Magnetic sensor bias point adjustment method
By designing resistors with different number of TMR structures in Wheatsden bridges, the operation of non-zero bias field is achieved, the problem of zero bias field limitation in the prior art is solved, and the sensitivity and output of the magnetic field sensor are improved. Voltage.
Patent Information
- Application Number
- CN202080006387.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2019-12-30
- Filing Date
- 2020-03-20
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2040-03-20
AI Technical Summary
Existing Wheatsden bridges usually require a zero bias field in the initial state, which cannot meet the requirements of non-zero initial state in some applications, especially when using magnets to generate fields in position sensors, the TMR resistor detects magnetic field changes but is difficult to achieve. Non-zero bias field operation.
Design a Wheatsden bridge with four resistors, each containing multiple TMR structures, where two resistors have the same TMR structure and the other two resistors have the same but different TMR structure from the former , and realize a non-zero working bias field by adjusting the number and design of the TMR structure.
The Wheatsden bridge is realized to operate effectively under a non-zero bias field, which enhances the sensitivity and output voltage of the magnetic field sensor, and meets the needs of the non-zero bias field in applications.
Smart Images

Figure CN113167843B_ABST
Abstract
Description
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS
[0002] This application claims priority to U.S. Patent Application No. 16 / 730,726, filed on December 30, 2019, which claims the benefit of U.S. Provisional Patent Application Serial No. 62 / 892,395, filed on August 27, 2019, both of which are incorporated herein by reference in their entirety. Technical Field
[0003] Embodiments of the present disclosure generally relate to a Wheatstone bridge and a method for manufacturing the same. Background Art
[0004] A Wheatstone bridge is a circuit used to measure unknown resistance by balancing two legs of a bridge circuit, one of which contains the unknown component. The Wheatstone circuit provides extremely accurate measurements compared to a simple voltage divider.
[0005] The Wheatstone bridge includes a plurality of resistors, which in particular recently include magnetic materials, such as magnetic sensors. The magnetic sensors may include Hall effect magnetic sensors, anisotropic magnetoresistive sensors (AMR), giant magnetoresistive (GMR) sensors, and tunnel magnetoresistive (TMR) sensors. TMR sensors have very high sensitivity compared to other magnetic sensors.
[0006] While the initial state of the Wheatstone bridge typically requires a zero bias field, some applications require a non-zero initial state. For position sensor applications, a magnet is used to generate the field. The TMR resistors in the Wheatstone bridge detect the magnetic field from the magnet. First, there is a field acting on the sensor, and the field strength increases or decreases as the magnet moves closer to or away from the sensor.
[0007] Therefore, there is a need in the art for a Wheatstone bridge magnetic sensor that operates under a bias field. Summary of the invention
[0008] The present disclosure generally relates to a Wheatstone bridge having four resistors. Each resistor comprises a plurality of TMR structures. Two resistors have the same TMR structure. The remaining two resistors also have the same TMR structure, but the TMR structure is different from the other two resistors. In addition, the two resistors having the same TMR structure have a different amount of TMR structure than the remaining two resistors having the same TMR structure. Therefore, the operating bias field of the Wheatstone bridge is non-zero.
[0009] In one embodiment, a TMR sensor device includes a first resistor including a first plurality of TMR structures and a second resistor including a second plurality of TMR structures, wherein the number of the first plurality of TMR structures is greater than the number of the second plurality of TMR structures.
[0010] In another embodiment, a TMR sensor device includes: a plurality of resistors, each containing a plurality of TMR structures, wherein at least two resistors of the plurality of resistors contain different amounts of TMR structures, and wherein the TMR structures of the at least two resistors are different.
[0011] In another embodiment, a method of manufacturing a TMR sensor device includes: forming a first resistor including a first plurality of TMR structures; forming a second resistor including a second plurality of TMR structures; forming a third resistor including the first plurality of TMR structures; and forming a fourth resistor including the second plurality of TMR structures, wherein the first plurality of TMR structures are different from the second plurality of TMR structures. BRIEF DESCRIPTION OF THE DRAWINGS
[0012] In order to understand the above-mentioned features of the present disclosure in detail, the present disclosure briefly summarized above can be described in more detail with reference to embodiments, some of which are shown in the accompanying drawings. However, it should be noted that the accompanying drawings only show typical embodiments of the present disclosure and therefore should not be considered to limit the scope of the present disclosure, because the present disclosure may allow for other equally effective embodiments.
[0013] Figure 1 is a schematic illustration of a Wheatstone bridge design.
[0014] Figure 2A and 2B is a schematic illustration of a TMR structure according to one embodiment.
[0015] Figure 3A and 3B is a graph showing the operating bias fields of two different Wheatstone bridges.
[0016] Figure 4 is a schematic illustration of a Wheatstone bridge with multiple TMR structures for each resistor.
[0017] Figure 5 is a graph showing the calculated resistance response from a TMR structure with different arrays to adjust the operating bias point.
[0018] Figure 6 is a graph showing the operating bias points for various array configurations.
[0019] Figure 7is a flow chart illustrating a method of manufacturing a Wheatstone bridge.
[0020] To facilitate understanding, identical element numerals have been used, where possible, to designate identical elements that are common to the figures. It is contemplated that elements disclosed in one embodiment may be beneficially utilized on other embodiments without specific recitation. DETAILED DESCRIPTION
[0021] Hereinafter, reference is made to embodiments of the present disclosure. However, it should be understood that the present disclosure is not limited to the specific described embodiments. In fact, any combination of the following features and elements (whether or not related to different embodiments) is carefully considered to implement and practice the present disclosure. In addition, although the embodiments of the present disclosure can achieve advantages that are superior to other possible solutions and / or superior to the prior art, whether a specific advantage is achieved by a given embodiment does not limit the present disclosure. Therefore, the following aspects, features, embodiments and advantages are merely illustrative and should not be regarded as elements or limitations of the appended claims unless explicitly stated in the claims. Similarly, reference to "the present disclosure" should not be interpreted as a generalization of any inventive subject matter disclosed herein, and should not be regarded as elements or limitations of the appended claims unless explicitly stated in the claims.
[0022] The present disclosure generally relates to a Wheatstone bridge having four resistors. Each resistor comprises a plurality of TMR structures. Two resistors have the same TMR structure. The remaining two resistors also have the same TMR structure, but the TMR structure is different from the other two resistors. In addition, the two resistors having the same TMR structure have a different amount of TMR structure than the remaining two resistors having the same TMR structure. Therefore, the operating bias field of the Wheatstone bridge is non-zero.
[0023] Figure 1 1 is a schematic illustration of a Wheatstone bridge 100 design. The bridge 100 includes a bias source 102, a first resistor 104, a second resistor 106, a third resistor 110, a fourth resistor 108, a first output pad 112, a second output pad 114, and a ground connection 116. A bias voltage is applied across the bridge from the bias source 102 to the ground connection 116. The bridge output is the potential difference across the first output pad 112 and the second output pad 114. Any change in resistance due to temperature variations from the resistors 104, 106, 108, 110 is invalid due to the nature of the differential output.
[0024] As discussed herein, resistors 104, 106, 108, 110 are each made of a TMR film. In one embodiment, the TMR resistors are each distinct and different, such that resistors 104, 106, 108, 110 have different resistances. In another embodiment, the TMR films are the same, but resistors 104, 106, 108, 110 are different. In yet another embodiment, resistors 104, 110 are identical to one another (as are the TMR films from which resistors 104, 110 are made), and resistors 106, 108 are identical to one another (as are the TMR films from which resistors 106, 108 are made) but are different from resistors 104, 110.
[0025] Typical magnetic field sensors use TMR resistors in a Wheatstone bridge circuit. TMR resistors must have different responses to the magnetic field in order to generate a differential output voltage. As discussed in this article, a new method of manufacturing a magnetic field sensor will manufacture two different TMR films in the same layer. The reliability and performance of the TMR film determines the magnetoresistive response. In this way, combined with different TMR film features, a perfect Wheatstone bridge design for a magnetic field sensor can be manufactured.
[0026] about Figure 1 If the free layer of the TMR film making resistors 104, 106, 108, and 110 has a long axis that is +45° or -45° relative to the magnetization direction of the pinned layer, the easy axis of the free layer is constrained to be along the long axis due to shape anisotropy, and the magnetization direction can be set bidirectionally along the long axis by the Ampere field from a set line, which is located on the top of the free layer and orthogonal to the long axis of the free layer.
[0027] When a magnetic field is applied along the Y axis, the resistance of 110 and 104 increases with the magnetic field, while the resistance of 106, 108 decreases with the magnetic field. This different response enables a Wheatstone bridge, and the sensor sensitivity is proportional to the output voltage, which is proportional to the resistance difference between resistor 110 (or resistor 104) and resistor 106 (or resistor 108). However, due to the 45° free layer or pinned layer initial state, only half of the magnetoresistance change is used. If the free layer to pinned layer initial magnetization state can be set to 90° and still have two different magnetoresistance changes, the full range of magnetoresistance changes will be used, and the sensor sensitivity can be increased by a factor of two.
[0028] The pinned layer magnetization direction is set by the magnetic annealing direction. Typically, resistors 104, 106, 108, 110 are made of the same TMR film and undergo the same process, and therefore all have the same pinned layer direction. Each device can operate at a full MR ratio, but all devices respond to external fields in the same way, and therefore there is no output voltage at all. A simple way to solve this problem is to shield resistors 106 and 108 by covering them with a thick NiFe film so that resistors 106 and 108 will not respond to the magnetic field. Alternatively, resistors 106 and 108 can be replaced with constant resistors. However, this type of half-bridge sensing scheme will also reduce the output voltage and therefore limit the sensitivity.
[0029] Figure 2A and 2B is a schematic illustration of a TMR structure 200, 250 according to one embodiment. It should be understood that the terms "TMR resistor" and "TMR structure" are used interchangeably. The TMR resistors 200, 250 each include a seed layer 202, 252 to be formed on a bottom conductive line (not shown). In one embodiment, the seed layer 202, 252 includes a conductive material such as ruthenium, and has a thickness between about 10 angstroms and about 100 angstroms, and is deposited by a well-known deposition method such as electroplating, electroless plating, or sputtering. In addition, it should be understood that although ruthenium has been exemplified as the seed layer 202, 252 material, other materials are contemplated, and the embodiments discussed herein are not limited to the use of ruthenium for the seed layer 202, 252. In addition, the seed layers 202, 252 are deposited simultaneously.
[0030] An antiferromagnetic (AFM) layer 204, 254 is disposed on the seed layer 204, 254. Suitable materials for the AFM layer 204, 254 include IrMn, NiMn, PdMn, or PtMn with a thickness between about 40 angstroms and about 500 angstroms. The AFM layer 204, 254 can be formed by well-known deposition methods such as sputtering. In addition, it should be understood that although IrMn, NiMn, PdMn, and PtMn have been exemplified as AFM layer 204, 254 materials, other materials are contemplated, and the embodiments discussed herein are not limited to using IrMn, PdMn, NiMn, or PtMn for the AFM layer 204, 254. In addition, the AFM layer 204, 254 is deposited simultaneously.
[0031] The pinning layer 206, 256 is disposed on the AFM layer 204, 254. Suitable materials for the pinning layer 206, 256 include CoFe or Co / CoFe / Co multilayer stacks with a thickness between about 20 angstroms and about 30 angstroms. The pinning layer 206, 256 can be formed by well-known deposition methods such as sputtering. In addition, it should be understood that although CoFe or Co / CoFe / Co has been exemplified as the pinning layer 206, 256 material, other materials are carefully considered, and the embodiments discussed herein are not limited to using CoFe or Co / CoFe / Co for the pinning layer 206, 256. In addition, the pinning layers 206, 256 are deposited simultaneously.
[0032] The spacer layer 208, 258 is disposed on the pinning layer 206, 256. Suitable materials for the spacer layer 208, 258 include Ru with a thickness between about 4 angstroms and about 10 angstroms. The spacer layer 208, 258 can be formed by well-known deposition methods such as sputtering. In addition, it should be understood that although ruthenium has been exemplified as the spacer layer 208, 258 material, other materials are contemplated and the embodiments discussed herein are not limited to the use of ruthenium for the spacer layer 208, 258. In addition, the spacer layers 208, 258 are deposited simultaneously.
[0033] Reference layers 210, 260 are disposed on spacer layers 208, 258. Suitable materials for reference layers 210, 260 include CoFe / Ta / CoFeB / CoFe as a multilayer stack. The thickness of the first CoFe layer may be between about 8 angstroms and about 10 angstroms. The thickness of the Ta layer may be between about 0.5 angstroms and about 2 angstroms. The thickness of the CoFeB layer may be between about 10 angstroms and about 15 angstroms. The thickness of the second CoFe layer may be between about 3 angstroms and about 10 angstroms. Reference layers 210, 260 may be formed by well-known deposition methods such as sputtering. In addition, it should be understood that although CoFe / Ta / CoFeB / CoFe has been exemplified as reference layer 210, 260 materials, other materials are contemplated and the embodiments discussed herein are not limited to using CoFe / Ta / CoFeB / CoFe for reference layers 210, 260. In addition, reference layers 210, 260 are deposited simultaneously.
[0034] Barrier layers 212, 262 are disposed on reference layers 210, 260. Suitable materials for barrier layers 212, 262 include MgO having a thickness between about 10 angstroms and about 20 angstroms. It should be understood that while MgO is illustrated as barrier layers 212, 262, other insulating materials are contemplated. Furthermore, barrier layers 212, 262 are deposited simultaneously.
[0035] The first free layer 214, 264 is disposed on the barrier layer 212, 262. Suitable materials for the first free layer 214, 264 include a CoFe / CoFeB / Ta / NiFe multilayer stack. The thickness of the first CoFe layer may be between about 3 angstroms and about 10 angstroms. The thickness of the CoFeB layer may be between about 10 angstroms and about 20 angstroms. The thickness of the Ta layer may be between about 0.5 angstroms and about 2 angstroms. The thickness of the NiFe layer may be between about 3 angstroms and about 300 angstroms, for example, between about 3 angstroms and about 10 angstroms or between about 10 angstroms and about 300 angstroms. The first free layer 214, 264 may be formed by a well-known deposition method such as sputtering. In addition, it should be understood that although CoFe / CoFeB / Ta / NiFe has been exemplified as the first free layer 214, 264 material, other materials are carefully considered, and the embodiments discussed herein are not limited to using CoFe / CoFeB / Ta / NiFe for the first free layer 214, 264. Furthermore, the first free layers 214, 264 are deposited simultaneously.
[0036] An additional spacer layer 216 is disposed on the first free layer 214. In one embodiment, the spacer layer 216 is a multilayer structure including Co / Ru / Co. It should be understood that the spacer layer 216 can be a single layer or other multilayer stack including a first magnetic layer, a non-magnetic conductive layer, and a second magnetic layer. In an embodiment where the spacer layer 216 is Co / Ru / Co, the thickness of the first Co layer can be between about 3 angstroms and about 6 angstroms, the thickness of the Ru layer can be between about 6 angstroms and about 10 angstroms, and the thickness of the second Co layer can be between about 3 angstroms and about 6 angstroms. The Co layer is to enhance synthetic antiferromagnetic (SAF) coupling. The spacer layer 216 can be formed by well-known deposition methods such as sputtering.
[0037] The second free layer 218 is disposed on the spacer layer 216. Suitable materials for the second free layer 218 include NiFe. The thickness of the NiFe layer can be between about 100 angstroms and about 300 angstroms, for example, between about 100 angstroms and about 200 angstroms (the moment of the second free layer 218 is greater than the magnetic moment of the first free layer 214) or between about 200 angstroms and about 300 angstroms. The second free layer 218 can be formed by well-known deposition methods such as sputtering. In addition, it should be understood that although NiFe has been exemplified as the second free layer 218 material, other materials are carefully considered, and the embodiments discussed herein are not limited to using NiFe for the second free layer 218. The first free layer 214, together with the spacer layer 216 and the second free layer 218, form a non-equilibrium synthetic AFM structure.
[0038] For a Wheatstone bridge, all resistors may not be identical. In practice, resistors 104, 110 are identical to each other, and resistors 106, 108 are identical to each other and different from resistors 104, 110. TMR sensor 250 will represent resistors 106, 108 subject to additional processing.
[0039] Another magnetic layer 270 is deposited on the exposed first free layer 264 of the TMR 250. The composition of the other magnetic layer 270 is substantially equivalent to the second free layer 218, but will have a thickness substantially equal to the combined thickness of the spacer layer 216 and the second free layer 218. Suitable materials for the second magnetic layer 270 include NiFe. The thickness of the NiFe layer can be between about 100 angstroms and about 320 angstroms, such as between about 100 angstroms and about 200 angstroms, or between about 200 angstroms and about 320 angstroms. The magnetic layer 270 can be formed by well-known deposition methods such as sputtering or ion beam deposition. In addition, it should be understood that although NiFe has been exemplified as a magnetic layer 270 material, other materials are contemplated, and the embodiments discussed herein are not limited to using NiFe for the magnetic layer 270.
[0040] The cap layer may be formed over the second free layer 218 and the second magnetic layer 270. The TMR structures 200, 250 are annealed in a magnetic furnace at a temperature between about 250 degrees Celsius and about 300 degrees Celsius at a magnetic field between about 10,000 Oersted and about 50,000 Oersted. The second magnetic layer 270 has a magnetic moment greater than the magnetic moment of the first free layer 214, 264. It should be understood that the second magnetic layer 270 has a thickness greater than the thickness of the first free layer 264. In the TMR structure 250, the second magnetic layer 270 is ferromagnetically coupled to the first free layer 264, and the first free layer 264 will provide magnetic resistance. After annealing, the pinned layers 206, 256 are pinned in the -Z direction, and the reference layers 210, 260 have a magnetic moment in the +Z direction. The hard bias field HBias is shown by arrow 272. When a hard bias field is applied, the first free layer 214 of the TMR structure 200 has a magnetic moment, indicated by arrow 276, which is antiparallel to the magnetic moment, indicated by arrow 278, of the first free layer 264 of the TMR structure 250. In addition, the second free layer 218 and the second magnetic layer 270 have parallel magnetic moments under the applied hard bias, indicated by arrows 274, 280. Under the same hard bias field, the magnetic moment of the first free layer 214 is antiparallel to the magnetic moment of the second free layer 218, while the magnetic moment of the first free layer 264 is parallel to the magnetic moment of the second magnetic layer 270.
[0041] Figure 3A and 3B is a graph showing the operating bias fields of two different Wheatstone bridges. Film A may be referred to as TMR structure 200 , while film B may be referred to as TMR structure 250 . Figure 3APoint A in is where the lines of membrane A and membrane B intersect. Figure 3A In the example, point A is at a position where the bias field is zero. As discussed above, typically, the user requires the position where the lines of film A and film B intersect to be a non-zero position. Therefore, the displacement of the lines to either or both of film A or film B can be used to accommodate the user's need for a non-zero position. Figure 3B , point B is where the lines of membrane A and membrane B cross, which is at a non-zero position. The non-zero position is shown as -350 Oersted, but it should be understood that the position does not have to be -350 Oersted, but can be selected by the user. Thus, the Wheatstone bridge can be designed to meet user needs as discussed below.
[0042] Figure 4 is a schematic illustration of a Wheatstone bridge 400 having multiple TMR structures for each resistor R1, R2, R3, R4. R1 may correspond to resistor 104; R2 may correspond to resistor 106; R3 may correspond to resistor 110; and R4 may correspond to resistor 108. When the working field bias is set to 0, then R1=R2=R3=R4. In addition, based on the TMR structure, resistors R1 and R3 are different from resistors R2 and R4 to provide two different magnetoresistive responses.
[0043] In the Wheatstone bridge 400, each resistor R1, R2, R3, R4 includes multiple TMR structures 200, 250. More specifically, in one embodiment, resistors R1 and R3 will include multiple TMR structures 200, and resistors R2 and R4 will include multiple TMR structures 250. In another embodiment, resistors R1 and R3 will include multiple TMR structures 250, and resistors R2 and R4 will include multiple TMR structures 200. For simplicity, Figure 4 Resistors R1 and R3 are shown to have TMR structures 200, while resistors R2 and R4 have TMR structures 250. The number and design of the TMR structures 200, 250 in resistors R1 and R3 are both the same. Similarly, the number and design of the TMR structures 200, 250 in resistors R2 and R4 are both the same.
[0044] Typical magnetic field sensors use MR devices in a Wheatstone bridge circuit. The key is to change the MR in different ways in the bridge. Herein, the magnetic field sensor has an adjustable bias point. Two different sets of TMR structures 200, 250 have two different magnetoresistance responses. Both TMR structures 200, 250 have free layer and pinned layer magnetic moments that are orthogonal to each other, but the magnetoresistance responses are reversed (i.e., the resistance of one TMR structure increases linearly with the external magnetic field, while the resistance of the other TMR structure decreases linearly with the external magnetic field). In addition, the bias point can be adjusted to operate within a given external magnetic field range.
[0045] When the user needs a Wheatstone bridge with a non-zero operating field bias, adjustments to the resistors need to be made. In the embodiments discussed herein, the resistance area (RA) is the same for all TMR structures 200, 250. More specifically, the TMR structures 200, 250 have the same height, length, and width. In order to cause a non-zero operating field bias, resistors R1 and R3 have a set number of TMR structures 200, and resistors R2 and R4 have a set number of TMR structures 250 that are different from the set number of TMR structures 200 of resistors R1 and R3. Different numbers of TMR structures 200, 250 result in a non-zero bias field. If resistors R1-R4 all have the same number of TMR structures 200, 250 and all have the same RA, the operating field bias will be zero. By making resistors R1 and R3 different in number from the TMR structures of resistors R2 and R4, the operating field bias is non-zero. Furthermore, although the number of TMR structures is different, RA is the same for all TMR structures 200 , 250 , even though different resistors R1 - R4 have different TMR structures 200 , 250 .
[0046] for Figure 4 In the embodiment shown in FIG. 2 , the RA of the TMR structure 200 is equal to the RA of the TMR structure 250. The magnetoresistance of the TMR structures 200, 250 is the same. For the resistors R1-R4, there are multiple TMR structures 200, 250 connected in series in an array.
[0047] In one embodiment, resistors R1 and R3 have a plurality of TMR structures 200 arranged in an array, and resistors R2 and R4 have a plurality of TMR structures 250 arranged in an array; and the number of TMR structures 200 of resistors R1 and R3 is greater than the number of TMR structures 250 of resistors R2 and R4. In another embodiment, resistors R1 and R3 have a plurality of TMR structures 250 arranged in an array; resistors R2 and R4 have a plurality of TMR structures 200 arranged in an array; and the number of TMR structures 250 of resistors R1 and R3 is greater than the number of TMR structures 200 of resistors R2 and R4. In any embodiment, the RA of the TMR structures 200, 250 is the same.
[0048] Figure 5 is a graph showing the calculated resistance response from a TMR structure with different arrays to adjust the operating bias point. Figure 5As shown, resistors R1 and R3 each have an array of 42 TMR structures 200. Resistors R2 and R4 have fewer TMR structures 250 than resistors R1 and R3. If the number of TMR structures 200, 250 of resistors R1-R4 is equal, the lines of resistors R2 and R4 will cross the lines of resistors R1 and R3 at 0. In the case of 30 TMR structures 250 for resistors R2 and R4, the operating bias field is about -250 Oersted. In the case of 26 TMR structures 250 for resistors R2 and R4, the operating bias field is about -350 Oersted. In the case of 20 TMR structures 200, 250 for resistors R2 and R4, the operating field bias is about -500 Oersted. Therefore, changing the number of TMR structures of one pair of resistors R1 and R3 to be different from the number of TMR structures of another pair of resistors R2 and R4 achieves a non-zero bias field to meet consumer demand.
[0049] Figure 6 is a graph showing the operating bias points for various array configurations. Figure 6 As shown in FIG. 1 , when the number of TMR structures 200 is set to 42 for resistors R1 and R3, then the number of TMR structures 250 for resistors R2 and R4 can be selected to achieve a specific bias point. In operation, the end user selects a specific range of bias points. The manufacturer then selects the midpoint of the range and manufactures a corresponding number of TMR sensors 250 for the two resistors R2 and R4 to achieve the pre-selected midpoint of the operating field bias.
[0050] It should be understood that although reference has been made to 42 TMR structures 200 for a set of resistors R1 and R3, the number of TMR structures 200 is not limited. In fact, the number of TMR structures 200, 250 for resistors R1-R4 can be selected to achieve a desired operating field bias point. As long as RA is equal for all TMR structures 200, 250, the number of TMR structures 200, 250 for resistors R1-R4 can be selected to achieve a desired operating bias field point.
[0051] Figure 7 7 is a flow chart illustrating a method 700 of manufacturing a Wheatstone bridge. The method operates by initially receiving a working field range from a user in step 702. Next, the number of TMR structures is set for the two resistors in step 704. Subsequently, in step 706, based on the set number of TMR structures for the two resistors, the number of TMR structures necessary to achieve the midpoint of the working field range selected by the user is determined. Finally, in step 708, the desired number of TMR structures for each resistor is simultaneously manufactured.
[0052] In one embodiment, a TMR sensor device includes: a first resistor including a first plurality of TMR structures; and a second resistor including a second plurality of TMR structures, wherein the number of the first plurality of TMR structures is greater than the number of the second plurality of TMR structures. The TMR structures in the first plurality of TMR structures are identical to each other. The TMR structures in the second plurality of TMR structures are identical to each other. The TMR structures in the first plurality of TMR structures are different from the TMR structures in the second plurality of TMR structures. The device further includes: a third resistor including a third plurality of TMR structures; and a fourth resistor including a fourth plurality of TMR structures. The number of the third plurality of TMR structures is greater than the number of the fourth plurality of TMR structures. The number of the third plurality of TMR structures is equal to the number of the first plurality of TMR structures. The number of the fourth plurality of TMR structures is equal to the number of the second plurality of TMR structures. The TMR structures in the third plurality of TMR structures are identical to each other. The TMR structures in the fourth plurality of TMR structures are identical to each other. The TMR structures in the third plurality of TMR structures are equivalent to the TMR structures in the first plurality of TMR structures. The TMR structures in the fourth plurality of TMR structures are equivalent to the TMR structures in the second plurality of TMR structures.
[0053] In another embodiment, a TMR sensor device includes: a plurality of resistors, each of which contains a plurality of TMR structures, wherein at least two of the plurality of resistors contain different amounts of TMR structures, and wherein the TMR structures of the at least two resistors are different. The plurality of resistors have substantially the same RA. The TMR sensor device has a bias point that is non-zero Oersted. At least one TMR structure contains a synthetic antiferromagnetic structure. There are more TMR structures that contain synthetic antiferromagnetic structures than TMR structures that do not contain synthetic antiferromagnetic structures.
[0054] In another embodiment, a method of manufacturing a TMR sensor device includes: forming a first resistor including a first plurality of TMR structures; forming a second resistor including a second plurality of TMR structures; forming a third resistor including the first plurality of TMR structures; and forming a fourth resistor including the second plurality of TMR structures, wherein the first plurality of TMR structures are different from the second plurality of TMR structures. The third resistor is substantially the same as the first resistor. The number of the first plurality of TMR structures is more than twice the number of the second plurality of TMR structures.
[0055] In one embodiment, the TMR sensor is used in a camera and operates as a single-axis sensor. An example of this sensor can be found in U.S. Patent Application Publication No. 2019 / 0020822A1, which is incorporated herein by reference. However, upon careful consideration, the TMR sensor can be used as a two-dimensional or even three-dimensional sensor. In addition, upon careful consideration, the TMR sensor can be integrated and utilized in inertial measurement unit technologies other than cameras, such as wearable devices, compasses, and MEMS devices. In addition, the TMR sensor can be operated as a position sensor, a bridge angle sensor, a magnetic switch, a current sensor, or a combination thereof. The TMR sensor can be used to focus a camera such as a smartphone camera by using the TMR sensor as a position and angle sensor. In addition, the TMR sensor can be used as a switch, current, and angle sensor in the automotive industry to replace the current Hall, anisotropic magnetoresistive (AMR), and giant magnetoresistive (GMR) sensors. TMR sensors can also be used as position and angle sensors in drones and robotics industries. Medical devices can also use TMR sensors for flow rate control of infusion systems and endoscope camera sensors, etc. Therefore, the TMR sensors discussed herein are well suited for applications other than smartphone cameras, and therefore should not be limited to use as sensors for smartphone cameras.Furthermore, the TMR sensors need not be arranged in a Wheatstone bridge arrangement, but may be arranged in any number of ways.
[0056] By changing the number of TMR structures within a particular set of resistors in a Wheatstone bridge while keeping the RA of all TMR structures constant, the operating bias field point can be adapted to meet the needs of the user.
[0057] While the foregoing is directed to embodiments of the present disclosure, other and further embodiments of the disclosure may be devised without departing from the basic scope of the disclosure, which is determined by the claims that follow.
Claims
1. A tunnel magnetoresistance sensor device, i.e., a TMR sensor device, comprising: a first resistor comprising a first plurality of TMR structures; a second resistor comprising a second plurality of TMR structures, wherein the number of the first plurality of TMR structures is greater than the number of the second plurality of TMR structures; a third resistor comprising a third plurality of TMR structures; as well as a fourth resistor comprising a fourth plurality of TMR structures, wherein the number of the third plurality of TMR structures is greater than the number of the fourth plurality of TMR structures, wherein the first resistor, the second resistor, the third resistor and the fourth resistor have the same resistance area and form a Wheatstone bridge; Wherein the TMR structure in the third plurality of TMR structures is the same as the TMR structure in the first plurality of TMR structures, and wherein the TMR structure in the fourth plurality of TMR structures is the same as the TMR structure in the second plurality of TMR structures. 2 . The TMR sensor device of claim 1 , wherein the TMR structures in the first plurality of TMR structures are identical to one another. 3 . The TMR sensor device of claim 2 , wherein the TMR structures in the second plurality of TMR structures are identical to one another. 4 . The TMR sensor device of claim 3 , wherein the TMR structure in the first plurality of TMR structures is different from the TMR structure in the second plurality of TMR structures. 5 . The TMR sensor device of claim 1 , wherein the number of the third plurality of TMR structures is equal to the number of the first plurality of TMR structures. 6 . The TMR sensor device of claim 5 , wherein the number of the fourth plurality of TMR structures is equal to the number of the second plurality of TMR structures. 7 . The TMR sensor device of claim 6 , wherein the TMR structures in the third plurality of TMR structures are identical to one another. 8 . The TMR sensor device of claim 7 , wherein the TMR structures in the fourth plurality of TMR structures are identical to one another.
9. The TMR sensor device of claim 1, wherein an operating field bias of the TMR sensor device is non-zero.
10. A TMR sensor device comprising: A plurality of resistors forming a Wheatstone bridge and each containing a plurality of TMR structures, the plurality of resistors having the same resistance area, wherein: At least two resistors of the plurality of resistors contain different amounts of TMR structures, The TMR structures of the at least two resistors are different, At least one TMR structure contains a synthetic antiferromagnetic structure, The number of TMR structures including the synthetic antiferromagnetic structure is greater than that of TMR structures not including the synthetic antiferromagnetic structure.
11. The TMR sensor device of claim 10, wherein the TMR sensor device has a bias point that is non-zero Oersted. 12 . The TMR sensor device of claim 10 , wherein at least two resistors of the plurality of resistors contain the same number of TMR structures. 13 . The TMR sensor device of claim 10 , wherein each TMR structure has the same height, the same length, and the same width.
14. A method of manufacturing a TMR sensor device, comprising: forming a first resistor including a first plurality of TMR structures; forming a second resistor including a second plurality of TMR structures, wherein the number of the first plurality of TMR structures is more than twice the number of the second plurality of TMR structures; forming a third resistor including a third plurality of TMR structures, the third plurality of TMR structures being identical to the first plurality of TMR structures; as well as forming a fourth resistor including a fourth plurality of TMR structures, the fourth plurality of TMR structures being identical to the second plurality of TMR structures, wherein the first plurality of TMR structures are different from the second plurality of TMR structures, The first resistor, the second resistor, the third resistor and the fourth resistor have the same resistance area and form a Wheatstone bridge. The method of claim 14 , wherein the third resistor and the first resistor are the same. 16 . The method of claim 14 , wherein each TMR structure of the first plurality of TMR structures has a same height, a same length, and a same width as each TMR structure of the second plurality of TMR structures. The method of claim 14 , wherein the second resistor and the fourth resistor are the same.