ULTRA-HIGH-STRENGTH CEMENT-BOUND COMPOSITE MATERIAL MADE FROM RIVER SEDIMENT SAND AND ITS MANUFACTURING PROCESS

BE1033498B1Active Publication Date: 2026-11-04ZHENGZHOU UNIV
1 Cites 0 Cited by

Patent Information

Application Number
BE2026007144
Authority / Receiving Office
BE · BE
Patent Type
Patents
Current Assignee / Owner
Filing Date
2026-03-18
Publication Date
2026-11-04
Estimated Expiration
2046-03-18
Patent Text Reader

Abstract

The present invention discloses an ultra-high-strength cementitious composite material made from river sediment sand and its manufacturing process, and belongs to the field of concrete technology. The manufacturing process comprises the following steps: drying and sieving the river sediment sand, producing an ultra-high-strength cementitious composite material by completely replacing quartz sand with the pretreated river sediment sand, and obtaining the ultra-high-strength cementitious composite material from river sediment sand.By drying and screening river sediment sand from the lower reaches of the Yellow River and subsequently completely replacing quartz sand in the production of the ultra-high-strength cementitious composite, the present invention effectively solves the problem of the need for large quantities of expensive natural quartz sand for the production of the ultra-high-strength cementitious composite, while simultaneously ensuring the ductility of the material. Furthermore, the present invention effectively contributes to reducing the large-scale silting of river sediment sand, protects the local environment, and enables the resource utilization of river waste.
Need to check novelty before this filing date? Find Prior Art

Description

2. Ordinary quartz sand costs around 300 yuan / ton, while refined quartz sand can cost up to 800 yuan / ton. These high costs hinder the large-scale production of UHTCC. Against this background, a process for the production of an ultra-high-strength cement-bound composite (UHTCC) is proposed, in which fluvial sediment sand is used instead of quartz sand as the fine aggregate, while maintaining the strength of the UHTCC. This production process is of great importance for the research, development, and application of cement-bound materials. CONTENT OF THE PRESENT INVENTION 10. To solve the aforementioned technical problems, the present invention proposes an ultra-high-strength cement-bound composite made of fluvial sediment sand,whose manufacturing process and application. By using dried river sediment sand instead of quartz sand, the weaknesses of existing technologies are overcome. While maintaining the same ductility of the ultra-high-strength cement-bound composite material, the required amount of quartz sand is significantly reduced, and at the same time the resource of the silted river sediment sand is utilized. Technical solution: The present invention relates to a process for producing an ultra-high-strength cement-bound composite material from river sediment sand,which includes the following steps: 20 (1) Drying of fluvial sediment sand; and (2) Producing an ultra-high-strength cement-bound composite by completely replacing quartz sand with fluvial sediment sand and maintaining the ultra-high-strength cement-bound composite from fluvial sediment sand. The present invention analyzes the material properties of the river sediment sand 25 from the lower reaches of the Yellow River and investigates the suitability of the river sediment sand as a replacement for quartz sand as a fine aggregate for UHTCC; after drying the river sediment sand, an ultra-high-strength cement-bound composite material is produced using a suitable shaping process, in which the quartz sand is completely replaced by river sediment sand. This results in the ultra-high-strength cement-bound composite material made from river sediment sand.and this opens up a new possibility for the use of river sediment sand. The specific method for analyzing the material properties of the river sediment sand is as follows: Taking 300g samples of sediment sand from the lower reaches of the Yellow River, drying in a drying oven until constant weight, and then sieving through 0.2mm and 0.075mm analytical sieves. The analysis shows that BE2026 / 7144 3 has a proportion of particles <0.075mm in a total weight of the river sediment sand from the sedimentation basin of 81.4%. An X-ray diffraction (XRD) analysis of the river sediment sand shows that the main components of the sediment sand in the sedimentation basin are 72.3% SiO2 and 10.6% Al2O3. Furthermore, the raw materials of the ultra-high-strength cement-bound composite material comprise, based on mass fractions, 100 parts fluvial sediment sand, 83.5 parts cement, 83.5 parts fly ash, 2.7 parts polyvinyl alcohol fibers (PVA fibers), 0.5 parts water reducing agent, 0.3 parts thickening agent and 58.6 parts water. Furthermore, the cement is ordinary Portland cement P·O42.5.10 Furthermore, the fly ash is Class II fly ash. Furthermore, the polyvinyl alcohol fiber is PVA fiber. Furthermore, the water reducing agent is a high-performance polycarboxylate water reducing agent; and the water reduction rate of the high-performance polycarboxylate water reducing agent is greater than 30%.15 Furthermore, the thickening agent is a hydroxypropyl methylcellulose of type HPMC-20 with a viscosity grade of 200,000. Furthermore, the shaping process is as follows: all powdered materials (cement, fly ash, water reducing agent and thickener) as well as the granular materials (river sediment sand and quartz sand) are placed in a mixer and dry-mixed for 2 to 20 minutes at a low speed of 108 rpm; then the water is added and mixed for a further 3 minutes at a low speed of 108 rpm.To ensure uniform mixing of all raw materials, the mixer continues to run at a low speed of 108 rpm while the PVA fibers are added evenly and slowly along the cylinder wall; this process takes approximately 3 minutes. After all PVA fibers have been added, the mixer speed is increased and set to a medium level of 188 rpm for 3 minutes. To ensure even distribution of the PVA fibers, the mixer speed is set to a high level of 403 rpm for 1 minute before the UHTCC mixture is dispensed. During casting, all samples are filled in two batches: first, material is poured to half the mold height, then the molds are held on a [unclear - possibly a pressure washer or similar device] for 1 minute. A vibrating table is used to compact the material. The material is compacted with a small tamping bar to reduce internal air bubbles; the cast samples are covered with a layer of cling film.To avoid moisture loss, after 24 to 48 hours of curing at room temperature, the samples are removed from the molds and stored in a standard climate-controlled room until testing. BE2026 / 7144 4 Technical Solution II of the present invention is an ultra-high-strength cement-bound composite material made of fluvial sediment sand, which is produced by the above-mentioned manufacturing process. Technical Solution III of the present invention is an application of the ultra-high-strength cement-bound composite material made of fluvial sediment sand in construction. 5 Compared to the prior art, the present invention offers the following advantages and technical effects. (1) Analysis of the material properties reveals that the particle size and composition of fluvial sediment sand and quartz sand are very similar. This suggests that fluvial sediment sand has the potential to replace quartz sand as a fine aggregate 10 for UHTCC. Furthermore, a suitable shaping process is applied,to ensure a uniform distribution of the extremely fine fluvial sediment sand and sufficient dispersion of the PVA fibers. The technical solution according to the invention establishes for the first time the use of fluvial sediment sand in ultra-high-strength cementitious composites. The ductility of the UHTCC produced from fluvial sediment sand is superior to that of the reference group UHTCC. (2) In river sediment sand, the proportion of particles with a grain size <75 μm is 81.4% of the total weight. According to the classification of sand and soil in engineering geology, this is to be called silt. River sediment sand has a very small grain size. Even when used as an aggregate in normal concrete, it may only be mixed with 20% river sand, whereby the proportion must not exceed 30%, otherwise the properties will be impaired. This invention provides for,to use river sediment sand as a complete replacement for fine aggregates in ultra-high-performance cement-bound composite materials. This enables the large-scale application of river sediment sand in concrete and maximizes its utilization. The technical solution of this 25 invention offers a new approach to the resource utilization of river sediment sand. (3) Quartz sand, a non-renewable natural aggregate, is becoming increasingly scarce. Conventional UHTCC uses expensive quartz sand as a fine aggregate, which leads to high production costs and limits its distribution. River sediment sand, on the other hand, is abundant and flows continuously from the middle and upper reaches of rivers with an average annual sand transport of 1.6 billion tons, making it suitable for long-term use. This invention utilizes river sediment sand as a replacement for 100% of the natural quartz sand. This saves 700 kg of quartz sand per 1 m³ of produced multi-high-strength cement-bonded composite.which significantly reduces production costs. This corresponds to the concepts of green, economic and sustainable development and promotes the regional dissemination and application of BE2026 / 7144 5 UHTCC. This technical solution addresses the two main problems of conventional UHTCC: the scarcity of quartz sand resources and the high production costs. (4) The ultra-high-strength cement-bonded composite material made from fluvial sediment sand (UHTCC made from fluvial sediment sand) produced according to the invention achieves a compressive strength of 26.4 MPa and a flexural strength of 11.5 MPa after 28 days of standard curing, which does not represent a significant deterioration compared to the reference group UHTCC. The maximum tensile strain of the UHTCC from river sediment reaches 3.71% and is therefore higher than that of the reference group UHTCC. Furthermore, it meets the requirement of 3% tensile strain for UHTCC, which indicates good hardening behavior. The maximum bending load and the maximum deflection are 5917.73 N and 4 N, respectively.05mm and thus 10 above the values ​​of reference group UHTCC. The equivalent bending strength is also higher than that of reference group UHTCC. This shows that the UHTCC from flow sediment sand has better deformation and energy absorption capacity compared to reference group UHTCC. The technical solution of this invention solves the problem of the insufficient bending and tensile strength of conventional cement-bound materials. (5) After complete replacement of quartz sand with river sediment sand as the fine aggregate of the UHTCC, scanning electron microscopy (SEM) shows that the river sediment sand has no negative effect on the microstructure of the UHTCC. The micromorphology of the UHTCC produced with river sediment sand is similar to that of the 20 reference group, and the fibers can be easily extracted. Mercury intrusion porosimetry (MIP) analysis shows that the pore structure parameters of the UHTCC produced with river sediment sand are comparable to those of the reference group. DESCRIPTION OF THE DRAWING 25 The attached drawings,The components of this invention serve to improve understanding of the present invention. The exemplary embodiments of the invention and their descriptions serve to explain the invention and do not constitute an inadmissible limitation of the invention. In the drawings: Fig. 1 shows a dimensioned drawing of a uniaxial tensile specimen of the present invention; Fig. 2 shows a stress-strain curve of UHTCC produced in embodiment 1 from flow sediment and in a uniaxial tensile test; Fig. 3 shows a photograph of the fracture morphology of a UHTCC specimen produced in embodiment 1 from flow sediment and in a uniaxial tensile test; Fig. 4 shows a bending strength-deflection curve of UHTCC from flow sediment and produced in embodiment 1; BE2026 / 7144 6 Fig. 5 shows matrix SEM images of UHTCC from flow sediment sand produced in formulation 1 and of the reference UHTCC; where (a) is the reference group and (b) is the substitution group for flow sediment sand; Fig. 6 shows SEM images of the fibers of UHTCC from flow sediment sand,which is produced in embodiment 1, and the reference UHTCC; wherein (a) the reference group-5 and (b) the substitution group for flow sediment sand; and Fig. 7 shows pore size distribution curves of the UHTCC from flow sediment sand produced in embodiment 1, and the reference UHTCC. DETAILED DESCRIPTION 10 Various exemplary embodiments of the present invention are now described in detail, which are not to be regarded as limitations of the present invention, but are to be understood as more detailed descriptions of certain aspects, features and embodiments of the present invention. It is to be understood that the terms described in the present invention 15 serve to describe specific embodiments,and not to be used to limit the present invention. In addition, the value ranges specified in the present invention shall be understood as the specific disclosure of each intermediate value between the upper and lower limits of this range. Each smaller range between each specified value or range of statements and each other specified value or intermediate value within the range is also contained in the present invention. The upper and lower limits of these smaller ranges can be included or excluded from the range independently of each other. Unless otherwise specified, all technical and scientific terms used herein have the same meaning as they are generally understood by experts in the field of the present invention. While the present invention describes only preferred methods and materials, any method and material similar or equivalent to those described herein may be incorporated herein.also in the performance or testing of the present invention. All documents mentioned in this description alone are incorporated by reference to disclose and describe methods and / or materials relating to those documents. In the event of any conflict with any of the incorporated documents, the contents of this specification shall prevail. Various modifications and variations may be made to the specific embodiment of the present invention without departing from the scope or spirit of the disclosure contained in BE 2026 / 7144 7, which is obvious to persons skilled in the art. Other embodiments obtained from the description of the present invention are also obvious to persons skilled in the art. The descriptions and embodiments of the present invention are only examples. As used herein, “including”, “comprise”, “exhibit”, “contain” and the like are all open terms, i.e. the meaning “including”,but not “limited to”. Unless otherwise specified, the term “parts” in this invention refers to parts by weight. The specific experiments described in this invention are as follows: 10 (1) Flexural strength test The flexural strength test is to be carried out in accordance with the standard "Test method for the strength of cement mortar" (GB / T17671-2021). The loading is carried out with an integrated flexural and compressive strength testing machine for cement from the company Jinan Tianchen. The specimens have the dimensions of a cuboid of 160 mm × 40 mm × 40 mm, with three specimens being tested per group. During the loading, the mold surface of the specimens faces outwards, the loading rate is (50 ± 10) N / s. The flexural strength is calculated according to formula (1). 3b L1.5F R ff= (1), in formula(1):Rf—flexural strength of UHTCC (MPa);20 Ff—breaking load (N); L—distance between the two support points (mm), here 100mm; b—the side length (mm) of the square cross-section of the prism,Here, 40 mm. The mean value of the bending strength test on a group of three prisms is used as the test result. If one of the three strength values ​​exceeds the mean value by 25 ± 10%, it is discarded and the mean of the remaining values ​​is used as the bending strength test result. If two of the three strength values ​​exceed the mean value by ± 10%, the remaining single value is used as the bending strength result. (2) Compressive Strength Testing The compressive strength test is carried out in accordance with the standard "Test methods for the strength of cement mortars" (GB / T17671-2021). The test is carried out using an integrated bending and compression testing machine for cement from the company Jinan Tianchen. The compressive strength specimens are half-prisms after failure in the bending strength test. Each group comprises six specimens, with the compression area being selected as the side face. BE2026 / 7144 8 The compression area is 40 mm × 40 mm. The loading rate is (2400 ± 200) N / s. The compressive strength is calculated according to formula (2). AN fu m.cu = (2),in Formula(2): fm.cu—compressive strength of UHTCC (MPa); Nu—maximum load (N); 5 A—the bearing area of ​​the sample, here 1600 mm². The test result is the mean of six compressive strength measurements taken on a group of three prisms. If any one of the six measurements exceeds the mean by ±10%, this result is discarded, and the mean of the remaining five measurements is considered the result. If any one of the five measurements also exceeds the mean by ±10%, the entire data set is invalid. If two or more of the six measurements simultaneously exceed the mean by ±10%, the entire data set is invalid. (3) Uniaxial tensile test The test shall be carried out in accordance with the reference standard “Test methods for the mechanical properties of high ductility fiber reinforced cement-bonded materials” (JC / T2461-15 2018). The uniaxial tensile test shall be carried out on a microcomputer-controlled electronic universal testing machine WDW-20.which is connected to a static stress-strain testing and analysis system. For the tensile test, a tensile specimen in the shape of a dog bone is used, and the dimensions of the specimen are given in Fig. 1. The specimen is secured in a special clamping device, and a removable linear variable differential transformer (LVDT) is attached to the left and right as a displacement sensor. After data acquisition, the mean of the two measured values ​​is used as the final displacement. A force transducer is attached to the connection between the clamping device and the universal testing machine. The displacement and force transducers are connected to the stress-strain testing and analysis system. The load bar of the testing machine is slowly lowered to clamp the specimen stably before loading and data acquisition. The loading is displacement-controlled with a loading speed of 0,5 mm / min. During the loading process, attention is paid to the general trend change of the force-displacement curve as well as to crack formation on the specimen surface. When the load value decreases significantly and the force-displacement curve shows a clear downward trend, the loading is stopped, the data is saved, and the machine is returned. The uniaxial tensile strength index of the UHPC specimen is calculated according to formulas (3)–(5). The tensile strength of the initial crack is calculated according to formula (3): BE2026 / 7144 9 AF σfc fc = (3), where: σfc—tensile strength of the initial crack (MPa); Ffc—the maximum tensile force (N) at the inflection point during the stress increase in the stress-strain curve. A—initial cross-sectional area (mm²) of the measuring range of the specimen's deformation. 5 The tensile strength is calculated according to formula (4): AF σ tu tu = (4), where: σtu—tensile strength (MPa); Ftu—the maximum tensile force (N) that the specimen can withstand; A—initial cross-sectional area (mm²) of the measuring range of the specimen's deformation. 10 The maximum tensile strain is calculated according to formula (5): tg 0tu tu L ll ε = (5),where:εtu—the maximum tensile strain (%); ltu—the mean value (mm) of the displacement sensors on both sides when the specimen reaches its maximum tensile stress; L0—the initial mean value (mm) of the displacement sensors on both sides; Ltg—the measured reference length (mm) of the displacement sensor, here 80 mm. (4) Four-point bending test. The four-point bending test is based on the standard "Technical specification for the application of high-ductility concrete" (DBJ61 / T112-2021). The loading is carried out using a microcomputer-controlled electronic universal testing machine of type WDW-20. For the four-point bending test, rectangular specimens with dimensions of 160 mm × 40 mm × 40 mm are used, with three specimens tested per group. A computer-connected dial gauge is mounted in the middle of the span below the specimen, and the loading is applied in a displacement-controlled manner at a loading rate of 0.2 mm / min. If the specimens have been post-treated up to the test point, they are removed from the curing room, whereby the surface moisture must be wiped off to ensure thatthat the loading surface is flat, clean, and free of defects. During the loading process, the phenomena are to be observed in a timely manner and the data recorded on 30. As soon as the load drops to 0.85 times the maximum load, the loading is stopped, the data are recorded again, and the load-deflection curve is generated. Subsequently, the initial crack load, the initial crack deflection, the maximum bending load, and the maximum bending deflection can be further analyzed. The equivalent bending strength is calculated using the following formula (6). u 2 uu eq δbh LΩ f= (6),5 where: u eqf —equivalent bending strength (N / mm2, to within 0.1 N / mm2); Ωu —area (N·mm) under the load-deflection curve when the deflection at the midpoint of the span is δu; δu —the deflection value (mm) corresponding to the load falling to δu times the peak load, where δu is assumed to be 0.85;10 b,h – the width and height (mm) of the cross-section of the sample; L – the span of the sample (mm). (5) Microscopic Experiments Scanning electron microscopy (SEM) is performed on the fractured UHTCC samples from flow sediment sand to analyze their microstructure. Before the examination, the samples are dried for one hour at 50°C in a vacuum drying oven to prevent reactions of the samples with moisture and carbon dioxide in the air. The SEM examination is carried out with a high-resolution cold-field emission scanning electron microscope (MPEM) of the type Hitachi S-4800, manufactured by Hitachi, Ltd., Japan, and the samples are magnified up to 50,000x. Mercury intrusion porosimetry (MIP) is performed on samples from the UHTCC matrix using a fully automated mercury porosimetry instrument of the type Autopo- reIV9500 from Micromeritics, USA,The experiment was carried out. Before the experiment, the samples, with a side length of approximately 10 mm, were dried for 24 hours at 50°C in a vacuum drying oven and then immediately sealed. The pore structure of the UHTCC-25 matrix was analyzed using MIP analysis, and its porosity, mean pore size, and the proportion of different pore sizes were determined. The mechanism of action of flow sediment and cement-bound materials was investigated from the perspective of the micropores. The preparation of the test specimens according to the present invention is carried out in detail as follows: (1) Stirring. In the preparation of the UHTCC, a planetary mixer was used, the mixing sequence being as follows: BE2026 / 7144 11 ① first, the mixing trough and the mixing blades of the mixer are moistened with water, taking care that the inner wall is moist, but no flowing water escapes; ② all powdered materials (cement, fly ash, water reducing agent, thickener) and granular materials (river sediment sand,Quartz sand) are placed in a mixer and mixed dry for 2 minutes at a low speed of 108 rpm; ③ the water is added to the mixer and mixed further for 3 minutes at 108 rpm; ④ The mixer continues to run at a speed of 108 rpm; after the mixture 10 is evenly mixed, the PVA fiber is added evenly and slowly, and the entire process takes no longer than 3 minutes; and ⑤ After all the PVA fibers have been added to the mixer, the speed of the mixer is increased to a medium speed of 188 rpm for 3 minutes to ensure an even distribution of the PVA fibers; the speed of the mixer is then set to a high speed of 403 rpm for 1 minute 15 before the UHTCCC mixture is removed from the container. (2) Molding After completion of the mixing process, the samples are cast. All samples are filled in two layers. First, the mixture is filled to half the mold height and then compacted for one minute on a vibrating table. During the vibration, the mixture is further compacted with a small tamping bar.to reduce internal air bubbles. The second filling is carried out using the same procedure. For surface treatment, the surface of the samples is smoothed with a moistened trowel, excess mixture is scraped off, and the surface is covered with PE cling film to prevent moisture evaporation. The samples are then stored at a room temperature of 20 ± 5°C. The dimensions of the samples for the flexural strength test are 160 × 40 × 40 mm, with three samples used per group. For the compressive strength test, half of the samples broken in the flexural test are used, with six pieces per group being examined. The 30 Samples for the four-point bending test have dimensions of 160 × 40 × 40 mm, with three samples used per group. (3) Curing After demolding the samples, which have been left to rest indoors for 1–2 days at a relative humidity above 50% and a temperature of 20 ± 5°C,wer-35 BE2026 / 7144 12 densie 28 days in a curing chamber with constant temperature and humidity (set temperature 20±1°C, humidity ≥95%). Example 1: Production of an ultra-high-strength cement-bound composite from river sediment sand. To produce an ultra-high-strength cement-bound composite from river sediment sand, i.e., UHTCC from riverbed sediment sand (group: R), quartz sand is substituted with completely dried river sediment. The mixture composition is shown in Table 1. A reference group is established, i.e., Reference UHTCC (Group B). The only difference between the reference group and the group with the ultra-high-strength 10 cement-bound composite material made of flow sediment sand is thatthat the addition of fluvial sediment sand is omitted. The mixture composition is shown in Table 1. Table 1. Mixture composition of the ultra-high-strength cement-bound composite material made of fluvial sediment sand (kg / m³) Group Flux sediment sand Quartz sand Cement Fly ash PVA fiber Water reducing agent Thickening agent Water B0700585585193.51.8410 R7000585585193.51.8410 The fluvial sediment sand used in Table 1 is dried fluvial sediment sand. The quartz sand is 80-120 mesh quartz sand, supplied by Henan Zhongbang Environmental Protection Technology Co., Ltd. The cement is ordinary Portland cement 20 P·O42.5, manufactured by Zhengzhou Cement Co., Ltd. of the Tianrui Group (Henan). All fly ash is Class II fly ash. The PVA fibers are polyvinyl alcohol fibers from Kuraray Co., Ltd., Japan, with a diameter of 40 μm.a length of 12 mm and a tensile strength of 1560 MPa. The water reducing agent is a highly efficient polycarboxylate water reducing agent with a water reduction rate of over 25-30%. The thickening agent is hydroxypropyl methylcellulose of type HPMC-20, manufactured by Shanghai Chenqi Chemical Technology Co., Ltd., with a viscosity class of 200,000. The water used is clean, uncontaminated normal tap water. The performance of the two groups of ultra-high-performance cement-bonded composites from embodiment 1 is tested, and the results are as follows: BE2026 / 7144 13 (1) Flexural strength test. The results of the compressive strength test of the two groups of UHTCC are shown in Table 2. Table 2 Results of the bending strength test 5 Group Replacement rate of flow sediment sand / % Mean bending strength / MPa B0 12.2 R100 11.5 As shown in Table 2, the bending strength of the UHTCC produced from flow sediment sand reaches 11.5 MPa after three days of steam curing.after the quartz sand has been completely replaced by fluvial sediment. Compared to Group B, the compressive strength of Group R decreases by only 6.25%. 10 (2) Compressive strength test The results of the compressive strength test of the two groups of UHTCC are shown in Table 3. Table 3 Results of the compressive strength test 15 Group Replacement rate of flow sediment sand / % Mean compressive strength / MPa B0 27.4 R10 26.4 As shown in Table 3, the compressive strength of the UHTCC decreases after the quartz sand has been completely replaced by flow sediment sand. After 28 days of standard hardening, the compressive strength of the UHTCC from flow sediment sand reaches 26.4 MPa. Compared to Group B, the compressive strength of Group R decreases by only 6.25%. 20 (3) Uniaxial tensile test A typical stress-strain curve of the UHTCC from flow sediment sand in the tensile test is shown in Fig. 2. 1) Elastic phase: before reaching the load of the initial crack, there is a linear relationship between stress and strain,and the stress-strain curve is approximately linear. In this phase, the 25 specimen undergoes elastic deformation, with the stress inside the specimen being mainly carried by the matrix. The point at the end of the elastic phase is defined as the point of initiation of the crack; the associated stress is the initiation crack strength σfc, and the associated strain is the initiation crack strain εfc. 2) Strain- BE2026 / 7144 14 Strengthening phase: after the strain of the specimen has exceeded the elastic limit strain, the stresses inside the specimen show slight fluctuations. With further increasing strain, the PVA fibers inside the specimen act as bridges, and the Internal stress gradually increases with a continuous stress distribution. At this point, the cracks on the sample surface become increasingly visible, and the internal stress is jointly carried by the PVA fibers and the matrix. The stress at the highest point of the “peak” on the right side of this phase corresponds to the tensile strength σtu.and the associated strain of the maximum tensile strain is εtu. 3) Strain-softening phase: After exceeding the tensile strain, the stress gradually decreases with increasing strain. The stress-strain curve 10 exhibits a sawtooth pattern, which indicates continuous sliding of PVA fibers. The inner cracks of the sample widths develop continuously and form a continuous main crack, which leads to a loss of load-bearing capacity, and the test is terminated. Even after the first crack formation in the specimen, the load can still increase to approximately twice the load of the initial crack, which shows that the material retains good load-bearing capacity even after the first crack formation. After the specimen breaks, numerous fine cracks appear, resulting in multiple crack formation.and the fracture form is shown in Fig. 3. The calculation results for the relevant uniaxial tensile properties of the two sample groups UHTCC from flow sediment sand and reference UHTCC are shown in Table 420. Table 4: Uniaxial tensile properties of the two sample groups Group Tensile strength of the initial crack σfc / MPa Tensile strain of the initial crack εfc / % Maximum tensile strength σtu / MPa Maximum tensile strain εtu / % B 0.48 0.05 1.60 3.20 R 0.47 0.02 1.83 3.71 As shown in Table 4, the UHTCC from flow sediment sand exhibits good uniaxial tensile properties. The tensile strength of the initial crack is close to that of the reference UHTCC, while both the maximum tensile strength and the maximum tensile strain are better than those of the reference UHTCC. This proves,that the replacement of natural quartz sand with fluvial sediment sand in the production of UHTCC effectively optimizes its axial tensile strength. 30 (4) Four-point bending test BE2026 / 7144 15 A load-deflection curve of the UHTCC made from fluvial sediment sand in the bending strength test is shown in Fig. 4. This curve can be divided into three phases: 1) Elastic phase. From the beginning of loading the specimen until the occurrence of the first crack. In this phase, the matrix of the UHTCC made from fluvial sediment sand and the fibers share the external load, with the matrix bearing the largest part of the load. The load-load-deflection curve increases approximately linearly. The point at the end of the elastic phase is defined as the point of the initial crack. The associated load is the initial crack load Ffc and the associated strain is the initial crack deflection δfc. 2) Strain-strengthening phase. From the appearance of the first crack on the specimen until the cracks are uniformly distributed and the point,and the number of cracks no longer increases.10 In this phase, the rise of the bending load-deflection curve slows down and exhibits a wave-like pattern. The number of waves corresponds to the number of cracks that have formed in the bending range of the specimen. The highest point of the peak on the right side of this phase represents the maximum bending load Ftu, and the associated strain is the maximum deflection δtu.3) Strain-softening phase. From the point at which the cracks15 are uniformly distributed and their number no longer increases, the weakest crack opens further and connects with neighboring cracks to form a principal crack, which leads to the failure of the specimen. During this phase, the bending load decreases continuously with increasing deflection in the middle of the span,and the curve is downward sloping. Calculation results of the four-point bending performance index of the two sample groups UHTCC from fluvial sediment sand and reference UHTCC are shown in Table 5. Table 5: Calculation results of the four-point bending performance index of the two sample groups. Group Initial crack load Ffc / N Initial crack deflection δfc / mm Maximum bending load Ftu / N Maximum bending deflection δtu / mm Equivalent bending strength fe / MPa B3 133.13 0.01 55 96.8 13.7 11 1.22 R2 86 7.15 0.02 59 17.7 34.0 51 2.27 As shown in Table 5, the initial crack load and initial crack deflection of the UHTCC from flow sediment sand are lower than those of the reference UHTCC. The initial crack load and initial crack deflection are mainly due to the matrix bears the load. The reduced compressive strength indicates that the matrix strength of the UHTCC from fluvial sediment sand is lower than that of the reference UHTCC. However, the maximum bending load and the maximum bending deflection of group R are increased.which suggests that the maximum load-bearing capacity of the UHTCC from flow sediment sand is better than that of the reference UHTCC. Furthermore, the equivalent flexural strength of the UHTCC from flow sediment sand in Group Rim is higher than that of the reference UHTCC compared to Group B. 5 (5) Microscopic Experiments Fig. 5 shows the microstructure of the matrix for UHTCC from flow sediment sand and reference group UHTCC, where (a) the reference group UHTCC and (b) the UHTCC from flow sediment sand are shown. The left image shows a denser microstructure due to the higher density of the C-SH gel formed, which has a dense solid state with fewer pore-10 structures. In the right image, a greater amount of finer-grained C-SH- A gel with lower density is formed. CSH gel contributes significantly to the strength of cement-bound materials; this corresponds to the results of macroscopic mechanical tests.The compressive strength of UHTCC from flow sediment sand is lower than that of reference group UHTCC. Figure 6 shows the fiber pull-out behavior of UHTCC from flow sediment sand and reference group UHTCC, where (a) reference group UHTCC, (b) UHTCC from flow sediment sand. It is evident that the integrity of UHTCC from flow sediment sand and reference group UHTCC is good after fiber pull-out, with only some minor cracks appearing. This indicates that the chemical bond strength between matrix and fiber is sufficient during fiber detachment in the matrix and that the fiber pull-out process proceeds smoothly. Macroscopically, both groups exhibit a maximum tensile strain of over 3%. The pore size distribution curves of the two groups of UHTCC samples are shown in Fig. 7, and the pore structure parameters of the two groups of samples are listed in Table 25. Table 6: Pore structure parameters of the two sample groups. Group: Porosity (%), Average pore size (nm), Distribution range of pore size: 3 nm to 50 nm, 50–1000 nm, >1000 nm. B: 29.00360327%45%28% R30.0633.3126%50%24% Wiei,

Citation Information

Patent Citations

  • Yellow river sand ultra-high toughness cement-based composite material as well as preparation method and application thereof