Oxidation tank
A protective layer on the light receiving window in oxidation tanks prevents deterioration and maintains efficiency, addressing the issue of reduced light transmittance and energy conversion in long-term operation.
Patent Information
- Application Number
- PCT/JP2023/019109
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-23
- Publication Date
- 2024-11-28
AI Technical Summary
The light receiving window in oxidation tanks deteriorates over long-term operation due to reaction with aqueous solutions, leading to reduced light transmittance and decreased light energy conversion efficiency in water splitting reactions.
A protective layer made of light-transmitting resin is formed on the inner surface of the light receiving window to prevent contact with the electrolyte solution, maintaining light transmittance and stability of the window.
The protective layer effectively prevents devitrification and maintains light energy conversion efficiency over extended operation, ensuring consistent hydrogen production in water oxidation and proton reduction reactions.
Smart Images

Figure JP2023019109_28112024_PF_FP_ABST
Abstract
Description
Oxidation tank
[0001] The present disclosure relates to an oxidation bath.
[0002] There is a device that generates hydrogen through a water splitting reaction using a semiconductor photoelectrode (Non-Patent Document 1). This device has an oxidation tank and a reduction tank. An aqueous solution and an oxidation electrode are placed in the oxidation tank. An aqueous solution and a reduction electrode are placed in the reduction tank. The oxidation tank and reduction tank are connected via a proton exchange membrane. The oxidation electrode and reduction electrode are electrically connected by a conductor.
[0003] The water splitting reaction using a photocatalyst consists of a water oxidation reaction and a proton reduction reaction. When light is irradiated onto an n-type photocatalytic material, electrons and holes are generated and separated within the photocatalyst. The holes move to the surface of the photocatalytic material and contribute to the water oxidation reaction. Meanwhile, the electrons move to the reduction electrode and contribute to the proton reduction reaction. Ideally, this oxidation-reduction reaction proceeds, resulting in the water splitting reaction.
[0004] Oxidation reaction: 2H2O + 4h + → O2 + 4H + Reduction reaction: 4H + + 4e - → 2H2
[0005] The oxidation electrode is a semiconductor film. For example, the oxidation electrode is a gallium nitride thin film grown on a sapphire substrate. In the gallium nitride thin film, holes generated and separated under light irradiation are consumed in the etching reaction of the gallium nitride itself as well as in the oxidation reaction of water. The photoelectrode may deteriorate, and the light energy conversion efficiency may decrease with the duration of light irradiation.
[0006] To prevent this deterioration, examples have been reported in which a promoter (nickel oxide) for oxygen generation was formed as a protective layer, thereby improving the lifespan. The increased lifespan of the oxidation electrode has made it possible to operate the battery for extended periods of time.
[0007] S. Yotsuhashi, et al., “CO2Conversion with Light and Water by GaN Photoelectrode”, Japanese Journal of Applied Physics, The Japan Society of Applied Physics, 2012, Volume 51, pp. 02BP07-1-02BP07-3
[0008] During long-term operation, the aqueous solution reacts with the light-receiving window that receives light into the oxidation tank. The surface of the material that makes up the light-receiving window becomes rough, and the light transmittance of the window deteriorates (it becomes devitrified). As a result, the light energy that reaches the oxidation electrode is attenuated by the deteriorated light-receiving window. This can reduce the light energy conversion efficiency at the oxidation electrode.
[0009] The present disclosure has been made in consideration of the above circumstances, and an object of the present disclosure is to provide a technology capable of protecting the light-receiving window of an oxidation tank.
[0010] An oxidation tank according to one embodiment of the present disclosure includes an oxidation electrode and an electrolyte solution provided within the oxidation tank, a light-receiving window installed in the oxidation tank for receiving light onto the oxidation electrode, a conductor electrically connecting the oxidation electrode to a reduction electrode in a reduction tank, and an electrolyte membrane separating the oxidation tank from the reduction tank, and a protective layer is formed on the surface of the light-receiving window that faces the inside of the oxidation tank.
[0011] An oxidation basin according to one embodiment of the present disclosure includes an oxidation electrode and an electrolyte solution provided within the oxidation basin, a first light-receiving window installed in the oxidation basin and receiving light that reaches the oxidation electrode, a second light-receiving window installed in the oxidation basin and receiving light that has passed through the oxidation electrode, a conductor that electrically connects the oxidation electrode to a reduction electrode in a reduction basin, and an electrolyte membrane that separates the oxidation basin from the reduction basin, and a protective layer is formed on the surfaces of the first light-receiving window and the second light-receiving window that face the inside of the oxidation basin.
[0012] According to the present disclosure, a technology can be provided that can protect the light-receiving window of an oxidation tank.
[0013] Fig. 1 is a diagram illustrating an apparatus according to a first embodiment, Fig. 2 is a diagram illustrating an apparatus according to a second embodiment, and Fig. 3 is a diagram illustrating a conventional apparatus.
[0014] Hereinafter, embodiments of the present disclosure will be described with reference to the drawings. In the description of the drawings, the same parts are designated by the same reference numerals and the description thereof will be omitted.
[0015] First, referring to Figure 3, an apparatus 100 used in an oxidation-reduction reaction test will be described. The apparatus 100 includes a light source 101, an oxidation tank 102, a reduction tank 103, a proton exchange membrane 104, and a lead wire 106. The oxidation tank 102 contains an oxidation electrode 121 and an aqueous solution 122. The oxidation tank 102 is provided with a light-receiving window 124. The light-receiving window 124 receives light from the light source 101 to the oxidation electrode 121. The reduction tank 103 contains a reduction electrode 131 and an aqueous solution 132.
[0016] In the oxidation bath 102, the oxidation electrode 121 is in contact with an aqueous solution 122. The oxidation electrode 121 is made of a nitride semiconductor, titanium oxide, amorphous silicon, etc. The aqueous solution 122 is, for example, an aqueous sodium hydroxide solution, an aqueous potassium hydroxide solution, or hydrochloric acid.
[0017] In the reduction tank 103, the reduction electrode 131 is in contact with an aqueous solution 132. The reduction electrode 131 is a metal or a metal compound, such as nickel, iron, gold, platinum, silver, copper, indium, or titanium. The aqueous solution 132 is, for example, an aqueous solution of sodium bicarbonate, a potassium chloride, or a sodium chloride.
[0018] The proton exchange membrane 104 is sandwiched between the oxidation chamber 102 and the reduction chamber 103. Protons are generated in the oxidation chamber 102. The generated protons diffuse into the reduction chamber 103 through the proton exchange membrane 104. The proton exchange membrane 104 is, for example, a perfluorocarbon material. The purple perfluorocarbon material is composed of a hydrophobic Teflon (registered trademark) skeleton made of carbon and fluorine, and perfluoro side chains with sulfonic acid groups. The proton exchange membrane 104 is, for example, Nafion (registered trademark).
[0019] The oxidation electrode 121 and the reduction electrode 131 are electrically connected by a conductor 106. Electrons move from the oxidation electrode 121 to the reduction electrode 131 via the conductor 106.
[0020] The light source 101 is, for example, a xenon lamp, a mercury lamp, a halogen lamp, a solar simulant, sunlight, or a combination thereof. The light source 101 emits light of a wavelength that can be absorbed by the material that constitutes the oxide electrode 121. For example, in the case of the oxide electrode 121 made of gallium nitride, the wavelength that can be absorbed by the oxide electrode 121 is 365 nm or shorter.
[0021] In this device 100, the life of the oxidation electrode has been extended, enabling long-term operation. However, during long-term operation, the aqueous solution 122 reacts with the light-receiving window 124, which receives light entering the oxidation tank 102. The surface of the material composing the light-receiving window 124 becomes rough, and the light transmittance of the light-receiving window 124 deteriorates (devitrification occurs). As a result, the light energy reaching the oxidation electrode 121 is attenuated by the deteriorated light-receiving window 124. This may result in a decrease in the light energy conversion efficiency of the oxidation electrode 121.
[0022] The present disclosure prevents deterioration of the light-receiving window 124 due to deterioration of the light-receiving window. The present disclosure enables long-term operation of a device in which a water oxidation reaction and a proton reduction reaction proceed.
[0023] Specifically, in the device according to the present disclosure, a protective layer is formed on the surface of the light-receiving window that faces the inside of the oxidation tank. The protective layer is formed so as to prevent contact between the light-receiving window and the electrolyte (aqueous solution). Since the light-receiving window and the electrolyte do not come into contact with each other, deterioration of the light-receiving window can be prevented.
[0024] The protective layer is formed of a light-transmitting resin that transmits light. By forming the protective layer from the light-transmitting resin, the light transmittance of the light-receiving window is ensured, and light from the light source can be irradiated onto the oxidation electrode.
[0025] The protective layer is made of a material that does not react with the electrolyte, and since the protective layer does not react with the electrolyte even when it comes into contact with the electrolyte, the protective effect of the protective layer on the light receiving window can be maintained.
[0026] The light-receiving window is coated with a protective layer to prevent it from coming into contact with the electrolyte, which prevents devitrification of the light-receiving window and improves the stability of the light energy conversion efficiency.
[0027] (First embodiment) An apparatus 1 according to a first embodiment will be described with reference to Fig. 1. The apparatus 1 is used for an oxidation-reduction reaction test, similar to the apparatus 100 shown in Fig. 3. In the oxidation-reduction reaction test, an oxidation reaction of water and a reduction reaction of protons proceed.
[0028] The device 1 includes an oxidation tank 2 and a reduction tank 3. The oxidation tank 2 and the reduction tank 3 are separated by an electrolyte membrane 4. In the device 1, the oxidation tank 2 and the reduction tank 3 are described as being adjacent to each other in the horizontal direction, but this is not limiting, and the oxidation tank 2 and the reduction tank 3 may also be adjacent to each other in the vertical direction.
[0029] An electrolytic solution 5 is poured into the oxidation tank 2 and the reduction tank 3. The electrolytic solution 5 is used in the oxidation-reduction reaction. The electrolytic solution 5 may be an aqueous solution in which an electrolyte that moves ions is dissolved. Examples of the electrolytic solution 5 include sodium hydroxide, a potassium hydroxide aqueous solution, a rubidium hydroxide aqueous solution, and a cesium hydroxide aqueous solution.
[0030] The oxidation vessel 2 is provided with an oxidation electrode 21 , a gas inlet line 22 , a gas exhaust line 23 and a light receiving window 24 .
[0031] The oxidation electrode 21 is provided so as to be in contact with the electrolyte 5. The oxidation electrode 21 is provided so that light passing through a light receiving window 24 provided in the housing of the oxidation tank 2 is irradiated onto the oxidation electrode 21. The oxidation electrode 21 is a nitride semiconductor such as a GaN (gallium nitride)-based material. The oxidation electrode 21 may be an oxide semiconductor other than a nitride semiconductor.
[0032] The gas inlet line 22 and the gas exhaust line 23 have a hollow pipe shape. One end of the gas inlet line 22 is in contact with the air above the electrolytic solution 5, and the other end is in contact with the electrolytic solution 5. Both ends of the gas exhaust line 23 are in contact with the air above the electrolytic solution 5. Nitrogen gas is introduced into the electrolytic solution 5 by the gas inlet line 22. The gas exhaust line 23 collects oxygen gas exhausted from the electrolytic solution 5.
[0033] The light-receiving window 24 is installed in the housing of the oxidation tank 2. The light-receiving window 24 receives light from a light source outside the oxidation tank 2 and is directed toward the oxidation electrode 21. The light from the light source is transmitted through the light-receiving window 24. The transmitted light irradiates the oxidation electrode 21.
[0034] The reduction tank 3 is provided with a reduction electrode 31 , a gas inlet line 32 , and a gas exhaust line 33 .
[0035] The reduction electrode 31 is provided so as to be in contact with the electrolyte 5 .
[0036] The gas inlet line 32 and the gas exhaust line 33 are similar to the gas inlet line 22 and the gas exhaust line 33, respectively, provided in the oxidation tank 2. In the reduction tank 3, nitrogen gas is introduced into the electrolytic solution 5 through the gas inlet line 32. The gas exhaust line 33 collects hydrogen gas exhausted from the electrolytic solution 5.
[0037] The oxidation electrode 21 and the reduction electrode 31 are electrically connected by a conductor 6. Electrons move from the oxidation electrode 21 to the reduction electrode 31 via the conductor 6.
[0038] In the device 1 shown in FIG. 1 , a protective layer 25 is formed on the surface of the light-receiving window 24 facing the inside of the oxidation tank 2. The protective layer 25 is formed on a portion of the surface of the light-receiving window 24 that may come into contact with the electrolyte 5. The protective layer 25 prevents the light-receiving window 24 from coming into contact with the electrolyte 5. The light-receiving window 24 is protected. The light transmittance of the light-receiving window 24 does not deteriorate even during long-term oxidation-reduction reaction tests. As a result, light energy transmitted through the light-receiving window 24 reaches the oxidation electrode 21 without attenuation. The light energy conversion efficiency of the oxidation electrode 21 is maintained.
[0039] The protective layer 25 is preferably formed of a light-transmitting resin that transmits light. This allows the light-receiving window 24 to maintain light transmittance in the same manner as if the protective layer 25 were not present. The protective layer 25 is formed of, for example, an acrylic resin. In addition to acrylic resin, the protective layer 25 may also be formed of polyethylene terephthalate-based, polyvinyl chloride-based, polystyrene-based, or other materials.
[0040] The protective layer 25 is preferably made of a material that does not react with the electrolyte solution 5. This allows the performance of the protective layer 25 to be maintained even during a long-term oxidation-reduction reaction test.
[0041] Second Embodiment An apparatus 1 according to a second embodiment will be described with reference to Fig. 2. The apparatus 1a is used for oxidation-reduction reaction tests, similar to the apparatus 100 shown in Fig. 3. In the oxidation-reduction reaction tests, an oxidation reaction of water and a reduction reaction of protons proceed.
[0042] The device 1a includes an oxidation tank 2 and a reduction tank 3, similar to the device 1 shown in Fig. 1 . The oxidation tank 2 and the reduction tank 3 are separated by an electrolyte membrane 4. In the device 1a, the oxidation tank 2 and the reduction tank 3 are described as being adjacent to each other in the vertical direction, but this is not limiting; the oxidation tank 2 and the reduction tank 3 may also be adjacent to each other in the horizontal direction. In the oxidation tank 2 of the device 1a according to the second embodiment, light passes through the first light-receiving window 24a, the oxidation electrode 21, and the second light-receiving window 24b, so it is preferable to install the oxidation tank 2 and the reduction tank 3 in a vertical direction. This is because the reduction tank 3 is not installed around the oxidation tank 2.
[0043] The device 1a has a configuration similar to that of the device 1 shown in Fig. 1. The device 1a differs from the device 1 in that it includes a photovoltaic power generation element 7 and in that the oxidation basin 2 includes a first light-receiving window 24a and a second light-receiving window 24b.
[0044] The photovoltaic power generation element 7 emits light irradiated onto the oxidation electrode 21. The photovoltaic power generation element 7 is, for example, a silicon (Si)-based element. In addition to Si-based elements, the photovoltaic power generation element 7 may be made of various light-emitting elements such as a CIS (thin film: copper indium selenium)-based element, a CIGS (copper indium gallium selenium)-based element, a GaAs (gallium arsenide)-based element, an organic-based element, or a perovskite-based element.
[0045] The first light-receiving window 24a is disposed in the oxidation tank 2 and receives light that reaches the oxidation electrode 21. The second light-receiving window 24b is disposed in the oxidation tank 2 and receives light that has passed through the oxidation electrode 21. In the oxidation tank 2, light irradiated by the photovoltaic power generation element 7 passes through the first light-receiving window 24a, the oxidation electrode 21, and the second light-receiving window 24b.
[0046] A first protective layer 25a is formed on the surface of the first light-receiving window 24a facing the inside of the oxidation tank 2. Similarly, a second protective layer 25b is formed on the surface of the second light-receiving window 24b facing the inside of the oxidation tank 2. The first protective layer 25a in the second embodiment is similar to the protective layer 25 described in the first embodiment.
[0047] The first protective layer 25a and the second protective layer 25b are made of a light-transmitting resin that transmits light, and a material that does not react with the electrolyte.
[0048] The materials of the device 1 shown in the first embodiment and the device 1a shown in the second embodiment are merely examples and are not limited thereto. In the present disclosure, the case where the target product is hydrogen has been described. By changing the material of the reduction electrode 31 or the atmosphere within the device, it is possible to generate various target products, such as the production of carbon compounds through the reduction reaction of carbon dioxide or the production of ammonia through the reduction reaction of nitrogen. The reduction electrode 31 may be formed of, for example, Ni (nickel), Fe (iron), Au (gold), Pt (platinum), Ag (silver), Cu (copper), In (indium), Ti (titanium), Co (cobalt), or Ru (ruthenium).
[0049] Next, the results of an oxidation-reduction reaction test using the device according to the present disclosure will be described. In the test, the amount of hydrogen gas generated after a predetermined time was measured for each of several combinations of electrodes and aqueous solutions, with and without a resin protective layer 25 formed on the light-receiving window 24, as shown in Table 1. In this test, the aqueous solution was electrolyte solution 5.
[0050] Example 1 In Example 1, the device 1 according to the first embodiment shown in FIG. 1 was used.
[0051] The production of the light-receiving window 24 on which the protective layer 25 is formed will now be described. Quartz was used as the material for the light-receiving window 24. Only the surface that comes into contact with the aqueous solution was coated with acrylic resin. The light transmittance of the acrylic resin-coated light-receiving window 24 was 90%.
[0052] The generation of the oxidation electrode 21 will now be explained. A GaN substrate was used as the substrate. A silicon-doped n-GaN semiconductor thin film was epitaxially grown on a 2-inch diameter GaN substrate by MOCVD (Metal Organic Chemical Vapor Deposition). The thickness of the n-GaN film was 2 μm, which is sufficient for light absorption. The carrier density was 3×10 18 cm 3 After that, aluminum gallium nitride (AlGaN) was grown. The aluminum composition ratio was 10%. The film thickness was set to 100 nm, which is sufficient to absorb light. The 2-inch semiconductor thin film was then cleaved into four equal pieces, one of which was used to fabricate an electrode.
[0053] Next, a 1-nm-thick Ni film was deposited on the AlGaN surface by electron beam (EB) deposition, and the semiconductor thin film was then heat-treated at 300°C for 1 hour in an air atmosphere on a hot plate to form NiO.
[0054] Next, the oxidation-reduction reaction test in Example 1 will be described. In the oxidation-reduction reaction test, parts of the NiO and AlGaN surfaces were scribed to expose the n-GaN surface. A conducting wire 6 was connected to part of the exposed n-GaN surface and soldered using In. The wire was then covered with epoxy resin so that the In surface was not exposed. This was installed as the oxidation electrode 21 in Figure 1.
[0055] The electrolyte solution 5 was a 1 mol / L aqueous solution of sodium hydroxide. The reduction electrode 31 was made of platinum (manufactured by Nilaco). The electrolyte membrane 4 was made of Nafion (registered trademark). Nitrogen gas was flowed through each reaction vessel at a rate of 10 mL / min. The light irradiation area of the oxidation electrode 21 was 1 cm. 2 It was decided.
[0056] After the atmosphere inside the reaction vessels was thoroughly replaced with nitrogen gas, the oxidation electrode 21, fabricated using the procedure described above, was fixed so that the light source faced the NiO-formed surface. The light source was a 300W high-pressure xenon lamp (illuminance 5mW / cm2). The oxidation electrode 21 was uniformly irradiated with light. During the light irradiation, gas samples were taken from each reaction vessel at random times, and the reaction products were analyzed using a gas chromatograph. The results confirmed that oxygen was produced in the oxidation vessel 2 and hydrogen was produced in the reduction vessel 3.
[0057] Example 2 The same procedure as in Example 1 was carried out except that the electrolyte solution 5 in Example 1 was changed to a 1 mol / L aqueous potassium hydroxide solution.
[0058] Example 3 The same procedure as in Example 1 was carried out except that the electrolyte solution 5 in Example 1 was changed to a 1 mol / L aqueous solution of rubidium hydroxide.
[0059] Example 4 The same procedure as in Example 1 was carried out except that the electrolyte solution 5 in Example 1 was changed to a 1 mol / L aqueous cesium hydroxide solution.
[0060] Example 5 In Example 5, the device 1a according to the second embodiment shown in FIG. 2 was used.
[0061] The following describes the production of the first light receiving window 24a with a first protective layer 25a formed thereon. The second light receiving window 24b with a second protective layer 25b formed thereon was also produced in the same manner. Quartz was used as the material for the first light receiving window 24a. Only the surface that comes into contact with the aqueous solution was coated with acrylic resin. The light transmittance of the acrylic resin-coated light receiving window 24 was 90%.
[0062] The generation of the oxidation electrode 21 will now be described. A GaN substrate was used as the substrate. A silicon-doped n-GaN semiconductor thin film was epitaxially grown on a 2-inch diameter GaN substrate by MOCVD (Metal Organic Chemical Vapor Deposition). The n-GaN film thickness was 2 μm, which is sufficient for light absorption. The carrier density was 3×10 18 cm 3After that, indium gallium nitride (InGaN) was grown. The indium composition ratio was 10%. The film thickness was set to 100 nm, which is sufficient to absorb light. After that, the 2-inch semiconductor thin film was cleaved into four equal pieces, and one of them was used to fabricate an electrode.
[0063] Next, an oxidation-reduction reaction test in Example 5 will be described. As shown in FIG. 2 , an oxidation electrode 21 was installed. A silicon-based pn junction semiconductor element was used as the photovoltaic power generation element 7. The oxidation electrode 21, the photovoltaic power generation element 7, and the reduction electrode 31 were connected in series. The rest of the experiment was the same as in Example 1.
[0064] Example 6 The same procedure as in Example 5 was carried out except that the electrolyte solution 5 in Example 5 was changed to a 1 mol / L aqueous potassium hydroxide solution.
[0065] Example 7 The same procedure as in Example 5 was carried out, except that the electrolyte solution 5 in Example 5 was changed to a 1 mol / L aqueous rubidium hydroxide solution.
[0066] Example 8 The same procedure as in Example 5 was carried out except that the electrolyte solution 5 in Example 5 was changed to a 1 mol / L aqueous cesium hydroxide solution.
[0067] Comparative Example 1 Comparative Example 1 was carried out in the same manner as in Example 1, except that the protective layer 25 was not formed.
[0068] Comparative Example 2 Comparative Example 2 was carried out in the same manner as in Example 2, except that the protective layer 25 was not formed.
[0069] Comparative Example 3 This example was the same as Example 3 except that the protective layer 25 was not formed.
[0070] Comparative Example 4 Comparative Example 4 was carried out in the same manner as in Example 4, except that the protective layer 25 was not formed.
[0071] Comparative Example 5 Comparative Example 5 was carried out in the same manner as Example 5, except that the first protective layer 25a and the second protective layer 25b were not formed.
[0072] Comparative Example 6 Comparative Example 6 was carried out in the same manner as Example 6, except that the first protective layer 25a and the second protective layer 25b were not formed.
[0073] Comparative Example 7 Comparative Example 7 was carried out in the same manner as Example 7, except that the first protective layer 25a and the second protective layer 25b were not formed.
[0074] Comparative Example 8 Comparative Example 8 was carried out in the same manner as Example 8, except that the first protective layer 25a and the second protective layer 25b were not formed.
[0075] Table 1 shows the amount of hydrogen gas produced for each example 1 hour and 500 hours after light irradiation.
[0076]
[0077] The amount of each gas produced was normalized by the surface area of the semiconductor photoelectrode. In all cases, hydrogen was produced upon light irradiation.
[0078] There was no significant difference in the amount of hydrogen generated one hour after light irradiation between Examples 1 to 4. Furthermore, there was no significant difference in the amount of hydrogen generated one hour after light irradiation between Comparative Examples 4 and 5.
[0079] On the other hand, the amount of hydrogen generated after 500 hours in Example 1 was greater than that in Comparative Example 1. The same was true when comparing each of Examples 2 to 4 with each of Comparative Examples 2 to 4.
[0080] This is thought to be because the protection by the resin prevented the devitrification of the quartz and suppressed the attenuation of light energy to the electrode.
[0081] Furthermore, since the amount of hydrogen generated after 500 hours was greater in Example 4 than in Example 1, it can be said that CsOH is effective in extending the life of the oxidation electrode 21. RbOH and CsOH are more corrosive than NaOH or KOH and therefore have a greater impact on the devitrification of quartz. However, by protecting the quartz with resin, it is believed that this drawback can be prevented and the life of the oxidation electrode 21 can be extended. The same was true for Examples 5 to 8.
[0082] In the present disclosure, a protective layer 25 is formed on the light-receiving window 24 to prevent contact between the light-receiving window 24 and the electrolyte 5. The protective layer 25 prevents devitrification of the light-receiving window 24 and improves the stability of the light energy conversion efficiency.
[0083] Conventionally, although RbOH or CsOH is expected to extend the life of the oxidation electrode 21, it has been thought that it is difficult to apply RbOH or CsOH to the light-receiving window 24 due to its high corrosiveness to quartz. However, as in the device 1 according to the present disclosure, by forming a protective layer 25 on the light-receiving window 24 made of RbOH or CsOH, it is possible to further improve stability.
[0084] In this way, by forming a protective layer 25 on the light-receiving window 24, contact between the light-receiving window 24 and the electrolyte 5 can be prevented, thereby preventing devitrification of the light-receiving window 24 and improving the stability of the light energy conversion efficiency.
[0085] The present disclosure is not limited to the above-described embodiments, and various modifications are possible within the scope of the gist of the present disclosure.
[0086] REFERENCE SIGNS LIST 1, 100 Apparatus 2, 102 Oxidation tank 3, 103 Reduction tank 4 Electrolyte membrane 5 Electrolyte solution 6, 106 Lead wire 7 Photovoltaic power generation element 21, 121 Oxidation electrode 22, 32 Gas inlet line 23, 33 Gas exhaust line 24, 124 Light receiving window 25 Protective layer 31, 131 Reduction electrode 101 Light source 122, 132 Aqueous solution
Claims
1. An oxidation cell comprising: an oxidation electrode and an electrolyte solution provided within an oxidation cell; a light-receiving window disposed in said oxidation cell for receiving light onto said oxidation electrode; a conductor electrically connecting said oxidation electrode and a reduction electrode in a reduction cell; and an electrolyte membrane separating said oxidation cell from said reduction cell, wherein a protective layer is formed on the surface of said light-receiving window that faces the inside of said oxidation cell.
2. The oxidation tank according to claim 1, wherein the protective layer is formed of a light-transmitting resin that transmits light.
3. The oxidation cell according to claim 1, wherein the protective layer is formed of a material that does not react with the electrolyte.
4. An oxidation tank comprising: an oxidation electrode and an electrolyte provided in an oxidation tank; a first light-receiving window provided in the oxidation tank and receiving light that reaches the oxidation electrode; a second light-receiving window provided in the oxidation tank and receiving light that has passed through the oxidation electrode; a conductor electrically connecting the oxidation electrode and a reduction electrode in a reduction tank; and an electrolyte membrane separating the oxidation tank from the reduction tank, wherein a protective layer is formed on the surfaces of the first light-receiving window and the second light-receiving window that are facing the inside of the oxidation tank.
5. The oxidation tank according to claim 4, wherein the protective layer is formed of a light-transmitting resin that transmits light.
6. The oxidation cell according to claim 4, wherein the protective layer is formed of a material that does not react with the electrolyte.
Citation Information
Patent Citations
Glass material provided with alkali elusion-proof film and its production
JP1986163142A
Tision-based multilayer thin film-coated glass and its production
JP1992285033A
Method for generating hydrogen, and hydrogen generator used therefor
JP2015206085A
Photoelectrochemical reactor
JP2017031467A
Photo-assisted electrolysis
US20020060161A1