Magnesium-containing urea and preparation method therefor

By adding magnesium sulfur alum and flux to the urea, magnesium-containing urea is prepared, which solves the problems of low utilization rate of urea nitrogen fertilizer and complex compounding of magnesium fertilizers, improves the efficiency of nitrogen fertilizer absorption, and reduces environmental pollution and production costs.

WO2024244492A1PCT designated stage expired Publication Date: 2024-12-05SHENZHEN KS TRADING CO LTD
View PDF 11 Cites 0 Cited by

Patent Information

Application Number
PCT/CN2024/072497
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-05-29
Filing Date
2024-01-16
Publication Date
2024-12-05

AI Technical Summary

Technical Problem

When existing urea is a nitrogen fertilizer, the nitrogen loss is high, the utilization rate is low, and its production process consumes a lot of energy, resulting in environmental pollution. At the same time, the combination method of traditional magnesium fertilizer is complex and cannot achieve industrial production.

Method used

Magnesium sulfur alum is used as the source of magnesium elements, and magnesium-containing urea is prepared through reasonable proportioning and process flow with urea and flux, which improves the utilization efficiency of nitrogen fertilizers and reduces production costs.

Benefits of technology

It improves the absorption and utilization rate of nitrogen fertilizer by crops, reduces greenhouse gas emissions, reduces resource waste and environmental pollution, realizes the sufficient addition of magnesium in urea, meets crop needs, and simplifies the production process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2024072497_05122024_PF_FP_ABST
    Figure CN2024072497_05122024_PF_FP_ABST
Patent Text Reader

Abstract

The present application relates to the technical field of compound fertilizers, and specifically relates to magnesium-containing urea and a preparation method therefor. The magnesium-containing urea comprises the following components in parts by weight: about 75-90 parts of urea, about 6-25 parts of kieserite and about 1-10 parts of a fluxing agent.
Need to check novelty before this filing date? Find Prior Art

Description

Magnesium-containing urea and preparation method thereof

[0001] Related applications

[0002] This application claims priority to Chinese patent application No. 2023106147117, filed on May 29, 2023, entitled “Magnesium-containing urea and preparation method thereof,” the entire text of which is hereby incorporated by reference. Technical Field

[0003] The present application relates to the technical field of compound fertilizers, and in particular to magnesium-containing urea and a preparation method thereof. Background Art

[0004] Nitrogen is one of the mineral nutrients necessary for plant growth and development. It plays a key role in the growth and yield formation of crops. Nitrogen is often called the life substance of plants. Nitrogen fertilizer is an important fertilizer variety in agricultural production and is also the variety with the largest annual application amount. Among the directly applied nitrogen fertilizers, urea has a long history, high nutrient content, and low price. It is deeply favored by growers in the base fertilizer and topdressing stages of certain crops. Urea usage accounts for more than 80% of the direct application nitrogen fertilizer market, with an annual usage of about 17 million tons. As a nitrogen fertilizer with high nitrogen content and easy water solubility, urea has the advantages of fast fertilizer effect, but high nitrogen loss and low nutrient efficiency. The average nitrogen fertilizer efficiency of urea applied to different crops is about 40%, and the remaining approximately 60% of nitrogen fertilizers are respectively used as NH4 + 、NO3 - Urea is leached into the soil in the form of NH3 and NH₃, flowing into runoff or volatilizing into the air. This not only fails to promote agricultural production but also pollutes water and air. Furthermore, urea production is an energy-intensive process, consuming significant amounts of coal, natural gas, and other energy sources. Improving urea's fertilizer utilization rate can not only improve its fertilizer efficiency and promote agricultural production, but also save energy and reduce pollution.

[0005] Considering the scale of fertilizer production and its destination, scientific research results in recent years have shown that the scientific application of magnesium fertilizer can improve the absorption and utilization efficiency of nitrogen fertilizer, phosphorus fertilizer, and potassium fertilizer by crops, especially significantly improving the absorption and utilization efficiency of nitrogen fertilizer. Studies have shown that magnesium is an essential nutrient in the process of converting inorganic nitrogen into protein. When crops are deficient in magnesium, protein synthesis stops, thereby blocking the absorption and utilization of nitrogen by crops and resulting in a decrease in the utilization rate of nitrogen fertilizer. Magnesium supplementation can also reduce the emission of the greenhouse gas nitrous oxide (NO2) during agricultural production. Therefore, adding magnesium to urea can improve the utilization efficiency of nitrogen in urea, promote crop growth, and reduce resource waste and environmental pollution.

[0006] The research results of the International Magnesium Nutrition Institute tell us that urea, as an important variety of single nitrogen fertilizer, replaces effective magnesium elements during the application of urea, which is one of the scientific ways to improve the efficiency of crops in absorbing and utilizing nitrogen in urea. It can also be achieved by using the dominant single nitrogen fertilizer variety as a carrier to more efficiently solve the problem of magnesium deficiency in agriculture.

[0007] The method of compounding magnesium fertilizer in urea is often to add hydrated magnesium sulfate and / or anhydrous magnesium sulfate. However, anhydrous magnesium sulfate does not exist in nature. The acquisition of anhydrous magnesium sulfate requires high-temperature baking of hydrated magnesium sulfate, which is a complex production process with high energy consumption and cost. In addition, during the preparation process of compounding hydrated magnesium sulfate in urea, the non-crystalline hydrated magnesium sulfate will continuously release its internal crystal water, making granulation difficult and preventing industrial production.

[0008] Summary of the Invention

[0009] According to various embodiments of the present application, a magnesium-containing urea and a preparation method thereof are provided.

[0010] In a first aspect, the present application provides a magnesium-containing urea comprising the following components in parts by weight:

[0011] About 75-90 parts of urea,

[0012] About 6 to 25 parts of kieserite, and

[0013] The flux is about 1 to 10 parts.

[0014] In some embodiments, the following components are included in parts by weight:

[0015] The urea is about 79 to 81 parts,

[0016] The kieserite is about 13 to 14 parts, and

[0017] The flux is about 5 to 8 parts.

[0018] In some embodiments, the following components are included in parts by weight:

[0019] The urea is about 81 parts,

[0020] About 13 parts of the kieserite, and

[0021] The flux is about 6 parts.

[0022] In some embodiments, the following components are included in parts by weight:

[0023] The urea is about 81 parts,

[0024] About 14 parts of the kieserite, and

[0025] The flux is about 5 parts.

[0026] In some embodiments, the following components are included in parts by weight:

[0027] The urea is about 79 parts,

[0028] About 13 parts of the kieserite, and

[0029] The flux is about 8 parts.

[0030] In some embodiments, the flux includes one or both of ammonium sulfate and ammonium chloride.

[0031] In some embodiments, the magnesium-containing urea is in granular form, and the average particle size of the magnesium-containing urea is about 2 mm to 5 mm.

[0032] In some embodiments, in the magnesium-containing urea, the mass percentage of nitrogen is about 32% to 39.26%, and the mass percentage of magnesium is about 1% to 4%.

[0033] In some embodiments, in the magnesium-containing urea, the mass percentage of nitrogen is about 32% to 38%, and the mass percentage of magnesium is about 1% to 4%.

[0034] In a second aspect, the present application further provides a method for preparing the magnesium-containing urea as described in the first aspect, comprising the following steps:

[0035] The granular urea and the flux are heated and melted at a first temperature according to a preset ratio; the heated and melted material is cooled to a second temperature; the kieserite in a preset weight portion is added to the cooled material and heated and mixed to prepare a mixed slurry, or

[0036] heating and mixing the liquid urea, the flux, and the kieserite at a second temperature according to a preset ratio to prepare a mixed slurry; and

[0037] The mixed slurry is granulated to prepare the magnesium-containing urea.

[0038] In some embodiments, the first temperature is about 116° C. to 126° C., and the heating time is about 20 min to 40 min;

[0039] The second temperature is about 100° C. to 115° C., and the heating time is about 3 min to 6 min.

[0040] In some embodiments, the method used to granulate the mixed slurry is a high tower granulation method.

[0041] In some embodiments, the temperature used in the high tower granulation method is about 100°C to 115°C.

[0042] In some embodiments, the step of cooling the obtained magnesium-containing urea is further included, wherein the cooling comprises:

[0043] The magnesium-containing urea droplets exchange heat with the rising air through convection during the dripping process from the top of the tower to the bottom, and are cooled for about 10s to 15s; after leaving the tower, they are cooled by drum cooling and plate cooling respectively.

[0044] In some embodiments, after the cooling, the step of coating the magnesium-containing urea with an anti-caking agent is further included.

[0045] The details of one or more embodiments of the present application are set forth in the following drawings and description. Other features, objects, and advantages of the present application will become apparent from the description, drawings, and claims. BRIEF DESCRIPTION OF THE DRAWINGS

[0046] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the conventional technology, the following briefly introduces the drawings required for use in the embodiments or the conventional technology descriptions. Obviously, the drawings described below are merely embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on the disclosed drawings without any creative work.

[0047] FIG1 is a process flow chart for producing magnesium-containing urea in Example 1 provided in this application;

[0048] Figure 2 is a process flow chart for producing magnesium-containing urea in Example 2 provided in this application;

[0049] FIG3 is a physical picture of the board formed by preparing a high tower granulation pulp board using kieserite provided in this application;

[0050] FIG4 is a physical picture of the board formation of a high tower granulation pulp board prepared by using amorphous magnesium sulfate monohydrate provided by the present application;

[0051] FIG5 is a physical picture (stacked) of the magnesium-containing urea prepared in Example 1 provided in this application;

[0052] Figure 6 is a physical picture (flattened) of the magnesium-containing urea prepared in Example 1 provided in this application. DETAILED DESCRIPTION

[0053] The following will be combined with the drawings in the embodiments of this application to clearly and completely describe the technical solutions in the embodiments of this application. Obviously, the embodiments described are only part of the embodiments of this application, not all of the embodiments. Based on the embodiments in this application, all other embodiments obtained by ordinary technicians in this field without making creative efforts are within the scope of protection of this application.

[0054] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by those skilled in the art to which this application pertains. The terms used herein in the specification of this application are for the purpose of describing specific embodiments only and are not intended to limit this application. The term "and / or" as used herein includes any and all combinations of one or more of the associated listed items.

[0055] Urea (carbamide) is a colorless or white, needle-shaped or rod-shaped crystal that is highly soluble in water (1080 g / L (20°C)). Therefore, the introduction of water must be strictly controlled during the production of magnesium-containing urea. Magnesium sulfate is composed of magnesium ions (Mg 2+ ) and sulfate ions (SO4 2- Urea, a high-nitrogen, water-soluble nitrogen fertilizer, has the advantage of rapid fertilizer effect, but it also has high nitrogen loss and low nutrient efficiency.

[0056] The average nitrogen fertilizer efficiency of urea applied to different crops is about 40%, and the remaining 60% of nitrogen fertilizer is in the form of NH4 + 、NO3 - Magnesium leaches into the soil in the form of nitrogen and NH3, flowing into runoff or volatilizing into the air. This not only fails to promote agricultural production but also pollutes water and air. From a systemic perspective, the scientific application of magnesium fertilizer can improve the absorption and utilization efficiency of nitrogen, phosphorus, and potassium fertilizers, especially nitrogen fertilizer efficiency. Data from magnesium fertilizer trials show that the application of magnesium fertilizer to crops improves nitrogen absorption efficiency by an average of approximately 17%, and nitrogen utilization efficiency by crops by an average of approximately 45.8%. Magnesium supplementation can also reduce the emission of the greenhouse gas nitrous oxide (NO2) during agricultural production. Therefore, increasing the application of magnesium fertilizer during fertilization can improve the fertilizer efficiency of nitrogen fertilizers, promote crop growth, and reduce resource waste and environmental pollution. Furthermore, as urea is an important type of single nitrogen fertilizer, the incorporation of effective magnesium during urea application not only effectively addresses magnesium deficiency in agriculture by using the dominant single nitrogen fertilizer type as a carrier, but also represents a scientific approach to improving the absorption and utilization efficiency of nitrogen from urea by crops.

[0057] However, like other fertilizer nutrients, only magnesium fertilizers that can dissolve in the soil aqueous solution can effectively provide magnesium to crops. In particular, due to the rapid dissolution of urea, the magnesium fertilizer compounded with it should have good water solubility. Among them, the main sources of water-soluble magnesium fertilizers include: magnesium sulfate, magnesium chloride, and magnesium nitrate. Magnesium sulfate is a type of water-soluble magnesium fertilizer and can provide crops with the essential elements magnesium and sulfur. Magnesium chloride is highly hygroscopic, prone to deliquesce and clump, and is not an ideal fertilizer composition. Magnesium nitrate is highly water-soluble, but similar to magnesium chloride, it is highly hygroscopic and prone to clumps. Therefore, magnesium sulfate has higher nutrient effectiveness and safety as an agricultural fertilizer.

[0058] In addition to the availability of magnesium, the amount of magnesium introduced will also affect the crop's demand for magnesium in fertilizers. The amount of magnesium introduced should take into account the crop's demand for magnesium and the crop's demand for nitrogen at a specific application period.

[0059] First, consider that crop nitrogen demand peaks when urea is applied alone, and the addition of magnesium reduces the nitrogen content in urea. To ensure crop nitrogen needs are met, the urea ratio should not be too low. Magnesium added to urea can increase the partial productivity of nitrogen fertilizers, or nitrogen fertilizer efficiency, by an average of approximately 45.8%, maintaining a nitrogen content of no less than 32%. At the average level of magnesium supplementation, urea can replace approximately 46% of traditional urea. Only the sufficient addition of magnesium can reflect the value of magnesium supplementation for crops, and the compound ratio of magnesium, first, refers to the magnesium labeling standard on fertilizer packaging bags in the national standard GB / T 15063-2020 for compound fertilizers, and the elemental magnesium content must be greater than or equal to 1% (Mg≥1%) to be labeled; second, the crops that are currently directly applied with urea are mainly field crops such as wheat and rice. Based on the customary application rate of urea on these crops of about 20 to 40 kilograms per mu, according to the average level of crop yield, the per mu demand for magnesium is about 0.5 kilograms to about 1 kilogram (calculated as elemental magnesium Mg), that is, more than 1% magnesium must be compounded in urea to meet the crop's demand for magnesium.

[0060] When anhydrous magnesium sulfate and hydrated magnesium sulfate (MgSO4·nH2O, 1≤n≤11) are added to urea as magnesium sources, the following problems arise: hydrated magnesium sulfate that can stably exist includes magnesium sulfate heptahydrate (MgSO4·7H2O), magnesium sulfate pentahydrate (MgSO4·5H2O), magnesium sulfate trihydrate (MgSO4·3H2O) and magnesium sulfate monohydrate (MgSO4·H2O). Among them, there is no natural anhydrous magnesium sulfate. Anhydrous magnesium sulfate must be prepared by baking hydrated magnesium sulfate at high temperature. The preparation process is complicated, and the energy consumption and cost are high (about 2 tons of magnesium sulfate heptahydrate and about 400Nm2 of magnesium sulfate are consumed to produce about 1 ton of anhydrous magnesium sulfate). 3 ~450Nm 3 Natural gas); when the temperature of hydrated magnesium sulfate rises, crystal water will precipitate. For example, when the temperature rises to about 68 ° C, MgSO4·7H2O will gradually lose its crystal water.

[0061] If this magnesium sulfate containing crystal water is used in urea production, the gradual release of crystal water will make granulation difficult and industrial production impossible. MgSO4·5H2O, MgSO4·3H2O, and MgSO4·H2O are produced by gradually dehydrating MgSO4·7H2O by heating it. The structure of the hydrated magnesium sulfate produced in this way is an amorphous structure with no repeating atomic structure or fixed shape, resulting in no fixed melting point and loss of water over a wide temperature range (approximately 80°C to approximately 276°C). If it is used to produce magnesium-containing urea, crystal water will be continuously released throughout the production process, making the slurry unable to granulate and thus unsuitable as a raw material for the production of magnesium-containing urea. Moreover, the characteristic of hydrated magnesium sulfate losing crystal water also results in insufficient magnesium addition to urea, which cannot meet the magnesium needs of crops.

[0062] To this end, the present application provides a magnesium-containing urea, which uses sylvite as raw material to solve the problems of the inability to achieve industrial production of magnesium-containing urea, low nitrogen utilization rate in pure urea, and insufficient fertilizer efficiency. At the same time, urea is used as an effective carrier to bring magnesium into the soil to solve the problem of magnesium deficiency in soil and crops.

[0063] In a first aspect, the present application provides a magnesium-containing urea comprising the following components in parts by weight:

[0064] About 75-90 parts of urea,

[0065] About 6 to 25 parts of kieserite, and

[0066] The flux is about 1 to 10 parts.

[0067] The present application uses kaolin as the source of magnesium in magnesium-containing urea. It is naturally occurring and does not require later synthesis. It can be widely used in the production of magnesium-containing urea with urea as a carrier, and has the advantages of simple source, effective nutrients, and low cost. Moreover, kaolin is added to urea as a magnesium source. On the one hand, the introduction of magnesium can improve the utilization efficiency of nitrogen by crops, avoid the emission of greenhouse gases in the production process of magnesium-containing urea, promote the growth of crops, and reduce resource waste and environmental pollution. On the other hand, kaolin itself is a crystal, in which the magnesium ions, sulfate and water molecules are fixed in specific positions. They are arranged in a regular repeating three-dimensional lattice, so that kaolin has a stable molecular structure and a fixed and high dehydration temperature (about 300°C). It has high chemical stability. Therefore, the preparation process of magnesium-containing urea will not cause the precipitation of crystal water. Sufficient magnesium can be introduced into urea to fully meet the needs of crops for nitrogen and magnesium. In summary, the use of kieserite as the magnesium source in magnesium-containing urea is feasible, effective and has a relatively high cost-effectiveness, which enables the industrial production of magnesium-containing urea to be implemented.

[0068] In addition, the flux in magnesium-containing urea can reduce the melting temperature of urea and kieserite during the production process, thereby inhibiting the precipitation of crystal water in kieserite, that is, ensuring that kieserite is always distributed in the urea in the form of crystals; and the reduction of the urea melting temperature can effectively control the generation of biuret.

[0069] Kieserite, also known as kieserite ore crystal powder, natural magnesium sulfate monohydrate, and magnesium sulfate fertilizer, is derived from natural kieserite ore. The atoms, ions, and molecules in kieserite expand to form a three-dimensional arrangement, resulting in a stable crystal structure. Magnesium ions, sulfate groups, and water molecules are locked in place and arranged in a regular, repeating three-dimensional array (lattice). This crystal structure gives kieserite a fixed shape and a dehydration temperature (approximately 300°C), which is higher than the melting point of urea. Therefore, the crystal water within the kieserite is not easily precipitated during the production process, which does not affect urea granulation, making it a very suitable raw material for the production of magnesium-containing urea.

[0070] In some embodiments, the following components are included in parts by weight:

[0071] About 79-81 parts of urea,

[0072] About 13-14 parts of kieserite, and

[0073] About 5 to 8 parts of flux.

[0074] In some embodiments, the following components are included in parts by weight:

[0075] About 81 parts of urea,

[0076] About 13 parts of kieserite, and

[0077] About 6 parts of flux.

[0078] In some embodiments, the following components are included in parts by weight:

[0079] About 81 parts of urea,

[0080] About 14 parts of kieserite, and

[0081] About 5 parts of flux.

[0082] In some embodiments, the following components are included in parts by weight:

[0083] About 79 parts of urea,

[0084] About 13 parts of kieserite, and

[0085] About 8 parts of flux.

[0086] It is understood that the kieserite used in this application can be prepared using commonly used processes in the field of kieserite preparation. For example, physical methods, such as electrostatic separation technology, can be used to separate kieserite ore crystal powder from potassium magnesium ore. The entire preparation process is a physical process without chemical reactions, which is energy-saving and environmentally friendly.

[0087] The process flow of electrostatic separation technology is described in the document “Ullmann Encyclopedia of Industrial Chemistry, Wiley-VCH Verlag GmbH & Co. KGaA: Weinheim, Germany, 2016; pp. 1–35. ISBN 978-3-527-30673-2, in which the author is M.; Wachsmuth, U.; Waldmann, L.; Flachberger, H.; Mirkowska, M.; Brands, L.; Beier, P.-M.; Stahl, I. ". For further information, see page 22 for the separation of kieserite using electrostatic separation (ESTA) technology.

[0088] In the present application, the specific type of urea is not limited, and urea commonly used in the field of fertilizer preparation can be selected, for example, granular urea and / or liquid urea.

[0089] In some embodiments, the flux includes one or both of ammonium sulfate and ammonium chloride.

[0090] In some embodiments, the magnesium-containing urea is in granular form, and the average particle size of the magnesium-containing urea is about 2 mm to 5 mm. That is, the magnesium-containing urea provided in this application is granular magnesium-containing urea with an average particle size of about 2 mm to 5 mm.

[0091] In some embodiments, the weight percentage of nitrogen in the magnesium-containing urea is about 32% to 38%, and the weight percentage of magnesium is about 1% to 4%. It is understood that the weight percentage of nitrogen here refers to the total nitrogen content in the magnesium-containing urea, and the magnesium content can be at least 1%, thereby meeting the magnesium needs of crops.

[0092] In a second aspect, the present application further provides a method for preparing magnesium-containing urea as in the first aspect, comprising steps S100 to S200:

[0093] Step S100: heating and melting granular urea and flux at a first temperature according to a preset ratio; cooling the heated and melted material to a second temperature; adding a preset weight portion of kieserite to the cooled material and heating and mixing to prepare a mixed slurry, or

[0094] Liquid urea, flux and kieserite are heated and mixed at a second temperature according to a preset ratio to prepare a mixed slurry.

[0095] In some embodiments, the first temperature is about 116° C. to 126° C., and the heating time is about 20 min to 40 min;

[0096] The second temperature is about 100° C. to 115° C., and the heating time is about 3 min to 6 min.

[0097] The addition of flux can lower the melting temperature of urea, thereby achieving a lower heating temperature, inhibiting the separation of crystal water in kieserite, and implementing high-tower granulation at a lower granulation temperature, thereby solving the problem that magnesium-containing urea particles cannot harden due to insufficient cooling time during the process of falling from the top of the tower.

[0098] Step S200: granulating the mixed slurry to prepare magnesium-containing urea.

[0099] In some embodiments, the method used to granulate the mixed slurry is a high-tower granulation method, that is, the mixed slurry is sent to a high-tower granulator through a rotary shear spray granulator for spray granulation, and the granulated material sprayed into the granulation tower by the granulator exchanges heat with the air rising from the bottom of the tower through convection during the process of descending from the high tower, and the temperature is reduced and gradually hardened until it falls to the bottom of the tower.

[0100] In some embodiments, the temperature used in the high tower granulation method is about 100°C to 115°C.

[0101] In some embodiments, the step of cooling the obtained magnesium-containing urea after granulation is further included, and the cooling comprises:

[0102] The magnesium-containing urea droplets exchange heat with the rising air through convection during the dripping process from the top of the tower to the bottom, and are cooled for about 10s to 15s; after leaving the tower, they are cooled by drum cooling and plate cooling respectively.

[0103] This process cools the magnesium-containing urea liquid and gradually hardens it until it reaches the bottom of the tower, forming strong and round magnesium-containing urea granules. After leaving the tower, it is cooled to packaging temperature through drum cooling and plate cooling.

[0104] In some embodiments, after cooling, the method further comprises coating the magnesium-containing urea with an anti-caking agent.

[0105] It is understood that the coating method is not limited and any commonly used method in the field of particle coating can be used, for example, spraying.

[0106] In the present application, the type of anti-caking agent is not limited, and any anti-caking agent commonly used in the field of fertilizer preparation can be selected. In some embodiments, the anti-caking agent includes one or more of a powdered anti-caking agent and a liquid anti-caking agent.

[0107] The present application is further described in detail below with reference to specific embodiments.

[0108] The urea used in the following examples and comparative examples is granular urea with the brand name Sunstone purchased from Jincheng Coal Industry Group Co., Ltd.; the kieserite ore crystal powder (kieserite) is a high-purity kieserite ore crystal powder obtained by physical electrostatic separation technology using potassium magnesium ore from potassium magnesium fertilizer mining areas in Thuringia and Hesse, Germany as raw material; wherein the content of magnesium sulfate monohydrate is above 93%, and the rest is a small amount of sulfate and chloride.

[0109] The process flow of electrostatic separation technology is described in the document “Ullmann Encyclopedia of Industrial Chemistry, Wiley-VCH Verlag GmbH & Co. KGaA: Weinheim, Germany, 2016; pp. 1–35. ISBN 978-3-527-30673-2, in which the author is M.; Wachsmuth, U.; Waldmann, L.; Flachberger, H.; Mirkowska, M.; Brands, L.; Beier, P.-M.; Stahl, I. ". For further information, see page 22 for the separation of kieserite using electrostatic separation (ESTA) technology.

[0110] Example 1

[0111] Figure 1 is a process flow chart for producing magnesium-containing urea in this embodiment. As shown in Figure 1, due to the addition of flux, the melting temperature of granular urea and the temperature of the mixing tank during the melting process are reduced. Among them, the mixing tank includes a primary mixing tank and a secondary mixing tank, the temperature of the melting tank is about 116°C to 126°C; the temperature of the primary mixing tank is about 116°C to 126°C; the temperature in the secondary tank is about 100°C to 115°C. The reduction in temperature in each of the above stages can inhibit the precipitation of crystallization water in sulphur magnesium alum, and can implement high-tower granulation at a lower granulation temperature, thereby solving the problem that magnesium-containing urea granules cannot harden due to insufficient cooling time during the process of falling from the top of the tower. The preparation steps are as follows:

[0112] 1) Weigh about 81 parts of urea, about 13 parts of kaolinite and about 6 parts of ammonium chloride. Add urea and ammonium chloride to a melting tank at a temperature of about 116℃~126℃ for high-temperature melting, and stir evenly to form a molten slurry; then uniformly overflow the molten slurry into a first-level mixing tank at a temperature of about 116℃~126℃, and all return materials also enter the mixing tank to maintain the uniform overflow of the slurry, and obtain a uniformly stirred first-level overflow slurry in the first-level mixing tank. Subsequently, the first-level overflow slurry is introduced into a second-level mixing tank at a temperature of about 100℃~112℃, and kaolinite ore crystal powder is added to the second-level mixing tank and stirred for about 3min~6min to obtain a second-level overflow slurry; wherein, the return material refers to the substandard magnesium-containing urea granules formed after high-tower granulation and first-level cooling.

[0113] 2) The second-stage overflow slurry prepared in step 1) is introduced into an emulsifier, and high-speed emulsification and mixing is performed at a temperature of about 112° C. and a rotation speed of about 100 rpm to prepare a mixed slurry.

[0114] 3) The mixed slurry prepared in step 2) is introduced into a high-tower granulator and subjected to centrifugal shear granulation to produce magnesium-containing urea granules. The main process is: as the droplets of the mixed slurry drip from the top of the tower to the bottom of the tower, they form convection with the rising air and exchange heat, thereby lowering the droplet temperature and gradually hardening until the droplets drip to the bottom of the tower to form strong and round magnesium-containing urea granules.

[0115] 4) The magnesium-containing urea granules prepared in step 3) are introduced into a primary cooler and forced cooled at room temperature for about 10 minutes, followed by screening to obtain magnesium-containing urea granules having an average particle size of about 2.89 mm. The magnesium-containing urea granules are then introduced into a secondary cooler and cooled to below about 40° C.

[0116] 5) The magnesium-containing urea particles prepared in step 4) are introduced into a coating conditioning cylinder, and an anti-caking agent is sprayed on the particles through an atomization process. After being coated with the anti-caking agent, magnesium-containing urea with a particle size of about 2.0 mm to 5.0 mm is obtained.

[0117] Example 2

[0118] Figure 2 is a process flow chart for producing magnesium-containing urea in this embodiment. As shown in Figure 2, due to the addition of flux, the melting temperature of granular urea and the temperature of the mixing tank during the melting process are reduced. Among them, the mixing tank includes a primary mixing tank and a secondary mixing tank, the temperature of the melting tank is about 116°C to 126°C; the temperature of the primary mixing tank is about 116°C to 126°C; the temperature in the secondary tank is about 100°C to 112°C. The reduction in temperature in each of the above stages can inhibit the precipitation of crystallization water in sulphur magnesium alum, and can implement high-tower granulation at a lower granulation temperature, thereby solving the problem that magnesium-containing urea granules cannot harden due to insufficient cooling time during the process of falling from the top of the tower. The preparation steps are as follows:

[0119] 1) Weigh approximately 81 parts of urea, approximately 14 parts of kieserite, and approximately 5 parts of ammonium chloride. Add approximately 50 parts of urea and approximately 3 parts of ammonium chloride to a melting tank at a temperature of approximately 116°C to 126°C for high-temperature melting and stir evenly to form a molten slurry; then, uniformly overflow the molten slurry and the remaining approximately 31 parts of urea and approximately 2 parts of ammonium chloride into a primary mixing tank at a temperature of approximately 116°C to 126°C. All return materials also enter this mixing tank, maintaining a uniform overflow of the slurry, and obtain a uniformly stirred first-stage overflow slurry in the primary mixing tank. Subsequently, the first-stage overflow slurry is introduced into a secondary mixing tank at a temperature of approximately 100°C to 112°C, and kieserite ore crystal powder is added to the secondary mixing tank and stirred for approximately 3 minutes to 6 minutes to obtain a second-stage overflow slurry; wherein, the return material refers to the substandard magnesium-containing urea granules formed after high-tower granulation and primary cooling.

[0120] 2) The second-stage overflow slurry prepared in step 1) is introduced into an emulsifier, and high-speed emulsification and mixing is performed at a temperature of about 110° C. and a rotation speed of about 100 rpm to prepare a mixed slurry.

[0121] 3) The mixed slurry prepared in step 2) is introduced into a high-tower granulator and subjected to centrifugal shear granulation to produce magnesium-containing urea granules. The main process is: as the droplets of the mixed slurry drip from the top of the tower to the bottom of the tower, they form convection with the rising air and exchange heat, thereby lowering the droplet temperature and gradually hardening until the droplets drip to the bottom of the tower to form strong and round magnesium-containing urea granules.

[0122] 4) The magnesium-containing urea granules prepared in step 3) are introduced into a primary cooler and forced cooled at room temperature for about 10 minutes, followed by screening to obtain magnesium-containing urea granules having an average particle size of about 2.89 mm. The magnesium-containing urea granules are then introduced into a secondary cooler and cooled to below about 40° C.

[0123] 5) The magnesium-containing urea particles prepared in step 4) are introduced into a coating conditioning cylinder, and an anti-caking agent is sprayed on the particles through an atomization process. After being coated with the anti-caking agent, magnesium-containing urea with a particle size of about 2.0 mm to 5.0 mm is obtained.

[0124] Example 3

[0125] The preparation method of this embodiment is basically the same as that of Example 1, except that the amounts of urea, kieserite, and ammonium chloride added are different. The steps are as follows:

[0126] 1) Weigh about 79 parts of urea, about 13 parts of kaolinite and about 8 parts of ammonium chloride. Add urea and ammonium chloride to a melting tank at a temperature of about 116℃~126℃ for high-temperature melting, and stir evenly to form a molten slurry; then uniformly overflow the molten slurry into a first-level mixing tank at a temperature of about 116℃~126℃, and all return materials also enter the mixing tank to maintain the uniform overflow of the slurry, and obtain a uniformly stirred first-level overflow slurry in the first-level mixing tank. Subsequently, the first-level overflow slurry is introduced into a second-level mixing tank at a temperature of about 100℃~112℃, and kaolinite ore crystal powder is added to the second-level mixing tank and stirred for about 3min~6min to obtain a second-level overflow slurry; wherein, the return material refers to the substandard magnesium-containing urea granules formed after high-tower granulation and first-level cooling.

[0127] 2) The second-stage overflow slurry prepared in step 1) is introduced into an emulsifier, and high-speed emulsification and mixing is performed at a temperature of about 110° C. and a rotation speed of about 100 rpm to prepare a mixed slurry.

[0128] 3) The mixed slurry prepared in step 2) is introduced into a high-tower granulator and subjected to centrifugal shear granulation to produce magnesium-containing urea granules. The main process is: as the droplets of the mixed slurry drip from the top of the tower to the bottom of the tower, they form convection with the rising air and exchange heat, thereby lowering the droplet temperature and gradually hardening until the droplets drip to the bottom of the tower to form strong and round magnesium-containing urea granules.

[0129] 4) The magnesium-containing urea granules prepared in step 3) are introduced into a primary cooler and forced cooled at room temperature for about 10 minutes, followed by screening to obtain magnesium-containing urea granules having an average particle size of about 2.89 mm. The magnesium-containing urea granules are then introduced into a secondary cooler and cooled to below about 40° C.

[0130] 5) The magnesium-containing urea particles prepared in step 4) are introduced into a coating conditioning cylinder, and an anti-caking agent is sprayed on the particles through an atomization process. After being coated with the anti-caking agent, magnesium-containing urea with a particle size of about 2.0 mm to 5.0 mm is obtained.

[0131] Comparative Example 1

[0132] The preparation method of Comparative Example 1 was carried out using a laboratory high tower simulated pulp plate experiment. The difference from Example 1 is that amorphous magnesium sulfate monohydrate was used instead of kieserite. The steps are as follows:

[0133] Weigh approximately 81 parts urea, approximately 14 parts magnesium sulfate monohydrate, and approximately 5 parts ammonium chloride. Premix the urea and ammonium chloride and gradually heat to approximately 120°C to produce a molten material. Stir the molten material continuously while slowly adding magnesium sulfate monohydrate, continuing to stir to ensure uniform mixing. Pour the homogenized material onto a dedicated platform for simulated granulation towers and assess granulation feasibility.

[0134] As shown in Figures 3 and 4, judging from the board-forming situation of the pulp board, after adding the magnesium sulfate monohydrate with an amorphous structure, the slurry density is small, the concentration is low, the slurry fluidity is too good, and the slurry is not completely solidified into a board within about 30 seconds after landing. Because in the high tower process, the time for the slurry to do free fall from the top of the tower to the bottom of the tower will not exceed 15 seconds. Therefore, the slurry with the addition of magnesium sulfate monohydrate with an amorphous structure cannot be solidified into particles with suitable hardness before landing. It can be seen from this that this slurry formula cannot be put on the tower and industrial production cannot be achieved. That is, according to the high tower simulation pulp board experimental evaluation method, it can be seen that Comparative Example 1 cannot be granulated using the high tower process.

[0135] The magnesium-containing urea prepared in Examples 1 to 3 and Comparative Example 1 was subjected to relevant performance tests, and the test results are shown in Table 1 below.

[0136] The actual images of the magnesium-containing urea prepared in Example 1 are shown in Figures 5 and 6 respectively.

[0137] 1) The total magnesium content in the magnesium-containing urea prepared in Examples 1 to 3 was measured according to the national standard GB / T 19203-2003, calculated as Mg;

[0138] 2) testing the free water content in the magnesium-containing urea prepared in Examples 1 to 3 according to the national standard GB / T 8576-2010;

[0139] 3) The total nitrogen content in the magnesium-containing urea prepared in Examples 1 to 3 was measured according to the national standard GB / T 2440-2017, calculated as N;

[0140] 4) The biuret content in the magnesium-containing urea prepared in Examples 1 to 3 was tested according to the national standard GB / T 22924-2008.

[0141] Table 1

[0142] As can be seen from Table 1 above, after adding kieserite and flux, qualified magnesium-containing urea can be produced under strict and effective control of process conditions, which not only can achieve sufficient addition of magnesium in urea, but also can effectively control the production of biuret.

[0143] The technical features of the above-mentioned embodiments can be combined arbitrarily. In order to make the description concise, not all possible combinations of the technical features in the above-mentioned embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.

[0144] The above-described embodiments merely represent several implementation methods of the present application. While the descriptions are relatively specific and detailed, they should not be construed as limiting the scope of the patent application. It should be noted that a person of ordinary skill in the art may make various modifications and improvements without departing from the spirit of the present application, and these modifications and improvements fall within the scope of protection of the present application. Therefore, the scope of protection of the present patent application shall be determined by the appended claims.

Claims

1. A magnesium-containing urea, characterized in that: The invention comprises the following components in parts by weight: about 75 to 90 parts of urea, about 6 to 25 parts of kieserite, and about 1 to 10 parts of flux.

2. The magnesium-containing urea according to claim 1, characterized in that The invention comprises the following components in parts by weight: about 79 to 81 parts of urea, about 13 to 14 parts of kieserite, and about 5 to 8 parts of flux.

3. The magnesium-containing urea according to any one of claims 1 to 2, characterized in that The invention comprises the following components in parts by weight: about 81 parts of urea, about 13 parts of kieserite, and about 6 parts of flux.

4. The magnesium-containing urea according to any one of claims 1 to 2, characterized in that The invention comprises the following components in parts by weight: about 81 parts of urea, about 14 parts of kieserite, and about 5 parts of flux.

5. The magnesium-containing urea according to any one of claims 1 to 2, characterized in that The invention comprises the following components in parts by weight: about 79 parts of urea, about 13 parts of kieserite, and about 8 parts of flux.

6. The magnesium-containing urea according to any one of claims 1 to 5, characterized in that The flux includes one or both of ammonium sulfate and ammonium chloride.

7. The magnesium-containing urea according to any one of claims 1 to 6, characterized in that The magnesium-containing urea is in granular form, and the average particle size of the magnesium-containing urea is about 2 mm to 5 mm.

8. The magnesium-containing urea according to any one of claims 1 to 7, characterized in that In the magnesium-containing urea, the mass percentage of nitrogen element is about 32% to 39.26%, and the mass percentage of magnesium element is about 1% to 4%.

9. The magnesium-containing urea according to any one of claims 1 to 8, characterized in that In the magnesium-containing urea, the mass percentage of nitrogen element is about 32% to 38%, and the mass percentage of magnesium element is about 1% to 4%.

10. A method for preparing magnesium-containing urea according to any one of claims 1 to 9, characterized in that: The following steps are involved: The granular urea and the flux are heated and melted at a first temperature according to a preset ratio; the heated and melted material is cooled to a second temperature; a preset weight portion of the kieserite is added to the cooled material and heated and mixed to prepare a mixed slurry, or heating and mixing the liquid urea, the flux and the kieserite according to a preset ratio at a second temperature to prepare a mixed slurry; and The mixed slurry is granulated to prepare the magnesium-containing urea.

11. The preparation method according to claim 10, characterized in that: The first temperature is about 116°C to 126°C, and the heating time is about 20min to 40min; The second temperature is about 100° C. to 115° C., and the heating time is about 3 min to 6 min.

12. The preparation method according to any one of claims 9 to 10, characterized in that: The method used for granulating the mixed slurry is a high tower granulation method.

13. The preparation method according to claim 12, characterized in that: The temperature used in the high tower granulation method is about 100°C to 115°C.

14. The preparation method according to any one of claims 9 to 13, characterized in that: The method further comprises cooling the obtained magnesium-containing urea, wherein the cooling comprises: The magnesium-containing urea droplets exchange heat with the rising air through convection during the dripping process from the top of the tower to the bottom of the tower, and are cooled for about 10s to 15s; after leaving the tower, they are cooled by drum cooling and plate cooling respectively.

15. The preparation method according to claim 14, characterized in that: After the cooling, the method further comprises the step of coating the magnesium-containing urea with an anti-caking agent.

Citation Information

Patent Citations

  • Method for controlling content of biuret in compound fertilizers for melt granulation in prilling tower

    CN102701846A

  • Special peach tree fertilizer and preparation method thereof

    CN103992166A

  • Fertilizer formula for peach planting

    CN106348890A

  • Production method for urea-based melt compound fertilizer with low biuret content

    CN106365724A

  • High-magnesium-nitrogen-potassium compound fertilizer, preparation method thereof, and mineral-sourced long-acting magnesium-nitrogen-potassium compound fertilizer

    CN113214023A