Non-contact optical measurement device and method for dynamic process of energy transmission of magnetoelectric cyclotron

Through non-contact optical measurement device, laser Doppler vibrator and dynamic energy integration technology are used to solve the problem that the existing technology cannot accurately describe the dynamic energy transmission process of magnetoelectric cyclizers, and the energy transmission of magnetoelectric cyclizers is realized Accurate measurement and loss analysis of the process improve power conversion efficiency.

CN112433120BActive Publication Date: 2024-11-01ZHENGZHOU UNIVERSITY OF LIGHT INDUSTRY
View PDF 0 Cites 2 Cited by

Patent Information

Application Number
CN202011299740.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-11-19
Publication Date
2024-11-01
Estimated Expiration
2040-11-19

AI Technical Summary

Technical Problem

The existing static or quasi-static resistance strain gauge contact measurement methods cannot accurately describe the energy transmission process of magnetoelectric cyclizers during dynamic magnetic-mechanical-electric conversion, especially the main source of mechanical vibration loss, which makes it difficult to achieve energy transmission efficiency. promote.

Method used

Non-contact optical measurement device, including laser Doppler vibrator, phase lock amplifier, PC and static bias magnetic field application device, the vibration velocity signal of the magnetoelectric cyclizer is measured through laser Doppler vibrator, combined with Dynamic energy integration accurately determines the source of mechanical vibration loss of the device during efficient dynamic magnetic-mechanical-electric conversion.

Benefits of technology

It realizes accurate dynamic measurement of the energy transmission process of magnetoelectric cyclizers, can accurately locate the main source of mechanical vibration loss, improves measurement accuracy and quantitative description, and provides guiding significance for improving power conversion efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112433120B_ABST
    Figure CN112433120B_ABST
Patent Text Reader

Abstract

The present invention belongs to the technical field of electronic conversion devices, and discloses a non-contact optical measurement device for the dynamic process of energy transmission of a magnetoelectric gyro, wherein the measurement device comprises a laser Doppler vibrometer, a phase-locked amplifier, a PC, a static bias magnetic field application device, a magnetoelectric gyro, and a bracket; the laser Doppler vibrometer is connected to the voltage input end of the phase-locked amplifier through the voltage output end of the built-in speed decoder, the phase-locked amplifier is connected to the coil port of the magnetoelectric gyro through the output end of the internal oscillator, and the phase-locked amplifier is connected to the PC through a communication cable; the magnetoelectric gyro is fixed on the bracket, and the bracket is fixed in the middle of the static magnetic field application device. The present invention can accurately locate the main source of mechanical vibration loss of the device during the process of high-efficiency dynamic magneto-mechanical-electric conversion, and has the outstanding advantages of dynamic measurement, non-contact measurement, high accuracy and quantitative description.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of electronic conversion devices, and in particular relates to a non-contact optical measurement device and method for the dynamic process of energy transmission of a magnetoelectric cyclotron. Background Art

[0002] The ideal gyrator is a new type of passive, linear, non-reciprocal two-port element that can realize direct reciprocal conversion of voltage to current accompanied by efficient energy conversion, becoming the fifth type of basic network electrical element after resistors, capacitors, inductors and transformers. The ideal gyrator can realize the capacitive characteristics of inductive elements. In large-scale integrated circuits, inductive elements that are difficult to integrate on the chip can be replaced by gyrators and ordinary capacitors that are easier to integrate. Moreover, ordinary capacitors are closer to ideal elements than ordinary inductors. The inductive elements simulated by gyrators and ordinary capacitors are closer to ideal inductive elements than any ordinary inductors. The theoretical model of the hypothetical network topology of the ideal gyrator was first proposed by Tellegen of the Philips Laboratory in the Netherlands in 1948. Later, people worked hard to realize the gyrotron effect of the ideal gyrator by building discrete electrical components such as operational amplifiers. Until the beginning of this century, magnetostrictive / piezoelectric laminated structure transducers were widely used in data storage, magnetic field detection, power conversion and other fields due to their outstanding characteristics such as passivity and strong magnetoelectric coupling at room temperature. The four-wire-two-port element formed by winding coils around it provided a new way to realize the ideal gyrotron. The milestone work on magnetoelectric gyrotron was reported in 2006. Zhai et al. from Virginia Tech in the United States used the strong magnetoelectric coupling effect of the giant magnetostrictive material Terfenol-D and piezoelectric ceramic PZT composite and built a magnetoelectric gyrotron device by tightly winding coils around it, realizing the reciprocal conversion of the inductive-capacitive two-port electrical network. Since 2016, Leung et al. from Virginia Tech in the United States have carried out relevant theoretical modeling and experimental research on how to further improve the stability and power transmission efficiency of magnetoelectric gyrotrons through experimental means such as rare earth doping, changing the lamination method, and optimizing the coil size, and have achieved a series of original research results.

[0003] In order to further improve the energy transmission efficiency of magnetoelectric cyclotrons, researchers have used static or quasi-static resistance strain gauge contact measurement methods to analyze the coupling transfer process between magnetic energy, mechanical energy and electrical energy involved in the power transmission process, trying to find the main source of energy loss and further reduce it to improve efficiency. However, the normal operation of the magnetoelectric cyclotron is completed by the strong magnetoelectric coupling effect under resonant excitation, during which it undergoes a dynamic magneto-mechanical-electrical conversion process. This process cannot be accurately described by static or quasi-static resistance strain gauge contact measurement methods alone, and there are no reports of dynamic measurement methods used to describe the device during energy transmission at home and abroad. Summary of the invention

[0004] The purpose of the present invention is to provide a non-contact optical measurement device for the dynamic process of energy transmission of a magnetoelectric cyclotron, which can accurately locate the main source of mechanical vibration loss of the device during the process of high-efficiency dynamic magneto-mechanical-electric conversion, and has outstanding advantages such as non-contact measurement, high accuracy and quantitative description.

[0005] To achieve the above object, the present invention adopts the following technical solutions:

[0006] The invention provides a non-contact optical measuring device for the dynamic process of energy transmission of a magnetoelectric cyclotron. The measuring device comprises a laser Doppler vibrometer, a phase-locked amplifier, a personal computer, a static bias magnetic field applying device, a magnetoelectric cyclotron and a bracket. The laser Doppler vibrometer is connected to the voltage input end of the phase-locked amplifier via the voltage output end of a built-in velocity decoder, the phase-locked amplifier is connected to the coil port of the magnetoelectric cyclotron via the output end of an internal oscillator, and the phase-locked amplifier is connected to the personal computer via a communication cable. The magnetoelectric cyclotron is fixed on the bracket, and the bracket is fixed in the middle of the static magnetic field applying device. The personal computer adjusts the input voltage, AC magnetic field and frequency of the magnetoelectric cyclotron by the phase-locked amplifier, as well as the bias magnetic field applied by the static bias magnetic field applying device through a program.

[0007] Preferably, the magnetoelectric gyrator is composed of a magnetoelectric composite structure transducer and a coil uniformly surrounding the periphery of the magnetoelectric composite structure transducer. The magnetoelectric composite structure transducer is an asymmetric or symmetric multi-layer structure. The magnetoelectric composite structure transducer includes at least one magnetostrictive layer and one piezoelectric ceramic layer.

[0008] Preferably, the laser beam emitted by the laser Doppler vibrometer is a 632 nm helium-neon laser beam.

[0009] Preferably, the static bias magnetic field applying device is composed of neodymium iron boron permanent magnets arranged relatively on the guide rail.

[0010] The present invention also provides a non-contact optical measurement method for the dynamic process of energy transmission of a magnetoelectric cyclotron, comprising the following steps:

[0011] a. Grind the end faces of the magnetostrictive layer and the piezoelectric ceramic layer of the magnetoelectric gyrotron to be tested, and wipe them with acetone to remove the debris and oxide layer;

[0012] b. Cut the reflective film and stick it on the center of the end surface to be tested of each single-layer sample;

[0013] c. Fix the single-layer sample of the magnetostrictive layer at the center of the bracket so that it is in a free boundary vibration state;

[0014] d. Start the laser Doppler vibrometer, so that the laser beam passes through the focusing hole of the static bias magnetic field application device and focuses on the center position of the end surface to be measured of the magnetostrictive layer single-layer sample with a reflective film;

[0015] e. adjusting the input voltage, AC magnetic field and frequency of the lock-in amplifier to the single-layer sample, and the bias magnetic field applied by the static bias magnetic field applying device through a program;

[0016] f. The vibration velocity signal of the end face of the magnetostrictive layer single-layer sample to be measured is converted into a voltage signal by the velocity decoder built in the laser Doppler vibrometer. The voltage signal is collected by a lock-in amplifier, and the output kinetic energy of the magnetostrictive layer single-layer sample is obtained by dynamic energy integration.

[0017] g. Bond the magnetostrictive layer single-layer sample and the piezoelectric ceramic layer single-layer sample to obtain an asymmetric or symmetric magnetoelectric composite structure transducer, and evenly surround the coil around the periphery of the magnetoelectric composite structure transducer to form a magnetoelectric gyrator. Repeat steps c to f, and focus the laser beam layer by layer on the center position of the end surface to be tested of the magnetostrictive layer single-layer sample and the piezoelectric ceramic layer single-layer sample to obtain the interlayer dynamic kinetic energy transfer efficiency of the magnetoelectric gyrator.

[0018] Compared with the prior art, the present invention has the following beneficial effects:

[0019] The present invention focuses a polarized helium-neon light beam emitted by a laser Doppler vibrometer to the center of the vibrating end face of a sample. A system sensor collects reflected light with a frequency shift due to the surface vibration of the sample, and after comparing it with a reference light, a velocity decoder converts the vibration frequency signal of the sample into a vibration velocity signal. The input voltage, AC magnetic field and frequency of a phase-locked amplifier to a single-layer sample are adjusted by a program to obtain vibration information of a magnetostrictive layer and a piezoelectric layer of a magnetoelectric gyro under excitations of different frequencies. Dynamic energy integration is used to calculate the energy transmission efficiency and loss of each layer in the magnetoelectric gyro in dynamic state.

[0020] Compared with the traditional contact stress measurement method, the non-contact optical measurement method of the present invention can measure the dynamic energy transfer process, and can accurately locate the main source of mechanical vibration loss of the device during the high-efficiency dynamic magneto-mechanical-electrical conversion process. It has outstanding advantages such as dynamic measurement, non-contact measurement, high accuracy and quantitative description. The present invention conducts an in-depth analysis of the dynamic magneto-mechanical-electrical conversion process involved in the energy transmission process of the magneto-electric cyclotron, and directly proves the rationality of the non-contact optical measurement method of the present invention through experimental data. It has a clear guiding significance for further improving the power conversion efficiency in the design of magneto-electric cyclotron devices, and provides a new way for the field of power transmission efficiency testing of high-efficiency power electronic devices. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] Figure 1 It is a schematic structural diagram of the non-contact optical measuring device of the present invention.

[0022] Figure 2 It is a schematic diagram of the principle of the non-contact optical measurement device of the present invention.

[0023] Figure 3 The output vibration velocity spectra of the magnetostrictive layer of the magnetoelectric gyrotron with single-layer, double-layer and triple-layer structures in Example 1 at resonance.

[0024] Figure 4 This is the vibration velocity spectrum of each end surface of the NZTFO layer and the PZT layer of the double-layer magnetoelectric gyrator in Example 1 within the frequency range of 45kHz-70kHz.

[0025] Figure 5 The output mechanical kinetic energy spectra of the single-layer and double-layer magnetoelectric cyclotrons calculated in Example 1.

[0026] Figure 6 This is the vibration velocity spectrum of each end surface of the two NZTFO layers and the PZT layer of the three-layer magnetoelectric gyrator of Example 2 in the frequency range of 52.5kHz-75kH.

[0027] Figure 7 The output mechanical kinetic energy spectra of the single-layer and three-layer magnetoelectric cyclotrons calculated in Example 2. DETAILED DESCRIPTION

[0028] The following examples are used to illustrate the present invention, but are not intended to limit the scope of the present invention. Unless otherwise specified, the technical means used in the examples are conventional means known to those skilled in the art. The test methods in the following examples are conventional methods unless otherwise specified.

[0029] like Figure 1As shown, the present invention provides a non-contact optical measuring device for the dynamic process of energy transmission of a magnetoelectric cyclotron, and the measuring device includes a laser Doppler vibrometer, a phase-locked amplifier, a PC, a static bias magnetic field applying device, a magnetoelectric cyclotron and a bracket. The laser Doppler vibrometer is connected to the voltage input end of the phase-locked amplifier via the voltage output end of the built-in velocity decoder, the phase-locked amplifier is connected to the coil port of the magnetoelectric cyclotron via the output end of the internal oscillator, and the phase-locked amplifier is connected to the PC via a communication cable. The magnetoelectric cyclotron is fixed on the bracket, and the bracket is fixed in the middle of the static magnetic field applying device. The PC adjusts the input voltage, AC magnetic field and frequency of the phase-locked amplifier to the magnetoelectric cyclotron, as well as the bias magnetic field applied by the static bias magnetic field applying device through a program.

[0030] In the structure of the above-mentioned measuring device, the laser Doppler vibrometer and its built-in velocity decoder constitute a non-contact optical measurement system, while the phase-locked amplifier, the static bias magnetic field application device, the magnetoelectric gyro, the bracket and the PC constitute a magnetoelectric gyro signal input power control system that keeps the input power constant. The software control program in the PC is written by LabVIEW, which mainly completes the functions of instrument control, data acquisition, human-computer interaction and data storage. The magnetoelectric gyro is composed of a magnetoelectric composite structure transducer and a coil uniformly surrounding the periphery of the magnetoelectric composite structure transducer. The magnetoelectric composite structure transducer is an asymmetric or symmetric multi-layer structure. The magnetoelectric composite structure transducer includes at least one magnetostrictive layer and one piezoelectric ceramic layer. The static bias magnetic field application device is composed of neodymium iron boron permanent magnets relatively arranged on the guide rail. The instrument models used are: phase-locked amplifier (produced by Ametek, USA, model SR7280); laser Doppler vibrometer (produced by Polytech, Germany, model OFV5000 / 505), the laser beam emitted by the laser Doppler vibrometer is a 632nm helium-neon laser beam; velocity decoder (produced by Polytech, Germany, model VD-09); USB-GPIB communication cable (produced by National Instruments, USA, model USB-GPIB-HS).

[0031] The non-contact optical measurement method of the dynamic process of energy transmission of the magnetoelectric cyclotron comprises the following steps:

[0032] a. Use 600 # The end faces of the magnetostrictive layer and the piezoelectric ceramic layer of each single-layer sample in the magnetoelectric cyclotron were polished with sandpaper, and the debris and the oxide layer were wiped with acetone to obtain a smooth and clean end face;

[0033] b. Cut the reflective film into an area about 1 / 2 of the end surface to be tested, and stick it to the center of the end surface to be tested of each single-layer sample;

[0034] c. Fix the single-layer sample of the magnetostrictive layer at the center of the bracket so that it is in a free boundary vibration state;

[0035] d. Start the laser Doppler vibrometer, so that the laser beam passes through the focusing hole of the static bias magnetic field application device and focuses on the center position of the end surface to be measured of the magnetostrictive layer single-layer sample with a reflective film;

[0036] e. Using LabVIEW program, adjust the input voltage, AC magnetic field and frequency of the lock-in amplifier to the single-layer sample, as well as the bias magnetic field applied by the static bias magnetic field application device, so that the gyrator works in the best state and keeps the input power constant;

[0037] f. The vibration velocity signal of the end face of the magnetostrictive layer single-layer sample to be measured is converted into a voltage signal by the velocity decoder built in the laser Doppler vibrometer. The voltage signal is collected by a lock-in amplifier, and the output kinetic energy of the magnetostrictive layer single-layer sample is obtained by dynamic energy integration.

[0038] g. Bond the magnetostrictive layer single-layer sample and the piezoelectric ceramic layer single-layer sample to obtain an asymmetric or symmetric magnetoelectric composite structure transducer, and evenly surround the coil around the periphery of the magnetoelectric composite structure transducer to form a magnetoelectric gyrator. Repeat steps c to f, and focus the laser beam layer by layer on the center position of the end surface to be tested of the magnetostrictive layer single-layer sample and the piezoelectric ceramic layer single-layer sample to obtain the interlayer dynamic kinetic energy transfer efficiency of the magnetoelectric gyrator.

[0039] like Figure 2 As shown in the figure, the working principle of non-contact optical vibration velocity measurement is as follows: the laser beam splitter of the laser Doppler vibrometer divides the laser beam into a reference beam and a measurement beam. After passing through the second beam splitter, the polarized helium-neon beam emitted by the laser of the laser Doppler vibrometer is focused to the center of the vibrating end face of the sample. The system sensor collects the reflected light with frequency shift due to the surface vibration of the sample, and after comparing it with the reference light, the velocity decoder converts the vibration frequency signal of the sample into a vibration velocity signal. The input voltage, AC magnetic field and frequency of the phase-locked amplifier to the single-layer sample are adjusted by the program to obtain the vibration information of the magnetostrictive layer and piezoelectric layer of the magnetoelectric gyro under different frequency excitations, and the dynamic energy integration is used to calculate the energy transmission efficiency and loss of each layer in the magnetoelectric gyro in dynamic state.

[0040] Example 1

[0041] In this embodiment, the magnetoelectric composite structure transducer includes a nickel-zinc ferrite magnetostrictive layer (Ni 0.7 Zn 0.3 Tb 0.02 Fe 1.98O4, abbreviated as NZTFO) and a layer of lead zirconate titanate piezoelectric ceramic layer (PZT-8), and then an epoxy resin layer is used to form an MP structure. The size of the NZTFO layer is 38×5×1mm 3 , PZT-8 layer size is 40×5×1mm 3 The coil used is a copper enameled wire with a wire diameter of 0.2 mm and 260 turns.

[0042] The measurement process is as follows: use 600# fine sandpaper to grind the end faces of NZTFO and PZT8 respectively; use acetone to wipe the end faces to remove material debris and oxide layer; cut the reflective film into an area of ​​about 3×1mm 2 The size of the reflective film is tightly attached to the center of the end face to be measured using tweezers to ensure that the reflective surface of the reflective paper is flat and free of stains; the magneto-electric composite structure transducer is connected to the center of the beryllium bronze bracket using ethyl acrylate adhesive, and fixed in a non-magnetic support shell tightly wrapped with a copper coil, and then the bracket is fixed in the corresponding position of the guide rail fixture; the Doppler laser vibrometer is started, and the height and position of the laser are adjusted so that the helium-neon laser beam passes through the focusing hole of the neodymium iron boron permanent magnet on the adjustable magnetic track and vertically irradiates the end face to be measured and focuses on the center of the reflective film; the relative distance of the neodymium iron boron permanent magnet in the guide rail is adjusted to change the bias magnetic field to the optimal bias; the amplitude and frequency of the input voltage of the phase-locked amplifier to the coil are adjusted using the LabVIEW program to determine the AC magnetic field size and frequency to maintain the constant input power; after setting the corresponding AC magnetic field value and frequency, and the value of the static bias magnetic field, the system begins to measure and record the end face vibration velocity of the NZTFO single layer, the NZTFO layer after bonding, and the PZT8 layer at different frequencies, and uses the dynamic energy integration formula Automatically calculate the dynamic energy transfer and mechanical loss between layers. The results are as follows Figure 3~Figure 5 shown.

[0043] Figure 3 The output vibration velocity spectra of the magnetostrictive layer of the magnetoelectric gyrotron with single-layer, double-layer and triple-layer structures at resonance. Figure 3It can be seen that for the single-layer magnetostrictive layer sample, the maximum vibration speed is 8.74mm / s at its resonance frequency of 74.45kHz, for the double-layer magnetoelectric gyro sample, the magnetostrictive layer reaches a maximum vibration speed of 4.73mm / s at a resonance frequency of 54.13kHz, and for the three-layer magnetoelectric gyro sample, the vibration speed of the magnetostrictive layer reaches a maximum value of 5.81mm / s at a resonance frequency of 59.01kHz. In other words, after the magnetostrictive layer is bonded with PZT as a mechanical load, the maximum amplitude of its vibration speed and the resonance frequency both show a downward trend. This is due to the frequency deviation caused by the increase in thickness due to the intervention of the mechanical load. At the same time, with the increase in the volume fraction of the magnetostrictive layer in the gyro sample, its vibration frequency and vibration speed both show an upward trend.

[0044] Figure 4 The vibration velocity spectrum of each end surface of the NZTFO layer and the PZT layer of the double-layer magnetoelectric gyrotron in the frequency range of 45kHz-70kHz. Figure 4 It can be seen that with the increase of frequency, the vibration velocity of each layer end surface increases significantly, reaching the maximum value of resonant vibration velocity of 4.73mm / s at a frequency of 54.13kHz, and the vibration frequency and vibration velocity of each layer are basically consistent (such as Figure 4 The enlarged image of the interval in the upper right corner shows that each layer of the double-layer magnetoelectric gyrator after bonding basically maintains the same frequency and amplitude of mechanical vibration.

[0045] Figure 5 The calculated output mechanical kinetic energy spectra of the single-layer and double-layer magnetoelectric cyclotrons. At this time, the single-layer NZTFO is used as the dynamic energy input actuator of the magnetoelectric cyclotron. The vibration velocity spectrum of the single-layer sample of the magnetostrictive layer at the resonance under no-load condition is measured, and the total input kinetic energy is obtained after dynamic energy integration; the vibration velocity of each layer of the double-layer magnetoelectric cyclotron is summed after dynamic energy integration as the total output kinetic energy of the double-layer magnetoelectric cyclotron. It is calculated that the total input kinetic energy of the double-layer magnetoelectric cyclotron is 0.07nJ, and the total output kinetic energy is 0.04nJ. The inter-layer dynamic kinetic energy transfer efficiency of the double-layer magnetoelectric cyclotron is 57%.

[0046] Example 2

[0047] In another embodiment, the magnetoelectric composite structure transducer includes two layers of nickel-zinc ferrite magnetostrictive layers (Ni 0.7 Zn 0.3 Tb 0.02 Fe 1.98 O4, abbreviated as NZTFO) and a layer of lead zirconate titanate piezoelectric ceramic layer (PZT-8), and then an epoxy resin layer is used to form an MPM sandwich structure. The size of the NZTFO layer is 38×5×1mm 3, PZT-8 layer size is 40×5×1mm 3 The coil used is a copper enameled wire with a wire diameter of 0.2 mm and 260 turns. The measurement process is omitted and the results are as follows Figure 6~Figure 7 shown.

[0048] Figure 6 The vibration velocity spectra of the two NZTFO layers and the PZT layer of the three-layer magnetoelectric gyrotron in the frequency range of 52.5kHz-75kH. Figure 6 It can be seen that with the increase of frequency, the vibration velocity of each layer end surface increases significantly, reaching the maximum value of resonant vibration velocity of 6.21mm / s at a frequency of 59.01kHz, and the vibration frequency and vibration velocity of each layer are basically consistent (such as Figure 6 The enlarged image of the interval in the upper right corner shows that each layer of the three-layer magnetoelectric gyrator after bonding basically maintains the same frequency and amplitude of mechanical vibration.

[0049] Figure 7 The calculated output mechanical kinetic energy spectra of the single-layer and three-layer magnetoelectric cyclotrons. At this time, two layers of NZTFO of the same size are used as the dynamic energy input actuator of the magnetoelectric cyclotron. The vibration velocity spectrum of the single-layer sample of the magnetostrictive layer at the resonance under no-load condition is measured, and the dynamic energy is integrated and multiplied by 2 as the total input kinetic energy; the vibration velocity of each layer of the three-layer magnetoelectric cyclotron is integrated and summed as the total output kinetic energy of the three-layer magnetoelectric cyclotron. It is calculated that the total input kinetic energy of the three-layer magnetoelectric cyclotron is 0.14nJ, and the total output kinetic energy is 0.10 nJ, so the inter-layer dynamic kinetic energy transfer efficiency of the three-layer magnetoelectric cyclotron is 71%.

[0050] The embodiments described above are only preferred embodiments of the present invention and are only used to explain the present invention, not to limit the scope of implementation of the present invention. For those skilled in the art, other implementation methods can certainly be easily made by replacement or modification based on the technical contents disclosed in this specification. Therefore, all changes and improvements made on the principles of the present invention should be included in the scope of the patent application of the present invention.

Claims

1. A non-contact optical measurement method for the dynamic process of energy transmission of a magnetoelectric cyclotron, characterized in that: The following steps are involved: a. Grind the end faces of the magnetostrictive layer and the piezoelectric ceramic layer of the magnetoelectric gyrotron to be tested, and wipe them with acetone to remove the debris and oxide layer; b. Cut the reflective film and stick it on the center of the end surface to be tested of each single-layer sample; c. Fix the single-layer sample of the magnetostrictive layer at the center of the bracket so that it is in a free boundary vibration state; d. Start the laser Doppler vibrometer, so that the laser beam passes through the focusing hole of the static bias magnetic field application device and focuses on the center position of the end surface to be measured of the magnetostrictive layer single-layer sample with a reflective film; e. adjusting the input voltage, AC magnetic field and frequency of the lock-in amplifier to the single-layer sample, and the bias magnetic field applied by the static bias magnetic field applying device through a program; f. The vibration velocity signal of the end face of the magnetostrictive layer single-layer sample to be measured is converted into a voltage signal by the velocity decoder built in the laser Doppler vibrometer. The voltage signal is collected by a lock-in amplifier, and the output kinetic energy of the magnetostrictive layer single-layer sample is obtained by dynamic energy integration. g. Bonding a magnetostrictive layer single-layer sample and a piezoelectric ceramic single-layer sample to obtain an asymmetric or symmetric magnetoelectric composite structure transducer, uniformly surrounding the coil around the periphery of the magnetoelectric composite structure transducer to form a magnetoelectric gyrotron, repeating steps c to f, and focusing the laser beam layer by layer on the center position of the end surface to be tested of the magnetostrictive layer single-layer sample and the piezoelectric ceramic single-layer sample, to obtain the interlayer dynamic kinetic energy transfer efficiency of the magnetoelectric gyrotron; The laser Doppler vibrometer is connected to the voltage input end of the phase-locked amplifier through the voltage output end of the built-in velocity decoder, the phase-locked amplifier is connected to the coil port of the magnetoelectric cyclotron through the output end of the internal oscillator, and the phase-locked amplifier is connected to the PC through a communication cable; the magnetoelectric cyclotron is fixed on a bracket, and the bracket is fixed in the middle of the static magnetic field application device; the PC adjusts the input voltage, AC magnetic field and frequency of the phase-locked amplifier to the magnetoelectric cyclotron, as well as the bias magnetic field applied by the static bias magnetic field application device through a program.

2. The non-contact optical measurement method according to claim 1, characterized in that: The magnetoelectric composite structure transducer comprises at least one magnetostrictive layer and one piezoelectric ceramic layer.

3. The non-contact optical measurement method according to claim 1, characterized in that: The laser beam emitted by the laser Doppler vibrometer is a 632nm helium-neon laser beam.

4. The non-contact optical measurement method according to claim 1, characterized in that: The static bias magnetic field applying device is composed of NdFeB permanent magnets which are arranged relatively on the guide rail.

Citation Information

Cited By

  • Energy efficiency traceability verification method for magnetoelectric power divider

    CN117269638A

  • Energy efficiency traceability verification method for magneto-electric power divider

    CN117269638B