A high temperature tensile test device with atmosphere protection
By designing a high-temperature tensile test device with atmosphere protection, using sealed heating chamber and water circulation cooling system, the problems of low efficiency and sample oxidation in the existing technology are solved, and the oxidation-free high-temperature tensile test device and rapid cooling are achieved , provides detailed observation and analysis of the high-temperature fracture process of the material.
Patent Information
- Application Number
- CN201911139747.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2019-11-20
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2039-11-20
AI Technical Summary
When the existing high-temperature tensile testing device detects high-temperature tensile performance, the refractory bricks are prone to burst, resulting in damage to the heating furnace and low detection efficiency. The oxidation of the sample surface and long-term cooling affect the observation of the material's high-temperature fracture process and the acquisition of fracture information. .
A high-temperature tensile test device for atmosphere protection is designed, including a sealed heating chamber, heating system, water circulation cooling system, atmosphere protection system, optical microscope observation system and transmission control system. It adopts a short-wave infrared heating tube and water circulation cooling design, through Vacuum exhaust and fill the protective gas to achieve high-temperature stretching and rapid cooling of the sample without oxidation.
The high-temperature tensile test of the sample without oxidation is realized, which significantly shortens the experimental cycle and provides a platform for studying the high-temperature fracture of the material, which can accurately observe and analyze the fracture morphology and tissue information.
Smart Images

Figure CN110879180B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of material performance testing, in particular to an atmosphere-protected high-temperature tensile testing device. Background Art
[0002] At present, the high-temperature tensile performance of materials is mostly tested by installing a split-type resistance furnace on a room-temperature tensile machine. A large number of refractory bricks are built into the resistance furnace. If the heating furnace is opened directly after high-temperature stretching, the refractory bricks will be broken and the heating furnace will be damaged. Therefore, after stretching, the furnace body must be opened and the sample can be taken out only after the temperature in the furnace drops to a certain temperature. Due to the large furnace body and low heating and heat dissipation efficiency, the high-temperature tensile test process often takes 5 minutes, and the temperature rises and falls for 3 hours, and the detection efficiency is extremely low. In addition, the furnace body has no sealing design, so the surface of the sample is inevitably oxidized during the stretching process. From the research point of view, after stretching, it is affected by the surface oxidation and the tissue recovery process during the long cooling process. It is not only difficult to observe the high-temperature fracture process of the material, but also impossible to accurately extract the sample fracture and post-fracture tissue information, which is not conducive to the theoretical study of the high-temperature fracture process of the material. Based on the above test conditions, the invention of a high-temperature tensile test device that can achieve atmosphere protection and efficient temperature control has significant market prospects and research value. Summary of the invention
[0003] The technical problem to be solved by the present invention is to provide an atmosphere-protected high-temperature tensile test device, which is mainly composed of a sealed heating cabin, a heating system, a water circulation cooling system, an atmosphere protection system, an optical microscopic observation system, and a transmission control system. With the help of the optical microscopic observation system, the fracture process characterization of the material in the non-oxidized state during the high-temperature tensile process can be achieved. In addition, the realization of rapid cooling of the sample under atmosphere protection is more conducive to the observation and analysis of the fracture morphology and organization of the sample.
[0004] Specifically, the device includes a heating cabin, a heating system, a water circulation cooling system, an atmosphere protection system, an optical microscopic observation system and a transmission control system. The heating cabin is designed with an embedded water circulation cooling system; the heating system adopts a short-wave infrared heating tube, which is connected to the heating cabin; the atmosphere protection system is achieved by evacuating the sealed heating cabin and then filling it with protective gas; a high-temperature observation window is set on the heating cabin cover on the side of the heating cabin, and the optical microscopic observation system is connected through the high-temperature observation window; the transmission control system includes a moving beam, a bidirectional ball screw and a stretching shaft, the heating cabin is located in the middle of a stretching frame composed of a moving beam and two bidirectional ball screws, and the heating cabin is fixed to the moving beam through the stretching shaft.
[0005] Among them, the heating chamber is made of heat-resistant alloy, adopts reflective focusing heating design internally, cooling water pipeline is designed inside the heating chamber shell, and thermocouple is installed at the interface between the heating chamber and the external seal for temperature protection.
[0006] The heating chamber is a box structure with two cooling plates welded on the upper and lower parts respectively. A high-temperature extensometer sealing box is installed on one side of the heating chamber. A water outlet and a water inlet are arranged on the side opposite to the heating chamber cover. The interior of the heating chamber is a double elliptical reflective section. The two elliptical sections share a focus, and the tensile specimen is located at the focus. The short-wave infrared heating tube is installed at the other two foci of the two ellipses. According to the geometric characteristics of the ellipse, the infrared waves radiated from the heating tube can converge to the specimen, which significantly improves the heating efficiency.
[0007] The heating chamber and the stretching shaft are connected through a sealing sleeve, and a sealing ring inner groove is processed inside the sealing sleeve.
[0008] The high temperature extensometer sealing box is fixed on the heating chamber by bolt 2, and the quartz pin of the extensometer in the high temperature extensometer sealing box is inserted into the heating chamber through the extensometer slot and contacts the tensile specimen.
[0009] The heating cabin cover is fixed on the heating cabin by bolts, and a high-temperature sealing ring is placed in a sealing ring groove at a high-temperature observation window on the heating cabin cover.
[0010] External connection holes, heating pipe jacks, cooling water sealing ports and stretching shaft holes are processed on the cooling plate, and the sealing parts are connected to the external connection holes through high-temperature sealing rings and bolts.
[0011] The two ends of the bidirectional ball screw are respectively machined with forward threads and reverse threads.
[0012] In this device, the transmission control system consists of a stretching frame and a control system. The stretching frame is designed to be vertical, and the motor is located at the bottom of the frame and transmits the movement to the upper and lower beams through two bidirectional ball screws. Since the threads on both sides of the bidirectional ball screws are in opposite directions, the upper and lower beams drive the stretching axis to move in opposite directions at the same time. Different from the single-sided fixed feature of traditional stretching equipment, this design can ensure that the center position of the sample remains unchanged during the stretching process, achieving the effect of in-situ stretching.
[0013] The heating chamber body and the upper and lower cooling plates are internally processed with cooling water pipelines, which are welded together to form a complete circulating water circuit. During the heating process of the chamber, the external circulating water pump cools the heating chamber through the circulating water circuit of the heating chamber. A high-temperature observation window is designed on the heating chamber cover, which is composed of high-temperature resistant glass, high-temperature sealing ring and pressing sheet. Combined with an external optical microscopic observation system, real-time monitoring of the fracture process of the sample during high-temperature deformation can be achieved.
[0014] The heating chamber and its upper and lower cooling plates are fixed with tensile sleeves, high-temperature extensometer sleeves, and sealing interfaces for connecting thermocouples, barometers, protective gas pipelines, and vacuum pump pipelines. The sealing interfaces are connected to the heating chamber through high-temperature sealing rings and fastening bolts. Under high-temperature conditions, the temperature of the heating chamber is adjusted to be below the allowable temperature (220°C) of each high-temperature sealing ring through a cooling water pump.
[0015] The beneficial effects of the above technical solution of the present invention are as follows:
[0016] In the above scheme, high-temperature tensile testing of samples without oxidation can be realized, providing a research platform for high-temperature fracture analysis of materials; in addition, due to the design of its efficient heating and cooling system, the high-temperature tensile test cycle of materials can be significantly shortened. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 It is a schematic structural diagram of the atmosphere-protected high-temperature tensile testing device of the present invention;
[0018] Figure 2 The double elliptical cross-section cavity structure of the heating chamber in the atmosphere-protected high-temperature tensile testing device of the present invention;
[0019] Figure 3 The upper and lower cooling plates of the heating chamber in the atmosphere-protected high-temperature tensile test device of the present invention and its external accessories;
[0020] Figure 4 A schematic diagram of the internal water circulation path of the atmosphere-protected high-temperature tensile testing device of the present invention;
[0021] Figure 5 This is the 650°C surface oxidation-free stretching result achieved in Example 1 of the present invention.
[0022] Among them: 1-heating chamber; 2-moving crossbeam; 3-bidirectional ball screw; 4-forward thread; 5-reverse thread; 6-stretching shaft; 7-high temperature extensometer sealing box; 8-high temperature observation window; 9-short wave infrared heating tube; 10-seal; 11-sealing sleeve; 12-double elliptical reflection section; 13-cooling water pipeline; 14-extensometer slot; 15-sealing ring groove; 16-bolt one; 17-bolt two; 18-seal ring inner groove; 19-external connection hole; 20-cooling plate; 21-heating tube socket; 22-cooling water sealing port; 23-stretching shaft hole; 24-water outlet; 25-water inlet. DETAILED DESCRIPTION
[0023] In order to make the technical problems, technical solutions and advantages to be solved by the present invention more clear, a detailed description will be given below with reference to the accompanying drawings and specific embodiments.
[0024] The invention provides an atmosphere-protected high-temperature tensile testing device.
[0025] like Figure 1As shown, the device includes a heating chamber 1, a heating system, a water circulation cooling system, an atmosphere protection system, an optical microscopic observation system and a transmission control system. The heating chamber 1 is designed with an embedded water circulation cooling system; the heating system uses a short-wave infrared heating tube 9, which is connected to the heating chamber 1; the atmosphere protection system is realized by evacuating the sealed heating chamber 1 and then filling it with protective gas; a high-temperature observation window 8 is set on the heating chamber cover on the side of the heating chamber 1, and the optical microscopic observation system is connected through the high-temperature observation window 8; the transmission control system includes a moving beam 2, a bidirectional ball screw 3 and a stretching shaft 6. The heating chamber 1 is located in the middle of the stretching frame composed of the moving beam 2 and two bidirectional ball screws 3, and the heating chamber 1 is fixed to the moving beam 2 through the stretching shaft 6. The two ends of the bidirectional ball screw 3 are respectively processed with a forward thread 4 and a reverse thread 5. When the bidirectional ball screw 3 is driven by an external motor to rotate, the moving beams 2 on both sides will drive the stretching shaft 6 fixed thereon to move symmetrically in the upward and downward directions, respectively, thereby realizing the in-situ stretching of the sample, that is, the center of the sample remains unchanged during the stretching process.
[0026] The heating chamber 1 is made of a heat-resistant alloy and adopts a reflective focusing heating design internally. A cooling water pipeline 13 is designed inside the shell of the heating chamber 1. A thermocouple is installed at the interface between the heating chamber 1 and the external seal 10 for temperature protection.
[0027] like Figure 2 As shown, the heating chamber 1 is a box structure, with two cooling plates 20 welded on the upper and lower parts respectively, and a high-temperature extensometer sealing box 7 is installed on one side of the heating chamber 1; a water outlet 24 and a water inlet 25 are arranged on the side opposite to the heating chamber cover; the interior of the heating chamber 1 is a double elliptical reflective section 12, the two elliptical sections share a focus, the tensile specimen is located at the focus, and the short-wave infrared heating tube 9 is installed at the other two foci of the two ellipses.
[0028] The heating chamber 1 and the stretching shaft 6 are connected by a sealing sleeve 11, and a sealing ring inner groove 18 is processed inside the sealing sleeve 11. High temperature resistant sealing rings are used to seal between the connecting parts to ensure that the entire chamber can reach a vacuum degree of 10 -3 -10 - 5 Pa.
[0029] The high temperature extensometer sealing box 7 is fixed on the heating chamber 1 by bolts 17, and the quartz pins of the extensometer in the high temperature extensometer sealing box 7 are inserted into the heating chamber 1 through the extensometer slot 14 and contact the tensile specimen.
[0030] The heating cabin cover is fixed to the heating cabin 1 by bolts 16, and a high-temperature sealing ring is placed in the sealing ring groove 15 at the high-temperature observation window 8 on the heating cabin cover.
[0031] like Figure 3As shown, the cooling plate 20 is processed with an external hole 19, a heating pipe insertion hole 21, a cooling water sealing port 22 and a stretching shaft hole 23, and the sealing member 10 is connected to the external hole 19 through a high-temperature sealing ring and bolts.
[0032] The water circulation path of the heating chamber 1 is as follows Figure 4 As shown, cooling water flows in from the water inlet 25, and flows out through the water outlet 24 after circulation as shown by the arrow. The cooling water is provided by an external circulating water pump, and the flow rate and water temperature can be adjusted according to the temperature of the heating chamber to ensure that each component is within the safe temperature for use.
[0033] When the device is used, during the atmosphere protection high temperature stretching process, first fix the polished plate sample in the chuck with a slot through a pin. The chuck is replaceable and fixed to the stretching shaft through a thread. After the sample is clamped, fix the quartz pin of the high temperature extensometer to the parallel section of the sample according to its default gauge length, then cover the heating chamber cover and ensure that the protective gas switch is turned off. Turn on the vacuum exhaust interface switch, and evacuate the sealed heating chamber through an external molecular pump at room temperature until the air pressure in the chamber reaches 10 -3 ~10 -5 After reaching Pa, close the vacuum exhaust interface switch, open the protective gas switch to fill the heating chamber with protective gas, read the pressure inside the chamber through the barometer installed on the sealed interface, adjust the protective gas switch after it is higher than the ambient pressure, and allow the protective gas to slowly escape from the one-way gas valve connected to the other sealed interface. At this point, the heating chamber is filled with protective gas, and the slightly higher air pressure inside the chamber prevents the external environment from entering the heating chamber, thereby achieving the effect of atmosphere protection.
[0034] The target temperature and stretching conditions are set through the control panel of the heating system and the transmission control system. After the protective atmosphere is filled, the circulating water cooling system and the heating switch are turned on in sequence. After the sample temperature reaches the target temperature, it is kept warm for a certain period of time according to the national standard for high-temperature stretching, and then the transmission control system is started to obtain the high-temperature stretching curve of the material. During the stretching process, since the sealed heating chamber is filled with protective gas, the polished surface of the sample will not be oxidized. With the help of an external optical microscopic observation system, the fracture process of the material can be monitored and recorded in real time through the high-temperature observation window on the cabin cover.
[0035] After the material breaks, the heating switch is automatically turned off, and the protective gas flow rate is increased, and the broken sample is quickly cooled by air blowing. Due to the effects of air blowing cooling and circulating cooling water, the sample can be quickly cooled and taken out of the sealed heating chamber, and the high-temperature fracture will not be oxidized, which is conducive to the accurate characterization and analysis of the subsequent fracture characteristics.
[0036] This will be described below with reference to specific embodiments.
[0037] Example 1
[0038] An experimental steel plate sample with bainite structure was selected, and its surface was polished with sandpaper to be bright, and grid marking was done by confocal ion beam (FIB) system.
[0039] After the sample is fixed to the chuck of the tensile machine by a pin, the high temperature extensometer is installed, and then the heating cabin cover is closed, the protective gas (high purity argon) interface is closed, the vacuum pipeline interface is opened, and the vacuum is pumped to 4×10 -4 Pa, close the vacuum pipeline interface and the molecular pump, open the protective gas interface, adjust the gas valve to fill the sealed heating chamber with protective gas, and at the same time adjust the barometer to make the gas in the heating chamber slightly higher than the external atmospheric pressure (101.325KPa), and allow the protective gas to escape slowly through the one-way gas valve interface.
[0040] Set the high temperature heating temperature to 650℃, the heating rate to 100℃ / min, and the stretching rate to 10 -3 / s. Turn on the cooling water tank and the temperature control switch in turn, adjust the external optical microscope observation device, turn on the video recording button of the control software after completing the focus, and start recording. After heating to 650℃ and keeping warm for 10 minutes, turn on the transmission control system to start the high-temperature tensile test. After the sample breaks, the transmission control system automatically unloads the force and the heating system automatically shuts down. Adjust the protective gas valve to quickly cool the sample by air blowing. The average cooling rate of the sample in the range of 650-300℃ is measured to be about 10℃ / s. After the sample quickly cools to 50℃ for 3 minutes, take out the sample.
[0041] There is no oxide layer on the surface of the fractured sample. With the help of FIB grid marking, the grain boundary sliding phenomenon during the high-temperature tensile process of bainite can be clearly seen through electron microscopy. The results are as follows: Figure 5 As shown, no oxide is formed at the tensile fracture, and the surface of the sample and the fracture surface remain smooth.
[0042] The above is a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principles of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.
Claims
1. An atmosphere-protected high-temperature tensile testing device, characterized in that: The invention comprises a heating chamber (1), a heating system, a water circulation cooling system, an atmosphere protection system, an optical microscopic observation system and a transmission control system. The heating chamber (1) is designed with an embedded water circulation cooling system. The heating system adopts a short-wave infrared heating tube (9), which is connected to the heating chamber (1). The atmosphere protection system is realized by evacuating the sealed heating chamber (1) and then filling it with a protective gas. A high-temperature observation window (8) is arranged on the heating chamber cover on the side of the heating chamber (1), and the optical microscopic observation system is connected through the high-temperature observation window (8). The transmission control system comprises a moving crossbeam (2), a bidirectional ball screw (3) and a stretching shaft (6). The heating chamber (1) is located in the middle of a stretching frame formed by the moving crossbeam (2) and two bidirectional ball screws (3). The heating chamber (1) is fixed to the moving crossbeam (2) through the stretching shaft (6). The heating chamber (1) is a box structure, with two cooling plates (20) welded on the upper and lower parts respectively; a high-temperature extensometer sealing box (7) is installed on one side of the heating chamber (1); a water outlet (24) and a water inlet (25) are arranged on the side opposite to the heating chamber cover; the interior of the heating chamber (1) is a double elliptical reflection section (12), the two elliptical sections share a focus, the tensile specimen is located at the focus, and the short-wave infrared heating tube (9) is installed on the other two foci of the two ellipses; The high temperature extensometer sealing box (7) is fixed to the heating chamber (1) by means of bolt 2 (17); the quartz pins of the extensometer in the high temperature extensometer sealing box (7) are inserted into the heating chamber (1) through the extensometer slot (14) and contact the tensile specimen; The stretching frame is designed to be vertical, the motor is located at the bottom of the stretching frame and transmits movement to the upper and lower beams through two bidirectional ball screws. Since the threads on both sides of the bidirectional ball screws are in opposite directions, the upper and lower beams drive the stretching shaft to move in opposite directions at the same time.
2. The atmosphere-protected high-temperature tensile testing device according to claim 1, characterized in that: The heating chamber (1) is made of a heat-resistant alloy and adopts a reflective focusing heating design inside. A cooling water pipeline (13) is designed inside the shell of the heating chamber (1). A thermocouple is installed at the interface between the heating chamber (1) and the external sealing member (10) for temperature protection.
3. The atmosphere-protected high-temperature tensile testing device according to claim 1, characterized in that: The heating chamber (1) and the stretching shaft (6) are connected via a sealing sleeve (11), and a sealing ring inner groove (18) is machined inside the sealing sleeve (11).
4. The atmosphere-protected high-temperature tensile testing device according to claim 1, characterized in that: The heating chamber cover is fixed to the heating chamber (1) by means of bolt 1 (16), and a high-temperature sealing ring is placed in a sealing ring groove (15) at a high-temperature observation window (8) on the heating chamber cover.
5. The atmosphere-protected high-temperature tensile testing device according to claim 1, characterized in that: The cooling plate (20) is processed with an external connection hole (19), a heating pipe insertion hole (21), a cooling water sealing port (22) and a stretching shaft hole (23), and the sealing member (10) is connected to the external connection hole (19) via a high-temperature sealing ring and bolts.
6. The atmosphere-protected high-temperature tensile testing device according to claim 1, characterized in that: The two ends of the bidirectional ball screw (3) are respectively processed with a forward thread (4) and a reverse thread (5).
Citation Information
Patent Citations
Infrared heating furnace device
CN101685052A
Atmosphere-protected high-temperature tensile test device
CN211426115U
Stress-application observation device
JP2001165879A
Cited By
Aluminum alloy high-temperature stretching detection device
CN120369490A
Aluminum alloy high temperature tensile testing device
CN120369490B