Beneficiation method for copper-sulfur ore containing pyrrhotite and pyrite
ZA202601601BActive Publication Date: 2026-10-28CENT SOUTH UNIV +1
0 Cites 0 Cited by
Patent Information
- Application Number
- ZA202601601
- Authority / Receiving Office
- ZA · ZA
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2026-02-06
- Publication Date
- 2026-10-28
- Estimated Expiration
- 2046-02-06
Abstract
The present invention discloses a beneficiation method for a copper-sulfur ore containing pyrrhotite and pyrite, comprising: adding lime to a run-of-mine copper-sulfur ore containing pyrrhotite and pyrite, adjusting pH to 9, grinding the run-of-mine ore to a particle size smaller than 250 mm, and performing a first rougher flotation on an overflow pulp after classification; performing a second rougher flotation on a first rougher tailing pulp; classifying a second rougher concentrate pulp; regrinding an underflow, and combining a regrinding discharge with the second rougher concentrate pulp for classification; performing a separation rougher flotation on a second rougher concentrate classification overflow pulp; combining a first rougher concentrate pulp with a separation rougher concentrate pulp, and performing a first column cleaner flotation and a second column cleaner flotation; performing a first separation scavenger flotation and a second separation scavenger flotation on a separation rougher tailing pulp. The process flow of the present invention is simple, easy to operate, energy-saving, environmentally friendly, and has good applicability. The beneficiation method processes a copper-sulfur ore containing pyrrhotite and pyrite, with a copper recovery rate of over ninety percent and a copper grade in the copper concentrate of over twenty percent.
Need to check novelty before this filing date? Find Prior Art