A current design method for a filled three-dimensional electrode

By using unit volume current intensity "current stacking degree" to design the current of particle-filled three-dimensional electrodes in electrochemical engineering, it solves the problem of difficulty in calculating the total current intensity using traditional methods, and provides a more reasonable current design method that is suitable for on different materials and reaction systems.

CN113642190BActive Publication Date: 2024-10-18HUBEI UNIV +1
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202110981636.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-08-25
Publication Date
2024-10-18
Estimated Expiration
2041-08-25

AI Technical Summary

Technical Problem

In electrochemical engineering, it is difficult to accurately calculate the total current intensity of solid particle-filled three-dimensional electrodes using traditional methods, especially due to the inconsistent specific surface areas of different materials and batches, which makes current design difficult.

Method used

The current intensity required by the filled three-dimensional electrode is measured by the current intensity per unit volume, that is, the "current stack degree", and the current intensity is designed by calculating the formula I/V (ampere/cubic decimeter or milliamp/cubic decimeter). Design based on the functions and uses of different granular filling materials.

Benefits of technology

It solves the total current design problem of particle-filled three-dimensional electrodes in electrochemical engineering and provides a more reasonable current design method called "current stacking degree", which replaces the traditional single current density design and has important reference value. .

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113642190B_ABST
    Figure CN113642190B_ABST
Patent Text Reader

Abstract

The present invention relates to a current design method for a particle-filled three-dimensional electrode, and belongs to the field of electrochemical engineering and technology. The design method names the current intensity per unit volume as "current pile density" (or "pile current density", "volume current density"), and represents it with symbols. The calculation formula is: This current design method changes the traditional single "current density" design idea in the field of engineering technology, solves the total current design problem of the newly invented "particle-filled three-dimensional electrode" in the field of electrochemical engineering technology, and has important reference value for current design in the field of electrochemical engineering technology.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of electrochemical engineering and technology, and relates to a current design method for a filled three-dimensional electrode, in particular to a current design method for a particle-filled three-dimensional electrode. Background Art

[0002] Electrode materials are essential in all electrochemical engineering and technology fields, including electrolysis, electroplating, batteries, electrochemical synthesis, electrochemical oxidation, electrochemical separation, electrochemical coagulation and precipitation, and electrochemical wastewater treatment. Commonly used electrode materials are in fixed shapes, such as laths and blocks, serving as the positive (or anode) and negative (or cathode) electrodes. To improve electrochemical efficiency, recent patents, such as CN102910707A and CN101260530A, report methods and devices for using porous electrodes in the form of three-dimensional baskets (or frames) filled with solid particulate fillers as the positive (or anode) and negative (or cathode) electrodes. This method can significantly increase the specific surface area of ​​the electrodes, thereby significantly improving the efficiency of electrochemical reactions. However, when designing the total current requirement for an engineering project, traditional flat electrodes can be calculated using current density, such as A / dm², mA / dm², etc. This way, the total current intensity required for the entire electrolytic cell can be calculated based on the current density required, such as the number of amperes or milliamperes per square decimeter, and the total surface area of ​​the total electrodes (anode or cathode). However, the surface area of ​​the innovative three-dimensional electrodes filled with solid particles is very difficult to calculate. For example, the three-dimensional electrodes filled with activated carbon loaded with a catalyst have a very large specific surface area of ​​approximately 900 to 1500 m² / g. In addition, the surface area of ​​activated carbon made from different materials varies. Even activated carbon made from the same raw material (such as coal) has different specific surface areas depending on the batch. Therefore, it is difficult to calculate the total current intensity requirement for the electrolytic reaction of such filled three-dimensional electrodes using the traditional method of designing the total current intensity based on current density. Summary of the Invention

[0003] In view of the shortcomings of existing design methods, the present invention provides a current design method for a filled three-dimensional electrode. The details are as follows:

[0004] The technical solution of the present invention for the current design method of a particle filler-filled three-dimensional electrode in the current field of electrochemical engineering and technology is:

[0005] A current design method for a particle-filled three-dimensional electrode is characterized by calculating the required current intensity according to the volume of the particle filler filled in the three-dimensional electrode, that is, using the current intensity per unit volume to measure the current required by the filled three-dimensional electrode.

[0006] Furthermore, a current design method for a particle-filled three-dimensional electrode is characterized in that: the current intensity per unit volume is named as "current pile density" or ("pile current density", "volume current density"), and the symbol express.

[0007] Furthermore, a current design method for a particle-filled three-dimensional electrode is provided, characterized in that the calculation formula for the "current stacking degree" of the particle-filled three-dimensional electrode is:

[0008]

[0009] or:

[0010] Note: The units of the above factors are: I is: ampere A or milliampere mA, V is: cubic decimeter dm3, cubic centimeter cm3 or cubic meter m3, and the corresponding The units are: mA / dm3, A / dm3... different combinations.

[0011] Furthermore, a current design method for a particle-filled three-dimensional electrode is characterized in that: the "current stacking degree" of the particle-filled three-dimensional electrode is The size of the particles is designed according to the different functions and uses of different particle filling materials; the same material can be designed to be the same or different in the same electrochemical reaction system; the same material can be designed to be different or the same in different electrochemical reaction systems.

[0012] The beneficial effects of the design method of the present invention are:

[0013] 1. A current design method for a particle-filled three-dimensional electrode solves the total current design problem of the newly invented "particle-filled three-dimensional electrode" in the field of electrochemical engineering technology.

[0014] 2. A current design method for particle-filled three-dimensional electrodes proposes the concept of using different current intensities per unit volume, namely, the concept of "current density." This changes the traditional single "current density" approach in the field of engineering technology and is a supplement to the latter. It has important reference value for current design in the field of electrochemical engineering technology. DETAILED DESCRIPTION

[0015] Example 1

[0016] The present invention discloses a method for designing a current flow of a particle-filled three-dimensional electrode. The electrochemical treatment device is an electro-flocculation wastewater treatment system, which includes:

[0017] 1. Anode: This is an electrode device designed for current flow of a particle-filled three-dimensional electrode. The device is a basket (frame) type three-dimensional electrode. The basket shell is made of porous plastic. Sacrificial anode solid particle material: aluminum particles are implanted in the basket. The total volume of aluminum particles implanted in the basket is 200dm3. A conductive graphite block is set on the side of the basket and connected to the positive pole of the power supply through a wire.

[0018] 2. Cathode: Made of stainless steel plate, connected to the negative pole of the power supply through a wire.

[0019] When the electro-flocculation wastewater treatment system is working, in order to maintain the continuous slow dissolution of the sacrificial anode aluminum particles, this design gives the basket (frame) type three-dimensional electrode (anode) a "current stacking degree" is 0.05A / dm3, so the current intensity of the entire electrolytic cell is designed to be:

[0020] Example 2

[0021] The present invention discloses a method for designing a current flow of a particle-filled three-dimensional electrode. The electrochemical treatment device is an electrochemical catalytic degradation system for COD in organic wastewater, which includes:

[0022] 1. Anode: This is an electrode device designed for current flow of a particle-filled three-dimensional electrode. The device is a basket (frame) type three-dimensional electrode. The basket shell is made of porous plastic. Granular activated carbon anode reaction catalytic material (anode solid particle material) filled with a loaded catalyst is implanted in the basket. The total volume of the activated carbon anode reaction catalytic material implanted in the basket is 500 dm3. A conductive graphite block is set on the side of the basket and connected to the positive pole of the power supply through a wire.

[0023] 2. Cathode: An electrode device designed for current flow of a particle-filled three-dimensional electrode. The device is a basket (frame) type three-dimensional electrode. The basket shell is made of porous plastic. Granular activated carbon cathode reaction catalytic material (cathode solid particle material) filled with a loaded catalyst is implanted in the basket. The total volume of the activated carbon cathode reaction catalytic material implanted in the basket is 500 dm3. A conductive graphite block is set on the side of the basket and connected to the negative pole of the power supply through a wire.

[0024] When the organic wastewater COD electrochemical catalytic degradation system is working, in order to maintain the continuous and stable operation of the cathode and anode stereo electrodes, this design gives the basket (frame) type stereo electrode (anode) a "current stacking degree" is 0.08A / dm3, so the current intensity of the entire electrolytic cell is designed to be:

[0025] The current design method of a particle-filled three-dimensional electrode of the present invention adopts a unique design scheme to solve the total current design problem of the newly invented "particle-filled three-dimensional electrode" in the current electrochemical engineering technology field.

Claims

1. A current design method for a particle-filled three-dimensional electrode, characterized in that: The required current intensity is calculated according to the volume of the granular filler filled in the three-dimensional electrode, that is, the current intensity per unit volume is used to calculate the current required for the filled three-dimensional electrode; this design method names the current intensity per unit volume as "current pile density" or "pile current density" or "volume current density", and uses the symbol express; The calculation formula of the "current stacking degree" of the particle-filled three-dimensional electrode is: in is the current density, I is the current intensity, and V is the total volume of the particle filling material; The "current stacking degree" of the particle-filled three-dimensional electrode The size is designed according to the different functions and uses of different particle filling materials. The same material can be designed to be the same or different in the same electrochemical reaction system; the same material can be designed to be different or the same in different electrochemical reaction systems.

Citation Information

Patent Citations

  • Method and device for electrochemically degrading organic waste water by taking activated charcoal basket as anode

    CN102910707A

  • Device and technique for indirectly electric oxidation synthesis of organic substance electrolytic regeneration medium

    CN101260530A

  • Method for treating landfill leachate concentrated liquor by using three-dimensional electrode

    CN106044960A

  • Supercapacitor electrodes including graphenic carbon particles

    US20160111227A1