Semiconductor structure and method for forming the same
By using a high-fluidity dielectric layer in the semiconductor structure to fill the sidewall depressions and a high-hardness second dielectric layer for planarization, the short circuit problem caused by defects in the dielectric layer in the peripheral area is solved, and the performance and reliability of the semiconductor structure are improved.
Patent Information
- Application Number
- CN201911220677.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2019-12-03
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2039-12-03
AI Technical Summary
The dielectric layer in the peripheral area of the existing semiconductor structure is prone to defects during the planarization process, causing short circuit problems between metal contact holes and affecting the performance of the semiconductor structure.
A first dielectric layer with higher fluidity is used to fill the sidewall depression of the first device structure on the first area, and a second dielectric layer with a higher hardness than the dielectric layer is formed on its surface, and is planarized through a chemical mechanical polishing process. Simplify the process flow and improve the quality of the dielectric layer.
It effectively avoids defects in the dielectric layer in subsequent processes, improves the quality of the dielectric layer, prevents short circuit problems between metal contact holes, and improves the performance and reliability of the semiconductor structure.
Smart Images

Figure CN112908931B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor technology, and in particular to a semiconductor structure and a method for forming the same. Background Art
[0002] Dynamic Random Access Memory (DRAM) is a semiconductor memory device commonly used in computers, consisting of many repeated storage units, each of which usually includes a capacitor and a transistor.
[0003] Among them, the storage cell is located in the storage area, and the storage area is next to the peripheral area, and the peripheral circuit is formed in the peripheral area, including transistors and interconnect structures. Generally speaking, the capacitor located in the storage area has a larger height, so it has better storage charge efficiency, which also makes the peripheral area and the storage area have a larger height difference. After forming the circuit in the peripheral area and the storage cell in the storage area, it is necessary to deposit a dielectric layer to cover the peripheral area and the storage area. Due to the height difference of the devices in the two areas, the dielectric layers in the two areas will also have a considerable height difference, which needs to be flattened later by etching or CMP.
[0004] In the prior art, defects are easily generated in the dielectric layer on the peripheral area, resulting in problems such as short circuits between metal contact holes formed on the peripheral area.
[0005] The performance of semiconductor structures in the existing technology needs to be further improved. Summary of the invention
[0006] The technical problem to be solved by the present invention is to provide a semiconductor structure and a method for forming the same, so as to improve the performance of the semiconductor structure.
[0007] In order to solve the above problems, the present invention provides a method for forming a semiconductor structure, comprising: providing a substrate, the substrate comprising a first region and a second region, a first device structure being formed on the first region, a second device structure being formed on the second region, the height of the first device structure being greater than the height of the second device structure, the first device structure having a sidewall that is at least partially recessed, the recess being located at the junction of the first region and the second region; forming a first dielectric layer with fluidity on the second region, the first dielectric layer filling the recess.
[0008] Optionally, the surface of the first dielectric layer is lower than the top of the first device structure; and further comprising: forming a second dielectric layer covering the first region and the second region above the first dielectric layer, wherein the hardness of the second dielectric layer is greater than that of the first dielectric layer.
[0009] Optionally, the first dielectric layer is a silicon oxide layer having doping elements, and the doping elements include at least one of phosphorus and boron; if the doping elements include phosphorus, the doping ratio of phosphorus is 3-10%, and if the doping elements include boron, the doping ratio of boron is 3-8%.
[0010] Optionally, the method for forming the first dielectric layer includes: depositing a first dielectric material layer on the substrate; and doping the first dielectric material layer by oblique ion implantation to form the first dielectric layer.
[0011] Optionally, the method for forming the first dielectric layer includes: depositing the first dielectric layer having a doping element on the substrate through an in-situ doping process.
[0012] Optionally, the method further includes: etching back the first dielectric layer so that a surface of the first dielectric layer is lower than a top of the first device structure.
[0013] Optionally, the method for forming the second dielectric layer includes: forming a second dielectric material layer covering the first region and the second region; and planarizing the second dielectric material layer using a chemical mechanical polishing process to form a second dielectric layer with a flat surface.
[0014] Optionally, the second device structure includes a metal connection layer, and also includes: forming a metal contact hole on the second region that penetrates the first dielectric layer and is connected to the metal connection layer at the bottom; a method for forming the metal contact hole includes: etching the first dielectric layer to form a through hole that penetrates the first dielectric layer and exposes a portion of the metal connection layer at the bottom; depositing a metal barrier layer on the inner wall surface of the through hole; depositing a metal layer that fills the through hole on the surface of the metal barrier layer, and annealing and reflowing the metal layer.
[0015] A specific embodiment of the present invention also provides a semiconductor structure, including: a substrate, the substrate including a first region and a second region, a first device structure is formed on the first region, a second device structure is formed on the second region, the height of the first device structure is greater than the height of the second device structure, the first device structure has a side wall that is at least partially recessed, and the recess is located at the junction of the first region and the second region; a first dielectric layer, located on the second region, the first dielectric layer fills the recess, and the first dielectric layer has fluidity.
[0016] Optionally, the surface of the first dielectric layer is lower than the top of the first device structure; and further includes: a second dielectric layer located above the first dielectric layer and covering the first region and the second region, wherein the hardness of the second dielectric layer is greater than that of the first dielectric layer.
[0017] Optionally, the first dielectric layer is a silicon oxide layer with doping elements, and the doping elements include at least one of phosphorus and boron; if the doping element includes phosphorus, the doping ratio of phosphorus is 3-10%, and if the doping element includes boron, the doping ratio of boron is 3-8%.
[0018] Optionally, the second device structure includes a metal connection layer and further includes: a metal contact hole penetrating through the first dielectric layer and connected to the metal connection layer.
[0019] Optionally, the metal contact hole comprises: a metal barrier layer covering the inner surface of a through hole penetrating the first dielectric layer; and a metal layer located on the surface of the metal barrier layer and filling the through hole, wherein the metal layer has been subjected to an annealing reflow treatment.
[0020] Optionally, the first device structure includes a memory cell array.
[0021] The method for forming a semiconductor structure of the present invention uses a first dielectric layer with high fluidity to fill the depression of the side wall of the first device structure on the first area, thereby avoiding defects in the first dielectric layer in the subsequent process flow, thereby improving the quality of the first dielectric layer and avoiding short circuit problems between metal contact holes subsequently formed in the first dielectric layer. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1a to Figure 1c A schematic diagram of a process for forming a semiconductor structure according to a specific embodiment of the present invention;
[0023] Figures 2 to 6 It is a structural schematic diagram of a formation process of a semiconductor structure according to another specific embodiment of the present invention. DETAILED DESCRIPTION
[0024] As described in the background art, in the prior art, short circuits are easily generated between metal contact holes in the peripheral area.
[0025] The inventors have found that this problem is caused by defects generated in the dielectric layer on the peripheral area during the planarization process of the dielectric layer.
[0026] For details, please refer to Figures 1a to 1c , is a schematic diagram of a process for forming a semiconductor structure in a specific embodiment of the present invention.
[0027] Please refer to Figure 1a, an etching stop layer 103 is formed on the surface of the substrate 101, a storage capacitor 104 is formed on the storage area 10 (for illustration only, the specific structure is not shown), a capacitor dielectric layer 105, a capacitor wire 106 filling the capacitor hole, a conductive layer 107 above the capacitor hole, and a protective layer 108 covering the surface of the conductive layer 107 are formed on the storage capacitor 104. Since the capacitor wire 106, the conductive layer 107 and the protective layer 108 will cover the storage area 10 and the peripheral area 20 at the same time when deposited, it is necessary to remove the capacitor wire 106, the conductive layer 107 and the protective layer 108 on the peripheral area 20 through an etching process. During the etching process, an etching side wall of the capacitor wire 106, the conductive layer 107 and the protective layer 108 will be generated at the junction of the storage area 10 and the peripheral area 20. Since it is easy to suffer from strong ion collisions during the etching process, a lateral etching profile is generated, resulting in a depression 1091 at the etching side wall.
[0028] Please refer to Figure 1b , the subsequently deposited dielectric layer 109 is likely to be incompletely filled in the recess 1091, and has problems such as holes 1092. In the subsequent grinding process of the dielectric layer 109, due to the extrusion effect, the dielectric layer 109 on the peripheral area 20 is subjected to pressure, and part of the dielectric material will fill the holes 1092 in the recess 1091, resulting in defects 1093 in the dielectric layer 108 on the peripheral area 20, resulting in a decrease in the quality of the dielectric layer 109.
[0029] Please refer to Figure 1c , metal contact holes 114 and 116 are formed on the peripheral region 20 of the substrate 100, penetrating the dielectric layer 109 and connected to the connection structure 102. In the process of forming the metal contact holes in the dielectric layer 109, the defects 1093 in the dielectric layer 109 are also filled with conductive materials to form a conductive channel 1094, thereby causing a short circuit between the metal contact holes 114 and 116.
[0030] In view of the above problems, the inventors propose a new semiconductor structure and a method for forming the same.
[0031] The specific implementation methods of the new semiconductor structure and the method for forming the same provided by the present invention are described in detail below with reference to the accompanying drawings.
[0032] Please refer to Figure 2 , providing a substrate 200, the substrate 200 includes a first region I and a second region II, a first device structure 210 is formed on the first region I, a second device structure is formed on the second region II, the height of the first device structure 210 is greater than the height of the second device structure, the first device structure 210 has a sidewall that is at least partially recessed, and the recess 211 is located at the junction of the first region I and the second region II.
[0033] The substrate 200 includes a semiconductor substrate, which includes single crystal silicon, silicon germanium, silicon on insulator, etc., and the semiconductor substrate may have an isolation structure, a doped region, etc. The substrate 200 may also include a device layer on the semiconductor substrate, and the device layer may include a transistor, a metal connection structure, a dielectric layer, etc. A barrier layer 201 is also formed on the surface of the substrate 200, which is used as an etching barrier layer in an etching process. Preferably, the barrier layer 201 may be made of silicon nitride.
[0034] In some specific embodiments, the semiconductor structure is a memory, the first region I is a storage region for forming a memory cell array; the second region II is a peripheral region for forming a peripheral logic circuit. The memory may be an SRAM memory, a NAND memory, a DRAM memory, etc. The first device structure 210 includes a memory cell array. In order to improve the storage density of the memory, the storage region of the existing memory usually has a higher height. For example, for a 3D NAND structure, the memory cells are stacked vertically; for a DRAM structure, a capacitor with a larger height is usually formed. Therefore, the height of the first device structure 210 on the first region I is greater than the height of the second device structure.
[0035] In other specific embodiments, the semiconductor structure may also be other device structures, including two or more regions, wherein the device structure on at least one region is higher than the device structure on the adjacent region. The height of the device structure is the maximum height of all devices on the region.
[0036] The second region first device structure 210 of this specific embodiment includes a memory cell array, specifically a DRAM cell array, each DRAM cell includes a capacitor and a transistor. The transistor is formed in the first region I of the substrate 200, and the capacitor is formed above the substrate 200 and is electrically connected to the transistor.
[0037] In this specific implementation, the first device structure 210 includes a storage capacitor 203 (for illustration only, the specific structure is not shown), and a capacitor dielectric layer 204, a conductive filling layer 205 filling a capacitor hole (not shown in the figure), a conductive layer 206 filling the capacitor hole and covering the capacitor hole, and a protective layer 207 covering the conductive layer 206 are formed on the storage capacitor 203. The storage capacitor 203 includes a capacitor hole formed by a lower plate, a capacitor dielectric layer 204, an upper plate, a conductive filling layer 205 filling the capacitor hole, and a conductive layer 206 covering the capacitor hole, which are sequentially deposited in the capacitor hole. The material of the capacitor dielectric layer 204 is ZAZ (ZrO x / Al2O3 / ZrOx ) or TZT(TiO x / ZrO x / TiO x ), the entire thickness is about 5 to 20 nm; the material of the conductive filling layer 205 is poly, SiGe, etc., with a thickness of about 100 nm to 200 nm; the material of the conductive layer 206 is a metal material such as W, Cu or Al, with a thickness of about 50 nm to 200 nm; the protective layer 207 is a dielectric material, such as silicon oxide, silicon oxynitride, etc., with a thickness of 50 nm to 200 nm.
[0038] Due to the comprehensive coverage of the film deposition, during the formation of the storage capacitor 203, the capacitor dielectric layer 204, the conductive filling layer 205, the conductive layer 206 and the protective layer 207 will be formed on the first region I and the second region II of the substrate 200 at the same time, and therefore, will cover the surface of the second region II of the substrate 200 at the same time. After the storage capacitor 203 is formed, the material layer on the surface of the second region II is removed by an etching process. Therefore, in this specific embodiment, the first device structure 210 has an etched sidewall at the junction of the first region I and the second region II. The etching process usually adopts anisotropic etching, and the bottom position of the first device structure 210 is easily hit by etching ions, resulting in a certain degree of lateral etching, thereby generating a depression 211. In other specific embodiments, the etched sidewall may also have a partially rough sidewall, resulting in a number of pits at the sidewall. In some specific embodiments, due to the characteristics of anisotropic etching, the etching angle of the lateral etching is usually 60° to 75°.
[0039] In other specific embodiments, due to the comprehensive coverage of the film deposition, as long as devices with different structures are formed on the first region I and the second region II, and the height of the device on the first region I is greater than the height on the second region II, in the process of etching and removing the film layer on the second region II, a certain degree of lateral etching will be caused to the bottom of the side wall of the first device structure 210, resulting in a certain degree of depression.
[0040] A logic circuit is formed on the second region II, including transistors located in the substrate 200 and metal interconnect structures located above the transistors and connecting the transistors. Figure 2 In the figure, only the metal connection layer 221 located on the top layer of the substrate 200 for connecting the logic circuit is shown.
[0041] Please refer to Figure 3 , a first dielectric layer 300 with fluidity is formed on the second region II, and the first dielectric layer 300 completely fills the recess 211 .
[0042] The fluidity of the first dielectric layer 300 is higher than that of dielectric layers deposited by conventional deposition processes such as CVD, HDPCVD, and ALD.
[0043] Since the size of the recess 211 is small, the recess 211 is easily closed before the recess 211 is completely filled during the deposition of the dielectric material, resulting in defects such as holes in the recess 211. Since the first dielectric layer 300 has a high fluidity, it has a certain fluidity during the deposition process, and the possibility of defects such as holes is small; even if the recess 211 is closed before it is fully filled, as the deposition process proceeds, due to stress and other reasons, part of the dielectric material will be squeezed into the recess 211, and finally the recess 211 will be filled.
[0044] In a specific embodiment of the present invention, the first dielectric layer 300 is a silicon oxide layer with doping elements, and the doping elements include at least one of phosphorus or boron. In some specific embodiments, if the doping element includes phosphorus, the doping ratio of phosphorus is 3-10%, and if the doping element includes boron, the doping ratio of boron is 3-8%. The doping of phosphorus or boron elements can make the first dielectric layer have higher fluidity. The fluidity of the first dielectric layer 300 can be adjusted by controlling the concentration of the doping elements therein. If the fluidity is too small, it cannot play the role of completely filling the recess 211; if the fluidity is too large, it is easy to cause deformation and other problems in subsequent processes such as grinding and etching. Therefore, it is necessary to control the fluidity of the first dielectric layer 300. In a specific embodiment, the material of the first dielectric layer 300 is phosphorus-doped silicon oxide, wherein the doping ratio of phosphorus is 3-10%. In another specific embodiment of the present invention, the material of the first dielectric layer 300 is boron-doped silicon oxide, wherein the doping ratio of boron is 3-8%.
[0045] The method for forming the first dielectric layer 300 includes: depositing a first dielectric material layer on the substrate 200; and doping the first dielectric material layer by inclined ion implantation to form the first dielectric layer 300. The deposition of the first dielectric material layer may be carried out by chemical vapor deposition (CVD), high density plasma chemical vapor deposition (HDPCVD), atomic layer vapor deposition (ALD) and other processes. The direction of the inclined ion implantation forms an acute angle with the surface of the substrate 100, which may be 60° to 80°, and is inclined toward the first region I to reduce the impact on the first region I. The fluidity of the first dielectric material layer is improved by doping ion implantation.
[0046] In this specific implementation manner, the surface of the first dielectric layer 300 is lower than the top of the first device structure 210 .
[0047] Preferably, the thickness of the first dielectric layer 300 may be 2000nm to 3000nm, which may be adjusted according to the height of the first device structure 210. In the process of depositing and forming the first dielectric material layer, the first dielectric material layer covers the first region I and the second region II. After the first dielectric material layer is formed, or before or after the inclined ion implantation, the first dielectric material layer may be etched back to remove the first dielectric material on the first region II, so that the height of the first dielectric material layer on the second region II is less than the height of the first device structure 210.
[0048] In other specific embodiments, an in-situ doping process may also be used to perform doping during the process of depositing the first dielectric material layer. The in-situ doping process mainly includes introducing a gas containing a doping element, such as a boron-containing or phosphorus-containing gas, into a deposition chamber during the deposition process. After the in-situ doping deposition, a first dielectric layer 300 having a height less than that of the first device structure 210 may also be formed by back etching, so that the surface of the first dielectric layer 300 is lower than the top of the first device structure 210.
[0049] In other specific implementations, a first dielectric layer 300 having a surface lower than the top of the first device structure 210 may be directly formed by using a fluid chemical vapor deposition process (FCVD).
[0050] In other specific implementations, the thickness of the first dielectric layer 300 may also be greater than the height of the first device structure 210 and cover the surface of the first device structure 210 as an interlayer dielectric layer covering the entire first region I and the second region II.
[0051] Please refer to Figure 4 A second dielectric layer 400 covering the first region I and the second region II is formed on the first dielectric layer 300 , and the hardness of the second dielectric layer 400 is greater than the hardness of the first dielectric layer 300 .
[0052] In this specific embodiment, the material of the second dielectric layer 400 is silicon oxide. In other specific embodiments, the material of the second dielectric layer 400 may also be insulating dielectric materials such as silicon oxynitride, silicon nitride, silicon oxycarbide, etc. The thickness of the second dielectric layer 400 may be 500nm to 1000nm.
[0053] The method for forming the second dielectric layer 400 includes: forming a second dielectric material layer covering the first region I and the second region II; and flattening the second dielectric material layer using a chemical mechanical polishing (CMP) process to form a second dielectric layer 400 with a flat surface. The second dielectric material layer can be formed by chemical vapor deposition (CVD), high density plasma chemical vapor deposition (HDPCVD), atomic layer vapor deposition (ALD) and other processes.
[0054] Generally, when the height difference of the material layer surface is large, if the CMP process is directly used for planarization, it will take a long time, and the long CMP process will cause a large stress impact on the underlying device, and will cause CMP non-uniformity in different regions. Therefore, it is usually necessary to first use an etching process to etch back to reduce the height difference, and then use CMP for planarization, and the process steps are relatively complicated. However, in a specific embodiment of the present invention, the first dielectric layer 300 has been formed on the second region II, reducing the height difference between the first region I and the second region II, so that the height difference of the second dielectric material layer formed on the two regions is small, and the CMP process can be directly used for planarization, thereby simplifying the process flow.
[0055] Furthermore, since the hardness of the second dielectric layer 400 is greater than that of the first dielectric layer 300, forming the second dielectric layer 400 on the surface of the first dielectric layer 300 can reduce the stress on the first dielectric layer 300 during the CMP process, making the surface of the second dielectric layer 400 flatter.
[0056] In other specific embodiments, the second dielectric layer 400 may not be formed, and the first dielectric layer 300 covers both the first region and the second region. In the process of planarizing the first dielectric layer using CMP, since the material fluidity of the first dielectric layer is relatively high and the hardness is relatively low, it is easy for the surface to have problems such as depressions during the CMP process.
[0057] Since the first dielectric layer 300 has completely filled the recess 211 , during the planarization process of the second dielectric layer 400 , even if the first dielectric layer 300 is squeezed, no dielectric material transfer will occur, and thus no defects will be generated in the first dielectric layer 300 .
[0058] Please refer to Figure 5 , the second dielectric layer 400 and the first dielectric layer 300 are etched to form a first through hole 501 penetrating the first dielectric layer 300 and exposing a portion of the metal connection layer 221 at the bottom; and a metal barrier layer 503 is deposited on the inner wall surface of the first through hole 501.
[0059] This specific implementation also includes forming a second through hole 502 on the first region I that penetrates the second dielectric layer 400 and the protective layer 206 and exposes a portion of the conductive layer 206 .
[0060] After forming the first through hole 501 and the second through hole 502, a metal barrier layer 503 is deposited on the inner wall surfaces of the first through hole 501 and the second through hole 502. The material of the metal barrier layer 503 is TiN or TaN, etc., which is used to block the metal ions of the subsequently filled metal layer from diffusing outward and improve the adhesion between the second dielectric layer 400 and the first dielectric layer 300.
[0061] The metal barrier layer 503 may be formed by a sputtering process. The thickness of the metal barrier layer 503 is 3 nm to 8 nm to achieve better barrier and adhesion effects.
[0062] The metal barrier layer 503 covers the inner walls of the first through hole 501 and the second through hole 502 , and the surface of the second dielectric layer 400 .
[0063] Please refer to Figure 6 , depositing a metal layer 600 filling the first through hole 501 and the second through hole 502 on the surface of the metal barrier layer 503, and performing an annealing reflow treatment on the metal layer 600; performing a planarization treatment to remove the metal barrier layer and the metal layer located on the surface of the second dielectric layer 400. The material of the metal layer 600 can be a metal material such as W or Cu.
[0064] Through the annealing reflow treatment, the filling morphology of the metal layer 600 in the through hole can be improved, the defects in the metal layer 600 can be reduced, and defects in the metal contact hole can be prevented.
[0065] During the annealing reflow treatment, the hardness of the first dielectric layer 300 can be further improved, thereby preventing the stress generated in the subsequent formation of the metal interconnect structure in the second dielectric layer 400 and other processes such as the dielectric layer from affecting the first dielectric layer 300, thereby improving the overall reliability of the semiconductor structure.
[0066] The above-mentioned method for forming a semiconductor structure uses a first dielectric layer with high fluidity to fill the depression of the side wall of the first device structure on the first area, thereby avoiding defects in the first dielectric layer in the subsequent process flow, thereby improving the quality of the first dielectric layer and avoiding short circuit problems between metal contact holes subsequently formed in the first dielectric layer.
[0067] A specific embodiment of the present invention also provides a semiconductor structure formed by the above method.
[0068] Please refer to Figure 6, which is a schematic structural diagram of a semiconductor structure according to a specific embodiment of the present invention.
[0069] The semiconductor structure includes: the substrate 200 includes a first region I and a second region II, a first device structure 210 is formed on the first region I, a second device structure is formed on the second region II, the height of the first device structure 210 is greater than the height of the second device structure, the first device structure 210 has a sidewall that is at least partially recessed, and the recess 211 is located at the junction of the first region I and the second region II. The semiconductor structure also includes a first dielectric layer 300, which is located on the second region II, the first dielectric layer 300 fills the recess 211, and the first dielectric layer 300 has fluidity.
[0070] The substrate 200 includes a semiconductor substrate, which includes single crystal silicon, silicon germanium, silicon on insulator, etc., and the semiconductor substrate may have an isolation structure, a doped region, etc. The substrate 200 may also include a device layer on the semiconductor substrate, and the device layer may include a transistor, a metal connection structure, a dielectric layer, etc. A barrier layer 201 is also formed on the surface of the substrate 200, which is used as an etching barrier layer in an etching process. Preferably, the barrier layer 201 may be made of silicon nitride.
[0071] In this specific implementation, the first device structure 210 includes a storage capacitor 203 (for illustration only, the specific structure is not shown), and a capacitor dielectric layer 204, a conductive filling layer 205 filling a capacitor hole (not shown in the figure), a conductive layer 206 filling the capacitor hole and covering the capacitor hole, and a protective layer 207 covering the conductive layer 206 are formed on the storage capacitor 203. The storage capacitor 203 includes a capacitor hole formed by a lower plate, a capacitor dielectric layer 204, an upper plate, a conductive filling layer 205 filling the capacitor hole, and a conductive layer 206 covering the capacitor hole, which are sequentially deposited in the capacitor hole. The material of the capacitor dielectric layer 204 is ZAZ (ZrOx / Al2O3 / ZrOx) or TZT (TiOx / ZrOx / TiOx), and the entire thickness is about 5 to 20 nm; the material of the conductive filling layer 205 is poly, SiGe, etc., and the thickness is about 100 nm to 200 nm; the material of the conductive layer 206 is a metal material such as W, Cu or Al, and the thickness is about 50 nm to 200 nm; the protective layer 207 is a dielectric material, such as silicon oxide, silicon oxynitride, etc., and the thickness is 50 nm to 200 nm.
[0072] Due to the comprehensive coverage of the film deposition, during the formation of the storage capacitor 203, the capacitor dielectric layer 204, the conductive filling layer 205, the conductive layer 206 and the protective layer 207 will be formed on the first region I and the second region II of the substrate 200 at the same time, and therefore, will cover the surface of the second region II of the substrate 200 at the same time. After the storage capacitor 203 is formed, the material layer on the surface of the second region II is removed by an etching process. Therefore, in this specific embodiment, the first device structure 210 has an etched sidewall at the junction of the first region I and the second region II. The etching process usually adopts anisotropic etching, and the bottom position of the first device structure 210 is easily hit by etching ions, resulting in a certain degree of lateral etching, thereby generating a depression 211. In other specific embodiments, the etched sidewall may also have a partially rough sidewall, resulting in a number of pits at the sidewall. In some specific embodiments, due to the characteristics of anisotropic etching, the etching angle of the lateral etching is usually 60° to 75°.
[0073] In other specific embodiments, due to the comprehensive coverage of the film deposition, as long as devices with different structures are formed on the first region I and the second region II, and the height of the device on the first region I is greater than the height on the second region II, in the process of etching and removing the film layer on the second region II, a certain degree of lateral etching will be caused to the bottom of the side wall of the first device structure 210, resulting in a certain degree of depression.
[0074] A logic circuit is formed on the second region II, including transistors located in the substrate 200 and metal interconnect structures located above the transistors and connecting the transistors. Figure 6 In the figure, only the metal connection layer 221 located on the top layer of the substrate 200 for connecting the logic circuit is shown.
[0075] Since the first dielectric layer 300 has high fluidity and high filling capacity and can completely fill the recess 211 , in the subsequent process flow, the dielectric material in the first dielectric layer 300 will no longer be transferred due to gaps or the like.
[0076] In a specific embodiment of the present invention, the first dielectric layer 300 is a silicon oxide layer with doped elements, and the doped elements are at least one of phosphorus or boron. The doping of phosphorus or boron elements can make the first dielectric layer have higher fluidity. The fluidity of the first dielectric layer 300 can be adjusted by controlling the concentration of the doped elements. If the fluidity is too small, it cannot play the role of completely filling the recess 211; if the fluidity is too large, it is easy to cause deformation and other problems in subsequent processes such as grinding and etching. Therefore, it is necessary to control the fluidity of the first dielectric layer 300. In a specific embodiment, the material of the first dielectric layer 300 is phosphorus-doped silicon oxide, wherein the doping ratio of phosphorus is 3 to 10%. In another specific embodiment of the present invention, the material of the first dielectric layer 300 is boron-doped silicon oxide, wherein the doping ratio of boron is 3 to 8%.
[0077] In this specific implementation manner, the surface of the first dielectric layer 300 is lower than the top of the first device structure 210 .
[0078] Preferably, the thickness of the first dielectric layer 300 may be 2000nm to 3000nm, which may be adjusted according to the height of the first device structure 210. In other specific embodiments, the thickness of the first dielectric layer 300 may also be greater than the height of the first device structure 210, and cover the surface of the first device structure 210 as an interlayer dielectric layer covering the entire first region I and the second region II.
[0079] In this specific implementation, the semiconductor structure further includes a second dielectric layer 400 located above the first dielectric layer 300 and covering the first region I and the second region II, and the hardness of the second dielectric layer 400 is greater than the hardness of the first dielectric layer 300. The surface of the second dielectric layer 400 is flat.
[0080] In this specific embodiment, the material of the second dielectric layer 400 is silicon oxide. In other specific embodiments, the material of the second dielectric layer 400 may also be insulating dielectric materials such as silicon oxynitride, silicon nitride, silicon oxycarbide, etc. The thickness of the second dielectric layer 400 may be 500nm to 1000nm.
[0081] The semiconductor structure further includes a metal contact hole penetrating the first dielectric layer 300 and connected to the metal connection layer 221. In this specific embodiment, a metal contact hole penetrating the second dielectric layer 400 and the protective layer 207 is also formed on the first region I. The metal contact hole includes: a metal barrier layer 503 covering the inner surface of the through hole; a metal layer 600 located on the surface of the metal barrier layer 503 and filling the through hole, and the metal layer 600 has been subjected to annealing and reflow treatment, so the filling morphology of the metal layer 600 is good.
[0082] The material of the metal barrier layer 503 is TiN or TaN, etc., which is used to prevent the metal ions of the subsequently filled metal layer from diffusing outward and improve the adhesion between the second dielectric layer 400 and the first dielectric layer 300.
[0083] The material of the metal layer 600 is metal such as W or Cu.
[0084] The first dielectric layer of the semiconductor structure will not have defects such as holes due to material transfer, thereby improving the quality of the first dielectric layer, avoiding problems such as short circuits between metal contact holes formed in the first dielectric layer, and further improving the reliability of the semiconductor structure.
[0085] The above is only a preferred embodiment of the present invention. It should be pointed out that ordinary technicians in this technical field can make several improvements and modifications without departing from the principle of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.
Claims
1. A method for forming a semiconductor structure, characterized in that: include: Providing a substrate, the substrate comprising a first region and a second region, a first device structure being formed on the first region, a second device structure being formed on the second region, the first device structure being taller than the second device structure, the first device structure having a sidewall that is at least partially concave, and the concave being located at a junction of the first region and the second region; forming a first dielectric layer with fluidity on the second area, wherein the first dielectric layer completely fills the recess; The first area is a storage area, and the second area is a peripheral area.
2. The method for forming a semiconductor structure according to claim 1, wherein: The surface of the first dielectric layer is lower than the top of the first device structure; and further comprising: forming a second dielectric layer covering the first region and the second region above the first dielectric layer, wherein the hardness of the second dielectric layer is greater than that of the first dielectric layer.
3. The method for forming a semiconductor structure according to claim 1, wherein: The first dielectric layer is a silicon oxide layer with doping elements, and the doping elements include at least one of phosphorus and boron; if the doping elements include phosphorus, the doping ratio of phosphorus is 3-10%, and if the doping elements include boron, the doping ratio of boron is 3-8%.
4. The method for forming a semiconductor structure according to claim 1, wherein: The method for forming the first dielectric layer comprises: depositing a first dielectric material layer on the substrate; and doping the first dielectric material layer by oblique ion implantation to form the first dielectric layer.
5. The method for forming a semiconductor structure according to claim 1, wherein: The method for forming the first dielectric layer comprises: depositing the first dielectric layer having doping elements on the substrate through an in-situ doping process.
6. The method for forming a semiconductor structure according to claim 4 or 5, characterized in that: Also includes: The first dielectric layer is etched back so that a surface of the first dielectric layer is lower than a top of the first device structure.
7. The method for forming a semiconductor structure according to claim 2, wherein: The method for forming the second dielectric layer includes: forming a second dielectric material layer covering the first region and the second region; and planarizing the second dielectric material layer using a chemical mechanical polishing process to form a second dielectric layer with a flat surface.
8. The method for forming a semiconductor structure according to claim 1, wherein: The second device structure includes a metal connection layer, and also includes: forming a metal contact hole on the second region that penetrates the first dielectric layer and is connected to the metal connection layer at the bottom; the method for forming the metal contact hole includes: etching the first dielectric layer to form a through hole that penetrates the first dielectric layer and exposes a portion of the metal connection layer at the bottom; depositing a metal barrier layer on the inner wall surface of the through hole; depositing a metal layer that fills the through hole on the surface of the metal barrier layer, and annealing and reflowing the metal layer.
9. A semiconductor structure, characterized in that: include: A substrate, the substrate comprising a first region and a second region, a first device structure is formed on the first region, a second device structure is formed on the second region, the first device structure is higher than the second device structure, the first device structure has a sidewall that is at least partially concave, and the concave is located at a junction of the first region and the second region; A first dielectric layer is located on the second area, the first dielectric layer completely fills the recess, and the first dielectric layer has fluidity; The first area is a storage area, and the second area is a peripheral area.
10. The semiconductor structure according to claim 9, characterized in that: The surface of the first dielectric layer is lower than the top of the first device structure; and the second dielectric layer is further included: a second dielectric layer located above the first dielectric layer and covering the first region and the second region, wherein the hardness of the second dielectric layer is greater than that of the first dielectric layer.
11. The semiconductor structure according to claim 9, characterized in that: The first dielectric layer is a silicon oxide layer with doping elements, and the doping elements include at least one of phosphorus and boron; if the doping elements include phosphorus, the doping ratio of phosphorus is 3-10%, and if the doping elements include boron, the doping ratio of boron is 3-8%.
12. The semiconductor structure according to claim 9, characterized in that: The second device structure includes a metal connection layer and also includes: a metal contact hole penetrating through the first dielectric layer and connected to the metal connection layer.
13. The semiconductor structure according to claim 12, characterized in that: The metal contact hole comprises: a metal barrier layer covering the inner surface of the through hole penetrating the first dielectric layer; a metal layer located on the surface of the metal barrier layer and filling the through hole, and the metal layer has been subjected to annealing and reflow treatment.
14. The semiconductor structure according to claim 9, characterized in that: The first device structure includes a memory cell array.
Citation Information
Patent Citations
Manufacturing method of flash memory
CN107221533A
Memory and forming method thereof
CN110137177A
Semiconductor structure
CN211088261U
Semiconductor integrated circuit device and a method of manufacturing the same
US20030139027A1
Semiconductor devices having dual trench, methods of fabricating the same, and electronic system having the same
US20110165757A1