally, a reference electrode, configured to maintain a constant potential relative to the working electrode an electrolyte medium interposed between the electrodes, the electrolyte medium facilitating ionic conduction therebetween; and electrical connections configured to connect the electrodes to an external circuit, allowing for the flow of electrons generated at the electrode to perform electrical work.

[0030] In another aspect, the invention relates to a method of synthesizing a molecule through a photoredox catalytical reaction with a single electron transfer mechanism by using the catalytic system presented above. The SET reaction can be used to activate various organic functional groups, such as N-H of amines, amides and carbamides, OH of alcohols and acids, C-H of alkanes, alkenes, and alkynes, C-0 of alcohols and acids, as well as heteroatom-containing functional groups, such as halides, sulfonamides, and imines.

[0031] In a preferred embodiment, the reaction is selected from an oxidation, reduction, or redox-neutral reaction. In another preferred embodiment, the photoredox catalytical reaction is a photoelectrochemical reaction.

[0032] During photoelectrocatalysis, charge (e.g hot electrons or hot holes) is extracted in response to light exposure at the working electrode and is directed towards the counter electrode, while the opposite charge (hot holes or hot electrons, respectively) perform the single electron transfer oxidation / reduction reaction.

[0033] When an energy filter is used, only carriers with energies E surpassing the filter energy threshold Eoare extracted. However, plasmons also generate hot carriers with insufficient energy to overcome the energy filter Eo and drive photocatalysis. Their recombination would lead to unwanted local heat generation. Thus, in a preferred embodiment, the photoelectrocatalysis reaction is performed under light modulation, reducing local heat accumulation.

[0034] By light modulation, it is meant as a function applied to the light source that switches it between on and off at regular intervals. The light modulation function can be pulse, ramp, noise, arbitrary, sinusoidal or square, preferably sinusoidal, morepreferably square. The function frequency determines the amount of accumulated heat at the surface. Higher frequencies mean the light toggles on and off more quickly, reducing the time for heat to build up, whereas lower frequencies allow more heat accumulation due to longer periods of continuous light exposure. The frequency should be chosen depending on the experimental requirements, particularly in relation to how heat accumulation affects the experimental system. Preferably, the frequency range is between 1 .Hz - 100 MHz. In a more preferred example, the frequency is 20mHz.

[0035] In another aspect, the invention relates to a method of obtaining a catalytic system as described above comprising the step of modifying the surface of the metal nanoparticles with a ligand.

[0036] In a preferred embodiment, the method of obtaining the catalytic system comprises the steps of: providing a substrate selected from the group consisting of a conductive substrate, an n-type or p-type semiconductor or an energy filter as described above; depositing the metal nanoparticles onto the substrate; and modifying the surface of the metal nanoparticles with a ligand.

[0037] According to a preferred embodiment, The energy filter is deposited on the conductive substrate during its cooling at around 800-900 °C. According to another preferred embodiment, the energy filter layer is deposited via chemical vapor deposition on the conductive substrate.

[0038] According to a preferred embodiment, the depositing of the metal nanoparticles may be performed by spraying, sputtering, chemical vapor deposition, or any other method known in the art.

[0039] According to a preferred embodiment, the surface of the metal nanoparticles is modified by immersing the metal nanoparticles deposited on the desired substrate in a solution comprising the ligand.

[0040] Different aspects and embodiments of the invention will be described in closer detail below, in the description and examples, with reference to the drawings which show:Fig. 1 Reaction scheme depicting the reversible photo-oxidation of ferrocene with TiO2 / Au electrodes with thiol modification;Fig. 2 Chronoamperometry studies of the reversible ferrocene oxidation without applied potential depicting the effect of surface modification- ligth modulation with a square function with (on) under 532 nm CW laser illumination; and (off) without light. Examples

[0041] Au nanoparticles (NPs) synthesis:

[0042] Au NPs were prepared using a modified Turkevich method. Sodium citrate tribasic dihydrate 50 mL (6.6 mM) water solution was taken in a 100 mL round bottom flask and stirred at 70 °C in an oil bath. Then 0.1 mL (2.5 mM) tannic acid was added to the reaction mixture. Finally, 1 mL of (25 mM) HAuCk was added instantly. After 5 minutes, the reaction mixture changed from dark blue to a wine colour. The colour change confirms the formation of the Au nanoparticles. The synthesised Au nanoparticles were stored in a fridge at 4 °C. Dynamic light scattering (DLS) analysis showed a homogenous particle distribution with an average particle size of 10 nm with a localised plasmon resonance optical absorption centred at 515 nm.

[0043] Semiconductor layer preparation:

[0044] TiO2 was spin-coated using a paste purchased from Solaronix previously diluted in ethanol (150 pg paste / ml ethanol). 150 pl of the diluted paste was deposited on top of a cleaned FTO glass and spun at 3000 rpm for 30 sec. Then the TiO2-coated FTO glass plates were annealed at 500 °C for 30 min. The Au NPs were sprayed manually on TiO2 films and annealed at 500 °C for 30 min. The reproducibility of Au NPs deposition was evaluated by monitoring the UV-Vis absorption peak of the Au localised plasmon resonance and confirmed by X-ray photoelectron spectroscopy (XPS spectra were recorded using Al Ka (1487 eV)).

[0045] Energy filter:

[0046] The energy filter electrode was prepared via deposition of an ultrathin metal layer (Ti metal with 10 nm) on the FTO glass during its fabrication. The Ti metal layer is added to the FTO glass during its cooling at around 800-900 °C and air, and oxidizes to amorphous TiO2. The Au NPs were produced directly on the energy filter electrode via metal evaporation followed by annealing. A 2 nm layer of Au metal was evaporated from Au grains onto the energy filter and annealed at 450 °C for 30 min. The procedure yielded well distributed Au NPs with 10-20 nm size confirmed by SEM analysis. The reproducibility of Au NPs deposition was evaluated by monitoring the UV-Vis absorption peak of the Au localised plasmon resonance located at 610 nm andconfirmed by X-ray photoelectron spectroscopy. XPS spectra were recorded using Al Ka (1487 eV).

[0047] Thiophenol modifications:

[0048] The thiophenol modifications of the Au-TiO2 films or Au NPs deposited on the energy filter films were carried out as follows. Equimolar concentration (0.1 M) of the different thiophenol solutions (thiophenol, 4-methoxy thiophenol, 2-naphthalenethiol) were prepared in ethanol. The films were immersed into the thiophenol solutions for 30 min at room temperature without any disturbance (no stirring). After 30 min, the films were taken from the solution and rinsed with ethanol to remove unbonded thiophenol.

[0049] Tests on catalytic activity:

[0050] The photoelectrocatalytic tests were performed in a 1.5 mL photoelectrochemical spectroscopy cell from Redox.me. The tests were performed with single films (the cell can accommodate two films) in a three-electrode configuration with Ag / AgCI and Pt as reference and counter electrodes, respectively. The photoelectrode exposed area to light is 0.79 cm2. Plasmonic excitation was performed with a 532 nm laser of the intensity of 110 mW / cm2Due to the semitransparent nature of the electrodes, only a small fraction of the light is absorbed by the plasmons (ca. 15.5%). The ferrocene reversible oxidation experiments were carried out using the chronoamperometric method by applying a constant potential of 0.1 V (vs Ag / AgCI) for 2h. The tests were performed with thiol-modified and unmodified single films in a three-electrode configuration with Ag / AgCI and Pt as reference and counter electrodes, respectively. Ferrocene (0.1 M) dispersed in 1 ,4 dichlorobenzene was used as an electrolyte. Before the experiments, the electrolyte solution was degassed by sparged with N2 gas for 10 min.

[0051] Samples characterization:

[0052] The dynamic light scattering (DLS) was performed on a Malvern NanoS to determine the average gold colloidal particle size, determined to be 8 ± 2 nm.

[0053] The scanning electron microscopy (SEM) analysis were performed on a Zeiss Merlin microscope with an acceleration voltage was 5 or 10 kV, and the working distance was between 5-7 mm. SEM was used to determine the size of the Au NPs prepared on the energy filter electrode and the thickness of the semiconductor layer

[0054] The UV-Vis absorptions were determined by Cary 5000 UV-Vis-NIR spectrophotometer from Agilent. They established the presence of TiO2 and Au nanoparticles in the films.

[0055] The XPS spectra were recorded using Al Ka (1487 eV). The electron energy analyser used was a Scienta Omicron EW-R4000. The samples were measured as thin films on conductive glass. X-ray photoelectron spectroscopy (XPS) survey analysis was used to establish the Au relative abundance. Looking at the relative intensity of the Ti 2p and Au 4f peaks, it was established that the samples were relatively homogeneous in Au abundance. Thus, differences in catalytic output are unrelated to the samples' gold content.

[0056] Fig. 1 shows a schematic representation of a reversible ferrocene oxidation reaction and the electrodes used to evaluate the effect of gold-surface modifications. The excitation of the gold plasmon resonance results in the formation of hot electrons and holes. The electrons are transferred to the TiO2 (electron acceptor) and the holes to the thiophenol (hole acceptor), which in the figure is represented by the 4- methoxythiophenol. Once there, the hole can react with the ferrocene oxidising it. The electron is sent across the electrochemical cell and reacts with the oxidised ferrocene molecule at the counter electrode. Monitoring of the photoelectrochemical current provides direct information on system activity.

[0057] Fig 2 compares the activities of TiO2 / Au without modification (TiO2-Au) and modified with 4-methoxythiophenol (TiO2-Au-4MPT) in the absence and presence of ferrocene and light. Both systems showed very small photocurrents when ferrocene was absent, thus confirming that the measured photocurrent relates to the ferrocene oxidation reaction. No current was detected when the light was absent (not shown). In the presence of ferrocene, both systems showed measurable amounts of photocurrent, with the system modified with 4-methoxythiophenol showing ~ 4-5 times more photocurrent. From XPS analysis, it is possible to exclude the possibility that the changes in activity are related to differences in the amount of gold. Therefore, the increased photocurrent indicates a constructive role of surface modification in the catalytic output.

[0058] The approach's adaptability and versatility were evaluated using two additional thiophenols, 2-naphthalenethiol and thiophenol. These have an oxidation potential of 1 .33 V vs SCE and 1 .51 V vs SCE, respectively, which is higher than that of 4-methoxythiophenol (1.15 V vs SCE). All modifications positively affected the measured photocurrent.

[0059] Using an energy filter concept improves charge separation and reduces local heat accumulation, which are critical to improving process efficiency.

Claims

Claims1. A catalytic system for use in photoredox catalysis, comprising plasmonic nanoparticles, wherein a surface of the metal nanoparticles is modified with at least one ligand.

2. The catalytic system of claim 1 , wherein the plasmonic nanoparticles are selected from copper, gold, silver and aluminium.

3. The catalytic system of claim 1 or 2, wherein the plasmonic nanoparticles are gold nanoparticles.

4. The catalytic system according to any preceding claim, wherein the metal plasmonic nanoparticles have an average size of less than 200 nm, as measured by Dynamic Light Scattering (DLS).

5. The catalytic system according to any preceding claim, wherein the metal plasmonic nanoparticles are situated at a distance of at least 10 nm from each other.

6. The catalytic system according to any preceding claim, wherein the metal plasmonic nanoparticles have a concentration between 10-20% of a compact monolayer.

7. The catalytic system according to any preceding claim, further comprising an energy filter layer, wherein the plasmonic nanoparticles are deposited on the energy filter layer.

8. The catalytic system according to claim 7, wherein the energy filter layer is a noncrystalline semiconductor layer selected from TiO2, ZnO, SnO2, SrTiO3, BrTiO3, Sb2O5, doped ZnO, NiO, CuSCN, AgSCN, Cui, CuBr, CuXO2 and combinations thereof.

9. The catalytic system according to any of claims 1 to 6, further comprising a semiconductor and wherein the plasmonic nanoparticles are deposited on the semiconductor.

10. The catalytic system according to claim 9, wherein the semiconductor is an n- type semiconductor and is preferably chosen from TiO2, ZnO, SnO2, SrTiOs, BrTiOs, Sb2Os, doped ZnO such as AI:ZnO, ln:ZnO; doped Sb2Os such as Sn- Sb2O5; and combinations thereof.

11. The catalytic system according any of claims 9 and 10, wherein the n-type semiconductor has a thickness of about 200 nm or less, preferably 150 nm orless, more preferably 120 nm or less, e.g. 100 nm, 80 nm, 70 nm or less, as measured by Scanning Electron Microscopy (SEM).

12. The catalytic system according any of claims 9 to 11 , wherein the n-type semiconductor is transparent and / or colourless.

13. The catalytic system according to any of claims 1 to 6, wherein the semiconductor is a p-type semiconductor and is chosen from NiO, CuSCN, AgSCN, Cui, CuBr, CuXO2 (wherein X is for example Cr, B, Al, Ga, In, Sc, Fe), PEDOT.PSS (poly(3,4-ethylenedioxythiophene) polystyrene sulfonate), Spiro: OMeTAD (2,2',7,7'-Tetrakis[N,N-di(4-methoxyphenyl)amino]-9,9'-spirobifluorene), PTAA (Poly[bis(4-phenyl)(2,4,6-trimethylphenyl)amine), and combinations thereof.

14. The catalytic system according to claim 13, wherein the p-type semiconductor is transparent and / or colourless.

15. The catalytic system according to any of claims 13 or 14, wherein the p-type semiconductor has an average thickness of about 700 nm or less, preferably 400 nm or less, more preferably 150 nm or less, e.g. 120 nm, 100 nm, 50 nm or less, as measured by Scanning Electron Microscopy (SEM).

16. The catalytic system of any preceding claim, wherein the ligand has the formula RX-S pacer-Acceptor, with R being a group selected from hydrogen, a substituted or unsubstituted alkyl group; X being a group that is used to selectively coordinate to the plasmonic surface; Spacer being a substituted or unsubstituted alkyl group or a substituted or unsubstituted triazole group and Acceptor being one or more substituted or unsubstituted aromatic groups or substituted or unsubstituted methyl viologen groups.

17. The catalytic system of claim 16, wherein X is selected from an amino group or thiol group, more preferably a thiol group.

18. The catalytic system of any preceding claim further comprising a conductive substrate such as indium tin oxide, fluorinated tin oxide (FTO) or conductive polymers.

19. Electrode for use in an photoelectrochemical cell comprising a catalytic system according to any preceding claim.

20. Photoelectrochemical cell comprising: a working electrode, comprising a catalytic system according to any of claims 1 to 18; a counter electrode;optionally, a reference electrode, configured to maintain a constant potential relative to the working electrode an electrolyte medium interposed between the electrodes, the electrolyte medium facilitating ionic conduction therebetween; and electrical connections configured to connect the electrodes to an external circuit, allowing for the flow of electrons generated at the electrode to perform electrical work.21 . A method of synthesizing a molecule through a photoredox catalytical reaction with a single electron transfer mechanism by using the catalytic system of any of claims 1 -18 or the photoelectrochemical cell of claim 20.

22. The method of claim 21 , wherein the photoredox catalytical reaction is selected from the group consisting of oxidation, reduction, and redox-neutral reaction.

23. The method of any of claims 21 or 2, wherein the photoredox catalytical reaction is a photoelectrochemical reaction.

24. Method of obtaining the catalytic system according to any of claims 1 to 19 comprising the steps of: providing a substrate selected from the group consisting of a conductive substrate, an n-type or p-type semiconductor or an energy filter; depositing metal nanoparticles onto the substrate; and modifying the surface of the metal nanoparticles with a ligand.