Recombinant collagen contact lens lubricating solution and use thereof
By combining recombinant collagen with polyvinyl alcohol, a contact lens lubricant is formed, which solves the problem that existing lubricants cannot repair corneal and conjunctival damage. It improves lubrication, moisturization and stability, and enhances the healing effect of cornea/conjunctiva.
Patent Information
- Application Number
- PCT/CN2026/094228
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2025-05-08
- Filing Date
- 2026-04-30
- Publication Date
- 2026-11-12
AI Technical Summary
Existing lubricant products, while improving the lubrication of the ocular surface, cannot actively repair corneal and conjunctival damage, and the recombinant collagen lacks long-term stability in aqueous solutions, affecting product efficacy.
A compound of recombinant type III collagen, sodium chloride, sodium dihydrogen phosphate, disodium hydrogen phosphate, and polyvinyl alcohol is used to form a recombinant collagen contact lens lubricant. By forming a protective film on the corneal/conjunctival surface, it enhances lubrication and cell adhesion, promotes epithelial cell migration, improves the healing of corneal/conjunctival injuries, and remains stable at room temperature.
It achieves the lubricating and moisturizing properties of the lubricant, reduces friction between the ocular surface and the lens, repairs corneal/conjunctival damage, improves wearing comfort, and maintains long-term stability at room temperature.
Smart Images

Figure CN2026094228_12112026_PF_FP_ABST
Abstract
Description
A recombinant collagen contact lens lubricant and its application Technical Field
[0001] This invention belongs to the field of medical device and eye care technology, specifically relating to a recombinant collagen contact lens lubricant and its application. Background Technology
[0002] Due to lifestyle habits and genetic factors, the number of people with myopia is increasing year by year, especially among teenagers, whose age of onset is gradually decreasing and whose incidence rate is growing rapidly. Myopia has become a global medical and health problem and a hot topic in society. With the increasing demand for myopia prevention and refractive correction, the number of contact lens wearers is increasing, showing trends of younger onset and long-term wear.
[0003] Contact lenses can be categorized into rigid gas permeable (RGP) lenses and soft contact lenses based on their rigidity. A World Health Organization research report shows that the proportion of people worldwide choosing RGP lenses to correct various refractive errors has been rapidly increasing in recent years. RGP lenses mainly include rigid gas permeable (RGP) lenses, orthokeratology (Ortho-k) lenses, and scleral lenses. Ortho-k lenses, commonly known as OK lenses, are a special type of RGP lens suitable for children and adolescents aged 8-18. They are customized products that temporarily reduce myopia by altering the shape of the cornea, used to prevent and delay myopia progression. After wearing an Ortho-k lens, the curvature of the central cornea flattens within a certain range, thus temporarily reducing a certain amount of myopia. It is a reversible, non-surgical physical ortho-adjustment treatment method. Modern orthokeratology lenses reshape the cornea by being worn overnight. This method minimizes foreign body sensation, is easy to adapt to, and the lenses are less likely to be lost. Furthermore, wearers do not need to wear eyeglasses or soft contact lenses during the day, allowing for convenient participation in sports and recreational activities. However, due to varying levels of expertise among fitting institutions, insufficient professional knowledge, a lack of technical personnel, and inadequate safety management and supervision, the efficacy and safety (quality) of contact lenses and related products are particularly prominent issues. Additionally, orthokeratology lenses require high hygiene standards for lens care, necessitating the use of contact lens solutions and lubricants. Inadequate cleaning and care can lead to eye inflammation and other problems.
[0004] Currently, the main lubricating fluid products on the market are sodium hyaluronate and artificial tears. While these products can effectively improve the lubrication of the ocular surface, they lack the activity to actively repair the cornea and conjunctiva. In recent years, research has found that collagen has excellent lubricating properties and can effectively promote the repair of epithelial cells and peripheral nerve fibers in human tissues and organs. Furthermore, recombinant collagen has a positive effect on the migration of human corneal epithelial cells in vitro. Existing technology also reports a novel bioengineered cornea made from highly purified and strictly sterilized collagen extracted from pig skin. Researchers stabilized the loose collagen molecules to form a strong and transparent material capable of withstanding surgical procedures during processing and implantation in the eye. This material can not only be mass-produced but also effectively improves corneal thickness and curvature in visually impaired individuals, successfully helping blind patients regain their sight. This demonstrates that natural animal-derived collagen has a repairing effect on ocular surface tissues and possesses high biocompatibility.
[0005] Simpson's team sequentially added recombinant human type III collagen (RHCⅢ) aqueous solution, 2-morpholinoethanesulfonic acid, and 2-methacryloyloxyethyl phosphocholine (MPC) to a syringe mixing system to prepare RHCⅢ-MPC hydrogels at 0°C. After crosslinking, the gels were demolded, washed, and bottled in phosphate-buffered saline (PBS) or PBS containing 1% chloroform (C-PBS). The PBS bottles were irradiated with a 17 kGy electron beam. Implants irradiated with C-PBS and 17 kGy were then used in rabbits. Studies showed that the implants successfully achieved re-epithelialization, improving the regenerative capacity of corneal epithelium, stroma, and nerves, demonstrating great potential for corneal treatment. Malhotra also prepared composite implants based on recombinant human type III collagen and 2-methacryloyloxyethyl phosphocholine by introducing silica nanoparticles that release KR-12, reducing the spread of herpes simplex virus type I (HSV-1) and thus promoting corneal repair in HSV-1-infected corneas.
[0006] While recombinant collagen technology overcomes the problems of poor solubility and high immunogenicity of animal-derived collagen, its long-term stability in aqueous solutions still faces challenges. During storage, recombinant collagen is readily hydrolyzed into short peptides and amino acids in aqueous solutions, affecting product efficacy. Therefore, there is a need to develop an ophthalmic lubricant with excellent ocular surface lubrication properties, actively repairing corneal and conjunctival damage, and maintaining long-term stability under room temperature storage conditions. Summary of the Invention
[0007] To address some shortcomings in existing technologies, this invention provides a recombinant collagen contact lens lubricant and its application. The recombinant collagen contact lens lubricant comprises recombinant type III collagen, sodium chloride, sodium dihydrogen phosphate, disodium hydrogen phosphate, polyvinyl alcohol, and water for injection. This recombinant collagen contact lens lubricant can be safely and effectively used for moisturizing and lubricating contact lenses, improving and relieving dry eyes, and enhancing wearing comfort. Furthermore, the recombinant collagen contact lens lubricant can repair corneal and conjunctival damage and maintains long-term stability under normal temperature storage conditions, demonstrating excellent market application prospects.
[0008] To achieve the above-mentioned technical objectives, the present invention employs the following technical means:
[0009] The present invention first provides a recombinant collagen contact lens lubricant, which comprises: recombinant collagen, sodium chloride, sodium dihydrogen phosphate, disodium hydrogen phosphate, polyvinyl alcohol, and water for injection.
[0010] Preferably, each liter of recombinant collagen contact lens lubricant contains 2.5–10 g of polyvinyl alcohol, 4.25–17 g of sodium chloride, 0.03–0.12 g of disodium hydrogen phosphate, 0.7–2.8 g of sodium dihydrogen phosphate, and 20–80 g of recombinant collagen, with the remainder being water for injection.
[0011] Preferably, each liter of recombinant collagen contact lens lubricant contains 5g of polyvinyl alcohol, 8.5g of sodium chloride, 0.06g of disodium hydrogen phosphate, 1.4g of sodium dihydrogen phosphate, and 40g of recombinant collagen, with the remainder being water for injection.
[0012] Preferably, the recombinant collagen includes recombinant type III collagen, the amino acid sequence of which is shown in SEQ ID NO:1.
[0013] Preferably, the preparation method of the recombinant collagen contact lens lubricant includes:
[0014] Polyvinyl alcohol, sodium chloride, disodium hydrogen phosphate and sodium dihydrogen phosphate are mixed, then water for injection is added and premixed under stirring conditions. Then recombinant collagen is added at room temperature, mixed evenly, filtered, filled and stored at room temperature.
[0015] Preferably, the premixing is performed by stirring at 80°C and 300 r / min for 2 to 3 hours.
[0016] Preferably, the filtration process involves sequentially passing the material through 0.45μm and 0.22μm filter membranes.
[0017] The present invention also provides the application of the above-mentioned recombinant collagen contact lens lubricant as a contact lens lubricant.
[0018] Preferably, the contact lens includes any one of soft contact lenses, rigid contact lenses, colored contact lenses, and silicone hydrogel contact lenses.
[0019] Compared with the prior art, the beneficial effects of the present invention are as follows:
[0020] The recombinant type III collagen used in the recombinant collagen contact lens lubricant of this invention contains a large number of hydrophilic groups, which enhance the lubrication and moisturizing properties of the lubricant, moisturize the ocular surface, reduce friction between the ocular surface and the lens, and effectively improve discomfort symptoms such as dry eyes. Furthermore, the recombinant collagen has strong cell adhesion, which can guide epithelial cells to migrate into the defect area, enhance the adhesion and cell stability of epithelial cells around the corneal / conjunctival injury site, thereby accelerating the healing of corneal / conjunctival injuries. Moreover, the recombinant type III collagen is sequence-stable in aqueous solution, not easily degraded, and can maintain long-term stability under room temperature storage conditions.
[0021] This invention combines recombinant collagen with polyvinyl alcohol to obtain the recombinant collagen contact lens lubricant. The combination of recombinant collagen and polyvinyl alcohol enhances the film-forming properties and viscosity of either ingredient, forming a protective film on the corneal / conjunctival surface to protect the tissue beneath the cornea / conjunctiva and prolong its residence time on the ocular surface.
[0022] The recombinant collagen contact lens lubricant of this invention is non-irritating and non-cytotoxic to the eyes, and can safely and effectively relieve eye dryness and discomfort caused by wearing contact lenses, improving wearing comfort. In addition, the recombinant collagen contact lens lubricant can also repair corneal and conjunctival damage and maintain long-term stability under normal temperature storage conditions, showing great market application prospects. Attached Figure Description
[0023] Figure 1 is a flowchart of the preparation process of the recombinant collagen contact lens lubricant of the present invention.
[0024] Figure 2 shows cell images before and after cell migration.
[0025] Figure 3 shows the moisturizing rate of different lubricants.
[0026] Figure 4 shows the results of the corneal signs score.
[0027] Figure 5 shows the corneal healing rate.
[0028] Figure 6 shows the results of corneal HE staining after lubricant treatment; in the figure, a is recombinant collagen contact lens lubricant; b is sodium hyaluronate contact lens lubricant; and c is physiological saline.
[0029] Figure 7 shows the results of Masson staining of the cornea after lubricant treatment; in the figure, a is recombinant collagen contact lens lubricant; b is sodium hyaluronate contact lens lubricant; and c is physiological saline. Detailed Implementation
[0030] The present invention will be further described below with reference to the accompanying drawings and specific embodiments, but the scope of protection of the present invention is not limited thereto. In the embodiments of the present invention, unless otherwise described, conventional experimental methods are used. The processes involved in the embodiments, unless otherwise described, are those that can be understood and easily implemented by those skilled in the art based on the product manual or basic knowledge in the field, and therefore will not be described in detail.
[0031] The collagen used in Examples 1-3 was recombinant type III collagen, which was obtained from Jiangsu Chuangjian Medical Technology Co., Ltd., and its amino acid sequence is shown in SEQ ID NO:1; sodium chloride was obtained from Jiangsu Qinfen Pharmaceutical Co., Ltd.; sodium dihydrogen phosphate and disodium hydrogen phosphate were obtained from Hunan Jiudian Hongyang Pharmaceutical Co., Ltd.; and polyvinyl alcohol was obtained from Sichuan Laitejuxin Pharmaceutical Excipients Co., Ltd.
[0032] SEQ ID NO:1
[0033]
[0034] Example 1: Preparation of Recombinant Collagen Contact Lens Lubricant
[0035] Formula for 1L recombinant collagen contact lens lubricant:
[0036]
[0037] The preparation process of 1L recombinant collagen contact lens lubricant is shown in Figure 1. The specific steps include:
[0038] Polyvinyl alcohol, sodium chloride, disodium hydrogen phosphate, and sodium dihydrogen phosphate were added sequentially to a beaker, followed by water for injection. The mixture was premixed by stirring at 80°C and 300 rpm for 2–3 hours. After mixing, the mixture was cooled to room temperature. Then, recombinant type III collagen was added, and the mixture was stirred at 330 rpm for 10–20 minutes until homogeneous. The resulting solution was filtered sequentially through 0.45 μm and 0.22 μm filter membranes to obtain the recombinant collagen contact lens lubricant, which was then filled and stored at room temperature.
[0039] Formula for 1L recombinant collagen contact lens lubricant:
[0040]
[0041] Preparation of 1L recombinant collagen contact lens lubricant:
[0042] Polyvinyl alcohol, sodium chloride, disodium hydrogen phosphate, and sodium dihydrogen phosphate were added sequentially to a beaker, followed by water for injection. The mixture was premixed by stirring at 80°C and 300 rpm for 2–3 hours. After mixing, the mixture was cooled to room temperature. Then, recombinant type III collagen was added, and the mixture was stirred at 330 rpm for 10–20 minutes until homogeneous. The resulting solution was filtered sequentially through 0.45 μm and 0.22 μm filter membranes to obtain the recombinant collagen contact lens lubricant, which was then filled and stored at room temperature.
[0043] Example 3: Preparation of Recombinant Collagen Contact Lens Lubricant
[0044] Formula for 1L recombinant collagen contact lens lubricant:
[0045]
[0046] Preparation of 1L recombinant collagen contact lens lubricant:
[0047] Polyvinyl alcohol, sodium chloride, disodium hydrogen phosphate, and sodium dihydrogen phosphate were added sequentially to a beaker, followed by water for injection. The mixture was premixed by stirring at 80°C and 300 rpm for 2–3 hours. After mixing, the mixture was cooled to room temperature. Then, recombinant type III collagen was added, and the mixture was stirred at 330 rpm for 10–20 minutes until homogeneous. The resulting solution was filtered sequentially through 0.45 μm and 0.22 μm filter membranes to obtain the recombinant collagen contact lens lubricant, which was then filled and stored at room temperature.
[0048] Example 4: Toxicity Study of Recombinant Collagen Contact Lens Lubricant
[0049] In this embodiment, physiological saline was used as the blank control group, recombinant collagen solution was used as control group 1, polyvinyl alcohol solution was used as control group 2, and sodium hyaluronate contact lens lubricant (Shinton Biotechnology Co., Ltd.) was used as control group 3 to investigate the cytotoxicity of recombinant collagen contact lens lubricant.
[0050] The preparation method of the recombinant collagen solution is as follows: 8.5g of sodium chloride, 0.06g of disodium hydrogen phosphate, and 1.4g of sodium dihydrogen phosphate are added sequentially to a beaker. Then, 950.04g of water for injection is added to the beaker, and the mixture is premixed by stirring at 80℃ and 300r / min for 2-3 hours. After mixing, the mixture is cooled to room temperature, and then 40g of recombinant type III collagen is added. The mixture is stirred at 330r / min for 10-20 minutes until homogeneous, obtaining a mixed solution. The mixed solution is then filtered sequentially through 0.45μm and 0.22μm filter membranes to obtain the recombinant collagen solution, which is then filled into containers and stored at room temperature.
[0051] The preparation steps of the polyvinyl alcohol solution are as follows: Weigh 5g of polyvinyl alcohol, 8.5g of sodium chloride, 0.06g of disodium hydrogen phosphate and 1.4g of sodium dihydrogen phosphate and add them to a beaker in sequence. Then add 950.04g of water for injection to the beaker and stir for 2-3 hours at 80℃ and 300r / min for premixing. After mixing, cool to room temperature and filter through 0.45μm and 0.22μm filter membranes in sequence to obtain the polyvinyl alcohol solution. Fill the container and store at room temperature.
[0052] Preparation of sample extracts: Physiological saline, recombinant collagen solution, polyvinyl alcohol solution, sodium hyaluronate contact lens lubricant, and recombinant collagen contact lens lubricant were added to DMEM medium (Gibco) containing 15% fetal bovine serum (Gibco) at a concentration of 0.2 g / mL, and extracted by shaking for 24 h. After extraction, the sample extracts were obtained, namely physiological saline extract, recombinant collagen solution extract, polyvinyl alcohol solution extract, sodium hyaluronate contact lens lubricant extract, and recombinant collagen contact lens lubricant extract.
[0053] Mouse epithelial-like fibroblasts (L-929, purchased from the Shanghai Cell Bank, Chinese Academy of Sciences) were cultured. Cells were removed from the culture flask using trypsin (Gibco), centrifuged at 1000 rpm for 5 min, and the supernatant was discarded. The cell pellet was then resuspended in DMEM complete medium (Gibco) by pipetting and adjusting the concentration to 1×10⁻⁶. 5 Cells / mL were added to 100 μL of cell suspension per well of a 96-well plate, with a cell density of 1 × 10⁶ cells / mL to be tested. 4 Cells / well, 5% CO2, incubated at 37°C for 24 hours.
[0054] After incubation, the culture medium was aspirated, and 100 μL of the above-mentioned physiological saline extract, recombinant collagen solution extract, polyvinyl alcohol solution extract, sodium hyaluronate contact lens lubricant extract, and recombinant collagen contact lens lubricant extract were added to each well, respectively. After incubation for 24 h, the extracts in the wells were removed, and 50 μL of MTT solution (Sigma, 1 mg / mL) was added to each test well. The plates were incubated at 37°C for 2 h. Then, the MTT solution was discarded, and 100 μL of isopropanol solution (Sinopharm) was added to each well. The plates were shaken and placed on a microporous titration plate spectrophotometer with a 570 nm filter to measure the absorbance.
[0055] The cell viability was tested and found to be 98.77% in the blank control group, 97.20% in control group 1, 89.66% in control group 2, 97.17% in control group 3, and 98.20% in the experimental group. This demonstrates that both recombinant collagen and polyvinyl alcohol exhibit good cell activity.
[0056] Example 5: Cell proliferation and cell migration experiments
[0057] In this embodiment, physiological saline was used as the blank control group, recombinant collagen solution was used as control group 1, polyvinyl alcohol solution was used as control group 2, and sodium hyaluronate contact lens lubricant was used as control group 3 to investigate the cell proliferation and cell migration properties of recombinant collagen contact lens lubricant.
[0058] (1) Cell proliferation experiment:
[0059] The preparation methods of recombinant collagen solution and polyvinyl alcohol solution are shown in Example 4.
[0060] Preparation of sample extracts: Physiological saline, recombinant collagen solution, polyvinyl alcohol solution, sodium hyaluronate contact lens lubricant, and recombinant collagen contact lens lubricant were added to DMEM medium (Gibco) at a concentration of 0.2 g / mL and extracted by shaking for 24 h. After extraction, the sample extracts were obtained, namely physiological saline extract, recombinant collagen solution extract, polyvinyl alcohol solution extract, sodium hyaluronate contact lens lubricant extract, and recombinant collagen contact lens lubricant extract.
[0061] Human corneal epithelial cells (HCET, Wuhan Pronosai Life Science Technology Co., Ltd.) were cultured. Cells were removed from the culture flask using trypsin (Gibco), centrifuged at 1000 rpm for 5 minutes, and the supernatant was discarded. The cell pellet was then mixed with DMEM-F12 basal medium (Gibco) to prepare a cell suspension, and the concentration was adjusted to 1×10⁻⁶. 5Cells / mL were added to 100 μL of cell suspension per well of a 96-well plate, with a cell density of 1 × 10⁶ cells / mL to be tested. 4 Cells per well were incubated at 37°C for 24 hours with 5% CO2. After incubation, the culture medium was aspirated, and 100 μL of physiological saline extract, recombinant collagen solution extract, polyvinyl alcohol solution extract, sodium hyaluronate contact lens lubricant extract, and recombinant collagen contact lens lubricant extract were added to each well, respectively. After 24 hours of incubation, the culture medium was removed, and 50 μL of MTT solution (Sigma, 1 mg / mL) was added to each test well. The plates were incubated at 37°C for 2 hours. Then, the MTT solution was discarded, and 100 μL of isopropanol solution (Sinopharm) was added to each well. The plates were shaken and the absorbance was measured on a microplate spectrophotometer with a 570 nm filter. The above operation was repeated to measure cell viability after 48 hours of incubation. The test results are shown in Table 1.
[0062] Table 1. Results of Cell Proliferation Study
[0063]
[0064] As shown in Table 1, recombinant collagen contact lens lubricant can enhance the proliferative activity of corneal epithelial cells.
[0065] (2) Cell migration experiment:
[0066] First, use a marker pen to draw evenly spaced horizontal lines on the back of the 6-hole board, approximately every 0.5cm to 1cm, passing through the holes. Three lines should pass through each hole. Add approximately 8×10mm fillers to the holes. 5 Personal corneal epithelial cells (HCET, purchased from Wuhan Pronosei Life Science Technology Co., Ltd.). After culturing the cells for 24 hours, a 10 μL pipette tip was used to vertically align the well plate with a ruler and gently push downwards to create a longitudinal scratch. The cells were washed three times with PBS to remove the scratched cells. 2 mL of the physiological saline extract, recombinant collagen solution extract, polyvinyl alcohol solution extract, sodium hyaluronate contact lens lubricant extract, and recombinant collagen contact lens lubricant extract prepared in step (1) were added respectively. The cells were cultured at 37°C in a 5% CO2 incubator. After 0 hours and 24 hours, photographs were taken under a 40x microscope with the intersection of the horizontal and vertical scratches as the core. Nine images were obtained from each well, and a total of 27 data points were obtained from each combination.
[0067] The scratch area of each image was calculated using ImageJ image processing software. The cell migration rate of each group was calculated by dividing the total area of migrating cells in the fixed scratch area by the initial area of the fixed scratch area. A graph was plotted with time on the horizontal axis and the migration area ratio on the vertical axis (in %), and the photos of the experimental group and the control group at the initial time 0 and at the end of the experiment were compared. One-way ANOVA was used to analyze the differences in data between the experimental groups, and the chi-square test was performed. The results are shown in Table 2 and Figure 2.
[0068] Table 2. Results of Cell Migration Study
[0069]
[0070] As can be seen from Table 2 and Figure 2, recombinant collagen contact lens lubricant can enhance the migration activity of corneal epithelial cells.
[0071] In summary, the recombinant collagen contact lens lubricant exhibits good proliferative and migration activities.
[0072] Example 6: Lubrication and Moisturizing Properties Test of Recombinant Collagen Contact Lens Lubricant
[0073] (1) Lubricity test:
[0074] The recombinant collagen contact lens lubricant and sodium hyaluronate contact lens lubricant were tested according to the test conditions (condition A) in "NB / SH / T0189-2017 Determination of Anti-wear Properties of Lubricating Oils - Four-ball Method".
[0075] Note: The samples were sent to an outsourced four-ball friction testing organization, Hangzhou Yanqu Information Technology Co., Ltd. The four-ball friction testing machine uses four steel balls arranged in an equilateral tetrahedral configuration. A hydraulic system applies load from bottom to top. During the test, the contact points of all four steel balls are immersed in lubricant. After the test, the wear mark diameter of each steel ball in the oil tank is measured until an evaluation index representing the lubricant's load-bearing capacity is determined. The test results are shown in Table 3.
[0076] Table 3. Lubricity results of recombinant collagen contact lens lubricant
[0077]
[0078] As shown in Table 3, the coefficient of friction and the diameter of the friction ball of the recombinant collagen contact lens lubricant are both smaller than those of the sodium hyaluronate contact lens lubricant (p<0.05). Therefore, the lubrication effect of the recombinant collagen contact lens lubricant is significantly better than that of the sodium hyaluronate contact lens lubricant.
[0079] (2) Moisturizing test:
[0080] S1. Weigh a certain amount of agar powder, prepare a 5wt% agar solution, heat to dissolve, pour into a petri dish, let it solidify, and weigh (W1).
[0081] S2. Spread 1 mL of 0.9% physiological saline, recombinant collagen contact lens lubricant and sodium hyaluronate contact lens lubricant evenly on a culture dish containing solid agar, weigh the mass (W2) using an analytical balance, and then place it in an oven at 37°C.
[0082] S3. After placing the petri dish in a constant temperature and humidity chamber at 25℃ and 40% relative humidity for 0h, 2h, 4h, 6h and 8h, remove the petri dish and weigh the mass (W3). Immediately after weighing, put the petri dish back into the constant temperature and humidity chamber.
[0083] S4. Calculate its moisturizing rate, and the results are shown in Table 4 and Figure 3.
[0084] Moisturizing rate (%) = (W2-W3) / (W2-W1)*100%
[0085] W1 is the weight of agar and petri dish (g), W2 is the weight of the sample and agar plus petri dish before the experiment (g), and W3 is the weight of the sample and agar plus petri dish after the specified time interval (g).
[0086] Table 4. Moisture retention rate of different lubricants
[0087]
[0088] As shown in Table 4 and Figure 3, the moisturizing rate of each component decreased significantly with the extension of drying time. However, when comparing different time periods, the moisturizing properties of recombinant collagen contact lens lubricant were significantly better than those of sodium hyaluronate contact lens lubricant and physiological saline (p<0.05).
[0089] In summary, recombinant collagen contact lens lubricant has good lubrication and moisturizing properties.
[0090] Example 7: Efficacy Study of Recombinant Collagen Contact Lens Lubricant
[0091] In this embodiment, physiological saline was used as the blank control group, sodium hyaluronate contact lens lubricant (purchased from Xindong Biotechnology Co., Ltd.) was used as the positive control group, and the recombinant collagen contact lens lubricant prepared in Example 1 was used as the experimental group. The effectiveness of the recombinant collagen contact lens lubricant of the present invention was investigated through animal experiments. The specific steps are as follows:
[0092] 12 healthy New Zealand white rabbits (half male and half female, weighing about 2.0-2.5kg, purchased from Hunan Taiping Biotechnology Co., Ltd., license number: SCXK(Xiang)2020-0005) were randomly divided into 3 groups, namely a blank control group, a positive control group and an experimental group, with 4 rabbits in each group.
[0093] New Zealand white rabbits were acclimatized for 7 days, and after confirming that there was no inflammatory reaction or other lesions in their eyes, rabbit corneal injury models were prepared. The specific preparation steps are as follows: New Zealand white rabbits were anesthetized by intraperitoneal injection of sodium pentobarbital, and 0.4% oxybuprocaine hydrochloride eye drops (Santen) were instilled into the right eye twice for corneal surface anesthesia. Then, an 8mm corneal trephine was used to make a circular cut on the right cornea, an 8mm corneal trephine was used to make a scratch, the epithelium in the corneal injury area was carefully removed with microscopic forceps and fine ophthalmic scissors, and lincomycin hydrochloride eye drops (Wuhan Wujing) were applied to the eye for 3 days. The left eye of the rabbit was also subjected to the same anesthesia and lincomycin hydrochloride eye drop application operations to obtain the rabbit corneal injury model.
[0094] Administration method: The New Zealand white rabbits with the above rabbit corneal injury models were treated with normal saline, sodium hyaluronate contact lens lubricating solution and recombinant collagen contact lens lubricating solution respectively, 2 drops at a time, three times a day, for 13 consecutive days of treatment. Observations were carried out on the 1st, 3rd, 5th, 7th, 9th, 11th and 13th days of treatment, and corneal sign scoring and corneal epithelial injury area measurement were performed.
[0095] The grading score table is shown in Table 5, and the corneal sign scoring results are shown in Figure 4.
[0096] Table 5. Grading Score Table
[0097]
[0098] It can be seen from Figure 4 that there was no significant difference in the scores of the normal saline group in the first 5 days of administration, but the score decreased on the 7th day of administration; the scores of the sodium hyaluronate contact lens lubricating solution group showed no difference in the first 3 days of administration, and decreased significantly on the 5th day (p<0.05) and the 7th day (p<0.01). The recombinant collagen contact lens lubricating solution group had no significant difference in scores in the first 3 days of administration, while the score increased on the 5th day of administration (p<0.05), and the score decreased significantly on the 7th day of administration (p<0.05). In summary, the recombinant collagen contact lens lubricating solution has a better repair effect on corneal injury than the sodium hyaluronate contact lens lubricating solution and normal saline.
[0099] This example also investigated the corneal healing rate after treatment with normal saline, sodium hyaluronate contact lens lubricating solution and recombinant collagen contact lens lubricating solution, and the investigation results are shown in Table 6 and Figure 5.
[0100] Table 6. Corneal Healing Rate of Different Lubricating Solutions
[0101]
[0102] As shown in Table 6 and Figure 5, the corneal injury healing rates of both the sodium hyaluronate contact lens lubricant and the recombinant collagen contact lens lubricant groups increased during the drug administration period, and the healing rates of each group were basically consistent with each other, with no significant difference. In conclusion, the effects of sodium hyaluronate contact lens lubricant and recombinant collagen contact lens lubricant on the healing of corneal injuries in rabbits were comparable, and both were superior to the saline group (p<0.05).
[0103] In this embodiment, after the treatment cycle was completed, corneal tissue was taken, embedded in paraffin, sectioned, and the morphological changes of corneal tissue were observed under a light microscope after HE and Masson staining. The staining results are shown in Figures 6 and 7.
[0104] As shown in Figure 6, the corneal tissue structure of the recombinant collagen contact lens lubricant group was normal, with inflammatory cell infiltration in the stroma and capillary congestion in some samples. In the sodium hyaluronate contact lens lubricant group, some samples showed only a small amount of inflammatory cell infiltration, while others exhibited corneal tissue disarray, epithelial cell edema, and capillary congestion. In the saline group, corneal epithelial cell edema, stroma disorganization, and extensive inflammatory cell infiltration were observed. Therefore, both recombinant collagen and sodium hyaluronate contact lens lubricants have a certain degree of effect on corneal structure recovery.
[0105] As shown in Figure 7, compared with the saline group, the collagen fiber area of each drug group showed a decreasing trend, indicating that each drug has a certain effect on the treatment of corneal damage, but there is no significant difference between them.
[0106] In conclusion, recombinant collagen contact lens lubricant is effective in promoting corneal damage healing.
[0107] Example 8: Stability Test
[0108] In this embodiment, the recombinant collagen contact lens lubricant prepared in Example 1 was placed in an environment of 40°C and 40% RH and tested at time points of 0, 1, 2, 3, 6 and 9 months. The test items and requirements are shown in Table 7, and the test results are shown in Table 8.
[0109] Table 7. Stability Testing Items and Requirements for Recombinant Collagen Contact Lens Lubricant
[0110]
[0111]
[0112] Table 8. Stability test results of recombinant collagen contact lens lubricant
[0113]
[0114] As shown in Table 8, the main active ingredient of the recombinant collagen contact lens lubricant, recombinant collagen, is not easily degraded under high-temperature accelerated conditions, and its content and purity remain stable. Other indicators are all within the quality control range, proving that this product has long-term stability.
[0115] In summary, the recombinant collagen contact lens lubricant of this invention can be safely and effectively used to moisturize and lubricate contact lenses, improve and relieve dry eyes, and enhance wearing comfort. In addition, the recombinant collagen contact lens lubricant can actively repair corneal and conjunctival damage and maintain long-term stability under normal temperature storage conditions, showing great market application prospects.
[0116] The embodiments described above are preferred embodiments of the present invention, but the present invention is not limited to the above embodiments. Any obvious improvements, substitutions or modifications that can be made by those skilled in the art without departing from the essence of the present invention shall fall within the protection scope of the present invention.
Claims
1. A recombinant collagen contact lens lubricant, characterized in that, The recombinant collagen contact lens lubricant comprises: recombinant collagen, sodium chloride, sodium dihydrogen phosphate, disodium hydrogen phosphate, polyvinyl alcohol, and water for injection.
2. The recombinant collagen contact lens lubricant according to claim 1, characterized in that, Each liter of recombinant collagen contact lens lubricant contains 2.5–10g of polyvinyl alcohol, 4.25–17g of sodium chloride, 0.03–0.12g of disodium hydrogen phosphate, 0.7–2.8g of sodium dihydrogen phosphate, and 20–80g of recombinant collagen, with the remainder being water for injection.
3. The recombinant collagen contact lens lubricant according to claim 2, characterized in that, Each liter of recombinant collagen contact lens lubricant contains 5g of polyvinyl alcohol, 8.5g of sodium chloride, 0.06g of disodium hydrogen phosphate, 1.4g of sodium dihydrogen phosphate, and 40g of recombinant collagen, with the remainder being water for injection.
4. The recombinant collagen contact lens lubricant according to claim 1, characterized in that, The recombinant collagen includes recombinant type III collagen, whose amino acid sequence is shown in SEQ ID NO:
1.
5. The recombinant collagen contact lens lubricant according to claim 1, characterized in that, The preparation method of the recombinant collagen contact lens lubricant includes: Polyvinyl alcohol, sodium chloride, disodium hydrogen phosphate and sodium dihydrogen phosphate are mixed, then water for injection is added and premixed under stirring conditions. Then recombinant collagen is added at room temperature, mixed evenly, filtered, filled and stored at room temperature.
6. The recombinant collagen contact lens lubricant according to claim 5, characterized in that, The premixing process involves stirring at 80°C and 300 rpm for 2–3 hours.
7. The recombinant collagen contact lens lubricant according to claim 5, characterized in that, The filtration process involves sequentially passing the material through 0.45μm and 0.22μm filter membranes.
8. The use of the recombinant collagen contact lens lubricant according to any one of claims 1 to 7 as a contact lens lubricant.
9. The application according to claim 8, characterized in that, The contact lenses include any one of soft contact lenses, rigid contact lenses, colored contact lenses, and silicone hydrogel contact lenses.