Consumable product for heat-not-burn aerosol product and preparation method and application thereof
By spirally winding multiple layers of material to form a cylindrical structure, the problem of high equipment cost and low production efficiency of traditional heated non-combustible aerosol products is solved. This achieves strength and heating uniformity of consumables, improving industrial production efficiency and user suction experience.
Patent Information
- Application Number
- CN202410871810.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-01
- Publication Date
- 2026-01-06
AI Technical Summary
Traditional heated non-combustible aerosol products require expensive equipment, have complex processes, and low production efficiency. Furthermore, the consumable materials used in aerosol generation have low structural strength, leading to uneven heating and unstable absorption resistance.
A cylindrical structure is formed by spirally winding multiple layers of material, with no overlap between the layers. Hollow holes and butt joints are designed, and food-grade plant polysaccharides are used as adhesives to simplify the preparation process.
It improves the strength and production efficiency of consumables, ensures uniform heating and aerosol overflow, stabilizes suction resistance, simplifies the production process, and is suitable for large-scale industrial production.
Smart Images

Figure CN121264685A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of tobacco product technology, and more specifically, to a consumable for heated non-combustible aerosol products, its preparation method, and its application. Background Technology
[0002] Tobacco is an important economic crop, and tobacco products such as cigarettes and heated tobacco products have a wide consumer market worldwide. In the manufacturing process of tobacco products, the smoke-generating material is one of the key factors characterizing the quality of tobacco products, determining their flavor, draw resistance, and other characteristics. Therefore, the preparation of the smoke-generating material is crucial for providing a richer and / or easier smoking experience.
[0003] Currently, the traditional preparation of heated tobacco aerosol products mainly involves two steps: shredding and compounding into rods. First, the tobacco raw material is shredded. Then, using compounding technology, the shredded tobacco raw material, cooling elements, and filter tips are combined together, and finally, the product is cut into segments to obtain the finished heated tobacco aerosol product. However, shredding equipment is expensive, requires many pieces of equipment, involves complex processes, and is slow, making it unsuitable for large-scale production. Other new aerosol generation consumables suffer from problems such as low structural strength and low production efficiency.
[0004] In view of this, the present invention is proposed. Summary of the Invention
[0005] The purpose of this invention is to provide a consumable for heated non-combustible aerosol products, its preparation method, and its application, which can improve the strength of the consumable for heated non-combustible aerosol products and increase the production efficiency of the consumable.
[0006] The embodiments of the present invention are implemented as follows:
[0007] In a first aspect, the present invention provides a consumable for heating non-combustible aerosol products, comprising at least two layers of roll-to-roll material, the roll-to-roll material having a sheet structure, and the roll-to-roll material comprising at least an aerosol generating sheet.
[0008] When the same layer of spiral material is wound, the edges of adjacent spirals do not overlap. Multiple layers of spiral material are spirally wound and overlap each other to form a cylindrical structure with hollow holes. The width of each layer of spiral material satisfies the following formula:
[0009]
[0010] Where b represents the width of the coiled material, n represents the number of layers of the coiled material from the inside out, R0 represents the diameter of the hollow hole, d represents the thickness of the coiled material, and α represents the tilt angle of the coiled material.
[0011] Optionally, the tilt angle α of the rolled material is 25° to 80°.
[0012] Preferably, the ratio of the diameter of the hollow hole to the width of the rolled material is 0.1 to 0.7.
[0013] Optionally, after the outermost layer of spiral material is wound, the adjacent edges of the spirals contact but do not overlap, and after the next outermost layer of spiral material is wound, a butt joint is formed between the adjacent edges of the spirals.
[0014] Preferably, the gap between the butt joints is less than 1.1 mm.
[0015] Preferably, the outermost layer of roll material covers the joint of the adjacent second outermost layer of roll material.
[0016] Preferably, the centerline region of the outermost layer of roll material covers the joint of the adjacent second outermost layer of roll material.
[0017] Optionally, the consumable with a cylindrical structure has 2 to 8 layers in its cross-section, preferably 3 to 4 layers.
[0018] Preferably, the outer diameter of the consumable is 7.1 mm ± 10% or 5.3 mm ± 10%.
[0019] Preferably, the diameter of the hollow hole in the consumable is greater than 1.5 mm; more preferably, the diameter of the hollow hole in the consumable is 1.5 mm to 4 mm.
[0020] Preferably, the length of the consumable is 7mm to 84mm.
[0021] Alternatively, the roll material may also include at least one of filler paper, fragrance paper, and metal foil.
[0022] Preferably, the aerosol-generated sheet is reconstituted tobacco paper, and the raw materials for reconstituted tobacco paper include at least one of papermaking reconstituted tobacco, slurry reconstituted tobacco, dry reconstituted tobacco, and roll-pressed reconstituted tobacco.
[0023] Secondly, the present invention provides a method for preparing a consumable as described in any of the foregoing embodiments, comprising coaxially spirally winding a multi-layered spiral material into a hollow cylindrical shape, and then cutting and drying the wound material after fixing it.
[0024] Optionally, the winding and fixing includes: synchronously spirally winding multiple layers of rolled material from the inside to the outside along the same central axis.
[0025] Preferably, the inner side of the outer layer of the roll material is coated with an adhesive to bond the outer layer of the roll material to the inner layer of the roll material.
[0026] Preferably, the preparation of the adhesive includes dissolving food-grade plant polysaccharides in a solution to obtain a viscous liquid.
[0027] Preferably, the concentration of food-grade plant polysaccharides in the binder is 1% to 10%.
[0028] Preferably, the food-grade plant polysaccharide includes any one of guar gum, starch, carboxymethyl cellulose, carboxymethyl starch, xanthan gum, and sodium alginate.
[0029] Preferably, the method of coating the roll material with the adhesive includes at least one of dip coating or transfer coating.
[0030] Preferably, the drying temperature is 60℃~90℃.
[0031] Thirdly, the present invention provides a heat-not-burn aerosol product, comprising an outer packaging paper, wherein a filter section and a smoke-generating section are sequentially disposed within the outer packaging paper, and the smoke-generating section is a consumable as described in any of the foregoing embodiments or a consumable prepared by the preparation method described in the foregoing embodiments.
[0032] Optionally, the heating method for heating non-combustible aerosol products includes electromagnetic heating or contact heating.
[0033] Optionally, a cooling section may also be included between the filtration section and the smoke generation section.
[0034] Fourthly, the present invention provides the use of a consumable as described in any of the foregoing embodiments or a consumable prepared by the preparation method described in the foregoing embodiments in the preparation of tobacco products.
[0035] The beneficial effects of the embodiments of the present invention are:
[0036] This invention provides a consumable for heated non-combustible aerosol products, its preparation method, and its application. The consumable has a spirally wound structure, and the edges of adjacent spirals do not overlap after the same layer of winding material is wound, ensuring that the number of layers in the cross-section of the consumable is the same everywhere, thus guaranteeing uniformity throughout the consumable. This structure not only significantly improves the strength of the consumable but also ensures uniform heating throughout, resulting in uniform aerosol overflow after heating, further guaranteeing the stability of suction resistance. The hollow interior of the wound structure serves as an airflow channel, ensuring the stability of suction resistance. Furthermore, the winding material includes at least an aerosol generating sheet. When the aerosol generating sheet is heated, it generates aerosol, which overflows through the seams of each layer of winding material and then into the airflow channel in the middle of the consumable, improving the user's suction experience. Furthermore, by controlling the number and thickness of the coiled material, the diameter of the hollow holes, and the tilt angle of the coiled material during the coiling process, the width of the coiled material can be calculated. Calculating a suitable width using this formula can make the consumables more efficient in the manufacturing process, reduce the risk of overlapping edges between the same layers during winding, and reduce the number of winding turns, which is conducive to achieving large-scale industrial production. Attached Figure Description
[0037] To more clearly illustrate the technical solutions of the embodiments of the present invention, the accompanying drawings used in the embodiments will be briefly introduced below. It should be understood that the following drawings only show some embodiments of the present invention and should not be regarded as a limitation on the scope. For those skilled in the art, other related drawings can be obtained based on these drawings without creative effort.
[0038] Figure 1 A schematic diagram of the structure of a consumable provided in an embodiment of the present invention;
[0039] Figure 2 This is a schematic diagram of the spiral winding of the coiled material provided in an embodiment of the present invention;
[0040] Figure 3 This is a schematic diagram of the consumable winding process provided in an embodiment of the present invention;
[0041] Figure 4 A top view of a consumable provided in an embodiment of the present invention;
[0042] Figure 5 This is a schematic diagram of the consumable winding process provided in an embodiment of the present invention;
[0043] Figure 6 This is a cross-sectional view of the heat-not-combustible aerosol product provided in Embodiment 6 of the present invention;
[0044] Figure 7 This is a cross-sectional view of the heat-not-burning aerosol product provided in Embodiment 7 of the present invention.
[0045] Icons: 100 - Consumables; 110 - Splicing material; 111 - Butt joint; 112 - Airflow channel; 113 - First long side; 114 - Second long side; 115 - Width; 116 - Inner layer splicing material; 117 - Second outer layer splicing material; 118 - Outermost layer splicing material; 10 - Heated non-combustible aerosol products; 200 - Filter section; 300 - Cooling section; 400 - Outer packaging paper. Detailed Implementation
[0046] To make the objectives, technical solutions, and advantages of the embodiments of the present invention clearer, the technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. The components of the embodiments of the present invention described and shown in the accompanying drawings can generally be arranged and designed in various different configurations.
[0047] Please refer to Figure 1 and Figure 2In a first aspect, the present invention provides a consumable 100 for heating non-combustible aerosol products, comprising at least two layers of splicing material 110, wherein the splicing material 110 is a sheet structure, and the splicing material 110 comprises at least an aerosol generating sheet.
[0048] Each layer of the spiral material 110 has the same tilt angle, and the adjacent edges of the spiral after the same layer of spiral material 110 is wound do not overlap. Multiple layers of spiral material 110 are spirally wound and overlap each other to form a cylindrical structure with hollow holes. The hollow holes inside the consumable 100 are the airflow channels 112.
[0049] It should be noted that the consumable 100 used in the heated non-combustible aerosol product is a smoke-generating material of the heated non-combustible aerosol product 10. By heating the consumable 100, the coiling material 110 in the consumable 100 will evaporate and generate aerogel, providing users with a suction experience.
[0050] The width of each layer of roll material 110 satisfies the following formula:
[0051]
[0052] Where b represents the width 115 of the coiled material 110, in mm; n represents the number of layers of the coiled material 110 from the inside out; R0 represents the diameter of the hollow hole, in mm; d represents the thickness of the coiled material 110, in mm; and α represents the tilt angle of the coiled material 110, in °.
[0053] Therefore, it is understandable that b n That is, the width 115 of the nth layer of the roll material 110 counted from the inside out.
[0054] Because there is a certain relationship between the width 115 and the tilt angle α of the winding material 110, assuming the tilt angle of the winding material 110 is the same, the narrower the width 115, the longer the length of the winding material 110 required to wind the same length of consumable 100, and the more turns are needed. Therefore, it is necessary to control the relationship between the width 115 and the tilt angle of the winding material 110 to avoid multiple windings during the production of consumable 100, which would reduce production efficiency. Furthermore, multiple windings also increase the probability of overlap between edges, making it difficult to control the quality of consumable 100.
[0055] Furthermore, in order to ensure that the edge area formed after the winding material 110 is wound does not overlap with the winding material 110, it is also necessary to consider the influence of the hollow hole based on the parameters of the winding material 110. Therefore, the tilt angle of the winding material 110 during the winding process needs to be determined by both the parameters of the winding material 110 and the parameters of the hollow hole.
[0056] In an optional embodiment, after the outermost layer of spiral material 118 is wound, the adjacent spiral edges contact each other but do not overlap. After the next outermost layer of spiral material 110 is wound, a butt joint 111 is formed between its adjacent spiral edges to ensure that the number of layers in the cross-section of the consumable 100 is the same everywhere. The purpose of providing the butt joint 111 in the inner layer is to facilitate the overflow of aerosols. However, the outermost layer needs to ensure that the overall strength of the consumable 100 meets the requirements. Therefore, it is not necessary to deliberately leave a butt joint 111 of a certain width. It is sufficient to ensure that the two adjacent edges contact each other but do not overlap after winding. The meaning of contacting but not overlapping is that the two adjacent edges of the outermost layer of spiral material 110 have a very small gap after winding, which can be ignored.
[0057] Among them, the roll-to-roll material 110 includes at least an aerosol-generated sheet.
[0058] It is understandable that, in order to form the aforementioned consumable 100, a single sheet of winding material 110 can be wound to form one layer of the consumable 100. Therefore, the number of layers in the consumable 100 is the same as the number of sheets of winding material 110. When the consumable 100 has a structure of three or more layers, the layers are arranged sequentially from the outermost layer to the innermost layer: the first layer, the second layer, the third layer, and so on. The first layer is the outermost layer, the second layer is the second outermost layer, and the third layer and subsequent layers are collectively referred to as inner layers.
[0059] Please refer to Figure 2 and Figure 3 Taking one layer of consumable 100 wrapped with a roll of material 110 as an example, the roll of material 110 is a rectangular or strip-shaped sheet structure with a width of 115. The two long sides perpendicular to the width of 115 are the first long side 113 and the second long side 114, which are the edge portions.
[0060] When the spiral material 110 is spirally wound to form the consumable 100, the width 115 of the spiral material 110 is wound at an angle to the central axis. The first long side 113 will first spirally wound to form a curved surface. After one turn, the second long side 114 will be wound to be parallel to the first long side 113 everywhere. The first long side 113 and the second long side 114 do not overlap each other, and there is a butt joint 111 between the first long side 113 and the second long side 114. The number of cross-sectional layers of the consumable 100 obtained by winding in the above manner is the same everywhere. It can be understood that the cross-section here refers to the cross-section perpendicular to the axis of the consumable 100.
[0061] Furthermore, the consumable 100 provided by the present invention uses a winding material 110 that includes at least an aerosol generating sheet. The aerosol generating sheet is a sheet-like structure made of a material with smoke-generating ability, generally made from various recycled tobacco leaves, and is in the form of thin paper. When heated, the aroma components of tobacco will volatilize and generate aerosols. These aerosols will overflow along the joint seams 111 of each layer of the consumable 100. The hollow consumable 100 forms an airflow channel 112 in its internal cavity, which is beneficial to the user's smoking experience. Furthermore, since the aerosol generating sheet is evenly distributed during the winding process and the number of layers in the cross-section of the consumable 100 is equal everywhere, the consumable 100 can be heated evenly, further ensuring the stability of the draw resistance.
[0062] In an optional embodiment, the aerosol-generating sheet is recycled tobacco paper, and the raw materials for the recycled tobacco paper include at least one of paper-processed recycled tobacco, slurry-processed recycled tobacco, dry-processed recycled tobacco, and roll-pressed recycled tobacco. The above are only some examples of the sources of the aerosol-generating sheet. In practical applications, the aerosol-generating sheet can be paper made from tobacco materials capable of producing tobacco aroma and smoking experience, obtained by any existing method.
[0063] Since aerosol generating sheets are one of the materials that provide the necessary suction experience for consumable 100, the roll-to-roll material 110 provided by the present invention includes at least aerosol generating sheets. However, in order to adapt to various heating devices and the suction experience of various groups of people, the roll-to-roll material 110 in consumable 100 provided by the present invention also includes at least one of filling paper, fragrance paper and metal foil.
[0064] The filler paper can be any food-grade ordinary paper, and its function is to be wound as a filler or diluent material to form a hollow consumable 100. For example, assuming a conventional consumable 100 is formed by winding four layers of aerosol-generating sheets with a conventional tobacco concentration, when a consumable 100 with a lower tobacco concentration needs to be prepared, one or two layers of aerosol-generating sheets can be replaced with filler paper. Alternatively, if the selected aerosol-generating sheet has a high tobacco concentration, using all four layers of aerosol-generating sheets would result in a high tobacco concentration in the consumable 100; therefore, one layer of aerosol-generating sheet can be replaced with filler paper. Whether or not filler paper needs to be added and the amount of filler paper can be designed according to the actual vaping requirements.
[0065] Flavored paper is a tobacco product with a special aroma. It can be made by combining tobacco with other flavoring ingredients or by using non-tobacco ingredients alone. It can give consumable 100 a richer smoking experience. Therefore, depending on the design requirements of the product, one or more layers of consumable 100 can be designed as flavored paper.
[0066] By incorporating one or more layers of metal foil into the consumable 100, typically one layer, the consumable 100 containing the aforementioned metal foil can be adapted to a wider variety of heating devices. For example, the consumable 100 with metal foil can be heated not only by heat transfer but also by electromagnetic heating, thus adapting to heating devices with various heating methods.
[0067] In an optional embodiment, the tilt angle α of the coiled material 110 is 25° to 80°, which is the angle between the tangent of the butt joint 111 and the central axis O of the cylindrical consumable 100. It can also be understood that during the winding process, one end of the coiled material 110 that has not yet been wound needs to be tightened before the winding is completed. Therefore, the angle β between the tightened end of the coiled material 110 that has not yet been wound and the axis of the consumable 100 is 25° to 80°.
[0068] Wherein, the tangent of the butt joint 111 and the central axis of the consumable 100 are located in two planes. Therefore, the included angle α here is the included angle when the two are translated into the same plane and intersect. The included angle α is 25° to 80°, for example, it can be any value among 25°, 30°, 35°, 40°, 45°, 50°, 55°, 60°, 65°, 70°, 75° or 80°, or any range value and point value between any two values.
[0069] Preferably, the ratio of the diameter of the hollow hole to the width 115 of the coiled material 110 is 0.1 to 0.7. That is, the diameter of the hollow hole is smaller than the width 115 of the coiled material 110, so as to reduce the number of winding turns and improve the production efficiency of the consumable 100.
[0070] In some preferred embodiments, the ratio of the diameter of the hollow hole to the width 115 of the roll material 110 can be any value among 0.1, 0.2, 0.3, 0.4, 0.5, 0.6 or 0.7, or a range or point value between any two values.
[0071] In an optional implementation, to ensure uniform aerosol overflow and avoid uneven thickness of the consumable 100, the gap between the butt joints 111 satisfies the condition 0 mm < butt joint 111 < 1.1 mm. For example, the gap between the butt joints 111 can be any value from 1 mm, 0.9 mm, 0.8 mm, 0.7 mm, 0.6 mm, 0.5 mm, 0.4 mm, 0.3 mm, 0.2 mm, or 0.1 mm, or any range or point value between any two values. It should be noted that the multi-layered rolled material 110 in the consumable 100 must not overlap within each layer to ensure uniform heating of the consumable 100. The outermost rolled material 110 does not need to have intentionally wide butt joints 111; the first long side 113 and the second long side 114 can be kept adjacent to each other to better control the strength of the consumable 100. In addition to the outermost layer, all the inner layers of rolled material 110 need to have a relatively wide gap during the winding process to facilitate the overflow of aerosol, namely the aforementioned butt joint 111.
[0072] Please refer to Figure 5 In order to prevent the aerosol from overflowing too quickly and to improve the mechanical strength of the consumable 100 and prevent it from bending easily, preferably, the outermost layer of the roll material 110 covers the butt joint 111 of the adjacent inner layer of the roll material 110.
[0073] For example, a consumable 100 has a three-layer structure, consisting of an outermost layer of roll material 118, a second outermost layer of roll material 117, and an innermost layer of roll material 116, from the outside in. If the seams 111 of the three roll materials 110 completely overlap, the aerosol will overflow directly and rapidly from the seams 111 into the airflow channel 112, resulting in excessively fast overflow. Furthermore, this would lead to insufficient mechanical strength in the consumable 100, making it prone to bending. Therefore, the preferred solution is to cover the seam 111 of the second outermost layer of roll material 117 with the outermost layer of roll material 118. Whether the seams 111 of the innermost layer of roll material 116 and the second outermost layer of roll material 117 overlap can be determined as needed.
[0074] For example in Figure 5 In the middle, the butt joint 111 of the inner layer and the second outer layer of the roll material 117 overlaps, while the outermost roll material 118 covers the butt joint 111 of the second outer layer of the roll material 117.
[0075] Preferably, in order to further ensure the coverage of the butt joint 111 of the outermost layer of the roll material 118 over the second outermost layer of the roll material 117, the centerline region of the outermost layer of the roll material 118 covers the butt joint 111 of the second outermost layer of the roll material 117.
[0076] Among them, the centerline of the outermost layer of roll material 118 in the axial direction refers to the centerline that is parallel to the first long side 113 and the second long side 114 of the roll material 110, and whose endpoints bisect the width 115.
[0077] Please refer to Figure 3 and Figure 4 In order to further improve the mechanical strength of the product, more preferably, the seam 111 of the roll material 118 from the innermost layer to the outermost layer is covered by the roll material 110 of the adjacent inner layer.
[0078] Among them, the innermost layer of the roll material 110 refers to the roll material 110 located outside the innermost layer of the roll material 110.
[0079] For example, a consumable 100 has a three-layer structure, consisting of an outermost layer of roll material 118, a second outermost layer of roll material 117, and an innermost layer of roll material 116, from the outside to the inside. The second outermost layer of roll material 117 covers the butt joint 111 of the innermost layer of roll material 116, and the outermost layer of roll material 118 covers the butt joint 111 of the second outermost layer of roll material 117.
[0080] Preferably, in order to ensure that each layer other than the inner layer covers the joint 111 of the adjacent inner layer, the centerline region of the roll material 110 from the second inner layer to the outermost layer coincides with the joint 111 of the roll material 110 of the adjacent inner layer.
[0081] The axial centerline of the roll material 110 from the innermost layer to the outermost layer refers to the centerline that is parallel to the first long side 113 and the second long side 114 of the roll material 110 and whose endpoints bisect the width 115.
[0082] Furthermore, since the outer layer of the winding material 110 needs to cover the butt joint 111 formed by the adjacent inner layer of the winding material 110 during the winding process, it is inevitable that the number of cross-sectional layers at the left and right ends of the consumable 100 will not be consistent when the winding is just completed. This part of the consumable 100 needs to be cut and discarded in actual use. Moreover, the consumable 100 formed in one batch is relatively long, and it also needs to be cut into a suitable length before use in actual use.
[0083] In an optional embodiment, the consumable 100 with a cylindrical structure has 2 to 8 layers in its cross-section, preferably 3 to 4 layers. The number of layers in the cross-section of the consumable 100 can be set as needed, and the material of the roll-up material 110 for each layer can also be specifically selected as needed.
[0084] Preferably, the outer diameter of the consumable 100 is 7.1 mm ± 10% or 5.3 mm ± 10%.
[0085] Preferably, to ensure the width of the gas channel while ensuring that the outer diameter of the consumable 100 meets the requirements, the diameter of the hollow hole of the consumable 100 is greater than 1.5 mm. More preferably, the diameter of the hollow hole of the consumable 100 is 1.5 mm to 4 mm, for example, the diameter of the hollow hole of the consumable 100 is any value among 1.5 mm, 2 mm, 2.5 mm, 3 mm, 3.5 mm or 4 mm, or any range or point value between any two values.
[0086] The consumable 100 for heating non-combustible aerosol products formed by winding is a long, hollow cylindrical structure that needs to be cut into fixed lengths. Preferably, the length of the cut consumable 100 is 7mm to 84mm. For example, the inner diameter of the consumable 100 is any value among 7mm, 12mm, 20mm, 30mm, 40mm, 50mm, 60mm, 75mm or 84mm, or any range or point value between any two values.
[0087] Among them, compressive strength refers to the compressive strength along the cross-sectional direction of the tube of consumable 100; elastic modulus refers to the Young's elastic modulus along the cross-sectional direction of consumable 100.
[0088] Secondly, the present invention provides a method for preparing a consumable 100 as described in any of the foregoing embodiments, comprising coaxially spirally winding a multilayer spiral material 110 into a hollow cylindrical shape, and then cutting and drying the wound material after fixing it.
[0089] The winding method is preferably suited to meet the structure of the consumable 100 as described in any of the foregoing embodiments.
[0090] In an optional embodiment, the winding fixation includes: synchronously spirally winding multiple layers of coiled material 110 from the inside to the outside along the same central axis. For example, after the first layer of coiled material 110 is wound twice, the second layer of coiled material 110 is started to be wound, and this winding speed is maintained to synchronously wind until the end.
[0091] Preferably, the inner side of the outer layer of winding material 110 is coated with adhesive to bond the outer layer of winding material 110 to the inner layer of winding material 110. Therefore, it can be understood that the innermost layer, that is, the first winding material 110 used for winding, does not need to be coated with adhesive. Starting from the second layer, each winding material 110 needs to be coated with adhesive on one side, and then the side coated with adhesive is used as the side that contacts the inner layer of winding material 110 to ensure the structural stability of the consumable 100.
[0092] Preferably, the adhesive is prepared by dissolving food-grade plant polysaccharides in a solution to obtain a viscous liquid. The solution can be water or other food-grade materials that can dissolve the food-grade plant polysaccharides.
[0093] Preferably, the concentration of food-grade plant polysaccharides in the adhesive is 1% to 10%, for example, it can be any value among 1%, 2%, 3%, 4%, 5%, 6%, 7%, 8%, 9% or 10%, or any range or point value between any two values.
[0094] Preferably, the food-grade plant polysaccharide includes any one of guar gum, starch, carboxymethyl cellulose, carboxymethyl starch, xanthan gum, and sodium alginate.
[0095] Preferably, the method of coating the roll material 110 with the adhesive includes at least one of dip coating or transfer coating. Dip coating involves immersing one side of the roll material 110 in the adhesive to adhere it; transfer coating refers to a method of transferring the adhesive to the paper surface using the rotation of a roller.
[0096] Preferably, since each sheet of roll material 110 is coated with adhesive starting from the second layer, the resulting consumable 100 has a certain humidity and needs to be dried. The drying method can be a conventional drying method, such as hot air drying or oven drying, and the drying temperature is 60℃~90℃, for example, any value among 60℃, 65℃, 70℃, 75℃, 80℃, 85℃ or 90℃, or any range or point value between any two values.
[0097] Thirdly, the present invention provides a heat-not-burn aerosol product 10, comprising an outer packaging paper 400, wherein a filter section 200 and a smoke-generating section are sequentially disposed within the outer packaging paper 400, and the smoke-generating section is a consumable 100 as described in any of the foregoing embodiments or a consumable 100 prepared by the preparation method described in the foregoing embodiments.
[0098] In an optional embodiment, the heating method for heating the non-combustible aerosol article 10 includes electromagnetic heating or contact heating.
[0099] In an optional embodiment, a cooling section 300 is also included between the filtration section 200 and the smoke-generating section.
[0100] Fourthly, the present invention provides the use of a consumable 100 as described in any of the foregoing embodiments or a consumable 100 prepared by the preparation method as described in the foregoing embodiments in the preparation of tobacco products.
[0101] The existing heated tobacco aerosol products (Category 10) require complex manufacturing processes, including cutting the tobacco into shreds and then combining them with cooling elements and filters. Furthermore, the uneven distribution of tobacco shreds during the compounding process leads to uneven heating of the heated tobacco aerosol products, affecting both the stable release of aroma and the stability of draw resistance during inhalation, thus impacting the smoking experience. Additionally, the heated tobacco aerosol products formed by compounding tobacco shreds lack stable, interconnected airflow channels (112) within the material, further affecting the uniformity of heating and the stability of draw resistance.
[0102] Based on this, the inventors propose a consumable 100 for heating non-combustible aerosol products. The consumable 100 is hollow, allowing for the formation of a stable and continuous airflow channel 112. The consumable 100 is formed by winding and splicing materials 110 together, with no overlap between layers during the winding process. Furthermore, the mechanical strength of the consumable 100 is improved by covering the inner layer seam with an outer layer. A butt joint 111 is provided between the edges of two adjacent layers of the same layer of the winding material 110, which facilitates the formation and flow of aerosols, thus providing the advantages of this invention. The heat-not-burning aerosol product 10 of the consumable 100, after heating, heats evenly due to the uniform distribution of the rolled material 110, and can form an aerosol evenly and stably. The aerosol can stably overflow along the butt joint 111 and be drawn in through the hollow airflow channel 112, ensuring the stability of the suction resistance during the suction process. At the same time, the combination of the design of the butt joint 111 and the hollow airflow channel 112 can also effectively reduce the suction resistance, giving users a better suction experience. In addition, the raw materials of the consumable 100 provided by the present invention are all plant materials, which are environmentally friendly and biodegradable.
[0103] Furthermore, the consumable 100 provided by this invention has a simple preparation method, which can be obtained by rolling. Compared with the traditional slicing and composite rod forming process, it does not require the setting of complex and expensive slicing equipment, resulting in low equipment investment. At the same time, it does not require a complex slicing process, which greatly simplifies the production process and improves the operating efficiency. It is suitable for large-scale industrial production and has good industrial applicability.
[0104] Example 1
[0105] Please refer to Figures 1-4This embodiment provides a consumable 100 for heating non-combustible aerosol products, comprising three layers of spiral material 110. Each layer of spiral material 110 is spirally wound and overlaps each other to form a hollow cylindrical structure. The hollow area inside the consumable 100 is the airflow channel 112, and the diameter of the hollow hole in the consumable 100 is 4 mm. The second layer of spiral material 110 covers the butt joint 111 of the first layer of spiral material 110, and the third layer of spiral material 110 covers the butt joint 111 of the second layer of spiral material 110. After the winding is completed, the number of layers in the cross-section of the consumable 100 is the same everywhere. The parameters of each layer of spiral material 110 are shown in Table 1.
[0106] Table 1 Parameters of the coiled material 110
[0107]
[0108]
[0109] This embodiment also provides a method for preparing a consumable 100 for a heat-resistant non-combustible aerosol product, comprising winding and molding as described above, and, starting from the second sheet of winding material 110, coating one side of each sheet of winding material 110 with a 3% guar gum solution. The surface of the winding material 110 coated with the adhesive side is then bonded to the inner layer of winding material 110.
[0110] After all the coiled materials 110 are wound, they are cut into consumables 100 with a length of 12mm, and then conveyed to an online hot air drying oven for drying at a temperature of 75℃. After drying, consumables 100 are obtained.
[0111] Example 2
[0112] Please refer to Figure 5 This embodiment provides a consumable 100 for heating non-combustible aerosol products, comprising three layers of spiral material 110. Each layer of spiral material 110 is spirally wound and overlaps each other to form a hollow cylindrical structure. The hollow area inside the consumable 100 is the airflow channel 112, and the diameter of the hollow hole in the consumable 100 is 4 mm. The butt joint 111 of the second layer of spiral material 110 coincides with the butt joint 111 of the first layer of spiral material 110, and the third layer of spiral material 110 covers the butt joint 111 of the second layer of spiral material 110. After the winding is completed, the number of layers in the cross-section of the consumable 100 is the same everywhere, and the parameters of each layer of spiral material 110 are the same as in Embodiment 1.
[0113] This embodiment also provides a method for preparing a consumable 100 for a heat-resistant non-combustible aerosol product, comprising winding and molding as described above, and, starting from the second sheet of winding material 110, coating one side of each sheet of winding material 110 with a 3% guar gum solution. The surface of the winding material 110 coated with the adhesive side is then bonded to the inner layer of winding material 110.
[0114] After all the coiled materials 110 are wound, they are cut into consumables 100 with a length of 12mm, and then conveyed to an online hot air drying oven for drying at a temperature of 75℃. After drying, consumables 100 are obtained.
[0115] Example 3
[0116] This embodiment provides a consumable 100 for heating non-combustible aerosol products, the structure and preparation method of which are similar to those of Example 1, the only difference being:
[0117] The roll-on material 110 consists of four layers. The adhesive used for bonding each layer of roll-on material 110 is a 5% CMC solution. The parameters of each layer of roll-on material 110 are shown in Table 2.
[0118] Table 2 Parameters of Crimping Material 110
[0119]
[0120] After all the coiled materials 110 are wound, they are cut into consumables 100 with a length of 42mm, and then conveyed to an online hot air drying oven for drying at a temperature of 60℃. After drying, consumables 100 are obtained.
[0121] Example 4
[0122] This embodiment provides a consumable 100 for heating non-combustible aerosol products, the structure and preparation method of which are similar to those of Example 1, the only difference being:
[0123] The diameter of the hollow hole in consumable 100 is 4.2 mm. The splicing material 110 consists of five layers. The adhesive used for bonding each layer of splicing material 110 is a 2% CMS solution. The parameters of each layer of splicing material 110 are shown in Table 3.
[0124] Table 3 Parameters of Crimping Material 110
[0125]
[0126] After all the coiled materials 110 are wound, they are cut into consumables 100 with a length of 45mm, and then conveyed to an online hot air drying oven for drying at a temperature of 60℃. After drying, consumables 100 are obtained.
[0127] Example 5
[0128] This embodiment provides a consumable 100 for heating non-combustible aerosol products, the structure and preparation method of which are similar to those of Example 1, the only difference being:
[0129] The diameter of the hollow hole in consumable 100 is 5 mm. The roll material 110 consists of eight layers. The adhesive used for bonding each layer of roll material 110 is a 4% starch solution. The parameters of each layer of roll material 110 are shown in Table 4.
[0130] Table 4 Parameters of Crimping Material 110
[0131]
[0132]
[0133] After all the coiled materials 110 are wound, they are cut into consumables 100 with a length of 75mm, and then conveyed to an online hot air drying oven for drying at a temperature of 90℃. After drying, consumables 100 are obtained.
[0134] Example 6
[0135] This embodiment provides a heat-not-combustible aerosol product 10, comprising a smoke-generating section and a filter section 200 connected in sequence. The smoke-generating section can be any of the consumables 100 provided in embodiments 1 to 5 above, such as... Figure 6 As shown, the consumable 100 provided in Example 1 serves as the smoke-generating section of the heated non-combustible aerosol product 10 provided in this example.
[0136] Example 7
[0137] This embodiment provides a heat-not-combustible aerosol product 10, comprising a smoke-generating section, a cooling section 300, and a filtration section 200 connected in sequence. The smoke-generating section can be any of the consumables 100 provided in embodiments 1-5 above, such as... Figure 7 As shown, the consumable 100 provided in Example 1 serves as the smoke-generating section of the heated non-combustible aerosol product 10 provided in this example.
[0138] Comparative Example 1
[0139] This comparative example provides a heat-resistant non-combustible aerosol product 10, the preparation method of which includes cutting into shreds and compounding into rods, as detailed below:
[0140] S01, Shredding
[0141] The raw material selected is reconstituted tobacco leaf rolls made using the slurry method, with a width of 138mm, a thickness of 0.2mm, and a basis weight of 220g / m³. 2With a tensile strength of 300 N / m and a moisture content of 8%, the material is cut into 1 mm wide filaments using a filament cutter, then gathered into rods through a flared mouth, wrapped with a layer of packaging paper, and cut into 12 mm segments. This material is equivalent to the consumable 100 in the embodiment of the present invention.
[0142] SO2, composite rod
[0143] The materials of the small section, the cooling section 300, and the filter section 200 are combined, and an outer layer of packaging paper 400 is wrapped around the outside of these three parts to form a complete heated non-combustible cigarette.
[0144] Comparative Example 2
[0145] This embodiment provides a consumable 100, which is largely the same as that in embodiment 3, except that the winding angle is 45° and the width of each layer of the roll material 110 is 10.0 mm.
[0146] The consumable 100 provided in this comparative example has an excessively large width 115 at the inner layer winding material 116 and the second inner layer winding material, causing each layer of paper to overlap and cover each other after winding, resulting in an uneven diameter of the cigarette stick after winding; the width 115 at the outermost layer winding material 118 and the second outermost layer winding material 117 is too small, resulting in too large a seam between each layer of paper, causing the winding between layers to be weak.
[0147] Experimental Example 1
[0148] The consumables 100 in Examples 1, 3-5 and Comparative Examples 1-2 were subjected to performance tests. The weight was measured using a balance, the total wall thickness was measured using a thickness gauge, the density was calculated, the strength was measured using a universal testing machine, and the elasticity was measured using a universal testing machine. The results are shown in Table 1.
[0149] Table 1 Performance of Consumable 100
[0150]
[0151] As shown in Table 1, the compressive strength along the tube cross-section and the Young's modulus in the cross-sectional direction of the consumable 100 in the embodiment are both superior to those of the comparative example. Comparative Example 1, being a consumable 100 formed by slicing reconstituted tobacco leaves, has the worst strength. Comparative Example 2, due to its improper winding method, resulting in overlapping layers, inconsistent tube diameters, gaps between layers, and weak adhesion, has lower strength than the embodiment.
[0152] Experimental Example 2
[0153] The consumables 100 obtained in Examples 1, 3-5 and Comparative Example 2 were all prepared into heat-not-burning aerosol products 10 using the method of Example 7. The suction performance of the heat-not-burning aerosol product 10 in Comparative Example 1 was tested. The suction resistance was tested using a cigarette suction resistance tester according to GB / T22838.5. The results are shown in Tables 2 and 3.
[0154] Table 2. Suction stability of heat-resistant non-combustible aerosol products 10
[0155]
[0156]
[0157] Table 3. Suction performance of heated non-combustible aerosol product 10
[0158] energy aroma smoke volume Example 1 Larger and more uniform release Sufficient and stable Large and stable smoke volume Example 3 Moderate and evenly released Moderate and stable Large and stable smoke volume Example 4 Moderate and evenly released Moderate and stable Large and stable smoke volume Example 5 Moderate and evenly released Moderate and stable Large and stable smoke volume Comparative Example 1 Moderate, weaker in the first three bites Moderate, weaker in the first three bites Moderate, weaker in the first three bites Comparative Example 2 Smaller size, unstable release It is relatively weak and its release is unstable. Smaller size, unstable release
[0159] As shown in Table 2, the heat-not-burning aerosol product 10 made from the consumable 100 provided in this embodiment of the invention has a lower overall suction resistance and more stable suction resistance, resulting in a more uniform heating effect, because the winding angle and width are matched, and the hollow tube setting retains a sufficient and stable airflow channel 112. Comparative Example 1 uses a traditional shredding and rolling process, where the airflow can only pass through the channels squeezed and twisted between the shreds, resulting in a larger overall suction resistance. Furthermore, the tobacco shreds of different cigarettes shrink differently when heated, causing changes in the airflow channel 112 and unstable suction resistance. Comparative Example 2 suffers from an unreasonable winding method, leading to overlap between the same layer and between layers, inconsistent tube diameter, gaps between layers, and poor adhesion. Therefore, the airflow channel 112 is unstable, and the suction resistance fluctuates greatly.
[0160] As shown in Table 3, Example 1, consisting of three layers of tobacco paper, has a high tobacco content and density, resulting in the best sensory quality during inhalation, with a strong strength, rich aroma, and abundant smoke. Example 2, consisting of three layers of tobacco paper plus a layer of flavored paper, retains the tobacco flavor while providing a wider range of taste experiences, with a moderate strength, moderate aroma, and abundant smoke. Example 3, consisting of two layers of tobacco paper, two layers of flavored paper, and a layer of metal foil, provides a richer flavor and is compatible with electromagnetic heating devices, offering a moderate strength, moderate aroma, and abundant smoke. Comparative Examples 1 and 2, due to unstable draw resistance, exhibit inconsistent strength, aroma, and smoke release.
[0161] The above are merely preferred embodiments of the present invention and are not intended to limit the present invention. Various modifications and variations can be made to the present invention by those skilled in the art. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of the present invention should be included within the scope of protection of the present invention.
Claims
1. A consumable for use in heating a non-combustible aerosol article, characterised in that, The rolled material comprises at least two layers, the rolled material is in a sheet structure, and the rolled material comprises at least an aerosol generating sheet; The edges of the rolled material of the same layer are not overlapped after being spirally wound, the edges of the rolled material of the multiple layers are spirally wound and overlapped to form a cylindrical structure with a hollow hole, and the width of each layer of the rolled material satisfies the following formula: Wherein b represents the width of the rolled material, n represents the number of layers of the rolled material counted from inside to outside, R0 represents the diameter of the hollow hole, d represents the thickness of the rolled material, and a represents the inclination angle of the rolled material.
2. The consumable according to claim 1, wherein, The inclination angle a of the rolled material is 25°-80°; Preferably, the ratio of the diameter of the hollow hole to the width of the rolled material is 0.1-0.
7.
3. The consumable according to claim 1, wherein, The edges of the outermost layer of the rolled material are in contact but not overlapped after being spirally wound, and the edges of the next outer layer of the rolled material are formed into a butt joint after being spirally wound. Preferably, the gap of the butt joint is less than 1.1 mm. Preferably, the outermost layer of the rolled material covers the butt joint of the adjacent next outer layer of the rolled material. Preferably, the axial midline area of the outermost layer of the rolled material covers the butt joint of the adjacent next outer layer of the rolled material.
4. The consumable of claim 1, wherein, The number of layers of the cross section of the consumable of the cylindrical structure is 2-8 layers, preferably 3-4 layers. Preferably, the outer diameter of the consumable is 7.1 mm±10% or 5.3 mm±10%. Preferably, the diameter of the hollow hole of the consumable is greater than 1.5 mm, more preferably, the diameter of the hollow hole of the consumable is 1.5 mm-4 mm. Preferably, the length of the consumable is 7 mm-84 mm.
5. The consumable of claim 1, wherein, The rolled material further comprises at least one of a filler paper, a flavor paper, and a metal foil. Preferably, the aerosol generating sheet is a reconstituted tobacco paper, and the raw material of the reconstituted tobacco paper comprises at least one of a paper process reconstituted tobacco, a thick pulp process reconstituted tobacco, a dry process reconstituted tobacco, and a roll process reconstituted tobacco.
6. A method of preparing a consumable according to any one of claims 1 to 5, characterised in that, The rolled material comprises spirally winding multiple layers of the rolled material coaxially into a hollow cylindrical structure, and cutting and drying after being wound and fixed.
7. The preparation method according to claim 6, characterized in that, The winding and fixing comprises: sequentially and synchronously spirally winding multiple layers of the rolled material along the same central axis from inside to outside.
8. The production method according to claim 6 or 7, characterized by, The inner side of the outer layer of the rolled material is coated with an adhesive to bond the outer layer of the rolled material with the inner layer of the rolled material. Preferably, the preparation of the adhesive comprises dissolving a food-grade plant polysaccharide in a solution to obtain a viscous liquid. Preferably, the concentration of the food-grade plant polysaccharide in the adhesive is 1%-10%. Preferably, the food-grade plant polysaccharide comprises any one of guar gum, starch, carboxymethyl cellulose, carboxymethyl starch, xanthan gum, and sodium alginate. Preferably, the method for coating the rolled material with the adhesive comprises at least one of dip coating and transfer. Preferably, the drying temperature is 60°C-90°C.
9. A heat-not-burn aerosol article, characterized in that, The outer layer of the packaging paper is provided with a filter segment and a smoking segment in sequence, the smoking segment is the consumable of any one of claims 1-5 or the consumable prepared by the preparation method of claim 6 or 7.