Production method for dry lithium battery separator, and use thereof

By blending polybutene-1 with polypropylene and using high frequency and high voltage corona technology, the liquid absorption rate and mechanical properties of dry lithium battery separators are improved, and the problems of low porosity and poor thermal stability of existing separators are solved. , achieving higher lithium battery performance and environmental protection and low-cost production.

WO2024239527A1PCT designated stage expired Publication Date: 2024-11-28JIESHOU CITY TIANHONG PACKAGING MATERIAL
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
PCT/CN2023/125960
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-05-19
Filing Date
2023-10-23
Publication Date
2024-11-28

AI Technical Summary

Technical Problem

The existing dry-process lithium battery separators have problems such as low porosity, poor solvent wetting, poor thermal stability and low electrolyte liquid absorption, which affects the performance of lithium batteries.

Method used

Polybutene-1 is blended with polypropylene, and low-temperature plasma is generated on the plastic surface through high-frequency and high-voltage corona technology, resulting in free radical reaction and surface oxidation polarization, and improving the liquid absorption rate and hydrophilicity of the membrane.

Benefits of technology

It improves the mechanical properties and heat resistance of the diaphragm, enhances the affinity for electrolyte, improves the migration performance of lithium ions, and has a simple process, no environmental pollution and low cost.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 000001
    Figure 000001
  • Figure 000002
    Figure 000002
  • Figure 000003
    Figure 000003
Patent Text Reader

Abstract

A production method for a dry lithium battery separator, and a use thereof, relating to the technical field of lithium battery separators. According to the production method, polybutene-1 and polypropylene are blended to improve the mechanical properties and heat resistance of the separator; corona discharge is carried out on the treated plastic surface by using high frequency and high voltage, to generate low-temperature plasma, such that free radical reaction is generated on the surface of the separator to implement cross-linking of a polymer, the surface becomes rough, and the wettability to an electrolyte is improved; and molecules on the treated surface are oxidized and polarized, and the surface is corroded by means of ion electric shock, such that the surface properties are changed, the hydrophilic capacity is improved, a liquid absorption rate of the separator is improved, the affinity to an organic electrolyte is high, and the lyophilic performance is good. The production method is simple, convenient, and environmentally friendly, has low costs and high additional value, and is free of environmental pollution and the like.
Need to check novelty before this filing date? Find Prior Art

Description

Production method of dry-process lithium battery separator and its application Technical Field

[0001] The present invention belongs to the technical field of lithium battery separators, and in particular relates to a production method of a dry-process lithium battery separator and applications thereof. Background Art

[0002] A lithium-ion battery consists of four main components: the positive electrode, the negative electrode, the separator, and the electrolyte. The separator, a thin film with a microporous structure, is a critical component in lithium-ion batteries and a key internal component with the greatest technical barriers in the lithium-ion battery industry chain, accounting for approximately 10%-20% of the battery's total cost. The separator material is non-conductive, and its physical and chemical properties significantly influence battery performance. Because the electrolyte is an organic solvent system, a separator material with organic solvent resistance is required, typically using a high-strength, thin-film, porous polyolefin membrane. The lithium-ion battery separator is immersed in the electrolyte and has numerous micropores on its surface that allow lithium ions to pass through. The material, number, and thickness of these micropores affect the rate at which lithium ions pass through the separator, thereby affecting battery performance, such as discharge rate and cycle life. Previously, the mainstream lithium battery separator on the market was dry-process separator, which accounted for approximately 70% of the market share. Dry-process separators are primarily used in lithium iron phosphate batteries. Currently, there are three main methods for preparing battery separators: dry uniaxial stretching, dry biaxial stretching, and wet biaxial stretching. The dry-process separator process is the most commonly used method for preparing lithium-ion battery separators, but its corresponding wet-process allows for better control of pore size, distribution, and porosity. The dry-process biaxial stretching process is a separator manufacturing process unique to my country. This process incorporates a nucleating agent into PP and exploits the density differences between different PP phases to induce a crystal transformation during stretching to form micropores. CN201910450957.9, published on August 23, 2019, disclosed a high-puncture-strength dry-process separator and its preparation method. These separators utilize ceramic nano-reinforced particles and plasticizers, but in practice, their effectiveness has been poor, as the ceramic particles are prone to stress concentration and cracking. Compared to wet-process separators, dry-process uniaxial stretching offers lower costs and better long-term stability. Dry-process separators are primarily made from polypropylene, which exhibits high mechanical properties at room temperature. However, the resulting separators suffer from low porosity, poor solvent wettability, poor thermal stability, and low electrolyte absorption, hindering further improvement in lithium battery performance. Polyolefins have low polarity, resulting in poor interfacial compatibility between lithium-ion battery electrolytes and separators. They also have weak affinity for organic electrolytes and poor lyophilic properties, hindering the rapid migration of lithium ions and, in turn, negatively impacting battery performance. Consequently, polyolefin separators have low liquid absorption, leading to poor electrochemical performance in lithium-ion batteries. Those skilled in the art urgently need to develop dry-process lithium battery separator production methods and applications to meet existing market demands and performance requirements. Summary of the Invention

[0003] In view of this, the present invention provides a production method of a dry-process lithium battery separator and its application.

[0004] A dry-process lithium battery separator production method comprises the following steps: a first step of uniformly mixing a main resin and a polybutene-1 resin with a melt index of 0.6-0.65 at high speed to obtain a mixed resin; feeding the mixed resin into an extruder hopper, processing the mixed resin into a uniform melt, extruding and casting to obtain a cast base film, and then annealing after corona treatment to prepare an annealed base film; a second step of stretching: cold-drawing the annealed base film again at a temperature of 75-85°C and a heat-drawing ratio of 1.1-1.2; and then performing a heat-drawing treatment; the heat-drawing temperature is 135-145°C and the heat-drawing ratio is 1.2-1.4; and a third step of heat-setting: heat-setting the heat-drawn product to obtain the product.

[0005] Furthermore, the setting temperature of the third step heat setting treatment is 125-145° C., and the setting shrinkage rate is 12%-18%.

[0006] Furthermore, the main resin in the first step includes one or more of polypropylene and polyethylene.

[0007] Furthermore, in the first step, the mixing mass ratio of the main resin with a melt index of 2.0-3.0 and the polybutene-1 resin with a melt index of 0.6-0.65 is 90-95:10-15.

[0008] Furthermore, the extrusion casting process in the first step is as follows: the casting roller temperature is 80-100° C., the die opening is 1.2-1.25 mm, the casting die head temperature is 235-240° C., and the production line speed is 80-100 mm / min.

[0009] Furthermore, the corona process in the first step is as follows: an output voltage of 10-15 kV, a corona frequency of 28-35 kHz, and a corona time of 0.2-0.5 s.

[0010] Furthermore, the first annealing step is: annealing the cast base film at a temperature of 130-155° C. for 70-100 minutes.

[0011] Beneficial effects of the present invention:

[0012] The dry-process lithium battery separator production method disclosed in the present invention utilizes a blend of polybutene-1 and polypropylene to improve the separator's mechanical properties and heat resistance. High-frequency, high-voltage corona discharge is then applied to the treated plastic surface to generate low-temperature plasma, which generates free radical reactions on the separator surface, causing polymer crosslinking. This roughens the surface and increases its wettability to the electrolyte. The treated surface molecules oxidize and polarize, and ion shock erodes the surface, changing its surface properties and improving its hydrophilicity, thereby increasing the separator's liquid absorption rate. The method also exhibits strong affinity for organic electrolytes and good lyophilic properties. The production method disclosed in the present invention is simple and convenient, does not use any organic solvents, and is environmentally friendly. It is low-cost, high-value-added, and pollution-free. DETAILED DESCRIPTION

[0013] The present invention can be better understood according to the following examples. However, it is easy for those skilled in the art to understand that the contents described in the examples are only used to illustrate the present invention, and should not and will not limit the present invention described in detail in the claims. Example 1

[0014] The production method of polypropylene dry process lithium battery separator comprises the following steps: first, the main body 802 polypropylene resin with a melt index of 2.8g / 10min at 190°C and 2.16kg and the HY-ED050 polybutene-1 resin with a melt index of 0.65g / 10min at 190°C and 2.16kg are mixed at a mass ratio of 90:10, the main body 802 polypropylene resin with a melt index of 2.8g / 10min and the Dongfang Hongye HY-ED050 polybutene-1 resin with a melt index of 0.65 are mixed at high speed to obtain a mixed resin; the mixed resin is fed into the feeding hopper of an extruder, the mixed resin is processed into a uniform melt, and extrusion casting is performed, wherein the extrusion casting process comprises the following steps: a casting roller temperature of 100°C, a die opening of 1.25mm, a casting die head temperature of 240°C, and a production line speed of 100mm / min to obtain a casting film; The base film is stretched and then corona treated and annealed to prepare an annealed base film. The corona process is that the output voltage of the corona machine of Nantong Sanxin Plastic CW-4030 is 15kV, the corona frequency is 28kHz, the corona time is 0.2s, and the base film is annealed at 130°C for 100min. The second step is stretching: the annealed base film is cold-drawn again, the cold-drawing temperature is 75°C, and the heat-drawing ratio is 1.1; then hot-stretching treatment is performed; the hot-drawing stretching temperature is 135°C, and the heat-drawing ratio is 1.4; the third step is heat setting: the product of the heat-drawing treatment is heat-set at a setting temperature of 145°C and a setting shrinkage rate of 18%.

[0015] Membrane product performance: thickness 25.2μm, puncture strength 405gf, transmittance 4.32s / mL, porosity 40.9%, tensile strength MD139.6MPa, TD24.2MPa, elongation at break MD32.4%, TD128.96%, average pore size 1.0μm, liquid absorption rate 159%. Example 2

[0016] The production method of a dry-process lithium battery separator comprises the following steps: the first step is to mix the main body FS3028 polypropylene resin with a melt index of 2.4g / 10min at 190°C and 2.16kg and the main body FS3028 polypropylene resin with a melt index of 0.6 at 190°C and 2.16kg at a mass ratio of 95:15; 0.6 D600 Tengzhou Ruida polybutene-1 resin is mixed at high speed to obtain a mixed resin; the mixed resin is put into the extruder hopper, the mixed resin is processed into a uniform melt, and extrusion casting is performed. The extrusion casting process is a casting roller temperature of 80°C, a die opening of 1.2mm, a casting die head temperature of 235°C, and a production line speed of 80mm / min to obtain a cast base film, and then corona annealing is performed to prepare an annealed base film. The corona process is an output voltage of 10kV, a corona frequency of 35kHz, a corona time of 0.5s, and annealing at 155°C for 70min; the second step is stretching: the annealed base film is then cold-drawn once, the cold-drawing temperature is 85°C, and the hot-drawing ratio is 1.2; then a hot-drawing treatment is performed; the hot-drawing stretching temperature is 145°C, and the hot-drawing ratio is 1.2; the third step is heat setting: the product of the hot-drawing treatment is heat-set, the setting temperature of the heat setting treatment is 125°C, and the setting shrinkage rate is 12%.

[0017] Membrane product performance: thickness 25.1μm, puncture strength 412gf, transmittance 4.32s / mL, porosity 40.1%, tensile strength MD139.8MPa, TD24.5MPa, elongation at break MD31.8%, TD131.35%, average pore size 1.0μm, liquid absorption rate 168%.

[0018] Note: Refer to GB / T 36363-2018, Polyolefin Separators for Lithium-ion Batteries; liquid absorption is based on QB / T 2303.1-2008, Battery Pulp Paper, Part 11: Determination of Liquid Absorption; puncture strength is tested according to ASTM D4833-00e1. The needle shape is a hemisphere with a diameter of 1.0 mm, and the needle travels at a speed of 1 mm / s.

[0019] The above description is only a preferred embodiment of the present invention and is not intended to limit the scope of protection of the present invention. All equivalent changes and modifications made based on the content of the present invention are included in the patent scope of the present invention.

Claims

1. A method for producing a dry lithium battery separator, characterized in that: The following steps are involved: The first step is to mix the main resin and the polybutene-1 resin with a melt index of 0.6-0.65 at high speed to obtain a mixed resin; the mixed resin is put into the feeding hopper of the extruder, the mixed resin is processed into a uniform melt, extruded and cast to obtain a cast base film, and then corona annealing is performed to prepare an annealed base film; the second step is stretching: the annealed base film is cold-drawn again, the cold-drawing temperature is 75-85°C, and the heat-drawing ratio is 1.1-1.2; and then hot-drawing treatment is performed; the stretching temperature of the hot-drawing is 135-145°C, and the heat-drawing ratio is 1.2-1.4; the third step is heat setting: the product of the hot-drawing treatment is heat-set to obtain.

2. The method for producing a three-layer cast diaphragm according to claim 1, characterized in that: The third step of heat setting treatment has a setting temperature of 125-145° C. and a setting shrinkage rate of 12%-18%.

3. The preparation method according to claim 1, characterized in that: The main resin is polypropylene with a melt index of 2.0-3.

0.

4. The method for producing a dry lithium battery separator according to claim 1, characterized in that: The mixing mass ratio of the main resin to the polybutene-1 resin with a melt index of 0.6-0.65 is 90-95:10-15.

5. The method for producing a dry lithium battery separator according to claim 1, characterized in that: The extrusion casting process in the first step is as follows: the casting roller temperature is 80-100° C., the die opening is 1.2-1.25 mm, the casting die head temperature is 235-240° C., and the production line speed is 80-100 mm / min.

6. The method for producing a dry lithium battery separator according to claim 1, characterized in that: The corona process in the first step is as follows: output voltage 10-15 kV, corona frequency 28-35 kHz, corona time 0.2-0.5 s.

7. The method for producing a dry lithium battery separator according to claim 1, characterized in that: The first annealing step is: annealing the cast base film at a temperature of 130-155° C. for 70-100 minutes.

8. Application of a dry-process lithium battery separator produced by the production method of a dry-process lithium battery separator as described in any one of claims 1 to 7 in a lithium battery.

Citation Information

Patent Citations

  • Microporous polypropylene film

    CN101880419A

  • Lithium ion secondary battery polymer separation film corona processing method

    CN103236510A

  • Polyolefin multilayer microporous film, method for producing same, and cell separator

    CN107405902A

  • Method for modifying polyolefin lithium-ion battery separator

    CN110010824A