Manufacturing method for container products

Through mold design and gas pressure technology controlled by the blowing port, a honeycomb-like plastic cup is formed, which solves the problems of poor insulation and manufacturing complexity of the plastic cup, and achieves better thermal insulation effect and improved appearance texture.

WO2024239240A1PCT designated stage expired Publication Date: 2024-11-28APLUS MOLDS & PLASTICS
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
PCT/CN2023/095827
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-23
Publication Date
2024-11-28

AI Technical Summary

Technical Problem

The existing plastic cups have poor thermal insulation, which causes the temperature of the hot drink to be transmitted outside the cup, causing discomfort in the hands. At the same time, local temperature control methods increase manufacturing complexity and difficult to control.

Method used

Using a mold design, including the first and second components, the plastic composition forms a micro-foaming and foaming zone in different areas by injecting a molten plastic composition with polymer and foaming agent, and controlling the gas pressure using the blowing nozzle, the plastic composition forms a micro-foaming and foaming zone in different areas. Form a honeycomb structure to improve thermal insulation while simplifying temperature control.

Benefits of technology

It achieves better thermal insulation and appearance texture, while reducing manufacturing complexity and improving product consistency and quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2023095827_28112024_PF_FP_ABST
    Figure CN2023095827_28112024_PF_FP_ABST
Patent Text Reader

Abstract

The present invention relates to a manufacturing method for container products, which comprises the following steps: S1: providing a mold, the mold comprising a first part and a second part; S2: closing the mold so as to define a cavity, the cavity forming a first region and a second region; S3: injecting into the cavity a molten plastic composition containing a polymer and a physical foaming agent under an injection pressure; S4: cooling the molten plastic composition in the mold cavity, such that the molten plastic composition in the first region is completely cooled and cured or there is a tiny amount of the non-cooled molten plastic composition in the center of same, while the molten plastic composition in the second region is in the molten state; S5, enabling the first part of the mold to move axially, and enabling the second region to undergo foaming expansion so as to form a honeycomb foam body; S6, a step of cooling; and S7, a step of opening the mold. On this basis, the present invention can easily control shapes and foam thickness of container products and can improve the texture of containers.
Need to check novelty before this filing date? Find Prior Art

Description

Container product manufacturing method Technical Field

[0001] The present invention relates to a method for manufacturing container products, mainly referring to a method for manufacturing cup-shaped container products by melting and molding polymer and foaming agent. Background Art

[0002] Currently, injection-molded plastic cups are commonly used as disposable cups. To reduce costs, the plastic cups must be thick enough to hold beverages. However, these thin plastic cups have poor thermal insulation. When hot beverages are placed in the cups, the heat is transferred to the outside of the cup, causing discomfort to the hands.

[0003] In order to improve the poor thermal insulation of the plastic cup, the current manufacturing of the plastic cup can be formed by forming a molten plastic composition consisting of a polymer and a foaming agent, and after molding, a plastic cup with thicker foam can be formed, which can provide better thermal insulation effect than a plastic cup without foam.

[0004] However, if the entire plastic cup is foamed with a relatively thick layer, the appearance will lack a variety of textures. For example, the plastic cup of US Pat. No. 11,446,849 uses a temperature-controlled method to cool a portion of the mold to prevent foaming in the cooled portion, while other uncooled portions can foam, thereby forming a plastic cup with both foamed and unfoamed layers. However, this localized cooling method increases manufacturing complexity and is difficult to control.

[0005] Summary of the Invention

[0006] The object of the present invention is to provide a method for manufacturing a container product that reduces manufacturing complexity and enables the product to have better thermal insulation effect and appearance texture, comprising the following steps.

[0007] S1: A mold is provided, wherein the mold includes a first component and a second component. The first component has a first surface, the second component has a second surface, and the second component has an air blowing port.

[0008] S2: The mold is closed to define a cavity between the first surface and the second surface, the cavity having an approximately conical annular cavity portion, the annular cavity portion having a first end corresponding to the axial direction, a second end corresponding to the axial direction with a smaller diameter than the first end, the second end having a bottom cavity portion corresponding to the axial direction, and the cavity having a first area and a second area, the distance between the first surface and the second surface corresponding to the first area being smaller than the distance between the first surface and the second surface corresponding to the second area; and the two ends of the second area corresponding to the axial direction being connected to the first area.

[0009] S3: injecting a molten plastic composition comprising a polymer and a physical foaming agent into the cavity under injection pressure.

[0010] S4: The molten plastic composition in the cavity is cooled so that the first zone can be completely cooled and solidified or a small amount of uncooled molten plastic composition is present in the center; and the second zone contacts the first surface and the second surface and has a first solid skin layer and a second solid skin layer respectively, with a molten plastic composition between the first solid skin layer and the second solid skin layer, and the molten plastic composition in the aforementioned cavity is exposed to a pressure greater than the gas pressure that maintains the physical foaming agent dissolved in the polymer, so that the molten plastic compositions in the first zone and the second zone do not foam.

[0011] S5: The blowing port blows air to make the plastic composition adhere to the first surface of the first component, and the blowing is stopped after adhesion. The first component of the mold is axially displaced, and the molten plastic composition in the cavity is exposed to a gas pressure less than the gas pressure that maintains the physical foaming agent dissolved in the polymer, so that the distance between the first surface and the second surface of the mold corresponding to the second zone position increases accordingly. At this time, the first solid skin layer is still in contact with the first surface, and the central molten plastic composition of the second zone is foamed and expanded to form a honeycomb foam body, and the second solid skin layer can be in contact with the second surface; the plastic composition of the first zone is in contact with the first surface, and the first zone has been solidified or can only form micro-bubbles. The shape and thickness of the first zone remain basically unchanged or the thickness increases only slightly, and the first zone restricts the second zone from expanding only toward the first surface.

[0012] S6: Cooling step, cooling the foamed container product in the mold to shape it.

[0013] S7: a mold opening step, wherein the first component and the second component of the mold are separated and the container product is taken out.

[0014] In one embodiment of the present invention, the first area is the bottom cavity portion and the portion of the annular cavity portion from the first end toward the second end; and the second area is the portion of the annular cavity portion from the first area to the bottom cavity portion.

[0015] The manufacturing method of the present invention does not require complex temperature control and can control the thickness of the container in conjunction with the displacement distance of the first component of the mold, thereby achieving better manufacturing quality, yield rate and product consistency. The container manufactured by the present invention has an annular wall, a bottom wall below the annular wall, and an opening above the annular wall. The annular wall is approximately a tapered surface with a gradually decreasing diameter from the upper opening to the lower bottom wall. The top and bottom wall of the annular wall are micro-foamed areas corresponding to the first area of ​​the mold. The annular wall has a foamed area corresponding to the second area of ​​the mold between the micro-foamed area at the top and the bottom wall. The thickness of the foamed area is greater than that of the micro-foamed area and can enhance the appearance and texture of the container product. The thicker foamed area can also provide better thermal insulation.

[0016] The present invention will be more clearly understood following the detailed description which, taken in conjunction with the accompanying drawings, illustrates illustrative embodiments of the invention. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] FIG1 is a schematic cross-sectional view of the mold closing and injection of the molten plastic composition according to the present invention.

[0018] FIG2 is a schematic cross-sectional view of the axial displacement of the first component of the mold of the present invention.

[0019] FIG3 is a schematic diagram of the first zone micro-foaming and the second zone foaming of the present invention.

[0020] FIG4 is a schematic diagram of a container product of the present invention.

[0021] Explanation of the accompanying drawings: 1 mold; 11 first component; 111 first surface; 12 second component; 121 second surface; 122 blowing port; 123 breathable block; 13 cavity; 14 annular cavity portion; 141 first end; 142 second end; 15 bottom cavity portion; 16 first zone; 17 second zone; 2 plastic composition; 21 gas; 22 first solid skin layer; 23 second solid skin layer; 24 foam; 3 container; 31 annular wall; 32 bottom wall; 33 opening; 34 micro-foaming zone; 35 foaming zone.

[0022] DETAILED DESCRIPTION

[0023] 1 to 3 , the container product manufacturing method of the present invention includes the following steps.

[0024] S1: Set up a mold 1, which includes a first component 11 and a second component 12. The first component 11 has a first surface 111, and the second component 12 has a second surface 121. The second component 12 has an air outlet 122, and the air outlet 122 has a breathable block 123 at a position corresponding to the second surface 121.

[0025] S2: The mold 1 is closed, and a cavity 13 is defined between the first surface 111 and the second surface 121. The cavity 13 has an approximately conical annular cavity portion 14, wherein Figures 1 and 2 only show a partial cross-section of the mold 1. The annular cavity portion 14 has a first end 141 corresponding to the axial direction, a second end 142 corresponding to the axial diameter smaller than the first end 141, and the second end 142 has a bottom cavity portion 15 corresponding to the axial direction. The blowing direction of the blowing port 122 corresponds to the bottom cavity portion 15. The cavity 13 also has a first area 16 and a second area 17. The second area 17 is connected to the first area 16 at its two axial ends. In this embodiment, the bottom cavity portion 15 and the portion of the annular cavity portion 14 from the first end 141 to the second end 142 form the first area 16. The second area 17 is formed in the annular cavity portion 14 from the first area 16 to the bottom cavity portion 15. A distance D1 between the first area 16 and the second surface 111 , 121 is smaller than a distance D2 between the second area 17 and the first surface 111 , 121 . In this embodiment, D1 may be approximately 0.5 mm, and D2 may be approximately 1 mm.

[0026] S3: A molten plastic composition 2 comprising a polymer and a physical foaming agent is injected into the cavity 13 under injection pressure, wherein the physical foaming agent is a gas 21 that dissolves the polymer, wherein the polymer may be polypropylene, and the foaming agent may be nitrogen, and the breathable block 123 may prevent the molten plastic composition 2 from flowing into the blowing port 122.

[0027] S4: The molten plastic composition 2 in the cavity 13 of the mold 1 is cooled so that the first zone 16 can be completely cooled and solidified or a small amount of uncooled molten plastic composition 2 is present in the center. The second zone 17 contacts the first surface 111 and the second surface 121 and has a first solid skin layer 22 and a second solid skin layer 23 as shown in Figures 2 and 3 respectively. The molten plastic composition 2 is present between the first solid skin layer 22 and the second solid skin layer 23.

[0028] The molten plastic composition 2 in the cavity 13 is exposed to a pressure of the gas 21 greater than the pressure required to maintain the physical foaming agent dissolved in the polymer, so that the molten plastic composition 2 in the first zone 16 and the second zone 17 does not foam.

[0029] Furthermore, the step S4 cools the first zone 16 and the second zone 17 at the same cooling temperature. Since the thickness D1 of the first zone 16 is small, the first zone 16 can be solidified or almost completely solidified by the cooling temperature, with only a small portion of the molten plastic composition 2 incompletely cooled in the center.

[0030] S5: The air port 122 blows air to adhere the plastic composition 2 to the first surface 111 of the first component 11. After adhesion, the air blowing stops. The first component 11 of the mold 1 is then axially displaced, and the molten plastic composition 2 in the cavity 13 is exposed to a pressure less than that of the gas 21 required to maintain the physical foaming agent dissolved in the polymer. This causes the distance D3 between the first surface 111 and the second surface 121 of the mold 1 corresponding to the second region 17 to increase accordingly. At this point, the first solid skin layer 22 still contacts the first surface 111. The molten plastic composition 2 in the center of the second region 17 expands and foams to form a honeycomb foam 24. The second solid skin layer 23 contacts the second surface 121. The displacement distance of the first component 11 defines the shape and thickness of the second region 17. In this embodiment, the thickness D3 of the foamed plastic composition 2 in the second region 17 is approximately 2.3 mm.

[0031] Because the first region 16 has already solidified or contains only a small amount of molten plastic composition 2 in its center, it can only form micro-foaming. The plastic composition 2 in the first region 16 remains in contact with the first surface 111, but cannot expand to contact the second surface 121. The shape and thickness of the first region 16 remain essentially unchanged, or the thickness increases only slightly. Furthermore, because the first region 16 is essentially fixed before the first component 11 is displaced, the molten plastic composition 2 in the second region 17 is limited to foaming and expanding toward the second surface 121 and does not expand axially toward the mold 1, thereby improving the shape stability of the container product.

[0032] S6: Cooling step, cooling the foamed container product in the mold 1 to set the shape, wherein the cooling method is to cool the first area 16 and the second area 17 to the same cooling temperature or to cool naturally at room temperature.

[0033] S7: a mold opening step, wherein the first component 11 and the second component 12 of the mold 1 are separated and the container product is taken out.

[0034] Referring to Figures 1 to 4 , a container 3 manufactured by the manufacturing method of the present invention comprises an annular wall 31 having a bottom wall 32 at its lower portion and an opening 33 at its upper portion. The annular wall 31 is tapered from the upper opening 33 to the lower bottom wall 32 in a gradually decreasing diameter manner. Furthermore, a micro-foamed region 34 corresponding to the first region 16 of the mold 1 is formed at the top portion of the annular wall 31 and the bottom wall 32. A foamed region 35 corresponding to the second region 17 of the mold 1 is formed between the micro-foamed region 34 at the top of the annular wall 31 and the bottom wall 32. The foamed region 35 is thicker than the micro-foamed region 34 and enhances the appearance and texture of the container 3 product. Furthermore, the thicker foamed region 35 provides better thermal insulation.

[0035] The present invention can control the foam thickness of the foaming area of ​​the container by the displacement distance of the first component of the mold, which can easily control the shape and thickness of the container. The present invention does not require different temperature controls in different areas, which can reduce manufacturing complexity and achieve better quality, yield and product consistency. In addition, the container has foaming areas and micro-foaming areas at different positions, which can achieve better product texture.

[0036] The aforementioned embodiments are illustrative of the present invention and are not intended to limit the present invention. Any equivalent modifications based on the spirit of the present invention should also fall within the scope of the present invention.

Claims

1. A method for manufacturing a container product, characterized in that: The following steps are involved: S1: a mold is provided, the mold comprising a first component and a second component, the first component has a first surface, the second component has a second surface, and the second component has a blowing port; S2: The mold is closed, and a cavity is defined between the first surface and the second surface, the cavity has an approximately conical annular cavity portion, the annular cavity portion has a first end corresponding to the axial direction, a second end corresponding to the axial direction with a smaller diameter than the first end, the second end has a bottom cavity portion corresponding to the axial direction and vertical, and the cavity has a first area and a second area, the distance between the first area corresponding to the first surface and the second surface is smaller than the distance between the second area corresponding to the first surface and the second surface; and the two ends of the second area corresponding to the axial direction are connected to the first area; S3: injecting a molten plastic composition comprising a polymer and a physical foaming agent into the cavity under injection pressure; S4: The molten plastic composition in the cavity is cooled so that the first zone can be completely cooled and solidified or has a small amount of uncooled molten plastic composition in the center; the second zone contacts the first surface and the second surface respectively and has a first solid skin layer and a second solid skin layer, and there is a molten plastic composition between the first solid skin layer and the second solid skin layer, and the molten plastic composition in the cavity is exposed to a pressure greater than the gas pressure that maintains the physical foaming agent dissolved in the polymer, so that the molten plastic composition in the first zone and the second zone does not foam; S5: The blowing port blows air to make the plastic composition adhere to the first surface of the first component, and the blowing is stopped after the adhesion, and the first component of the mold is axially displaced, and the molten plastic composition in the cavity is exposed to a gas pressure less than the gas pressure that maintains the physical foaming agent dissolved in the polymer, so that the distance between the first surface and the second surface of the mold corresponding to the second zone position increases accordingly, at this time, the first solid skin layer still contacts the first surface, and the central molten plastic composition of the second zone is expanded by foaming to form a honeycomb foam body, and the second solid skin layer can contact the second surface; the plastic composition of the first zone contacts the first surface, and the first zone has been solidified or can only form micro-foams, so the shape and thickness of the first zone are basically unchanged or the thickness is only slightly increased, and the first zone restricts the second zone to expand only toward the second surface; S6: cooling step, cooling the foamed container product in the mold to shape it; S7: a mold opening step, wherein the first component and the second component of the mold are separated and the container product is taken out.

2. The method for manufacturing a container product according to claim 1, characterized in that: The first area is the location of the bottom cavity part and the partial annular cavity part from the first end toward the second end; and the second area is the location of the annular cavity part from the first area to the bottom cavity part.

3. The method for manufacturing a container product according to claim 1, characterized in that: The blowing direction of the blowing port corresponds to the bottom cavity part.

4. The method for manufacturing a container product according to claim 1, characterized in that: The blowing port is provided with a ventilation block at a position corresponding to the second surface.

5. The method for manufacturing a container product according to claim 1, characterized in that: The polymer may be polypropylene.

6. The method for manufacturing a container product according to claim 1, characterized in that: The blowing agent may be nitrogen.

7. The method for manufacturing a container product according to claim 1, characterized in that: The S4 step cools the first zone and the second zone to the same cooling temperature.

8. The method for manufacturing a container product according to claim 1, characterized in that: The S6 cooling step is to cool the first zone and the second zone to the same cooling temperature or to cool them naturally under normal temperature.

Citation Information

Patent Citations

  • Method of forming article

    CN108778663A

  • Method of forming an article

    CN112789151A

  • Method of forming article

    CN115210056A

  • Method of making a plastic article

    EP0881052A1