A discrete element modeling method for selective laser sintering powder laying process considering the properties of the sintered powder layer
By adopting a discrete element modeling method that considers the properties of the sintered powder layer in selective laser sintering, the problem of poor powder spreading uniformity in the existing technology is solved, achieving more accurate simulation of the sintering process and improving part quality.
Patent Information
- Application Number
- CN202210352357.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-04-04
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2042-04-04
AI Technical Summary
The existing technology is difficult to realize real-time monitoring of particle movement during selective laser sintering, and fails to effectively consider the impact of the sintered layer on the powder spreading process, resulting in poor uniformity of powder spreading, resulting in defects such as spheroidization, pores or erosion, and reduces the Part quality.
A discrete element modeling method for the selective laser sintering powder coating process that takes into account the properties of the sintered powder layer is used. By establishing a three-dimensional closed calculation area, the particle accumulation is generated, the physical properties of the particles are set, the powder coating roller is imported, and the discrete element model is used to identify The particles in the sintering area are given physical properties of the sintered layer, and the powder spreading process of the particles on the sintered layer is simulated to study the powder spreading uniformity.
It achieves a more accurate simulation of the selective laser sintering powder coating process, improves powder coating uniformity, reduces defects, and improves the quality of finished parts.
Smart Images

Figure CN114692477B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the study of discrete element modeling and simulation of powder particle fluidity in selective laser sintering, and specifically relates to a discrete element modeling method for a selective laser sintering powder spreading process taking into account the properties of a sintered powder layer. Background Art
[0002] Additive manufacturing technology is a widely used processing technology in the manufacturing field. It integrates computer application, material processing and molding technology. Among them, selective laser sintering is a rapid processing technology that is currently used more frequently. As a powder-based 3D printing process, it has become an important technology for producing various components and structures in the past decade. It uses high-intensity laser as an energy source, and based on computer-aided design, it melts and sinters the selected areas of the powder material layer by layer. The process of selective laser sintering is mainly divided into two stages: the powder spreading stage and the melting stage. Among them, the powder spreading process is a crucial link, and the uniformity of the powder spreading has a significant impact on the quality of the sintered parts. It is generally believed that a loose powder bed with voids or displacement defects will make the powder melt worse, and then produce defects such as spheroidization, pores or erosion, which reduces the quality of the finished parts.
[0003] It is difficult to achieve real-time monitoring of particle movement in the experiment of powder uniformity in selective laser sintering. Therefore, most of the existing research on powder uniformity in the powder spreading process uses simulation modeling. In practice, what needs to be considered more is the effect of the sintered layer of the part on the flow properties of the particles in the powder spreading process. The particles in the sintered area often present a molten pool state, and the particles are mutually bonded. The sintered area has a certain adsorption force on the dry particles and the temperature is much higher than the unsintered area. Therefore, it is significantly different from the particles in the surrounding unsintered area. Existing public technical data or literature does not consider the simulation study of the effect of the properties of the sintered layer on the uniformity of particle powder spreading. Therefore, it is necessary to propose a discrete element modeling method for the selective laser sintering powder spreading process that considers the properties of the sintered powder layer. Summary of the invention
[0004] In view of the above technical problems existing in the prior art, this paper proposes a discrete element modeling method for the selective laser sintering powder laying process which takes into account the properties of the sintered powder layer.
[0005] The present invention adopts a discrete element modeling method for a selective laser sintering powder spreading process taking into account the properties of a sintered powder layer, and is characterized in that the method steps for establishing a discrete element model are as follows:
[0006] (1) Construct a coordinate system X0Y0Z0 and establish a three-dimensional closed calculation region. The closed calculation region takes a cube as an example. The length of each edge is L. Its coordinate axis X0Y0Z0 is parallel to the three intersecting edges of the cube. The geometric symmetry center of the closed calculation region is the origin of the constructed coordinate system X0Y0Z0.
[0007] (2) Generate a particle accumulation of 2 to 3 times the volume of the powder layer on one side of the closed calculation area constructed in step (1), and set the basic physical property parameters of the particle material including particle size distribution, Poisson's ratio, particle density, shear modulus, restitution coefficient, friction coefficient, etc.; the contact model can be set to a particle contact model such as Hertz-Mindlin (no-slip) and linear elastic contact model (i.e., the relative relationship between the contact force and the local deformation between the two contacting particles during the normal-tangential relative motion); then introduce a powder spreading roller parallel to the Y axis of the closed calculation domain, and set its translation speed and rotation speed to move along the positive direction of the X axis, so that the powder particles are spread into layers, and the powder spreading height each time is ΔZ;
[0008] (3) Establish a three-dimensional model of the part to be sintered according to the requirements, which can be any geometric shape;
[0009] (4) Import the three-dimensional model of the part to be sintered into the established closed calculation area. The imported model is now a non-solid area to be identified. Adjust the position of the three-dimensional model of the part to be sintered relative to the closed calculation area so that the whole part is completely within the closed calculation area and is located directly above the powder particles of the powder layer. The lowest point of the three-dimensional model to be sintered is tangent to the top particles of the powder layer. The X and Y coordinates of the three-dimensional model of the part to be sintered are parallel to the X0 and Y0 coordinate directions of the closed calculation domain respectively.
[0010] (5) Generate a particle accumulation of 2 to 3 times the volume of the powder layer on one side of the already laid powder layer, set the translation speed and rotation speed of the powder laying roller to lay the powder particles into layers, and the powder laying height is ΔZ;
[0011] (6) After the second powder spreading is completed, take a cross section of the 3D model of the part to be sintered at the height of the last powder spreading, and identify the boundary extreme point X of the projection of the 3D model on the XY plane in the cross section. min and X max , divide the cross-sectional area into N equal parts in the X direction, thereby obtaining the coordinates X of each equally divided point i The corresponding boundary value f u,k (X i ) and f d,k (X i ), where X max , X min are the maximum and minimum values of the three-dimensional model in the X direction at the iΔZ section layer position, respectively. u,kis the kth point X i The corresponding upper boundary value, f d,k is the kth point X i The corresponding lower boundary value is used to obtain the boundary of the sintering area in the cross-section layer;
[0012] (7) To identify the particles, first narrow the particle identification range to the i-th powder layer. The calculation boundary of this layer is:
[0013]
[0014] Here L is the length of the three-dimensional closed calculation area in the X direction established in step (1), and then the particle center coordinate P is determined. i (x i ,y i ,z i ) Whether the following conditions are met at the same time: ①x i ∈[X min ,X max ],②y i ∈[f d,k (X i ),f u,k (X i )],③z i ∈[(i-1)△Z,i△Z], if the conditions are met, the particle is defined as a sintering region particle, and the particle sintering layer is given physical material properties, relevant thermal coefficients, and a contact model with sintering layer properties, such as a bonding contact model, a JKR model and other particle contact models (i.e., when there is a liquid bridge between two particles or they are in an impregnated state, when the two particles have normal or tangential relative motion, the normal extrusion pressure or tangential resistance model generated by the fluid viscosity); the cycle is repeated until the central coordinates of all particles in the calculation domain of the cross-section layer are determined, that is, a discrete element model with sintering properties in the powder-laying cross-section layer of the three-dimensional model of the part to be sintered is obtained;
[0015] (8) Repeat steps (5-7). The particles are layered on the sintering layer model under the action of the powder spreading roller. The particle layer can be divided into a grid, and the powder mass in the grid can be sampled. The powder spreading uniformity can be studied through its mass standard deviation. Secondly, the translation speed of the powder spreading roller or the height of the powder spreading layer can be adjusted to further study the influence of related factors on the powder spreading uniformity of powder particles on the powder layer with sintering layer properties. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 The present invention is a flowchart of a discrete element modeling method for a selective laser sintering powder laying process taking into account the properties of the sintered powder layer.
[0017] Figure 2 This is a schematic diagram of an example three-dimensional closed calculation area.
[0018] Figure 3 This is a schematic diagram of powder spreading by powder spreading roller in a closed calculation area.
[0019] Figure 4 It is a schematic diagram of the three-dimensional model of the part to be sintered imported into the calculation domain.
[0020] Figure 5 It is a schematic diagram of the cross section of the iΔZth powder layer in the Z direction of the three-dimensional model to be sintered.
[0021] Figure 6 It is a schematic diagram for determining the maximum and minimum values of the iΔZth powder layer cross section in the X direction in the Z direction of the three-dimensional model to be sintered.
[0022] Figure 7 It is a schematic diagram of the boundary of the sintering area in the cross section of the iΔZth powder layer.
[0023] Figure 8 It is a schematic diagram of particle discrimination within the (i-1)ΔZ~iΔZ powder layer.
[0024] Fig. 9 It is a schematic diagram of re-laying powder on a powder bed that has the properties of a sintered layer for parts. DETAILED DESCRIPTION
[0025] In order to make the purpose, technical solutions and advantages of the present invention more clearly understood, the present method is further described in detail below in conjunction with the accompanying drawings and embodiments.
[0026] A discrete element modeling method for a selective laser sintering powder spreading process considering the properties of a sintered powder layer, characterized in that the modeling steps are as follows:
[0027] (1) Construct a coordinate system X0Y0Z0 and establish a three-dimensional closed calculation region. The closed calculation region is a cube with an edge length of L. Its coordinate axes X0Y0Z0 are parallel to the three intersecting edges of the cube. The geometric symmetry center of the closed calculation region is the origin of the constructed coordinate system X0Y0Z0, as shown in Figure 2 As shown;
[0028] (2) Generate a particle accumulation of 2 to 3 times the volume of the powder layer on one side of the closed calculation area constructed in step (1). The particle radius obeys the normal distribution, with an average value of 1 mm and a standard deviation of 0.05. All particles are assigned physical property parameters. The specific parameters are shown in the following table:
[0029] Table 1 Particle physical property parameters
[0030]
[0031]
[0032] The contact model is set to the Hertz-Mindlin (no-slip) model, and then the powder spreading roller is imported parallel to the Y axis of the closed calculation domain, and its translation speed is set to 30 mm / s and the rotation speed is set to 25 rad / s along the positive X axis, and the powder particles are spread into layers, and the height of each powder spreading is 0.3 mm. Figure 3 As shown;
[0033] (3) Establish a three-dimensional model of the part to be sintered with a sphere of 10 mm in diameter, and establish the coordinate system XYZ of the spherical model to be sintered with the lowest point of the spherical model;
[0034] (4) Import the spherical model to be sintered into the established closed calculation area. The imported spherical model is now a non-solid area to be identified. Adjust the position of the spherical model so that it is completely within the closed calculation area and directly above the initially laid powder layer. The origin of the coordinate system of the spherical model is tangent to the top particles of the initially laid powder layer with a thickness of 0.3 mm, and the X and Y coordinates of the spherical model to be sintered are parallel to the X0 and Y0 coordinate directions of the closed calculation domain, respectively. Figure 4 As shown;
[0035] (5) Generate a particle accumulation of 2 to 3 times the volume of the powder layer on one side of the already spread powder layer, set the translation speed of the powder spreading roller to 30 mm / s and the rotation speed to 25 rad / s, spread the powder particles into layers, and the powder spreading height each time is 0.3 mm;
[0036] (6) After the second powder spreading, the particle layer height in the calculation domain is 0.6 mm. Take the cross section of the sphere model at Z = 0.6 mm and identify the boundary extreme point X of the projection of the sphere model on the XY plane in the cross section. min and X max ,like Figure 6 As shown, the cross-sectional area is divided into N equal parts in the X direction, thereby obtaining the coordinates X of each divided point i The corresponding boundary value f u,k (X i ) and f d,k (X i ),like Figure 7 As shown, where X max , X min are the maximum and minimum values of the sphere model in the X direction when the cross section is at Z = 0.6 mm, respectively. u,k is the kth point X i The corresponding upper boundary value, f d,k is the kth point X i The corresponding lower boundary value is used to obtain the boundary of the sintering area of the spherical model in the cross-section layer of Z = 0.6 mm;
[0037] (7) To identify the particles, first narrow the particle identification range to the i-th powder layer. The calculation boundary of this layer is:
[0038]
[0039] Then determine the particle center coordinates P i (x i ,y i ,z i ) Whether the following conditions are met at the same time: ①x i ∈[X min ,X max ],②y i ∈[f d,k (X i ),f u,k (X i )],③z i ∈[(i-1)△Z,i△Z], if the conditions are met, the particle is defined as a sintering region particle, and a Heat Conduction model is added to the particle based on the linear contact bonding model, with the specific heat capacity set to 50J / (kg.k), the thermal conductivity to 1000W / (mk), and the temperature and heat flux to 300K; the process is repeated until the center coordinates of all particles in the calculation domain of the cross-section layer are determined, and a discrete element model with sintering properties in the powder-laying cross-section layer of the three-dimensional model of the part to be sintered is obtained, such as Figure 8 As shown;
[0040] (8) Repeat steps (5)-(7). The particles are layered on the sintering layer model under the action of the powder spreading roller. The particle layer can be divided into a grid, and the mass of the powder in the grid can be sampled. The uniformity of the powder spreading can be studied through its mass standard deviation. Secondly, the translation speed of the powder spreading roller or the height of the powder spreading layer can be adjusted to further study the influence of related factors on the uniformity of the powder particles on the powder layer with sintering layer properties.
Claims
1. A discrete element modeling method for selective laser sintering powder laying process considering the properties of the sintered powder layer, characterized in that: The modeling steps are as follows: (1) Construct the coordinate system X0Y0Z0 and establish a three-dimensional closed calculation area; (2) Generate a particle accumulation of 2 to 3 times the volume of the powder layer on one side of the closed calculation area constructed in step (1), set the basic physical property parameters of the particle material and the contact model between particles, then introduce a powder spreading roller parallel to the Y axis of the closed calculation area, and set its translation speed and rotation speed to move along the positive direction of the X axis, so that the powder particles are spread into layers, and the powder spreading height each time is ΔZ; (3) Establishing a three-dimensional model of the part to be sintered; (4) Import the three-dimensional model of the part to be sintered into the established closed calculation area. The imported model is now a non-solid area to be identified. Adjust the position of the three-dimensional model of the part to be sintered relative to the closed calculation area so that the whole part is completely within the closed calculation area and is located directly above the powder particles of the powder layer. The lowest point of the three-dimensional model to be sintered is tangent to the top particles of the powder layer. The X and Y coordinates of the three-dimensional model of the part to be sintered are parallel to the X0 and Y0 coordinate directions of the closed calculation domain respectively. (5) Generate a particle accumulation of 2 to 3 times the volume of the powder layer on one side of the already laid powder layer, set the translation speed and rotation speed of the powder laying roller to lay the powder particles into layers, and the powder laying height is ΔZ; (6) After the second powder spreading is completed, take a cross section of the 3D model of the part to be sintered at the height of the last powder spreading, and identify the boundary extreme point X of the projection of the 3D model on the XY plane in the cross section. min and X max , divide the cross-sectional area into N equal parts in the X direction, and obtain the coordinates X of each divided point i The corresponding boundary value f u,k (X i ) and f d,k (X i ), f u,k is the kth point X i The corresponding upper boundary value, f d,k is the kth point X i The corresponding lower boundary value is used to obtain the boundary of the sintering area in the cross-section layer; (7) Identify the particles. If the center coordinates of the particles are within the boundary of the sintering region described in step (6), define the particles as sintering region particles, and assign contact models, physical material properties, and related thermal coefficients of the sintering layer properties of the particles. Repeat the cycle until all particles are identified, and obtain a discrete element model with sintering properties in the powder-laying cross-section layer of the three-dimensional model of the part to be sintered. (8) Repeat steps (5)-(7). After completion, analyze the powder spreading uniformity of the particles on the discrete element model of the sintered powder layer, further adjust the powder layer height or the translation and rotation speed of the powder roller, and study their effects on the powder spreading uniformity of the powder particles in selective laser sintering.
2. A discrete element modeling method for selective laser sintering powder laying process considering the properties of the sintered powder layer according to claim 1, characterized in that: The three-dimensional closed calculation area described in step (1) is a cuboid, and the geometric symmetry center of the closed calculation area is the origin of the constructed coordinate system X0Y0Z0.
3. A discrete element modeling method for selective laser sintering powder laying process considering the properties of the sintered powder layer according to claim 1, characterized in that: The physical property parameters and contact model of the particle material described in step (2) can be adjusted. The particle physical property parameters include particle size distribution, Poisson's ratio, particle density, shear modulus, restitution coefficient, and friction coefficient. The contact model is set to Hertz-Mindlin and linear elastic contact models.
4. A discrete element modeling method for selective laser sintering powder laying process considering the properties of the sintered powder layer according to claim 1, characterized in that: The three-dimensional model of the part to be sintered described in step (3) is a geometric body of any shape.
5. The discrete element modeling method for selective laser sintering powder laying process considering the properties of the sintered powder layer according to claim 1, characterized in that: The particle identification described in step (7) first narrows the particle identification range to the i-th powder spreading layer, and the calculation boundary of this layer is: Here L is the length of the three-dimensional closed calculation area in the X direction established in step (1), and then the particle center coordinate P is determined. i (x i ,y i ,z i ) Whether the following conditions are met at the same time: ①x i ∈[X min ,X max ], where X max , X min are the maximum and minimum values of the three-dimensional model in the X direction at the iΔZ section layer position, ②y i ∈[f d,k (X i ),f u,k (X i )],③z i ∈[(i-1)ΔZ,iΔZ], if the conditions are met, the particle is defined as a sintering area particle, and the particle sintering layer is given physical material properties, relevant thermal coefficients, and a contact model with sintering layer properties, including a bonding contact model and a JKR model; the cycle is repeated until the center coordinates of all particles in the calculation domain of the cross-sectional layer are determined, and a discrete element model with sintering properties in the powder-laying cross-sectional layer of the three-dimensional model of the part to be sintered is obtained.
6. The discrete element modeling method for selective laser sintering powder laying process considering the properties of the sintered powder layer according to claim 1, characterized in that: The step (8) of analyzing the powder spreading uniformity of particles on the discrete element model of the sintered powder layer includes: the particles are layered on the sintered layer model under the action of a powder spreading roller, the particle layer is divided into grids, the powder mass in the grid is sampled, and the powder spreading uniformity is studied through its mass standard deviation; secondly, the translation speed of the powder spreading roller or the powder spreading layer height is adjusted to further study the influence of relevant factors on the powder spreading uniformity of powder particles on the powder layer having the properties of a sintered layer.
Citation Information
Patent Citations
Powder sintering neck generation process discrete element modeling method based on particle contact
CN107633147A
High-performance alloy steel selective laser melting thermal coupling behavior prediction method
CN112182921A