Array substrate and display panel

By setting a preset pattern in the source and drain metal layer of the OLED display panel, the side exposed area of ​​the metal layer is increased, and the problem of excessive depth of the Undercut structure is solved, the packaging effect is improved, and the device trust is improved.

CN113517305BActive Publication Date: 2024-11-08BOE TECHNOLOGY GROUP CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202110571874.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-05-25
Publication Date
2024-11-08
Estimated Expiration
2041-05-25

AI Technical Summary

Technical Problem

The VDD trace and VSS trace packaging effect of the source and drain metal layer in the OLED display panel is poor, resulting in too large depth of the Undercut structure, affecting device reliability and packaging effect.

Method used

The area in the source and drain metal layer that is not covered by the flat layer is provided with preset patterns, such as strip patterns or hollow patterns, to increase the side exposed area of ​​the metal layer, allocate the developing solution, and reduce the side corrosion effect of the development process on the metal. , reduce the Undercut depth.

Benefits of technology

It effectively reduces the side corrosion effect of the development process on metal, improves the packaging effect, reduces the risk of CVD packaging failure, and improves the reliability of OLED devices and the packaging effect of the display panel.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113517305B_ABST
    Figure CN113517305B_ABST
Patent Text Reader

Abstract

The present invention provides an array substrate and a display panel, wherein the array substrate includes a source-drain metal layer and a flat layer, wherein the area of ​​the source-drain metal layer not covered by the flat layer is provided with a preset pattern to increase the exposed area of ​​the source-drain metal layer; the area of ​​the source-drain metal layer not covered by the flat layer includes a first area; the first area is located between adjacent VDD and VSS traces on the IC side and is not covered by the flat layer. By adding a preset pattern to the area of ​​the source-drain metal layer not covered by the flat layer, the exposed side area of ​​the metal of the source-drain metal layer can be increased, so as to achieve the effect of allocating the developer to reduce the developer load effect, reduce the side etching effect of the development process on the metal, reduce the undercut depth, improve the packaging effect, and reduce the risk of CVD packaging failure, thereby solving the GDSX problem caused by water and oxygen invading the AA area and ensuring the reliability of OLED devices.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the technical field of OLED display, and in particular relates to an array substrate and a display panel. Background Art

[0002] At present, OLED display panels are developing rapidly. The VDD & VSS lines are located on the IC side of the OLED display panel, which can easily become channels for water and oxygen to invade the AA area (Active Area, display area). The packaging effect of the VDD and VSS lines of the source and drain metal layer (SD layer) will affect the reliability of the OLED device.

[0003] In actual technology, the HPLN (half-tone PLN) development process in the BP (backplane) process will cause side etching of the Al exposed on the side of the source and drain metal layer (2Al+2OH-+2H2O=2AlO 2- +3H2↑), forming a hollow undercut structure of Ti-Al-Ti. However, the excessive depth of the undercut structure can easily cause the CVD (chemical vapor deposition) packaging film layer to crack, resulting in packaging failure of the OLED device. Figure 1 shown.

[0004] Therefore, the art urgently needs to solve the problem of reducing the undercut depth and improving the packaging effect to ensure the reliability of OLED devices. Summary of the invention

[0005] In order to reduce the undercut depth and improve the packaging effect to ensure the reliability of OLED devices, the present invention provides an array substrate and a display panel.

[0006] In a first aspect, an embodiment of the present invention provides an array substrate, comprising a source-drain metal layer and a planar layer, wherein areas of the source-drain metal layer not covered by the planar layer are provided with a preset pattern to increase an exposed area of ​​the source-drain metal layer; areas of the source-drain metal layer not covered by the planar layer comprise a first area, wherein the first area is located between adjacent VDD lines and VSS lines on the IC side and is not covered by the planar layer.

[0007] In some embodiments, the region of the source and drain metal layer not covered by the planar layer further includes a second region, and the second region includes adjacent VDD traces and VSS traces on the IC side not covered by the planar layer.

[0008] In some embodiments, the preset pattern set in the first area includes a hollow pattern or a strip pattern;

[0009] When the preset pattern set in the first area includes a strip pattern, the strip pattern is one or more pieces.

[0010] In some embodiments, when there are multiple strip patterns, the multiple strip patterns are arranged in parallel in the first area horizontally or vertically.

[0011] In some embodiments, the width of at least one of the strip patterns is in the range of 1 μm to 5 μm, and the interval between two adjacent strip patterns is in the range of 1 μm to 30 μm.

[0012] In some embodiments, the spacing between the strip pattern closest to the VDD line and the VDD line is Δb, and the spacing between the strip pattern closest to the VSS line and the VSS line is Δc, where Δb=Δc=1 μm-30 μm.

[0013] In some embodiments, the width of the stripe pattern is in the range of 20 μm to 70 μm, and the interval between two adjacent stripe patterns is in the range of 10 μm to 50 μm.

[0014] In some embodiments, a plurality of first convex-shaped patterns are further arranged on both sides of the strip pattern along the length direction.

[0015] In some embodiments, the first convex shape pattern includes: a circular pattern and a connection portion pattern of the circular pattern and the strip pattern, the convex shape pattern and the strip pattern are connected to form an arc, and the diameter range of the circular pattern and the diameter range of the circle where the arc is located are 1μm to 30μm.

[0016] In some embodiments, the preset pattern set in the second area includes a hollow pattern.

[0017] In some embodiments, the hollow pattern includes a plurality of squares, and the plurality of squares enable the first region or the second region to form a grid pattern in which multiple strip patterns are perpendicular to each other; the width of the strip pattern ranges from 1 μm to 30 μm, and the interval between two adjacent parallel strip patterns ranges from 1 μm to 10 μm.

[0018] In some embodiments, the preset pattern set in the first area includes a plurality of second convex shape patterns;

[0019] Among the plurality of second protrusion-shaped patterns, a part is connected to the VDD wiring, and another part is connected to the VSS wiring; or

[0020] The plurality of second protrusion-shaped patterns are connected to a VDD line; or

[0021] The plurality of second protrusion-shaped patterns are connected to the VSS wiring.

[0022] In a second aspect, an embodiment of the present invention provides a display panel, comprising the array substrate described in the first aspect.

[0023] One or more embodiments of the present invention bring at least the following beneficial effects:

[0024] An array substrate and a display panel provided by the present invention can increase the side exposure area of ​​the source and drain metal layers by adding preset patterns to the areas of the source and drain metal layers that are not covered by the flat layer, thereby achieving the effect of allocating the developer to reduce the developer load effect, reducing the side etching effect of the development process on the metal, reducing the undercut depth, improving the packaging effect, and reducing the risk of CVD packaging failure, thereby solving the GDSX problem caused by water and oxygen intrusion into the AA area, ensuring the reliability of OLED devices, and improving the GDSX defect of OLED devices. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings required for use in the embodiments are briefly introduced below. It should be understood that the following drawings only show certain embodiments of the present invention and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without creative work.

[0026] Figure 1 This is the effect picture of the CVD packaging film layer cracking;

[0027] Figure 2 It is the result of the developer loading effect test;

[0028] Figure 3 It is a schematic diagram of the design of the adjacent VDD and VSS traces on the IC side of the source and drain metal layer of the array substrate in the related art;

[0029] Figure 4 is a schematic diagram of a display panel in the related art;

[0030] Figure 5 It is a wiring plane schematic diagram of VDD routing and VSS routing in the related technology;

[0031] Figure 6 yes Figure 3 The VDD cross-sectional view corresponding to the design schematic shown;

[0032] Figure 7 is a schematic diagram of a preset pattern provided by an embodiment of the present invention including a strip pattern;

[0033] Fig. 8A is a schematic diagram of a plurality of strip patterns provided by an embodiment of the present invention being arranged in parallel in a first area;

[0034] Figure 8B yes Fig. 8A Corresponding cross-sectional schematic diagram;

[0035] Fig. 9 is a schematic diagram of a plurality of strip patterns provided by an embodiment of the present invention being arranged longitudinally and parallelly in a first region;

[0036] Fig.10 is a schematic diagram of arranging a plurality of first convex-shaped patterns when a plurality of strip-shaped patterns are arranged in parallel in a first region in a transverse direction according to an embodiment of the present invention;

[0037] Fig.11 is a schematic diagram of arranging a plurality of first convex-shaped patterns when a plurality of strip-shaped patterns are longitudinally and parallelly arranged in a first region according to an embodiment of the present invention;

[0038] Fig.12 is a schematic diagram of a first convex shape pattern provided by an embodiment of the present invention;

[0039] Fig.13A A schematic diagram showing that a preset pattern for a second area setting provided by an embodiment of the present invention includes a hollow pattern;

[0040] Fig. 13B yes Fig.13A The corresponding cross-sectional diagram;

[0041] Fig.14 It is a schematic diagram of a preset pattern of a first area setting provided by an embodiment of the present invention including a plurality of second convex shape patterns. DETAILED DESCRIPTION

[0042] The technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only a part of the embodiments of the present invention, rather than all the embodiments. The components of the embodiments of the present invention generally described and shown in the drawings here can be arranged and designed in various different configurations. Therefore, the following detailed description of the embodiments of the present invention provided in the drawings is not intended to limit the scope of the claimed invention, but merely represents the selected embodiments of the present invention. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without making creative work belong to the scope of protection of the present invention.

[0043] Through the analysis of packaging failure mechanism and comparison of various products, it is found that GDSX failure is strongly correlated with CVD filling depth: the smaller the CVD filling depth, the better the packaging effect and the smaller the risk of GDSX failure (CVD filling depth target <450nm); at the same time, the CVD filling depth is related to the top Ti Undercut size and PI residue (PI THK) in the hollow Undercut structure of Ti-Al-Ti. The data is shown in Table 1.

[0044] Table 1: Correlation between CVD filling depth and top Ti Undercut and PI residue of each product

[0045]

[0046] After analysis and comparison, we can know that:

[0047] 1. Reducing the amount of PI residue can be achieved through overexposure and overdevelopment of the HPDL process.

[0048] 2. Reduce the Ti Undercut on the top of the source and drain metal layer. This can be achieved by reducing the development time of the HPLN process, but there is a risk of residual HPLN process holes in the AA area and residuals in other recessed areas;

[0049] The applicant conducted actual tests on the principle of developer loading effect, and the test results are as follows: Figure 2 As shown, it is proved that the developer loading effect does exist. According to the data after the HPLN process development, it can be seen that the developer has a strong side etching effect on the Al of the source and drain metal layers. The pattern density from large to small is: AA area>FOP / COP>VDD / VSS, and the Undercut of the source and drain metal layers from small to large is: AA area (0μm) <FOP (0.08μm) / COP (0.1μm) <VSS (0.86μm). The main reason is that the smaller the pattern density of the source and drain metal layers, the higher the replacement efficiency of the developer, and the deeper the side etching of Al.

[0050] The pattern design of the source and drain metal layer of the array substrate on the IC side adjacent to the VDD and VSS lines is as follows: Figure 3 As shown, Figure 3 The area shown is located in Figure 4 The area A on the IC side of the display panel (Panel) is shown, in which the VDD line and the VSS line are adjacent and not covered by the PLN layer. The area A includes a first area 1 located between the adjacent VDD line and the VSS line on the IC side and not covered by the flat layer, and a second area 2 including the adjacent VDD line and the VSS line on the IC side not covered by the flat layer. Figure 3 The corresponding cross-sectional diagram is shown in Figure 6As shown, the boundary position of the PLN layer can be seen. The boundary distance between the upper and lower PLN layers is about 50μm. In the source and drain metal layer area not covered by the PLN layer, the exposed Al on the side will undergo side etching to form a hollow Undercut structure of Ti-Al-Ti. Figure 5 It is a wiring plane diagram of VDD and VSS routing in related technologies. It is not limited to Figure 5 The wiring method shown, Figure 5 It cannot be considered as the only limitation on the wiring method of the VDD and VSS lines in the embodiment of the present invention. After detailed analysis, the applicant has come to the following conclusions: the spacing between the VDD and VSS lines is large, the pattern density is small, the Al side exposure area of ​​the source and drain metal layer is limited, and side etching is very likely to occur, thereby forming a deeper undercut structure, which poses a risk of packaging failure. During the reliability process, water and oxygen invade the AA area, which is very likely to cause pixel failure, thereby generating GDSX defects.

[0051] The embodiments of the present invention provide an array substrate and a display panel. By designing a pattern for the IC side area in the source and drain metal layer that is not covered by the flat layer, the metal side exposed area of ​​the source and drain metal layer is maximized, and finally the effect of reducing the development load effect per unit area is reduced, the side etching effect of the development process on the metal is reduced, the undercut depth is reduced, the packaging effect is improved, and the risk of CVD packaging failure is reduced, thereby solving the GDSX problem caused by water and oxygen intrusion into the AA area and ensuring the reliability of OLED devices.

[0052] The specific implementation modes of the present invention are described in detail below with reference to the embodiments.

[0053] Embodiment 1

[0054] The present embodiment provides an array substrate, including a source-drain metal layer and a planar layer (PLN layer), the area of ​​the source-drain metal layer not covered by the planar layer is provided with a preset pattern to increase the exposed area of ​​the source-drain metal layer, the area of ​​the source-drain metal layer not covered by the planar layer includes a first area, the first area is located between adjacent VDD lines and VSS lines on the IC side and is not covered by the planar layer.

[0055] The array substrate provided in this embodiment can increase the side exposed area of ​​the source and drain metal layer by adding a pattern in the first area of ​​the source and drain metal layer that is located between the adjacent VDD wiring and VSS wiring on the display panel IC side and is not covered by the flat layer, thereby achieving the effect of distributing the developer to reduce the developer load effect, reducing the side etching effect of the development process on the metal, reducing the undercut depth, improving the packaging effect, and reducing the risk of CVD packaging failure, thereby solving the GDSX problem caused by water and oxygen intrusion into the AA area and ensuring the reliability of the OLED device.

[0056] Furthermore, the region of the source and drain metal layer not covered by the planar layer further includes a second region, and the second region includes adjacent VDD traces and VSS traces on the IC side not covered by the planar layer.

[0057] By adding patterns in the first area between the adjacent VDD lines and VSS lines on the IC side of the display panel and not covered by the planar layer, and in the adjacent VDD lines and VSS lines on the IC side not covered by the planar layer, the side exposed area of ​​the source and drain metal layer can be greatly increased without changing the original planar layer boundary, thereby achieving the effect of distributing the developer to reduce the developer load effect, reducing the side etching effect of the development process on the metal, reducing the undercut depth, effectively improving the packaging effect, and reducing the risk of CVD packaging failure, thereby solving the GDSX problem caused by water and oxygen intrusion into the AA area and ensuring the reliability of OLED devices.

[0058] In one case, the above-mentioned array substrate can be an array substrate including a PVX layer (inorganic layer), and preset patterns are set in the first area and the second area of ​​the source and drain metal layer of the array substrate that are not covered by the flat layer to increase the exposed area of ​​the source and drain metal layer. The PVX layer is formed by adding a complete set of PVX mask processes (including exposure→development→dry etching→stripping) to cover the side edges of the source and drain metal layer to prevent the side edges of the source and drain metal layer from reacting with the developer of the HPLN process. This can effectively solve the GDSX problem caused by water and oxygen intrusion into the AA area and improve the packaging effect of the display panel.

[0059] In another case, the above-mentioned array substrate can be an array substrate without a PVX layer. For such an array substrate, the IC side has side corrosion of the source and drain metal layers due to the lack of PVX layer protection. The adjacent VDD and VSS lines on the IC side are etched by the undercut structure, resulting in poor packaging effect of CVD1 and CVD2 on the IC side. In severe cases, the direct packaging fails. After the packaging fails, a water and oxygen channel is formed on the IC side. The water and oxygen penetrate into the AA area to cause pixel failure, which will cause a relatively serious reliability GDSX (black spot defect) problem. If the PVX layer is to be used to encapsulate and protect the side of the source and drain metal layer, a complete set of mask processes (including exposure → development → dry etching → stripping) needs to be added to form the PVX layer, which will greatly affect the production capacity of the OLED display panel, and the introduction of the PVX layer may cause changes in parasitic capacitance in the AA area, increase in contact resistance, and other problems, thereby affecting the display effect, such as affecting the uniformity of OLED products and causing uneven light emission. By setting preset patterns in the first area and the second area of ​​the source and drain metal layer of the array substrate that are not covered by the flat layer, it is possible to effectively increase the exposed area of ​​the source and drain metal layer, improve the packaging effect, and effectively solve the GDSX problem caused by water and oxygen intrusion into the AA area, while avoiding the increase in PVX mask costs and production capacity loss caused by adding a PVX layer for packaging protection.

[0060] Embodiment 2

[0061] This embodiment provides an array substrate. Based on the first embodiment, the preset pattern set in the first area includes a hollow pattern or a strip pattern.

[0062] When the preset pattern set in the first area includes a strip pattern, the strip pattern is one or more rectangular strip patterns.

[0063] In some cases, when the strip pattern set in the first area is a block, such as Figure 7 As shown, a strip pattern 3 is set in the first area 1 not covered by the flat layer between the adjacent VDD wiring and VSS wiring on the IC side to increase the side exposure area of ​​the source and drain metal layer to a certain extent, distribute the developer in the development process, and reduce the depth of the undercut formed by the side etching.

[0064] In some embodiments, when the preset pattern includes multiple strip patterns 3, multiple strip patterns 3 are arranged in the area between the adjacent VDD and VSS traces on the IC side that is not covered by the flat layer, and the multiple strip patterns 3 are arranged horizontally and parallelly in the first area 1, such as Fig. 8A and Figure 8BAs shown, it can be seen that by adding multiple strip patterns 3 in the first area 1, the area of ​​the exposed metal on the side of the source and drain metal layer can be greatly increased. The developer in the development process can be effectively distributed through these strip patterns 3, thereby reducing the undercut depth and improving the packaging effect; or multiple strip patterns 3 are arranged in parallel in the first area 1, such as Fig. 9 As shown. It can be understood that the horizontal, vertical and parallel directions are only relative descriptions in a preferred embodiment, and do not only refer to the absolute horizontal direction, the absolute vertical direction and the absolute parallel direction. In practical applications, the horizontal direction can be the horizontal direction, or it can be a direction with a certain inclination angle to the horizontal direction, such as a direction with an inclination angle of ±15° to the horizontal direction. The vertical direction can be the vertical direction, or it can be a direction with a certain inclination angle to the vertical direction, such as a direction with an inclination angle of ±15° to the vertical direction. Parallelism can be absolute parallelism between multiple strip patterns 3, or it can be approximate parallelism between multiple strip patterns 3, that is, when the strip patterns 3 are arranged in parallel in the aforementioned horizontal or vertical directions, they are also regarded as parallel within a certain angle range (for example, ≤15°). The above 15° is only for example and does not constitute a limitation of the present invention. Figures 7 to 9 The first region 1 shown in the figure is only a schematic diagram and is not intended to limit the present invention. In practical applications, the first region may also include other regions in the source and drain metal layer on the IC side that are not covered by the planarization layer.

[0065] Further, the preset pattern includes a plurality of strip patterns 3, and when the plurality of strip patterns 3 are arranged in parallel in the first area 1 horizontally or vertically, in order to meet the principle of minimizing the line width under the exposure resolution, on the one hand, the minimum width of the strip pattern 3 that can be actually produced (the lower limit of the width range) is taken into consideration, and on the other hand, too wide a width will reduce the number of strip patterns 3 and reduce the effect of distributing the developer, so the width range of at least one strip pattern 3 is △L=1μm~5μm. In order to avoid too large a spacing between adjacent strip patterns 3 and reduce the number of strip patterns 3, thereby reducing the effect of distributing the developer, preferably, the spacing range between two adjacent strip patterns 3 is △a=1μm~30μm. It should be understood that the width of the strip pattern 3 refers to the distance between the two long sides of the strip pattern. The spacing between the strip pattern closest to the VDD line and the VDD line is △b, and the spacing between the strip pattern closest to the VSS line and the VSS line is △c, △b=△c=1μm~30μm. It should be understood that the spacing between the strip pattern closest to the VDD line and the VDD line refers to the distance between the side of the strip pattern closest to the VDD line and the VDD line, and the spacing between the strip pattern closest to the VSS line and the VSS line refers to the distance between the side of the strip pattern closest to the VSS line and the VSS line. In order to maximize the metal exposed area in the first region 1, preferably, the length of the strip pattern 3 is the difference between the spacing between the VDD line and the VSS line and 2△b, maximizing the side exposed area of ​​the source and drain metal layer metal, thereby reducing the undercut depth, improving the packaging effect, and ensuring the reliability of the device.

[0066] It can be understood that the width of each strip pattern can be the same or different, the interval between two adjacent strip patterns can also be the same or different, the spacing between the strip pattern closest to the VDD line and the VDD line, and the spacing between the strip pattern closest to the VSS line and the VSS line can be the same or different, and this embodiment does not make a sole limitation.

[0067] by Fig. 8A For example, when multiple strip patterns 3 are arranged horizontally and in parallel in the first area 1, if the lengths of the multiple strip patterns 3 are the same, the position of the short side of each strip pattern 3 close to the VDD line is the same from the VDD line, and each strip pattern 3 is the strip pattern closest to the VDD line, and the spacing from the VDD line is △b. Similarly, the position of the short side of each strip pattern 3 close to the VSS line is the same from the VSS line, and the spacing from the VSS line is △b for each strip pattern 3 closest to the VSS line.

[0068] by Fig. 9For example, when multiple strip patterns 3 are arranged longitudinally and parallelly in the first area 1, the leftmost strip pattern is the strip pattern closest to the VDD wiring, and the rightmost strip pattern is the strip pattern closest to the VSS wiring. The spacing between the leftmost strip pattern and the VDD wiring and the spacing between the rightmost strip pattern and the VSS wiring can be the same or different.

[0069] By arranging the plurality of strip patterns in parallel horizontally or vertically in the first area, the exposed side area of ​​the source and drain metal layer can be greatly increased, and the developer in the development process can be effectively distributed to reduce the depth of the undercut formed by the side etching, which is very beneficial to improving the packaging effect.

[0070] In addition, in some cases, the above-mentioned preset pattern includes multiple strip patterns 3, and when the multiple strip patterns 3 are arranged horizontally or vertically in parallel in the first area, the width range of the strip pattern can also be 20μm to 70μm, and accordingly, the interval range between two adjacent strip patterns can be 10μm to 50μm.

[0071] Embodiment 3

[0072] The present embodiment provides an array substrate. On the basis of the first and second embodiments, in a case where the preset pattern includes a plurality of strip patterns, and the plurality of strip patterns are arranged in parallel in the first area horizontally or vertically, in order to maximize the side perimeter of the strip pattern and significantly increase the metal side exposed area of ​​the source and drain metal layer, a plurality of first convex shaped patterns are further arranged on both sides along the length direction of the strip pattern 3, so as to form a plurality of braided patterns 3' in the first area 1 not covered by the flat layer between the adjacent VDD wiring and VSS wiring on the IC side, and the braided pattern 3' is obtained by adding a plurality of first convex shaped patterns on both sides in the length direction of the strip pattern 3 in the first embodiment.

[0073] When multiple stripe patterns 3 are arranged in parallel in the first area 1, multiple first convex shape patterns are arranged as follows: Fig.10 When multiple strip patterns 3 are arranged longitudinally and parallelly in the first area 1, multiple first convex shape patterns are arranged as shown in FIG. Fig.11 shown.

[0074] In some cases, such as Fig.12As shown, the first convex shape pattern includes: a circular pattern 31, and a connection part pattern 32 of the circular pattern 31 and the strip pattern 3. The first convex shape pattern and the strip pattern 3 are connected to form an arc. The diameter d1 of the circular pattern 31 (inner circle) and the diameter d2 of the (outer) circle where the arc is located are in the range of 1μm to 30μm. Each strip pattern 3 is provided with a plurality of first convex shape patterns connected thereto, so that each strip pattern forms a twist shape, so as to increase the side perimeter of the original strip pattern.

[0075] The first convex shape pattern can maximize the side perimeter of the strip pattern of the source and drain metal layer, greatly increase the metal side exposure area of ​​the source and drain metal layer, fully distribute the developer, reduce the depth of the undercut formed by the side etching, and ensure the packaging effect of the OLED device.

[0076] In other cases, the first convex shape pattern may also include a semicircular pattern connected to the strip pattern 3, a plurality of semicircular patterns are directly connected to the strip pattern 3, and the diameter range of the semicircular pattern is 1 μm to 30 μm. The purpose of increasing the side perimeter of the strip pattern of the source and drain metal layer can also be achieved through this semicircular pattern, so as to increase the metal side exposed area of ​​the source and drain metal layer.

[0077] In this embodiment, on the one hand, the minimum width (lower limit of the width range) of the braided pattern 3' that can be actually produced is taken into consideration, and on the other hand, too wide a width will reduce the number of braided patterns 3' and reduce the effect of distributing the developer, so the width range of the braided pattern 3' is △L=1μm~5μm. In order to avoid too large a spacing between adjacent braided patterns 3' and reduce the number of braided patterns 3' and thus reduce the effect of distributing the developer, preferably, the spacing range between two adjacent braided patterns 3' is △a=1μm~30μm. It should be understood that the width of the braided pattern 3' refers to the distance between the outermost sides of the first convex shape pattern of the two long sides of the braided pattern 3'. The spacing between the braided pattern 3' closest to the VDD line and the VDD line, and the spacing between the braided pattern 3' closest to the VSS line and the VSS line is △b = 1μm to 30μm. It should be understood that the spacing between the braided pattern 3' closest to the VDD line and the VDD line refers to the distance between the outermost side of the first convex shape pattern on the side of the braided pattern 3' closest to the VDD line and the VDD line, and the spacing between the braided pattern 3' closest to the VSS line and the VSS line refers to the distance between the outermost side of the first convex shape pattern on the side of the braided pattern 3' closest to the VSS line and the VSS line. In order to maximize the metal exposed area in the first region 1, preferably, the length of the braided pattern 3' is the difference between the spacing between the VDD line and the VSS line and 2△b, maximizing the side exposed area of ​​the source and drain metal layer metal, thereby reducing the undercut depth, improving the packaging effect, and ensuring the reliability of the device.

[0078] It can be understood that the width of each braided pattern 3' can be the same or different, the interval between two adjacent braided patterns 3' can also be the same or different, the spacing between the braided pattern 3' closest to the VDD line and the VDD line, and the spacing between the braided pattern 3' closest to the VSS line and the VSS line can be the same or different, and this embodiment does not make a sole limitation.

[0079] Embodiment 4

[0080] This embodiment provides an array substrate. Based on the first embodiment, the preset pattern provided in the second area 2 includes a hollow pattern.

[0081] In some cases, such as Fig.13A and Fig. 13BAs shown, the hollow pattern of the second area 2 includes a plurality of squares 4 (the squares may be squares or rectangles), and the plurality of squares enable the second area 2 to form a grid pattern in which a plurality of strip patterns are perpendicular to each other. The strip pattern in this case is similar to the strip pattern in Example 2. In order to enable this hollow pattern (grid pattern) to provide the source and drain metal layer with more metal side exposure area, the width w of the strip pattern in the grid pattern ranges from 1 μm to 30 μm, and the spacing between two adjacent parallel strip patterns ranges from 1 μm to 10 μm, so that the metal side leakage area of ​​the hollow pattern is as large as possible, thereby better distributing the developer. It can be understood that the width w of the strip pattern in the grid pattern is also the spacing between two adjacent squares, and the spacing between two adjacent parallel strip patterns is also the width of the square. Fig. 13B This is a cross-sectional diagram of a VDD or VSS trace with a hollow pattern. Fig. 13B It can be seen that by setting a hollow pattern for the VDD and VSS lines adjacent to the IC side that is not covered by the flat layer, the exposed area of ​​the metal side of the source and drain metal layers can be greatly increased, thereby effectively allocating the developer in the development process, thereby reducing the Undercut depth, improving the packaging effect, and ensuring the reliability of the device, and setting the VDD or VSS lines with a hollow pattern.

[0082] In other cases, the hollow pattern may also include other shapes such as a plurality of circles, diamonds, etc., so that the second region 2 forms a grid pattern to increase the metal side exposed area of ​​the source and drain metal layer.

[0083] Similar to the hollow pattern set in the second area 2, when the preset pattern set in the first area 1 is a hollow pattern, it may also include a number of squares (the squares may be squares or rectangles). The number of squares enables the first area 1 to form a grid pattern in which multiple strip patterns are perpendicular to each other. The strip pattern in this case is similar to the strip pattern in Example 2. In order to enable this hollow pattern (grid pattern) to bring more metal side exposure area to the source and drain metal layer, the width range of the strip pattern in the grid pattern is also 1μm to 30μm, and the interval range between two adjacent parallel strip patterns is 1μm to 10μm, so that the metal side leakage area of ​​the hollow pattern is as large as possible, thereby better distributing the developer.

[0084] It should be understood that the aforementioned perpendicularity does not only refer to the absolute perpendicularity between the strip patterns, but can also refer to the angle formed between the strip patterns being in the range of 90°±α, for example, α=15°, that is, the angle formed between the strip patterns being ≥75° or less than or equal to 105° is considered to be perpendicular to each other.

[0085] By setting a hollow pattern at the VDD and VSS lines adjacent to the IC side that is not covered by the planar layer, the metal side exposed area of ​​the source and drain metal layers can be greatly increased to fully distribute the developer, reduce the depth of the undercut formed by the side etching, and ensure the packaging effect of the OLED device.

[0086] It is worth noting that the method of setting a hollow pattern in the second area 2 provided in this embodiment can be implemented alone, or can be combined with the method of setting one or more strip patterns in the first area 1 in the second or third embodiment and implemented simultaneously, or can be combined with the method of setting a hollow pattern in the first area 1 in the second embodiment and implemented, and this embodiment is not limited to the selected implementation method. That is to say, in practical applications, the metal side exposure area of ​​the source and drain metal layer can be increased by setting one or more strip patterns in the first area 1, or the metal side exposure area of ​​the source and drain metal layer can be increased by setting a hollow pattern in the second area 2, or the metal side exposure area of ​​the source and drain metal layer can be increased by setting one or more strip patterns in the first area 1 and a hollow pattern in the second area 2, or the metal side exposure area of ​​the source and drain metal layer can be increased by setting a hollow pattern in the first area 1 and the second area 2 at the same time, thereby effectively reducing the depth of the undercut formed by the side etching effect and ensuring the packaging effect of the OLED device.

[0087] Embodiment 5

[0088] This embodiment provides an array substrate. Based on the first embodiment, in a first area 1 located between a VDD wiring and a VSS wiring on the IC side and not covered by a planar layer, Fig.14 As shown, the preset pattern may include a plurality of second convex shape patterns 5 .

[0089] Among the plurality of second protrusion-shaped patterns 5, a part is connected to the VDD wiring, and another part is connected to the VSS wiring; or

[0090] A plurality of second protrusion-shaped patterns 5 are connected to the VDD wiring; or

[0091] A plurality of second protrusion-shaped patterns 5 are connected to the VSS wiring.

[0092] By in the first region 1, such as Fig.14 As shown, several second protruding shapes 5 are connected at the VDD routing and the VSS routing respectively, or a plurality of second protruding shapes 5 are connected only at the VDD routing, or a plurality of second protruding shapes 5 are connected only at the VSS routing, which can effectively increase the metal side exposed area of ​​the source and drain metal layers.

[0093] In some cases, the second convex pattern 5 may be similar to the first convex pattern in the third embodiment, including a circular pattern connected to the VDD line or the VSS line, and a pattern of a connecting portion of the circular pattern and the VDD line or the VSS line, the second convex pattern 5 is connected to the VDD line or the VSS line to form an arc, the diameter d1 range of the circular pattern (inner circle) and the diameter d2 range of the (outer) circle where the arc is located are 1 μm to 30 μm. The edge of the VDD line or the VSS line in the first area 1 is provided with a plurality of second convex patterns 5 connected to the VDD line or the VSS line, so that the perimeter of the edge of the VDD line or the VSS line is increased to increase the metal side exposed area of ​​the source and drain metal layer.

[0094] In other cases, the second protruding pattern 5 may also include a semicircular pattern connected to the VDD line or the VSS line, a plurality of semicircular patterns are directly connected to the VDD line or the VSS line, and the diameter of the semicircular pattern ranges from 1 μm to 30 μm.

[0095] It can be understood that the above-mentioned multiple second protruding patterns 5 can be only arranged at the edge of the VDD routing in the first area 1 and connected thereto, or can be only arranged at the edge of the VSS routing in the first area 1 and connected thereto, or can be simultaneously arranged at the edges of the VDD routing and the VSS routing in the first area, thereby increasing the metal side exposed area of ​​the source and drain metal layer.

[0096] Embodiment 6

[0097] This embodiment provides a display panel, including the array substrate provided by the above embodiment.

[0098] The display panel of this embodiment designs patterns for the areas of the source and drain metal layers of the array substrate that are not covered by the flat layer, so as to maximize the metal side exposure area of ​​the source and drain metal layers, thereby reducing the developer load effect per unit area, reducing the side etching effect of the development process on the metal, thereby reducing the undercut depth, and further improving the packaging effect, reducing the risk of CVD packaging failure, thereby solving the GDSX problem caused by water and oxygen intrusion into the AA area, improving the packaging effect of the display panel, and ensuring the reliability of the OLED device.

[0099] In the several embodiments provided in the embodiments of the present invention, it should be understood that the disclosed system and method can also be implemented in other ways. The system and method embodiments described above are merely illustrative.

[0100] It should be noted that, in this article, the terms "include", "comprises" or any other variations thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, an element defined by the sentence "comprises a ..." does not exclude the existence of other identical elements in the process, method, article or device including the element.

[0101] Although the embodiments disclosed in the present invention are as above, the above contents are only embodiments adopted for facilitating the understanding of the present invention and are not intended to limit the present invention. Any technician in the technical field to which the present invention belongs can make any modifications and changes in the form and details of the implementation without departing from the spirit and scope disclosed in the present invention, but the patent protection scope of the present invention shall still be subject to the scope defined in the attached claims.

Claims

1. An array substrate, comprising a source-drain metal layer and a planar layer, It is characterized in that The area of ​​the source and drain metal layer not covered by the planar layer is provided with a preset pattern to increase the exposed area of ​​the source and drain metal layer; the area of ​​the source and drain metal layer not covered by the planar layer includes a first area; the first area is located between the adjacent VDD line and VSS line on the IC side and is not covered by the planar layer.

2. The array substrate according to claim 1, It is characterized in that The region of the source and drain metal layer not covered by the planar layer further includes a second region, and the second region includes adjacent VDD wiring and VSS wiring on the IC side not covered by the planar layer.

3. The array substrate according to claim 1, It is characterized in that The preset pattern set in the first area includes a hollow pattern or a strip pattern; When the preset pattern set in the first area includes a strip pattern, the strip pattern is one or more pieces.

4. The array substrate according to claim 3, It is characterized in that When there are multiple strip patterns, the multiple strip patterns are arranged in parallel in the first area in a horizontal or vertical direction.

5. The array substrate according to claim 4, It is characterized in that The width of at least one of the stripe patterns is in the range of 1 μm to 5 μm, and the interval between two adjacent stripe patterns is in the range of 1 μm to 30 μm.

6. The array substrate according to claim 4, It is characterized in that The spacing between the strip pattern closest to the VDD wiring and the VDD wiring is △b, and the spacing between the strip pattern closest to the VSS wiring and the VSS wiring is △c, △b=△c=1μm~30μm.

7. The array substrate according to claim 4, It is characterized in that The width of the stripe pattern is in the range of 20 μm to 70 μm, and the interval between two adjacent stripe patterns is in the range of 10 μm to 50 μm.

8. The array substrate according to any one of claims 3 to 7, It is characterized in that A plurality of first convex-shaped patterns are also arranged on both sides of the strip-shaped pattern along the length direction.

9. The array substrate according to claim 8, It is characterized in that The first convex shape pattern includes: a circular pattern and a connection portion pattern of the circular pattern and the strip pattern. The first convex shape pattern and the strip pattern are connected to form an arc. The diameter range of the circular pattern and the diameter range of the circle where the arc is located are 1μm to 30μm.

10. The array substrate according to claim 2, It is characterized in that The preset pattern set in the second area includes a hollow pattern.

11. The array substrate according to claim 3, It is characterized in that The hollow pattern includes a plurality of squares, and the plurality of squares enable the first region to form a grid pattern with multiple strip patterns perpendicular to each other; the width of the strip pattern ranges from 1 μm to 30 μm, and the interval between two adjacent parallel strip patterns ranges from 1 μm to 10 μm.

12. The array substrate according to claim 10, It is characterized in that The hollow pattern includes a plurality of squares, and the plurality of squares enable the second region to form a grid pattern with multiple strip patterns perpendicular to each other; the width of the strip pattern ranges from 1 μm to 30 μm, and the interval between two adjacent parallel strip patterns ranges from 1 μm to 10 μm.

13. The array substrate according to claim 1, It is characterized in that The preset pattern set in the first area includes a plurality of second convex shape patterns; Among the plurality of second protrusion-shaped patterns, a part is connected to the VDD wiring, and another part is connected to the VSS wiring; or The plurality of second protrusion-shaped patterns are connected to a VDD line; or The plurality of second protrusion-shaped patterns are connected to the VSS wiring.

14. A display panel, It is characterized in that The invention comprises the array substrate according to any one of claims 1 to 13.