Liquid state die forging machine
By adopting separate ejection and ejection unit design in liquid die forging technology, using multiple tie rods and air filling to reduce the displacement difference, the deformation problem during product ejection is solved, product quality is improved, and the heat dissipation mechanism is optimized Aluminum molding effect.
Patent Information
- Application Number
- PCT/CN2023/136853
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-28
- Filing Date
- 2023-12-06
- Publication Date
- 2024-10-31
AI Technical Summary
Existing liquid die forging technology can easily cause slight deformation when ejecting products, especially for thin products, affecting the quality of high-performance products.
It adopts the design of separate ejector unit and ejector unit. The ejector unit is located in the lower mold and the ejector unit is located in the upper mold. The product is ejected through multiple tie rods to reduce the contact area and displacement difference. Air filling is used to reduce the air pressure difference. , to achieve stable product ejection.
It effectively avoids product deformation and improves product quality. By optimizing the ejection mechanism and heat dissipation mechanism, the molding quality and molding speed of aluminum materials at high temperatures are ensured.
Smart Images

Figure CN2023136853_31102024_PF_FP_ABST
Abstract
Description
Liquid die forging machine Technical Field
[0001] The present invention relates to the field of die forging, in particular to a liquid die forging machine. Background Art
[0002] Liquid die forging is a metal forming process that combines the characteristics of casting with similarities to die forging. A certain amount of metal to be cast is directly injected into a lubricated mold cavity. Continuous pressure is applied, leveraging the metal's fluidity during solidification and its plastic deformation after solidification. This process causes the metal to crystallize and solidify under the pressure of the liquid die forging machine, forcibly eliminating shrinkage cavities and porosity caused by solidification shrinkage, resulting in a liquid die forged part free of casting defects.
[0003] In the existing technology, for liquid die forging of semi-solid aluminum materials, an ejector mechanism is usually used to apply upward pressure to the cavity. After the product is formed, the mold is opened and the ejector mechanism continues to move upward to eject the product in the mold. However, the ejector mechanism uses a large force to eject the product. For thinner products, when the mold is just opened, the product fits on the upper surface of the lower mold. When the product is ejected, it will deform due to its thin thickness. Although this deformation is small, it will still affect the product quality for high-end products with high performance requirements. Summary of the Invention
[0004] The present invention aims to provide a liquid die forging machine which can ensure product quality when ejecting products.
[0005] To achieve the above-mentioned purpose, the present invention adopts the following technical solution: a liquid die forging machine, including a lower die mechanism and an upper die mechanism, the lower die mechanism includes a lower die and an ejection unit, a first ejection hole is opened in the middle of the lower die, the ejection unit includes a material trough, the material trough and the first ejection hole are aligned, the upper die mechanism includes an upper die and an ejection unit, the lower surface of the upper die and the upper surface of the lower die are combined to form a die cavity, the ejection unit includes a plurality of tie rods, the plurality of tie rods pass through the upper die and contact the lower surface of the upper die, and the plurality of tie rods can eject the peripheral positions of the product in the upper die.
[0006] In order to improve product quality, the inventors looked for the reasons for product deformation from many aspects in order to find a solution. The deformation here does not refer to deformation visible to the naked eye, but tiny deformation that affects high-performance products.
[0007] Initially, the inventors increased the contact area between the ejector mechanism and the product to reduce pressure and thus avoid product deformation. However, this not only increased the size and cost of the ejector mechanism, but also led to a decline in molding quality. Specifically, because the ejector mechanism is movable and its position is not fixed, the molding quality of the part of the product that contacts the ejector mechanism is far worse than that of the part that contacts the lower mold cavity. Therefore, the smaller the area in contact with the ejector mechanism, the better the molding quality.
[0008] Subsequently, the inventors discovered that the ejector usually starts ejecting from the center of the product in the lower mold, while the side walls of the product are still attached to the lower mold. The center of the product has been ejected a distance by the ejector, but the edges of the product are still attached to the lower mold, causing product deformation. The greater the displacement difference between the center and the edges of the product, the greater the product deformation. Therefore, the inventors solved this problem from two aspects:
[0009] First, the inventors divided the prior art ejection mechanism into two parts: an ejection unit and an ejection unit. The ejection unit is located on the lower mold and pushes the aluminum material into the mold cavity after the mold is closed. The ejection unit is located on the upper mold. When the mold is opened, the ejection unit pushes the product upward, and the product moves upward with the upper mold. Because the upper side of the product is tightly attached to the upper mold, it is less likely to deform and moves upward with the upper mold.
[0010] In the existing technology, the product tends to move closer to the lower mold under the action of gravity. However, after the mold is opened in this solution, the product moves upward with the upper mold. Under the action of gravity, the product tends to move away from the upper mold. The ejection unit only needs a small thrust to demold the product. The displacement difference between the middle and edge of the product is small, and the product deformation is small.
[0011] Second, since the aluminum material is pushed into the mold cavity by the ejection unit and pressure is applied to the aluminum material from the middle of the mold cavity by the ejection unit, after the product is formed, the middle of the product fits most closely with the upper mold. If the product is ejected directly from the middle of the product, a large thrust is required to eject the product. The inventors dispersedly set the contact positions between the ejection unit and the product around the product. The ejection unit first pushes open the edge of the product, which not only reduces the displacement difference of each position when the product is ejected, thereby reducing product deformation, but also allows the surrounding air to enter from the edge of the product and gradually fill in the space between the upper mold and the product, reducing the air pressure difference between the upper and lower sides of the product, and then driving the middle of the product away from the upper mold through the edge of the product, so as to achieve the purpose of reducing deformation.
[0012] The beneficial effects of this program are:
[0013] The product is ejected from the upper mold through multiple tie rods. The contact surfaces between the tie rods and the product are dispersed, and the average displacement difference generated on each contact surface is small. The displacement difference is controlled within the elastic range of the product, thereby avoiding product deformation and improving product quality.
[0014] The ejection unit first pushes open the edge of the product, allowing the surrounding air to gradually fill in between the upper mold and the product, reducing the pressure difference between the upper and lower sides of the product, and then drives the middle of the product out of the upper mold through the edge of the product to achieve the purpose of reducing deformation.
[0015] Preferably, as an improvement, the upper mold mechanism further includes a center beam plate and an upper mold driver, the lower end of the upper mold driver output shaft is connected to the center beam plate, and the lower side of the center beam plate is connected to the upper mold, and the ejection unit further includes an ejection driver and a connecting plate, the ejection driver is arranged in the center beam plate, the upper end of the ejection driver output shaft passes through the center beam plate and is connected to the connecting plate, the upper ends of the pull rods are connected to the lower side of the connecting plate, and the lower ends of the pull rods pass through the center beam plate and the upper mold in sequence. Such an arrangement can produce the following effects:
[0016] 1. The upper die drive drives the center beam plate downward, thereby driving the upper die downward and providing pressure when the aluminum material is formed. After the aluminum material is formed, the upper die drive drives the center beam plate and the upper die upward, and the ejector drive drives the connecting plate downward, thereby driving the pull rod downward, and then ejecting the product downward.
[0017] 2. If the output shaft of the ejector drive is directly set downward, due to the thickness of the center beam plate, the ejector drive may have insufficient stroke to drive the pull rod to eject the product. Therefore, this solution sets the ejector drive in the opposite direction, setting the output shaft of the ejector drive upward and connecting it to the pull rod through a connecting plate, thereby meeting the stroke requirements for ejecting the product.
[0018] 3. If the tie rod only passes through the upper mold, it will be difficult to detect even if the upper mold is skewed relative to the center beam plate, which will cause the upper mold to shift when the lower mold is closed, thereby reducing the product molding quality; in this solution, the tie rod passes through the center beam plate and the upper mold in turn, and plays a positioning role for the center beam plate and the upper mold, thereby preventing the upper mold from skewing relative to the center beam plate, thereby ensuring the product molding quality.
[0019] Preferably, as an improvement, the ejection unit includes a receiving cup and a pressing rod, the receiving cup is cylindrical with upper and lower openings, a punch is provided on the top of the pressing rod, the material trough is composed of the top of the punch and the side wall of the receiving cup, the punch is a hollow structure, the punch is matched with the clearance of the lower opening of the receiving cup, and the top of the punch is perpendicular to the side wall of the receiving cup.
[0020] The temperature of the aluminum material is above 500°. In order to prevent the ejection mechanism from failing under the high temperature of the aluminum material, a heat dissipation mechanism is also set up, which has the following beneficial effects:
[0021] 1. The injection rod drives the punch to move upward, blocking the lower opening of the receiving cup. The punch and the receiving cup form a receiving groove, and the aluminum material is placed into the receiving groove from the upper opening of the receiving cup. After the upper and lower molds are closed, the injection rod drives the punch to move upward, pushes the aluminum material in the receiving cup upward, and applies pressure to the aluminum material in the mold cavity to facilitate the molding of the aluminum material. After the aluminum material is formed, the injection rod drives the punch downward to move out of the receiving cup for cooling and heat dissipation, thereby realizing the three-in-one functions of accommodating aluminum material, pushing aluminum material in, and cooling and heat dissipation.
[0022] The inventors discovered that temperature control is crucial during the aluminum die forging process, ensuring the aluminum reaches its optimal temperature and, in turn, improving the quality of the die. Specifically, at the optimal temperature, aluminum has a higher viscosity than liquid metal, resulting in less gas entrainment in the die and less oxidation, allowing for faster component forming and improved surface finish. Furthermore, aluminum has lower flow stress than solid metal, resulting in less resistance to deformation, allowing for faster forming speeds, complex parts, and high material utilization at a lower cost. Therefore, maintaining the optimal aluminum temperature is crucial.
[0023] 1. Before inserting the aluminum material, the punch is fitted with a gap to facilitate the reinsertion of the punch into the lower opening of the receiving cup to form a receiving groove. When pushing the aluminum material in, the punch is hollow to prevent the aluminum material from being squeezed into the gap between the punch and the receiving cup. Compared with a solid structure, the punch expands more significantly when heated. After the punch contacts the aluminum material, it expands due to heat and presses against the side wall of the receiving cup, preventing the aluminum material from being squeezed into the gap between the punch and the receiving cup when the punch pushes the aluminum material upward. This prevents the aluminum material from not fully entering the mold cavity and affecting the molding effect.
[0024] 2 When ejecting the aluminum material, the bottom of the receiving groove is completely formed by the punch, maximizing the contact area between the punch and the aluminum material, thereby reducing the pressure of the punch on the aluminum material; because the receiving cup is cylindrical, the top of the punch is perpendicular to the side wall of the receiving cup, and no eccentric force is generated. The punch at the bottom of the receiving cup is uniform and stable on the aluminum material, and after the punch expands, it is tightly pressed against the side wall of the receiving cup, thereby avoiding the gap between the punch and the side wall of the receiving cup affecting the quality of the product after the aluminum material is formed.
[0025] After the aluminum material is pushed in, the punch generates heat in the process of extruding the die cavity. The punch moves downward out of the receiving cup. The upper and lower openings of the receiving cup form a ventilated state. The temperature difference between the inside and outside of the receiving cup generates wind. The wind takes away the heat in the receiving cup and passes through the punch, also taking away the heat of the punch, thereby preventing the temperature of the punch from affecting the temperature of the next batch of aluminum material; at the same time, the punch cools down and shrinks, and the volume of the punch becomes smaller, so that it is easier to insert it into the lower opening of the receiving cup next time.
[0026] Preferably, as an improvement, a connector is provided between the injection rod and the punch, with external threads at both ends. The connector's upper and lower ends are threadedly connected to the punch and the top of the injection rod, respectively. With this arrangement, the punch is in direct contact with the hot aluminum material and needs to continuously squeeze the die cavity, making it susceptible to damage. The connector is threadedly connected to the punch to facilitate replacement. Since the punch expands outward when heated, this solution utilizes an outer threaded connection between the punch and the connector, rather than a threaded connection between the punch and the inside of the connector, to prevent the punch from expanding outward when heated and squeezing and damaging the connector.
[0027] Preferably, as an improvement, the connector and the plunger are both hollow structures, and the plunger, connector, and punch are internally connected. With this arrangement, the plunger, connector, and punch are all hollow structures. Liquid or gas in a hollow structure conducts heat faster than solids, and thus can quickly transfer heat from the punch to the connector and the plunger, thereby facilitating heat dissipation from the punch.
[0028] Preferably, as an improvement, the hollow cross-section within the connector is smaller than the hollow cross-sections within the injection rod and the punch, and a protruding central portion of the connector forms a load-bearing portion, which can transmit the impact force of the injection rod to the punch. With this arrangement, since the connector, the connector, and the injection rod are all hollow structures, their strength and stability are inferior to those of a solid structure. In particular, during the upward movement of the punch, when the punch rubs against the inner wall of the receiving cup, the lower end of the punch lacks support. However, the smaller hollow cross-section within the connector than within the injection rod and the punch strengthens the load-bearing capacity of the connector, and enhances the strength and stability of the overall structure formed by the connector, the connector, and the injection rod, similar to the web reinforcement of a T-beam.
[0029] Preferably, as an improvement, an external liquid inlet and an external liquid outlet are provided on the side wall of the injection rod, and a vertical internal cooling tube is provided inside the injection rod. The internal cooling tube includes a fixed portion, a liquid inlet portion, and a liquid outlet portion from bottom to top. The fixed portion is connected to the injection rod, an internal liquid inlet is provided on the side of the liquid inlet portion, and an internal liquid outlet is provided on the top of the liquid outlet portion. The external liquid inlet, internal liquid inlet, liquid inlet portion, liquid outlet portion, internal liquid outlet, and external liquid outlet are connected in sequence. Such an arrangement has the following effects:
[0030] 1. Both the external liquid inlet and the external liquid outlet can be set far away from the punch to prevent the coolant delivery pipe from being affected by high temperature, thereby improving durability.
[0031] 2. Completely wrap the inner cooling tube in coolant to avoid direct contact between the inner cooling tube and the connector, connector and injection rod, thereby improving the durability of the inner cooling tube.
[0032] 3. First, the coolant is transported to the top of the liquid outlet through the inner cooling tube, directly contacting the punch with the highest temperature. At this time, the coolant temperature is the lowest and the cooling effect is the best; then it flows back from the outside of the inner cooling tube, cooling the connector and the injection rod in turn. BRIEF DESCRIPTION OF THE DRAWINGS
[0033] Figure 1 is a front view of Example 1;
[0034] FIG2 is a side view of Example 1;
[0035] FIG3 is a bottom view of the center beam plate of Example 1;
[0036] FIG4 is a cross-sectional view of the push-in unit of Example 2;
[0037] FIG5 is a cross-sectional view of the inner cooling tube of Example 2. Implementation Method
[0038] The following is further described in detail through specific implementation methods:
[0039] The reference numerals in the drawings of the specification include: base 110, support legs 111, bottom plate 112, drive box 120, guide column 130, receiving cup 2, ejection drive member 3, injection rod 4, upper mold drive member 510, upper mold drive member output shaft 511, center beam plate 520, guide hole 521, bolt groove 522, ejection hole 523, ejection drive member 531, connecting plate 532, pull rod 533, baffle 610, frame 611, cardboard 612, guide ring 613, fixing plate 614, enclosure drive member 620, guide rod 630 , electrical box 7, upper connecting plate 2101, lower connecting plate 2102, positioning screw 2103, upper insulation part 2210, spiral channel 2211, lower positioning part 2220, external liquid outlet 2401, external liquid inlet 2402, connecting part 2500, external thread 2501, bearing part 2502, internal thread 2503, punch 2600, inner convex part 2601, sealing ring 2700, inner cooling pipe 2800, fixing part 2810, liquid inlet part 2820, inner liquid inlet 2821, liquid outlet part 2830, inner liquid outlet 2831. Example
[0040] Example 1 is basically as shown in Figure 1: a liquid forging machine, including a frame and an electrical box 7, the bracket includes a rectangular base 110 and a drive box 120, a second top entry hole is opened on the base 110, four legs 111 are integrally formed under the base 110, and a bottom plate 112 is integrally formed at the lower ends of the four legs 111. A guide column 130 is interference fit at each of the four corners on the upper side of the base 110, and the upper ends of the four guide columns 130 are interference fit with the lower side of the drive box 120.
[0041] An upper mold mechanism, a lower mold mechanism and a blocking mechanism are provided on the frame. The upper mold mechanism includes an upper mold driving component 510, a middle beam plate 520, an upper mold (not shown in the figure) and an ejection unit. The oil tank of the upper mold driving component 510 is bolted to the side of the driving box 120. The upper mold driving component 510 is bolted inside the driving box 120. In this embodiment, there are two upper mold driving components 510.
[0042] The lower ends of the output shafts of the two upper mold driving members 510 are bolted to the upper side of the middle beam plate 520. As shown in Figure 3, the middle beam plate 520 is rectangular, and a guide hole 521 is respectively opened at the four corners of the middle beam plate 520. The guide column 130 passes through the guide hole 521 and is slidably connected to the guide hole 521. The position between the upper mold driving member output shafts 511 of the two upper mold driving members 510, the middle beam plate 520 is provided with a plurality of vertical ejection holes 523, and the lower side of the middle beam plate 520 is provided with a plurality of bolt grooves 522.
[0043] Depending on the type of the upper mold, the upper mold can be directly bolted to the bolt groove 522, or the clamp can be first bolted to the bolt groove 522 and then the clamp can be used to fix the upper mold.
[0044] The ejection unit includes an ejection drive member 531, a connecting plate 532 and a plurality of tie rods 533, as shown in Figure 2. For ease of display, the figure only shows a cross-sectional view of the output shaft portion of the ejection drive member 531. The upper end of the output shaft of the ejection drive member 531 passes through the middle beam plate 520 and is threadedly connected to the left end of the connecting plate 532. The plurality of tie rods 533 are welded to the lower right end of the connecting plate 532. The plurality of tie rods 533 sequentially pass through the ejection hole 523 of the middle beam plate 520 and the upper mold (not shown in the figure) as shown in Figure 3, and then contact the lower surface of the mold cavity of the upper mold. The plurality of tie rods 533 can eject the peripheral position of the product in the upper mold downward.
[0045] As shown in Figure 1, the lower mold mechanism includes a lower mold (not shown in the figure) and an ejection unit. The lower surface of the upper mold and the upper surface of the lower mold are enclosed to form a closed mold cavity. The lower mold is bolted to the base 110. A first ejection hole is opened in the middle of the lower mold. The ejection unit includes a receiving cup 2, a shot rod 4 and an ejection drive. The ejection drive is bolted on the bottom plate 112. The upper end of the output shaft of the ejection drive is welded to the lower end of the shot rod 4. The top of the shot rod 4 is slidably connected to the receiving cup 2. The receiving cup 2 is bolted to the second ejection hole of the base 110. The top of the shot rod 4 and the side wall of the receiving cup 2 form a material trough that can accommodate aluminum material. The material trough is aligned with the first ejection hole.
[0046] As shown in Figures 1 and 2, the enclosure mechanism includes four enclosure units, which are respectively arranged in four directions of the frame. When the injection rod 4 presses the aluminum material into the mold cavity, it can prevent the aluminum material from splashing out under pressure and injuring people, thereby improving safety. The four enclosure units all include a baffle 610, an enclosure drive 620 and two vertically arranged guide rods 630. The upper ends of the two guide rods 630 are welded to the bottom side of the drive box 120, and the lower ends are welded to the upper side of the base 110. The baffle 610 includes a frame 611 and a cardboard 612. The cardboard 612 is glued to the frame 611 for easy replacement. Three guide rings 613 are welded on both sides of the frame 611. A guide rod 630 passes through the three guide rings 613 and is slidably connected to the three guide rings 613. An L-shaped fixing plate 614 is provided above the cardboard 612. One side of the fixing plate 614 is welded to the frame 611, and the other side of the fixing plate 614 is bolted to the upper end of the output shaft of the enclosure drive 620. The lower end of the enclosure drive 620 is bolted to the bottom plate 112.
[0047] The upper mold driving component 510 , the ejection driving component 531 , the insertion driving component and the enclosure driving component 620 are all hydraulic cylinders and are powered by the electrical box 7 .
[0048] The specific implementation steps are as follows:
[0049] 1. Bolt the upper mold to the lower side of the middle beam plate 520, so that the lower end of the pull rod passes through the upper mold and contacts the lower surface of the upper mold. Bolt the lower mold to the upper side of the base 110, align the first entry hole of the lower mold with the material trough, put the aluminum material into the material trough, drive the upper mold driving part 510 to drive the middle beam plate 520 to move downward, thereby driving the upper mold to move downward, and then closing the upper and lower molds.
[0050] 2. Drive the enclosure drive 620 to move the baffle 610 upward to surround the upper and lower molds.
[0051] 3. Drive the push-in driving member, which drives the injection rod 4 to move upward. The injection rod 4 pushes the aluminum material into the mold cavity. The injection rod 4 continuously applies pressure to the aluminum material in the mold cavity, thereby forming the aluminum material.
[0052] 4. Drive the enclosure drive 620, which drives the baffle 610 to move downward, exposing the upper and lower molds, and drives the upper mold drive 510, thereby driving the center beam 520 and the upper mold to move upward. At the same time, the ejection drive drives the injection rod 4 to move upward, and the injection rod 4 pushes the product upward, so that the product moves upward with the upper mold.
[0053] 5. The ejection drive member 531 drives the connecting plate 532 to move downward, thereby driving the pull rod 533 to move downward, and then ejecting the product downward, separating the product from the upper mold. Example
[0054] The jacking unit of Example 2 is different from the jacking unit of Example 1. Specifically, as shown in Figures 4 and 5, the jacking unit includes a frame, and the frame includes an upper connecting plate 2101 and a lower connecting plate 2102. Four vertical positioning screws 2103 are bolted between the upper connecting plate 2101 and the lower connecting plate 2102 (for ease of display, the positioning screws 2103 are indicated by bold straight lines, and only two of them are indicated in the figure; the section lines of the upper connecting plate 2101 and the lower connecting plate 2102 are omitted), and a positioning hole is opened on the upper connecting plate 2101.
[0055] A accommodating cup 2 is provided on the upper connecting plate 2101. The accommodating cup 2 is a cylinder with upper and lower openings. The accommodating cup 2 includes an upper insulation part 2210 and a lower positioning part 2220. An insulation unit is provided in the side wall of the upper insulation part 2210. The insulation unit includes an oil inlet, a spiral channel 2211 and an oil outlet that are connected in sequence. There is insulation oil in the spiral channel 2211. The inner diameter of the lower positioning part 2220 is equal to that of the upper insulation part 2210, and the outer diameter is smaller than that of the upper insulation part 2210; the bottom of the upper insulation part 2210 is bolted to the upper connecting plate 2101, and the lower positioning part 2220 is gap-matched with the positioning hole of the upper connecting plate 2101 and passes through the positioning hole.
[0056] The lower connecting plate 2102 is provided with an ejection mechanism, which includes an ejection drive member 3, a pressure injection rod 4, a connecting member 2500 and a punch 2600 from bottom to top. The lower connecting plate 2102 is bolted to the ejection drive member 3, and the upper end of the output shaft of the ejection drive member 3 is threadedly connected to the bottom of the pressure injection rod 4; as shown in Figure 4, the interior of the pressure injection rod 4, the connecting member 2500 and the punch 2600 are all hollow structures with circular cross-sections and are internally connected. The hollow section in the connecting member 2500 is smaller than the hollow section in the pressure injection rod 4 and the punch 2600. External threads 2501 are provided at the upper and lower ends of the connecting member 2500. The middle part of the connecting member 2500 protrudes circumferentially to form a bearing portion 2502, which bears The carrier 2502 can transmit the impact force of the injection rod 4 to the punch 2600. The lower end of the punch 2600 and the upper end of the injection rod 4 are both provided with internal threads 2503, and are respectively threadedly connected to the upper and lower ends of the connecting piece 2500. A sealing ring 2700 is provided between the connecting piece 2500, the punch 2600 and the injection rod 4; the punch 2600 is matched with the gap of the lower opening of the containing cup 2, the punch 2600 can close the lower opening of the containing cup 2 and slide with the inner wall of the containing cup 2, the top of the punch 2600 is perpendicular to the side wall of the containing cup 2, the punch 2600 is an inverted "U" shape, and the hollow structure of the punch 2600 forms a top inner cavity, and the middle part of the top inner cavity bulges inward to form an inner convex portion 2601.
[0057] An external liquid inlet 2402 and an external liquid outlet 2401 are provided on the side wall of the injection rod 4. As shown in FIG5 , a vertical internal cooling tube 2800 is also provided in the injection rod 4 (for ease of display, the internal cooling tube 2800 is omitted in FIG4 ). The internal cooling tube 2800 includes a fixed portion 2810, a liquid inlet portion 2820 and a liquid outlet portion 2830 from bottom to top. The fixed portion 2810 and the liquid inlet portion 2820 are integrally formed. The liquid inlet portion 2820 and the liquid outlet portion 2830 are welded. The bottom of the fixed portion 2810 is bolted to the injection rod 4. Two sealing rings 2700 are also provided between the fixed portion 2810 and the side wall of the injection rod 4. The two sealing rings 2700 are both arranged below the external liquid outlet 2401. An internal liquid inlet 2821 is provided on the side of the liquid inlet portion 2820. 2830 is a copper tube. The liquid outlet 2830 passes through the connector 2500 and is inserted into the punch 2600. The top of the liquid outlet 2830 is an inner liquid outlet 2831. The space between the inner cooling tube 2800, the connector 2500, the connector 2500, and the injection rod 4 forms a return channel. The return channel connects the inner liquid outlet 2831 and the external liquid outlet 2401. The external liquid inlet 2402, the internal liquid inlet 2821, the liquid inlet 2820, the liquid outlet 2830, the inner liquid outlet 2831, the return channel, and the external liquid outlet 2401 are connected in sequence. The liquid inlet 2820 has an annular cutout located below the inner liquid inlet 2821 and above the two sealing rings 2700. Some coolant is contained between the annular cutout and the inner wall of the injection rod 4.
[0058] The specific implementation steps are as follows:
[0059] 1. The driving member 3 drives the injection rod 4 to move upward, and then drives the punch 2600 to move upward, blocking the lower opening of the receiving cup 2. The punch 2600 and the receiving cup 2 form a material trough, and the aluminum material is placed in the material trough. After the high-temperature aluminum material contacts the punch 2600, the punch 2600 is pressed against the side wall of the receiving cup 2 under the action of heating and expansion. The aluminum liquid is stirred with a stirring rod for tens of seconds to form an aluminum material; at the same time, the insulation oil enters from the oil inlet and flows out from the oil outlet to form a circulation, forming an insulation effect on the aluminum liquid in the spiral channel 2211; the coolant enters from the inside of the inner cooling tube 2800, first enters the punch 2600 through the liquid outlet 2830, and cools the punch 2600. The inner convex part 2601 of the punch 2600 blocks the coolant from flowing downward, thereby increasing the time the coolant stays in the punch to improve the cooling effect, and then the coolant flows out from the outside of the inner cooling tube 2800, that is, flows out of the reflux channel. When the coolant flow rate is too slow to reduce the temperature to a reasonable range, the coolant contained between the annular cutout and the inner wall of the injection rod 4 begins to expand due to the high temperature. The coolant generates a reaction force on both sides, thereby widening the gap between the fixing portion 810 and the inner wall of the injection rod 4. The fixing portion 2810 and the inner wall of the injection rod 4 cannot clamp the sealing ring 2700, causing the coolant to overflow outside the injection rod 4. The operator observes the coolant overflow and finds that the cooling effect is insufficient, and then speeds up the flow rate of the coolant to improve the cooling effect.
[0060] 2. The driving member 3 drives the injection rod 4 to continue to move upward, thereby driving the punch 2600 to move upward, pushing the aluminum material in the receiving cup 2 upward into the die cavity.
[0061] 3. After the aluminum material is formed into a product, the push-in driving member 3 is driven to drive the injection rod 4 to move upward to eject the product upward, and then the push-in driving member 3 is driven to drive the injection rod 4 to move downward, thereby driving the punch 2600 to move downward out of the receiving cup 2 for cooling. Specifically, the upper and lower openings of the receiving cup 2 form a ventilated state. Wind is generated due to the temperature difference between the inside and outside of the receiving cup 2. The thermal insulation oil in the spiral channel 2211 isolates the inside and outside of the receiving cup 2 to prevent the temperature from dissipating from the side wall of the receiving cup 2, so that the temperature can only be taken away by the wind from the upper and lower openings of the receiving cup 2, thereby increasing the time and size of the wind flow, so that the wind takes away the heat in the receiving cup 2 and passes through the punch 2600, and also takes away the heat of the punch 2600. The punch 2600 cools down and shrinks, and the volume of the punch 2600 becomes smaller, so as to facilitate the next insertion and closing of the lower opening of the receiving cup 2.
[0062] The above is only an embodiment of the present invention, and the common knowledge such as the specific technical solutions and / or characteristics in the solution are not described in detail here. It should be pointed out that for those skilled in the art, without departing from the technical solution of the present invention, several variations and improvements can be made, which should also be regarded as the scope of protection of the present invention, and these will not affect the effect of the implementation of the present invention and the practicality of the patent. The scope of protection required by this application shall be based on the content of its claims, and the specific implementation methods and other records in the description can be used to interpret the content of the claims.
Claims
1. Liquid die forging machine, Features: It includes a lower mold mechanism and an upper mold mechanism. The lower mold mechanism includes a lower mold and an ejection unit. An ejection hole is opened in the middle of the lower mold. The ejection unit includes a material trough. The material trough is aligned with the first ejection hole. The upper mold mechanism includes an upper mold and an ejection unit. The lower surface of the upper mold and the upper surface of the lower mold are combined to form a mold cavity. The ejection unit includes a plurality of tie rods. The plurality of tie rods pass through the upper mold and contact the lower surface of the upper mold. The plurality of tie rods can eject the peripheral position of the product in the upper mold.
2. The liquid die forging machine according to claim 1, Features: The upper mold mechanism also includes a center beam plate and an upper mold driving component. The lower end of the output shaft of the upper mold driving component is connected to the center beam plate, and the lower side of the center beam plate is connected to the upper mold. The ejection unit also includes an ejection driving component and a connecting plate. The ejection driving component is arranged in the center beam plate, and the upper end of the output shaft of the ejection driving component passes through the center beam plate and is connected to the connecting plate. The upper ends of the pull rods are connected to the lower side of the connecting plate, and the lower ends of the pull rods pass through the center beam plate and the upper mold in sequence.
3. The liquid die forging machine according to claim 2, Features: The ejection unit includes a receiving cup and a pressing rod. The receiving cup is a cylinder with upper and lower openings. A punch is provided on the top of the pressing rod. The material trough is composed of the top of the punch and the side wall of the receiving cup. The punch is a hollow structure. The punch can close the lower opening of the receiving cup and slide with the inner wall of the receiving cup. The top of the punch is perpendicular to the side wall of the receiving cup.
4. The liquid die forging machine according to claim 3, Features: A connecting piece is arranged between the injection rod and the punch, and external threads are arranged at both upper and lower ends of the connecting piece. The upper and lower ends of the connecting piece are respectively threadedly connected with the punch and the top of the injection rod.
5. The liquid die forging machine according to claim 4, Features: The connecting piece and the injection rod are both hollow structures, and the injection rod, the connecting piece and the punch are internally connected.
6. The liquid die forging machine according to claim 5, Features: The hollow section in the connecting piece is smaller than the hollow sections in the injection rod and the punch. The middle part of the connecting piece protrudes to form a bearing part, which can transmit the impact force of the injection rod to the punch.
7. The liquid die forging machine according to claim 6, Features: An external liquid inlet and an external liquid outlet are provided on the side wall of the injection rod, and a vertical internal cooling tube is provided inside the injection rod. The internal cooling tube includes a fixed part, a liquid inlet part and a liquid outlet part from bottom to top. The fixed part is connected to the injection rod, an internal liquid inlet is provided on the side of the liquid inlet part, and an internal liquid outlet is provided on the top of the liquid outlet part. The external liquid inlet, the internal liquid inlet, the liquid inlet part, the liquid outlet part, the internal liquid outlet and the external liquid outlet are connected in sequence.
Citation Information
Patent Citations
Aluminium alloy frying pan liquid die-forging die and technique for producing aluminium alloy frying pan
CN101468378A
Liquid forging and molding die for aluminum alloy wheel
CN105397066A
Punch assembly and die casting machine including punch assembly
CN109382496A
Injection punch of die-casting machine
CN114850437A
Liquid die forging machine
CN116511456A