Method for forming MEMS cavity structure

By forming an adhesive material layer on the bottom layer during the MEMS cavity structure formation process, adhesion is improved, and supporting structure and sacrificial layer are formed thereon, the problem of poor adhesion performance of amorphous films is solved, and the more High yield and device reliability.

CN114314501BActive Publication Date: 2024-11-01AAC ACOUSTIC TECH (SHENZHEN) CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202111630653.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2021-01-29
Filing Date
2021-12-28
Publication Date
2024-11-01
Estimated Expiration
2041-12-28

AI Technical Summary

Technical Problem

In the existing MEMS cavity structure formation method, the poor adhesion performance of amorphous films on dielectric and metal films leads to layering defects and surface fluorination, which affects the reliability and production yield of the device.

Method used

The adhesion material layer is formed on the bottom layer to improve adhesion, then a support structure and a sacrificial layer are formed thereon, and a cavity structure is formed through the capping layer, releasing the adhesion material layer to reduce the etchant exposure time and prevent surface fluorine change.

Benefits of technology

It improves the adhesion and functional stability of the MEMS cavity structure, enhances the production yield, and extends the reliability and service life of the device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114314501B_ABST
    Figure CN114314501B_ABST
Patent Text Reader

Abstract

The present invention relates to the field of semiconductor technology, and provides a method for forming a MEMS cavity structure, which can improve the process yield of MEMS integration and packaging with respect to the functional stability and reliability of the MEMS structure. The method comprises the steps of: forming an adhesive material layer on a bottom layer; forming a support structure on the adhesive material layer and filling a sacrificial layer in a space surrounded by the support structure; forming a capping layer on the support structure and the sacrificial layer, wherein the bottom layer, the support structure and the capping layer together form a cavity; and releasing the sacrificial layer and the adhesive material layer to form the cavity structure.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor technology, and more specifically, to a method for forming a MEMS cavity structure. Background Art

[0002] Micro-Electro-Mechanical Systems (MEMS) are formed on semiconductor substrates and CMOS substrates using thin film deposition, lithography and etching techniques. MEMS devices have the advantages of smaller size, ability to be integrated at a lower cost, and ability to be controlled with CMOS circuits. Therefore, MEMS devices are being widely used in various fields / applications.

[0003] Examples of MEMS devices include RF capacitors, RF ohmic switches, MEMS gyroscopes, MEMS ultrasonic devices, and all types of MEMS devices that consist of diaphragms made of oxide / nitride / metal layers, etc. Many MEMS devices need to be sealed and packaged in cavity structures to meet wafer-level packaging requirements. These cavity structures can protect these fragile MEMS devices from environmental influences and are necessary for high performance. These cavities can be maintained in different vacuum levels and / or partially filled with inert gas environments.

[0004] The MEMS cavity structure is a structure widely used in the MEMS field. For example, the cavity structure is formed in radio frequency capacitors, radio frequency ohmic switches, MEMS gyroscopes, MEMS ultrasonic devices, and all types of MEMS devices with oxide layers / nitride layers / metal layers as diaphragms. In the method for forming the MEMS cavity structure in the related art, the cavity structure is formed by depositing an amorphous sacrificial layer (such as a-Si, a-Ge or polymer), and then releasing the sacrificial layer by a wet etchant, a dry etchant, or a vapor etchant.

[0005] However, amorphous films have poor adhesion properties on materials such as dielectric films (e.g., aluminum oxide films) and metal films. As a result, delamination defects will appear in the sacrificial layer and in subsequent process steps such as deposition, cmp, or etching, the active layer will be adversely affected due to poor adhesion, resulting in low yield and in some cases, the entire wafer will be scraped off. At the same time, during the MEMS release process of fluorine-based etchants, after removing the sacrificial layer, the etchant will fluorinate the surface of the dielectric film and the metal film. The fluorinated dielectric layer and / or metal layer are highly hydrophilic and may cause MEMS failure during operation. In some cases, friction can cause severe material wear on the active surface and / or non-active surface during repeated physical contact under cyclic operation. Summary of the invention

[0006] The embodiments of the present invention provide a method for forming a MEMS cavity structure, which can improve the process yield of MEMS manufacturability, functional stability and reliability.

[0007] To solve the above technical problems, an embodiment of the present invention provides a method for forming a MEMS cavity structure, the method comprising: forming an adhesion material layer on a bottom layer; forming a support structure on the adhesion material layer and filling a sacrificial layer in a space surrounded by the support structure; forming a capping layer on the support structure and the sacrificial layer, the bottom layer, the support structure and the capping layer together forming a cavity; and releasing the sacrificial layer and the adhesion material layer to form the cavity structure.

[0008] Preferably, the bottom layer is a substrate.

[0009] Preferably, before forming the adhesive material layer on the bottom layer, the method further comprises: forming the bottom layer on a substrate.

[0010] Preferably, before forming the adhesive material layer on the bottom layer, the method further comprises: pre-treating the bottom layer to increase the surface energy of the bottom layer.

[0011] Preferably, before forming the support structure and the sacrificial layer on the adhesion material layer, the method further comprises: pre-treating the adhesion material layer to increase the surface energy of the adhesion material layer.

[0012] Preferably, before forming the adhesive material layer on the bottom layer, the bottom layer is subjected to no pretreatment; and before forming the support structure and the sacrificial layer on the adhesive material layer, the adhesive material layer is subjected to no pretreatment.

[0013] Preferably, the releasing the sacrificial layer and the adhesive material layer comprises: patterning the capping layer to form a releasing hole penetrating through the capping layer into the cavity; and releasing the sacrificial layer and the adhesive material layer through the releasing hole.

[0014] Preferably, the releasing the sacrificial layer and the adhesion material layer comprises: releasing the sacrificial layer and the adhesion material layer based on a designed etching time and etching rate, so as to further remove the adhesion material layer in the cavity after removing the sacrificial layer.

[0015] Preferably, the method further comprises: determining the designed etching time and etching rate based on the material and thickness of the adhesion material layer.

[0016] Preferably, the releasing the sacrificial layer and the adhesion material layer comprises: etching the sacrificial layer and the adhesion material layer with a wet etchant, a dry etchant or a vapor etchant.

[0017] Preferably, the material of the adhesion material layer is oxide, nitride, metal or suboxide.

[0018] Preferably, the bottom layer is a dielectric or metal film.

[0019] Preferably, the metal film is aluminum, ruthenium, rhodium, tungsten or iridium.

[0020] Preferably, the capping layer is a micro-electromechanical system structure or a membrane.

[0021] Preferably, the material of the sacrificial layer can be amorphous silicon, amorphous germanium, or polymer

[0022] Compared with the process method in the related art, in the method for forming the MEMS cavity structure provided by the embodiment of the present invention, an adhesion material layer is formed on the bottom layer, and then a sacrificial layer is formed on the adhesion material layer. The purpose of forming the adhesion material layer is to improve the adhesion between the amorphous film and the bottom layer of the cavity. By pre-treating the bottom layer and / or the adhesion material layer, the surface energy of the bottom layer and / or the adhesion material layer is improved; thereby further improving the adhesion between the sacrificial layer and the bottom layer. After the adhesion between the sacrificial layer and the underlying dielectric layer or metal layer is improved, the integrity of the sacrificial layer in the subsequent process is enhanced, and the amorphous layer will not be delaminated in the subsequent integration step, thereby obtaining a high production yield. At the same time, the adhesion material layer as an adhesion promoter also plays an isolating role, and the sacrificial layer is isolated from the bottom layer by the adhesion material layer. In this case, during the release process of the sacrificial layer, the adhesion material layer can reduce the exposure time of the bottom layer in the gaseous / gaseous chemical components of the etchant; thereby preventing the fluorination of the bottom surface layer, improving the hydrophobicity of the contact surface in the cavity, and extending the reliability and service life of the device. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] In order to better illustrate the technical solutions in the embodiments of the present invention or related technologies, the drawings used in the embodiments of the present invention and related technologies are briefly introduced as follows. It should be noted that the drawings described below are only part of the embodiments of the present invention, and other drawings can also be obtained by those skilled in the art without making creative efforts.

[0024] Figure 1 is a schematic flow chart of a method for forming a MEMS cavity structure according to an embodiment of the present invention; and

[0025] Figure 2A-2G They are schematic cross-sectional views of the MEMS cavity structure in each step of the method for forming the MEMS cavity structure. DETAILED DESCRIPTION

[0026] In order to illustrate the beneficial effects of the embodiments of the present invention, before describing the embodiments of the present invention in detail, the process in which the inventors of the present invention found problems in the prior art will be described below. In the method of forming a MEMS cavity structure in the related art, the cavity structure is formed by depositing a sacrificial layer and then releasing the sacrificial layer by an etchant. In some cases, an amorphous or polymer sacrificial layer is required on a material with a high contact angle, such as aluminum oxide. Therefore, the adhesion of the sacrificial layer to such a high contact angle material becomes complicated for MEMS integration. On the one hand, the interface adhesion of the amorphous or polymer sacrificial layer on the dielectric film material and the metal film material is poor, resulting in delamination of the sacrificial layer, causing defects in the active layer in subsequent process steps, such as deposition, CMP and etching. In addition, during the release process of the MEMS device, after the sacrificial layer is removed, the fluorine-based chemical etchant fluorinates the surface of the dielectric and / or metal film, resulting in MEMS failures related to friction during operation and causing material wear on the surface. Therefore, with regard to the above-mentioned problems, the present invention provides an improved method for forming a MEMS cavity structure.

[0027] Figure 1 FIG. 1 is a schematic flow chart of a method for forming a MEMS cavity structure according to an embodiment of the present invention. Figure 1 As shown, an embodiment of the present invention provides a method for forming a MEMS cavity structure, which includes the following steps.

[0028] In step S1, an adhesion material layer is formed on the bottom layer. The adhesion material layer can be an oxide, a nitride, a metal (e.g., W) or a metal suboxide, but not a thermal oxide. The bottom layer can be a substrate (CMOS substrate or a blank substrate). The bottom layer can also be a MEMS structure layer formed on the substrate before step S1. In this case, the bottom layer can be a dielectric layer or a metal layer. The material of the dielectric layer can be aluminum oxide, and the material of the metal layer can be aluminum, ruthenium, rhodium, tungsten or iridium.

[0029] In step S2, a support structure and a sacrificial layer filled in the space surrounded by the support structure are formed on the adhesive material layer. The material of the sacrificial layer can be a-Si, a-Ge, or a polymer. Even polymers on high contact angle materials may have adhesion problems. Therefore, before these layers are coated on the substrate, HMDS is used for polyimide, or photoresist.

[0030] In step S3, a capping layer is formed on the support structure and the sacrificial layer, and the bottom layer, the support structure and the capping layer together form a cavity. The capping layer may be an active MEMS structure or a membrane.

[0031] In step S4 , the sacrificial layer and the adhesive material layer are released, thereby forming a cavity structure.

[0032] The method for forming a cavity structure provided by the present invention can be applied to any process in which a cavity needs to be formed during the manufacturing process of a MEMS device. For example, the method can be applied to the manufacturing process of a MEMS device of any shape, such as a beam structure, a bridge structure or a diaphragm structure. Taking the diaphragm structure as an example, the diaphragm is a capping layer, and the diaphragm support structure can form a cavity.

[0033] Compared with the process methods in the related art, the method provided by the present invention forms an adhesion material layer on the bottom layer in step S1, and then forms a sacrificial layer on the adhesion material layer in step S2. One purpose of forming the adhesion material layer is to improve the adhesion of the amorphous layer on the bottom layer of the cavity. The adhesion material layer can be an ultra-thin oxide, nitride, metal or sub-oxide (such as WO x ,SnO x ), which can be formed by physical or chemical thin film deposition methods. The adhesion material layer can increase the contact angle for better adhesion of the amorphous layer. The low temperature sacrificial layer is adhered to the surface of aluminum oxide or other dielectric / metal. After the adhesion between the sacrificial layer and the underlying dielectric or metal layer is improved, the integrity of the sacrificial layer in subsequent processes is enhanced without delamination of the amorphous layer, resulting in higher production yields in later processing.

[0034] As a preferred embodiment provided by the present invention, before step S1, the bottom layer can be pre-treated to improve the surface energy of the bottom layer. And / or before step S2, the adhesion material layer is pre-treated to improve the surface energy of the adhesion material layer. The pre-treatment method includes plasma treatment, thermal induced gas treatment and / or wet chemical treatment. After the bottom surface is pre-treated, the adhesion between the bottom layer and the adhesion material layer can be further enhanced. Similarly, after the adhesion material surface is pre-treated, the adhesion between the adhesion material layer and the sacrificial layer can be further enhanced, and this surface chemical treatment will not affect the performance of the device.

[0035] In addition, the adhesion material layer as an adhesion promoter also plays an isolating role, and the sacrificial layer is isolated from the bottom layer by the adhesion material layer. In this case, when the sacrificial layer is released in step S4, the adhesion material layer can reduce the contact time of the bottom layer with the etching material, thereby preventing the surface of the bottom layer from being fluorinated. This method can increase the hydrophobicity of the contact surface in the cavity, and can modify and / or control the surface condition of the bottom layer for better hydrophobicity during the release process of the sacrificial layer, thereby extending the reliability of the device, for example, extending the switching cycle life of the RF device during operation.

[0036] Specifically, the process of releasing the sacrificial layer and removing the adhesive material layer in the cavity in step S4 includes: based on the designed etching time and etching rate, releasing the sacrificial layer and the adhesive material layer, so as to further remove the adhesive material layer in the cavity after removing the sacrificial layer. Here, the etching time and etching rate are determined according to the material and thickness of the adhesive material layer.

[0037] For example, XeF2 is used as an etchant, an ultra-thin oxide is used as an adhesion material layer, and an amorphous material is used as a sacrificial layer. After the ultra-thin oxide surface is exposed during the release etching process of the amorphous sacrificial layer, the ultra-thin oxide can be removed in XeF2. The etching rate of the oxide layer in XeF2 is much lower than that of the amorphous material. Therefore, the etching time and etching rate are determined based on the material and thickness of the selected ultra-thin oxide so that the ultra-thin oxide can be completely removed during the XeF2 release process, while minimizing the exposure time of the underlying surfaces to XeF2, thereby minimizing the fluorination of these surfaces.

[0038] The etch rate of the ultra-thin oxide can be considered for processing these layers to optimize the process parameters for the sacrificial layer release etch related to a specific MEMS design. The sacrificial layer release process in XeF2 is an exothermic process, therefore, the ultra-thin oxide can be etched faster within the cavity. However, during the MEMS release process, this layer is intact and can be detected on the dielectric layer / metal layer below the electric field dielectric area and / or the a-Si dummy fill area outside the released cavity. A proper disassembly process with suitable microscopy and / or chemical elemental analysis can detect this layer in the field area above the metal line or pad.

[0039] The preferred embodiment of the method for forming a MEMS cavity structure provided by the present invention is applied to the integration process of a radio frequency capacitor or a radio frequency ohmic switch, and will be described in detail below with reference to the accompanying drawings to further illustrate the technical method and effect of the present invention.

[0040] like Figure 2A As shown, the silicon wafer substrate 21 is processed until a specific step in which a bottom layer 22 is deposited and patterned on the silicon wafer substrate 21. The bottom layer 22 can be a dielectric, a metal film, or an atomic layer deposited by atomic layer deposition (ALD) technology.

[0041] like Figure 2B As shown, an adhesion material layer 23 is deposited on the bottom layer 22. The adhesion material layer is made of ultra-thin silicon dioxide (100-200A) and can be formed by ALD, APCVD, PECVD, HDPCVD, SACVD, sputtering, etc. Silicon dioxide has good adhesion to the bottom layer 22, and the bottom layer 22 is a dielectric, a metal film or an atomic layer.

[0042] like Figure 2C As shown, a support structure 24 and a sacrificial layer 25 filled in the space surrounded by the support structure 24 are formed on the adhesion material layer 23. The sacrificial layer 25 is made of amorphous silicon material, which has good adhesion to the adhesion material layer 23 made of silicon dioxide. Although only one cavity structure is illustrated in the figure, this does not mean that only one cavity structure is formed on the silicon wafer substrate 21 in the process of the present invention. Multiple cavity structures can be formed on the silicon wafer substrate 21. The thickness of the sacrificial layer defines the gap height of the MEMS above and / or below the moving MEMS structure. For acceptable changes in device operating parameters (e.g., pull-in, pull-up and release voltages, capacitance, contact force, etc.), it is necessary to accurately control the thickness of the a-Si sacrificial layer, which is critical to its operation.

[0043] like Figure 2D As shown, a capping layer 26 is formed on the support structure 24 and the sacrificial layer 25, and the bottom layer 22, the support structure 24 and the capping layer 26 together define a cavity.

[0044] like Figure 2E As shown, in this embodiment, a release hole 27 is formed for the MEMS release process. The release hole 27 penetrating the capping layer 26 into the cavity is formed by photolithography patterning and etching process.

[0045] like Figure 2F As shown, based on the designed etching time and etching rate, the amorphous sacrificial layer 25 is etched with XeF2. Within the designed etching time, the ultra-thin oxide of the adhesion material layer 23 can protect the bottom layer 22 from being affected by XeF2. Figure 2G As shown, after the amorphous sacrificial layer 25 is etched, XeF2 can further remove the ultra-thin oxide of the adhesion material layer 23 located below the sacrificial layer. In practical applications, some ultra-thin oxide residues may be left in the corners of the cavity. However, this process method can ultimately minimize the degree to which the dielectric, metal film or atomic layer of the bottom layer 22 is exposed to XeF2. In this way, the surface of the bottom layer can be prevented from becoming a hydrophilic surface to the greatest extent, thereby improving the hydrophobicity of the contact surface in the cavity, thereby extending the reliability and service life of the device.

[0046] Compared with the process method in the related art, in the method for forming the MEMS cavity structure provided in the embodiment of the present invention, an adhesion material layer is formed on the bottom layer, and then a sacrificial layer is formed on the adhesion material layer. The purpose of forming the adhesion material layer is to improve the amorphous adhesion of the bottom layer of the cavity. After the adhesion between the sacrificial layer and the underlying dielectric or metal layer is improved, the integrity of the sacrificial layer in the subsequent process steps is strengthened, thereby obtaining a higher production yield, and there is no amorphous layer stratification. At the same time, the adhesion material layer acts as an adhesion layer to isolate, and the sacrificial layer is isolated from the bottom layer by the adhesion material layer. In this case, when the sacrificial layer is released, the adhesion material layer can reduce the exposure time of the bottom layer to XeF2 in the etchant gaseous / gaseous chemical substances, thereby preventing the surface of the bottom layer from being fluorinated, and improving the hydrophobicity of the contact surface in the cavity, thereby extending the reliability and service life of the device.

[0047] The above description only includes exemplary embodiments of the present invention and is not intended to limit the scope of the present invention. Based on the description and drawings of the present invention, all equivalent structures or equivalent process transformations that can be directly or indirectly applied to other related technical fields are within the scope of the present invention.

[0048] Finally, it should be noted that the embodiments described above are only for the purpose of illustrating the present invention, but are not intended to provide any limitation. Although the present invention has been described in detail with reference to the above embodiments, it should be understood by those skilled in the art that the technical solutions described in the above embodiments can still be modified, or some or all of the technical features therein can be replaced by equivalents, but these modifications or replacements will not cause the essence of the corresponding technical solutions to deviate from the scope of the present invention.

Claims

1. A method for forming a MEMS cavity structure, characterized in that: include: forming an adhesive material layer on the base layer; forming a support structure on the adhesive material layer and filling a sacrificial layer in a space surrounded by the support structure; forming a capping layer on the supporting structure and the sacrificial layer, wherein the bottom layer, the supporting structure and the capping layer together form a cavity; as well as The sacrificial layer and the adhesive material layer are released to form the cavity structure.

2. The method for forming a MEMS cavity structure as claimed in claim 1, characterized in that: The bottom layer is a substrate.

3. The method for forming a MEMS cavity structure as claimed in claim 1, characterized in that: Before forming the adhesive material layer on the bottom layer, the method further comprises: The base layer is formed on a substrate.

4. The method for forming a MEMS cavity structure as claimed in claim 1, characterized in that: Before forming the adhesive material layer on the bottom layer, the method further comprises: The bottom layer is pre-treated to increase the surface energy of the bottom layer.

5. The method for forming a MEMS cavity structure as claimed in claim 1, characterized in that: Before forming a support structure and a sacrificial layer on the adhesive material layer, the method further includes: The adhesive material layer is pre-treated to increase the surface energy of the adhesive material layer.

6. The method for forming a MEMS cavity structure as claimed in claim 1, characterized in that: Before forming the adhesive material layer on the bottom layer, the bottom layer is not pre-treated; Before forming a support structure and a sacrificial layer on the adhesive material layer, the adhesive material layer is not pre-treated.

7. The method for forming a MEMS cavity structure as claimed in claim 1, characterized in that: The releasing the sacrificial layer and the adhesive material layer comprises: patterning the capping layer to form a release hole through the capping layer into the cavity; and The sacrificial layer and the adhesive material layer are released through the release hole.

8. The method for forming a MEMS cavity structure as claimed in claim 1, characterized in that: The releasing the sacrificial layer and the adhesive material layer comprises: Based on the designed etching time and etching rate, the sacrificial layer and the adhesion material layer are released to further remove the adhesion material layer in the cavity after removing the sacrificial layer.

9. The method for forming a MEMS cavity structure as claimed in claim 8, characterized in that: The method further comprises: Based on the material and thickness of the adhesion material layer, the designed etching time and etching rate are determined.

10. The method for forming a MEMS cavity structure as claimed in claim 1, characterized in that: The releasing the sacrificial layer and the adhesive material layer comprises: The sacrificial layer and the adhesion material layer are etched using a wet etchant, a dry etchant or a vapor etchant.

11. The method for forming a MEMS cavity structure as claimed in claim 1, characterized in that: The material of the adhesion material layer is oxide, nitride, metal or suboxide.

12. The method for forming a MEMS cavity structure as claimed in claim 1, characterized in that: The bottom layer is a dielectric or metal film.

13. The method for forming a MEMS cavity structure as claimed in claim 12, characterized in that: The metal film is aluminum, ruthenium, rhodium, tungsten or iridium.

14. The method for forming a MEMS cavity structure as claimed in claim 1, characterized in that: The capping layer is a micro-electromechanical system structure or a membrane.

15. The method for forming a MEMS cavity structure as claimed in claim 1, characterized in that: The sacrificial layer is made of amorphous silicon, amorphous germanium, or polymer.