Plastic container for liquids and method for producing a plastic container

By designing the material combination of the inner and outer layers in the plastic container to ensure that the welding contact surface is only composed of inner layer sections, the problem of incompatibility of welding contacts in multi-layer structures is solved and high-quality welding connections are achieved.

CN114616089BActive Publication Date: 2024-10-18PROTECHNA SA
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202080075652.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-09-25
Publication Date
2024-10-18
Estimated Expiration
2040-09-25

AI Technical Summary

Technical Problem

When welding existing plastic containers, the EVOH barrier layer in the multi-layer structure is incompatible with the polyethylene material, resulting in incompatibility of the welding contact surfaces, affecting the quality of the welding connection.

Method used

The container wall is designed to be composed of the first plastic material (inner layer) and the second plastic material (outer layer). The welding contact surface of the container nozzle is composed of the inner layer section to ensure that only the inner layer section is in contact during welding to avoid the outer layer. The contact with the EVOH layer is made using heating element butt welding or other welding methods.

Benefits of technology

A high-quality welding connection is achieved, welding contact between incompatible materials is avoided, and the stability and strength of the welding connection are ensured.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114616089B_ABST
    Figure CN114616089B_ABST
Patent Text Reader

Abstract

A plastic container (10) and a method for producing a plastic container for liquids, the container being in particular an inner container for a transport and storage container for liquids, having an outer cover consisting of a grid structure or a sheet material and a pallet-like base, wherein the plastic container (10) is formed as a blow-molded body by blow molding a tubular parison in a blow mold, and has a container connecting piece (17) provided with a container opening in a fitting connection area (16) of a container wall (13), the container connecting piece being used to connect a container fitting (18) and being connected to a connecting piece (21) of the container fitting (18) via a welded connection (52), wherein the container wall (13) has an inner layer formed of a first plastic material and an outer layer formed of a second plastic material, and the container connecting piece (17) has a longitudinal cross section widening toward the container opening, so that an end face of the container connecting piece (17) is at least partially formed by an inner layer section arranged opposite the outer layer, and a welding contact surface of the container connecting piece (17) is formed by the inner layer section.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a plastic container for liquids, in particular a container for transporting and storing liquids, which has an outer cover consisting of a grid structure or a plate and a tray-like base frame, wherein the plastic container is formed into a blow-molded body by blow molding a hose-shaped parison in a blow mold, and has a container connecting pipe with a container opening in the accessory connection area of ​​the container wall, the container connecting pipe is used to connect a container accessory and is connected to the connecting pipe of the container accessory via a welded connection. Background Art

[0002] A plastic container of the type mentioned at the outset is known from EP 1 630 105 A1, which has a container fitting connected to the container connector by a butt-welding connection via a heating element. The known plastic container is produced by a blow-molding method, wherein, in order to form the container connector for connecting the container fitting, a bulge is formed simultaneously with the production of the blow-molded body in the region of the fitting connection of the container wall, from which a wall region is removed by means of a cutting tool in order to form the container opening, in order to form the container connector. As a result, after the use of the cutting tool, the container connector has a container opening with an outer edge, which forms a welding contact surface in a plane parallel to the container wall. In the subsequent mirror welding method or butt welding method, a heating mirror is arranged as a heating element between the container connector and the oppositely arranged connection connector of the container fitting, in order to heat the welding contact surface formed at the container connector and the welding contact surface formed at the connection connector of the container fitting to the welding temperature, so that after the removal of the heating mirror, the welding contact surfaces are pressed against each other under pressure and can be cooled at this point in order to form the welded connection.

[0003] The above-described method for producing a welded connection between a container nozzle of a plastic container and a connecting nozzle of a container fitting is also used in particular in the case of plastic containers whose container wall has a multilayer structure, wherein an inner layer of polyethylene is combined with an outer layer of recycled material, for example separated by an EVOH barrier layer. The EVOH layer and the recycled layer of recycled material are not suitable for welding to the container fitting, which is usually made of polyethylene, so that the outer layer and the EVOH layer must first be removed in the region of the outer edge of the container nozzle in order to be able to produce the welded connection between the container nozzle and the container fitting. Summary of the invention

[0004] The invention is therefore based on the object of specifying a plastic container and a method for producing a plastic container which has a multi-layer wall structure and can be provided with container fittings in a simple manner by means of a welded connection.

[0005] In order to achieve the above object, the plastic container according to the present invention has the following features.

[0006] According to the present invention, the container wall has an inner layer formed by a first plastic material and an outer layer formed by a second plastic material, and the container connecting piece has a longitudinal cross-section that widens toward the container opening, so that the end face of the container connecting piece is at least partially formed by an inner layer section arranged opposite to the outer layer, and the welding contact surface of the container connecting piece is constituted by the inner layer section.

[0007] In this context, the term "end face" is understood to mean the surface projection of the container nozzle into the front plane of the plastic container, i.e., parallel to the plane of the container wall with the container nozzle, so that the inner layer section forms a surface projection into the end face and thus forms a welding contact surface of the container nozzle when establishing a welding contact between the connection nozzle of the container fitting and the container nozzle. Since the relative arrangement of the outer layer and the inner layer section is determined so that the outer layer is opposite to the inner layer section, i.e., arranged away from the inner layer section, it is prevented that welding contact will occur between the connection nozzle of the container fitting and the outer layer of the container wall when welding is performed. More precisely, due to the design according to the invention, the welding contact or the formation of the welding contact surface at the container nozzle is limited to the inner layer section. This ensures that welding contact between materials that are incompatible with respect to the welded connection does not occur, which adversely affects the quality of the welded connection.

[0008] In a particularly preferred embodiment of the plastic container, the container nozzle is conically designed so that the welding contact surface is formed by the outer side of an inner cone provided with an inner layer, which is welded to an outer cone formed on the connecting nozzle of the container fitting.

[0009] In the method according to the invention, when blow-molding a plastic container having a container wall to form a bulge, the container wall is expanded into the widened wall recess of the blow mold so that the bulge formed in the container wall has an enlarged cross section toward the top wall, and after the top wall is separated to form the container opening, a welding contact surface formed by an inner layer section extending toward the container opening is formed, wherein the container wall has an inner layer formed by a first plastic material and an outer layer formed by a second plastic material. The welding method subsequently carried out can be carried out in particular as a heating element butt welding method. Possible further welding methods that can be advantageously used are known friction welding methods, such as in particular spin welding and vibration welding.

[0010] This production method ensures that the welding contact surface formed by the inner portion is arranged exposed in the end face of the tank neck, so that when the welding contact is produced between the connection neck of the tank fitting and the tank neck, a surface contact is formed between the inner portion and the connection neck of the tank fitting.

[0011] It is particularly preferred that the expansion to the conically widening recess takes place in such a way that the conically shaped welding contact surface explained above is achieved, with the advantageous effects resulting therefrom.

[0012] If the formation of the bulge is carried out in at least two expansion steps, so that in a first expansion step the central region of the bulge is formed and subsequently in a second expansion step the conical wall region of the bulge arranged concentrically to the central region is formed, then the maximum expansion that occurs when forming the bulge can be reduced compared to forming the bulge in only one expansion step, so that the resulting wall thickness reduction of the container wall after the expansion is correspondingly limited. This can ensure, in particular, that the inner layer section has the material strength required for forming a high-quality welded connection.

[0013] It is particularly advantageous here if the central region of the elevation is cylindrical in design, so that a uniform wall thickness distribution can be achieved in the conical region.

[0014] Preferably, the formation of the central region of the bead can be carried out simultaneously with the formation of the blow-molded body, so that by carrying out the two-stage expansion method there is no significant increase in the blow-molding time for producing the blow-molded body. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] The preferred embodiments of the present invention are described in detail below with reference to the accompanying drawings. The accompanying drawings show:

[0016] Figure 1 A perspective view of a liquid container designed as a tray-type container having an inner container designed as a plastic container is shown;

[0017] Figure 2 A side view, shown in partial section, shows an enlarged view of the fitting connection area of ​​the plastic container;

[0018] Figure 3a An enlarged detail view showing a welded connection formed between a tank connector and a connecting connector of a tank fitting;

[0019] Figure 3b Show Figure 3a A front view of the container nozzle shown in FIG.

[0020] Figure 4a A first production step for producing a container nozzle by a blow molding method is shown;

[0021] Figure 4b The central region of the raised portion for forming the container neck is shown. Figure 4a In the first manufacturing step shown in , it is produced at the plastic container;

[0022] Figure 5aA second production step for producing a container nozzle is shown;

[0023] Figure 5b The bulge produced on the plastic container by means of a second production step for forming a container neck is shown;

[0024] Figure 5c Shown in Figure 5b A cross-sectional view of a raised portion shown in FIG.

[0025] Figures 6a to 6c A schematic diagram shows the connection of a tank fitting to a tank connecting piece using a heating element butt welding method. DETAILED DESCRIPTION

[0026] Figure 1 A transport and storage container which can be used as a disposable and reusable container is shown, which has a plastic container 10 which is in the form of a cuboid and which in the present case has a filling nozzle 15 which is formed in a container wall 13 on the upper side of the plastic container 10 and is provided with a cover 14 and a container nozzle 17 for connecting a container fitting 18 which is in the present case designed as a withdrawal fitting in a fitting connection area 16 of the container wall 13 on the front side of the plastic container 10 .

[0027] For the purpose of forming a transport and storage container, the plastic container 10 is arranged on a pallet-like base frame 19 which, for supporting the plastic container 10 , has a supporting base 20 which is formed in the present case as a flat bottom trough.

[0028] The plastic container 10 is produced by blow molding from a tubular parison, wherein the container nozzle 17 is produced together with the cuboid main body of the plastic container 10 in the blow molding process.

[0029] Figure 2 The welded connection 52 between the container connector 17 and the connecting connector 21 of the container fitting 18 is shown after the plastic container 10 has been produced by the blow molding method. Figure 2As can be seen in the figure and also shown in particular in the enlarged view in FIG. 3 , the container wall 13 of the plastic container 10 has a multilayer wall structure, wherein in the present case, an inner layer 22 consisting of HDPE is separated from an outer layer 24 by a barrier layer 23 consisting of EVOH in the present case. Since the inner layer 22 is subject to increased demands on the quality of the material due to direct contact with the liquid contained in the plastic container 10, especially in the case of food contact, the inner layer is usually made of a homogeneous material of a defined composition, such as HDPE. In contrast, as a material for the outer layer 24, a so-called recycled material is usually used, which is produced by shredding and grinding the plastic material of used plastic containers. In addition, in the present case, the plastic container 10 designed as an explosion-proof container has a front layer 25 formed of an electrically conductive material as an outer surface.

[0030] Here, the term outer layer refers to a layer which, unlike the inner layer, is arranged toward the outside of the plastic container, wherein the outer layer does not necessarily have to constitute the outermost layer of the plastic container, but a further layer arranged toward the outside of the plastic container can be provided, such as the front layer or other functional or decorative layers mentioned above by way of example. Preferably, the inner layer consists of a first-use material, while the outer layer consists of a material formed from ground material, wherein the ground material can come from production waste generated during the production of the blow molded body or also from recycled plastic containers.

[0031] In contrast to the exemplary embodiment described, the inner layer and the outer layer can also be arranged directly on each other. In the case of an intermediate functional layer, such as the barrier layer mentioned above by way of example, an adhesion promoter can also be provided between the functional layer and the adjacent layer.

[0032] As in Figures 6a to 6c As shown in FIG. 1 , a connection piece 21 is formed between the container connector 17 and the container fitting 18. Figure 2 3, so that the welding contact surfaces 26, 27, which are to be welded to each other at the container connection 17 and the connection connection 21, are heated by means of a welding mirror 28 arranged between the welding contact surfaces 26, 27 arranged opposite each other until a pasty consistency is achieved. For this purpose, the welding contact surfaces 26, 27 are moved toward the heating surfaces 29, 30 of the welding mirror 28 and heated by heat conduction, such as in Figure 6b After the required welding temperature in the welding contact surfaces 26, 27 has been reached or the container connector 17 and the connection connector 21 have been melted in the region of the welding contact surfaces 26, 27, the welding mirror 28 is removed from its position. Figure 6b The intermediate position shown in FIG. 1 is moved out and the welding contact surfaces 26, 27 are made as in FIG. Figure 6c , are moved toward each other under pressure so that during subsequent cooling a welded connection 52 can be formed.

[0033] Since the production of a welded connection requires corresponding material compatibility in the region of the welding contact surfaces 26 , 27 , welding of a container fitting 18 made of PE material to an electrically conductive front layer 25 that is incompatible with the material of the barrier layer 23 or container wall 13 made of EVOH material is not possible.

[0034] In order to ensure Figures 6a to 6c The welded connection shown as a heating element butt weld connection by way of example can be produced between the container wall 13 which, in addition to the inner layer 22, also has a barrier layer 23, an outer layer 24 and a front layer 25 and the connecting piece 21, as in particular in Figure 2 and 3a As shown in FIG. , the container connection piece 17 has a longitudinal cross section which widens toward the container opening 31 formed at the container connection piece 17 , as shown in FIG. Figure 3a As shown in FIG. 1 , the container takes over 17 at Figure 3b The end face 32 shown in FIG. 1 , ie, the end face of the container connecting piece 17 at the container connecting piece 17 at the Figure 3b The surface projected into the drawing plane in the front view X shown in FIG. 1 has an inner layer section 33, which, when establishing the butt-welded connection 52, is exposed to provide for the connection with the connecting piece 21 in order to form the welding contact surface 26. Figure 3a The barrier layer 23 and the front layer 25 can be arranged in such a way that the inner layer section 33 forming the contact surface 26 of the container nozzle 17 does not hinder the establishment of the welded connection 52.

[0035] exist Figure 2 In the exemplary embodiment shown in FIGS. 1 and 3 , the container connector 17 is conically designed so that the welding contact surface 26 of the container connector 17 is formed by the outer side 34 of the inner cone 35 formed by the container connector 17 , which is welded to the outer cone 36 formed on the connecting connector 21 of the container fitting 18 .

[0036] Next, we will refer to Figures 4a to 5c The production of a container nozzle 17 formed on the container wall 13 in a blow molding process is described, wherein the container nozzle 17 is formed based on a bulge 37 that is initially formed in the container wall 13. Figure 4a and 5a As shown in the comparison of FIG. 1 , the production of the raised portion 37 is carried out in two expansion steps, wherein Figure 4a As shown, a molding tool 40 is used which is arranged in the mold wall 38 of the blow mold at the wall recess 39, and in the present case has a cylindrical inner slide 41 and an outer slide 42 which is arranged coaxially with the cylindrical inner slide 41, wherein the inner slide 41 and the outer slide 42 with their slide bottoms 43 or 44 form the mold bottom 46 of the wall recess 39 except for the radial edge area 45.

[0037] like Figure 4aand 5a As shown, the recess 39 is designed in such a way that it widens in the direction of the mold base 46 into the mold wall 38 so that an annular undercut 47 is formed in the mold wall 38 , so that the recess 39 is conical overall.

[0038] like Figure 4a As shown in the figure, the inner slider 41 and the outer slider 42 are arranged relative to each other when implementing the first expansion step, wherein the slider bottom 43 of the inner slider 41 is located in the plane of the mold bottom 46 and the slider bottom 44 of the outer slider 42 is basically arranged in the plane of the mold wall surface 48, so that the undercut 47 is covered by the outer slider 42 and a cylindrical mold cavity 49 is formed within the wall recess 39.

[0039] As from Figure 4a and 4b From the overview of FIG. 1 , it can be seen that when the container wall 13 is expanded into the wall recess 39, the middle region 50 of the bulge 37 is first formed, that is, the preform of the bulge 37, which is then only formed in the Figure 5a In order to carry out the second expansion step, the slider bottom 44 of the outer slider 42 is moved to a flush arrangement with the slider bottom 43 of the inner slider, so that from now on the two slider bottoms 43, 44 are arranged in the plane of the mold bottom 46 and form a mold cavity 51 which is supplemented by the undercut 47.

[0040] In the second expansion step, an annular wall region 53 of the fitting connection region 16 of the container wall 13, which surrounds the middle region 47 and is still supported on the outer slide 42 in the first expansion step, is expanded, wherein the area of ​​the wall region 53 corresponds to the sum of the area of ​​the slide base 44 of the outer slide and the slide inner wall area 54 formed by the slide projection s of the outer slide 42 relative to the inner slide 41. Since the area is only slightly smaller than the partial surface of the wall recess 39, which is formed by the sum of the surfaces of the slide base 44 of the outer slide 42 and the undercut 47, in Figure 5a The expansion in the second expansion step shown in the figure essentially causes the edge area 53 supported on the outer slide 42 to flip over into the radial edge area 45 of the mold bottom 46 and the adjacent undercut 47, so that the wall area 52 undergoes only a limited expansion and the most expanded part of the protrusion 37 is formed in the area of ​​the top wall 55 of the protrusion 37 that is in contact with the mold bottom 46.

[0041] like Figure 5c As indicated by the dividing line in the figure, the top wall 55 forms the part of the protrusion 37 which is removed by the separating cut to form the container opening 31 at the container connecting piece 17 , so that the finished container connecting piece 17 does not have a wall thickness reduction that impairs the functionality of the container connecting piece 17 compared to the surrounding fitting connection area 16 of the container wall 13 .

Claims

1. A plastic container (10) for liquids, the plastic container (10) being formed as a blow-molded body by blow molding from a tubular parison in a blow mold, and having a container connecting piece (17) for connecting a container fitting (18) in a fitting connection region (16) of a container wall (13), the container connecting piece (17) being provided with a container opening (31) and being connected to a connecting piece (21) of the container fitting (18) via a welded connection (52), The container wall (13) comprises an inner layer (22) formed from a first plastic material and an outer layer (24) formed from a second plastic material, and the container nozzle (17) has a longitudinal cross section which widens towards the container opening (31), so that an end face (32) of the container nozzle (17) is at least partially formed by an inner layer section (33) arranged opposite the outer layer (24), and a welding contact surface (26) of the container nozzle (17) is formed by the inner layer section (33), It is characterized in that The container nozzle (17) is designed to be conical so that the welding contact surface (26) is formed by the outer side (34) of an inner cone (35) which is provided with the inner layer (22) and is welded to an outer cone (36) formed on the connecting nozzle (21) of the container fitting (18) which extends outside the plastic container (10).

2. The plastic container according to claim 1, It is characterized in that The plastic container (10) is an inner container for a transport and storage container for liquids, the transport and storage container having an outer cover made of a grid structure or a plate material and a tray-type base frame.

3. A method for producing a plastic container (10) for liquids, the plastic container (10) being formed into a blow-molded body by blow-molding a tubular parison in a blow mold and having a container connecting piece (17) for connecting a container fitting (18), the container connecting piece (17) being formed in a fitting connecting region (16) of a container wall (13) and being provided with a container opening (31), wherein, for forming the container connecting piece (17), a bulge (37) of the container wall (13) closed by a cover wall (55) is formed in a wall recess (39) of the blow mold, the container opening (31) is subsequently formed by separating the cover wall (55), and the connection of the container connecting piece (17) to the connecting piece (21) of the container fitting (18) is subsequently formed as a welded connection (52), The container wall (13) comprises an inner layer (22) formed of a first plastic material and an outer layer (24) formed of a second plastic material, and when the plastic container (10) is blow-molded to form a bulge (37), the container wall (13) expands into a widened wall recess (39) of the blow mold, so that the bulge (37) formed in the container wall (13) has an enlarged cross section toward the top wall (55), and after the top wall (55) is separated to form the container opening (31), a welding contact surface (26) formed by the inner layer section (33) extending toward the container opening (31) is formed, It is characterized in that The container wall (13) is expanded into the conically widening wall recess (39).

4. The method according to claim 3, It is characterized in that The plastic container (10) is an inner container for a transport and storage container for liquids, the transport and storage container having an outer cover made of a grid structure or a plate material and a tray-type base frame.

5. The method according to claim 3 or 4, It is characterized in that The formation of the raised portion (37) is carried out in at least two expansion steps, so that in a first expansion step a central region (50) of the raised portion (37) is formed, and subsequently in a second expansion step a conical wall region (53) of the raised portion, which is arranged concentrically with the central region, is formed.

6. The method according to claim 5, It is characterized in that The central region (50) of the elevation (37) is cylindrical in design.

7. The method according to claim 5, It is characterized in that The formation of the central region (50) of the raised portion (37) is performed simultaneously with the formation of the blow-molded body.

8. The method according to claim 6, It is characterized in that The formation of the central region (50) of the raised portion (37) is performed simultaneously with the formation of the blow-molded body.

Citation Information

Patent Citations

  • Method of manufacturing a plastic container for liquids

    EP1630105A2

  • Method for manufacturing fuel tanks

    CN102271894A

  • Method for manufacturing plastic liquid vessel

    CN1736691A