Semiconductor package with integrated fuse structure

The integration of a thermal fuse structure into semiconductor packages addresses the issue of uncontrolled temperature increases from short circuits by activating at a predefined temperature to create an open circuit, preventing further damage and potential fires.

WO2024245544A1PCT designated stage expired Publication Date: 2024-12-05HUAWEI DIGITAL POWER TECH CO LTD +1
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
PCT/EP2023/064491
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-31
Publication Date
2024-12-05

AI Technical Summary

Technical Problem

Short circuits in semiconductor power components can lead to uncontrolled temperature increases, causing damage to the component and potentially resulting in severe and extensive damage to the product, including the risk of fire, due to self-reinforcing thermal reactions.

Method used

Integration of a thermal fuse structure into the die metallization, which activates at a predefined temperature to create an open circuit by utilizing materials that melt, form brittle intermetallics, or lose adhesion, thereby interrupting current flow and preventing further temperature increase.

Benefits of technology

The thermal fuse structure effectively limits damage to the semiconductor package, preventing thermal runaway and potential fires by ensuring an open circuit is created when a short circuit occurs, thus protecting the component and surrounding PCB from extensive damage.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure EP2023064491_05122024_PF_FP_ABST
    Figure EP2023064491_05122024_PF_FP_ABST
Patent Text Reader

Abstract

The disclosure relates to a semiconductor package (100) with integrated fuse structure (112). The semiconductor package (100) comprises: a semiconductor die (101) comprising a die pad (102) arranged on a main surface (101a) of the semiconductor die (101) for electrically connecting the semiconductor die (101); a metal stack (110) positioned on top of the die pad (102); an encapsulant (103) encapsulating the semiconductor die (101) and the metal stack (110); and a metal connector (104) extending through the encapsulant (103) to the metal stack (110) for enabling a current flow (120) via the metal stack (110) to the semiconductor die (101); wherein the metal stack (110) comprises a fuse structure (112) that can be thermally activated, wherein the thermal activation of the fuse structure (112) reduces the current flow (120) to the semiconductor die (101).
Need to check novelty before this filing date? Find Prior Art

Description

[0001] SEMICONDUCTOR PACKAGE WITH INTEGRATED FUSE STRUCTURE

[0002] TECHNICAL FIELD

[0003] The disclosure relates to the field of semiconductor packages and embedded chip or component packages (ECP) for power applications. A semiconductor package with integrated fuse structure is provided. The disclosure also relates to an integrated chip level thermal fuse structure for ECP power packages.

[0004] BACKGROUND

[0005] Short circuit in a power component can damage not only the component itself but also the product or even the whole system. For example, in an ECP package a weakness together with moisture and impurities can cause a short circuit on the die surface. This short circuit can cause fast and uncontrollable temperature increase on the die surface that destroys the component and can cause huge damages also in the printed circuit board (PCB). The damage on component level can propagate to severe and extensive damages in the product. Further damage escalation by nature of self-reinforcing continuous thermal reactions (thermal runaway) may present a severe risk of fire that requires mitigation - either on component level (avoidance) or on systems / housing level (containment).

[0006] SUMMARY

[0007] This disclosure provides a solution for avoiding problems encountered with damage in semiconductor products related to uncontrolled temperature increase.

[0008] An anti-burning package is provided that can be incorporated in a semiconductor package by using an additional thermal fuse.

[0009] The foregoing and other objects are achieved by the features of the independent claims. Further implementation forms are apparent from the dependent claims, the description and the figures.

[0010] Embodiments of the disclosure are based on integrating a thermal fuse structure into the die metallization and using the known or pre-designed thermal expansion of the surrounding packaging materials to break and open the electrical connection between the PCB routing and the component as shown in the following. The new metal structure has an integrated weakness that will be activated only when the temperature increases above a predefined temperature. The thermally activated weakness together with thermal expansion of the used PCB materials will create an open circuit between the embedded component and package. This metal structure can replace, for example, the TiW / Cu bump or pad finish that is used in ECP. The fuse structure can be integrated either at the top side of the die and / or at the bottom side of the die.

[0011] The thermally activated designed weakness within the die pad metallization or finish will be activated when the temperature on the die surface reaches the predefined temperature. At the predefined temperature one layer or several layers in the die pad metallization stack will weaken to allow thermal expansion / stress (caused by the coefficient of thermal expansion (CTE) and / or CTE mismatch) to pull and separate the layers from each other. This will cause an open circuit that prevents current flow through the component and prevents the thermal runaway and more severe / extensive damages. The activation temperature is above the processing and soldering temperatures that are used during manufacturing. Different mechanisms can be used to activate the fuse and cut the current flow to the device as listed below.

[0012] A) Melting layer - or structure that undergoes solid-to-liquid phase transition

[0013] The layer between diffusion barrier / adhesion layers will melt when the selected temperature is reached. This can be done by using metals, metal alloys or a multilayer stack that will melt at the predefined temperature. The metal alloy or stack can be e.g. eutectic Au(80) / Sn(20).

[0014] B) Brittle intermetallic layer

[0015] The layer between diffusion barrier / adhesion layers will form brittle intermetallics when the selected temperature is reached. This can be done by using metal alloys or a multilayer stack that form brittle intermetallics or voids at selected temperatures. Metal alloy or stack examples are presented in the following.

[0016] C) De-wetting, detaching or reduced adhesion layer

[0017] The layer between diffusion barrier / adhesion layers is designed to lose adhesion when the selected temperature is reached. Examples of materials to induce de-wetting or detaching or de-adhesion are presented in the following. The solution presented in this disclosure is not product specific, it can be used for example in all ECP products, but also other package types, such as Flip-Chip, etc. where a metal stack structure is used / required on top of the normal Al pad metallization of the die.

[0018] The thermally activated weakness inside the die pad metallization stack can be created in several ways. The weakness can be activated at a preselected temperature, for example. Some exemplary options, possible metal alloys or metal stack or material system examples are presented in more detail in the following paragraphs / embodiments.

[0019] In order to describe the disclosure in detail, the following terms and notations will be used.

[0020] ECP Embedded Chip / Component Package

[0021] CE Chip Embedding

[0022] LV / MV / HV Low Voltage I Medium Voltage I High Voltage

[0023] TiW Titanium-Tungsten

[0024] PSiP Power Supply in Package

[0025] UBM: Under Bump Metallization - thin film metal layer(s) between the last metal layer of an Integrated Circuit (IC) pad and plated copper or solder bumps. The main purpose of the UBM is to form an electrical connection between the die metallization and the bump and act as a diffusion barrier layer to eliminate the unwanted diffusion between the metal layer under and above the UBM and / or act as an adhesion layer between the pad and the bump

[0026] SAC305 Lead-free solder alloy that contains 96.5% tin (S), 3% silver (A), and 0.5% copper (C)

[0027] ECP or Chip Embedding technology is a new packaging technology currently used in advanced power packaging. In ECP technology, the components are embedded inside a multilayer PCB laminate and the connections between the die and the package are made with plated micro-vias. Currently, the technology is used mainly in LV and LV applications, although the interest in MV and HV applications in future is on the rise.

[0028] According to a first aspect, the disclosure relates to a semiconductor package with integrated fuse structure, the semiconductor package comprising: a semiconductor die comprising a die pad arranged on a main surface of the semiconductor die for electrically connecting the semiconductor die; a metal stack positioned on top of the die pad; an encapsulant encapsulating the semiconductor die and the metal stack; and a metal connector extending through the encapsulant to the metal stack for enabling a current flow via the metal stack to the semiconductor die; wherein the metal stack comprises a fuse structure that can be thermally activated, wherein the thermal activation of the fuse structure reduces the current flow to the semiconductor die.

[0029] The term “on top of” specifies a relative direction that depends on the viewer’s position. It is understood that this can be on the bottom as well.

[0030] The fuse structure may reduce, limit or cut off the current flow to the semiconductor die.

[0031] Such a semiconductor package with integrated fuse structure can be applied to avoid problems encountered with damage in semiconductor products related to uncontrolled temperature increase. The metal stack with fuse structure provides an anti-burning package that can be incorporated in the semiconductor package in order to reduce short cut effects as described above with fast and uncontrollable temperature increase on the die surface.

[0032] A metal connector can be a metal via or a wire bond or a solder bump or a clip or a spacer or a stud, for example, or any other kind of electrical connection.

[0033] The fuse structure can be thermally activated at a fuse activation temperature. The fuse structure can comprise a metal or a combination of different metals or a combination of metals and non-metals, for example.

[0034] In an exemplary implementation of the semiconductor package, the fuse structure comprises a material or a combination of materials comprising at least one of metals, alloys and additives including non-metallic or metallic compounds. There may be also other materials that can be efficiently used as fuse structure for reducing or interrupting the current flow in short circuit scenarios.

[0035] In an exemplary implementation of the semiconductor package, the thermal activation of the fuse structure together with a thermal expansion of the encapsulant at the fuse activation temperature creates an open circuit between the semiconductor die and the metal connector in the semiconductor package. The open circuit interrupts the current flow, and no further temperature increase can happen. Thus, damage is limited to the package only, and the board will not be destroyed. In an exemplary implementation of the semiconductor package, the metal stack comprises two barrier layers, wherein the fuse structure is positioned between the two barrier layers. These barrier layers avoid diffusion of the fuse structure or fuse layer material between the fuse structure and the semiconductor die metallization layers or bump metallization which may be harmful for these components. This works in both directions, towards the semiconductor die and the bump layer (e.g., Cu).

[0036] The barrier layers can be sputtered barrier / metal layers, for example. These barrier layers can be acting as diffusion barrier layers or not acting as diffusion barrier layers. The barrier layers can be made of Ti, TiW, Co, Ru, Ta, TaN, InO, WN, TiN, etc...., for example, or combinations thereof. The barrier layers can also be deposited by other means than sputtering, e.g., by other suitable processes. Thus, the barrier layers and metal layers can be flexibly applied for protecting against diffusion or just as additional layers.

[0037] In an exemplary implementation of the semiconductor package, the barrier layers are diffusion barrier layers that are configured to adhere to the fuse structure and to prevent the fuse structure from diffusing to the die pad and / or the metal connector. The barrier layers can be applied for preventing the fuse structure from diffusing to the die pad and / or the metal connector.

[0038] In an exemplary implementation of the semiconductor package, the thermal activation of the fuse structure reduces adhesion of the barrier layers to the fuse structure. Reduction of adhesion results in an interruption or reduction of the current flow and thus reduces the uncontrolled temperature increase due to a short cut. The thermal expansion of the surrounding encapsulation material is acting on the metallization stack and thus the short circuit can be transformed to an open circuit. Transformation of the short circuit to an open circuit may be assisted by thermal expansion of the surrounding encapsulant acting on the stack.

[0039] In an exemplary implementation of the semiconductor package, the thermal activation of the fuse structure at least partially melts the fuse structure or at least undergoes partial or complete solid-to-liquid phase transition. Due to melting of the fuse structure, the current flow is interrupted or at least reduced and temperature increase can be reduced.

[0040] In an exemplary implementation of the semiconductor package, the fuse structure comprises a low melting metal or metal alloy melting at a temperature range between 118 and 365 degrees Celsius or at a temperature range between 118 and 1065 degrees Celsius. The melting material can be used as fuse material that protects the components against short circuit and short cut.

[0041] For example, Sn-ln alloys melt at about 118 degrees Celsius; Au-Ge, Au-Si alloys melt at about 365 degrees Celsius. Other high temperature solders may even melt at temperatures from about 450 degrees Celsius to about 1065 degrees Celsius, such as pure Au, Ag-Cu-ln, Ag-ln, Au-ln, etc.

[0042] In an exemplary implementation of the semiconductor package, the fuse structure comprises solder metals or alloys which undergo phase transition in an activation temperature range based on one or a combination of the following metals: Bi, Au, Sn, Pb, Ag, Cd, Zn, Ge, Cu, In.

[0043] A variety of different materials can be applied as fuse material. Such metals or alloys may be for example Bi, Au-Sn, Pb-Sn, Pb-Sn-Ag, Au-Ge, Cd-Zn, etc. In one example, the fuse structure may comprise eutectic 80Au / 20Sn solder alloy.

[0044] In an exemplary implementation of the semiconductor package, the thermal activation of the fuse structure makes the fuse structure to form brittle intermetallic and / or voids in areas of the metal stack reducing an adhesion of the fuse structure with the metal stack. The brittle intermetallics or voids can be used to create a short circuit that prevents the current flow.

[0045] In an exemplary implementation of the semiconductor package, the fuse structure comprises one or more intermetallic compounds. Such intermetallic compounds can be efficiently applied as the fuse structure.

[0046] In an exemplary implementation of the semiconductor package, the thermal activation of the fuse structure results in a de-wetting or detaching of the fuse structure from the metal stack reducing an adhesion of the fuse structure with the metal stack. In particular, thermal activation of the fuse structure or fuse layer makes the fuse structure de-wet or enable de-wetting of one or more layers of the metal stack. De-wetting allows the thermal expansion roll the layers from each other’s and to create a short circuit.

[0047] In an exemplary implementation of the semiconductor package, the fuse structure comprises one or more of metal or solder alloys, composite solder alloys, solder alloys with additives or metals / alloys encapsulating / sandwiching additives enabling temperature-triggered de-wetting. These composite solder alloys can be efficiently applied as the fuse structure.

[0048] For example, the fuse activation temperature may lie above processing and soldering temperatures applied in processing and manufacturing of the semiconductor package. In this scenario, the fuse structure will not be activated during normal processing or manufacturing of the semiconductor package and can only be activated at or beyond fuse activation temperature.

[0049] In an exemplary implementation of the semiconductor package, the semiconductor package comprises: a second die pad at a second main surface of the semiconductor die, the second main surface opposing the main surface of the semiconductor die; a second metal stack disposed on top of the second die pad; a second metal connector extending through the encapsulant to the second metal stack for enabling a second current flow via the second metal stack to the semiconductor die; wherein the second metal stack comprises a second fuse structure that can be thermally activated at the fuse activation temperature, wherein the thermal activation of the second fuse structure reduces the second current flow to the semiconductor die.

[0050] Thermal fuse layers can be applied for protecting on one or on both surfaces / sides of a semiconductor die in case of dies with double sided connections and vertical current flow. One or several different thermal fuse layers can also be used in such a semiconductor package.

[0051] In an exemplary implementation of the semiconductor package, forming an embedded component package (ECP) comprises: at least one semiconductor die embedded inside a multilayer printed circuit board (PCB), laminate and at least one metal connector electrically connecting the at least one semiconductor die, wherein the at least one metal connector comprises a plated microvia. Thus, the metal stack with the fuse structure can be efficiently applied in ECP packages.

[0052] According to a second aspect, the disclosure relates to a method for producing a semiconductor package with integrated fuse structure, the method comprising: forming a die pad on a main surface of the semiconductor die for electrically connecting the semiconductor die; disposing a metal stack on top of the die pad; encapsulating the semiconductor die and the metal stack by an encapsulant; and forming a metal connector extending through the encapsulant to the metal stack for enabling a current flow via the metal stack to the semiconductor die; wherein the metal stack comprises a fuse structure that can be thermally activated, wherein the thermal activation of the fuse structure prevents the current flow to the semiconductor die. The thermal activation of the fuse structure further prevents the adhesion between the fuse layer and the barrier layers within the metal stack. The thermal expansion of the encapsulant acts on the metal stack electrically disconnecting the layers of the metal stack.

[0053] Such a method allows producing a semiconductor package as described above.

[0054] In embodiments of the disclosure, the thermal fuse or fuse structure can be located on top of the die and is in direct contact with the die surface. The fuse can be located exactly on top of the critical area that generates heat in case of the failure which allows accurate and fast temperature detection.

[0055] The fuse can be integrated to the component during manufacturing processes. Manufacturing can be done with normal structuring or plating and sputtering processes that are used in wafer processing. Hence, no additional process steps are required in manufacturing which results in fast manufacturing process at low cost.

[0056] No additional components or structures or processes are required thereby resulting in small size and low cost when manufacturing the semiconductor package. Little or no additional parasitics such as increased resistance are introduced. The structure does not reduce electrical performance of the packaged device.

[0057] The manufacturing process is compatible with a normal ECP process. The process is thus easy to adapt to production and requires no major changes to product or concept.

[0058] BRIEF DESCRIPTION OF THE DRAWINGS

[0059] Further embodiments of the disclosure will be described with respect to the following figures, in which:

[0060] Figure 1 shows a cross section of a thermal fuse structure on a die surface according to the disclosure; Figure 2 shows a cross section of a semiconductor package with integrated fuse structure according to the disclosure with a prepreg as expansion layer;

[0061] Figure 3 shows a cross section of a semiconductor package with integrated fuse structure according to the disclosure with an additional expansion layer and an optional fuse structure that can be manufactured on the die back side;

[0062] Figures 4a and 4b show cross sections of a metal stack for a semiconductor package with a melting layer as integrated fuse structure according to a first embodiment;

[0063] Figures 4c and 4d show cross sections of a metal stack for a semiconductor package with a brittle intermetallic layer as integrated fuse structure according to a second embodiment; and

[0064] Figures 4e and 4f show cross sections of a metal stack for a semiconductor package with a de-wetting or detaching layer as integrated fuse structure according to a third embodiment.

[0065] DETAILED DESCRIPTION OF EMBODIMENTS

[0066] In the following detailed description, reference is made to the accompanying drawings, which form a part thereof, and in which is shown by way of illustration specific aspects in which the disclosure may be practiced. It is understood that other aspects may be utilized and structural or logical changes may be made without departing from the scope of the disclosure. The following detailed description, therefore, is not to be taken in a limiting sense, and the scope of the disclosure is defined by the appended claims.

[0067] It is understood that comments made in connection with a described method may also hold true for a corresponding device or system configured to perform the method and vice versa. For example, if a specific method step is described, a corresponding device may include a unit to perform the described method step, even if such unit is not explicitly described or illustrated in the figures. Further, it is understood that the features of the various exemplary aspects described herein may be combined with each other, unless specifically noted otherwise.

[0068] Figure 1 shows a cross section of a thermal fuse structure 112 on a die surface according to the disclosure. The semiconductor package 100 comprises: a semiconductor die 101 with die pad 102 (e.g., made of Aluminum, Al or AICu) arranged on a main surface of the semiconductor die 101 for electrically connecting the semiconductor die 101.

[0069] The semiconductor package 100 comprises a metal stack 110 disposed on top of the die pad 102. The metal stack 110 comprises a fuse structure 112 that can be thermally activated.

[0070] The semiconductor package 100 comprises a metal connector 104 or bump (e.g., made of Copper, Cu) disposed on the metal stack 110 for enabling a current flow via the metal stack 110 to the semiconductor die 101 .

[0071] An encapsulant encapsulating the semiconductor die 101 and the metal stack 110 is not shown in Figure 1.

[0072] The thermal activation of the fuse structure 112 will reduce a current flow to the semiconductor die 101. Thus, the fuse structure 112 can protect the semiconductor die 101 against short circuit which can result in damage.

[0073] The fuse structure 112 can comprises a material or a combination of materials comprising at least one of metals, alloys and additives including non-metallic or metallic compounds.

[0074] The thermal activation of the fuse structure 112 allows thermal expansion to create an open circuit between the semiconductor die 101 and the metal connector 104 in the semiconductor package 100, e.g., as described below with respect to Figures 2 and 3.

[0075] The metal stack 110 may comprise two barrier layers 111 , 113. The fuse structure 112 is layered between the two barrier layers 111 , 113.

[0076] These barrier layers 111 , 113 are diffusion barrier layers that are configured to adhere to the fuse structure 112 and to prevent the fuse structure 112 from diffusion to the die pad 102 and / or the metal connector 104.

[0077] The thermal activation of the fuse structure 112 reduces an adhesion of the barrier layers 111 , 113 to the fuse structure 112. In one exemplary implementation described in this disclosure as the first embodiment and further described below with respect to Figures 4a and 4b, the thermal activation of the fuse structure 112 at least partially melts the fuse structure 112 or at least undergoes partial or complete solid-to-liquid phase transition.

[0078] The fuse structure 112 may comprise a low melting metal or metal alloy melting at a temperature range between 118 and 365 degrees Celsius, for example, or at a temperature range between 118 and 1065 degrees Celsius, for example.

[0079] For example, Sn-ln alloys melt at about 118 degrees Celsius; Au-Ge, Au-Si alloys melt at about 365 degrees Celsius. Other high temperature solders may even melt at temperatures from about 450 degrees Celsius to about 1065 degrees Celsius, such as pure Au, Ag-Cu-ln, Ag-ln, Au-ln, etc.

[0080] In one example, the fuse structure 112 may comprise solder metals or alloys which undergo phase transition in an activation temperature range based on one or a combination of the following metals: Bi, Au, Sn, Pb, Ag, Cd, Zn, Ge, Cu, In.

[0081] Such metals or alloys may be for example Bi, Au-Sn, Pb-Sn, Pb-Sn-Ag, Au-Ge, Cd-Zn, etc. In one example, the fuse structure may comprise eutectic 80Au / 20Sn solder alloy.

[0082] In one exemplary implementation described in this disclosure as the second embodiment and further described below with respect to Figures 4c and 4d, the thermal activation of the fuse structure 112 makes the fuse structure 112 to form brittle intermetallic and / or voids in areas of the metal stack 110 reducing an adhesion of the fuse structure 112 with the metal stack 110.

[0083] The fuse structure 112 may comprise one or more intermetallic compounds, for example.

[0084] In one exemplary implementation described in this disclosure as the third embodiment and further described below with respect to Figures 4e and 4f, the thermal activation of the fuse structure 112 makes the fuse structure 112 de-wetting from the metal stack 110 reducing an adhesion of the fuse structure 112 with the metal stack 110.

[0085] The fuse structure 112 may comprise one or more of metal or solder alloys, composite solder alloys, solder alloys with additives or metals / alloys encapsulating / sandwiching additives enabling temperature-triggered de-wetting, for example. The fuse activation temperature lies above processing and soldering temperatures applied in processing and manufacturing of the semiconductor package 100.

[0086] Figure 2 shows a cross section of a semiconductor package 100 with integrated fuse structure 112 according to the disclosure with a prepreg 103 as expansion layer.

[0087] The semiconductor package comprises: a semiconductor die 101 comprising one or more die pads 102 arranged on a main surface 101a of the semiconductor die 101 for electrically connecting the semiconductor die 101 ; a metal stack 110 disposed on top of the one or more die pads 102; an encapsulant 103 encapsulating the semiconductor die 101 and the metal stack 110; and a metal connector 104 extending through the encapsulant 103 to the metal stack 110 for enabling a current flow 120 via the metal stack 110 to the semiconductor die 101. The metal stack 110 comprises a fuse structure 112 that can be thermally activated. The metal stack 110 forms a melting or temperature reduced adhesion interface 202 as can be seen from the upper drawing in Figure 2. The thermal activation of the fuse structure 112 reduces the current flow 120 to the semiconductor die 101 as can be seen from the lower drawing where the open circuit configuration with reduced or interrupted current flow 121 is depicted.

[0088] The encapsulant 103 can be for example a prepreg with enough high CTE in z-direction, i.e., from bottom to the top in these drawings. The encapsulant 103 can also be a resin film, molding sheet, molding resin or other filled or non-filled polymer material. The open circuit with open connection 122 as shown in the lower drawing results due to thermal expansion 123 of the prepreg 103.

[0089] Figure 2 thus shows the functionality of the fuse structure 112 or thermal fuse structure, respectively. The thermal fuse structure 112 is integrated into the die metallization and the thermal expansion 123 of the surrounding packaging materials, e.g., prepreg 103, is used to break and open the electrical connection 120 between the PCB routing and the component 101. The idea is that the new metal structure 110 has an integrated weakness (i.e., the fuse structure) that will be activated only when the temperature increases above a predefined temperature. The thermally activated weakness together with thermal expansion 123 of the used PCB materials will create an open connection 122 in the fuse structure 112 which results in an open circuit 121 between the embedded component 101 and package. This metal structure 110 can replace a normal TiW / Cu bump that is used in ECPs. The fuse structure 112 can be integrated either to the top side of the die 101 as shown in Figure 2 and / or bottom side of the die as shown in Figure 3.

[0090] The thermally activated weakness inside the die pad metallization or metal stack 110 will be activated when the temperature on the die surface reaches the predefined temperature. In this predefined temperature one layer or several layers in the die pad metallization stack 110 will weaken to allow thermal expansion / stress (caused by the CTE and / or CTE mismatch) to pull and separate the layers from each other resulting in an open connection 122. This open connection 122 will cause an open circuit 121 that prevents current flow 120 through the component and prevents the uncontrollable self-heating and more severe / extensive damages. The activation temperature is above the normal processing and soldering temperatures. Different mechanisms can be used to activate the fuse and cut the current flow to the device as described below with respect to Figures 4a to 4f.

[0091] Figure 3 shows a cross section of a semiconductor package 100 with integrated fuse structure 112 according to the disclosure with an additional expansion layer 310 and an optional fuse structure 132 that can be manufactured on the die back side. The layers 310 and 103 are marked with the same pattern in Figure 3. This means that the materials for the additional expansion layer 310 and the encapsulant 103 can be the same but processed at different times. An additional resin film 311 as shown in Figure 3 can be applied or alternatively be replaced by the encapsulant 103 and / or the additional expansion layer 310.

[0092] The semiconductor package 100 comprises: a semiconductor die 101 comprising one or more die pads 102 arranged on a main surface 101a of the semiconductor die 101 for electrically connecting the semiconductor die 101 ; a metal stack 110 disposed on top of the one or more die pads 102; an encapsulant 103 encapsulating the semiconductor die 101 and the metal stack 110; and a metal connector 104 extending through the encapsulant 103 to the metal stack 110 for enabling a current flow 120 via the metal stack 110 to the semiconductor die 101. As already described above with respect to Figure 2, the metal stack 110 comprises a fuse structure 112 that can be thermally activated. The metal stack 110 forms a melting or temperature reduced adhesion interface 202 as can be seen from the upper drawing in Figure 3. The thermal activation of the fuse structure 112 reduces the current flow 120 to the semiconductor die 101 as can be seen from the lower drawing where the open circuit configuration with reduced or interrupted current flow 121 is depicted. The semiconductor package 100 comprises: a second die pad 105 at a second main surface 101b of the semiconductor die 101. The second main surface 101b (e.g., bottom surface) is opposing the main surface 101a (e.g., top surface) of the semiconductor die 101.

[0093] The semiconductor package 100 comprises: a second metal stack 130 disposed on top of the second die pad 105; a second metal connector 106 extending through the encapsulant 103 to the second metal stack 130 for enabling a second current flow via the second metal stack 130 to the semiconductor die 101 .

[0094] The second metal stack 130 comprises a second fuse structure 132 that can be thermally activated at the fuse activation temperature. The thermal activation of the second fuse structure 132 reduces the second current flow to the semiconductor die 101 , e.g. as described above for the first fuse structure 112, and results in an open connection 122 at the second main surface 101 b (here the bottom surface) as shown in the lower drawing of Figure 3.

[0095] Beside the encapsulant 103 that may be a prepreg as described above with respect to Figure 2, an additional expansion layer 310, e.g., an additional prepreg may be formed as thermal expansion layer. This additional expansion layer 310 may have the same or different CTE (coefficient of thermal expansion) than the encapsulant 103 or first prepreg. Besides, a resin film 311 (e.g., Tg>260° C) may be formed on top of the additional expansion layer 310 and / or on bottom of the expansion layer 103 as can be seen from Figure 3.

[0096] The semiconductor package 100 may form an embedded component package, ECP, which comprises: at least one semiconductor die 101 embedded inside a two-layer or a multilayer printed circuit board, PCB, laminate and at least one metal connector 104 electrically connecting the at least one semiconductor die 101. The at least one metal connector 104 may comprise a plated microvia as shown in Figure 3. While Figure 3 shows a 2-layer PCB, it understands that a multilayer PCB, i.e. , a PCB with 3, 4 or more layers, can be implemented as well.

[0097] Figures 4a and 4b show cross sections of a metal stack 110 for a semiconductor package 100 with a melting layer 401 as integrated fuse structure 112 according to a first embodiment.

[0098] The layer 401 between diffusion barrier / adhesion layers 111 , 113 melts when the selected temperature is reached as can be seen in Figure 4b. Remaining melted layers 401a, 401b are shown in Figure 4b. Material-systems that can be utilized as the melting layer 401 are metals and alloys with sharp phase-change points e.g., melting point, liquidus temperature (temperature above which the material is completely liquid) or solidus temperature (temperature below which the material is completely solid). The phase change of these materials at the specified temperatures are abrupt, which is ideal for the concept described here. Below the temperature trigger, these materials maintain electrical contact. Above the temperature trigger, the abrupt phase change allows the thermal stress or thermal expansion to pull the parts away and create an open circuit. Example systems with melting / liquidus / solidus temperatures in the example range 265- 310 degrees Celsius are for example: Bi, Au80Sn20, Pb90Sn10, Pb92Sn5.5Ag2.5, Pb88Sn10Ag2, Pb90Sn5Ag5, Pb92.5Sn5Ag2.5, Pb93.5Sn5Ag1.5, Pb95.5Sn2Ag2.5, Cd82.5Zn17.5, Cd70Zn30.

[0099] Metals or alloy compositions can be altered to tune the phase change temperatures. The metal or alloys listed above are typical solder systems (high temperature solders).

[0100] Therefore, these systems can be incorporated as melting layer 401 using associated soldering techniques. Fabrication of these melting layers 401 can also be done by magnetron sputtering of appropriate alloy targets, electroplating or physical vapor deposition techniques.

[0101] Figures 4c and 4d show cross sections of a metal stack 110 for a semiconductor package 100 with a brittle intermetallic layer 402 as integrated fuse structure 112 according to a second embodiment.

[0102] The layer 402 between diffusion barrier / adhesion layers 111 , 113 will form intermetallics that crack when selected temperatures are reached. Cracked intermetallics layers 402a, 402b are shown in Figure 4d.

[0103] Intermetallics formed, especially at solder joints are brittle and considered problematic for reliability. However, controlled intermetallic formation by predefined (fuse activation) temperature that are brittle can be used as a thermal fuse. Thermal fuse material systems can either form intermetallics either with the Ti barrier layer or with copper or within the thermal fuse system. These systems are typically solder alloys and / or multilayer stacks that retain electrical contact during normal operation. These alloys can either be applied as a molten layer, sputtered, physically vapor deposited, etc. Examples of thermal fuse structures that form intermetallics with Ti barrier include Au / Au-Sn (forming AuTi4), Sn (forming Ti2Sns) or SnojCu (forming TieSne), Ni / Au-Sn (forming Au4Ti[Sn]). Material systems that form intermetallics with copper include solders such as Sns.sAg, Sn3.5Ago.5Cu, SnojCu, etc. (typically, leading to CueSnsq-phase or CusSne-phase intermetallics). These systems may also work as multilayer stacks for the described purpose. Multilayer stacks that can form intermetallics within themselves on thermal triggers include Au / Au-Sn / Ni systems that form AusSn, (Au,Ni)sSn or (Ni,Au)sSn2. The rate and temperature of formation of these intermetallics can be tailored by the layer thickness and compositions in the range of about 260-350 degrees Celsius. Further, the addition of additives to solders (e.g., TiC>2, ZnO, etc. to Sn-based solders) can cause CTE mismatch and local stresses with intermetallics formed. These additives (in terms of content, size, etc.) can be used to further tailor the formation-temperature and mechanical stability of intermetallics.

[0104] Figures 4e and 4f show cross sections of a metal stack 110 for a semiconductor package 100 with a de-wetting or detaching layer 403 as integrated fuse structure 112 according to a third embodiment.

[0105] The layer 403 between diffusion barrier / adhesion layers 111 , 113 will de-adhere or detach when the temperature reaches the selected temperature. Detaching and detached layer 403a is shown in Figure 4f.

[0106] In one example, a Titanium barrier layer can be made to de-adhere or detach from e.g., Cu by inducing oxidation using an intermediate underlayer that releases oxygen when the specified temperature is attained. This can be brought about using solders with additives such as graphene oxide or graphite oxide that release oxidizing species (hydroxy groups or water) on thermal degradation triggered at specific temperatures. These materials can also be tailored to release oxidizing species at specific temperatures (e.g., about 248-300 degrees Celsius) depending on the amount and type of oxygen moieties in graphite oxide or graphene oxide.

[0107] Other candidate materials to bring about Ti-oxidation are materials such as charged lithium- ion battery cathode materials, which give out oxygen on thermal degradation in a temperature- controlled manner. For example, Delithiated LixNiO.5Mn1.5O4 (LNMO), Li0.33 Ni0.8 Co0.15AI0.05O2 and Lio.33 Nii / 3 C01 / 3 Mni / 302 release oxygen in the range of about 260-280 degrees Celsius.

[0108] While a particular feature or aspect of the disclosure may have been disclosed with respect to only one of several implementations, such feature or aspect may be combined with one or more other features or aspects of the other implementations as may be desired and advantageous for any given or particular application. Furthermore, to the extent that the terms "include", "have", "with", or other variants thereof are used in either the detailed description or the claims, such terms are intended to be inclusive in a manner similar to the term "comprise". Also, the terms "exemplary", "for example" and "e.g." are merely meant as an example, rather than the best or optimal. The terms “coupled” and “connected”, along with derivatives may have been used. It should be understood that these terms may have been used to indicate that two elements cooperate or interact with each other regardless whether they are in direct physical or electrical contact, or they are not in direct contact with each other.

[0109] Although specific aspects have been illustrated and described herein, it will be appreciated by those of ordinary skill in the art that a variety of alternate and / or equivalent implementations may be substituted for the specific aspects shown and described without departing from the scope of the disclosure. This application is intended to cover any adaptations or variations of the specific aspects discussed herein.

[0110] Although the elements in the following claims are recited in a particular sequence with corresponding labeling, unless the claim recitations otherwise imply a particular sequence for implementing some or all of those elements, those elements are not necessarily intended to be limited to being implemented in that particular sequence.

[0111] Many alternatives, modifications, and variations will be apparent to those skilled in the art in light of the above teachings. Of course, those skilled in the art readily recognize that there are numerous applications of the disclosure beyond those described herein. While the disclosure has been described with reference to one or more particular embodiments, those skilled in the art recognize that many changes may be made thereto without departing from the scope of the disclosure. It is therefore to be understood that within the scope of the appended claims and their equivalents, the disclosure may be practiced otherwise than as specifically described herein.

Claims

CLAIMS1 . A semiconductor package (100) with integrated fuse structure (112), the semiconductor package (100) comprising: a semiconductor die (101) comprising a die pad (102) arranged on a main surface (101a) of the semiconductor die (101) for electrically connecting the semiconductor die (101); a metal stack (110) positioned on top of the die pad (102); an encapsulant (103) encapsulating the semiconductor die (101) and the metal stack (110); a metal connector (104) extending through the encapsulant (103) to the metal stack (110) for enabling a current flow (120) via the metal stack (110) to the semiconductor die (101); wherein the metal stack (110) comprises a fuse structure (112) that can be thermally activated, wherein the thermal activation of the fuse structure (112) reduces the current flow (120) to the semiconductor die (101).

2. The semiconductor package (100) of claim 1 , wherein the fuse structure (112) comprises a material or a combination of materials comprising at least one of metals, alloys and additives including non-metallic or metallic compounds.

3. The semiconductor package (100) of claim 1 or 2, wherein the thermal activation of the fuse structure (112) together with a thermal expansion (123) of the encapsulant (103) at the fuse activation temperature creates an open circuit (121) between the semiconductor die (101) and the metal connector (104) in the semiconductor package (100).

4. The semiconductor package (100) of any of the preceding claims, wherein the metal stack (110) comprises two barrier layers (111 , 113), wherein the fuse structure (112) is positioned between the two barrier layers (111 , 113).

5. The semiconductor package (100) of claim 4, wherein the barrier layers (111 , 113) are diffusion barrier layers (111 , 113) that are configured to adhere to the fuse structure (112) and to prevent the fuse structure (112) from diffusion to the die pad (102) and / or the metal connector (104).

6. The semiconductor package (100) of claim 4 or 5, wherein the thermal activation of the fuse structure (112) reduces an adhesion of the barrier layers (111 , 113) to the fuse structure (112).

7. The semiconductor package (100) of any of claims 4 to 6, wherein the thermal activation of the fuse structure (112) at least partially melts the fuse structure (112) or at least undergoes partial or complete solid-to-liquid phase transition.

8. The semiconductor package (100) of any of claims 4 to 7, wherein the fuse structure (112) comprises a low melting metal or metal alloy melting at a temperature range between 118 and 365 degrees Celsius or at a temperature range between 118 and 1065 degrees Celsius.

9. The semiconductor package (100) of any of claims 4 to 8, wherein the fuse structure (112) comprises solder metals or alloys which undergo phase transition in an activation temperature range based on one or a combination of the following metals: Bi, Au, Sn, Pb, Ag, Cd, Zn, Ge, Cu, In.

10. The semiconductor package (100) of any of claims 4 to 9, wherein the thermal activation of the fuse structure (112) makes the fuse structure (112) to form brittle intermetallic and / or voids in areas of the metal stack (110) reducing an adhesion of the fuse structure (112) with the metal stack (110).11 . The semiconductor package (100) of any of claims 4 to 10, wherein the fuse structure (112) comprises one or more intermetallic compounds.

12. The semiconductor package (100) of any of claims 4 to 11 , wherein the thermal activation of the fuse structure (112) makes the fuse structure (112) de-wetting from the metal stack (110) reducing an adhesion of the fuse structure (112) with the metal stack (110).

13. The semiconductor package (100) of any of claims 4 to 12, wherein the fuse structure (112) comprises one or more of metal or solder alloys, composite solder alloys, solder alloys with additives or metals / alloys encapsulating / sandwiching additives enabling temperature-triggered de-wetting.

14. The semiconductor package (100) of any of the preceding claims, comprising: a second die pad (105) at a second main surface (101 b) of the semiconductor die (101), the second main surface (101b) opposing the main surface (101a) of the semiconductor die (101); a second metal stack (130) disposed on top of the second die pad (105); a second metal connector (106) extending through the encapsulant (103) to the second metal stack (130) for enabling a second current flow via the second metal stack (130) to the semiconductor die (101); wherein the second metal stack (130) comprises a second fuse structure (132) that can be thermally activated at the fuse activation temperature, wherein the thermal activation of the second fuse structure (132) reduces the second current flow to the semiconductor die (101).

15. The semiconductor package (100) of any of the preceding claims, forming an embedded component package, ECP, comprising: at least one semiconductor die (101 ) embedded inside a multilayer printed circuit board, PCB, laminate and at least one metal connector (104) electrically connecting the at least one semiconductor die (101), wherein the at least one metal connector (104) comprises a plated microvia.

Citation Information

Patent Citations

  • Semiconductor device and its manufacture

    JP1999224900A

  • Fuse device

    JP2004103604A

  • Semiconductor device and trimming method thereof

    JP2021044306A

  • Method for manufacturing semiconductor device

    KR1020090085466A

  • Printed wiring board, manufacturing method for printed wiring board and electronic device

    US20100032194A1