Power storage module
The power storage module addresses productivity losses by using a resin sealing part with joined linear members to form spacer layers, reducing material waste and maintaining efficiency in larger module sizes.
Patent Information
- Application Number
- PCT/JP2024/016122
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-11
- Filing Date
- 2024-04-24
- Publication Date
- 2024-11-14
AI Technical Summary
The existing power storage module productivity decreases due to high waste rates of sheet materials when forming rectangular frame-shaped sealing layers, especially as the module size increases, leading to inefficiencies in the manufacturing process.
The power storage module employs a resin sealing part with rectangular frame-shaped seal layers and spacer layers, where the spacer layers are formed by joining linear members with a joining member, eliminating the need to punch out sheet material into a rectangular frame shape, thus reducing waste and maintaining productivity.
This approach reduces material waste and maintains productivity by allowing the efficient use of sheet materials without the need for punching out rectangular frames, particularly benefiting larger module sizes.
Smart Images

Figure JP2024016122_14112024_PF_FP_ABST
Abstract
Description
Energy storage module
[0001] The present disclosure relates to an energy storage module.
[0002] Patent Document 1 discloses a bipolar battery that includes a bipolar electrode having a positive electrode on one side of a current collector and a negative electrode on the other side, a gel electrolyte sandwiched between the positive electrode and the negative electrode, and a seal layer that surrounds the periphery of a cell composed of the positive electrode, the negative electrode, and the gel electrolyte and is provided between the current collectors.
[0003] Japanese Patent Application Laid-Open No. 2004-158343
[0004] In the battery (energy storage module) disclosed in Patent Document 1, the current collector is made of rectangular metal foil, and a rectangular frame-shaped sealing layer made of resin is provided around the periphery of the current collector. The rectangular frame-shaped sealing layer is formed, for example, by punching a long sheet material unwound from a raw material roll into a rectangular frame shape. However, when forming the sealing layer by punching sheet material, a large amount of sheet material is wasted, which reduces the productivity of the energy storage module. In particular, as the energy storage module becomes larger, the amount of sheet material wasted increases, which reduces the productivity of the energy storage module more significantly.
[0005] An object of the present disclosure is to provide an energy storage module that can suppress a decrease in productivity.
[0006] An energy storage module according to one aspect of the present disclosure includes a stack of multiple electrodes and a resin sealing portion. Each of the multiple electrodes has a rectangular, metallic current collector. The sealing portion is provided on the periphery of the current collector so as to surround the stack when viewed in the stacking direction of the multiple electrodes. Each of the multiple electrodes has an active material layer on a first surface of the current collector and on a second surface opposite the first surface. The sealing portion includes multiple rectangular frame-shaped sealing layers and multiple rectangular frame-shaped spacer layers. The multiple sealing layers are bonded to the first and second surfaces of the current collectors at the periphery of each of the multiple electrodes. Each of the multiple spacer layers is located between adjacent sealing layers in the stacking direction. Each of the multiple spacer layers, together with the multiple sealing layers, seals an internal space formed between adjacent current collectors in the stacking direction. Each of the multiple spacer layers includes multiple linear members and bonding members. The multiple linear members are arranged spaced apart from each other when viewed in the stacking direction and each have a linearly extending region. The joining members are joined to the edges of adjacent linear members so as to fill the gaps between the edges.
[0007] In the energy storage module, each spacer layer included in the resin sealing portion is formed into a rectangular frame shape by joining the edges of linearly extending members with a joining member. This eliminates the need to punch out a long sheet material unwound from a roll into a rectangular frame shape. This makes it easier to use the sheet material without waste. Such spacer layers can prevent an increase in the waste rate of sheet material. This can prevent a decrease in productivity of the energy storage module.
[0008] The joining members may be injection molded members. Each of the spacer layers may include a welding layer formed at the junction between the joining member and an edge of the linear member, the welding layer fusing the joining member and the linear member together.
[0009] The joining member may be an injection molded member. The joining member may have a melt flow rate greater than the melt flow rate of the straight member.
[0010] When viewed from the stacking direction, the area of the joint member may be smaller than the area of the straight member.
[0011] The thickness of the joining member may be equal to or less than the thickness of the straight member.
[0012] The plurality of straight members may include a pair of first straight members and a pair of second straight members. The pair of first straight members are rectangular and face each other in a first direction as viewed from the stacking direction. The pair of second straight members are rectangular and face each other in a second direction orthogonal to the first direction as viewed from the stacking direction. The joining member may join a region of the edge forming a long side of the first straight member to a region of the edge forming a short side of the second straight member.
[0013] The plurality of straight members may include a pair of first straight members and a pair of second straight members. The pair of first straight members are rectangular and face each other in a first direction as viewed from the stacking direction. The pair of second straight members are rectangular and face each other in a second direction orthogonal to the first direction as viewed from the stacking direction. The joining member may join a region of the edge that forms a short side of the first straight member to a region of the edge that forms a short side of the second straight member.
[0014] The plurality of linear members may include a pair of linear members. The pair of linear members have longitudinal directions that coincide with each other when viewed from the stacking direction. The pair of linear members are adjacent to each other in the longitudinal direction.
[0015] According to the present disclosure, it is possible to provide an energy storage module that can suppress a decrease in productivity.
[0016] FIG. 1 is a schematic plan view showing an example of an energy storage module. FIG. 2 is a schematic cross-sectional view taken along line II-II in FIG. 1. FIG. 3 is a schematic plan view showing a spacer layer. FIG. 4 is a schematic cross-sectional view taken along line IV-IV in FIG. 3. FIG. 5 is a flowchart showing a method for forming a spacer layer. FIG. 6 is a schematic plan view for explaining the method for forming a spacer layer. FIG. 7 is a schematic side view for explaining the method for forming a spacer layer. FIG. 8 is a schematic plan view showing a spacer layer of a comparative example. FIG. 9 is a schematic cross-sectional view taken along line IX-IX in FIG. 8. FIG. 10 is a schematic plan view showing a spacer layer according to a first modified example. FIG. 11 is a schematic plan view showing a spacer layer according to a second modified example.
[0017] Hereinafter, embodiments of the present disclosure will be described in detail with reference to the accompanying drawings. In the description of the drawings, the same or equivalent elements are designated by the same reference numerals, and redundant description will be omitted. In the description, a Cartesian coordinate system defined by X-axis, Y-axis, and Z-axis may be referenced.
[0018] (Embodiment) Fig. 1 is a schematic plan view of an energy storage module according to this embodiment. The energy storage module 11 shown in Fig. 1 can be used as a battery for various vehicles, such as a forklift, a hybrid vehicle, or an electric vehicle. The energy storage module 11 is, for example, a secondary battery, such as a nickel-metal hydride secondary battery or a lithium-ion secondary battery. The energy storage module 11 may be an electric double layer capacitor or an all-solid-state battery. Here, the case where the energy storage module 11 is a lithium-ion secondary battery is shown.
[0019] FIG. 2 is a cross-sectional view taken along line II-II in FIG. 1 , and schematically illustrates the layer structure of the energy storage module 11. The energy storage module 11 is a single cell having a rectangular parallelepiped shape that is flattened in the Z-axis direction. In this embodiment, a bipolar lithium-ion secondary battery is exemplified as the energy storage module 11. The energy storage module 11 is configured to include an electrode stack (stack) 12 in which multiple electrodes are stacked, and a resin sealing portion 30. The multiple electrodes include multiple bipolar electrodes 14. The stacking direction of the multiple electrodes is along the Z-axis direction and coincides with the stacking direction of the energy storage modules 11 in the module stack formed by stacking the energy storage modules 11.
[0020] The bipolar electrode 14 includes a current collector 21, a positive electrode active material layer 22, and a negative electrode active material layer 23. The current collector 21 is a chemically inactive electrical conductor that allows current to continue to flow through the positive electrode active material layer 22 and the negative electrode active material layer 23 during discharging or charging of the lithium ion secondary battery.
[0021] The current collector 21 is a sheet-like conductive member having a rectangular shape in a plan view. The current collector 21 has a first surface 21a and a second surface 21b located on the opposite side of the first surface 21a. The current collector 21 is made of metal and is composed of, for example, a metal foil or an alloy foil. Examples of metal foils include copper foil, aluminum foil, titanium foil, and nickel foil. Examples of alloy foils include stainless steel foil (e.g., SUS304, SUS316, SUS301, etc., as specified in JIS G 4305:2015), plated steel foil, and stainless steel foil. The alloy foil may be an alloy foil of the metals listed above as examples of the metal foil material. The current collector 21 may be formed by integrating or laminating multiple metal foils, or by plating another metal layer on the surface of one metal foil.
[0022] In the illustrated example, the current collector 21 is formed by bonding an aluminum foil 21A and a copper foil 21B together so that the first surface 21a is an aluminum layer and the second surface 21b is a copper layer. The current collector 21 may be, for example, a clad foil formed by rolling and bonding an aluminum foil 21A and a copper foil 21B together. The current collector 21 may also be a laminated foil. That is, the current collector 21 may be formed by bonding and integrating the aluminum foil 21A and the copper foil 21B with a conductive adhesive resin (adhesive layer) so that the first surface 21a is an aluminum layer and the second surface 21b is a copper layer. The current collector 21 may be formed by copper vapor deposition or copper plating on one side of an aluminum foil so that the first surface 21a is an aluminum layer and the second surface 21b is a copper layer. The aluminum layer on the first surface 21a of the current collector 21 may be chromate-treated. Furthermore, the copper layer on the second surface 21b of the current collector 21 may be nickel-plated. In this case, the nickel-plated layer may be a roughened surface, i.e., a protruding plated surface having fine protrusions on its surface. The roughened surface may be rougher than the unprocessed metal foil, and may be formed by roughening processes such as etching and electroplating. For example, the thickness of the current collector 21 may be approximately 30 μm to 150 μm, but is not limited to this.
[0023] The positive electrode active material layer 22 is provided on the first surface 21a of the current collector 21. The current collector 21 and the positive electrode active material layer 22 provided on the first surface 21a of the current collector 21 constitute the positive electrode of the bipolar electrode 14. The positive electrode active material layer 22 is formed in a rectangular shape in the center of the first surface 21a so that the peripheral edge portion 21c of the current collector 21 is exposed.
[0024] The positive electrode active material layer 22, for example, is provided on the first surface 21 a of the current collector 21 via an adhesive layer. For example, the adhesive layer may be formed of an adhesive such as acetylene black. The adhesive layer, for example, may be provided on the entire first surface 21 a of the current collector 21. Furthermore, the edge of the adhesive layer may be formed along the edge of the negative electrode active material layer 23 that surrounds the positive electrode active material layer 22, as viewed from the stacking direction.
[0025] The positive electrode active material layer 22 is a layered member containing a positive electrode active material, a conductive additive, and a binder. Examples of the positive electrode active material include a composite oxide, metallic lithium, and sulfur. The composition of the composite oxide includes, for example, at least one of iron, manganese, titanium, nickel, cobalt, and aluminum, and lithium. Examples of the composite oxide include olivine-type lithium iron phosphate (LiFePO 4 ), LiCoO 2 , LiNiMnCoO 2 etc.
[0026] The binder serves to anchor the active material or conductive additive to the surface of the current collector 21 and maintain the conductive network within the electrode. Examples of binders include fluorine-containing resins such as polyvinylidene fluoride, polytetrafluoroethylene, and fluororubber; thermoplastic resins such as polypropylene and polyethylene; imide resins such as polyimide and polyamideimide; alkoxysilyl group-containing resins; acrylic resins containing monomer units such as acrylic acid and methacrylic acid; styrene-butadiene rubber (SBR); carboxymethyl cellulose; alginates such as sodium alginate and ammonium alginate; water-soluble cellulose ester crosslinks; and starch-acrylic acid graft polymers. These binders can be used alone or in combination. Examples of conductive additives include acetylene black, carbon black, and graphite. The positive electrode active material layer 22 may contain a viscosity-adjusting solvent such as N-methyl-2-pyrrolidone (NMP).
[0027] The negative electrode active material layer 23 is provided on the second surface 21b of the current collector 21. The current collector 21 and the negative electrode active material layer 23 provided on the second surface 21b of the current collector 21 constitute the negative electrode of the bipolar electrode 14. The negative electrode active material layer 23 is formed in a rectangular shape at the center of the second surface 21b so that the peripheral edge portion 21c of the current collector 21 is exposed. In one example, the positive electrode active material layer 22 is contained within the region of the negative electrode active material layer 23 when viewed from the stacking direction. In other words, the outer edge of the positive electrode active material layer 22 is slightly smaller than the outer edge of the negative electrode active material layer 23.
[0028] The negative electrode active material layer 23 is a layered member containing a negative electrode active material, a conductive additive, and a binder. Examples of the negative electrode active material include carbon such as graphite, artificial graphite, highly oriented graphite, mesocarbon microbeads, hard carbon, and soft carbon, metal compounds, elements or compounds of such elements that can be alloyed with lithium, and boron-doped carbon. Examples of elements that can be alloyed with lithium include silicon and tin. The conductive additive and binder of the negative electrode active material layer 23 can be the same as those used in the positive electrode active material layer 22.
[0029] To form the positive electrode active material layer 22 and the negative electrode active material layer 23 on the current collector 21, a conventionally known method such as roll coating, die coating, dip coating, doctor blade coating, spray coating, or curtain coating is used. Specifically, an active material, a solvent, and, if necessary, a binder and a conductive additive are mixed to produce a slurry-like active material layer-forming composition, which is then applied to the first surface 21a and the second surface 21b and dried. Examples of the solvent include N-methyl-2-pyrrolidone, methanol, methyl isobutyl ketone, and water. The dried electrode may be compressed to increase electrode density.
[0030] In the electrode stack 12, adjacent bipolar electrodes 14, 14 in the stacking direction are arranged so that the positive electrode active material layer 22 of one bipolar electrode 14 faces the negative electrode active material layer 23 of the other bipolar electrode 14. A separator 15 is arranged between adjacent bipolar electrodes 14, 14 in the stacking direction. In this embodiment, the separator 15 is a sheet-like member having a rectangular shape in a plan view, and prevents short circuits between adjacent bipolar electrodes 14, 14 in the stacking direction.
[0031] The separator 15 has a rectangular shape that is larger than the positive electrode active material layer 22 and the negative electrode active material layer 23 when viewed from the stacking direction, and smaller than the current collector 21. When viewed from the stacking direction, the end 15 a of the separator 15 is located outside the positive electrode active material layer 22 and the negative electrode active material layer 23. In other words, when viewed from the stacking direction, the end 15 a of the separator 15 does not overlap with either the positive electrode active material layer 22 or the negative electrode active material layer 23.
[0032] The separator 15 is formed, for example, in a sheet shape. The separator 15 is, for example, a porous sheet or nonwoven fabric containing a polymer that absorbs and retains an electrolyte. Examples of materials that constitute the separator 15 include polypropylene, polyethylene, polyolefin, and polyester. The separator 15 may have a single-layer structure or a multi-layer structure. In the case of a multi-layer structure, the separator 15 may include, for example, a substrate layer and a pair of adhesive layers, and may be bonded and fixed to the positive electrode active material layer 22 and the negative electrode active material layer 23 by the pair of adhesive layers. The separator 15 may also include a ceramic layer that serves as a heat-resistant layer. The separator 15 may be reinforced with a vinylidene fluoride resin compound.
[0033] The separator 15 is formed by stretching a molten resin using a dry process or a wet process. In this case, the separator 15 has a direction in which it shrinks more and a direction in which it shrinks less, depending on the stretching process. The separator 15 may be rectangular, with the direction in which it shrinks more along its short sides and the direction in which it shrinks less along its long sides. In one example, the separator 15 is formed using a wet process, and the TD (Transverse Direction) direction in which it shrinks more is along its short sides, and the MD (Machine Direction) direction in which it shrinks less is along its long sides.
[0034] Examples of the electrolyte impregnated into the separator 15 include a liquid electrolyte (electrolytic solution) containing a non-aqueous solvent and an electrolyte salt dissolved in the non-aqueous solvent, and a polymer gel electrolyte containing an electrolyte held in a polymer matrix. When the separator 15 is impregnated with an electrolyte, the electrolyte salt may be LiClO. 4 , LiAsF 6 , LiPF 6 , LiBF 4 , LiCF 3 SO 3 , LiN(FSO 2 ) 2 , LiFSi, LiN(CF 3 SO 2 ) 2Known lithium salts such as those listed above can be used. Furthermore, known solvents such as cyclic carbonates, cyclic esters, chain carbonates, chain esters, and ethers can be used as the non-aqueous solvent. These known solvent materials may be used in combination of two or more.
[0035] In addition to the bipolar electrode 14, the electrode laminate 12 also includes a positive terminal electrode 16 and a negative terminal electrode 17. The positive terminal electrode 16 is composed of a current collector 21 and a positive electrode active material layer 22 provided on a first surface 21a of the current collector 21. The positive terminal electrode 16 is disposed at one end of the electrode laminate 12 in the stacking direction, such that the positive electrode active material layer 22 on the first surface 21a faces the negative electrode active material layer 23 of the distal bipolar electrode 14. In the positive terminal electrode 16, the second surface 21b of the current collector 21 is not provided with the positive electrode active material layer 22 or the negative electrode active material layer 23, and the second surface 21b is electrically connected to an adjacent conductive plate (not shown). The current collector 21 used in the positive terminal electrode 16 may be composed of aluminum foil.
[0036] The negative terminal electrode 17 is composed of a current collector 21 and a negative electrode active material layer 23 provided on a second surface 21b of the current collector 21. The negative terminal electrode 17 is arranged on the other end side in the stacking direction of the electrode laminate 12 so that the negative electrode active material layer 23 on the second surface 21b faces the positive electrode active material layer 22 of the terminal bipolar electrode 14. In the negative terminal electrode 17, the first surface 21a of the current collector 21 is not provided with the positive electrode active material layer 22 or the negative electrode active material layer 23, and the first surface 21a is electrically connected to an adjacent conductive plate (not shown). The current collector 21 used in the negative terminal electrode 17 may be made of copper foil.
[0037] The separators 15 are disposed between the bipolar electrodes 14, 14 adjacent to each other in the stacking direction, as well as between the bipolar electrode 14 and the positive terminal electrode 16, and between the bipolar electrode 14 and the negative terminal electrode 17. The separators 15 are disposed to prevent short circuits between the bipolar electrode 14 and the positive terminal electrode 16, and between the bipolar electrode 14 and the negative terminal electrode 17.
[0038] The sealing portion 30 is a member that seals the internal space S between adjacent current collectors 21 in the stacking direction. The sealing portion 30 has electrical insulation properties. The sealing portion 30 is bonded (joined) to the edge portion of the current collector 21. When viewed from the stacking direction, the sealing portion 30 is spaced apart from the positive electrode active material layer 22 and the negative electrode active material layer 23. When viewed from the stacking direction, the sealing portion 30 is frame-shaped and disposed between adjacent current collectors 21 in the stacking direction so as to surround the peripheries of the positive electrode active material layer 22 and the negative electrode active material layer 23. When viewed from the stacking direction, the sealing portion 30 is provided on the peripheral portion 21c of the current collector 21 so as to surround the electrode stack 12. In the energy storage module 11, an internal space S is defined by the sealing portion 30 and adjacent current collectors 21 in the stacking direction. An electrolyte solution (not shown) containing an electrolyte is accommodated in the internal space S. The sealing portion 30 is disposed between the current collectors 21 adjacent to each other in the stacking direction, and thus also functions as a spacer that maintains the distance between the adjacent current collectors 21 .
[0039] An example sealing portion 30 includes a plurality of first sealing layers 31, a plurality of second sealing layers 32, and a plurality of spacer layers 33. The first sealing layers 31, the second sealing layers 32, and the spacer layers 33 each have a rectangular frame shape when viewed in the stacking direction. For example, the thicknesses of the first sealing layers 31 and the second sealing layers 32 (lengths in the stacking direction) may be approximately 50 μm to 200 μm. The thicknesses of the first sealing layers 31 and the second sealing layers 32 may be the same. Furthermore, the thickness of the spacer layers 33 may be thicker than the thicknesses of the first sealing layers 31 and the second sealing layers 32, and may be, for example, approximately 200 μm to 500 μm. The thickness of the spacer layers 33 is defined as the thickness T1 of the linear members 41 described below.
[0040] The first seal layer 31 is bonded to the first surface 21a along the peripheral edge 21c of the current collector 21. In one example, when viewed from the stacking direction, the outer edge 31b of the first seal layer 31 is larger than the edge 21d of the current collector 21 and surrounds the current collector 21. When viewed from the stacking direction, the edge 21d of the current collector 21 is larger than the inner edge 31a of the first seal layer 31 and surrounds the inner edge 31a of the first seal layer 31. The first seal layer 31 and the current collector 21 are bonded to each other in an overlapping region when viewed from the stacking direction. That is, the first seal layer 31 and the current collector 21 are bonded to each other in a region from the inner edge 31a of the first seal layer 31 to the edge 21d of the current collector 21. When viewed from the stacking direction, the inner edge 31a of the first seal layer 31 is spaced from the positive electrode active material layer 22. The first sealing layer 31 is bonded to the first surface 21 a at the peripheral portion 21 c of the current collector 21 so as to extend beyond the edge 21 d of the current collector 21 .
[0041] The second sealing layer 32 is bonded to the second surface 21b along the peripheral edge 21c of the current collector 21. In one example, when viewed in the stacking direction, the outer edge 32b of the second sealing layer 32 is larger than the edge 21d of the current collector 21 and surrounds the current collector 21. For example, the second sealing layer 32 and the current collector 21 are bonded to each other in an overlapping region. That is, the second sealing layer 32 and the current collector 21 are bonded to each other in a region from the inner edge 32a of the second sealing layer 32 to the edge 21d of the current collector 21. When viewed in the stacking direction, the inner edge 32a of the second sealing layer 32 is spaced from the negative electrode active material layer 23. The second sealing layer 32 is bonded to the second surface 21b at the peripheral edge 21c of the current collector 21 so as to protrude beyond the edge 21d of the current collector 21.
[0042] The spacer layer 33 is located between the first seal layer 31 and the second seal layer 32 that are adjacent to each other in the stacking direction. The spacer layer 33, together with the first seal layer 31 and the second seal layer 32, seals the internal space S formed between the current collectors 21 that are adjacent to each other in the stacking direction.
[0043] FIG. 3 is a schematic plan view showing the spacer layer. FIG. 4 is a schematic cross-sectional view taken along line IV-IV in FIG. 3. As shown in FIGS. 3 and 4, the spacer layer 33 has a plurality of straight members 41 and a plurality of joining members 42. The plurality of straight members 41 are arranged spaced apart from one another when viewed from the stacking direction. The straight members 41 are resin members having a region extending linearly. The straight members 41 have a region extending in one direction. A bent portion or a curved portion may be provided at one or both ends of the region extending in one direction. The straight member 41 may have two straight regions extending in different directions, and a bent portion or a curved portion may be provided at the intersection where the two straight regions intersect.
[0044] The joining members 42 are joined to the edges 41a of the linear members 41 so as to fill the gaps between the edges 41a of adjacent linear members 41 as viewed from the stacking direction. The joining members 42 join the edges 41a of adjacent linear members 41 as viewed from the stacking direction. The area of the joining members 42 is smaller than the area of the linear members 41 as viewed from the stacking direction. Because the joining members 42 are formed so as to fill the gaps between adjacent linear members 41, the joining members 42 tend to have a smaller shape than the linear members 41. In this embodiment, of the edges 41a, regions at both longitudinal ends of the linear members 41 are joined to the joining members 42. In this embodiment, the spacer layer 33 has four linear members 41 and four joining members 42. Each of the four sides of the rectangular frame-shaped spacer layer 33 is formed by one linear member 41.
[0045] The plurality of linear members 41 include a pair of linear members 43 extending linearly in the Y-axis direction and a pair of linear members 44 extending linearly in the X-axis direction. The plurality of linear members 41 are arranged such that the linear members 43 and the linear members 44 are adjacent to each other. Each of the pair of linear members 43 has a rectangular shape with its longitudinal direction (or long side direction) in the Y-axis direction when viewed from the stacking direction. When viewed from the stacking direction, the edge 41a of the linear member 43 includes a region 43L that forms the long side of the linear member 43 and a region 43S that forms the short side of the linear member 43. When viewed from the stacking direction, the pair of linear members 43 face each other in the X-axis direction. One linear member 43 forms a liquid inlet side (described later) and is formed wider than the other linear member 43. In other words, the region 43S of one linear member 43 is longer than the region 43S of the other linear member 43.
[0046] Each of the pair of straight members 44 has a rectangular shape with its longitudinal direction (or long side direction) in the X-axis direction when viewed from the stacking direction. That is, in this embodiment, the longitudinal directions of adjacent straight members 41 are perpendicular to each other. When viewed from the stacking direction, the edge 41a of the straight member 44 includes a region 44L that forms the long side of the straight member 44 and a region 44S that forms the short side of the straight member 44. The pair of straight members 44 have the same shape. The region 44S of the pair of straight members 44 has, for example, the same length as the region 43S of the other straight member 43. The pair of straight members 44 face each other in the Y-axis direction.
[0047] In this embodiment, the length of the spacer layer 33 in the X-axis direction is longer than the length of the spacer layer 33 in the Y-axis direction. Similarly, the length of the current collector 21 in the X-axis direction is longer than the length of the current collector 21 in the Y-axis direction. The X-axis direction can be said to be the longitudinal direction (or long side direction) of the spacer layer 33 and the current collector 21. The Y-axis direction can be said to be the lateral direction (or short side direction) of the spacer layer 33 and the current collector 21. Note that the length of the spacer layer 33 in the X-axis direction may be equal to or shorter than the length of the spacer layer 33 in the Y-axis direction. Similarly, the length of the current collector 21 in the X-axis direction may be equal to or shorter than the length of the current collector 21 in the Y-axis direction.
[0048] The joining member 42 joins a region 43L of the edge 41a, which is a side surface that forms the long side of the linear member 43, to a region 44S of the edge 41a, which is a side surface that forms the short side of the linear member 44. In other words, all four corners 33c of the rectangular frame-shaped spacer layer 33 are formed by the linear member 43. As shown by the dashed lines in FIG. 3 , the corners 33c are rectangular portions where the linear member 43 and a region obtained by extending the linear member 44 in the X-axis direction overlap, as viewed from the stacking direction. The length of the corners 33c in the X-axis direction is equal to the length of the linear member 43 in the X-axis direction. The length of the corners 33c in the Y-axis direction is equal to the length of the linear member 44 in the Y-axis direction.
[0049] In this embodiment, the length L2 of the straight member 44 in the longitudinal direction (X-axis direction) is longer than the length L1 of the straight member 43 in the longitudinal direction (Y-axis direction). The thickness T2 of the joining member 42 is thinner than twice the thickness T1 of the straight member 41. The thickness T2 of the joining member 42 is equal to or smaller than the thickness T1 of the straight member 41. In this embodiment, the thickness T2 of the joining member 42 is equal to the thickness T1 of the straight member 41. The joining member 42 is joined only to the end edge 41a of the straight member 41 and is arranged so as not to overlap with the straight member 41 in the stacking direction.
[0050] 4, in this embodiment, a welding layer 40 is provided between the joining member 42 and the edge 41 a of the straight member 41, i.e., at the interface between the joining member 42 and the straight member 41 where they contact each other, where the welding layer 40 fuses the joining member 42 and the straight member 41. That is, the spacer layer 33 includes the welding layer 40 formed at the joint between the joining member 42 and the edge 41 a of the straight member 41, where the welding layer 40 fuses the joining member 42 and the straight member 41.
[0051] As shown in FIGS. 1 and 2 , the first sealing layer 31, the second sealing layer 32, and the spacer layer 33 are welded to one another by edge welds R1. The outer edge 33b of the spacer layer 33 may be located at the same position as the outer edge 31b of the first sealing layer 31 and the outer edge 32b of the second sealing layer 32, as viewed from the stacking direction. The outer edge 33b of the spacer layer 33 may be welded to the outer edge 31b of the first sealing layer 31, outside the edge 21d of the current collector 21, as viewed from the stacking direction. The outer edge 33b of the spacer layer 33 may be welded to the outer edge 32b of the second sealing layer 32, outside the edge 21d of the current collector 21, as viewed from the stacking direction. That is, the first sealing layer 31, the second sealing layer 32, and the spacer layer 33 are integrated and welded to one another by the edge welds R1 in a region outside the edge 21d of the current collector 21.
[0052] The end surface welds R1 are formed by welding together the end portions (peripheral edges) of the plurality of first sealing layers 31, the plurality of second sealing layers 32, and the plurality of spacer layers 33 opposite the internal space S. In other words, the first sealing layer 31 and the spacer layer 33 are not welded to each other except at the end surface welds R1, and are only in contact with each other. Similarly, the second sealing layer 32 and the spacer layer 33 are not welded to each other except at the end surface welds R1, and are only in contact with each other. Because the spacer layer 33 is connected to the first sealing layer 31 and the second sealing layer 32 by the end surface welds R1, stress due to expansion and contraction of the spacer layer 33 can affect the current collector 21 to which the first sealing layer 31 and the second sealing layer 32 are melted and joined.
[0053] The edge weld R1 has a rectangular frame shape surrounding the electrode stack 12 when viewed from the stacking direction. When viewed from the stacking direction, the edge weld R1 is formed outside the edge 21d of the current collector 21. That is, the first seal layer 31, the second seal layer 32, and the spacer layer 33 each have an overlapping portion that overlaps the current collector 21 when viewed from the stacking direction, and an extending portion that extends outside the edge 21d of the current collector 21. The edge weld R1 is provided in the extending portion. The side of the edge weld R1 opposite the internal space S extends along the stacking direction and forms the outer surface of the sealing portion 30. In other words, the sealing portion 30 includes an inner surface facing the internal space S and an outer surface opposite the inner surface.
[0054] The sealing portion 30 has communication holes 35 formed therein that communicate with each of the multiple internal spaces S. As an example, the communication holes 35 are formed by partially cutting out the spacer layer 33 and penetrate the spacer layer 33 and the end surface welded portion R1. The communication holes 35 have one opening in the internal space S and the other opening on the outer surface of the sealing portion 30. In the energy storage module 11, a cell including one internal space S is formed between a pair of adjacent current collectors 21. Here, one communication hole 35 is formed for one cell. The communication hole 35 can be used as a liquid filling port for filling the internal space S with electrolyte. That is, a liquid filling port (opening of the communication hole 35) is provided on the outer surface of the sealing portion 30. In the energy storage module 11 that is rectangular when viewed in the stacking direction, the side on which the communication hole 35 is provided is referred to as the liquid filling port side.
[0055] When viewed from the stacking direction, the inner edge 33a of the spacer layer 33 around the liquid inlet is located more inward (toward the internal space S) than the inner edge 31a of the first seal layer 31 and the inner edge 32a of the second seal layer 32. In this embodiment, the inner edge 33a of the spacer layer 33 around the liquid inlet is located, for example, 1 mm or more inward from the inner edges 31a, 32a and is exposed from the first seal layer 31 and the second seal layer so as to face the internal space S. When viewed from the stacking direction, the inner edge 33a of the spacer layer 33 around the liquid inlet other than the liquid inlet may be located more outward than the inner edge 31a of the first seal layer 31 and the inner edge 32a of the second seal layer 32, or may be located more inward than the inner edge 31a of the first seal layer 31 and the inner edge 32a of the second seal layer 32.
[0056] The end 15a of the separator 15 is fixed to the second seal layer 32 between the second seal layer 32 and the spacer layer 33. It is sufficient that the end 15a of the separator 15 is fixed near the inner edge 32a of the second seal layer 32 when viewed from the stacking direction. The end 15a may be partially adhered (welded) to the second seal layer 32 by, for example, spot welding.
[0057] When viewed from the stacking direction, the first sealing layer 31 is spaced apart from the positive electrode active material layer 22, and the inner edge 31 a is located outside the positive electrode active material layer 22. When viewed from the stacking direction, the second sealing layer 32 is spaced apart from the negative electrode active material layer 23, and the inner edge 32 a is located outside the negative electrode active material layer 23. In this embodiment, when viewed from the stacking direction, the first sealing layer 31 is also spaced apart from the negative electrode active material layer 23, but the first sealing layer 31 may overlap the negative electrode active material layer 23 as long as it is spaced apart from the positive electrode active material layer 22.
[0058] In the stacking direction, the thickness of the first sealing layer 31 and the thickness of the second sealing layer 32 are, for example, thinner than the thickness of the spacer layer 33. As described above, the thickness of the spacer layer 33 is the thickness T1 of the straight member 41. The thickness of the first sealing layer 31 is the thickness of a portion of the first sealing layer 31 that is sandwiched between the current collector 21 and the spacer layer 33. The thickness of the second sealing layer 32 is the thickness of a portion of the second sealing layer 32 that is sandwiched between the current collector 21 and the spacer layer 33.
[0059] The thickness of the spacer layer 33 is the thickness of the portion of the linear member 41 sandwiched between the first seal layer 31 and the second seal layer 32. The thicknesses of the first seal layer 31 and the second seal layer 32 may be, for example, 1 / 10 to 1 / 2 of the thickness of the spacer layer 33. The thicknesses of the first seal layer 31 and the second seal layer 32 may be, for example, equal to or different from each other. The thicknesses of the first seal layer 31 and the second seal layer 32 may be thicker than the thickness of the spacer layer 33.
[0060] The first sealing layer 31, the second sealing layer 32, and the spacer layer 33 are made of an electrolyte-resistant resin material, such as acid-modified polyethylene (acid-modified PE), acid-modified polypropylene (acid-modified PP), polyethylene, or polyethylene. The resin materials making up the first sealing layer 31, the second sealing layer 32, and the spacer layer 33 may be the same or different. Here, the same resin material means that the type of resin material is the same, for example, acid-modified polyethylene, acid-modified polypropylene, polyethylene, or polyethylene. If the type of resin material is the same, it is treated as the same resin material even if the average molecular weight or melt flow rate is different.
[0061] The melt flow rate is an index that indicates the fluidity of a molten resin. In JIS K7210, the melt flow rate is divided into two parts: the melt mass flow rate (MFR) expressed in g / 10 min and the melt mass flow rate (MFR) expressed in cm 3 There are two types of melt flow rates: melt volume flow rate (MVR) expressed in units of 1 / 10 min and melt mass flow rate (MFR). The melt flow rate used in this embodiment is melt mass flow rate (MFR). In this embodiment, the first seal layer 31 and the second seal layer 32 are made of acid-modified polyethylene or acid-modified polypropylene. The spacer layer 33 is made of polyethylene or polypropylene.
[0062] The straight member 41 and the connecting member 42 are formed so that the MFR of the connecting member 42 is greater than the MFR of the straight member 41. The MFR is determined in accordance with JIS K7210. Each MFR is adjusted, for example, by the molecular weight of the constituent materials. For example, the MFR of the straight member 41 is 0.5 g / 10 min or more at a temperature of 190° C. and a load of 2.16 kgf, and the MFR of the connecting member 42 is 20 g / 10 min or less at a temperature of 190° C. and a load of 2.16 kgf.
[0063] The straight members 41 and the joining members 42 may be made of, for example, the same resin material. That is, both the straight members 41 and the joining members 42 may be made of, for example, polyethylene or polypropylene. In this case, the straight members 41 and the joining members 42 may be formed such that the average molecular weight of the joining members 42 is smaller than the average molecular weight of the straight members 41. This makes it easy to achieve a configuration in which the MFR of the joining members 42 is greater than the MFR of the straight members 41.
[0064] The linear members 41 are obtained, for example, by punching or cutting a long sheet material unwound from a roll. The joining members 42 are, for example, injection-molded members formed by injection molding. By forming the joining members 42 between the edges 41 a of adjacent linear members 41 (in this embodiment, between the region 43L of the linear member 43 and the region 44S of the linear member 44), the linear members 41 are connected to each other, and the spacer layer 33 is formed.
[0065] A method for forming the spacer layer 33 will be described with reference to Fig. 5 to Fig. 7. Fig. 5 is a flowchart showing the method for forming the spacer layer 33. Fig. 6 is a schematic plan view for describing the method for forming the spacer layer 33. Fig. 7 is a schematic side view for describing the method for forming the spacer layer 33.
[0066] As shown in FIG. 5 , the method for forming the spacer layer 33 includes a first preparation step S1, a placement step S2, a second preparation step S3, a third preparation step S4, an injection molding step S5, and a removal step S6. As shown in FIG. 6 , the first preparation step S1 is a step of placing either a first intermediate mold M3a or a second intermediate mold M3b at a predetermined position on the lower mold M1. The lower mold M1 is a mold that functions as a mounting table. The first intermediate mold M3a and the second intermediate mold M3b are molds having the same thickness as the straight member 41, for example. In this embodiment, the first intermediate mold M3a is provided with an injection port Mh for injecting resin. The injection port Mh may also be provided in the second intermediate mold M3b.
[0067] The arrangement step S2 is a step of arranging multiple straight members 41 at predetermined positions on the lower mold M1 while aligning them using either the first intermediate mold M3a or the second intermediate mold M3b arranged in the first preparation step S1. The second preparation step S3 is a step of arranging the remaining mold, either the first intermediate mold M3a or the second intermediate mold M3b, at predetermined positions on the lower mold M1. The third preparation step S4 is a step of arranging the upper mold M2 on the lower mold M1 so as to sandwich the multiple straight members 41, the first intermediate mold M3a, and the second intermediate mold M3b, as shown in FIG.
[0068] The injection molding process S5 is a process of filling the space defined by the multiple straight members 41, the first intermediate mold M3a, the second intermediate mold M3b, the lower mold M1, and the upper mold M2 with resin to form the joining members 42. The resin is injected in a molten state through the injection port Mh. The joining members 42 formed by the injected resin are formed to join the edges 41a of the multiple straight members 41 together. This forms the spacer layer 33 in which the multiple straight members 41 are joined by the joining members 42. Note that the multiple joining members 42 may be formed simultaneously or sequentially. The removal process S6 is a process of removing the upper mold M2, the first intermediate mold M3a, and the second intermediate mold M3b and removing the spacer layer 33.
[0069] The thickness T2 of the joining member 42 can be set appropriately depending on the shape of the lower surface of the upper mold M2. As shown in Fig. 7, by making the lower surface of the upper mold M2 flat, the thickness T2 can be made equal to the thickness T1 of the straight member 41. By providing a convex portion on the lower surface of the upper mold M2, the thickness T2 can be made thinner than the thickness T1. By providing a concave portion on the lower surface of the upper mold M2, the thickness T2 can be made thicker than the thickness T1.
[0070] The method for manufacturing the energy storage module 11 includes the step of forming the spacer layer 33 as described above.
[0071] As described above, in the energy storage module 11, each spacer layer 33 included in the resin sealing portion 30 is formed into a rectangular frame shape by joining the edges 41 a of the linear members 41 with the joining members 42. The linear members 41, each having a linearly extending region, are resin members formed by cutting a long sheet material at regular intervals. When a long sheet material unwound from a raw roll is punched into a rectangular frame shape, the central portion of the punched sheet material is discarded. However, when the edges 41 a of the linear members 41 are joined with the joining members 42 to form the rectangular frame-shaped spacer layer 33 as in the present embodiment, there is no need to punch the long sheet material into a rectangular frame shape, thereby reducing discard. In particular, when the size of the electrodes increases, the discard reduction effect is greater compared to punching into a rectangular frame shape. In other words, in this embodiment, the sheet material is easily utilized without waste. Such a spacer layer 33 can prevent an increase in the sheet material waste rate. Therefore, a decrease in the productivity of the energy storage module 11 can be prevented.
[0072] A spacer layer 50 of a comparative example will be described with reference to FIGS. 8 and 9 . FIG. 8 is a schematic plan view showing the spacer layer of the comparative example. FIG. 9 is a schematic cross-sectional view taken along line IX-IX in FIG. 8 . As shown in FIGS. 8 and 9 , the spacer layer 50 of the comparative example is formed into a rectangular frame shape by connecting four rectangular resin members 51 with welded portions 52. The welded portions 52 are formed by overlapping and welding the longitudinal ends of adjacent resin members 51 together. Therefore, the welded portions 52 are thicker than other portions. Therefore, a sealing portion including multiple stacked spacer layers 50 may have large thickness variations due to the welded portions 52, which may result in reduced sealing performance. Furthermore, the welded portions 52 may not only have upwardly protruding convex portions, but may also have concave portions between the edge of the underlying resin member 51 and the overlying resin member 51.
[0073] In contrast, in the energy storage module 11 of this embodiment, each spacer layer 33 included in the sealing portion 30 is not formed by overlapping and welding longitudinal ends of the straight members 41 together, but is formed by joining the end edges 41 a of the straight members 41 together with the joining members 42. Such spacer layers 33 can suppress variations in the thickness of the sealing portion 30, and therefore suppress deterioration of the sealing performance of the sealing portion 30.
[0074] The joining members 42 are injection-molded members, and between the joining members 42 and the edges 41a of the straight members 41 there is a welding layer 40 through which the joining members 42 and the straight members 41 are fused together. Therefore, regardless of the shape of the edges 41a of the straight members 41, the joining members 42 can be produced by injection molding resin into the gaps between the edges 41a of the straight members 41. Because the joining members 42 and the straight members 41 are fused together in the welding layer 40, the bonding strength between the straight members 41 and the joining members 42 can be improved. Therefore, defects in the energy storage module 11 due to insufficient bonding between the straight members 41 and the joining members 42 can be suppressed.
[0075] The MFR of the joining members 42 is greater than the MFR of the straight members 41. Therefore, for example, when forming the joining members 42 by pouring resin into the gaps between the edges 41 a of adjacent straight members 41 by injection molding or potting, even if the gaps between the edges 41 a of adjacent straight members 41 are made small, the joining members 42 easily fill the gaps because of their large MFR. Therefore, such a spacer layer 33 allows the joining members 42 to be positioned with precision.
[0076] The straight members 41 and the joining members 42 may be made of the same resin material. The average molecular weight of the joining members 42 may be smaller than that of the straight members 41. When the average molecular weight of the joining members 42 is smaller than that of the straight members 41, it is easy to realize a configuration in which the MFR of the joining members 42 is larger than that of the straight members 41.
[0077] The thickness T2 of the joining members 42 is equal to or less than the thickness T1 of the straight members 41. Therefore, unlike the spacer layer 50 of the comparative example, which is formed by overlapping and welding the ends of the resin members 51, the spacer layer 33 does not have locally thick portions. This makes it possible to suppress variations in the thickness of the sealing portion 30. If the thickness T2 of the joining members 42 is thinner than the thickness T1 of the straight members 41, the amount of resin in the joining members 42 is reduced, which is expected to suppress cost increases.
[0078] The plurality of linear members 41 include a pair of linear members 43 and a pair of linear members 44. The joining member 42 joins a region 43L of the end edge 41a that forms the long side of the linear member 43 to a region 44S of the end edge 41a that forms the short side of the linear member 44. Therefore, the spacer layer 33 can be formed by four linear members 41 and four joining members 42.
[0079] Length L2 is longer than length L1. Therefore, the thermal contraction of linear member 44 in the longitudinal direction (X-axis direction) is greater than the thermal contraction of linear member 43 in the longitudinal direction (Y-axis direction). Joining member 42 joins region 43L and region 44S. Therefore, corner portions 33c of rectangular frame-shaped spacer layer 33 are formed by short linear member 43.
[0080] (First Modification) Fig. 10 is a schematic plan view showing a spacer layer according to a first modification. In the above embodiment, as shown in Fig. 3, each side of the rectangular frame-shaped spacer layer 33 is formed by one straight member 41. In contrast, in the first modification, as shown in Fig. 10, each side of the rectangular frame-shaped spacer layer 33A is formed by a plurality of straight members 41. In this modification, each side of the spacer layer 33A is formed by a pair of straight members 41. The spacer layer 33A has a total of eight straight members 41.
[0081] The eight straight members 41 include four straight members 45 that extend linearly in the Y-axis direction and four straight members 46 that extend linearly in the X-axis direction. When viewed from the stacking direction, the straight members 45 are rectangular in shape with their longitudinal direction (or long side direction) in the Y-axis direction. When viewed from the stacking direction, the edge 41 a of each straight member 45 includes a region 45L that forms the long side of the straight member 45 and a region 45S that forms the short side of the straight member 45. When viewed from the stacking direction, the straight member 46 is rectangular in shape with its longitudinal direction (or long side direction) in the X-axis direction. When viewed from the stacking direction, the edge 41 a of each straight member 46 includes a region 46L that forms the long side of the straight member 46 and a region 46S that forms the short side of the straight member 46.
[0082] Each side of the spacer layer 33A is composed of either a pair of linear members 45 or a pair of linear members 46. That is, the multiple linear members 41 include two pairs of linear members 45 and two pairs of linear members 46. The longitudinal directions (long side directions) of the two pairs of linear members 45 coincide with each other when viewed from the stacking direction. The two pairs of linear members 45 are adjacent to each other in the longitudinal direction (long side direction) when viewed from the stacking direction. The longitudinal directions (long side directions) of the two pairs of linear members 46 coincide with each other when viewed from the stacking direction. The two pairs of linear members 46 are adjacent to each other in the longitudinal direction (long side direction). A pair of linear members 41 constituting the same side of the spacer layer 33, i.e., a pair of linear members 45 or a pair of linear members 46, have the same shape. In a pair of linear members 45 constituting the same side of the spacer layer 33, regions 45S are joined by a joining member 42. In a pair of linear members 46 that form the same side of the spacer layer 33, the regions 46S are joined together by the joining member 42. In adjacent linear members 45 and 46, the regions 45L and 46S are joined together by the joining member 42.
[0083] Unlike the above embodiment, in this modification, the longitudinal directions of adjacent linear members 41 may be perpendicular to each other or may be aligned with each other. According to this modification, a large spacer layer 33A can be formed by joining short linear members 45, 46. While the example shown here illustrates a case where each side of the spacer layer 33A is made up of multiple linear members 41, one side of the spacer layer 33A may also be made up of multiple linear members 41. Furthermore, a pair of linear members 41 that make up the same side of the spacer layer 33A may have different shapes.
[0084] (Second Modification) FIG. 11 is a schematic plan view showing a spacer layer according to a second modification. As shown in FIG. 11, a spacer layer 33B according to the second modification differs from the spacer layer 33 (see FIG. 3) in that the bonding members 42 form the entire corners 33c of the spacer layer 33. When viewed from the stacking direction, the shape of the bonding members 42 matches the shape of the corners 33c. In the spacer layer 33B, the multiple linear members 41 include a pair of linear members 47 and a pair of linear members 48. The linear members 47 differ from the linear members 43 (see FIG. 3) in that they do not form the corners 33c. The length L5 of the linear members 47 in the longitudinal direction (Y-axis direction) is shorter than the length L1 of the linear members 43 by the length of the corners 33c. The linear members 48 differ from the linear members 44 (see FIG. 3) in that they extend to the corners 33c. A length L6 of the straight member 48 in the longitudinal direction (X-axis direction) is longer than the length L2 of the straight member 44. The length L6 is longer than the length L5.
[0085] When viewed from the stacking direction, edge 41a of straight member 47 includes region 47L forming the long side of straight member 47 and region 47S forming the short side of straight member 47. When viewed from the stacking direction, edge 41a of straight member 48 includes region 48L forming the long side of straight member 48 and region 48S forming the short side of straight member 48. Joining member 42 joins region 47S of edge 41a forming the short side of straight member 47 and region 48S of edge 41a forming the short side of straight member 48. In this modification as well, the number of straight members 41 is minimized, and therefore the productivity of energy storage module 11 can be improved.
[0086] Although an example embodiment of the present disclosure has been described in detail above, the present disclosure is not limited to the above embodiment and modifications.
[0087] The joining member 42 may not be an injection-molded member, but may be a member formed by a method other than injection molding. For example, as shown in Fig. 6, after the straight member 41 is placed on the lower mold M1 together with the first intermediate mold M3a and the second intermediate mold M3b, the upper mold M2 is not placed, and resin is poured from above into the gap between the edges 41a of the straight member 41 to form the joining member 42. In this case, the first intermediate mold M3a and the second intermediate mold M3b that are not provided with the injection port Mh can be used.
[0088] In the spacer layer 33, the pair of linear members 43 may have the same shape as each other. The length of the region 43S of the pair of linear members 43 may be equal to the length of the region 44S of the pair of linear members 44.
[0089] The number of straight members 41 may be plural. The joining member 42 may join the region 43S of the straight member 43 and the region 44L of the straight member 44. The longitudinal length L2 of the straight member 44 may be shorter than the longitudinal length L1 of the straight member 43. The straight member 41 and the joining member 42 may be made of different resin materials. The straight member 41 may have a region that extends linearly, and may have a shape other than a rectangular shape, such as an L-shape or a U-shape.
[0090] The configuration of the spacer layer 33 can also be applied to the first sealing layer 31 and the second sealing layer 32. That is, each of the first sealing layer 31 and the second sealing layer 32 may include a plurality of straight members arranged spaced apart from each other when viewed in the stacking direction, and a joining member that joins the edges of adjacent straight members together.
[0091] DESCRIPTION OF SYMBOLS 11... Energy storage module, 12... Electrode laminate (laminate), 14... Bipolar electrode, 21... Current collector, 21a... First surface, 21b... Second surface, 21c... Peripheral portion, 22... Positive electrode active material layer, 23... Negative electrode active material layer, 30... Sealing portion, 31... First seal layer, 32... Second seal layer, 33, 33A, 33B... Spacer layer, 40... Welding layer, 41... Linear member, 41a... Edge, 42...joint member, 43...straight member, 43L...region, 43S...region, 44...straight member, 44L...region, 44S...region, 45...straight member, 45L...region, 45S...region, 46...straight member, 46L...region, 46S...region, 47...straight member, 47L...region, 47S...region, 48...straight member, 48L...region, 48S...region, S...internal space.
Claims
1. An energy storage module comprising: a stack of a plurality of electrodes, each having a rectangular current collector; and a resin sealing portion provided on a peripheral portion of the current collector so as to surround the stack when viewed from a stacking direction of the plurality of electrodes, wherein each of the plurality of electrodes has an active material layer on a first surface and a second surface opposite to the first surface of the current collector, the sealing portion including a plurality of rectangular frame-shaped sealing layers and a plurality of rectangular frame-shaped spacer layers, the plurality of sealing layers being joined to the first surface and the second surface at the peripheral portion of the current collector of each of the plurality of electrodes, each of the plurality of spacer layers being located between adjacent sealing layers in the stacking direction and sealing an internal space formed between adjacent current collectors in the stacking direction together with the plurality of sealing layers, the plurality of straight members being arranged spaced apart from each other when viewed from the stacking direction, each having a region extending in a straight line, and a joining member being joined to the edges so as to fill a gap between edges of adjacent straight members.
2. The energy storage module according to claim 1, wherein the joining member is an injection molded member, and each of the spacer layers has a welding layer formed at the joint between the joining member and the edge of the straight member, through which the joining member and the straight member are fused to each other.
3. The energy storage module according to claim 1 or 2, wherein the joining members are injection molded members, and the melt flow rate of the joining members is greater than the melt flow rate of the straight members.
4. The energy storage module according to any one of claims 1 to 3, wherein an area of the joining members is smaller than an area of the straight members when viewed in the stacking direction.
5. The energy storage module according to any one of claims 1 to 4, wherein the thickness of the joining members is equal to or less than the thickness of the straight members.
6. The energy storage module according to any one of claims 1 to 5, wherein the plurality of straight members include a pair of rectangular first straight members facing each other in a first direction as viewed from the stacking direction, and a pair of rectangular second straight members facing each other in a second direction perpendicular to the first direction as viewed from the stacking direction, and the joining member joins a region of the edge forming a long side of the first straight members and a region of the edge forming a short side of the second straight members.
7. The energy storage module according to any one of claims 1 to 5, wherein the plurality of straight members include a pair of rectangular first straight members facing each other in a first direction as viewed from the stacking direction, and a pair of rectangular second straight members facing each other in a second direction perpendicular to the first direction as viewed from the stacking direction, and the joining member joins a region of the edge that forms a short side of the first straight members and a region of the edge that forms a short side of the second straight members.
8. The energy storage module according to any one of claims 1 to 7, wherein the plurality of straight members include a pair of straight members whose longitudinal directions coincide with each other when viewed from the stacking direction and which are adjacent to each other in the longitudinal direction.
Citation Information
Patent Citations
Method for manufacturing power storage module and power storage module
JP2019040792A
Manufacturing method of power storage module
JP2020087870A
Power storage module
JP2020135931A
Power storage device
JP2023045567A