Methods of forming paper products and paper products formed through the methods

By adding a glyoxalated polyvinylamide adduct to the diluted aqueous suspension post-high shear operation, the method improves dry strength in paper products while minimizing additive use, addressing the inefficiencies of conventional methods.

WO2026055418A1 Publication Date: 2026-03-12SOLENIS TECHNOLOGIES CAYMAN LP +1
7 Cites 0 Cited by

Patent Information

Application Number
PCT/US2025/045013
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2024-09-06
Filing Date
2025-09-05
Publication Date
2026-03-12

AI Technical Summary

Technical Problem

Existing papermaking processes using glyoxalated polyvinylamides as dry strength additives do not maximize dry strength, and these additives are expensive with limited shelf life, necessitating a more efficient method to enhance dry strength while minimizing their use.

Method used

Adding an aqueous composition comprising a glyoxalated polyvinylamide adduct to the diluted aqueous suspension after the last high shear operation and before the headbox, avoiding further high shear operations, to maximize dry strength and reduce additive usage.

Benefits of technology

The method achieves comparable or greater dry strength in paper products with reduced glyoxalated polyvinylamide usage, enhancing process efficiency and flexibility in additive addition points.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

Methods of forming paper products are provided herein. A method comprises providing an aqueous suspension of cellulosic fibers; diluting the aqueous suspension with water to form a diluted aqueous suspension having a solids content from about 0.3 wt% to about 1.8 wt%, based on a total weight of the diluted aqueous suspension; subjecting the diluted aqueous suspension to a high shear operation; adding an aqueous composition comprising an adduct formed from the reaction of glyoxal and a polyvinylamide prepolymer to the diluted aqueous suspension; forming the diluted aqueous suspension into a sheet; and drying the sheet. The aqueous composition is added after the diluted aqueous suspension is subjected to the high shear operation and before the diluted aqueous suspension is passed to a headbox. The method is free of any high shear operation after the aqueous composition is added and before the diluted aqueous suspension is passed to the headbox.