Method for manufacturing plate glass and device for manufacturing plate glass
By using a combination of auxiliary support members and adsorption pads during the cutting process of plate glass, the problem of uneven bending stress caused by warpage of the plate glass is solved, and stable cutting and efficient production of plate glass are achieved.
Patent Information
- Application Number
- CN202080059233.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-09-15
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2040-09-15
AI Technical Summary
During the cutting process of plate glass, the elastic properties of the adsorption pad lead to insufficient support, making it difficult to correct warpage, resulting in uneven bending stress and prone to cracking and scattering of glass powder.
Use an auxiliary support member that forms a score line on the surface of the boundary between the first area and the second area of the plate glass and extends along the direction of the score line for support, and combines with an adsorption pad to apply force to the back of the second area to ensure equal bending stress. Distributed to avoid poor warping.
It can effectively correct the warpage of plate glass, ensure uniform bending stress during cutting, avoid cracking and scattering of glass powder, and improve the stability and efficiency of cutting.
Smart Images

Figure CN114302866B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to improvements in the technology for manufacturing plate glass, including a technology for cutting the plate glass along a score line. Background Art
[0002] As is well known, plate glass is used in various fields, represented by glass substrates for displays such as liquid crystal displays, plasma displays, and organic EL displays, and cover glass for organic EL lighting. When manufacturing such plate glass, a process of cutting small plate glass from a large plate glass, a process of trimming the end of the plate glass along the edge, etc. are performed. In these processes, the following contents are usually performed: after the plate glass forms a score line, the plate glass is cut along the score line.
[0003] As a specific example of such a method for cutting plate glass, the method disclosed in Patent Document 1 can be cited. In the method disclosed in the document, after a score line is formed on the surface of the plate glass, the back side of the first area (the area on one side of the score line) of the plate glass is supported in advance by a back support member. Then, in this state, the back side of the second area (the area on the other side of the score line) of the plate glass is supported by adsorption using an adsorption pad in advance, and a force toward the back side is applied to the second area while the roller (rolling body) is rolled along the surface of the second area. As a result, bending stress is applied near the score line, and the plate glass is cut along the score line.
[0004] Prior art literature
[0005] Patent Literature
[0006] Patent Document 1: Japanese Patent Application Publication No. 2017-226549 Summary of the invention
[0007] Problems to be solved by the invention
[0008] However, in the structure disclosed in Patent Document 1 in which the back surface of the second region of the plate glass is supported by suction by a suction pad and the plate glass is cut, the following problems occur due to the characteristics of the plate glass and the characteristics of the suction pad.
[0009] That is, sometimes warping occurs in the plate glass before it is cut. When the plate glass with such warping is cut, if the back side of the second area of the plate glass is supported by adsorption using an adsorption pad, the adsorption support portion becomes sparse. In addition, since the adsorption pad is formed of elastic components such as rubber and resin, it has properties such as being highly elastic. As a result, there are insufficient elements to support the back side of the second area of the plate glass, making it difficult to fully correct the warping of the plate glass when it is cut. Therefore, the bending stress cannot be applied evenly to the vicinity of the scribed line of the plate glass, and proper cutting along the scribed line is hindered. As a result, undesirable conditions such as chipping (improper cracks on the cut end face) and flying of a large amount of glass powder may occur in the cut portion of the plate glass.
[0010] From the above viewpoints, an object of the present invention is to enable favorable support of the back surface of the second region of the plate glass during cleavage, thereby enabling appropriate cleavage of the plate glass along the scribed lines.
[0011] Solutions to Solve Problems
[0012] The first aspect of the present invention made to solve the above-mentioned problems is a method for manufacturing plate glass, including a cutting step of forming a scribe line on the surface side of the boundary between the first area and the second area of the plate glass and cutting the plate glass along the scribe line, wherein the method for manufacturing plate glass is characterized in that, in the cutting step, a force is applied to the second area toward the back side while the back side of the first area is supported by a back support member and the second area is supported by an adsorption pad and an auxiliary support member extending in the direction of the scribe line, thereby cutting the plate glass along the scribe line. Here, the plate glass has a plate thickness of 500 μm or less, preferably 300 μm or less. In addition, the plate glass is preferably flexible.
[0013] According to this method, in the cutting process, the second area of the plate glass is supported by the adsorption pad and the auxiliary support member extending in the direction along the scribed line, so as a support part, a preferred support part extending in the direction along the scribed line is added to the adsorption support part based on the adsorption pad. Therefore, even if the plate glass is warped, the warping can be fully corrected by adding the support part of the preferred method mentioned above. In addition, the adsorption pad pulls the second area in, so when the auxiliary support member contacts the second area, the pulling force based on the adsorption pad acts on the contact part, and the second area is strongly pressed against the auxiliary support member. As a result, the correction of the warping becomes further sufficient. According to the above content, when the plate glass is cut, the bending stress acts evenly on the vicinity of the scribed line, and appropriate cutting is performed, so that the undesirable situation such as cracking and a large amount of glass powder flying in the cut part of the plate glass is appropriately avoided. It should be noted that it is particularly effective if the warping of the plate glass is a warping such as the scribed line in the surface of the plate glass and any imaginary straight line parallel to the scribed line.
[0014] In this method, the suction pad and the auxiliary supporting member may support the back side of the second region, and the pressing member may contact the surface of the second region and press the second region toward the back side, thereby applying a force toward the back side to the second region.
[0015] In this way, in a state where the warping of the plate glass is sufficiently corrected by the suction pad and the auxiliary support member, the pressing member disposed on the front side can appropriately apply force toward the back side to the second region. Therefore, the plate glass can be stably cut.
[0016] In the above method, in the cutting step, the plate glass may be suspended and supported so that the scribed line faces in a vertical direction.
[0017] In this way, the effects described above can be significantly obtained when the plate glass is warped. Specifically, when the plate glass is placed on a platform or the like in a horizontal position and cut, the warping of the plate glass becomes smaller, but when the plate glass is suspended and supported as in the structure here, the warping becomes larger. In this way, even when the warping of the plate glass is large, the warping of the plate glass can be appropriately dealt with as described above, so the effects become particularly significant.
[0018] In the above method, the auxiliary supporting member may be arranged at a position having a shorter separation distance from the scribe line than the suction pad.
[0019] This is advantageous when the dimension from the scribed line to the end edge opposite to the scribed line in the second region is shorter. In detail, since the adsorption pad has been used in the past, there is a preferred position for the adsorption support position of the adsorption pad on the back of the second region. Therefore, if the auxiliary support member is to be arranged at a position of the second region that is closer to the above-mentioned end edge side than the preferred adsorption support position, it is sometimes unreasonable in terms of space. However, according to the structure here, the auxiliary support member is arranged at a position that is closer to the side opposite to the above-mentioned end edge side than the previous adsorption support position, so that the above-mentioned undesirable situation can be eliminated. Therefore, even if a substantial improvement is not made to the previous structure, the auxiliary support member can be added and arranged.
[0020] Contrary to the configuration in this method, the auxiliary supporting member may be arranged at a position having a longer separation distance from the scribe line than the suction pad.
[0021] In this way, the effect of correcting the larger warping of the plate glass becomes significant. In detail, there is a tendency for the warping of the plate glass to become particularly large at the end edge portion of the second region opposite to the scribed line and its vicinity. This tendency is particularly significant when the end edge portion is thicker than other parts of the second region. According to the relative positional relationship between the adsorption pad and the auxiliary support member described here, since the auxiliary support member can be brought into contact with the end edge portion and its vicinity, the above-mentioned particularly large warping can be fully corrected.
[0022] In the above method, the auxiliary supporting member may be in contact with a region of the back surface of the second region excluding both ends in a direction along the scribe line.
[0023] This is advantageous when the end faces at both ends of the second region are cut surfaces. That is, since the cut surfaces have micro cracks, when the auxiliary support member contacts the cut surfaces, the micro cracks may develop and cause the plate glass to break. However, according to the structure here, the auxiliary support member does not contact the two ends, so this undesirable situation does not occur.
[0024] Contrary to the structure in this method, the auxiliary supporting member may be in contact with a region including both ends of the back surface of the second region in a direction along the scribe line.
[0025] In this manner, the warping of the plate glass can be corrected by the auxiliary supporting members in the entire region to the above-mentioned both ends of the second region, and therefore the plate glass can be cut more appropriately.
[0026] In the above method, the contact portion of the auxiliary supporting member that contacts the second region may be formed of a cushioning material.
[0027] Thus, for example, the shock when the auxiliary support member contacts the second region can be mitigated by the buffer material. Therefore, even if the auxiliary support member contacts the second region at high speed, the plate glass is unlikely to be broken or damaged, and the operation can be accelerated.
[0028] The second aspect of the present invention made to solve the above-mentioned problems is a manufacturing device for plate glass, which is equipped with a cutting device for cutting plate glass having a scoring line formed on the surface side of a boundary between a first area and a second area along the scoring line. The manufacturing device for plate glass is characterized in that the cutting device is configured to cut the plate glass along the scoring line by applying a force toward the back side to the second area while supporting the back side of the first area with a back supporting member and supporting the second area with an adsorption pad and an auxiliary supporting member extending in the direction of the scoring line.
[0029] According to this manufacturing apparatus, similarly to the case of the manufacturing method described above, the plate glass is appropriately cut, and chipping, scattering of a large amount of glass powder, etc., are avoided during cutting.
[0030] Effects of the Invention
[0031] According to the present invention, the back surface of the second region of the plate glass is well supported during cleavage, and the plate glass is appropriately cleaved along the scribed lines. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] Figure 1 It is a perspective view which shows the cutting device included in the manufacturing apparatus of the plate glass which concerns on embodiment of this invention.
[0033] Figure 2 It is a schematic perspective view showing the main part of the cutting device included in the manufacturing apparatus of the plate glass according to the embodiment of the present invention.
[0034] Figure 3a It is a schematic side view which looked at the cutting device included in the manufacturing apparatus of the plate glass which concerns on embodiment of this invention from the side.
[0035] Figure 3b It is an enlarged schematic bottom view which saw the principal part of the cleaving device included in the manufacturing apparatus of the plate glass which concerns on embodiment of this invention from below.
[0036] Figure 4a It is a schematic bottom view showing a cutting process included in the manufacturing method of the plate glass according to the embodiment of the present invention.
[0037] Figure 4bIt is a schematic bottom view showing a cutting process included in the manufacturing method of the plate glass according to the embodiment of the present invention.
[0038] Figure 4c It is a schematic bottom view showing a cutting process included in the manufacturing method of the plate glass according to the embodiment of the present invention.
[0039] Figure 5 It is a schematic bottom view showing a first modified example of the cutting step included in the method for producing plate glass according to the embodiment of the present invention.
[0040] Figure 6 It is a schematic bottom view showing a second modification of the cutting step included in the method for producing plate glass according to the embodiment of the present invention.
[0041] Figure 7 It is a schematic bottom view showing a third modified example of the cutting step included in the method for producing plate glass according to the embodiment of the present invention.
[0042] Figure 8 It is a schematic bottom view showing a first modified example of the cleaving device included in the manufacturing apparatus of the plate glass according to the embodiment of the present invention.
[0043] Fig. 9 It is a schematic bottom view showing a second modification of the cutting device included in the manufacturing apparatus of the plate glass according to the embodiment of the present invention. DETAILED DESCRIPTION
[0044] Hereinafter, a method and an apparatus for producing plate glass according to an embodiment of the present invention will be described with reference to the drawings.
[0045] Figure 1 This is a stereoscopic diagram illustrating a cutting device 1 included in a manufacturing device for plate glass according to an embodiment of the present invention. As shown in the figure, the plate glass G is divided by a scribed line S formed on the surface side (the side marked with reference numerals Ga and Gx), and one side in the width direction (the side in the direction of arrow A) is set as a first area G1, and the other side in the width direction (the side in the direction of arrow B) is set as a second area G2. In this embodiment, the first area G1 becomes a product part, and the second area G2 becomes a non-product part. However, both the first area G1 and the second area G2 may become product parts. In the example, the scribed line S does not reach the upper and lower ends of the plate glass G, but it may reach the upper and lower ends thereof.
[0046] The plate glass G is suspended and supported in a manner that the score line S is oriented in the vertical direction. The thickness of the plate glass G can be set to 200 to 2000 μm, for example. Since warping is easily generated in the plate glass G, the thickness of the plate glass G is preferably 500 μm or less, and more preferably 300 μm or less. In addition, the plate glass G is preferably flexible. In this embodiment, warping occurs in the plate glass G. The warping is in the shape of a curve of the score line S on the surface of the plate glass G and any imaginary straight line parallel to the score line S.
[0047] The cutting device 1 uses bending stress to cut the plate glass G along the scoring line S. In detail, the cutting device 1 includes: a holding mechanism 2 that suspends and supports the plate glass G; a back support member 3 that supports the back side Gb of the first area G1; a back auxiliary support mechanism 4 that supports the back side Gy of the second area G2; and a plate-shaped member (pressing member) 5 that rotates in the direction of arrow C while contacting the surface Gx of the second area G2 and applies a force (pressing force) to the second area G2 toward the back side Gy.
[0048] The holding mechanism 2 moves the plate glass G in the width direction while holding the upper end of the first region G1. It should be noted that the holding mechanism 2 is slidably held on a guide rail (not shown) extending in the width direction above the plate glass G. When the process of cutting the plate glass G is performed, the holding mechanism 2 and the plate glass G are stopped. In addition, the holding mechanism 2 may be arranged at multiple locations in the width direction of the upper end of the first region G1.
[0049] The back support member 3 is arranged on the back side Gb of the end of the first region G1 on the side of the scribed line S. The back support member 3 is a columnar body or a plate-like body (platform) whose supporting surface supporting the back side Gb of the first region G1 is flat and is long in the vertical direction. It should be noted that the shape of the back support member 3 can also be a round rod or the like. In addition, the back support member 3 extends up and down from the upper end Gf and the lower end Gg of the first region G1, but it can also be a length that does not reach the upper end Gf and the lower end Gg.
[0050] The back auxiliary support mechanism 4 includes: a holding substrate 6 that is elongated in the vertical direction; an adsorption pad 7 that is mounted on the holding substrate 6; and an auxiliary support member 8 that is fixed to the holding substrate 6. The holding substrate 6 is a structure that is moved by the operation of a driving mechanism (not shown) such as a robot arm.
[0051] Figure 2The detailed structure of the back auxiliary support mechanism 4 is illustrated. As shown in the figure, on the surface side of the substrate 6, a plurality of (5 in the example) adsorption pads 7 are arranged at equal intervals in the up and down directions. The adsorption pad 7 is formed of an elastic member such as rubber, resin, etc. that can be stretched and retracted, and uses negative pressure to adsorb and support the back side Gy of the second region G2. In addition, an auxiliary support member 8 that is long in the up and down direction is arranged on the surface side of the substrate 6. The auxiliary support member 8 is fixed to the surface of the surface side of the substrate 6, and provides contact support to the back side Gy of the second region G2. The end face 8a of the auxiliary support member 8 that contacts the second region G2 becomes a plane, so that the auxiliary support member 8 is in surface contact with the back side Gy of the second region G2. The contact portion of the auxiliary support member 8 that contacts the second region G2 is formed by a cushioning material 8x composed of a foamed resin represented by a PP foam board. The buffer material 8x is assembled on the front end of the plate-like base 8y, and the plate-like base 8y is made of a metal material (such as aluminum, aluminum alloy or various steels) or a material having the same degree of rigidity. The area in the back side Gy of the second region G2 in contact with the auxiliary support member 8 is set as the area excluding the upper end Gf and the lower end Gg of the second region G2. In this embodiment, the auxiliary support member 8 is arranged on the retaining substrate 6 in a manner that the separation distance from the scoring line S is shorter than that of the adsorption pad 7. That is, in the width direction of the plate glass G, the auxiliary support member 8 is arranged between the adsorption pad 7 and the scoring line S. In addition, the auxiliary support member 8 extends continuously in the direction along the scoring line S, but can also extend in the direction along the scoring line S at predetermined intervals. In other words, the auxiliary support member 8 can also be divided into a plurality of parts in the direction along the scoring line S. It should be noted that the scoring line S here is as follows. Figure 2 As shown, the scribed lines are formed on the plate glass G which has no warping at all.
[0052] like Figure 1As shown, the plate-like member 5 is arranged on the surface Gx side of the second region G2. In this embodiment, the plate-like member 5 is a flat plate whose side in contact with the surface Gx of the second region G2 is flat and is long in the vertical direction. In addition, the plate-like member 5 extends up and down from the upper end Gf and the lower end Gg of the second region G2, but it can also be a length that does not reach the upper end Gf and the lower end Gg. A belt roller member 9 is arranged on the surface side of the plate-like member 5 to keep the plate-like member 5 so that it can be loaded and unloaded. The belt roller member 9 includes: a roller shaft 10, which extends in the direction along the score line S; a plurality of (5 in the example) rollers 11, which are arranged at equal intervals in the axial direction of the roller shaft 10; and a support body 12, which supports the roller shaft 10. It should be noted that the score line S mentioned here is also the same as the case described above, and is the score line S when the plate glass G is completely free of warping. In this embodiment, the plate-like member 5 is connected to the roller shaft 10 using a binding belt 13. The strapping band 13 can be wound and unwound across the plate-like member 5 and the roller shaft 10, thereby the plate-like member 5 can be loaded and unloaded relative to the belt roller member 9. The support body 12 is a structure that moves by the action of a driving mechanism (not shown) such as a robot arm, thereby the belt roller member 9 and the plate-like member 5 move synchronously. Here, the roller shaft 10 and the roller 11 are configured to move straight in the D direction. The D direction is a direction orthogonal to the surface Gx of the second region G2. The surface Gx of the second region G2 mentioned here refers to the surface Gx of the second region G2 before the cutting process when there is no warping at all.
[0053] Next, a method for producing plate glass using the production apparatus configured as described above will be described.
[0054] First, in Figure 1 In the process on the upstream side of the position shown in FIG. 1 , the plate glass G is suspended and supported by the holding mechanism 2, and the surface Gx of the plate glass G is pressed by the wheel cutter, irradiated with laser, etc., to form the scoring line S. Next, the plate glass G with the scoring line S formed thereon is conveyed in the width direction and stopped while the plate glass G is suspended and supported by the holding mechanism 2. When the plate glass G stops, as shown in FIG. Figure 1 As shown, the back support member 3 moves toward the front side and contacts the back side Gy of the first region G1 of the plate glass G. In addition, the belt roller member 9 moves back side, so that the plate-like member 5 contacts the surface Gx of the second region G2. Moreover, the holding base 6 of the back auxiliary support mechanism 4 moves toward the front side, so that the suction pad 7 and the auxiliary support member 8 contact the back side Gy of the second region G2.
[0055] After that, the suction pad 7 attracts the second region G2, so that the auxiliary support member 8 is firmly in contact with the back surface Gy of the second region G2. At the same time, the plate-like member 5 presses the second region G2 to the back side, so that the plate-like member 5 is in contact with the surface Gx of the second region G2. Maintaining this state, the plate-like member 5 gradually presses the second region G2 to the back side Gy. At this stage, the support portion Gw of the second region G2 supported by the suction pad 7 and the auxiliary support member 8 is in contact with the surface Gx of the second region G2. Figure 3a The side view shown and Figure 3b When viewed from above, it becomes a flat shape with almost no warping. In this case, assuming that the back side Gy of the second region G2 is supported by adsorption only by the adsorption pad as disclosed in Patent Document 1, the supporting elements (the elements described) are insufficient, and the warping of the second region G2 cannot be fully corrected. Therefore, it is difficult to generate uniform bending stress near the scribed line S when the plate glass G is cut. In contrast, if the back side Gy of the second region G2 is supported by the adsorption pad 7 and the auxiliary support member 8, the supporting parts can be increased and the warping of the second region G2 can be reduced. Moreover, the auxiliary support member 8 extends in the direction along the scribed line S, so as the supporting part of the back auxiliary support mechanism 4, a preferred supporting part extending in the direction along the scribed line S is added to the adsorption supporting part based on the adsorption pad 7. Therefore, the warping of the second region G2 is fully corrected by adding the supporting parts of the preferred method described above. Furthermore, the adsorption pad 7 pulls the second region G2 in, so when the auxiliary support member 8 contacts the second region G2, the pulling force based on the adsorption pad 7 acts on the contact portion, and the second region G2 is strongly pressed against the auxiliary support member 8 (buffer material 8x). As a result, the correction of the warping becomes further sufficient. According to the above contents, when the plate glass G is cut, the bending stress acts evenly near the scribe line S, and appropriate cutting is performed, thereby effectively avoiding undesirable situations such as cracking at the cut portion of the plate glass G and a large amount of glass powder flying. In this embodiment, the warping of the second region G2 is also corrected by the plate-like member 5 being in surface contact with the surface Gx of the second region G2, so that the plate glass G is further appropriately cut.
[0056] Figure 4a , Figure 4b as well as Figure 4c The process of gradually cutting the plate glass G by pressing the second region G2 toward the back surface Gy side through the actions of the suction pad 7, the auxiliary support member 8, and the plate-shaped member 5 is illustrated in time series. Figure 4aAs shown, the belt roller member 9 and the back auxiliary support mechanism 4 are moved, so that the plate-like member 5 is in surface contact with the surface Gx of the second region G2, and the back surface Gy of the second region G2 is supported by the suction pad 7 and supported by the back surface Gy of the second region G2 by the auxiliary support member 8. At this time, the roller 11 is in contact with the plate-like member 5, and both the plate-like member 5 and the holding substrate 6 are in a non-inclined state (parallel to the surface Gx of the first region G1). Hereinafter, this state is referred to as the initial state.
[0057] Next, if Figure 4b As shown, the roller 11 moves straight in the D direction, so that the plate-like member 5 maintains a state of surface contact with the surface Gx of the second region G2 and rotates around the roller shaft 10 (axis 9a). In this way, during the rotation of the plate-like member 5, the angle of the plate-like member 5 changes following the angle change of the second region G2. At the same time, the substrate 6 is kept moving along a prescribed curved track, so that the angle of the substrate 6 changes following the angle change of the second region G2. The prescribed curved track mentioned here refers to a curved track such as a circular track centered near the back support member 3 and the scribed line S, or a track similar to the circular track. As a result, the plate glass G is bent with the back support member 3 as the starting point. In this process, the portion of the second region G2 from the surface contact portion Gw in contact with the plate-like member 5 to the scribed line S becomes a shape that is close to a flat shape, so the vicinity of the scribed line S of the second region G2 becomes a shape that is close to a bend, that is, a shape that is curved with a large curvature. Here, the curved line W shown by the dot-dash line in the figure depicts the shape when the surface Gx of the second region G2 is bent only by the roller 11 and the suction pad 7 as disclosed in Patent Document 1. In the curved line W, the vicinity of the scribe line S of the second region G2 is curved with a small curvature. Compared with the case where the vicinity of the scribe line S is curved with a small curvature, when the curvature is curved with a large curvature, the bending stress acting near the scribe line S becomes larger.
[0058] After that, the roller 11 further moves straight in the direction D, and the second region G2 is further pressed toward the back surface Gy. When the bending stress acting near the scribed line S becomes large enough, as shown in FIG. Figure 4c As shown, the plate glass G is cut along the score line S. In this case, as already described based on Figure 4bAs described, when the second region G2 is bent, the portion of the second region G2 from the surface contact portion Gw to the scribed line S becomes nearly flat. Therefore, even if the distance that the roller 11 moves straight in the D direction is short, the plate glass G can be cut. As a result, the time required for cutting the plate glass G is shortened, the working efficiency is improved, and the mechanism for moving the belt roller member 9 and the mechanism for moving the back auxiliary support mechanism 4 are also made compact. It should be noted that after the plate glass G is cut and the second region G2 is separated from the first region G1, the second region G2 does not fall, but maintains a state of being adsorbed and held by the adsorption pad 7. In addition, after the second region G2 is transported to a retreat position that does not affect the first region G1, the adsorption by the adsorption pad 7 is released, and the second region G2 is dropped and recovered.
[0059] The manufacturing device and manufacturing method of the plate glass of the above-mentioned embodiment may replace the above-mentioned exemplary configuration, and Figure 5 As shown, the plate-like member 5 is in contact with the surface Gx of the second region G2 including the end edge Gz opposite to the scribed line S. In detail, the end edge Gz of the second region G2 (the portion called the ear portion) is thicker than other portions of the second region G2. Moreover, in the state shown in the figure, the length of the second region G2 in the width direction (the separation distance from the end edge Gz to the scribed line S) is shortened. Even under such conditions, as shown in the figure, by supporting the back surface Gy of the second region G2 with the adsorption pad 7 and the auxiliary support member 8, the plate glass G can be properly cut.
[0060] In addition, the manufacturing apparatus and manufacturing method of the plate glass of the above-mentioned embodiment can be modified in structure as shown below. That is, first, the binding belt 13 of the belt roller member 9 is untied and the plate-shaped member 5 is removed. Figure 6 As shown, the roller 11 is brought into contact with the surface Gx of the second region G2 in a rollable manner, and the back surface Gy of the second region G2 is supported by the suction pad 7 and the auxiliary support member 8. This state is set as the initial state, and as described above Figure 4b The second region G2 is bent as shown in the state shown in FIG. 1 , and when the bending stress acting on the scribed line S becomes sufficient, as described above, Figure 4c The plate glass G is cut as shown.
[0061] Furthermore, the manufacturing device and manufacturing method of the plate glass of the above-mentioned embodiment can be applied not only to the case where the plate glass G is cut at one location, but also to the case where the plate glass G is cut at two locations as shown below. Figure 7As shown, the central side area of the width direction of the plate glass G is set as the first area G1, and the scoring lines S are formed on both sides thereof, and the outer areas of the width direction of each scoring line S are respectively set as the second area G2. In addition, a belt roller member 9 is respectively arranged on the surface Gx side of each second area G2, and a back auxiliary support mechanism 4 is respectively arranged on the back Gy side of each second area G2. In addition, a back support member 3 is respectively arranged on the back Gb side at both ends in the width direction of the first area G1. In this case, if each belt roller member 9 is used as a reference, the central side in the width direction becomes Figure 1 The arrow A direction side and the two outer sides in the width direction become Figure 1 If these are taken as the premise, substantially the same action as that already described is performed on both sides in the width direction of the plate glass G, and substantially the same effect as that already described is obtained.
[0062] According to the above embodiment, in addition to the effects already described, the following effects can be obtained. That is, in the above embodiment, the plate glass G is suspended and supported in such a manner that the scribed line S is oriented in the vertical direction (see Figure 1 ), so it is possible to obtain a significant effect when the plate glass G has a large warp. In detail, when the plate glass G is placed in a horizontal position and cut, the warp of the plate glass G becomes smaller, but when the plate glass G is suspended and supported, the warp becomes larger. In this way, even when the warp of the plate glass G is large, it can be properly dealt with as described above, so its effect becomes particularly significant.
[0063] In the above-described embodiment, the auxiliary support member 8 is disposed at a position where the separation distance from the scribe line S is shorter than that of the adsorption pad 7 (see Figure 2 etc.), so it is advantageous when the dimension from the scribe line S to the end edge Gz opposite to the scribe line S in the second region G2 is shorter. In detail, since the adsorption pad 7 has been used in the past, there is a preferred position for the adsorption support position of the adsorption pad 7 on the back side Gy of the second region G2. Therefore, if the auxiliary support member 8 is to be arranged at a position on the side of the end edge Gz mentioned above in the second region G2 that is closer to the preferred adsorption support position, it is sometimes unreasonable in terms of space. However, according to the relative position relationship here, the auxiliary support member 8 is arranged at a position on the side opposite to the end edge Gz side mentioned above than the previous adsorption support position, so that such an undesirable situation can be eliminated. Therefore, even if no substantial improvement is made to the previous structure. The auxiliary support member 8 can be added and arranged.
[0064] In the above-described embodiment, the auxiliary supporting member 8 is in contact with the area of the back surface Gy of the second region G2 excluding the upper end Gf and the lower end Gg (see Figure 2 etc.), so it is advantageous when the end faces of the upper end Gf and the lower end Gg are cut surfaces. That is, since the cut surface has cracks, etc., when the auxiliary support member 8 contacts the cut surface, the cracks, etc. may develop and cause the plate glass G to break. However, in the structure here, the auxiliary support member 8 does not contact the upper end Gf and the lower end Gg, so this undesirable situation will not occur.
[0065] In the above embodiment, the contact portion of the auxiliary support member 8 that contacts the second region G2 is formed of the buffer material 8x, so the buffer material 8x can be used to mitigate the impact when the auxiliary support member 8 contacts the second region G2. Therefore, even if the auxiliary support member 8 contacts the second region G2 at a high speed, it is difficult to cause breakage or damage to the plate glass G, and the operation can be accelerated.
[0066] It should be noted that, in the above embodiment, the auxiliary support member 8 is arranged at a position where the separation distance from the scribe line S is shorter than that of the adsorption pad 7, but the opposite may be true, such as Figure 8 As shown, the auxiliary support member 8 is arranged at a position where the separation distance from the scribe line S is longer than that of the adsorption pad 7. In this way, the effect of correcting the larger warping of the plate glass G becomes significant. In detail, there is a tendency for the warping of the plate glass G to become particularly large at the end edge portion Gz of the second region G2 opposite to the scribe line S and its vicinity. This tendency is particularly significant when the end edge portion Gz is thicker than other parts of the second region G2 as shown in the figure. According to the relative positional relationship between the adsorption pad 7 and the auxiliary support member 8 here, since the auxiliary support member 8 can be brought into contact with the vicinity of the end edge portion Gz, the above-mentioned larger warping can be fully corrected.
[0067] In the above embodiment, the auxiliary support member 8 is in contact with the area of the back surface Gy of the second region G2 except for the upper end Gf and the lower end Gg, but the reverse may be true. Fig. 9 As shown, the auxiliary support member 8 contacts the region including the upper end Gf and the lower end Gg. In this way, the warping of the plate glass G can be corrected by the auxiliary support member 8 in the entire region from the upper end Gf to the lower end Gg of the second region G2, so the plate glass G can be cut more appropriately.
[0068] Furthermore, in the above embodiment, the warping of the plate glass G takes the shape in which the scribed line S on the surface of the plate glass G and any imaginary straight line parallel to the scribed line S are bent, but the warping may take a shape different from this.
[0069] Moreover, in the above-mentioned embodiment, although the plate glass G is suspended and supported in a vertical posture, the plate glass G may be laid flat in a horizontal posture (preferably a horizontal posture).
[0070] Moreover, in the above embodiment, the surface Gx of the second region G2 of the plate glass G is pressed toward the back side Gy by using a pressing member such as a plate-shaped member 5 and a roller 11, but the use of the pressing member may be eliminated, and the second region G2 may be pulled in only by using the back auxiliary support mechanism 4. In this case, a pulling force toward the back side Gy is applied to the second region G2. Alternatively, the surface Gx of the second region G2 of the plate glass G may be supported by the suction pad 7 and the auxiliary support member 8, and the suction pad 7 and the auxiliary support member 8 may be pressed toward the back side Gy.
[0071] The back auxiliary support mechanism 4 moves the suction pad 7 and the auxiliary support member 8 synchronously by attaching the suction pad 7 and the auxiliary support member 8 to the holding substrate 6 . However, the suction pad 7 and the auxiliary support member 8 may be moved synchronously in a separated state.
[0072] Description of Reference Numerals
[0073] 1 Plate glass manufacturing device (cutting device)
[0074] 3 Back support member
[0075] 4 Back auxiliary support mechanism
[0076] 6. Maintain the substrate
[0077] 7. Absorption pad
[0078] 8 Auxiliary support components
[0079] 8x Cushioning Materials
[0080] G Plate Glass
[0081] G1 First Area
[0082] G2 Second Area
[0083] Gb The back of the first area
[0084] Gy The back of the second area
[0085] Gz The edge of the second region
[0086] S Score line.
Claims
1. A method for manufacturing a plate glass, comprising forming a scribe line on a surface side of a boundary between a first region and a second region of the plate glass and cutting the plate glass along the scribe line, The method for producing plate glass is characterized in that: In the cutting step, a force is applied to the second region toward the back side, while the back side of the first region is supported by a back support member and the second region is supported by an adsorption pad and an auxiliary support member extending in a direction along the score line, so that the plate glass is cut along the score line. The adsorption pad and the auxiliary support member support the back side of the second area, The pressing member is brought into contact with the surface of the second region to press the second region toward the back side, thereby applying a force toward the back side to the second region.
2. A method for manufacturing a plate glass, comprising forming a scoring line on a surface side of a boundary between a first region and a second region of the plate glass and cutting the plate glass along the scoring line, The method for producing plate glass is characterized in that: In the cutting step, a force is applied to the second region toward the back side to cut the plate glass along the score line while the back side of the first region is supported by a back support member and the second region is supported by an adsorption pad and an auxiliary support member extending in a direction along the score line, and In the cutting step, the plate glass is suspended and supported so that the scribed line faces in the up-down direction.
3. A method for manufacturing a plate glass, comprising forming a scribe line on a surface side of a boundary between a first region and a second region of the plate glass and cutting the plate glass along the scribe line, The method for producing plate glass is characterized in that: In the cutting step, a force is applied to the second region toward the back side, while the back side of the first region is supported by a back support member and the second region is supported by an adsorption pad and an auxiliary support member extending in a direction along the score line, so that the plate glass is cut along the score line. The contact portion of the auxiliary supporting member that contacts the second region is formed of a cushioning material.
4. A method for manufacturing plate glass, comprising forming a scribe line on a surface side of a boundary between a first region and a second region of the plate glass and cutting the plate glass along the scribe line, The method for producing plate glass is characterized in that: In the cutting step, a force is applied to the second region toward the back side, while the back side of the first region is supported by a back support member and the second region is supported by an adsorption pad and an auxiliary support member extending in a direction along the score line, so that the plate glass is cut along the score line. The auxiliary support member is disposed at a position separated from the scribe line by a longer distance than the suction pad.
5. The method for producing a plate glass according to any one of claims 1 to 3, wherein: The auxiliary support member is disposed at a position having a shorter separation distance from the scribe line than the suction pad.
6. The method for producing a plate glass according to any one of claims 1 to 4, wherein: The auxiliary supporting member is in contact with a region of the back surface of the second region excluding both ends in a direction along the scribe line.
7. The method for producing a plate glass according to any one of claims 1 to 4, wherein: The auxiliary supporting member is in contact with a region of the back surface of the second region including both ends in a direction along the scribe line.
8. A manufacturing device for plate glass, comprising a cutting device for cutting a plate glass having a scribe line formed on a surface side of a boundary between a first region and a second region along the scribe line, The manufacturing device of the plate glass is characterized in that: The cutting device is configured to cut the plate glass along the score line by applying a force toward the back side of the second area while supporting the back side of the first area with a back side support member and supporting the second area with an adsorption pad and an auxiliary support member extending in the direction along the score line. The adsorption pad and the auxiliary support member support the back side of the second area, The cutting device is configured to cause a pressing member to contact the surface of the second region and press the second region toward the back side, thereby applying a force toward the back side to the second region.
9. A manufacturing device for plate glass, comprising a cutting device for cutting a plate glass having a scribe line formed on a surface side of a boundary between a first region and a second region along the scribe line, The manufacturing device of the plate glass is characterized in that: The cutting device is configured to apply force toward the back side of the second area to cut the plate glass along the score line while the back side of the first area is supported by a back support member and the second area is supported by an adsorption pad and an auxiliary support member extending in the direction of the score line. The plate glass is suspended and supported in a manner so that the score line is oriented in the up and down directions.
10. A manufacturing device for plate glass, comprising a cutting device for cutting a plate glass having a scribe line formed on a surface side of a boundary between a first region and a second region along the scribe line, The manufacturing device of the plate glass is characterized in that: The cutting device is configured to cut the plate glass along the score line by applying a force toward the back side of the second area while supporting the back side of the first area with a back side support member and supporting the second area with an adsorption pad and an auxiliary support member extending in the direction along the score line. The contact portion of the auxiliary supporting member that contacts the second region is formed of a cushioning material.
11. A manufacturing device for plate glass, comprising a cutting device for cutting a plate glass having a scribe line formed on a surface side of a boundary between a first region and a second region along the scribe line, The manufacturing device of the plate glass is characterized in that: The cutting device is configured to cut the plate glass along the score line by applying a force toward the back side of the second area while supporting the back side of the first area with a back side support member and supporting the second area with an adsorption pad and an auxiliary support member extending in the direction along the score line. The auxiliary support member is disposed at a position separated from the scribe line by a longer distance than the suction pad.
Citation Information
Patent Citations
Cutting of plate glass and device therefor
JP1992280828A
Method for cutting glass plate and device therefor
JP1993132328A
Manufacturing method of sheet glass and manufacturing apparatus of the same
JP2017226549A