A mold that makes the cross section of a double-chamfered shading ring non-shiny and non-luminous
By using a mold to stamp the double chamfer structure on the cross section of the shading ring, the problem of glare and ghosting caused by the shading ring in the prior art is solved, and the shooting quality is significantly improved.
Patent Information
- Application Number
- CN202110462559.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-04-27
- Publication Date
- 2025-01-24
- Estimated Expiration
- 2041-04-27
AI Technical Summary
The shading aperture in existing shooting lenses is prone to glare and ghosting, affecting shooting quality and reliability.
Design a mold to process the double chamfer structure on the cross section of the shading ring through stamping technology. The chamfer and arc spherical design are used to reduce the reflection of incident rays and reduce stray light in the lens.
It effectively reduces the glare and ghosting in the lens, improves the camera effect, and enhances the shooting quality and reliability of use.
Smart Images

Figure CN113147077B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of moulds, and more particularly to a mould capable of making the cross section of a double-chamfered shading ring non-bright and non-luminous. Background Art
[0002] As we all know, the shading ring plays a shading role, such as the shading ring of the mobile phone lens and the shading ring of the camera lens; it is a piece of Mylar sheet stamped and formed with shading materials such as SOMA or KIMOTO, and embedded in the lens; because it plays a shading role, everyone calls it a shading ring or a shading gasket; in recent years, with the rapid development of electronic products, mobile phones, tablets, and car-mounted products have higher and higher requirements for shooting pixels. With the development of science and technology, users also have higher and higher requirements for the quality of electronic products, so in addition to the continuous improvement of the quality of shooting equipment. The shading ring technology used in existing shooting lenses is also required to be higher and higher. On the parallel section with a certain thickness and parallel to the optical axis of the inner hole of the shading ring, after the light source is irradiated to this section, it is easy to form glare and ghosting through the section reflection to the imaging surface, thereby affecting the imaging quality of the shooting lens. The glare and ghosting formed by the shading ring in the traditional shooting lens are serious, resulting in the inability to improve the shooting quality and low reliability, so a mold that makes the double chamfered shading ring section non-shiny and non-luminous is proposed to solve the above problems. Summary of the invention
[0003] 1. Technical issues to be solved
[0004] The purpose of the present invention is to solve the shortcomings of the prior art and to propose a mold that makes the cross section of the double-chamfered shading ring non-bright and non-luminous.
[0005] 2. Technical solution
[0006] To solve the above problems, the present invention adopts the following technical solutions.
[0007] A mold that makes the cross section of a double chamfered shading ring non-shiny and non-luminous, comprising a mold handle, an upper mold base, a lower mold base and a lower pad, wherein the upper mold base is installed at the bottom of the mold handle, and the lower pad is fixedly installed on the top of the lower mold base, the upper mold base corresponds to the lower mold base and the upper mold base is located above the lower mold base, the top of the upper mold base is fixedly connected with an upper pad, the bottom of the upper pad is provided with an upper clamping plate, the top of the upper clamping plate is provided with a mounting groove, an inner pressure plate is provided in the mounting groove, and the top of the inner pressure plate is interspersed with There is an outer punch, the top of which extends to the inside of the upper pad, the bottom of which penetrates and extends to the bottom of the upper splint, an inner punch adapted to it is inserted inside the bottom of the outer punch, an outer sleeve of the outer punch is provided with an outer withdrawal sleeve adapted to it, the tangent surface of the outer withdrawal sleeve is T-shaped, the outer withdrawal sleeve is installed on the inner bottom wall of the mounting groove and the bottom of the outer withdrawal sleeve penetrates and extends to the bottom of the upper splint, and the bottoms of the outer punch, the inner punch and the outer withdrawal sleeve are all provided with processed chamfers.
[0008] As a further embodiment of the present invention:
[0009] Inner guide pillars are inserted on both the left and right sides of the upper pad, the top ends of the two inner guide pillars are respectively fixedly connected to the bottom of the upper mold base, and the bottom ends of the two inner guide pillars pass through the upper clamping plate respectively.
[0010] As a further embodiment of the present invention:
[0011] A spring is arranged in the installation groove and on the top of the inner pressure plate.
[0012] As a further embodiment of the present invention:
[0013] The tip of the chamfered bottom of the inner punch is in the shape of an arc spherical surface.
[0014] As a further embodiment of the present invention:
[0015] The width of the chamfered annular wall is between 0.005 mm and 0.012 mm.
[0016] 3. Beneficial effects
[0017] Compared with the prior art, the advantages of the present invention are:
[0018] After the mold design and processing of this scheme, the base groove is processed into a double chamfer structure, and the incident ray and the inclined surface of the hole wall where the incident point is located form a reflected ray that greatly reduces the entry into the lens, thereby improving the camera effect. Although the existing technology cannot completely and effectively eliminate stray light, it can greatly reduce glare and ghosting; the double-sided chamfering, in which the front and back chamfer depths are both 50%, makes it easier to wrap the substrate, making the substrate non-reflective, and the processing operation is simple, which is worthy of promotion. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] Figure 1 It is a structural schematic diagram of the present invention;
[0020] Figure 2 For the present invention Figure 1 Enlarged view of the middle and upper pad;
[0021] Figure 3 It is a schematic diagram of the structure of the inner punch in the present invention;
[0022] Figure 4 It is a bottom view of the outer material withdrawal sleeve in the present invention.
[0023] Description of the numbers in the figure:
[0024] 1. Die handle; 2. Upper die base; 3. Lower die base; 4. Lower pad; 5. Upper pad; 6. Upper clamp; 7. Mounting groove; 8. Inner pressure plate; 9. External punch; 10. Internal punch; 11. Inner guide pin; 12. External ejector sleeve; 13. Spring. DETAILED DESCRIPTION
[0025] The technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention; it is obvious that the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments, and all other embodiments obtained by ordinary technicians in this field based on the embodiments of the present invention without making creative work are within the scope of protection of the present invention.
[0026] See also Figures 1 to 4 A mold that makes the cross section of a double chamfered shading ring non-shiny and non-luminous, comprising a mold handle 1, an upper mold base 2, a lower mold base 3 and a lower pad 4, the upper mold base 2 is installed at the bottom of the mold handle 1, the lower pad 4 is fixedly installed on the top of the lower mold base 3, the upper mold base 2 corresponds to the lower mold base 3 and the upper mold base 2 is located above the lower mold base 3, the top of the upper mold base 2 is fixedly connected with an upper pad 5, the bottom of the upper pad 5 is provided with an upper clamping plate 6, the top of the upper clamping plate 6 is provided with a mounting groove 7, the mounting groove 7 is provided with an inner pressure plate 8, and the top of the inner pressure plate 8 is interspersed with an outer Punch 9, the top end of the outer punch 9 extends to the inside of the upper pad 5, the bottom of the outer punch 9 penetrates and extends to the bottom of the upper clamp 6, the inner bottom of the outer punch 9 is interspersed with an inner punch 10 adapted thereto, the outer side of the outer punch 9 is sleeved with an outer withdrawal sleeve 12 adapted thereto, the tangent surface of the outer withdrawal sleeve 12 is T-shaped, the outer withdrawal sleeve 12 is installed on the inner bottom wall of the mounting groove 7 and the bottom of the outer withdrawal sleeve 12 penetrates and extends to the bottom of the upper clamp 6, the bottoms of the outer punch 9, the inner punch 10 and the outer withdrawal sleeve 12 are all provided with processed chamfers.
[0027] When in use, the double-layer substrate is placed on the lower pad 4, and the outer punch 9, the inner punch 10 and the outer withdrawal sleeve 12 are driven to punch the substrate through the cooperation of the punching device, and the substrate is made into a double chamfered structure by processing the chamfer. The operation is simple and the processing is convenient. After processing, the chamfer of the substrate is about 20% deep on the front side and about 80% deep on the back side.
[0028] Furthermore, inner guide pillars 11 are interspersed on both sides of the upper pad 5 , the top ends of the two inner guide pillars 11 are fixedly connected to the bottom of the upper die base 2 , and the bottom ends of the two inner guide pillars 11 pass through the upper clamping plate 6 .
[0029] Furthermore, a spring 13 is provided in the mounting groove 7 and on the top of the inner pressure plate 8 .
[0030] Furthermore, the sharp corner of the chamfered bottom of the inner punch 10 is in the shape of an arc spherical surface, which is mirror-processed by a spark rack and the size of the sphere can be adjusted according to demand.
[0031] Furthermore, the width of the chamfered ring wall is between 0.005 mm and 0.012 mm.
[0032] A method for processing a mold that makes the cross section of a double-chamfered shading ring non-bright and non-luminous is invented, comprising the following steps:
[0033] 1) Place the double-layer substrate on the lower pad 4, with the upper clamping plate 6 on the substrate, and initially clamp the substrate by the upper clamping plate 6 and the lower pad 4;
[0034] 2) The die is pressed downward, and the substrate is pressed by the machined inclined surface of the outer withdrawal sleeve 12, the machined chamfer of the inner punch 10, and the arc spherical surface at the bottom thereof, so that the substrate rebounds to form a chamfer. After processing, the substrate is chamfered in a shape with a chamfer depth of 50% on both the front and back sides.
[0035] Through the above arrangement, after the cut surface is chamfered through mold processing, the incident ray and the inclined surface of the hole wall where the incident point is located form a reflected ray that greatly reduces the entry into the lens, thereby improving the camera effect. Although the existing technology cannot completely and effectively eliminate stray light, it can greatly reduce glare and ghosting, and the double-sided chamfering is more convenient for installation, without considering the front and back sides, saving installation time.
[0036] The above is only a preferred specific implementation of the present invention; however, the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical solution and its improved conception within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.
Claims
1. A mold for making the cross section of a double-chamfered shading ring non-shiny and non-luminous, comprising a mold handle (1), an upper mold base (2), a lower mold base (3) and a lower pad (4), characterized in that: The upper die base (2) is mounted on the bottom of the die handle (1), the lower pad (4) is fixedly mounted on the top of the lower die base (3), the upper die base (2) corresponds to the lower die base (3) and the upper die base (2) is located above the lower die base (3), the top of the upper die base (2) is fixedly connected with an upper pad (5), the bottom of the upper pad (5) is provided with an upper clamping plate (6), the top of the upper clamping plate (6) is provided with a mounting groove (7), the mounting groove (7) is provided with an inner pressure plate (8), the top of the inner pressure plate (8) is interspersed with an outer punch (9), the top of the outer punch (9) extends to the upper Inside the pad (5), the bottom of the outer punch (9) passes through and extends to the bottom of the upper clamp (6), the bottom of the outer punch (9) is interspersed with an inner punch (10) adapted thereto, the outer side of the outer punch (9) is sleeved with an outer material withdrawal sleeve (12) adapted thereto, the tangent surface of the outer material withdrawal sleeve (12) is T-shaped, the outer material withdrawal sleeve (12) is mounted on the inner bottom wall of the mounting groove (7) and the bottom of the outer material withdrawal sleeve (12) passes through and extends to the bottom of the upper clamp (6), and the bottoms of the outer punch (9), the inner punch (10) and the outer material withdrawal sleeve (12) are all provided with processed chamfers.
2. A mold for making the cross section of a double-chamfered shading ring non-bright and non-luminous according to claim 1, characterized in that: Inner guide pillars (11) are inserted on both left and right sides of the upper pad (5), the top ends of the two inner guide pillars (11) are respectively fixedly connected to the bottom of the upper die seat (2), and the bottom ends of the two inner guide pillars (11) respectively penetrate the upper clamping plate (6).
3. A mold for making the cross section of a double-chamfered shading ring non-bright and non-luminous according to claim 1, characterized in that: A spring (13) is provided in the installation groove (7) and at the top of the inner pressure plate (8).
4. A mold for making the cross section of a double-chamfered shading ring non-bright and non-luminous according to claim 1, characterized in that: The tip of the chamfered bottom of the inner punch (10) is in the shape of an arc spherical surface.
5. The mold for making the cross section of the double-chamfered shading ring non-shiny and non-luminous according to claim 1, characterized in that: The width of the chamfered annular wall is between 0.005 mm and 0.012 mm.
Citation Information
Patent Citations
Die for preventing cross section of double-chamfer shading ring from shining and emitting light