Wafer-level chip scale packaging with varying thickness
By designing thinner critical parts and thicker non-critical parts in WLCSP, the BLR and CTE mismatch problem in prior art WLCSPs in manufacturing smaller size and lower profile packages is solved, achieving higher board-level reliability and longer service life.
Patent Information
- Application Number
- CN202010538245.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2020-05-14
- Filing Date
- 2020-06-12
- Publication Date
- 2025-03-07
- Estimated Expiration
- 2040-06-12
AI Technical Summary
Existing WLCSPs face problems with high board-level reliability (BLR) and coefficient of thermal expansion (CTE) mismatch when manufacturing semiconductor packages with smaller sizes and lower profiles, resulting in damage to WLCSP and electronic components, thereby reducing their expected life.
Reduce CTE mismatch with printed circuit boards (PCBs) and improve tolerance for onboard temperature cycles (TCOBs) by designing thinner critical sections and thicker non-critical sections in WLCSP.
Improves WLCSP's board-level reliability (BLR), extends its service life, and increases resistance to external stresses and forces, making it more tolerant during handling and shipment.
Smart Images

Figure CN112086408B_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to wafer level chip scale packages (WLCSPs) having varying thicknesses. Background Art
[0002] Typically, WLCSPs are manufactured by coupling solder balls to the active side of a semiconductor wafer. The solder balls are then coupled to tape to support the wafer during dicing of the wafer into individual WLCSPs. The wafer is then diced into individual WLCSPs by sawing, cutting, etching, or some other dicing technique. After the wafer is diced, the diced WLCSPs are removed from the tape. These individual WLCSPs can be coupled to a printed circuit board (PCB) for use and installation within an electronic device.
[0003] As the demand for smaller size and lower profile semiconductor packages for manufacturing electronic devices increases, there are significant challenges in producing WLCSPs with high pin counts, smaller size and lower profile.
[0004] A significant challenge in producing smaller size and lower profile WLCSP is to achieve high board level reliability (BLR) against temperature cycling on board (TCOB) due to the thermal coefficient of expansion (CTE) mismatch between the WLCSP and the PCB. Typically, the PCB has a much higher CTE than the WLCSP. This CTE mismatch between the PCB and the WLCSP can cause damage to the WLCSP and the electronic components in the WLCSP, which can cause the WLCSP to fail or reduce efficiency. Because of this CTE mismatch between the WLCSP and the PCB, the life expectancy of the WLCSP due to temperature cycling is significantly reduced.
[0005] Another significant challenge is handling and transporting smaller and thinner WLCSPs. Thinner WLCSPs are more susceptible to damage caused by external stresses and forces. For example, small external forces such as dropping the WLCSP during handling, moving during shipping, rapid temperature changes, or other similar external forces or stresses can cause significant damage to smaller and thinner WLCSPs. Summary of the invention
[0006] The present disclosure relates to various wafer-level chip scale packages (WLCSP) having a thinner critical portion and a non-critical portion that is thicker than the critical portion. In this context, the critical portion describes the portion of the die of the WLCSP, where the die may bend or flex due to heat or thermal exposure, which may cause damage to the die or components within the die. The non-critical portion describes the area where the die is unlikely to bend or flex due to heat or thermal exposure. These thinner portions reduce the CTE mismatch between the WLCSP and the printed circuit board (PCB), improving the board-level reliability (BLR) of the WLCSP against temperature cycling on board (TCOB). Additionally, the thicker portion allows further processing and manipulation of the WLCSP, such as for the pick-up and placement of the WLCSP coupled to the PCB. The WLCSP with thinner portions and thicker portions can be manufactured using semiconductor manufacturing techniques (such as using tape, etching techniques, and cutting techniques).
[0007] According to one embodiment of the WLCSP, the WLCSP includes a die, a passivation layer, a redistribution layer (RDL), an under-bump metallization (UBM), and a solder ball coupled to the UBM. The WLCSP includes a passive first surface and a second surface surrounding the first surface, the second surface also being a passive surface. The WLCSP includes a first surface and a third surface opposite to the second surface, the third surface being active. The first surface is farther from the third surface than the second surface. The fourth surface extends from the first surface to the second surface. The third surface includes a contact pad or UBM. Additionally, the solder ball is coupled to a contact pad or UBM on the third surface. The sidewall extends between the second surface and the third surface.
[0008] This embodiment of the WLCSP also includes a first portion, a second portion, and a third portion. The first portion has a first thickness extending between the third surface and the first surface. The second portion has a second thickness extending between the third surface and the second surface. The third portion has a third thickness extending between the third surface and the fourth surface. The first thickness of the first portion is greater than the second thickness of the second portion. The first portion and the second portion are separated and coupled to each other by the third portion. The third thickness of the third portion varies between the second thickness and the first thickness. The fourth surface extends obliquely from the second surface to the first surface. The first portion is thicker than the second portion, meaning that the first portion extends in an outward direction from the second surface of the WLCSP. The first portion is a critical portion, the second portion is a non-critical portion, and the third portion is a transition portion. The first portion is positioned at the center of the WLCSP and is surrounded by the second portion and the third portion. The critical portion includes features that are susceptible to deformation that may cause flexure, bending, or other similar deformations in response to stress or thermal exposure.
[0009] In this embodiment, the thicker non-critical portion makes the WLCSP stronger at the center of the WLCSP, thereby allowing further handling and manipulation, such as picking up and placing the WLCSP on a PCB or shipping the WLCSP. In other words, this thicker non-critical portion allows the WLCSP to have a stronger resistance to external forces because the non-critical portion is thicker. The increase in strength and thickness reduces the possibility of damaging the WLCSP caused by external stresses and forces during further handling, processing, shipping, or other similar processes.
[0010] In this embodiment, when the WLCSP is mounted to a PCB, the thinner critical portion reduces the CTE mismatch between the PCB and this embodiment of the WLCSP. The reduction in CTE mismatch between the PCB and this embodiment of the WLCSP improves the BLR of the WLCSP by increasing the tolerance of the WLCSP to TCOB. This embodiment of the WLCSP is more tolerant to bending, flexing, expansion, and contraction in the PCB and the WLCSP due to temperature changes that expose the WLCSP and the PCB because when the WLCSP and the PCB have similar CTEs, the WLCSP and the PCB bend or flex in a similar manner.
[0011] In alternative embodiments of the above WLCSP, the fourth surface separating the second surface from the third surface may be vertical rather than inclined.
[0012] In another alternative embodiment, the WLCSP may have a first surface, a second surface, and a third surface, the third surface being opposite to a fourth surface, the fourth surface including a contact. The second surface extends from the first surface to the first sidewall, and the third surface extends from the first surface to the second sidewall. In this embodiment, the second surface and the third surface are inclined, which results in the WLCSP having a second portion and a third portion with varying thicknesses. Additionally, the WLCSP in this embodiment includes a first portion having a uniform thickness, the first portion separating the second portion from the third portion and coupling the second portion to the third portion. The first portion is positioned between the first surface and the fourth surface of the WLCSP.
[0013] In another alternative embodiment of the WLCSP, the first portion extends from the surface of the WLCSP in an outward direction and has a plus sign shape. In this alternative embodiment, the corners of the WLCSP are thinner than the first portion having the plus sign shape. Additionally, the first portion is located at the center of the WLCSP and extends from one sidewall to another opposite sidewall.
[0014] In another alternative embodiment, a plurality of thicker portions may extend in an outward direction from the surface of the WLCSP. The plurality of thicker portions may have any shape. Additionally, this alternative embodiment of the WLCSP may include thinner portions that are aligned with grooves, gaps, or spaces that extend between and through the plurality of thicker portions. The thinner portions include a first set of thinner portions extending in a first direction and a second set of thinner portions extending in a second direction transverse to the first direction.
[0015] The above embodiments and alternative embodiments of the WLCSP having thinner portions and thicker portions are fabricated by a method that includes coupling a wafer to a tape, etching the wafer, dicing the wafer into individual WLCSPs, and removing the individual and diced WLCSPs. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] In the drawings, identical reference numbers identify similar elements or acts unless context dictates otherwise. The sizes and relative proportions of elements in the drawings are not necessarily drawn to scale.
[0017] Figure 1A is a top view of one embodiment of a WLCSP;
[0018] Figure 1B yes Figure 1A A side view of an embodiment of a WLCSP in FIG.
[0019] Figure 1C It is along Figure 1A A cross-sectional view taken along line 1C-1C in FIG.
[0020] Figure 1D yes Figure 1A and Figure 1B A bottom view of an embodiment of a WLCSP in FIG.
[0021] Figure 1E yes Figure 1A An example of a WLCSP along Figure 1A , Figure 1B and Figure 1D A cross-sectional view taken along line 1E-1E in FIG.
[0022] Figure 2A-2C is an alternative embodiment of a WLCSP;
[0023] Figure 3A is a top view of an alternative embodiment of a WLCSP;
[0024] Figure 3B yes Figure 3A A side view of an alternative embodiment of a WLCSP in FIG.
[0025] Figure 4 is a top view of an alternative embodiment of a WLCSP;
[0026] Figure 5A is a top view of an alternative embodiment of a WLCSP;
[0027] Figure 5B yes Figure 5A An alternative embodiment of the WLCSP along Figure 5A A cross-sectional view taken along line 5B-5B in FIG.
[0028] Figure 6 is a top view of an alternative embodiment of a WLCSP;
[0029] Figure 7 is a flow chart of a manufacturing method according to the disclosed embodiment; and
[0030] Figure 8A-8E is a side view of sequential steps of a package fabrication process according to the disclosed embodiment. DETAILED DESCRIPTION
[0031] In the following description, certain specific details are set forth in order to provide a thorough understanding of various embodiments of the present disclosure. However, those skilled in the art will appreciate that the present disclosure may be practiced without these specific details. In other cases, well-known structures and fabrication techniques associated with electronic components have not been described in detail to avoid unnecessarily obscuring the description of the embodiments of the present disclosure.
[0032] Unless the context requires otherwise, throughout this specification and the claims that follow, the word "comprise" and variations such as "comprises" and "comprising" are to be interpreted in an open, inclusive sense, ie, "including, but not limited to."
[0033] The use of ordinal numbers such as first, second, and third does not necessarily imply a sense of sequential ordering, but rather serves only to distinguish between multiple instances of an action or structure.
[0034] Throughout the specification, references to "one embodiment" or "an embodiment" mean that a particular feature, structure, or characteristic described in connection with the embodiment is included in at least one embodiment. Thus, the phrases "in one embodiment" or "in an embodiment" appearing in various places throughout the specification are not necessarily all referring to the same embodiment. Furthermore, in one or more embodiments, the particular features, structures, or characteristics may be combined in any suitable manner.
[0035] As used in this specification and the appended claims, the singular forms "a," "an," and "the" include plural referents unless the content clearly dictates otherwise. It should also be noted that the term "or" is generally employed in its sense including "and / or" unless the content clearly dictates otherwise.
[0036] The present disclosure relates to wafer level chip scale packages (WLCSP) that include multiple thicknesses on the passive side of a die. For example, Figure 1A-1E One embodiment of WLCSP 100 is directed to, which includes a die 132 having a first surface 110, a second surface 112, and a third surface 114 on a first side of the die, the first side being the inactive side of the die. The die 132 includes a fourth surface 116 on a second side of the die, the second side being opposite to the first side and being the active side of the die 132. The die includes a substrate, which may be made of, for example, silicon, silicon germanium, or other suitable materials. The die 132 includes a sidewall 118 extending from the fourth surface 116 of the die 132 to the first surface 112. The fourth surface 116 of the die 132 includes an under-bump metallization (UBM) 120 and a solder ball 122 coupled to the UBM 120. A redistribution layer (RDL) 131 is positioned between the die 132 and the UBM 120. The die 132 is a silicon material or other suitable semiconductor material. Transistors, resistors, capacitors, and other circuits may be formed in die 132 using electrical connections that extend to the active side of the die. The passive side of the die does not include any electrical components on the surface farthest from the active side of the die.
[0037] In this embodiment, if Figure 1A As shown, the first surface 110, the second surface 112, and the fourth surface 116 are opposite to the third surface 114. The die 132 has different thicknesses between different surfaces. The first surface 110 of the WLCSP 100 is positioned at the center of the die 132 and has a thickness of Figure 1A The first surface is shown in the shape of a square, wherein the sides of the square are substantially parallel to the corresponding sides of the die. However, in alternative embodiments, the shape of the first surface may be circular, oval, triangular, diamond, or any other shape. Figure 2A-2C Furthermore, in alternative embodiments, first surface 110 may be located at a different location on WLCSP 100 rather than at the center of WLCSP 100 .
[0038] The fourth surface 116 surrounds the first surface 110 and is positioned between the first surface 110 and the second surface 112. The second surface surrounds the first surface 110 and the fourth surface 116 and is positioned between the fourth surface 116 and the sidewall 118. The fourth surface 116 extends between the first surface 110 and the second surface 112. The fourth surface 116 separates the first surface 110 from the second surface 112. The fourth surface 116 is transverse to the first surface 110, the second surface 112, and the third surface 114. Figure 1B As shown, the fourth surface 116 may be inclined. However, in alternative embodiments, the fourth surface 116 may be perpendicular or substantially perpendicular to the second surface.
[0039] The third surface 114 is opposite to the first surface 110 and the second surface 112, and the fourth surface 116 is a front side surface or other active surface where electrical contact is formed. The first surface 110, the second surface 112 and the fourth surface 114 are back side surfaces or other passive surfaces without electrical contact. It is possible that there are through-silicon vias or other contacts formed to extend to the passive surface. The sidewalls extend between the second surface 112 and the third surface 114. The sidewalls 118 have a first height H1.
[0040] like Figure 1B-Figure 1D As shown, UBM 120 is on third surface 114. A plurality of solder balls 122 are coupled to UBM 120 on third surface 114. Each respective solder ball 122 is coupled to its own respective UBM 120. Figure 1D , the UBMs are illustrated as being circular, however, these UBMs may be square or rectangular or any other suitable shape. Solder balls 122 are used to couple the WLCSP 100 to a PCB or other electronic components within an electronic device such as a smart phone, tablet, computer, calculator, or any other similar electronic device. Figure 1D As shown, a plurality of UBMs 120 , which may be a plurality of contact pads, bond pads, or some other electronic coupling locations, and a plurality of solder balls 122 are configured in a ball grid array (BGA) on the third surface 114 of the WLCSP 100 .
[0041] like Figure 1A-Figure 1CAs shown, WLCSP 100 includes a plurality of portions 125, 127, 129. The plurality of portions include a first portion 125, a second portion 127, and a third portion 129. The first portion 125 is positioned between the first surface 110 and the third surface 114, and has a first thickness T1 extending between the first surface 110 and the third surface 114. The second portion 127 is positioned between the second surface 112 and the third surface 114, and has a second thickness T2 extending between the second surface 112 and the third surface 114. The third portion 129 is positioned between the third surface 114 and the fourth surface 116, and has a third thickness T3 extending between the third surface 114 and the fourth surface 116.
[0042] The third thickness T3 is a varying thickness that varies between the first thickness T1 and the second thickness T2. The first thickness T1 of the first portion 125 is greater than the second thickness T2 of the second portion 127. The second portion 127 surrounds the first portion 125 and the third portion 129 of the WLCSP 100. The second portion 127 is thinner than the first portion 125 and forms a perimeter or boundary around the first portion 125 and the third portion 129. The second portion 127 is positioned adjacent to and along the sidewall 118. The first portion 125 is positioned at the center of the WLCSP 100. The third portion 129 surrounds the first portion 125 and separates the first portion 125 from the second portion 127 and couples the first portion 125 to the second portion 127. The third portion 129 acts as a transition portion between the first portion 125 and the second portion 127. The first portion 125 is a non-critical portion, while the second portion 127 is a critical portion. This critical portion is a location that can cause bending and deflection due to heat or thermal exposure. Such heat or thermal exposure resulting in bending and flexing may lead to cracks in die 132 , mechanical failure of electrical components in die 132 , or shorts between electrical components in die 132 .
[0043] The first thickness T1 of the non-critical portion 125 may be 200 microns to 400 microns, while the second thickness T2 of the critical portion 127 may be 100 microns to 150 microns. However, in other alternative embodiments, the thickness of the non-critical portion 125 and the critical portion 127 may have different values than the thickness discussed directly above. The first surface 110 shaped like a square may have an area of 2 mm×2 mm. However, in other alternative embodiments, the first surface may have areas of different sizes.
[0044] A benefit of the WLCSP 100 of the present disclosure is that when this embodiment of the WLCSP 100 is further processed or shipped, because the WLCSP is thicker at the center, the non-critical portion 125, which is thicker than the critical portion 127, causes the WLCSP 100 to be stronger and more resistant to external stresses and forces at the center. The more resistant center of stress and forces of the WLCSP 100 at the non-critical portion 125 allows the WLCSP 100 to be picked up and placed on a PCB, placed in a shipping container, or shipped to a customer at the non-critical portion 125 while reducing the possibility of damage caused by external stresses or forces. These external stresses or forces are those stresses or forces to which the WLCSP 100 is exposed during the above process or other similar processes. When the non-critical portion 125 is also installed in an electronic device, the non-critical portion 125 also increases the stress resistance of the WLCSP 100 because the non-critical portion 125 is more resistant to external forces.
[0045] An alternative benefit of the WLCSP 100 of the present disclosure is that when the WLCSP 100 is mounted or coupled to a PCB, the critical portion 127 of the WLCSP 100, which is thinner than the non-critical portion 125, reduces the difference between a first coefficient of thermal expansion (CTE) of the WLCSP 100 and a second CTE of the PCB because the WLCSP 100 is thinner at the critical portion 127 than at the non-critical portion 125. By reducing this difference between the first CTE and the second CTE, which may be referred to as a CTE mismatch, the WLCSP 100 and the PCB will expand, warp, contract, and bend in a similar manner when the WLCSP 100 and the PCB are mounted within an electronic device and exposed to rapid or slow temperature changes. This similarity in expansion, contraction, warping, and bending will reduce damage caused by the PCB expanding faster or slower than the WLCSP 100, or vice versa. By reducing the CTE mismatch between the WLCSP 100 and the PCB, the board level reliability (BLR) of the WLCSP 100 when exposed to temperature cycling on board (TCOB) increases, resulting in a longer useful life for the WLCSP 100. The reduction in CTE mismatch also reduces the chance of damage due to temperature changes when used in an electronic device that could cause the WLCSP 100 or PCB to fail or reduce efficiency.
[0046] An alternative benefit of the WLCSP 100 of the present disclosure is that the non-critical portion 125 and the critical portion 127 allow the WLCSP 100 to be made thinner.
[0047] Even though these benefits are not discussed with respect to every embodiment or alternative embodiment of a WLCSP having thickness variations of the present disclosure, these benefits apply to every embodiment of the WLCSP disclosed in the present disclosure.
[0048] Figure 1Eis through Figure 1A , Figure 1B and 1D FIG. 1 is an enhanced view of a die 132 in section 1E-1E in FIG. WLCSP 100 includes a die 132 having a plurality of bonding pads or contact pads 130 that are coupled to various active and passive circuits (not shown) in the die. Additionally, WLCSP 100 includes a redistribution layer (RDL) 131 that includes a first dielectric layer 124, a conductive layer 126, and a second dielectric layer 128. RDL 131 couples bonding pads 130 from the die to UBM 120 and ultimately to the outside world. UBM 120 is coupled to RDL 131 and solder balls 122 are coupled to UBM 120.
[0049] Bond pad 130 is electrically coupled to RDL 131, and RDL 131 is electrically coupled to UBM 120. A first dielectric layer 124 material is positioned between die 132 and conductive layer 126. First dielectric layer 124 may be a polyimide layer, a passivation layer, or some other non-conductive or insulating material layer. Conductive layer 126 may be a copper material, a gold material, a metal alloy, or some other conductive material. A second dielectric layer 128 material is positioned between conductive layer 126 and UBM 120. Second dielectric layer 128 may be a polyimide layer, a passivation layer, or some other non-conductive or insulating material layer. As previously described with respect to Figure 1B and Figure 1D As discussed, solder balls 122 are coupled to UBM 120 .
[0050] The bond pads 130, conductive layer 126, UBM 120, and solder balls 122 of die 132 are electrically coupled together. The bond pads 130, conductive layer 126, UBM 120, and solder balls 122 may be used to electrically couple die 132 to other external electronic or semiconductor components to which WLCSP 100 may be mounted or coupled, such as another semiconductor die, a PCB, or some other electronic device. Solder balls 122 also physically couple WLCSP 100 to the external electronic or semiconductor components.
[0051] The first dielectric layer 124 positioned between the die 132 and the conductive layer 126 electrically isolates the bonding pads 130 and a portion of the conductive layer 126 from other corresponding bonding pads 130 and corresponding portions of the conductive layer 126 to avoid crosstalk between the bonding pads 130 and portions of the conductive layer 126. Crosstalk occurs when two electronic components within the WLCSP become electrically coupled to each other due to defects or damage in the WLCSP, which can reduce the efficiency of the WLCSP, cause the WLCSP to fail completely, or reduce the life of the WLCSP.
[0052] The second dielectric layer 128 positioned between the UBM 120 and the conductive layer 126 electrically isolates portions of the conductive layer 126 and the UBM 120 from other corresponding portions of the conductive layer 126 and the UBM 120 to avoid crosstalk between the portions of the conductive layer 126 and the UBM 120. This is similar to how the first dielectric layer 124 isolates the bonding pads 130 and portions of the conductive layer 126 from other bonding pads 130 and portions of the conductive layer 126 as previously discussed with respect to the first dielectric layer 124. The second dielectric layer 128 also helps form the UBM 120, which will be discussed directly below.
[0053] The first dielectric layer 124, the conductive layer 126, and the second dielectric layer 128 are formed by multiple etching and masking steps. The first dielectric layer 124 can be formed by first placing a passivation material on the die 132. After the passivation material is placed, a mask material is placed on the passivation material, exposing certain areas of the passivation material and covering other areas of the passivation material. The mask material can be a photoresist mask, a hard mask, or some other masking material. After the masking material is placed, the passivation material is etched. The etching can be chemical etching, plasma etching, radiation etching, or some other etching technique. The masking material protects the portion of the passivation layer that it covers from being removed. After the etching step is completed, the masking material is removed to leave the first dielectric layer 124. The process is then repeated to form the conductive layer 126, the second dielectric layer 128, and the UBM 120 of the WLCSP 100. Alternatively, a flip chip process may be used to form dielectric layer 124 , conductive layer 126 , second dielectric layer 128 , and UBM 120 of WLCSP 100 .
[0054] Figure 2A-2C Alternative embodiments of WLCSP 200, 300, 400 are directed to having various thicknesses of the die in the package. WLCSP 200 includes a die 202 having a first surface 204 with a rounded shape of a thicker portion 206, such as Figure 2A The thicker portion 206 has a greater cross-sectional thickness than the thinner portion 208 surrounding the thicker portion 206. The die 202 includes a surface 210 between the thicker portion 206 and the thinner portion 208, which surface may be angled due to processing steps.
[0055] like Figure 2B As shown, WLCSP 300 includes a die 302 having an oval-shaped first surface 304. Oval-shaped first surface 304 is the surface of the thickest portion of die 302 measured from the active surface of die 302. Second surface 306 is the surface of the thinnest portion of die 302.
[0056] like Figure 2CAs shown, WLCSP 400 includes a die 402 having a diamond-shaped first portion 404. The first portion 404 is thicker than a second portion 406 surrounding the first portion 404. A corner or tip 408 of the first portion 404 is not aligned with a corner 410 of the die 402. Instead, the corner 408 is aligned in a middle region of a side 412 of the die 402. Figure 2C An alternative embodiment of the WLCSP 400 having a diamond-shaped first surface is similar to that previously discussed. Figure 1A , but in this alternative embodiment of the WLCSP 400 , the square first surface 110 is rotated about a corner 410 of the die 402 .
[0057] Figure 3A-3B An alternative embodiment relates to WLCSP 500 , which includes a die 532 , a first surface 510 , a second surface 512 , a third surface 516 , a fourth surface 514 , a first sidewall 518 , a second sidewall 513 , a plurality of UBMs 520 , and a plurality of solder balls 522 .
[0058] In this alternative embodiment, the first surface 510, the second surface 512, and the third surface 516 are opposite to the fourth surface 514. The first surface 510 is positioned at the center of the WLCSP 500. However, in alternative embodiments, the first surface 510 can be at a different location on the WLCSP 500. The first surface separates the second surface 512 from the third surface 516 and couples it to the third surface 516. The second surface extends between the first surface 510 and one of the first sidewalls 518 of the plurality of sidewalls 513, 518. The third surface 516 extends between the first surface 510 and another of the first sidewalls 518 of the plurality of sidewalls 513, 518. The first surface 510, the second surface 512, and the third surface 516 extend between one of the second sidewalls 513 and another of the second sidewalls 513. The first sidewall 518 has a rectangular shape and the second sidewall 513 has a trapezoidal shape or other non-rectangular shape on the rectangular shape. However, in alternative embodiments, the first sidewall 518 and the second sidewall may have different shapes. The second surface 512 and the third surface 516 are inclined. The inclination of the second surface 512 and the third surface 516 may be the same or may be different.
[0059] The UBM 520 is on the fourth surface 514. Solder balls 522 are coupled to the UBM 520 on the fourth surface 514. The die includes an RDL that is not shown in these figures. Each respective solder ball 522 is coupled to its own respective UBM 520. The solder balls 522 are used to couple the WLCSP 500 to a PCB or other electronic components within an electronic device such as a smart phone, tablet, computer, calculator, or any other similar electronic device. There may be a plurality of UBMs 520 that may be a plurality of contact pads, bonding pads, or some other electronic coupling locations, and the plurality of solder balls 522 are configured in a ball grid array (BGA) on the fourth surface 514. The plurality of solder balls 522 are coupled to the plurality of UBMs 520. Each respective solder ball 522 in the plurality of solder balls 522 is coupled to a respective UBM 520 in the plurality of UBMs 520. UBM 520 electrically and physically couples WLCSP 500 and die 532 of WLCSP 500 to other electronic components or semiconductor devices.
[0060] The WLCSP 500 has a first thickness T1 extending between the first surface 510 and the fourth surface 514, the first thickness T1 being a constant thickness that remains constant at any position positioned between the first surface 510 and the fourth surface 514. The WLCSP 500 has a second thickness T2 extending between the second surface 512 and the fourth surface 514. The second thickness T2 is a varying thickness that varies between the first height H1 of the sidewall 518 and the first thickness T1. The WLCSP 500 has a third thickness T3 extending between the third surface 516 and the fourth surface 514, the third thickness T3 being a varying thickness that varies between the first height H1 of the first sidewall 518 and the first thickness T1. The surfaces 510, 512, 514, 516 and the thicknesses T1, T2, T3 of the WLCSP 500 define portions of the WLCSP 500.
[0061] The plurality of portions 525, 527, 529 include a first portion 525, a second portion 527, and a third portion 529. The first portion 525 is positioned between the first surface 510 and the fourth surface 514 and has a first thickness T1. The second portion 527 is positioned between the second surface 512 and the fourth surface 514 and has a second thickness T2. As the second portion 527 of the WLCSP 500 extends from the first portion 525 toward the first sidewall 518, the thickness of the second thickness T2 decreases. The third portion 529 is positioned between the third surface 516 and the fourth surface 514 and has a third thickness T3. As the third portion 529 extends from the first portion 525 toward the first sidewall 518, the thickness of the third thickness T3 decreases.
[0062] The first sidewall 518 has a first height H1. The first thickness T1 is greater than the first height H1 of the first sidewall 518. The first portion 525 separates the second portion 527 and couples it to the third portion 529. The second portion 527 and the third portion 529 are adjacent to the first portion 525. As described above, the second thickness T2 of the second portion 527 and the third thickness T3 of the third portion 529 are variable thicknesses. As the second portion 527 extends toward the first sidewall 518, the second thickness T2 varies between the first thickness T1 of the first portion 525 and the first height H1 of the first sidewall 518. As the third portion 529 extends toward the first sidewall, the third thickness T3 varies between the first thickness T1 of the first portion 525 and the first height H1 of the first sidewall 518. The first portion 525 is positioned at the center of the die 532. The first portion 525 is a non-critical portion and the second portion 527 and the third portion 529 are critical portions.
[0063] Similar to Figure 1A-1E , this alternative embodiment of WLCSP 500 includes a die 532 having bonding pads 130. Additionally, WLCSP 500 includes an RDL that is not shown in this alternative embodiment. The RDL includes a first dielectric layer between the die 532 and the conductive layer, a second dielectric layer positioned between the conductive layer and UBM 520, and a conductive layer positioned between the first dielectric layer and the second dielectric layer. Figure 1E As shown, the configuration of these components is the same or very similar to that discussed above with respect to the RDL of FIG. 1 .
[0064] In another alternative embodiment, WLCSP 500 may not have sidewalls 518, but instead, second surface 512 and third surface 516 may extend from first surface 510 and the edge of WLCSP 500 without sidewalls 518. In other words, the edge of WLCSP 600 is formed where the respective second surface 614 intersects the third surface.
[0065] Figure 4 Another alternative embodiment relates to WLCSP 600. WLCSP 600 includes a die 632 having a first surface 610, a plurality of second surfaces 614, a third surface (not shown) opposite the first and second surfaces, and a plurality of sidewalls 612.
[0066] The first surface 610 and the plurality of second surfaces 614 are opposite to a third surface that is not visible but is similar to Figure 1B and Figure 1EThe third surface 114 in the die 632. The first surface 610 and the plurality of second surfaces 614 constitute a backside surface, which is an inactive surface. The third surface constitutes a frontside surface, which is an active surface. The first surface 610 is positioned at the center of the die 632 and has a square shape. However, in alternative embodiments, the first surface can be circular, oval, rectangular, or some other shape as desired. Each of the corresponding second surfaces 614 in the plurality of second surfaces 614 extends between the first surface and the corresponding sidewall of the plurality of sidewalls 612. As shown in FIG. Figure 4 As shown, the second surface 614 surrounds the first surface 610. In this alternative embodiment, the second surface 614 has a trapezoidal shape. However, in other alternative embodiments, the second surface can have a different shape. The second surface 614 is inclined or otherwise changes thickness between the first surface 610 and the sidewall. Figure 4 For each of the second surfaces 614 in the second surface 614, the inclination is the same. However, in other alternative embodiments, the second surfaces may be at different inclinations.
[0067] WLCSP 600 has a first thickness extending between first surface 610 and a third surface, which again is not visible but is similar to Figure 1B and Figure 1E The third surface 114 in the WLCSP 600. The WLCSP 600 includes a second thickness that varies. The second thickness extends between the second surface 614 and the third surface. The first surface 610, the second surface 614, and the third surface define a plurality of portions of the WLCSP 600. The plurality of portions 625, 627 include a first portion 625 and four second portions 627 surrounding the first portion 625. The first portion 625 is positioned between the first surface 610 and the third surface and has a first thickness. The sidewall 612 has a first height. The first height of the sidewall 612 is less than the first thickness of the first portion 625. The second portion 627 surrounds the first portion 625 and forms a perimeter or boundary around the first portion 625. The second portion 627 is positioned between the respective second surface 614 and the third surface of the plurality of second surfaces 614, and each second portion 627 has a respective variable thickness of a second thickness that varies between the first thickness of the first portion 625 and the first height H1 of the sidewall 612. The first portion 625 is a non-critical portion 625 and the second portion 627 is a critical portion 627. The non-critical portion 625 and the critical portions 627 also allow the WLCSP 600 to be made even thinner.
[0068] In another alternative embodiment, WLCSP 600 may not have sidewalls 612, but instead second surface 614 may extend between first surface 610 and an edge of WLCSP 600 without sidewalls. In other words, the edge of WLCSP 600 is formed where the respective second surface 614 intersects the third surface.
[0069] Similar to Figure 1A-1E , this alternative embodiment of WLCSP 600 includes a die 632 having a bonding pad. Additionally, WLCSP 600 includes a UBM, solder balls, and an RDL having a first dielectric layer and a second dielectric layer. The configuration of these components is similar to that described above with respect to Figure 1E As discussed and Figure 1E Same as shown.
[0070] Figure 5A-Figure 5B Another alternative embodiment of WLCSP 700 is directed to. WLCSP 700 includes a die 732 including a first surface 710, a plurality of second surfaces 712, a third surface 714 opposite to the first surface 710, and a plurality of second surfaces 712. Die 732 includes a plurality of fourth surfaces 716, a plurality of sidewalls 718, a plurality of UBMs 720, and a plurality of solder balls 722. RDLs are appropriately contemplated, but are not illustrated for simplicity.
[0071] In this alternative embodiment, the first surface 710, the second surface 712, and the fourth surface 716 are on opposite sides of the die compared to the third surface 714. Figure 5A As shown, the first surface 710 has a plus sign shape centered at the center of the die 732. However, in other alternative embodiments, the plus sign shape of the first surface 710 can be offset from the center or can be another shape. The fourth surface 716 is perpendicular to the first surface 710 and the second surface 712 or is otherwise transverse to the first surface 710 and the second surface 712. However, in other alternative embodiments, the fourth surface 716 can be inclined. The second surface 712 is positioned at the corner of the WLCSP 700. The first surface 710, the second surface 712, and the fourth surface 716 constitute the back side surface of the WLCSP 700, which is a passive surface. The third surface 714 is the front side surface of the WLCSP 700, which is an active surface.
[0072] The plurality of sidewalls 718 include four sidewalls 718. The four sidewalls 718 are inverted T-shaped as shown. However, in other alternative embodiments, the sidewalls 718 may have a rectangular shape, a trapezoidal shape, or some other shape. The first sidewall is opposite to the second sidewall, and the third sidewall is opposite to the fourth sidewall. However, in other alternative embodiments, the WLCSP may have any number of sidewalls or may have no sidewalls.
[0073] The WLCSP 700 has a first thickness T1 extending between the first surface 710 and the third surface 714. The WLCSP 700 has a second thickness T2 extending between the second surface 712 and the fourth surface 714. The second thickness T2 is less than the first thickness T1. The surfaces 710, 712, 714 and the thicknesses T1, T2 of the WLCSP 700 define a plurality of portions 725, 727 of the WLCSP 700. The plurality of portions 725, 727 include a first portion 725 and a set of second portions 727. The first portion 725 is positioned between the first surface 710 and the third surface 714 and has a first thickness T1. The first portion 725 extends from the first sidewall to the second sidewall, and the first portion 725 extends from the third sidewall to the fourth sidewall. The second portion 727 is positioned between the second surface 712 and the third surface 714 and has a second thickness T2. The second portion 727 is positioned at a corner of the WLCSP 700. However, in other alternative embodiments, the second portion may have thicknesses that are all different, all the same, or any combination of thicknesses or varying thicknesses. The first portion 725 is a non-critical portion 725 and the second portion 727 is a critical portion 727. These non-critical portions 725 and critical portions 727 also allow the WLCSP 700 to be made thinner.
[0074] Similar to Figure 1A-1E , this alternative embodiment of WLCSP 700 includes a die 732 having a pad. Additionally, WLCSP 700 includes UBMS 720, solder balls 722, and an RDL having a first dielectric layer and a second dielectric layer. The configuration of these components is similar to that described above with respect to Figure 1E As discussed and Figure 1E The same as shown, even though for simplicity in Figure 5B RDL is not shown in the figure.
[0075] Figure 6 Another embodiment of the WLCSP 800 is directed to. The WLCSP 800 includes a die 832 including a plurality of first surfaces 810, a second surface 812 surrounding the plurality of first surfaces, a third surface opposite the first surface 810 and the second surface 810, a plurality of fourth surfaces 816 extending between the plurality of first surfaces 810 and the second surface 812, and a plurality of sidewalls 818 surrounding the other surfaces listed above.
[0076] The plurality of first surfaces 810, the second surface 812, and the plurality of fourth surfaces 816 are opposite to the third surface, which is not visible but is similar to Figure 1B and Figure 1EThe plurality of first surfaces 810, the second surface 812, and the plurality of fourth surfaces 816 constitute a backside surface, which is an inactive surface. The third surface constitutes a frontside surface, which is an active surface. The plurality of first surfaces 810 are arranged in an array of uniform shapes spaced equidistantly from each other. The first surface 810 of the plurality of first surfaces 810 has a square shape. However, in other alternative embodiments, such as Figure 6 As shown, the plurality of first surfaces 810 may be Figure 6 The array shown is arranged in different forms, and the first surface 810 of the plurality of first surfaces 810 can have a circular shape, an elliptical shape, or a different shape. The second surface 812 surrounds each of the plurality of first surfaces 810. The plurality of fourth surfaces 816 are vertical surfaces, or are transverse to the first surface 810 and the second surface 812. Each fourth surface 816 extends between a corresponding first surface 810 and the second surface 812 of the plurality of first surfaces 810. However, in other alternative embodiments, the fourth surface 816 can be inclined. The first surface 810, the second surface 812, the third surface, and the fourth surface 816 define a portion of the WLCSP 800.
[0077] WLCSP 800 includes a plurality of first portions 825 and second portions 827. These portions represent the semiconductor material regions remaining after the process of forming different thicknesses on the passive surface of the die or wafer. Each of the first portions 825 is positioned between the corresponding first surface 810 and the third surface of the plurality of first surfaces 810. Each first portion 825 has a first thickness extending between the corresponding first surface 810 and the third surface. The second portion 827 extends between the second surface 812 and the third surface and has a second thickness extending between the second surface 812 and the third surface. The second portion 827 surrounds each first portion 825. The first thickness of the first portion 825 is greater than the second thickness of the second portion 827. The second portion 827 is aligned with the groove, gap or space extending between the first portions 825. The first portion 825 is a non-critical portion 825 and the second portion 827 is a critical portion 827. These non-critical portions 825 and the critical portion also allow the WLCSP 800 to be made even thinner.
[0078] Similar to Figure 1A-1E 1 , this alternative embodiment of WLCSP 800 includes a die 832 having bonding pads. Additionally, WLCSP 800 includes UBMS, solder balls, and RDL on a third surface. The RDL includes a first dielectric layer and a second dielectric layer. The configuration of these components is similar to that discussed above with respect to FIG. 1 and as shown in FIG. Figure 1E The same as shown, even though for simplicity in Figure 6The RDL is not shown.
[0079] Figure 7 and Figure 8A-8E A method of forming the above-mentioned WLCSP is related. A first step 911 includes coupling a wafer to a tape. The wafer includes a plurality of bare chips having active and passive electronic components arranged in a manner to perform a desired process, such as sensing, processing, data storage, data transmission, or any other suitable use for the bare chip or chip. A second step 913 includes etching the wafer. The etching may be an isotropic etching, an anisotropic etching, or a combination of the two. The etching may be a wet etching or a dry etching. The etching process results in varying thicknesses of various embodiments of WLCSPs having varying thicknesses as discussed in the present disclosure. A third step 915 includes cutting the etched wafer into a plurality of WLCSPs using a cutting device 943. The cutting device 943 may be a laser, a saw, or some other device capable of cutting a wafer into a plurality of WLCSPs. A fourth step 917 includes removing the WLCSPs from the tape 940. Removing the WLCSPs from the tape may be accomplished by a pick and place process. However, while the flow chart includes several steps, in other alternative embodiments, there may be more or fewer steps in manufacturing the embodiments of the WLCSP discussed above and other alternative embodiments of the WLCSP.
[0080] Figure 8A-8B A first step 911 involves coupling a wafer 932 to a tape 940 or other support for a packaging process. The wafer 932 includes an inactive backside surface 901 opposite an active frontside surface 914. A lateral side 918 separates the inactive backside surface 901 from the active frontside surface 914. A plurality of UBMs 920 are on the active frontside surface 914 of the wafer 932, and a plurality of solder balls 922 are coupled to the UBMs 920. In this representation, before cutting, the wafer is processed to include an RDL (not shown) coupled to the UBMs and solder balls. In other embodiments, the RDL and other features may be formed after cutting. The RDL may include a first dielectric layer, a second dielectric layer, and a conductive layer. However, in other alternative embodiments, the RDL may include any number of conductive or non-conductive layers.
[0081] The wafer is coupled to adhesive 942 of tape 940. Tape 940 may be a polyimide tape, a copper tape, or some other carrier suitable for holding the wafer during the process. The adhesive may be glue, a die attach film, or some other adhesive material. Figure 8BAs shown, wafer 932 is coupled to adhesive 942 of tape 940 by placing a plurality of solder balls 922 in adhesive 942 of tape 940. However, in alternative embodiments of the method, wafer 932 may be coupled to adhesive 942, solder balls 922 may be on adhesive layer 942, or some other coupling technique may be utilized to attach wafer 932 to tape 940.
[0082] Figure 8C A second step 913 of etching a wafer 932 is involved, wherein a portion of the silicon or other semiconductor material of the wafer is removed, thereby forming various shapes and thicknesses on the passive side of the wafer. After the first etching step 913, the wafer 932 includes a first surface 910, a second surface 912, and a third surface 916 between the first surface 910 and the second surface 912. In this embodiment, the third surface 916 is an inclined surface 916. However, in other alternative embodiments, the third surface 916 can be a vertical surface. The first surface 910, the second surface 912, and the third surface 916 constitute a backside surface, which is a passive surface. As described above, etching can form various shapes and patterns to accommodate the bottom circuit in the die (critical and non-critical parts).
[0083] The backside surface 901 having surfaces 910, 912, 916, which is an inactive surface, is opposite to the frontside surface 914, which is an active surface. The first etching step 913 may include applying a mask material to the backside 901 of the wafer. The mask may be a photoresist mask, a hard mask, or some other type of mask material used to etch the wafer 932 using some etching technique. The etching technique may be anisotropic etching, isotropic etching, chemical etching, radiation etching, plasma etching, water jet etching, or some other type of etching technique. The mask defines the portion of the wafer 932 that will be retained and removed during the etching step 913. After the wafer 932 has been etched, the mask is then removed.
[0084] Fig.8D A third step 915 involves cutting the etched wafer 932 into different multiple WLCSPs. The wafer 932 can be cut into individual multiple WLCSPs by a cutting device 943. The cutting device 943 can be a saw, a laser, a water jet, or some other cutting device. On the other hand, the wafer 932 can be cut into individual multiple WLCSPs by a second etching step. If a second etching step is used, a second mask can be applied to the wafer 932 and then the wafer 932 is etched again. The second etching step of cutting the wafer 932 into individual multiple WLCSPs can be anisotropic etching, isotropic etching, chemical etching, water jet etching, plasma etching, radiation etching, or some other type of etching technology. After the second etching step is completed, the second mask will be removed.
[0085] Fig. 8E A fourth step 917 involves removing the plurality of WLCSPs from the tape 940. In this removal step 917, the individual plurality of WLCSPs are removed from the adhesive 942 of the tape 940. At this point, the plurality of WLCSPs are ready for further processing or shipment.
[0086] The various embodiments described above may be combined to provide other embodiments. All of the U.S. patents, U.S. patent application publications, U.S. patent applications, foreign patents, foreign patent applications, and non-patent publications mentioned in this specification and listed in the Application Data Sheet are incorporated herein by reference in their entirety. If it is necessary to adopt the concepts of various patents, applications, and publications to provide further embodiments, aspects of the embodiments may be modified.
[0087] These and other changes can be made to the embodiments in light of the above detailed description. Generally, in the following claims, the terms used should not be interpreted as limiting the claims to the specific embodiments disclosed in the specification and claims, but should be interpreted to include all possible embodiments and the full range of equivalents to which the claims are entitled. Therefore, the claims are not limited by the present disclosure.
Claims
1. A device comprising: A die of semiconductor material, the die comprising: a central area and a peripheral area surrounding the central area; The semiconductor material has a first surface area at a first surface of the central region; A second surface of the semiconductor material located in the peripheral region has a second surface area, the second surface area is larger than the first surface area and the second surface surrounds the first surface; a plurality of inclined surfaces of the semiconductor material extending from the first surface to the second surface; a third surface of the semiconductor material, the third surface being opposite to the first surface, the second surface, and the plurality of inclined surfaces; a first portion, the first portion being located in the central area and having a first thickness extending from the third surface to the first surface, the first surface having a rectangular shape, and the first surface including a plurality of edges, the plurality of inclined surfaces extending from the plurality of edges; a second portion extending from the first portion, the second portion having a varying thickness extending from the plurality of inclined surfaces to the third surface; and a third portion extending from the second portion, the third portion being spaced apart from the first portion by the second portion, the third portion having a second thickness extending from the second surface to the third surface, the second thickness being less than the first thickness, the third portion surrounding the first portion and the second portion and being located in the peripheral region, the third portion including a plurality of first side walls, and each of the plurality of first side walls of the third portion being angled with each of the plurality of edges of the first surface. 2 . The apparatus of claim 1 , wherein the plurality of inclined surfaces extending from the first surface to the second surface are transverse to the first surface and the second surface. 3 . The apparatus of claim 1 , wherein the first surface is positioned at a center of the die.
4. The apparatus of claim 2, wherein the die further comprises: The sidewall of the semiconductor material has the second thickness and extends from the third surface to the second surface.
5. The apparatus of claim 1, wherein the first portion and the second portion extend away from the third portion. 6 . The apparatus of claim 1 , wherein the third surface of the die comprises a plurality of contact pads and a plurality of solder balls coupled to the plurality of contact pads.
7. A device comprising: Bare wafers of semiconductor material, including: The surface of the semiconductor material; a first sidewall of the semiconductor material, the first sidewall being transverse to the surface; a second sidewall of the semiconductor material opposite the first sidewall, the second sidewall being transverse to the surface; a first portion having a first thickness, the first portion being centrally located along the die, the first portion having a central surface of a first surface area, the central surface being opposite the surface; and a second portion having a second thickness less than the first thickness, the second portion extending from the first portion to the first sidewall, the second portion comprising a first inclined surface of the semiconductor material, the first inclined surface extending from the first portion to the first sidewall, the first inclined surface being transverse to the first sidewall, transverse to a central surface of the first portion, and having a second surface area greater than the first surface area; a third portion having a third thickness less than the first thickness, the third portion extending from the first portion to the second sidewall, the third portion being spaced apart from the second portion by the first portion, the third portion comprising a second inclined surface of the semiconductor material, the second inclined surface extending from the first portion to the second sidewall, the second inclined surface being transverse to the second sidewall; and A third sidewall of the semiconductor material extends from the first sidewall to the second sidewall, from the first inclined surface, the second inclined surface and the center surface to the surface, and is transverse to the first sidewall, the second sidewall, the first inclined surface, the second inclined surface and the center surface.
8. The apparatus of claim 7 , wherein the die further comprises a fourth sidewall of the semiconductor material, the fourth sidewall opposite the third sidewall, extending from the first sidewall to the second sidewall, from the first inclined surface, the second inclined surface, and the center surface to the surface, and transverse to the first sidewall, the second sidewall, the first inclined surface, the second inclined surface, and the center surface.
Citation Information
Patent Citations
Electronic device
CN212991081U
Semiconductor device, semiconductor wafer and manufacturing method of the same
US20100308442A1