Display module, method for manufacturing display module, and display device

By setting a light shielding layer and a reflective layer in the OLED flexible screen, the curing effect is improved by using multi-angle curing light sources, the problem of unsatisfactory curing of the glue layer is solved, and the folding reliability and performance of the OLED screen is improved.

WO2024245298A1PCT designated stage expired Publication Date: 2024-12-05BOE TECHNOLOGY GROUP CO LTD +1
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
PCT/CN2024/096128
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-05-29
Filing Date
2024-05-29
Publication Date
2024-12-05

AI Technical Summary

Technical Problem

When making OLED flexible screens, the glue layer curing effect is not ideal, resulting in insufficient adhesive force, the edges of the OLED screen are prone to cracking, and the lower edge area cannot be completely cured, which reduces the reliability of folding and product performance.

Method used

By setting a light shielding layer and a reflective layer in the display module, the transparent adhesive layer is irradiated from the display area and sides with a cured light source, ensuring that the light can effectively penetrate and fully cure the adhesive layer, improving the bonding strength and folding trust sex.

Benefits of technology

It achieves a more complete curing effect, improves the folding trust and product performance of the OLED flexible screen, and enhances the stability and competitiveness of the edge.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2024096128_05122024_PF_FP_ABST
    Figure CN2024096128_05122024_PF_FP_ABST
Patent Text Reader

Abstract

Disclosed are a display module, a method for manufacturing a display module, and a display device, which relate to the technical field of displays. The display module comprises a display panel (100), a transparent adhesive layer (110), a cover plate (120), a light-shielding layer (130) and a first light-reflecting layer (140), wherein the transparent adhesive layer (110) is located on a side of a light emission surface (101) of the display panel (100); the cover plate (120) is located on the side of the transparent adhesive layer (110) away from the display panel (100); the orthographic projection of the light-shielding layer (130) located between the cover plate (120) and the display panel (100) on the display panel (100) is located in a peripheral area (20) of the display panel (100); and the orthographic projection of the first light-reflecting layer (140) located between the transparent adhesive layer (110) and the light-shielding layer (130) on the display panel (100) is located in the peripheral area (20) of the display panel (100), and the orthographic projection of the first light-reflecting layer (140) on the display panel (100) and the orthographic projection of the light-shielding layer (130) on the display panel (100) have an overlapping area. The present disclosure improves the folding reliability of the display module.
Need to check novelty before this filing date? Find Prior Art

Description

Display module, method for manufacturing display module, and display device

[0001] This disclosure claims priority to Chinese patent application No. 202310622325.2, filed on May 29, 2023, entitled “Display module, method for manufacturing display module and display device,” the entire contents of which are incorporated herein by reference. Technical Field

[0002] The present disclosure relates to the field of display technology, and in particular to a display module, a method for manufacturing a display module, and a display device. Background Art

[0003] Organic Light-Emitting Diode (OLED), also known as Organic Electroluminesence Display (OLED) or organic light-emitting semiconductor, works on the principle that organic semiconductor materials and luminescent materials, driven by an electric field, emit light through carrier injection and recombination. Compared with traditional liquid crystal panels and thin film transistor (TFT) screens, OLED has the advantages of faster response speed, higher contrast, wider viewing angle, lighter weight, and better flexibility. OLED is currently widely used in electronic products such as mobile phones, tablets, and watches. With the development of display technology, OLED flexible screens can be made into display modules in various forms such as curved, foldable, special-shaped, and curled due to their soft properties. Flexible products are becoming more and more widely used, and improving their bending and curling properties is becoming increasingly important.

[0004] Summary of the Invention

[0005] The present disclosure provides a display module, a method for manufacturing the display module, and a display device.

[0006] In one aspect, a display module is provided, comprising: a display panel having a display area and a peripheral area surrounding the display area;

[0007] a transparent adhesive layer, the transparent adhesive layer being located on one side of the light emitting surface of the display panel;

[0008] a cover plate, the cover plate being located on a side of the transparent adhesive layer away from the display panel;

[0009] a light shielding layer, the light shielding layer being located between the cover plate and the display panel, and an orthographic projection of the light shielding layer on the display panel being located in a peripheral area of ​​the display panel;

[0010] At least one light-reflecting layer, the at least one light-reflecting layer comprising a first light-reflecting layer located between the transparent adhesive layer and the light-shielding layer, the orthographic projection of the first light-reflecting layer on the display panel being located in a peripheral area of ​​the display panel, and an orthographic projection of the first light-reflecting layer on the display panel and an orthographic projection of the light-shielding layer on the display panel having an overlapping area.

[0011] Optionally, the orthographic projection of the first light reflecting layer on the display panel completely overlaps with the orthographic projection of the light shielding layer on the display panel.

[0012] Optionally, the at least one reflective layer further includes a second reflective layer located between the transparent adhesive layer and the display panel, the orthographic projection of the second reflective layer on the display panel is located in a peripheral area of ​​the display panel, and the orthographic projection of the second reflective layer on the display panel and the orthographic projection of the shading layer on the display panel have an overlapping area.

[0013] Optionally, an orthographic projection of the second light reflecting layer on the display panel completely overlaps with an orthographic projection of the light shielding layer on the display panel.

[0014] Optionally, the reflective layer includes a multi-layer composite structure, and each layer of the composite structure includes niobium oxide and silicon dioxide stacked together.

[0015] Optionally, the reflective layer includes five layers of the composite structure, and the thickness of each layer of the composite structure is in a range of 100 nanometers to 800 nanometers.

[0016] Optionally, the light-shielding layer includes a first straight portion and a second straight portion stacked in sequence along a direction close to the light-emitting surface of the display panel, and the orthographic projection area of ​​the first straight portion on the display panel is larger than the orthographic projection area of ​​the second straight portion on the display panel.

[0017] Optionally, the orthographic projection of the second straight portion on the display panel is located in a central area of ​​the orthographic projection of the first straight portion on the display panel.

[0018] Optionally, the cross-sectional shape of the light shielding layer along a direction perpendicular to the light emitting surface of the display panel is one of the following: a plane type, a wave type, or a groove type structure; wherein the notch of the groove type structure faces the display panel.

[0019] Optionally, the material of the transparent adhesive layer is optical glue or optical resin.

[0020] Optionally, the display panel includes a base substrate and a plurality of light-emitting devices, a pixel defining layer and an encapsulation layer sequentially arranged on one side of the base substrate, and the pixel defining layer is used to separate the plurality of light-emitting devices.

[0021] Optionally, the light-emitting device is a bottom-emitting light-emitting device, and the encapsulation layer includes a first inorganic layer, an organic layer, and a second inorganic layer stacked in a direction away from the base substrate;

[0022] The display module further includes a waterproof layer and an adhesive layer. The waterproof layer is located on a side of the second inorganic layer away from the base substrate, and the adhesive layer is located between the second inorganic layer and the waterproof layer.

[0023] Optionally, the waterproof layer is aluminum foil or copper foil.

[0024] Optionally, along a direction parallel to the plane where the base substrate is located, the edge of the organic layer is retracted by 1 mm to 2 mm relative to the edges of the first inorganic layer and the second inorganic layer;

[0025] The display module further includes a first adhesive layer, which is disposed on the same layer as the organic layer and is used to bond the first inorganic layer and the second inorganic layer.

[0026] Optionally, along a direction parallel to the plane of the base substrate, the outer edges of the waterproof layer and the second inorganic layer are flush and indented by 0.5 mm to 1 mm relative to the edge of the first inorganic layer; the edge of the organic layer is indented by 1 mm to 2 mm relative to the edge of the first inorganic layer;

[0027] The display module further includes a second adhesive layer, which covers the surface of the waterproof layer away from the base substrate, as well as side surfaces of the waterproof layer, the adhesive layer, the second inorganic layer, the organic layer, and the first inorganic layer.

[0028] In another aspect, a method for manufacturing a display module is provided, for manufacturing the display module according to any one of the above aspects, the manufacturing method comprising:

[0029] preparing a display panel, the display panel having a display area and a peripheral area surrounding the display area;

[0030] preparing a transparent adhesive layer on one side of the light emitting surface of the display panel;

[0031] A light shielding layer is formed on a side of the transparent adhesive layer away from the display panel, wherein an orthographic projection of the light shielding layer on the display panel is located in a peripheral area of ​​the display panel;

[0032] A first light reflecting layer is formed on a side of the light-shielding layer away from the display panel, wherein an orthographic projection of the first light reflecting layer on the display panel is located in a peripheral area of ​​the display panel, and an orthographic projection of the first light reflecting layer on the display panel overlaps with an orthographic projection of the light-shielding layer on the display panel;

[0033] A cover plate is prepared on a side of the first light reflecting layer away from the display panel.

[0034] Optionally, a first light reflecting layer is formed on a side of the light shielding layer away from the display panel, comprising:

[0035] The first light reflecting layer is prepared on the side of the light shielding layer away from the display panel by adopting a discontinuous coating process, a coating process, a bonding process or a hot-melt process.

[0036] Optionally, before preparing the transparent adhesive layer on one side of the light emitting surface of the display panel, the manufacturing method further includes:

[0037] A second light reflecting layer is prepared on one side of the light emitting surface of the display panel, the orthographic projection of the second light reflecting layer on the display panel is located in the peripheral area of ​​the display panel, and the orthographic projection of the second light reflecting layer on the display panel and the orthographic projection of the light shading layer on the display panel have an overlapping area.

[0038] Optionally, a second light reflecting layer is prepared on one side of the light emitting surface of the display panel, comprising:

[0039] The second light reflecting layer is prepared on one side of the light emitting surface of the display panel by adopting a discontinuous coating process, a coating process, a bonding process or a hot-melt process.

[0040] In yet another aspect, a display device is provided, comprising the display module described in any one of the above aspects. BRIEF DESCRIPTION OF THE DRAWINGS

[0041] FIG1 is a schematic structural diagram of a display module provided by an embodiment of the present disclosure;

[0042] FIG2 is a schematic diagram of a curing light source according to an embodiment of the present disclosure irradiating a transparent adhesive layer from a display area;

[0043] FIG3 is a schematic diagram of a curing light source provided by an embodiment of the present disclosure irradiating a transparent adhesive layer from the side of a display module;

[0044] FIG4 is a schematic structural diagram of another display module provided by an embodiment of the present disclosure;

[0045] FIG5 is a schematic diagram of a combined structure of a light-shielding layer and a light-reflecting layer provided in an embodiment of the present disclosure;

[0046] FIG6 is a schematic structural diagram of another display module provided by an embodiment of the present disclosure;

[0047] FIG7 is a schematic structural diagram of another display module provided in an embodiment of the present disclosure;

[0048] FIG8 is a schematic diagram of the film layer composition of a display module provided by an embodiment of the present disclosure;

[0049] FIG9 is a schematic structural diagram of another display module provided in an embodiment of the present disclosure;

[0050] FIG10 is a schematic structural diagram of a display module provided in another embodiment of the present disclosure;

[0051] FIG11 is a schematic structural diagram of another display module provided by another embodiment of the present disclosure;

[0052] FIG12 is a schematic structural diagram of another display module provided in another embodiment of the present disclosure;

[0053] FIG13 is a schematic structural diagram of yet another display module provided in another embodiment of the present disclosure;

[0054] FIG14 is a schematic diagram of preparing a first adhesive layer according to an embodiment of the present disclosure;

[0055] FIG15 is a schematic diagram of preparing a second inorganic layer according to an embodiment of the present disclosure;

[0056] FIG16 is a cross-sectional view of an edge of the display module shown in FIG7 provided by an embodiment of the present disclosure;

[0057] FIG17 is a flow chart of a method for manufacturing a display module provided in an embodiment of the present disclosure. DETAILED DESCRIPTION

[0058] The following will be combined with the accompanying drawings in the embodiments of the present disclosure to clearly and completely describe the technical solutions in the embodiments of the present disclosure. Obviously, the embodiments described are only part of the embodiments of the present disclosure, rather than all the embodiments. Based on the embodiments of the present disclosure, all other embodiments obtained by ordinary technicians in this field based on the present disclosure are within the scope of protection of the present disclosure.

[0059] Currently, when making OLED flexible screens, it is necessary to use an adhesive layer to bond the display panel and the cover plate, and the adhesive layer absorbs the curing light before performing the curing. During the curing process, since ink is provided on the lower edge of the OLED flexible screen cover plate, when the display panel is deformed or the angle of the curing light changes, the curing light will be absorbed by the ink, resulting in the curing light being unable to penetrate the adhesive layer along the side of the adhesive layer. The curing depth is limited, and the curing effect is not ideal, resulting in insufficient adhesion of the adhesive layer, which in turn causes the edge of the OLED flexible screen to crack easily. In addition, the lower edge area of ​​the OLED flexible screen is close to the bending area, and excessive side curing energy will damage the display panel. Therefore, curing light with too high energy cannot be used, resulting in the lower edge area of ​​the OLED flexible screen being unable to achieve complete curing, reducing the reliability and trustworthiness of the OLED flexible screen folding, and reducing the performance and competitiveness of the display product.

[0060] To improve the folding reliability of OLED flexible screens and enhance product performance and competitiveness, embodiments of the present disclosure provide a display module. For example, Figure 1 is a schematic structural diagram of a display module provided by embodiments of the present disclosure. As shown in Figure 1 , the display module includes a display panel 100, a transparent adhesive layer 110, a cover plate 120, a light-shielding layer 130, and at least one reflective layer. The at least one reflective layer includes a first reflective layer 140.

[0061] The display panel 100 has a display area 10 and a peripheral area 20 surrounding the display area 10 .

[0062] The transparent adhesive layer 110 is located on a side of the light emitting surface 101 of the display panel 100 . The cover plate 120 is located on a side of the transparent adhesive layer 110 away from the display panel 100 .

[0063] The light shielding layer 130 is located between the cover plate 120 and the display panel 100, and its orthographic projection on the display panel 100 is located in the peripheral area of ​​the display panel 100. In the disclosed embodiment, by disposing the light shielding layer 130 between the cover plate 120 and the display panel 100 and in the peripheral area 20 of the display panel 100, the light shielding layer 130 can shield the metal traces in the peripheral area 20 of the display panel 100, thereby meeting the appearance requirements of the display module.

[0064] The first light reflecting layer 140 is located between the transparent adhesive layer 110 and the light shielding layer 130. Specifically, the first light reflecting layer 140 is located on the side of the transparent adhesive layer 110 away from the display panel 100, and on the side of the light shielding layer 130 closer to the display panel 100. The orthographic projection of the first light reflecting layer 140 on the display panel 100 overlaps with the orthographic projection of the light shielding layer 130 on the display panel 100. The side of the first light reflecting layer 140 away from the light emitting surface 101 of the display panel 100 can be laminated to the light shielding layer 130, and the side closer to the light emitting surface 101 of the display panel 100 can be laminated to the transparent adhesive layer 110.

[0065] The transparent adhesive layer 110 is used to bond the display panel 100 and the cover plate 120. During the bonding process, after the transparent adhesive layer 110 is printed or applied to the display panel 100, the transparent adhesive layer 110 is first pre-cured, that is, the surface of the transparent adhesive layer 110 is irradiated with a curing light source so that the surface of the transparent adhesive layer 110 is first cured. After the cover plate 120 and the transparent adhesive layer 110 are attached to each other, the curing light source is used to irradiate the transparent adhesive layer 110 for main curing (that is, deep curing of the transparent adhesive layer 110), thereby making the display panel 100 and the cover plate 120 fully bonded to improve the folding performance of the flexible display screen. In the embodiment of the present disclosure, a curing light source can be set to irradiate the transparent adhesive layer 110 from above the display module (that is, the display area 10) and from the side of the display module. For example, Figure 2 is a schematic diagram of the curing light source provided in the embodiment of the present disclosure irradiating the transparent adhesive layer from the display area. As shown in FIG2 , the curing light source 700 can irradiate the transparent adhesive layer 110 from the display area 10 of the display module, so that the middle portion of the transparent adhesive layer 110 that is not blocked by the light shielding layer 130 can be deeply cured, thereby enabling the cover plate 120 and the middle portion of the display panel 100 to be fully bonded. For another example, FIG3 is a schematic diagram of the curing light source provided in an embodiment of the present disclosure irradiating the transparent adhesive layer from the side of the display module. As shown in FIG3 , the curing light source 700 can irradiate the transparent adhesive layer 110 from the side of the display module, which can achieve deep curing of the edge of the transparent adhesive layer 110, thereby enabling the cover plate 120 and the edge portion of the display panel 100 to be fully bonded.

[0066] When a curing light source is configured to illuminate the transparent adhesive layer from the display area to cure the transparent adhesive layer 110, due to the light shielding layer 130 provided between the cover plate 120 and the display panel 100, the curing light perpendicular to the transparent adhesive layer 110 will be absorbed by the light shielding layer 130, resulting in the curing light being unable to illuminate the transparent adhesive layer 110. This in turn causes the edges of the transparent adhesive layer 110 to not be cured or to be incompletely cured. When a curing light source is configured to illuminate the transparent adhesive layer from the side of the display module to cure the transparent adhesive layer 110, if the curing light source 700 is tilted or the display panel 100 is deformed, the curing light will not be parallel to the extension direction of the transparent adhesive layer 110. In this case, the curing light will be absorbed by the light shielding layer 130 after being illuminated, and will not be able to penetrate the transparent adhesive layer 110 in the peripheral area 20. This will prevent the curing light from completely curing the sides of the transparent adhesive layer. In the embodiment of the present disclosure, a first light reflecting layer 140 is provided between the light shielding layer 130 and the transparent adhesive layer 110. The first light reflecting layer 140 has excellent light reflecting properties. When the curing light irradiates the transparent adhesive layer 110 along the side of the display module, even if the curing light is not parallel to the transparent adhesive layer 110, the curing light can be reflected by the first light reflecting layer 140. As a result, the curing light does not directly irradiate the light shielding layer 130 and be absorbed, but is instead reflected onto the transparent adhesive layer 110. This achieves efficient utilization of the curing light, ensures that the transparent adhesive layer 110 is fully irradiated by the curing light, and further ensures that the edges of the transparent adhesive layer 110 are fully cured, thereby improving the folding reliability of the display module and further enhancing the performance and competitiveness of the product.

[0067] Optionally, the orthographic projection of the first light reflecting layer 140 on the display panel 100 completely overlaps with the orthographic projection of the light shielding layer 130 on the display panel 100. That is, the first light reflecting layer 140 can completely cover the light shielding layer 130, thereby reducing the probability of the curing light being absorbed by the light shielding layer 130 when irradiated from the side of the display module.

[0068] Optionally, the material of the first reflective layer 140 includes, but is not limited to, aluminum oxide, titanium dioxide, niobium oxide, zinc oxide, zirconium dioxide, or titanium dioxide. The material of the first reflective layer 140 is a metal or plastic material with high ultraviolet reflectivity. The present embodiment does not limit the material of the first reflective layer.

[0069] Optionally, the material of the light shielding layer 130 includes but is not limited to black ink, and may also be other black coatings or plating layers. The light shielding layer 130 may be prepared by an inkjet printing process.

[0070] Optionally, the material of the cover plate 120 includes but is not limited to polyethylene terephthalate (PET), colorless polyimide (CPI) or colorless glass.

[0071] Optionally, the at least one reflective layer further includes a second reflective layer. For example, FIG4 is a schematic structural diagram of another display module provided by an embodiment of the present disclosure. As shown in FIG4 , in addition to the display module shown in FIG1 , the display module further includes a second reflective layer 150. The second reflective layer 150 is positioned between the transparent adhesive layer 110 and the display panel 100. The orthographic projection of the second reflective layer 150 on the display panel 100 is located in the peripheral area 20 of the display panel 100, and the orthographic projection of the second reflective layer 150 on the display panel 100 overlaps with the orthographic projection of the light-shielding layer 130 on the display panel 100.

[0072] Optionally, the orthographic projection of the second light reflecting layer 150 on the display panel 100 completely overlaps with the orthographic projection of the light shielding layer 130 on the display panel 100 .

[0073] In the disclosed embodiment, when curing light is irradiated onto the first light reflecting layer 140 and the second light reflecting layer 150, since both the first light reflecting layer 140 and the second light reflecting layer 150 have reflective properties, curing can be performed simultaneously on both the upper and lower surfaces of the transparent adhesive layer 110. This can further improve the curing effect of the transparent adhesive layer 110 compared to curing only the upper layer of the transparent adhesive layer 110. Furthermore, since the first light reflecting layer 140 and the second light reflecting layer 150 are provided on the upper and lower surfaces of the transparent adhesive layer 110, respectively, light that has passed through the transparent adhesive layer 110 can be reflected back to the surface of the transparent adhesive layer 110, thereby improving the utilization rate of the reflected light and ensuring that the transparent adhesive layer 110 can be completely cured even with low-energy curing light.

[0074] Optionally, the side of the second light reflecting layer 150 away from the light emitting surface 101 of the display panel 100 may be attached to the transparent adhesive layer 110 , and the side close to the light emitting surface 101 of the display panel 100 may be attached to the display panel 100 .

[0075] Optionally, the second light reflecting layer 150 may be made of the same material and have the same thickness as the first light reflecting layer 140 .

[0076] Alternatively, Figure 5 is a schematic diagram of a combined structure of a light-shielding layer and a light-reflecting layer provided in an embodiment of the present disclosure. As shown in Figure 5 , the light-reflecting layer (e.g., the first light-reflecting layer 140 and the second light-reflecting layer 150) comprises a multi-layer composite structure, each layer of which comprises a stacked arrangement of niobium oxide and silicon dioxide.

[0077] For example, please continue to refer to Figure 12. The reflective layer (such as the first reflective layer 140) is a discontinuous electroplating layer (Non-conductive vacuum metalization, NCVM). The reflective layer is a multi-layer composite structure, which enables the reflective layer to fully reflect light. Due to the different refractive indices of niobium oxide and silicon dioxide, the high and low refractive indices of the media in the composite structure overlap with each other, which can achieve a higher reflectivity of the reflective layer, thereby allowing the edge of the transparent adhesive layer 110 to be better cured. Among them, the composite structure can be a laminated structure, and the present disclosure does not limit the stacking order in the laminated structure. For example, along the direction from the light shielding layer 130 to the display panel 100, the stacking order can be niobium oxide, silicon dioxide, niobium oxide and silicon dioxide, or it can be silicon dioxide, niobium oxide, silicon dioxide, niobium oxide.

[0078] Optionally, the reflective layer comprises a five-layer composite structure. For example, the first reflective layer 140 and the second reflective layer 150 each comprise a five-layer composite structure. The thickness of each composite structure layer ranges from 100 nanometers to 800 nanometers, meaning the thickness of the reflective layer ranges from 500 nanometers to 4000 nanometers. The 100-800 nanometer thickness of each layer allows the curing light to penetrate the laminated layers, thereby allowing the curing light to be fully reflected between the first reflective layer 140 and the second reflective layer 150. For example, the thickness of each composite structure layer ranges from 200 nanometers to 400 nanometers.

[0079] Optionally, Figures 6 and 7 are schematic diagrams of the structure of a display module provided in an embodiment of the present disclosure. As shown in Figure 6, based on the display module shown in Figure 1, a protective film 800 may be provided on the side of the cover plate 120 away from the display panel 100. As shown in Figure 7, based on the display module shown in Figure 4, a protective film 800 may be provided on the side of the cover plate 120 away from the display panel 100. The protective film 800 is used to protect the cover plate 120 from scratches, thereby extending the service life of the display module.

[0080] Alternatively, Figure 8 is a schematic diagram of the film layer composition of a display module provided in an embodiment of the present disclosure. As shown in Figure 8, the display module may include a display panel 100, a transparent adhesive layer 110, a cover plate 120, a polarizer 200, a backing film 300, a support member 400, a control chip 500, and a flexible circuit board 600. The backing film 300 may be made of a transparent insulating material, such as polyester resin, and is used to protect and support the display panel 100.

[0081] Alternatively, Figure 9 is a schematic structural diagram of another display module provided by an embodiment of the present disclosure. As shown in Figure 9, the light shielding layer 130 includes a first straight portion 131 and a second straight portion 132 stacked sequentially along a direction approaching the light-emitting surface 101 of the display panel 100. The orthographic projection area of ​​the first straight portion 131 on the display panel 100 is larger than the orthographic projection area of ​​the second straight portion 132 on the display panel 100.

[0082] In the disclosed embodiment, as shown in FIG9 , the area of ​​the first straight portion 131 is greater than the area of ​​the second straight portion 132, resulting in the light-shielding layer 130 exhibiting an inverted stepped structure. Therefore, the transparent adhesive layer 110 can fill the inverted step, increasing the thickness of the transparent adhesive layer 110 at the step. This enhances the adhesion between the cover plate 120 and the display panel 100 in the area covered by the light-shielding layer 130. Furthermore, as shown in FIG9 , the light-shielding layer 130 exhibits an inverted stepped shape, and thus the first light-reflecting layer 140 also exhibits an inverted stepped shape. Compared to a straight first light-reflecting layer 140, the inverted stepped shape of the first light-reflecting layer 140 increases the reflection area of ​​the curing light, thereby more completely reflecting the curing light onto the transparent adhesive layer 110. This results in a better curing effect of the transparent adhesive layer 110, thereby improving the folding reliability of the display module and enhancing product performance and competitiveness.

[0083] Optionally, referring to FIG. 9 , the orthographic projection of the second straight portion 132 on the display panel 100 is located in the central area of ​​the orthographic projection of the first straight portion 131 on the display panel 100 , that is, the second straight portion 132 is in the middle of the first straight portion 131 .

[0084] In the embodiment of the present disclosure, when the second straight portion 132 is located in the middle of the first straight portion 131, the two sides of the light-shielding layer 130 are symmetrical and in an inverted stepped shape, so that the curing light can be irradiated from both sides in a stepped manner to the first light-reflecting layer 140 and reflected, thereby allowing more light to be reflected to the transparent adhesive layer 110, thereby achieving a better curing effect of the transparent adhesive layer 110.

[0085] Optionally, the cross-sectional shape of the light shielding layer 130 along the direction perpendicular to the light emitting surface 101 of the display panel 100 is one of the following: flat, wavy, or grooved, that is, the cross-sectional shape is flat, wavy, or grooved. The notch of the grooved structure faces the display panel 100.

[0086] For example, referring to Figures 1, 4, 6, or 7, the cross-section of the light shielding layer 130 is planar. The light shielding layer 130 is bonded to the cover plate 120. Compared to light shielding layers 130 formed in other shapes, a light shielding layer 130 with a planar cross-section can completely shield metal traces while saving manufacturing processes. For another example, Figures 10 and 11 are schematic structural diagrams of a display module provided in another embodiment of the present disclosure. As shown in Figures 10 and 11, the cross-section of the light shielding layer 130 is wavy. Because the cross-section of the light shielding layer 130 is wavy, the transparent adhesive layer 110 and the first light reflective layer 140 are also wavy. This wavy structure does not affect the reflective properties of the first light reflective layer 140. Furthermore, the wavy shapes of the first and second light reflective layers 140, 150 also change the reflection angle of the curing light. Due to the curved angle, the curing light can be reflected over a wider area of ​​the transparent adhesive layer 110, thereby improving the curing effect of the transparent adhesive layer 110. When the cross section of the light-shielding layer 130 is a groove-shaped structure, the cross section of the first light-reflecting layer 140 can also be a convex structure that cooperates with the groove-shaped structure. The height difference formed by the convex structure makes the reflective surface of the first light-reflecting layer 140 larger, thereby making the reflective effect of the curing light better.

[0087] Optionally, the material of the transparent adhesive layer 110 is optically clear adhesive (OCA) or optical clear resin (OCR).

[0088] Among them, optical glue is a double-sided laminating tape without a matrix material, which has the advantages of high light transmittance and high adhesion, and its thickness is uniform and flat, and it will not cause yellowing, aging, fogging, detachment from the adhered surface, and bubbles after long-term use. Using optical glue as the transparent adhesive layer 110 to bond the cover plate 120 and the display panel 100 can maintain good adhesion and stability during the use of the display module. Compared with optical glue, optical resin has free shape and does not require cutting. It can correspond to various shapes such as holes, special shapes, 3D, etc. through program adjustment. The thickness of optical resin can be selected in a wide range, and the filling performance is excellent, which can meet the needs of different thicknesses in different positions on the same product. Optical resin also has advantages such as excellent folding performance. Using optical resin as the transparent adhesive layer 110 can achieve a smaller folding radius, longer folding life, and a more stringent folding reliability environment for the display module.

[0089] Alternatively, Figures 12 and 13 are schematic structural diagrams of a display module provided in another embodiment of the present disclosure. As shown in Figures 12 or 13, the display panel 100 includes a base substrate, a plurality of light-emitting devices (not shown) sequentially arranged on one side of the base substrate, a pixel defining layer (not shown), and an encapsulation layer 160. The pixel defining layer is used to separate the plurality of light-emitting devices.

[0090] Among them, the light-emitting device is a top-emitting light-emitting device or a bottom-emitting light-emitting device. Light-emitting devices can be divided into top-emitting light-emitting devices and bottom-emitting light-emitting devices according to the different directions of light emission from the device. Top-emitting light-emitting devices have an optical microcavity structure, so the front brightness is multiplied compared to bottom-emitting light-emitting devices, and are widely used in mobile phones and other products. The ultra-thin metal electrodes of top-emitting devices are inherently unstable and easily corroded by water vapor, so they have high requirements for packaging. For bottom-emitting light-emitting devices, because they have a thicker cathode, they have better stability. In addition, since the light-emitting side is generally a non-metallic anode farther away from the light-emitting layer, the optical loss is smaller.

[0091] Optionally, the light-emitting device is a bottom-emitting light-emitting device. As shown in FIG12 or FIG13 , the encapsulation layer 160 includes a first inorganic layer 162, an organic layer 161, and a second inorganic layer 163 stacked in a direction away from the base substrate. The display module also includes a waterproof layer 170 and a first adhesive layer 173. The waterproof layer 170 is located on the side of the second inorganic layer 163 away from the base substrate. The first adhesive layer 173 is located between the second inorganic layer 163 and the waterproof layer 170. In other words, the waterproof layer 170 is provided on the side of the second inorganic layer 163 away from the base substrate. The waterproof layer 170 is bonded to the second inorganic layer 163 via the first adhesive layer 173.

[0092] In the disclosed embodiment, the light-emitting side of the display module is bottom-emitting, resulting in minimal optical loss. As shown in Figures 12 and 13, a waterproof layer 170 is provided on one side of the encapsulation layer 160, imparting a degree of waterproofing to the display module, improving the encapsulation effect and extending the life of the display module. The organic layer 161 is positioned between the first inorganic layer 162 and the second inorganic layer 163 to achieve planarization and reduce stress between the inorganic encapsulation layers 160.

[0093] Optionally, the first inorganic layer 162 and the second inorganic layer 163 may be made of different materials. For example, the oxygen content of the first inorganic layer 162 may be higher than that of the second inorganic layer 163. Thus, the first inorganic layer 162 having a higher oxygen content can facilitate the preparation of the organic encapsulation layer 160, particularly facilitating the leveling of the organic liquid material used to prepare the organic encapsulation layer 160. The second inorganic layer 163 may have a lower oxygen content or even contain no oxygen, thereby providing a better water and oxygen barrier effect, thereby improving the encapsulation effect of the display panel 100.

[0094] Optionally, in a multilayer stack structure comprising a first inorganic layer 162, an organic layer 161, and a second inorganic layer 163, the first and second inorganic layers 162, 163 can be deposited using plasma enhanced chemical vapor deposition (PECVD) or atomic layer deposition (ALD), thereby achieving efficient water and oxygen barrier properties. The organic layer 161 can be prepared using methods including, but not limited to, polymer monomer deposition, PECVD to form a hybrid organic layer, or inkjet printing (IJP).

[0095] Continuing with Figures 12 and 13 , the cover plate 120 and the display panel 100 are indirectly bonded via a transparent adhesive layer 110. Optionally, a backing film 300 is further included between the transparent adhesive layer 110 and the cover plate 120. The cover plate 120 and the transparent adhesive layer 110 are indirectly bonded via the backing film 300. The cover plate 120 may be a protective film. The backing film 300 may be made of a transparent insulating material, such as polyester resin, and serves to protect and support the display panel 100.

[0096] Optionally, waterproof layer 170 is aluminum foil or copper foil. In the disclosed embodiment, waterproof layer 170 uses aluminum foil or copper foil to waterproof display panel 100 and encapsulation layer 160. Aluminum foil and copper foil provide better waterproofing than waterproof layers made of other materials. Furthermore, aluminum foil and copper foil can provide electromagnetic shielding within the display module, resulting in better display performance during use.

[0097] Optionally, referring to Figure 12 , the edge of the organic layer 161 is recessed by 1 to 2 mm relative to the edges of the first and second inorganic layers 162 and 163 in a direction parallel to the plane of the base substrate. The display module also includes a first adhesive layer 171. The first adhesive layer 171 is disposed on the same layer as the organic layer 161. The first adhesive layer 171 is used to bond the first and second inorganic layers 162 and 163. In other words, the first adhesive layer 171 is disposed at the recessed portion of the organic layer 161 to bond the first and second inorganic layers 162 and 163.

[0098] In the embodiment of the present disclosure, in order to prevent the liquid organic layer 161 from overflowing outside the first inorganic layer 162 and the second inorganic layer 163 and then overflowing onto the display panel 100, when manufacturing the organic layer 161, the organic layer 161 is retracted a certain distance relative to the edge of the first inorganic layer 162 to prevent the liquid organic layer 161 from flowing out into the display panel 100. A first adhesive layer 171 is provided at the retracted portion of the organic layer 161. The first adhesive layer 171 can serve to bond the edges of the first inorganic layer 162 and the second inorganic layer 163, thereby reducing the probability of gaps forming at the corners of the display module. In addition, the first adhesive layer 171 can also fill the gap left by the retracted portion of the organic layer 161. Therefore, the first adhesive layer 171 seals and prevents water vapor intrusion at the retracted portion of the organic layer 161, thereby greatly reducing the defective rate of the display module, preventing the thin film encapsulation (TFE) from being exposed to a water vapor environment, and greatly reducing the erosion rate. This can meet the vehicle reliability specifications and achieve the goal of smoothly applying flexible OLED screens to special-shaped, curved, and foldable projects such as vehicle windows, central control, and headlights.

[0099] Optionally, the material of the first adhesive layer 171 can be an optical resin or a fluorinated adhesive. The first adhesive layer 171 can be prepared by inkjet printing or coating. For example, referring to FIG12 , after the display module is manufactured, the first adhesive layer 171 can be coated on the indentation of the organic layer 161, so that the first adhesive layer 171 adheres the indentation between the first inorganic layer 162 and the second inorganic layer 163 to prevent water vapor from invading from the indentation and causing the encapsulation layer 160 to be corroded. Alternatively, as shown in FIG14 , after the organic layer 161 is prepared, the first adhesive layer 171 is first prepared on the indentation of the organic layer 161. As shown in FIG15 , after the organic layer 161 and the first adhesive layer 171 are prepared, the second inorganic layer 163, the first adhesive layer 173 and the waterproof layer 170 are sequentially prepared on the side of the organic layer 161 and the first adhesive layer away from the display panel 100.

[0100] Optionally, referring to Figure 13 , the outer edges of the waterproof layer 170 and the second inorganic layer 163 are flush with each other in a direction parallel to the plane of the base substrate and are recessed by 0.5 to 1 mm relative to the edge of the first inorganic layer 162. The edge of the organic layer 161 is recessed by 1 to 2 mm relative to the edge of the first inorganic layer 162. The display module also includes a second adhesive layer 172. This second adhesive layer 172 covers the surface of the waterproof layer 170 facing away from the base substrate, as well as the side surfaces of the waterproof layer 170, the first adhesive layer 173, the second inorganic layer 163, the organic layer 161, and the first inorganic layer 162.

[0101] In the disclosed embodiment, waterproof layer 170 is flush with the outer edge of second inorganic layer 163, allowing waterproof layer 170 to completely cover second inorganic layer 163. This allows waterproof layer 170 to provide a better waterproofing effect on encapsulation layer 160. As shown in Figure 13, second adhesive layer 172 covers the outer surface of waterproof layer 170, forming a waterproof barrier outside waterproof layer 170, preventing water vapor from adhering to waterproof layer 170. For waterproof layers made of metal, second adhesive layer 172 can also isolate the waterproof layer from air, thereby preventing waterproof layer 170 from rusting. The second glue layer 172 also covers the side surfaces of the waterproof layer 170, the first adhesive layer 173, the first inorganic layer 162, the organic layer 161 and the second inorganic layer 163, so that the side surfaces of the waterproof layer 170, the first adhesive layer 173, the first inorganic layer 162, the organic layer 161 and the second inorganic layer 163 are isolated from the external air, reducing the probability of external water vapor entering from the sides of the waterproof layer 170, the first adhesive layer 173, the first inorganic layer 162, the organic layer 161 and the second inorganic layer 163, thereby achieving further waterproofing of the display module and thereby improving the working performance of the display module.

[0102] Optionally, when the light emitting device is a bottom-emitting light emitting device, since the light emitted by the light emitting device does not pass through the first adhesive layer 173 , the first adhesive layer 173 may be a transparent adhesive layer, or may be an opaque adhesive layer.

[0103] Optionally, Figure 16 is a cross-sectional view of the edge of the display module shown in Figure 7 provided by an embodiment of the present disclosure. As shown in Figure 16, the display panel 100 further includes a second adhesive layer 174, a foam layer 175, a heat dissipation layer 176, and a polarizer 200. The second adhesive layer 174 is disposed on the side of the back film 300 away from the transparent adhesive layer 110. The second adhesive layer 174 may be a pressure-sensitive adhesive. A foam layer 175 and a heat dissipation layer 176 are sequentially disposed on the second adhesive layer 174 along the side of the second adhesive layer 174 away from the transparent adhesive layer 110. When the display panel 100 is bent, the foam layer 175 acts as a buffer. The foam layer 175 is bonded to the back film 300 via the second adhesive layer 174. Heat generated during operation of the display panel 100 can be dissipated through the heat dissipation layer 176, thereby preventing heat accumulation within the display panel 100.

[0104] It should be noted that in COE (Color filter on encapsulation) products, the polarizer 200 can be replaced by PET, which can increase the strength of the display product.

[0105] FIG17 is a flow chart of a method for manufacturing a display module according to an embodiment of the present disclosure. As shown in FIG17 , the manufacturing method includes but is not limited to the following steps 1701 to 1705 .

[0106] In step 1701 , a display panel is prepared, wherein the display panel has a display area and a peripheral area surrounding the display area.

[0107] In step 1702 , a transparent adhesive layer is prepared on one side of the light emitting surface of the display panel.

[0108] In step 1703 , a light shielding layer is prepared on a side of the transparent adhesive layer away from the display panel. The orthographic projection of the light shielding layer on the display panel is located in a peripheral area of ​​the display panel.

[0109] In step 1704, a first light reflecting layer is prepared on a side of the light shading layer away from the display panel. The orthographic projection of the first light reflecting layer on the display panel is located in a peripheral area of ​​the display panel, and there is an overlapping area between the orthographic projection of the first light reflecting layer on the display panel and the orthographic projection of the light shading layer on the display panel.

[0110] Optionally, an implementation of step 1704 includes: preparing a first light reflecting layer on a side of the light shielding layer away from the display panel by using a discontinuous coating process, a coating process, a bonding process, or a hot-melt process.

[0111] Among them, the discontinuous coating process, also known as non-conductive electroplating technology, refers to the organic transformation of metal materials under vacuum conditions using specific chemical, physical and other means to convert the metal into particles, which are deposited or adsorbed on the surface of the plastic material to form a film. The coating produced using the discontinuous coating process has a metallic texture and does not affect wireless communications.

[0112] In the embodiment of the present disclosure, the first light reflecting layer can also be formed by applying a light reflecting solution, or the first light reflecting layer can be prepared first and then bonded to the transparent adhesive layer.

[0113] In step 1705, a cover plate is prepared on a side of the first light reflecting layer away from the display panel.

[0114] The structure of the display module obtained by the manufacturing method shown in FIG17 provided by the embodiment of the present disclosure can be as shown in FIG1, FIG6, or FIG10. When the curing light is irradiated on the transparent adhesive layer 110 along the side of the display module, even if the curing light is not parallel to the transparent adhesive layer 110, the curing light can be reflected multiple times on the first reflective layer 140, so that the curing light is not absorbed by the light shielding layer 130 and is reflected onto the transparent adhesive layer 110. This achieves efficient utilization of the curing light, ensures that the transparent adhesive layer 110 is fully irradiated by the curing light, and further ensures that the edges of the transparent adhesive layer 110 are fully cured, thereby improving the folding reliability of the display module and further enhancing the performance and competitiveness of the product.

[0115] Optionally, before forming the transparent adhesive layer on the light-emitting surface of the display panel, a second light-reflecting layer may be formed on the light-emitting surface of the display panel. The orthographic projection of the second light-reflecting layer on the display panel is located in the peripheral area of ​​the display panel, and the orthographic projection of the second light-reflecting layer on the display panel overlaps with the orthographic projection of the light-shielding layer on the display panel. The structure of the display module obtained by this manufacturing method may be shown in Figures 4, 7, or 11.

[0116] Optionally, one implementation of preparing the second light reflecting layer on one side of the light emitting surface of the display panel includes: preparing the second light reflecting layer on one side of the light emitting surface of the display panel by using a discontinuous coating process, a coating process, a bonding process or a hot melt process.

[0117] Optionally, the first light reflecting layer and the second light reflecting layer may be reflective layers made of a single material, or may be a composite laminated structure, which is not limited in the embodiment of the present disclosure.

[0118] An embodiment of the present disclosure further provides a display device, comprising any one of the above-mentioned display modules.

[0119] In an embodiment of the present disclosure, as shown in any one of Figures 1, 4, 6 to 7, and 9 to 11, a display device including the above-mentioned display module can be provided with a first light reflecting layer 140 between the light shielding layer 130 and the display panel 100. When curing light irradiates the transparent adhesive layer 110 along the side of the display device, even if the curing light is not parallel to the transparent adhesive layer 110, the curing light can be reflected multiple times on the first light reflecting layer 140, so that the curing light is not absorbed by the light shielding layer 130 and is reflected onto the transparent adhesive layer 110, thereby achieving efficient utilization of the curing light, allowing the transparent adhesive layer 110 to be fully irradiated by the curing light, and further allowing the edges of the transparent adhesive layer 110 to be fully cured, thereby improving the folding reliability of the display module and further improving the performance and competitiveness of the product.

[0120] Optionally, the display device includes but is not limited to: a computer monitor, a television, a billboard, a laser printer with display function, a telephone, a mobile phone, a personal digital assistant (PDA), a laptop computer, a digital camera, a camcorder, a viewfinder, a vehicle, a large wall, a theater screen or a stadium sign, etc.

[0121] It should be noted that, in this document, relational terms such as first and second, etc., are used only to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply the existence of any such actual relationship or order between these entities or operations. Moreover, the terms "comprises," "comprising," or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article, or device comprising a series of elements includes not only those elements, but also other elements not explicitly listed, or elements inherent to such process, method, article, or device. In the absence of further limitations, an element defined by the phrase "comprising a ..." does not exclude the presence of other identical elements in the process, method, article, or device comprising the element.

[0122] Each embodiment in this specification is described in a related manner. Similar parts between the various embodiments can be referred to in conjunction with each other. Each embodiment focuses on the differences between the other embodiments. In particular, the system embodiment is generally similar to the method embodiment, so the description is relatively simple. For related parts, refer to the description of the method embodiment.

[0123] The above description is only an optional embodiment of the present disclosure and is not intended to limit the scope of protection of the present disclosure. Any modifications, equivalent replacements, improvements, etc. made within the spirit and principles of the present disclosure are included in the scope of protection of the present disclosure.

Claims

1. A display module, comprising: A display panel (100), the display panel (100) comprising a display area (10) and a peripheral area (20) surrounding the display area (10); a transparent adhesive layer (110), the transparent adhesive layer (110) being located on one side of the light emitting surface (101) of the display panel (100); a cover plate (120), the cover plate (120) being located on a side of the transparent adhesive layer (110) away from the display panel (100); a light shielding layer (130), the light shielding layer (130) being located between the cover plate (120) and the display panel (100), and the orthographic projection of the light shielding layer (130) on the display panel (100) being located in a peripheral area (20) of the display panel (100); At least one light reflecting layer, the at least one light reflecting layer comprising a first light reflecting layer (140) located between the transparent adhesive layer (110) and the light shielding layer (130), the orthographic projection of the first light reflecting layer (140) on the display panel (100) being located in a peripheral area (20) of the display panel (100), and the orthographic projection of the first light reflecting layer (140) on the display panel (100) and the orthographic projection of the light shielding layer (130) on the display panel (100) having an overlapping area.

2. According to the display module of claim 1, the orthographic projection of the first light reflecting layer (140) on the display panel (100) completely overlaps with the orthographic projection of the light shielding layer (130) on the display panel (100).

3. The display module according to claim 1 or 2, wherein the at least one reflective layer further comprises a second reflective layer (150) located between the transparent adhesive layer (110) and the display panel (100), an orthographic projection of the second reflective layer (150) on the display panel (100) being located in a peripheral area (20) of the display panel (100), and an orthographic projection of the second reflective layer (150) on the display panel (100) and an orthographic projection of the shading layer (130) on the display panel (100) having an overlapping area.

4. The display module according to claim 3, wherein an orthographic projection of the second light reflecting layer (150) on the display panel (100) completely overlaps with an orthographic projection of the light shielding layer (130) on the display panel (100). 5 . The display module according to claim 1 , wherein the reflective layer comprises a multi-layer composite structure, and each layer of the composite structure comprises stacked niobium oxide and silicon dioxide. 6 . The display module according to claim 5 , wherein the reflective layer comprises five layers of the composite structure, and the thickness of each layer of the composite structure ranges from 100 nanometers to 800 nanometers.

7. According to the display module according to any one of claims 1 to 6, the light shielding layer (130) comprises a first straight portion (131) and a second straight portion (132) which are sequentially stacked in a direction close to the light emitting surface of the display panel (100), and an orthographic projection area of ​​the first straight portion (131) on the display panel (100) is larger than an orthographic projection area of ​​the second straight portion (132) on the display panel (100).

8. The display module according to claim 7, wherein the orthographic projection of the second straight portion (132) on the display panel (100) is located in a central area of ​​the orthographic projection of the first straight portion (131) on the display panel (100).

9. According to the display module according to any one of claims 1 to 8, the cross-sectional shape of the light shielding layer (130) along a direction perpendicular to the light emitting surface (101) of the display panel (100) is one of the following: a plane type, a wave type, or a groove type structure; wherein: The notch of the groove-shaped structure faces the display panel (100).

10. The display module according to any one of claims 1 to 9, wherein the material of the transparent adhesive layer (110) is optical glue or optical resin.

11. According to the display module according to any one of claims 1 to 10, the display panel (100) comprises a base substrate and a plurality of light-emitting devices, a pixel defining layer and an encapsulation layer (160) arranged in sequence on one side of the base substrate, and the pixel defining layer is used to separate the plurality of light-emitting devices.

12. The display module according to claim 11, wherein the light emitting device is a bottom emitting light emitting device, and the encapsulation layer (160) comprises a first inorganic layer (162), an organic layer (161) and a second inorganic layer (163) stacked in a direction away from the base substrate; The display module further comprises a waterproof layer (170) and an adhesive layer (173); the waterproof layer (170) is located on a side of the second inorganic layer (163) away from the base substrate; and the adhesive layer (173) is located between the second inorganic layer (163) and the waterproof layer (170).

13. The display module according to claim 12, wherein the waterproof layer (170) is aluminum foil or copper foil.

14. The display module according to claim 12 or 13, wherein along a direction parallel to the plane where the base substrate is located, an edge of the organic layer (161) is retracted by 1 mm to 2 mm relative to edges of the first inorganic layer (162) and the second inorganic layer (163); The display module further comprises a first adhesive layer (171), the first adhesive layer (171) being arranged on the same layer as the organic layer (161), and the first adhesive layer (171) being used for bonding the first inorganic layer (162) and the second inorganic layer (163).

15. The display module according to claim 12 or 13, wherein in a direction parallel to the plane where the base substrate is located, the outer edges of the waterproof layer (170) and the second inorganic layer (163) are flush and are retracted 0.5 mm to 1 mm relative to the edge of the first inorganic layer (162); the edge of the organic layer (161) is retracted 1 mm to 2 mm relative to the edge of the first inorganic layer (162); The display module further comprises a second glue layer (172), wherein the second glue layer (172) covers the surface of the waterproof layer (170) away from the base substrate, as well as the side surfaces of the waterproof layer (170), the adhesive layer (173), the second inorganic layer (163), the organic layer (161) and the first inorganic layer (162).

16. A method for manufacturing a display module, for manufacturing the display module according to any one of claims 1 to 15, the manufacturing method comprising: preparing a display panel, the display panel having a display area and a peripheral area surrounding the display area; Preparing a transparent adhesive layer on one side of the light emitting surface of the display panel; A light shielding layer is prepared on a side of the transparent adhesive layer away from the display panel, wherein the orthographic projection of the light shielding layer on the display panel is located in a peripheral area of ​​the display panel; A first light reflecting layer is prepared on a side of the light shielding layer away from the display panel, wherein an orthographic projection of the first light reflecting layer on the display panel is located in a peripheral area of ​​the display panel, and an orthographic projection of the first light reflecting layer on the display panel overlaps with an orthographic projection of the light shielding layer on the display panel; A cover plate is prepared on a side of the first light reflecting layer away from the display panel.

17. The manufacturing method according to claim 16, wherein a first light reflecting layer is formed on a side of the light shielding layer away from the display panel, comprising: The first light reflecting layer is prepared on the side of the light shielding layer away from the display panel by adopting a discontinuous coating process, a coating process, a bonding process or a hot-melt process.

18. The manufacturing method according to claim 16 or 17, before preparing a transparent adhesive layer on one side of the light emitting surface of the display panel, the manufacturing method further comprises: A second light reflecting layer is prepared on one side of the light emitting surface of the display panel, the orthographic projection of the second light reflecting layer on the display panel is located in the peripheral area of ​​the display panel, and there is an overlapping area between the orthographic projection of the second light reflecting layer on the display panel and the orthographic projection of the light shielding layer on the display panel.

19. The manufacturing method according to claim 18, wherein a second light reflecting layer is prepared on one side of the light emitting surface of the display panel, comprising: The second light reflecting layer is prepared on one side of the light emitting surface of the display panel by adopting a discontinuous coating process, a coating process, a bonding process or a hot-melt process.

20. A display device, comprising the display module according to any one of claims 1 to 15.

Citation Information

Patent Citations

  • Display panel and preparation method thereof

    CN109860418A

  • Display device

    CN110488528A

  • Cover plate, display module, manufacturing method of display module and display device

    CN115421327A

  • Display module, manufacturing method of display module and display device

    CN116568100A

  • Display devices and methods of manufacturing display devices

    US20150219950A1