Solvent-resistant foaming material and preparation method thereof
Through the synergistic effect of base polymer and solvent-resistant modifier, combined with antioxidant and phased process, the problem of easy swelling and aging of rubber foam materials in solvent environment is solved, high solvent resistance, long-term anti-aging and stable foam structure are achieved, and the overall performance of the material is improved.
Patent Information
- Application Number
- CN202511330014.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-09-17
- Publication Date
- 2025-10-21
- Estimated Expiration
- 2045-09-17
AI Technical Summary
Traditional rubber foam materials are prone to swelling and deformation when exposed to organic solvents for a long time. Anti-aging agents are prone to migration and volatilization during high-temperature foaming, resulting in sealing failure, a sudden drop in mechanical properties, unstable foam structure, and shortened service life.
By adopting the synergistic effect of base polymer and fluorine-based solvent-resistant modifier, combined with molecular structure-optimized antioxidant and staged processing technology, a uniform closed-cell structure with high solvent resistance and long-term anti-aging is formed through specific raw material combinations and process steps.
Significantly improve the material's solvent resistance and aging resistance, maintain structural integrity, extend service life, and improve dynamic fatigue performance and cell wall strength.
Smart Images

Figure SMS_8 
Figure SMS_10 
Figure QLYQS_1
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of polymer compound rubber foam materials, and in particular to a solvent-resistant foam material and a preparation method thereof. Background Art
[0002] Foam materials, due to their lightweight, cushioning, and thermal insulation properties, are widely used in automotive seals, industrial gaskets, medical devices, and other fields. However, traditional rubber foam materials are prone to swelling, deformation, and even dissolution when exposed to organic solvents (such as lubricants and alcohols) for a long time, leading to seal failure and a sudden drop in mechanical properties. This has become a long-standing technical bottleneck in the industry, especially for seals exposed to oily environments.
[0003] At the same time, the aging problem of foam materials is equally prominent. Conventional antioxidants easily migrate and volatilize during the high-temperature foaming process, resulting in an incomplete anti-aging network within the material. The porous nature of the foam structure further accelerates the penetration of oxygen and ozone, causing chain breakage and cross-link failure. This manifests as surface powdering, hardening and brittle cracking, a sharp decline in dynamic fatigue performance, and a shortened service life.
[0004] Therefore, developing a high-performance material that has high solvent resistance, long-term anti-aging ability, and a stable foaming structure is crucial to improving the reliability and life of key sealing components. Summary of the Invention
[0005] The purpose of the present invention is to provide a solvent-resistant foaming material and a preparation method thereof. Through the synergistic effect of a specific base polymer and a fluorine-based solvent-resistant modifier, combined with an antioxidant with optimized molecular structure and a staged processing technology, the problems of existing foaming materials being easy to swell and deform in a solvent environment, failure of the antioxidant system during high-temperature foaming, and poor stability of the foam structure are solved, thereby achieving the unity of high solvent resistance, long-term anti-aging and uniform closed-cell structure.
[0006] To achieve the above object, the technical solution adopted by the present invention is: a solvent-resistant foaming material is prepared from the following raw materials in parts by weight: 90 parts of a base polymer, 5-25 parts of a chemical foaming agent, 0.5-5 parts of a cross-linking agent, 0.5-8 parts of a foaming aid, 5-40 parts of a filler, 10-30 parts of a solvent-resistant modifier, 0.5-5 parts of a processing aid, and 0.5-1.5 parts of an antioxidant; The antioxidant has a structure shown in Formula 1: The formula 1 is: ; R1 in Formula 1 is a substituent, and R1 is any one of hydrogen, methyl, hydroxy, fluorine, methyl ester, and alkoxy with 1 to 3 carbon atoms; The base polymer is selected from: a mixture of nitrile rubber and butadiene rubber in a mass ratio of 1:1; The solvent-resistant modifier is selected from at least one of polytetrafluoroethylene powder, perfluoropolyether, and chlorosulfonated polyethylene.
[0007] Furthermore, the chemical foaming agent is selected from at least one of azodicarbonamide, 4,4'-oxybisbenzenesulfonylhydrazide, p-toluenesulfonylhydrazide and p-toluenesulfonylsemicarbazide.
[0008] Furthermore, the cross-linking agent is selected from at least one of dicumyl peroxide and di-tert-butyl peroxyisopropylbenzene.
[0009] Furthermore, the foaming aid is selected from at least one of zinc oxide, stearic acid and urea.
[0010] Furthermore, the filler is selected from at least one of calcium carbonate, talc, white carbon black, carbon black, and diatomaceous earth.
[0011] Furthermore, the processing aid is selected from at least one of zinc stearate, paraffin wax, polyethylene wax, and silicone oil.
[0012] Furthermore, the antioxidant is selected from any one of the compounds shown in the following structures: ; ; ; .
[0013] A method for preparing a solvent-resistant foaming material comprises the following steps: (1) Banburying: adding the base polymer, filler, solvent resistance modifier, antioxidant and processing aid into a banbury mixer, and mixing at 120-150° C. for 3-8 minutes to obtain a mixture A; (2) Open mixing: the mixture A is transferred to an open mixing mill, cooled to 60° C.-80° C., the chemical foaming agent, cross-linking agent and foaming aid are added, and mixed uniformly to obtain a rubber compound; (3) Foaming molding: The rubber mixture is placed in a mold, foamed and kept warm at 160-190° C. and 5-15 MPa for 5-15 minutes, and then cooled and demolded to obtain a solvent-resistant foam material. Furthermore, the banburying in step (1) is carried out in two stages: The first stage: mixing the base polymer, filler and solvent-resistant modifier at 120-130° C. for 3-5 minutes; The second stage: adding the antioxidant and processing aid, raising the temperature to 140-150° C. and continuing mixing for 2-3 minutes.
[0014] Furthermore, the foaming molding in step (3) adopts a step-by-step heating program: first, the temperature is raised to 140-150°C at 5-8°C / min for pre-curing for 2-4 minutes; then the temperature is raised to 160-190°C at 3-5°C / min for foaming and heat preservation; and the cooling rate is controlled at 15-20°C / min.
[0015] The NH structure in the antioxidant possesses lone pairs of electrons, effectively capturing alkyl and alkoxy radicals generated during material aging, interrupting oxidation chain reactions. The fused conjugated system formed by the aromatic ring and heteroatoms (N and O) disperses and stabilizes the stable products generated by capturing free radicals, preventing them from initiating new oxidation reactions and enhancing the durability of anti-aging properties. The antioxidant also acts as a chelating agent to chelate residual metal ions (such as copper and iron) in the material, inhibiting metal-ion-catalyzed oxidation reactions and reducing accelerated aging caused by metal impurities.
[0016] The present invention improves solvent resistance through the synergistic effect of the base polymer combination (nitrile rubber and butadiene rubber in a 1:1 ratio) and the solvent resistance modifier: the polar cyanide group of the nitrile rubber resists swelling in non-polar solvents, the butadiene rubber compensates for elasticity, and the fluorine-based material migrates to the surface after dispersion in the mixing stage (120-150°C) to form a low surface energy barrier. Its highly electronegative fluorine element forms a physical cross-linking point with the polar group of the rubber, reducing the volume swelling rate in the solvent; long-term anti-aging is achieved through the synergistic effect of a special structure antioxidant and a peroxide cross-linking agent: the antioxidant is added to the second stage of mixing. The cross-linked network stabilizes its molecules, inhibiting aging through a triple mechanism of capturing free radicals, stabilizing free radical products, and chelating metal ions. Simultaneously, the cross-linker builds a stable network during the foaming stage (160-190°C), reducing chain breakage and increasing tensile strength retention. The cell structure is controlled through the synergistic combination of chemical blowing agents, fillers, and a step-by-step temperature ramping process: the filler is dispersed during the first stage of mixing to enhance cell wall strength, while the blowing agent uniformly decomposes and nucleates within the partially cross-linked matrix during the pre-curing stage at 140-150°C. The step-by-step temperature ramp aligns bubble growth with cross-linking rates, while rapid cooling locks the structure in place. This achieves a synergistic breakthrough in solvent resistance, aging resistance, and cell structure stability.
[0017] Compared with the prior art, the present invention has the following beneficial effects: 1. Significantly improved solvent resistance: This invention solves the problem of traditional foam materials being prone to swelling and deformation in organic solvent environments through the synergistic effect of the base polymer (nitrile rubber and butadiene rubber mixed in a 1:1 ratio) and a solvent-resistant modifier (such as polytetrafluoroethylene powder). This effectively reduces the volume swelling rate and mass change of the material in solvents, enhances its anti-penetration ability, and maintains its structural integrity when exposed to lubricating oils or alcoholic solvents for a long time, thereby extending the service life of the seal. 2. Enhanced long-term anti-aging capabilities: This invention utilizes a synergistic mechanism between a specifically structured antioxidant and a peroxide crosslinker to address the issue of antioxidant migration and volatilization during high-temperature foaming. This significantly slows the material's aging process, improving dynamic fatigue performance and tensile strength retention. The antioxidant forms a more durable anti-aging network through a triple mechanism of free radical capture, stabilization of free radical products, and chelation of metal ions.
[0018] 3. Improved Cell Structure Stability: This invention optimizes the bubble nucleation and growth process through the coordinated control of chemical foaming agents, fillers, and a stepped temperature ramp. This results in a more uniform and dense closed-cell structure, enhancing cell wall strength and overall material cushioning performance. Specifically, by matching bubble growth and crosslinking rates during the pre-curing stage, combined with rapid cooling and locking the structure, the material's dimensional stability and mechanical property consistency during the foaming process are improved. DETAILED DESCRIPTION
[0019] The following will clearly and completely describe the technical solution of the present invention in conjunction with the inventive content of the present invention. Obviously, the embodiments described are only some embodiments of the present invention, not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative efforts are within the scope of protection of the present invention.
[0020] Preparation Example 1 Preparation of antioxidant 1: ; 10 g of compound A and 8.50 g of compound B were dissolved in 120 ml of dichloromethane, stirred until uniformly dispersed, and then 14.43 g of 1-ethyl-(3-dimethylaminopropyl)carbodiimide hydrochloride and 6.14 g of 1-hydroxybenzotriazole were added. The mixture was reacted at 50 ° C for 9 hours, filtered through diatomaceous earth, and the filtrate was concentrated and dried. The filtrate was separated and purified by silica gel column chromatography using a mixed solution of n-heptane and petroleum ether as eluent, and 14.31 g of compound C was obtained after drying.
[0021] ; Under nitrogen, 14.31 g of compound C and 4.96 g of compound D were dissolved in 180 mL of a mixed solvent of 1,4-dioxane / diisopropylamine (120 mL / 60 mL). To this mixture were added 0.13 g of palladium acetate, 0.30 g of 2-dicyclohexylphosphino-2',4',6'-triisopropylbiphenyl, and 0.30 g of CuI. The mixture was reacted at 90°C for 5 h. After the reaction, the temperature was slightly lowered and the mixture was filtered through diatomaceous earth to remove salts and the catalyst. The reaction solution was concentrated and separated by silica gel column chromatography using a mixed solvent of n-heptane and ethyl acetate as the eluent. The mixture was then spin-dried to obtain 13.89 g of antioxidant 1.
[0022] Structure identification: Mass spectrum of compound C: 471, tested using M / Z MS+1; Mass spectrum of antioxidant 1: 571, tested using M / Z MS+1; NMR of antioxidant 1: 1 H NMR (Chloroform-d): δ 8.44 (d, 1H), 7.93 – 7.84 (m,2H), 7.72 (dd, 1H), 7.59 (dd, 1H), 7.53 – 7.39 (m, 7H), 7.39 – 7.27 (m, 4H), 7.17 (s, 2H).
[0023] Preparation Example 2-Preparation Example 6 In Preparation Examples 2 to 6, antioxidants were prepared by referring to the preparation method of Preparation Example 1, replacing Compound B therein, and remaining the same as in Preparation Example 1. For details, see Table 1.
[0024] Table 1.
[0025]
[0026] Example 1 Preparation of a solvent-resistant foaming material: 1. Raw material composition: Base polymer: 90 parts, made by mixing nitrile rubber and butadiene rubber in a mass ratio of 1:1. The nitrile rubber was purchased from Wuhan Xinyang Ruihe Chemical Technology Co., Ltd., and the butadiene rubber was purchased from Shanghai MacLean Biochemical Technology Co., Ltd. Chemical foaming agent: 15 parts, selected from: azodicarbonamide, purchased from: Xingyang No. 10 Chemical Co., Ltd.; Cross-linking agent: 2 parts, selected from: dicumyl peroxide, purchased from: Jiangsu Daoming Chemical Co., Ltd.; Foaming aid: 4 parts, selected from: zinc oxide, purchased from: Shanghai Aladdin Biochemical Technology Co., Ltd.; Filler: 20 parts, selected from: calcium carbonate, purchased from: Shanghai Nuocheng Pharmaceutical Co., Ltd.; Solvent resistance modifier: 20 parts, selected from: polytetrafluoroethylene powder, purchased from: Fuzhou Taipuda New Materials Co., Ltd.; Processing aid: 3 parts, selected from: zinc stearate, purchased from: Dongguan Hanwei Technology Co., Ltd.; Antiaging agent: 1 part, selected from: Antiaging agent 1, synthesized by the method of Preparation Example 1; 2. Preparation method: (1) Internal mixing: the base polymer (a mixture of nitrile rubber and butadiene rubber), filler (calcium carbonate) and solvent resistance modifier (polytetrafluoroethylene powder) were added to an internal mixer and mixed at 125°C for 4 minutes; the antioxidant (antioxidant 1) and processing aid (zinc stearate) were added, the temperature was raised to 145°C and the mixing was continued for 2.5 minutes to obtain mixture A; (2) Open mixing: Transfer the mixture A to an open mixing mill, cool it to 70°C, add the chemical foaming agent (azodicarbonamide), the cross-linking agent (diisopropylbenzene peroxide) and the foaming aid (zinc oxide), and mix them evenly to obtain a rubber mix; (3) Foaming molding: The rubber mixture is placed in a mold, and a pressure of 8 MPa is applied. The following procedures are followed: first, the temperature is raised to 145°C at a heating rate of 7°C / min, and pre-cured for 3 minutes; then, the temperature is raised to 175°C at a heating rate of 4°C / min, and foaming and heat preservation is performed for 10 minutes; then, the temperature is lowered to room temperature at a cooling rate of 18°C / min, and then demolded to obtain the solvent-resistant foaming material.
[0027] Example 2-Example 6 In Examples 2 to 6, a solvent-resistant foaming material was prepared in sequence. Referring to the preparation method of Example 1, the antioxidant was replaced with the antioxidant prepared in Preparation Examples 2 to 6, and the rest remained the same as in Example 1.
[0028] Comparative Example 1 A preparation method of a solvent-resistant foaming material, referring to the preparation method of Example 1, replacing the antioxidant with (antioxidant MC), and the rest remain the same as in Example 1.
[0029] Comparative Example 2 A solvent-resistant foaming material was prepared by referring to the preparation method of Example 1, except that the antioxidant was replaced with antioxidant AW, and the rest remained the same as Example 1.
[0030] Comparative Example 3 A solvent-resistant foaming material was prepared by referring to the preparation method of Example 1, except that the antioxidant was not added, and the rest of the preparation method remained the same as Example 1.
[0031] Comparative Example 4 A solvent-resistant foaming material was prepared by referring to the preparation method of Example 1, except that the polytetrafluoroethylene powder was not added, and the rest of the process remained the same as Example 1.
[0032] Performance testing: 1. Tensile Strength: Tensile strength was tested using a universal tensile testing machine according to the method specified in GB / T 528-2009. The tensile rate was 500 mm / min, the test temperature was 23°C, and the effective length of the specimen was 25 mm and the width was 6 mm. See Table 2 for the data.
[0033] 2. Solvent Resistance Test: Solvent resistance was tested according to the method specified in GB / T 1690-2010. The test conditions were 23°C for 48 hours. The test solvents included toluene and acetone. The rate of change in mass was recorded. The data is shown in Table 2.
[0034] 3. Anti-aging test: Refer to the method specified in GB / T 3512-2014, heat aging temperature is 100±2°C, heat aging time is 336 hours, and tensile strength retention (%) is tested. Data are shown in Table 2.
[0035] Table 2.
[0036]
[0037] The examples (using the specific antioxidant and solvent resistance modifier of the present invention) exhibit significant advantages in overall performance, including higher tensile strength, lower solvent absorption rate (as measured by the mass change of toluene and acetone), and excellent aging resistance (high tensile strength retention), demonstrating synergistic optimization of mechanical strength, solvent resistance, and long-term stability. In contrast, in the comparative examples: Comparative Examples 1 and 2, when using alternative antioxidants (such as MC or AW), exhibit significant degradation in aging resistance, highlighting the critical role of antioxidant structural design in long-term material protection. Comparative Example 3, which completely lacks an antioxidant, exhibits overall performance deterioration, particularly in aging resistance. Comparative Example 4, in which the solvent resistance modifier is omitted, exhibits significant degradation in solvent resistance, but relatively retained aging resistance, highlighting the crucial contribution of the solvent resistance modifier to solvent resistance. Overall, this trend confirms that the synergistic effect of the antioxidant and solvent resistance modifier of the present invention is the decisive factor in improving the material's overall performance.
[0038] While embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions, and variations may be made to these embodiments without departing from the principles and spirit of the invention, and that the scope of the invention is defined by the appended claims and their equivalents.
Claims
1. A solvent-resistant foaming material, characterized in that: The invention is prepared from the following raw materials in parts by weight: 90 parts of base polymer, 5-25 parts of chemical foaming agent, 0.5-5 parts of cross-linking agent, 0.5-8 parts of foaming aid, 5-40 parts of filler, 10-30 parts of solvent resistance modifier, 0.5-5 parts of processing aid, and 0.5-1.5 parts of antioxidant; The antioxidant has a structure shown in Formula 1; The formula 1 is: ; R1 in Formula 1 is a substituent, and R1 is any one of hydrogen, methyl, hydroxy, fluorine, methyl ester, and alkoxy with 1 to 3 carbon atoms; The base polymer is selected from: a mixture of nitrile rubber and butadiene rubber in a mass ratio of 1:1; The solvent-resistant modifier is selected from at least one of polytetrafluoroethylene powder, perfluoropolyether, and chlorosulfonated polyethylene.
2. A solvent-resistant foam material according to claim 1, characterized in that: The chemical foaming agent is selected from at least one of azodicarbonamide, 4,4'-oxybisbenzenesulfonylhydrazide, p-toluenesulfonylhydrazide and p-toluenesulfonylsemicarbazide.
3. The solvent-resistant foaming material according to claim 1, characterized in that: The cross-linking agent is selected from at least one of dicumyl peroxide and di-tert-butyl peroxycumene.
4. The solvent-resistant foaming material according to claim 1, characterized in that: The foaming aid is selected from at least one of zinc oxide, stearic acid and urea.
5. The solvent-resistant foaming material according to claim 1, characterized in that: The filler is selected from at least one of calcium carbonate, talc, white carbon black, carbon black, and diatomaceous earth.
6. The solvent-resistant foaming material according to claim 1, characterized in that: The processing aid is selected from at least one of zinc stearate, paraffin wax, polyethylene wax and silicone oil.
7. The solvent-resistant foaming material according to claim 1, characterized in that: The antioxidant is selected from any one of the compounds shown in the following structures: ; ; ; 。 8. A method for preparing a solvent-resistant foaming material according to any one of claims 1 to 7, characterized in that: The following steps are involved: (1) Banburying: adding the base polymer, filler, solvent resistance modifier, antioxidant and processing aid into a banbury mixer, and mixing at 120-150° C. for 3-8 minutes to obtain a mixture A; (2) Open mixing: the mixture A is transferred to an open mixing mill, cooled to 60° C.-80° C., the chemical foaming agent, cross-linking agent and foaming aid are added, and mixed uniformly to obtain a rubber compound; (3) Foaming molding: The rubber mixture is placed in a mold, foamed and kept warm at 160-190° C. and 5-15 MPa for 5-15 minutes, and then cooled and demolded to obtain a solvent-resistant foam material.
9. The method for preparing a solvent-resistant foaming material according to claim 8, characterized in that: In the step (1), the refining is carried out in two stages: The first stage: mixing the base polymer, filler and solvent-resistant modifier at 120-130° C. for 3-5 minutes; The second stage: adding the antioxidant and processing aid, raising the temperature to 140-150° C. and continuing mixing for 2-3 minutes.
10. The method for preparing a solvent-resistant foaming material according to claim 8, characterized in that: The foaming molding in step (3) adopts a step-by-step heating program: first, the temperature is raised to 140-150°C at 5-8°C / min for pre-curing for 2-4 minutes; then the temperature is raised to 160-190°C at 3-5°C / min for foaming and curing; the cooling rate is controlled at 15-20°C / min.
Citation Information
Patent Citations
Composite low temperature resistant and oil resistant rubber seal material and preparation method thereof
CN105885130A
Preparation method and application of oil-water non-slip rubber material
CN112778588A
Composite foaming material and preparation method thereof
CN118440414A
Medium-resistant high-elasticity rubber material for sealing element and preparation method of medium-resistant high-elasticity rubber material
CN118725430A
Nitrile rubber composition and cross-linked rubber
US20180057628A1
Cited By
Micro-foaming silicone rubber battery cell buffering strip-shaped material and preparation process thereof
CN121022113A
Ultraviolet aging resistant color master batch and preparation method thereof
CN121182071A
Uv-aging resistant color master batch and preparation method thereof
CN121182071B
Highly oil-resistant PVC protective gloves with thickened cuffs and preparation method of highly oil-resistant PVC protective gloves
CN121319524A