Solar shading device and shading material

The solar radiation shielding device with a diffuse reflection layer and photocatalyst layer addresses interference fringes by diffusing light, enhancing performance and energy efficiency in blinds.

JP2024162498APending Publication Date: 2024-11-21TACHIKAWA

Patent Information

Application Number
JP2023078049
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-10
Publication Date
2024-11-21

AI Technical Summary

Technical Problem

Interference fringes occur on the surfaces of solar radiation shielding materials, such as slats in blinds, due to factors like rotation angle and sunlight/indoor light incident angles, affecting their performance.

Method used

A solar radiation shielding device with a base material having a diffuse reflection layer and a photocatalyst layer, where the diffuse reflection layer contains light-diffusing particles, and the photocatalyst layer is made of titanium oxide, is used to suppress interference fringes by diffusing light at various angles.

Benefits of technology

The solution effectively suppresses interference fringes and reduces glare, enhancing antifouling, antibacterial, and deodorizing effects while improving energy efficiency by diffusing light regardless of incident angles.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024162498000001_ABST
    Figure 2024162498000001_ABST
Patent Text Reader

Abstract

To provide a solar shading device capable of suppressing the occurrence of interference fringes in a shading material.SOLUTION: A solar shading device comprises a slat 13 supported by a support member, and the slat 13 comprises: a base material 21; a diffuse reflection layer 22 having light diffusing particles 22a dispersed therein and provided on at least one surface of the base material 21; and a photocatalyst layer 23 provided on the upper side of the diffuse reflection layer 22.SELECTED DRAWING: Figure 3
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a solar shading device and a solar shading material that reflects solar radiation. [Background technology]

[0002] A horizontal blind as a sunshade device has a lifting cord hanging down from a head box, and a plurality of slats as shading materials arranged parallel to one another between a bottom rail and the head box. The slats are supported by ladder cords hanging down from the head box. The slats are rotated by the ladder cords (see Patent Document 1).

[0003] Some slats have a surface coated with a photocatalyst (see Patent Document 1). When such slats are used, the stain-proofing, antibacterial, deodorizing effects, etc. of the slats can be improved. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2009-127377 A Summary of the Invention [Problem to be solved by the invention]

[0005] The slats have a long rectangular plate shape and have opposing first and second surfaces. The slats are supported by ladder cords so that the first surface faces upward. However, when a photocatalyst such as titanium oxide is applied to the surface of the slats, interference fringes may occur on the surface of the slats due to various factors such as the rotation angle of the slats, the angle of incidence of solar radiation, and the angle of incidence of indoor light. For example, interference fringes are likely to occur near the long sides of the slats. This problem applies not only to the shading materials of horizontal blinds, but also to the shading materials of various solar shading devices such as the slats of vertical blinds. [Means for solving the problem]

[0006] A solar shading device for solving the above problem comprises a shading material supported by a support member, the shading material comprising a base material, a diffuse reflective layer having dispersed light diffusing particles provided on at least one surface of the base material, and a photocatalyst layer provided on the upper side of the diffuse reflective layer.

[0007] In the solar radiation shading device, the photocatalyst in the photocatalyst layer may be made of titanium oxide. In the solar shading device, the base material may have opposing surfaces that are a convex curved surface and a concave curved surface.

[0008] In the above-mentioned solar shading device, the support member may rotatably support the shading material, and the shading material may be configured so that, by rotation, the one side and the other side opposite to the one side are selectively faced toward the inside of the room.

[0009] The shielding material for solving the above problem includes a substrate, a diffuse reflection layer having dispersed therein light-diffusing particles and provided on at least one surface of the substrate, and a photocatalyst layer provided on the upper side of the diffuse reflection layer. Effect of the Invention

[0010] According to the present invention, the occurrence of interference fringes in the shielding material can be suppressed. [Brief description of the drawings]

[0011] [Figure 1] FIG. [Diagram 2] FIG. 2 is a front view of a horizontal blind. [Diagram 3] 1 is a schematic diagram showing how a slat having a diffuse reflective layer using a light-transmitting paint reflects solar radiation. FIG. [Figure 4] FIG. 2 is a schematic diagram showing the state of a slat reflecting solar radiation. [Diagram 5]1 is a schematic diagram showing how a slat having a diffuse reflection layer using a light-blocking paint reflects solar radiation. FIG. [Figure 6] FIG. 4 is a cross-sectional view of a slat according to a reference example. [Figure 7] (a) is a diagram explaining the specular reflectance of artificial lighting equivalent to visible light at an incidence angle of 30°, and (b) is a diagram explaining the specular reflectance of artificial lighting equivalent to visible light at an incidence angle of 60°. [Figure 8] (a) is a diagram showing the specular reflectance of a slat that does not contain light-diffusing particles in the diffuse reflective layer, (b) is a diagram showing the specular reflectance of a slat that has been given a matte finish, (c) is a diagram showing the specular reflectance of a slat that has a light-blocking diffuse reflective layer, and (d) is a diagram showing the specular reflectance of a slat that has a light-transmitting diffuse reflective layer. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] Hereinafter, a horizontal blind to which the present invention is applied will be described with reference to the drawings. [Overall structure] As shown in Figures 1 and 2, in the horizontal blind 1, a plurality of slats 13 are suspended in parallel to one another via a plurality of ladder cords 12 suspended from a head box 11. The ladder cords 12 are support members that support the slats 13. The upper end of each ladder cord 12 is supported by an angle adjustment device for the slats 13 disposed in the head box 11, and the lower end is connected to a bottom rail 14. A plurality of lifting cords 15 suspended from the head box 11 are inserted into the slats 13 near the ladder cords 12. The upper end of each lifting cord 15 is wound around a winding shaft 16 rotatably supported within the head box 11, and the lower end is connected to the bottom rail 14.

[0013] A pulley case 17 is provided at one end of the head box 11. An endless operating cord 18 hangs down from the pulley case 17. A pulley is rotatably supported within the pulley case 17. The pulley is rotated forward and backward by operating the operating cord 18. The operating cord 18 and the pulley case 17 constitute the operating section of the horizontal blind 1.

[0014] When the operating cord 18 is pulled in one direction or the other, the pulley is rotated, which in turn rotates the drive shaft 19 connected to the winding shaft 16 via a gear box or the like. Specifically, when the drive shaft 19 is rotated in the forward direction, the winding shaft 16 is rotated in the unwinding direction of the lift-up cord 15, thereby lowering the slats 13 and the bottom rail 14. When the drive shaft 19 is rotated in the reverse direction, the winding shaft 16 is rotated in the winding direction of the lift-up cord 15, thereby lifting the slats 13 and the bottom rail 14. In the horizontal blind 1, the angle adjustment device of the slats 13 operates in parallel with the lifting and lowering operation of the slats 13 based on the forward and reverse rotation of the winding shaft 16, so that each slat 13 is rotated in the same phase via the ladder cord 12.

[0015] The head box 11 is fixed to a mounting surface such as the upper part of a window via mounting brackets 9 attached to at least both ends thereof. The slats 13 serving as shielding materials have a long and narrow rectangular thin plate shape. The multiple slats 13 are lined up along the lifting direction, which is the height direction of the horizontal blind 1. The slats 13 are supported by ladder cords 12 suspended from the head box 11 so that the tilt can be adjusted. A bottom rail 14 having approximately the same length as the slats 13 is disposed below the lowermost slat 13. The bottom rail 14 is a fixed part to which the lower end of a lifting cord 15 is fixed by a cord holder 14a or the like.

[0016] The bottom rail 14 is a weight member that maintains the multiple slats 13 in a lowered state. The bottom rail 14 has approximately the same longitudinal length and lateral width as the slats 13. When the bottom rail 14 is raised, the multiple slats 13 are stacked on the bottom rail 14. The ladder cord 12 has a pair of warp threads whose lower ends are connected to the bottom rail 14 by a cord holder 14a or the like. The ladder cord 12 also has a weft thread between the pair of warp threads. The slats 13 are supported by the weft thread. The bottom rail 14 is connected to the lower end of a lifting cord 15 that is pulled out from the head box 11. The bottom rail 14 is suspended from the head box 11 by the lifting cord 15.

[0017] [Slat configuration] As shown in FIG. 3, the slat 13 includes a base material 21, a diffuse reflection layer 22 applied to the surface of the base material 21, and a photocatalyst layer 23 provided on the upper layer of the diffuse reflection layer 22. The base material 21 is formed of a light-shielding material such as a synthetic resin plate, aluminum, or stainless steel. In this embodiment, aluminum is used for the base material 21. The base material 21 may also be formed of a fireproof material, or may be formed of a wooden board or resin. The base material 21 has a cross-sectional arc shape. The first surface of the slat 13 is a convex curved surface 21a. The second surface opposite to the first surface is a concave curved surface 21b.

[0018] The convex curved surface 21a, which is the first surface, faces upward when the slats 13 are fully opened on the weft of the ladder cord 12. The convex curved surface 21a faces the outside of the room when the slats 13 are in the forward shading mode. The concave curved surface 21b, which is the second surface, faces the inside of the room. When the slats 13 are in the forward shading mode, the upper slat 13 overlaps the lower slat 13 in the vertically adjacent slats 13 when viewed from the outside of the room, so that the solar radiation 31 is less likely to enter the room through the gaps between the slats 13. Even if the diffusive reflective layer 22 and the photocatalytic layer 23 are provided on the convex curved surface 21a of the slat 13, a convex curved surface with the same curvature as the convex curved surface 21a appears on the surface of the slat 13. Even if the diffusive reflective layer 22 and the photocatalytic layer 23 are provided on the concave curved surface 21b, a concave curved surface with the same curvature as the concave curved surface 21b appears on the surface of the slat 13.

[0019] The diffuse reflection layer 22 is formed by applying a light-transmitting or light-shielding paint in which light diffusion particles 22a, which are fine particles, are dispersed on the surface of the substrate 21. That is, the diffuse reflection layer 22 is provided on the convex curved surface 21a and the concave curved surface 21b. The paint forming the diffuse reflection layer 22 contains light diffusion particles 22a, which are fine particles. The light diffusion particles 22a are dispersed not only on the surface of the diffuse reflection layer 22 but also inside the layer. The light diffusion particles 22a are inorganic particles. As an example, the light diffusion particles 22a may be glass beads, acrylic beads, silica, or the like, or may be formed by mixing these beads.

[0020] The particle size of the light diffusing particles 22a is 1 μm or more. By making the particle size of the light diffusing particles 22a 1 μm or more, light can be sufficiently diffusely reflected on the surface and inside of the diffuse reflection layer 22. In addition, the particle size is 30 μm or less or 10 μm or less. By making the particle size of the light diffusing particles 22a 30 μm or less or 10 μm or less, the light diffusing particles 22a can be sufficiently and uniformly dispersed within a required predetermined thickness of the diffuse reflection layer 22. As an example, the particle size of the light diffusing particles 22a is about 3 μm.

[0021] The thickness of the diffuse reflection layer 22 is 10 μm or more, or 50 μm or less, or 20 μm or less. The particle size of the light diffusing particles 22a is preferably smaller than the thickness of the diffuse reflection layer 22. This allows the light diffusing particles 22a to be dispersed in the diffuse reflection layer 22 as well.

[0022] The light diffusing particles 22a are contained in the light-transmitting or light-shielding paint at a content of 2% by mass or more or 4% by mass or more. By containing the light diffusing particles 22a in the paint at a content of 2% by mass or more or 4% by mass or more, the light is diffusely reflected on the surface of the diffuse reflection layer 22, thereby reducing the regular reflectance.

[0023] Furthermore, when the paint is light-transmitting, the light diffusion particles 22a are contained in the paint at 2% by mass or 4% by mass or more, so that light is diffusely reflected inside the diffuse reflection layer 22, thereby reducing the regular reflectance. The light diffusion particles 22a are contained in the light-transmitting or light-blocking paint at 10% by mass or less or 5% by mass or less. The light diffusion particles 22a can be uniformly dispersed in the paint by containing the light diffusion particles 22a at 10% by mass or 5% by mass or less in the light-transmitting or light-blocking paint. Also, it is possible to prevent the paint from becoming too viscous, which makes it difficult to apply the paint.

[0024] The photocatalyst layer 23 is formed by applying a coating agent in which photocatalyst particles are dispersed in a dispersion liquid. As the photocatalyst particles, titanium oxide is preferable, but tungsten oxide or the like may also be used. The photocatalyst layer 23 is a coating applied to the upper layer of the diffuse reflection layer 22. The thickness of the photocatalyst layer 23 is 6 nm or more. Also, it is 50 nm or less. Light irradiated to the photocatalyst layer 23 passes through the photocatalyst layer 23 and is reflected by the diffuse reflection layer 22. By setting the thickness of the photocatalyst layer 23 to 6 nm or more and 50 nm or less, the antifouling, antibacterial, deodorizing effects, etc. of the slats 13 can be sufficiently exhibited. Furthermore, when the thickness of the photocatalyst layer 23 is 6 nm or less, the density of the photocatalyst particles becomes insufficient, and the antifouling, antibacterial, deodorizing effects, etc. of the slats 13 cannot be sufficiently obtained. Furthermore, if the thickness of the photocatalyst layer 23 is made 6 nm or less, the density of the photocatalyst particles becomes insufficient, and the antifouling, antibacterial, deodorizing effects, etc. of the slats 13 cannot be sufficiently obtained. Furthermore, if the thickness is made thicker than 50 nm, the color tone of the diffuse reflection layer 22 is affected.

[0025] As shown in FIG. 4, when fully open, the slats 13 are spaced apart from each other and parallel to each other. Most of the solar radiation 31 enters from diagonally above outside the room, and after passing through the photocatalyst layer 23, it is diffusely reflected by the diffuse reflection layer 22. The solar radiation 31 then enters the room. As shown in FIG. 3, when the solar radiation 31 enters the room while the slats 13 are in the open state, the solar radiation 31 passes through the photocatalyst layer 23 and is diffusely reflected by the many light diffusion particles 22a on the surface of the diffuse reflection layer 22. The diffuse reflection layer 22 shown in FIG. 3 has translucency. Therefore, the solar radiation 31 enters the inside of the diffuse reflection layer 22, and the solar radiation 31 that has entered the inside is diffusely reflected by the many light diffusion particles 22a inside.

[0026] The angle of incidence of solar radiation 31 on the slats 13 is small when the sun's altitude is high at noon or around noon, and is large in the morning and evening. The angle of incidence here is the angle between the incident direction of solar radiation (visible light) and the normal to the slats 13. Therefore, if the diffuse reflective layer 22 is translucent, the larger the angle of incidence, the longer the optical path length that the solar radiation 31 passes through the diffuse reflective layer 22. Accordingly, the solar radiation 31 repeatedly hits the light diffusing particles 22a in the diffuse reflective layer 22, and is diffusely reflected to a greater extent.

[0027] 5, when the diffuse reflective layer 22 has a light blocking property, even if light diffusing particles 22a are dispersed within the layer, almost no solar radiation 31 penetrates into the diffuse reflective layer 22. The solar radiation 31 is simply diffusely reflected by the numerous light diffusing particles 22a on the surface of the diffuse reflective layer 22.

[0028] 6 shows, as a reference example, a slat 41 provided with a photocatalytic layer 23 on the substrate 21 without providing a diffuse reflection layer 22. In the example of FIG. 6, the regular reflectance of the substrate 21 increases, causing interference between the light entering the photocatalytic layer 23 and the light regularly reflected by the substrate 21, resulting in the formation of interference fringes.

[0029] As described above, providing the diffuse reflection layer 22 containing the light diffusing particles 22a between the substrate 21 and the photocatalyst layer 23 is related to the occurrence of interference fringes in the photocatalyst layer 23. When providing the photocatalyst layer 23, it is necessary to reduce the light regularly reflected by the substrate 21.

[0030] 8 shows the regular reflectance of artificial lighting equivalent to visible light in the slat 13. Specifically, (a) shows a case where the layer corresponding to the diffuse reflective layer 22 does not contain light diffusing particles 22a. (b) shows a case where the layer corresponding to the diffuse reflective layer 22 is matte-finished using a light-blocking paint (the amount of light diffusing particles 22a is less than in (c) and (d)). (c) shows a case where the light-blocking diffuse reflective layer 22 is used. (d) shows a case where the light-transmitting diffuse reflective layer 22 is used.

[0031] Each of Figures 8(a) to (d) shows the specular reflectance at an incidence angle of 30° (see Figure 7(a)) and at an incidence angle of 60° (see Figure 7(b)) of artificial lighting equivalent to visible light. In the case of Figure 8(b), the light diffusing particles 22a are contained in the paint at about 1 mass %. In addition, in Figures 8(c) and (d), the light diffusing particles 22a are contained in the paint at 2 mass % or more and 10 mass % or less.

[0032] 8, the specular reflectance of the slats 13 is lower when the layer corresponding to the diffuse reflection layer 22 is matte-finished (see FIG. 8(b)) than when the layer does not contain light diffusing particles 22a and is not matte-finished (see FIG. 8(a)). Furthermore, the specular reflectance decreases as the light diffusing particles 22a contained in the layer increases (see FIGS. 8(c) and (d)).

[0033] 8(a) to 8(c), comparing the specular reflectance of visible light at an incidence angle of 30° with that at an incidence angle of 60°, the specular reflectance at an incidence angle of 60° is higher than that at an incidence angle of 30°. In contrast, in (d), the specular reflectance at an incidence angle of 60° is lower than that at an incidence angle of 30°. This is because the larger the incidence angle, the longer the optical path length through which the solar radiation 31 passes through the diffuse reflection layer 22. The solar radiation 31 repeatedly hits the light diffusion particles 22a in the diffuse reflection layer 22, and is repeatedly diffusely reflected. In addition, the solar radiation 31 is attenuated by the repeated diffuse reflection. This phenomenon in which the specular reflectance at an incidence angle of 60° is lower than that at an incidence angle of 30° also occurs at incidence angles of 70° and 80°, which are larger than 60°.

[0034] 8(c) and (d), the regular reflectance is significantly reduced compared to (a) and (b). Therefore, in the slats 13 shown in Fig. 8(c) and (d), even when a photocatalytic layer 23 is provided on the diffuse reflection layer 22, the occurrence of interference fringes can be suppressed.

[0035] [Operation of the embodiment] The horizontal blind 1 configured as above has the following effects. First, the case of lowering the slats 13 will be described. When the operating cord 18 is pulled to move the slats 13 downward, the slats 13 rotate in the initial movement so as to be in a fully closed state that blocks solar radiation 31. Next, the winding shaft 16 rotates in the unwinding direction of the lifting / lowering cord 15, and the slats 13 and bottom rail 14 are moved downward and lowered. Thereafter, the slats 13 rotate so as to be in a fully open state parallel to each other.

[0036] Next, the case where the slats 13 are raised will be described. When the slats 13 are moved upward, the operating cord 18 is first pulled in the opposite direction to that when lowering. Then, the slats 13 rotate from a fully closed state to a fully open state in which the slats 13 are parallel to each other, and then to a reverse fully closed state in which the slats 13 are reversely rotated. After this, the slats 13 and the bottom rail 14 are raised.

[0037] As described above, the slats 13 rotate during the raising and lowering motion. Therefore, the slats 13 are irradiated with light at various angles of incidence. The diffuse reflection layer 22 diffuses and reflects the light that passes through the photocatalyst layer 23, regardless of the angle of incidence. Therefore, the slats 13 can suppress the occurrence of interference fringes, regardless of their vertical position or rotation angle.

[0038] [Effects of the embodiment] The horizontal blind 1 as described above can provide the following effects. (1) The slat 13 has a photocatalytic layer 23 provided on the diffuse reflective layer 22. This makes it possible to suppress the occurrence of interference fringes in the photocatalytic layer 23.

[0039] (2) For the photocatalyst of the photocatalyst layer 23, general-purpose titanium oxide can be used. (3) The diffuse reflection layer 22 can diffusely reflect light that has passed through the photocatalyst layer 23. In the slat 13, the convex curved surface 21a and the concave curved surface 21b allow light to enter the photocatalyst layer 23 at various angles of incidence, and the light is diffusely reflected by the diffuse reflection layer 22. Therefore, the slat 13 can suppress the occurrence of interference fringes at any position of the convex curved surface 21a and the concave curved surface 21b.

[0040] (4) The slats 13 rotate during their up-down movement, allowing light to be irradiated at various angles of incidence. The diffuse reflection layer 22 diffuses and reflects the light that passes through the photocatalyst layer 23, regardless of the angle of incidence. Therefore, the slats 13 can suppress the occurrence of interference fringes, regardless of their vertical position or rotation angle.

[0041] (5) The diffuse reflection layer 22, whether the paint is light-transmitting or light-blocking, can suppress the occurrence of interference fringes in the photocatalyst layer 23 by containing a predetermined amount of predetermined light-diffusing particles 22a.

[0042] (6) By providing the slats 13 with the diffuse reflective layer 22, the regular reflectance can be reduced. This reduces glare caused by regular reflection of solar radiation 31 from the slats 13. Furthermore, the lower regular reflectance can increase the energy saving effect. It is more preferable to install such horizontal blinds 1 on windows facing south, east and west, which are prone to receive solar radiation 31.

[0043] The horizontal blind 1 can be further modified as follows. In addition to the above embodiment, the present embodiment may be modified as follows, or may be a combination of at least two of the modified examples that are not mutually contradictory.

[0044] The slats 13 do not have to have a shape having the convex curved surface 21a and the concave curved surface 21b, and may be flat plates with both surfaces formed as flat surfaces. The operating part of the horizontal blind 1 may be a one-pole type with an equalizer at the tip of the tilt pole.Alternatively, it may be a pole type with a separate pole and cord, where the slats 13 are opened and closed by turning the pole, and the slats 13 are raised and lowered by pulling the lifting cord 15.

[0045] The slats 13 may be provided with a diffuse reflective layer 22 on the upwardly facing surface, which is the incident surface for solar radiation 31 at least in the open state, i.e., the convex curved surface 21a in this case. The diffuse reflective layer 22 may be omitted on the lower concave curved surface 21b. In other words, the convex curved surface 21a and the concave curved surface 21b may be different colors.

[0046] When providing the diffuse reflective layer 22 on the base material 21, a base layer may be provided on the surface of the base material 21 first. Between the diffuse reflection layer 22 and the photocatalytic layer 23, for example, an intermediate layer for protecting the diffuse reflection layer 22 may be provided.

[0047] -Applicable to manual horizontal blinds1 as well as motorized horizontal blinds. The solar shading device may be a slat used in a manual or electric vertical blind instead of the horizontal blind 1. [Explanation of symbols]

[0048] 1. Horizontal blinds 9…Mounting bracket 11…Head box 12...Ladder cord 13…Slat 14…Bottom rail 14a…Cord holder 15…Lifting cord 16…Winding shaft 17...Pulley case 18...Operation code 19…Drive shaft 21...Base material 21a...Convex curved surface 21b…Concave curved surface 22...Diffuse reflection layer 22a...Light diffusing particles 23…Photocatalyst layer 31…Solar radiation

Claims

1. A shielding material supported by a support member is provided, The shielding material is A substrate; a diffuse reflection layer having light diffusing particles dispersed therein, the diffuse reflection layer being provided on at least one surface of the substrate; A photocatalytic layer provided on the upper side of the diffuse reflective layer; A solar shading device comprising:

2. The photocatalyst in the photocatalyst layer is titanium oxide. The solar shading device according to claim 1 .

3. The substrate has opposing surfaces that are configured as a convex curved surface and a concave curved surface. The solar shading device according to claim 1 or 2.

4. The support member rotatably supports the shielding material, The shielding material is rotated so that the one surface and the other surface opposite to the one surface are selectively oriented toward the indoor side. The solar shading device according to claim 1 or 2.

5. A substrate; a diffuse reflection layer having light diffusing particles dispersed therein, the diffuse reflection layer being provided on at least one surface of the substrate; A photocatalytic layer provided on the upper side of the diffuse reflective layer; A shielding material comprising:

Citation Information

Patent Citations

  • Blind

    JP2009127377A

Cited By

  • Separator, electrochemical cell, stack, electrolysis device, and fuel cell

    CN121709654A