Element of an outer part for a timepiece or jewellery and method of manufacturing same
By integrating a metallic glass insert into a fiber-reinforced polymer matrix composite material, the mechanical resistance and aesthetic appeal of timepiece and jewelry outer parts are improved, achieving efficient and precise manufacturing.
Patent Information
- Application Number
- JP2022188097
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2022-10-13
- Filing Date
- 2022-11-25
- Publication Date
- 2024-11-18
- Estimated Expiration
- 2042-11-25
AI Technical Summary
Existing composite materials used for timepiece and jewelry outer parts suffer from low mechanical resistance and matte appearance, making them unsuitable for high-grade applications.
Incorporating a metallic glass insert into a fiber-reinforced polymer matrix composite material, specifically forming a cavity in the outer part to house the insert, which is made by injecting metallic glass to provide mechanical strength and aesthetic appeal.
The solution provides outer parts with enhanced mechanical resistance and shine, allowing for efficient manufacturing with reduced time and cost, while maintaining high precision.
Smart Images

Figure 0007585284000001 
Figure 0007585284000002
Abstract
Description
[Technical field]
[0001] The present invention relates to an element of an external piece for a timepiece or an article of jewellery.The present invention further relates to a method for manufacturing an element of such an external piece. [Background technology]
[0002] Numerous methods have already been proposed for manufacturing elements of external parts for timepieces or jewellery such as cases, middles, bezels, bracelet links, etc. Among these known manufacturing methods, there is one for manufacturing such elements of external parts using composite materials obtained by dispersing fibres in a polymer matrix. An example of such a composite material is one in which carbon fibres are dispersed in a polymer matrix, also known as Carbon Fibre Reinforced Polymer (CFRP).
[0003] It has been observed that external part elements for timepieces or jewellery made with composite materials are often subject to two major problems during use: a low mechanical resistance to external attack and a low luminance. Indeed, it has been found that the polymer matrix with dispersed carbon fibres is relatively soft and easily scratched. For this reason, it has been found that the techniques for producing decorations and reliefs with such composite materials do not technically allow for a long service life. Furthermore, external part elements obtained with composite materials of the carbon fibre reinforced polymer matrix type have a matte appearance, which makes it difficult to conceive of using such external part elements for external parts of high-end portable timepieces (e.g. wristwatches, pocket watches).
[0004] To remedy these problems, alternative methods have already been proposed: metals and ceramic materials are used to make the elements of the external parts that are most exposed to external attacks, such as bezels, crown-type controls and pushers; other composite materials of metallic matrix or fiber-reinforced type are also used; and recently it has also been proposed to make the elements of the external parts for timepieces or jewellery using composite materials, commonly called cermets, consisting of a metallic matrix with a ceramic reinforcement.
[0005] Although progress has been made in terms of the mechanical resistance of the elements of the external parts thanks to the use of composite materials with a metal matrix and fibers, composite materials reinforced by ceramics, the elements of the external parts obtained still do not fully meet the requirements in the field of wristwatches and jewellery in terms of the mechanical resistance of their decoration or relief. In fact, the techniques usually used to produce decorations and reliefs on the elements of these external parts combine physical vapor deposition (PVD) and electroforming, which only allow very thin layers to be obtained. As a result, although these thin layers have a glossy appearance due to their metallic nature, they are very small in thickness and the mechanical resistance of these thin layers to friction and wear is not high.
[0006] For example, European Patent Application EP2315673A1 proposes another technique for decorating watch bezels and the like. Briefly, this technique involves forming a recess in the surface of the bezel, made of ceramics or the like, to receive the time index or the like. An annular flange made of amorphous metal is then deposited on the surface of the bezel. The amorphous metal flange is then heated to a temperature above its glass transition temperature Tg and pressure is applied so that the amorphous metal fills the recess. The amorphous metal is then cooled and excess material is removed.
[0007] Thanks to this technique, an external part element for a timepiece is obtained, which is formed with a solid decoration resistant to mechanical stress and wear, but this technique requires the preparation of an amorphous metal flange, heating, pressing, cooling and finally removing the excess amorphous metal at the face of the external part element, which makes it time-consuming and expensive to carry out. Summary of the Invention [Problem to be solved by the invention]
[0008] The present invention aims to remedy these and other problems by providing an element of an external part for a timepiece or piece of jewellery, made from a material that fully meets the requirements required in the field of watchmaking or jewellery, in particular as it relates to mechanical resistance and aesthetics. The invention also provides a method for manufacturing such an element of an external part. [Means for solving the problem]
[0009] In view of this situation, the present invention relates to an element or component of an external piece for a timepiece or piece of jewelry made with a fiber-reinforced polymer matrix composite material, said element or component of an external piece having, in at least one of its faces, at least one cavity for accommodating an insert made of metallic glass.
[0010] In particular embodiments of the invention, the polymeric material used to form the matrix is thermoplastic or thermosetting.
[0011] In another particular embodiment of the invention, the polymeric material is selected from the group consisting of polyetheretherketone (PEEK), polytetrafluoroethylene (PTFE) and polyamideimide (PAI).
[0012] In another particular embodiment of the invention, the fibers reinforcing the polymer matrix are selected from the group consisting of glass fibers, carbon fibers, and aramid fibers.
[0013] In another particular embodiment of the invention, the metallic glass used to make the insert is of the bulk metallic glass type (BMG).
[0014] In another particular embodiment of the invention, the metallic glass used in the insert comprises zirconium or platinum.
[0015] In a more particular embodiment of the invention, the metallic glass used to make the insert is derived from an alloy of zirconium, copper, titanium, nickel, aluminum, niobium, and titanium, except for unavoidable impurities.
[0016] In another particular embodiment of the invention, the metallic glass used to make the insert comprises zirconium, copper, titanium, nickel, aluminum and niobium in the following amounts by weight: 60≦Zr≦75, 10≦Cu≦20, 0≦Ti≦6, 7≦Ni≦15, 0≦Al≦8, 0≦Nb≦6.
[0017] In another embodiment of the invention, the metallic glass used to make the insert is the alloy Vit106a, with the composition Zr70Cu13Ni9.9Al3.65Nb3.4, or the alloy Vit105, with the composition Zr65.7Cu15.6Ni11.7Al3.7Ti3.3, in weight percent.
[0018] In a more particular embodiment of the invention, the metallic glass used to make the insert is derived from an alloy of platinum, copper, nickel and phosphorus, except for unavoidable impurities.
[0019] In another particular embodiment of the invention, the metallic glass used to make the insert comprises platinum, copper, nickel and phosphorus in the amounts, in weight percent, of 80≦Pt≦90, 5≦Cu≦10, 1≦Ni≦3, 4≦P≦7.
[0020] In another particular embodiment of the invention, the metallic glass used to make the insert has the composition, in weight percent, Pt85Cu7Ni2.3P5.7.
[0021] In another particular embodiment of the invention, the metallic glass used to make the insert has a glass transition temperature of 350° C. or less.
[0022] In another particular embodiment of the invention, said outer part for a timepiece or an article of jewellery is a back, a middle, a bezel, a bracelet link or a clasp.
[0023] The invention further relates to a method for manufacturing an element or component of an outer piece for a timepiece or an article of jewellery, - making the elements of the outer part using a fiber reinforced polymer matrix composite material; machining at least one surface of the element or component of the external part to form at least one cavity; heating the metallic glass to its melting point; injecting and filling the at least one void with a metallic glass to form an insert; and a step of performing finishing operations as required.
[0024] In a particular embodiment of the invention, said recess is formed by milling.
[0025] In another particular embodiment of the invention, the finishing operation involves removing excess material, polishing, and / or trimming the insert.
[0026] Thanks to these characteristics, the invention makes it possible to provide an element of an external part for a timepiece or a piece of jewellery, which is covered on the outside with one or more inserts, such as time indexes, numbers, logos or other technical or decorative indicia. Such inserts, made by injecting metallic glass, are in the form of a solid block and therefore have a good mechanical resistance to friction and wear. They also have an appearance that meets the aesthetic requirements in the field of wristwatches and jewellery. In fact, due to the thickness of such inserts, any finishing operation can be carried out, which can give them a metallic sheen. Likewise, such inserts are made in a single step of injecting metallic glass, which allows to save a great deal of time and costs and ensures a good manufacturing precision. It should be noted that for all practical purposes and for the purposes of this specification, "metallic glass" refers to the category of metal alloys, which have the particularity of being at least partially solidifiable in an amorphous state, i.e. without a regular atomic arrangement. Metallic glasses are therefore distinct from traditional metals, which in particular crystallize according to organized structures such as simple cubic, body-centered or face-centered, hexagonal, and variants of these structures. They are generally obtained from ternary, quaternary, or higher alloys, in which elements that are not dimensionally compatible with one another combine to obtain the property of solidifying in an amorphous state by slowing down the solidification rate system from a given cooling rate sufficiently to obtain a disordered solid crystal structure. The behavior of this group of materials allows applications similar to those of polymeric materials, such as injection molding and hot processing. These materials have the advantages of being particularly corrosion-resistant, hard, and behaving elastically to reduce internal mechanical losses.
[0027] Other characteristics and advantages of the invention will become apparent from reading the following detailed description of an embodiment of an element of an outer piece for a timepiece or jewellery according to the invention, with reference to the accompanying drawings, in which: This example is given purely for illustrative and non-limiting purposes. [Brief description of the drawings]
[0028] [Figure 1] FIG. 2 is a top view of the bezel for the portable watch according to the present invention. [Diagram 2] FIG. 2 is a cross-sectional view taken along line BB in FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0029] The invention is based on an inventive concept which involves providing an element of an external part for a timepiece or jewellery, which has mechanical and aesthetic characteristics that meet the requirements in the field of wristwatches. For this purpose, the invention teaches to produce such an element of an external part using a fibre-reinforced polymer matrix composite material and to produce at least one cavity in the surface of the element of the external part, in which a decorative or functional insert made of metallic glass is received. Thanks to the use of a fibre-reinforced polymer matrix composite material, the element of the external part according to the invention has mechanical wear resistance and aesthetic characteristics that are perfectly suitable for timepiece applications. Furthermore, the insert produced by injection of metallic glass forms a solid block, which is thick enough to withstand mechanical attacks from the outside. Furthermore, due to its thickness, such an insert is easier to withstand finishing operations, which allows it to obtain the highest brightness and brilliance. Finally, such an insert is produced by a single injection step, which allows considerable time savings and excellent manufacturing precision.
[0030] The bezel as a whole is assigned the reference number 1 and is shown in Figure 1 as an example of an exterior element for a timepiece according to the invention, other exterior elements such as backs, middles, bracelet links, clasps etc. are also contemplated.
[0031] According to the invention, the bezel 1 is made of a fiber-reinforced polymer matrix composite material. In the illustrative example, the polymer material used to form the matrix is thermoplastic or thermosetting, but not limiting. The polymer material is preferably selected from the group consisting of polyetheretherketone (PEEK), polytetrafluoroethylene (PTFE) and polyamide-imide (PAI). The matrix is reinforced by fibers, preferably selected from the group consisting of glass fibers, carbon fibers and aramid fibers. A number of such bezels 1 can be individually characterized in a plate of composite material having the required thickness.
[0032] For example, the filament winding method of the SPIDE TP type, developed by the French technical centre for the mechanical industry CETIM, can be used to produce elements of an external part such as the bezel 1 according to the invention. Briefly described, this filament winding method is a method in which fibres, pre-impregnated with a polymer material, are wound on a mould, such as a tube, with a cross section forming a cylindrical shape, to obtain a specific contour. At the same time that these fibres, pre-impregnated with polymer, are wound around the mould according to a given number of layers and according to an angle relative to the longitudinal axis of symmetry of the mould, they are heated to a temperature high enough to melt the impregnated polymer and pressed against the mould. This mould is selected in particular depending on the subsequent use of the part obtained by cutting the contour. Finally, the part obtained is worked in the traditional way, using lathes and milling machines, to obtain the final dimensions.
[0033] In the case of the present invention, the bezel 1 is obtained by cutting a cylindrical profile having an inner diameter of typically about 30 mm and an outer diameter of about 45 mm. The cylindrical profile to be cut to obtain the bezel 1 according to the present invention is obtained by winding carbon fibers impregnated with polyetheretherketone (PEEK), which has a melting point of 341°C and a diameter of typically about 5 to 25 mm. To obtain the desired tubular profile to be later cut to obtain the bezel 1 according to the present invention, the carbon fibers are preferably wound perpendicularly at an angle of 90° to the longitudinal axis of symmetry of the tubular profile.
[0034] The material with a tubular profile, used in particular to make the bezel 1, typically contains 35% by weight PEEK polymer and 65% by weight carbon fiber (25-45% PEEK polymer and 55-75% carbon fiber) within a range of ±10%. It is therefore found that the elements of the outer part obtained from such a tubular profile contain a high content of carbon fiber, which significantly improves its thermal conductivity and makes it possible to quickly dissipate the heat that penetrates during the injection of the metallic glass. As a result, the bezel 1 does not decompose and does not become distorted, even though the temperature at which the metallic glass is injected is higher than the melting point of the polymer matrix. It is also noted that the reduction in the thickness of the injected insert, combined with the good thermal conductivity of the mould and the composite, allows a significant reduction in the exposure time of the polymer to temperatures above the melting point of the polymer. For this reason, it is not necessary to carry out special additional measures to limit the degradation of the polymer during the short contact with the metallic glass. Also, the visible parts of the composite that may have been in contact with the metallic glass are further removed in a surface finishing operation after removal from the mould.
[0035] The bezel 1 is formed with one or more cavities 4 in the top surface 2, typically formed by milling. According to the present invention, these cavities 4 are filled with a metallic glass type material to form inserts 6. As shown in FIG. 1, these inserts 6 represent numbers and indexes in shapes such as triangles and circles, but are not limited thereto. Preferably, these cavities 4 form an undercut angle α of 5-10° to ensure that the inserts 6 have good mechanical strength.
[0036] The metallic glass used to make the insert 6 is of the bulk metallic glass (BMG) type. Preferably, this metallic glass contains zirconium. For example, alloys containing zirconium, copper, titanium, nickel, aluminium and niobium, excluding unavoidable impurities, can be used. By way of example, the metallic glass used to make said insert contains these materials in the following amounts in weight %: 60≦Zr≦75, 10≦Cu≦20, 0≦Ti≦6, 7≦Ni≦15, 0≦Al≦8, 0≦Nb≦6.
[0037] Examples of metallic glasses containing zirconium that are suitable for the needs of the present invention include the alloys Vit106a, which has the composition, in weight percent, Zr70Cu13Ni9.9Al3.65Nb3.4, and Vit105, which has the composition, in weight percent, Zr65.7Cu15.6Ni11.7Al3.7Ti3.3.
[0038] The metallic glass used to make the insert 6 can also be based on platinum. For example, an alloy containing platinum, copper, nickel, aluminum and phosphorus, excluding unavoidable impurities, can be used. According to one embodiment, the metallic glass used to make the insert contains these materials in the following weight percents: Includes amounts of 80≦Pt≦90, 5≦Cu≦10, 1≦Ni≦3, 4≦P≦7.
[0039] In another particular embodiment of the invention, the metallic glass used to make the insert is given by the composition Pt85Cu7Ni2.3P5.7, in weight percent.
[0040] In another particular embodiment of the present invention, the metallic glass used to make the insert has a glass transition temperature of 350° C. or less.
[0041] According to the invention, the metallic glass is filled into the cavity 4 by injection to form the insert 6. For this purpose, an ingot of the metallic glass is prepared, placed in a melting chamber and heated to a temperature above its melting point. After the ingot of the metallic glass has melted, the metallic glass is injected into a mould in which the bezel 1 is placed, the mould being configured such that the metallic glass fills the cavity 4 of this bezel 1. Such injection of the metallic glass into the mould in which the bezel 1 is placed can be carried out by mechanical pressure provided by a piston or by gas pressure. The cavity 4 is preferably filled with a slight excess thickness of metallic glass to provide an optimum link between the bezel 1 and the insert 6.
[0042] After cooling of the metallic glass, the bezel 1 is removed from the mould and may undergo finishing operations such as removal of excess material, grinding and / or mechanical or chemical polishing. Any excess thickness or burrs are removed by trimming.
[0043] Naturally, the invention is not limited to the embodiments described herein, and various modifications and simple variations are conceivable by those skilled in the art without departing from the scope of the invention as defined by the appended claims. In particular, it is understood that within the scope of the invention, the metallic glass must be temporarily heated to its melting point in order to be able to be injected using an injection device. [Explanation of symbols]
[0044] 1 Bezel 2 Top side 4 Hollow part 6 Insert
Claims
1. An element or component of an external part for a timepiece or a piece of jewelry, made using a fiber-reinforced polymer matrix composite material obtained by dispersing fibers in a polymer matrix, comprising: the device includes at least one cavity (4) formed in at least one of the faces (2) for pouring a molten metallic glass therein, and an insert (6) in the form of a solid block in which the molten metallic glass solidifies within the cavity (4); the fiber reinforced polymer matrix composite material contains a quantity of the fibers having a predetermined thermal conductivity, so that when the metallic glass, which melts at a temperature higher than the melting point of the polymer material forming the polymer matrix, is injected into the cavity (4), the diffusion of heat through the fibers does not cause deformation of the elements or components of the external part, The polymeric material used to form the matrix is thermoplastic or thermosetting; the polymeric material is selected from the group consisting of polyetheretherketone (PEEK), polytetrafluoroethylene (PTFE), and polyamideimide (PAI); 10. An exterior part element or component, wherein the fibers reinforcing the polymer matrix are selected from the group consisting of glass fibers, carbon fibers, and aramid fibers.
2. The composite material comprises 35% PEEK polymer and 65% carbon fiber within a range of ±10%. An element of an outer part according to claim 1 .
3. The metallic glass used to make the insert is of the bulk metallic glass (BMG) type. An element or component of an external part according to claim 1 or 2.
4. The metallic glass used in the insert contains zirconium or platinum. An external part element or component according to claim 3.
5. The metallic glass used to make the insert is derived from an alloy of zirconium, copper, nickel, aluminum, niobium, and / or titanium, except for unavoidable impurities. An external part element or component according to claim 4.
6. The metallic glass used to make the insert contains zirconium, copper, titanium, nickel, aluminum and niobium in the following amounts by weight: 60≦Zr≦75, 10≦Cu≦20, 0≦Ti≦6, 7≦Ni≦15, 0≦Al≦8, 0≦Nb≦6. An external part element or component according to claim 5.
7. The metallic glass used to make the insert is an alloy having the composition Zr70Cu13Ni9.9Al3.65Nb3.4, or an alloy having the composition Zr65.7Cu15.6Ni11.7Al3.7Ti3.3, in weight percent. An external part element or component according to claim 6.
8. The metallic glass used to make the insert contains platinum, copper, nickel and phosphorus in the amounts, by weight percent, of 80≦Pt≦90, 5≦Cu≦10, 1≦Ni≦3, 4≦P≦7. An external part element or component according to claim 4.
9. The metallic glass used to make the insert has the composition, by weight, of Pt85Cu7Ni2.3P5.
7. An external part element or component according to claim 8.
10. The metallic glass used to make the insert has a glass transition temperature of 350°C or less. An external part element or component according to claim 3.
11. The outer part for a timepiece or jewelry is a back, a middle, a bezel (1), a bracelet link, or a clasp. An element or component of an external part according to claim 1 or 2.
12. A method for manufacturing an element or component of an external part according to claim 1 or 2, comprising the steps of: making an element or component of the exterior part using the fiber reinforced polymer matrix composite material obtained by dispersing the fibers in the polymer matrix formed from the polymer material; machining at least one of the faces (2) of the element or component of the external part to form the at least one recess (4); heating the metallic glass to its melting point; filling said at least one cavity (4) with said metallic glass to form said insert (6); and performing finishing operations as necessary; In the step of filling the at least one cavity (4) with the metallic glass to form the insert (6), the elements or components of the outer part are configured so that they are not deformed by the heat of the heated metallic glass being diffused through the fibers having a predetermined thermal conductivity and content. A method comprising:
13. The void portion is formed by milling.
13. The method of claim 12.
14. The finishing operation involves removing excess material, polishing, and / or trimming the insert (6).
14. The method of claim 13.
15. The recess (4) has an undercut angle (α) of 5 to 10°.
14. The method of claim 13.
Citation Information
Patent Citations
High-strength carbon fiber reinforced polyether-ether-ketone composite material and preparation method thereof
CN103374197A
Accessory and its manufacture
JP2000050923A
Package and sealing method therefor
JP2011108862A
Decorative parts made by inlay
JP2012502813A
Strong iron-based bulk metallic glass alloy
JP2012527541A
Cited By
External component element for timepiece or jewel, and method for manufacturing the same
JP2024174185A