Electronic device and patterned glass layer thereof

By applying textured areas and specific coatings on the glass layer of electronic devices, the problem of indistinguishable appearance of the glass layer is solved, and visual distinction and decorative effect are improved.

CN114882799BActive Publication Date: 2024-11-12APPLE INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210684240.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2017-12-13
Filing Date
2018-07-18
Publication Date
2024-11-12
Estimated Expiration
2038-07-18

AI Technical Summary

Technical Problem

In electronic devices, the appearance of the glass layer is difficult to visually distinguish, resulting in undesired shading or excessive surface shining.

Method used

Visually distinguishable by selectively applying textured areas, alternating stacks of high-refractive or low-refractive dielectric layers or other thin-film interference filter coatings, ink layers, adhesive layers, etc. on the glass layer, a visually distinguishable filter coating is formed on the glass layer. area, such as logos, text, etc.

Benefits of technology

Visual distinction of the glass layer is achieved, undesired shading and excessive shine are avoided, and the decorative and visibility of the equipment is enhanced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114882799B_ABST
    Figure CN114882799B_ABST
Patent Text Reader

Abstract

An electronic device and a patterned glass layer thereof are disclosed. The electronic device may have a display on the front of the device and may have a glass layer that forms part of the housing on the back of the device. The glass layer may be provided with regions having different appearances. The regions may be textured, may have a coating such as a thin film interference filter coating formed from a stack of dielectric materials having alternating refractive indices, may have a metal coating, and / or may have an ink coating. The textured surface may be formed on a thin glass layer and a polymer film coupled to the glass layer. The glass layer may be formed from a pair of coupled glass layers. The coupled layer may have one or more grooves or other structures to visually distinguish different regions of the glass layer.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] Division Statement

[0002] This application is a divisional application of the Chinese invention patent application with the application date of July 18, 2018, the invention name of which is “Patterned Glass Layer in Electronic Devices” and the application number is 201880049255.3.

[0003] Priority declaration

[0004] This application claims priority to U.S. Patent Application No. 15 / 841,117 filed on December 13, 2017 and Provisional Patent Application No. 62 / 539,454 filed on July 31, 2017, which are hereby incorporated by reference in their entirety. Technical Field

[0005] The present disclosure relates generally to electronic devices, and more particularly, to forming visually distinguishable areas in glass structures in electronic devices. Background Art

[0006] The present disclosure relates generally to electronic devices, and more particularly, to forming visually distinguishable areas in glass structures in electronic devices.

[0007] Electronic devices such as cell phones, computers, watches, and other devices may include glass structures. For example, an electronic device may have a display in which an array of pixels is covered with a transparent glass layer. In some devices, a rear housing wall may be covered by the glass layer. A decorative layer may be applied to the glass layer to help improve the appearance of the rear housing wall. Summary of the invention

[0008] The electronic device may include electronic components and other components mounted within the interior of the housing.The device may have a display on the front face of the device and may have a glass layer forming a rear housing wall on the opposite back face of the device.

[0009] The rear housing wall may be provided with regions having different appearances. The regions may be selectively textured, may be selectively provided with a coating, such as a thin film interference filter coating formed from a stack of dielectric materials having alternating refractive indices, a metal coating, and / or an ink coating, and / or may have other structures that visually distinguish regions.

[0010] An area of ​​the rear housing wall may have a matte appearance formed by a textured surface.The textured surface may be formed directly on the glass layer, and / or the textured surface may be formed on a thin glass layer and a polymer film coupled to the glass layer.

[0011] The glass layer may be formed from a pair of coupled glass layers. The coupled layers may have one or more grooves or other structures to visually distinguish different areas of the glass layer. BRIEF DESCRIPTION OF THE DRAWINGS

[0012] Figure 1 is a perspective view of an exemplary electronic device according to an embodiment.

[0013] Figure 2 is a cross-sectional side view of an illustrative electronic device according to an embodiment.

[0014] Figure 3 is a rear view of an exemplary electronic device according to an embodiment.

[0015] Figure 4 is a cross-sectional side view of an exemplary glass layer having textured and smooth regions overlapped by a coating on an outer surface of the glass layer according to an embodiment.

[0016] Figure 5 is a cross-sectional side view of an exemplary glass layer having an outer surface including a textured region and a smooth region and having an inner surface with a coating overlapping the smooth region according to an embodiment.

[0017] Figure 6 is a cross-sectional side view of an exemplary glass layer having an inner film including a textured region according to an embodiment.

[0018] Figure 7 is a cross-sectional side view of an exemplary glass layer covered with a textured thin glass layer and a plurality of coatings interposed between the thin glass layer and an outer surface of the glass layer according to an embodiment.

[0019] Figure 8 is a cross-sectional side view of an exemplary glass layer having an outer surface covered with layers such as a thin glass layer and an intervening coating according to an embodiment.

[0020] Fig. 9 is a cross-sectional side view of an illustrative glass layer coated with multiple selectively textured layers according to an embodiment.

[0021] Fig.10 is a cross-sectional side view of an exemplary glass layer having a textured coating film attached to a glass layer with an interposed adhesive layer according to an embodiment.

[0022] Fig.11 is a cross-sectional side view of an exemplary glass layer having a textured region formed directly on an outer surface of the glass according to an embodiment.

[0023] Fig.12is a cross-sectional side view of an exemplary glass layer having a textured region formed directly on an interior surface of the glass according to an embodiment.

[0024] Fig.13 is a cross-sectional side view of an exemplary glass layer having a textured surface and having grooves with a tapered cross-sectional profile according to an embodiment.

[0025] Fig.14 is a cross-sectional side view of an illustrative glass layer formed from a pair of coupled sub-layers having overlapping grooves defining a cavity within the glass layer according to an embodiment.

[0026] Fig.15 is a cross-sectional side view of an illustrative glass layer having visible internal structures such as laser damaged regions embedded within the glass layer according to an embodiment.

[0027] Fig.16 is a cross-sectional side view of an illustrative glass layer having a coating including particles, such as glass particles, according to an embodiment. DETAILED DESCRIPTION

[0028] Electronic devices and other items may have structures formed of transparent materials. For example, an electronic device may include a display. The display may have a pixel array for displaying images to a user. In order to protect the pixel array from damage, the display may be covered by a layer of transparent material that acts as a display cover layer. The transparent material may be a ceramic, a polymer, a crystalline material (such as sapphire), or other suitable transparent material. Configurations in which such layers are formed of glass are sometimes described herein as examples. Some parts of the electronic device such as optical windows, buttons, housing walls (e.g., rear housing walls), and other structures other than the display cover layer may also be formed of ceramics, polymers, crystalline materials such as sapphire and / or glass, and may be transparent or may be colored. For example, the back of the electronic device may be covered with a glass layer that forms the rear housing wall.

[0029] It may be desirable to locally and / or globally change the appearance of a glass layer (or other material layer) in an electronic device. For example, it may be desirable to create an attractive decoration around a display, around the perimeter of a camera window or button, or other suitable location. In some arrangements, it may be desirable to selectively modify the appearance of a glass layer or other structure to form text, graphic patterns such as icons, logos, and / or other patterns visible to a user.

[0030] When creating structures such as these, there is the potential for unattractive features to form on the glass layer. For example, if care is not taken, undesirable shading may occur, or the surface may appear to be excessively shiny.

[0031] These issues can be addressed by forming visually distinguishable areas on glass layers (e.g., for forming visually distinguishable areas for logos, text, etc.) through the use of textured areas, neutral or non-neutral color reflective coatings formed from stacks of alternating high or low refractive index dielectric layers or other thin film interference filter coatings (sometimes referred to as dichroic layers or decorative layers), ink layers, adhesive layers, and / or other structures that apply visible changes selectively and / or globally to glass layers and other layers in an electronic device.

[0032] Figure 1 An illustrative electronic device of the type that may include a glass structure is shown in . Electronic device 10 may be a computing device such as a laptop computer, a computer monitor including an embedded computer, a tablet computer, a cellular telephone, a media player, or other handheld or portable electronic device, a smaller device such as a wristwatch device (e.g., a watch with a wristband), a hanging device, a headphone or earpiece device, a device embedded in glasses or other device worn on a user's head, or other wearable or miniature device, a television, a computer display that does not include an embedded computer, a gaming device, a navigation device, an embedded system (such as a system in which an electronic device with a display is installed in a kiosk or a car), a device that implements the functionality of two or more of these devices, or other electronic device. In Figure 1 In the exemplary configuration of , device 10 is a portable device, such as a cellular phone, a media player, a tablet computer, a wrist device, or other portable computing device. Other configurations can be used for device 10 if desired. Figure 1 The examples are for illustrative purposes only.

[0033] exist Figure 1 In the example of , device 10 includes a display, such as display 14 mounted in housing 12. Housing 12, which may sometimes be referred to as a casing or housing, may be formed of plastic, glass, ceramic, fiber composite materials, metal (e.g., stainless steel, aluminum, titanium, gold, etc.), other suitable materials, or a combination of any two or more of these materials. Housing 12 may be formed using a unitary configuration in which a portion or all of housing 12 is machined or molded into a single structure, or may be formed using multiple structures (e.g., an internal frame structure, one or more structures forming an external housing surface, etc.).

[0034] Display 14 may be a touch screen display that incorporates a conductive capacitive touch sensor electrode layer or other touch sensor component (e.g., a resistive touch sensor component, an acoustic touch sensor component, a force-based touch sensor component, a light-based touch sensor component, etc.) or may be a non-touch-sensitive display. Capacitive touch screen electrodes may be formed from an array of indium tin oxide pads or other transparent conductive structures.

[0035] Display 14 may include a pixel array formed from liquid crystal display (LCD) components, an electrophoretic pixel array, a plasma pixel array, an organic light emitting diode pixel array or other light emitting diodes, an electrowetting pixel array, or pixels based on other display technologies.

[0036] Display 14 may include one or more glass layers. For example, the outermost layer of display 14 (which may sometimes be referred to as a display cover layer) may be formed of a hard transparent material such as glass to help protect display 14 from damage. Other portions of device 10, such as portions of housing 12 and / or other structures, may also be formed of glass. For example, walls in housing 12, such as a rear housing wall, may be formed of glass.

[0037] Figure 2 For an exemplary device including a glass structure such as Figure 1 A cross-sectional side view of the device 10 is shown. Figure 2 As shown, device 10 may have opposing front and back sides. Display 14 may be formed on the front side of device 10. Housing 12 may have a rear housing wall formed by layer 24 on the opposing back side of device 10. Portions of housing 12 may also form side walls of device 10. These side wall portions of housing 12 may be formed from a material such as metal, for example.

[0038] Display 14 may include display cover layer 16 (e.g., a glass layer) and display module 18 (e.g., a display layer formed into an array of pixels that presents an image to a user on the front face of device 10). Display module 18 may be a liquid crystal display structure, an organic light emitting diode display structure, or other suitable display. During operation, module 18 may present an image visible through display cover layer 16. The rear portion of the housing of device 10 may be formed from a glass structure (e.g., layer 24 may be a glass layer). Layer 24 may have a thickness of 0.2 mm-5 mm, at least 0.05 mm, at least 0.1 mm, at least 0.2 mm, at least 0.5 mm, at least 0.75 mm, less than 1 mm, less than 2 mm, or other suitable thickness. If desired, a metal plate or other reinforcing structure may be laminated to the inner surface of layer 24 for enhanced strength. Internal components in device 10 such as component 22 (e.g., electronic components such as integrated circuits, sensors, etc.) may be mounted on one or more substrates, such as printed circuit 20.

[0039] Inactive border regions in layer 16 and portions of other glass structures in device 10 (such as some or all of glass layer 24) may be covered with coatings and other structures. In some arrangements, the coatings may be used primarily to block light (e.g., to hide internal device structures from view). For example, a coating may be formed on an interior surface of layer 24 to hide internal components from being viewed by a user (such as observer 26 viewing device 10 in direction 28). In other arrangements, patterned coatings may be used to form text, logos, decorations, and / or other visible patterns. Coatings that are not patterned and that coat all of glass layer 24 may also be used to prevent internal structures from being viewed and / or to provide a desired appearance for device 10. Patterned coatings may create visible elements and may also prevent internal structures from being seen.

[0040] The coatings for the glass structures in device 10 may be black or other neutral colors, or may have non-black (non-neutral) colors (e.g., blue, red, yellow, gold, rose gold, magenta, pink, etc.). In some configurations, some or all of the coatings for the glass structures in device 10 may be glossy (e.g., exhibiting a specular reflective surface having a reflectivity of at least 50%, less than 80%, at least 95%, less than 99.99%, or other suitable reflectivity). Textured features may also be formed.

[0041] If desired, the coating may include one or more layers defining textured areas on a layer, such as glass layer 24, interspersed with smooth and shiny areas that are not textured. For example, a logo may be formed as a shiny area and may be surrounded by a rough textured area. The textured and shiny areas may be formed by a textured and / or reflective surface on glass layer 24 and / or one or more layers coupled to glass layer 24. For example, the textured areas and / or shiny areas may be formed by a textured and / or shiny film adhered to glass layer 24. The textured areas and shiny areas may also be defined by directly texturing selected portions of glass layer 24.

[0042] Coatings on glass layer 24 and / or other glass structures in device 10 may be formed from metals, semiconductors, and / or dielectrics. Dielectric materials used for coatings may include organic materials such as polymer layers, and / or inorganic materials such as oxide layers, nitride layers, and / or other inorganic dielectric materials. In arrangements where it is desired to have a shiny surface, a metal coating with high reflectivity or a thin film interference filter with a dielectric layer (e.g., a stack of dielectric layers with alternating higher and lower refractive index values) may be configured to act as a mirror coating (reflective coating). Ink coatings may also be bonded to the glass structures.

[0043] Figure 3A top view of an exemplary configuration of the back side of device 10, in which one region (region 24-1) has a first appearance (textured, shiny, a particular color, etc.) and has a first shape (e.g., text, a logo, a decorative pattern, or other patterned shape), and in which another region (background region 24-2 in this example) has a second appearance (e.g., textured, shiny, a particular color, etc.). To ensure that region 24-1 is visible to a user of device 10, the appearance of regions 24-1 and 24-2 may contrast with each other. For example, in the case where region 24-1 is reflective (e.g., where region 24-1 is a shiny silver or gold region associated with a logo, text, etc.), region 24-2 may have a matte finish.

[0044] The glass layer 24 may have any suitable number of individual patterned regions, such as regions 24-1 and 24-2, each of which may have a different individual appearance. Configurations in which the glass layer 24 has one or more patterned layers that provide textured and shiny regions may sometimes be described herein as examples. Regions of the device 10 having different appearances may be formed by selectively patterning the glass layer 24 and associated coatings, films, and other structures. For example, these regions may be selectively formed by depositing a coating using a mask mask or other selective deposition technique (such as a printing technique) using physical vapor deposition, chemical vapor deposition, or other deposition techniques followed by photolithography and etching; selective surface treatment such as selective laser treatment, selective roughening, or polishing using mechanical or chemical mechanical polishing equipment; selective treatment using machining equipment, sandblasting equipment using other particles, or sandblasting equipment; roughening or otherwise treating the surface of the polymer film by using an imprinting tool, a press, and / or by using other equipment for selectively treating specific areas of a coating, film, and / or surface (e.g., a glass layer surface).

[0045] Textured surfaces in layer 24 and / or in coatings, films, and / or other layers coupled to layer 24 may provide a matte finish. These textured surfaces may have protruding surface structures with a height of 100 nm to 1 micron (e.g., at least 100 nm, at least 500 nm, less than 5 microns, less than 1 micron). Such textured surfaces may have an RMS surface roughness of 100 nm to 2 microns or other suitable values ​​and provide a desired appearance (e.g., a rough appearance). Smooth surfaces (e.g., polished surfaces or other smooth surfaces) may have protruding surface features with a height of less than 5 nm, surfaces with features with a height of less than 50 nm, etc. Such smooth surfaces may have an RMS surface roughness less than the RMS surface roughness of the textured surface (e.g., an RMS surface roughness less than 25 nm or other suitable values ​​and providing a desired appearance such as a smooth potential reflective appearance). If desired, areas of the rear housing wall or other glass layer structures of device 10 may have other roughness values ​​(e.g., those associated with strongly textured matte finishes and smooth reflective finishes). The use of textured surfaces and smooth surfaces to form visually distinct regions of glass layer 24 is merely illustrative.

[0046] Figures 4 to 16 Various examples of patterned areas on structures in device 10 are shown, such as a rear housing wall (e.g., glass layer 24) with potentially different visual appearances. These areas can be used to form logos, text, decorations, and / or other patterns. There can be any suitable number of patterned areas on layer 24, and these layers can include textured backgrounds and smooth backgrounds, textured foregrounds and smooth backgrounds, background and foreground elements of different colors, reflectivity values, etc. Coatings (e.g., anti-fouling coatings, anti-scratch coatings, etc.) can be provided on the outer surfaces of these exemplary patterned areas, or these external coatings can be omitted and / or combined with coatings, films, and surfaces to form layer 24 if desired. Figures 4 to 16 The examples are for illustrative purposes only.

[0047] Figure 4 2 is a cross-sectional side view of glass layer 24 in an exemplary configuration, wherein the outer surface of layer 24 has textured areas and coated areas such as smooth shiny areas. The textured areas are visually distinguishable from the smooth areas because the surface roughness of the textured areas is greater than the surface roughness of the smooth areas, thereby providing the textured areas with a matte appearance. Glass layer 24 can have opposing inner and outer surfaces, such as inner surface 32 and outer surface 30. Inner surface 32 can face internal device components, such as those located within housing 12 and device 10. Figure 1 Outer surface 30 may face a user of device 10 , such as an observer 42 viewing device 10 from outside of device 10 in direction 44 .

[0048] exist Figure 4, inner surface 32 is smooth and is coated by inner coating 34. Coating 34 may be a global layer covering the entire inner surface of layer 24 (for example). Outer coating 36 may be formed on region 40 of outer surface 30. Region 38 of outer surface 30 may be textured and may surround region 40 if desired. Coatings 36 and 34 may include one or more sub-layers (see, for example, exemplary sub-layer 46 of coating 34) or may each be formed of only a single material layer.

[0049] Coatings 36 and 34 may be shiny. For example, a stack of multiple dielectric sublayers in coatings 36 and / or 34 may have alternating refractive index values ​​to form a thin film interference filter or coatings 36 and / or coatings 34 may include a reflective material such as a metal. The texture of outer surface 30 in region 38 may provide glass layer 24 with a pleasing feel to the touch. Coating 36 in region 40 may be a physical vapor deposition coating deposited through a mask or other patterned layer, which may be shaped to form text, logos, or other visual elements, and may have a different appearance than the textured outer surface 30 in region 38. Coating 34 may help hide internal components from view by blocking light from being transmitted to the interior of device 10. If desired, coating 34 may be formed of an opaque material, such as a neutral color (white, black, or gray) or non-neutral color (red, blue, yellow, etc.) ink.

[0050] exist Figure 5 In the exemplary configuration of , the coating 36 in region 40 has been formed on the inner surface 32 of the glass layer 24. The outer surface 30 is smooth in region 40 and is textured in region 38. This method protects the coating 36 under the glass layer 24.

[0051] Figure 6 is a cross-sectional side view of an exemplary glass layer to which a layer of film having a textured region has been attached. Figure 6 As shown, film 48 (e.g., a flexible polymer sheet) may have a smooth surface attached to inner surface 32 of glass layer 24. Film 48 may be attached directly to surface 32, or may be attached to surface 32 using an intervening adhesive layer. Film 48 may have an inner surface that is textured in region 38 and smooth in region 40, so that regions 38 and 40 have a corresponding matte appearance and a shiny appearance. Film 48 may be covered with a polymer layer 50. Polymer layer 50 may have a lower refractive index than film 48 and may be covered with a coating 52. Coating 52 may be formed of ink or a shiny material such as metal. If desired, coating 52 may be a shiny coating formed of a thin film interference filter having a high reflectivity.

[0052] exist Figure 7In the example of , layer 54 can be a polymer film or can be a thin glass layer that is thinner than glass layer 24 (e.g., at least 3 times thinner, at least 7 times thinner, at least 10 times thinner, at least 20 times thinner, etc.). Using glass as an outer layer on top of glass layer 24 can help reduce scratches. In configurations where glass is used, the thickness of layer 54 can be relatively thin to enhance the appearance of a logo or other pattern formed by region 40. If desired, layer 54 can be a thin glass layer having a thickness of 20 microns-250 microns, at least 30 microns, at least 100 microns, at least 150 microns, less than 200 microns, less than 500 microns, or less than 800 microns. Thin glass layer 54 can have an outer surface that is textured in region 38 to provide region 38 with a matte appearance that is smooth in region 40, or textured region 38 can be formed by a textured surface on the inner surface of layer 54.

[0053] like Figure 7 As shown, the inner surface of layer 54 may be selectively coated with a first coating 56 (e.g., a patterned coating) in region 40. Coating 56 may be covered with a second coating such as a cover coating 58. Coatings 56 and 58 may provide an attractive appearance (e.g., a shiny appearance with a desired color, reflectivity, etc.). Coatings 56 and 58 may be formed of dielectric thin film interference filters (e.g., a stack of alternating high refractive index materials and low refractive index materials), may be formed of metals, and / or may be formed of other materials (e.g., inks). Because coating 56 is only present in region 40 and not in region 38, the presence of coating 56 will help visually distinguish regions 38 and 40. If desired, coating 56 may be omitted and / or coating 58 may be omitted, or coating 58 may be selectively omitted from region 40 but not region 38. An optically clear adhesive 60 may be used to attach film 54 and coatings 56 and 58 to outer surface 30 of layer 24. If desired, coating 56 (eg, a thin film interference filter, metal coating, and / or ink layer) may be formed on inner surface 32 of glass layer 24 rather than on the inner surface of film 54, as shown by coating 56'. In other configurations, both coatings 56 and 56' may be used.

[0054] Figure 8 24 in an exemplary configuration in which a thin glass layer having a textured inner surface has been coupled to an outer surface 30. Figure 8As shown, thin glass layer 66 (e.g., a glass layer having a thickness of at least 30 microns, at least 100 microns, at least 150 microns, less than 200 microns, less than 500 microns, or less than 800 microns, at least 3 times thinner, 7 times thinner, 10 times thinner, 20 times thinner, etc., than layer 24) may have a textured inner surface in region 38 to provide a rough appearance to region 38. The inner surface of thin glass layer 66 may be smooth in region 40. Coating 64 (e.g., a dielectric thin film interference coating, a metallic thin film coating, or other material such as an ink) may be formed on the inner surface of layer 66. Other patterned coatings such as coating 64 may be provided, such as in combination with the coating 64, if desired. Figure 7 The optically clear adhesive 62 may be used to attach the layer 66 and the coating 64 to the outer surface 30 of the layer 24.

[0055] If desired, chemical strengthening can be used to strengthen the thin glass layer, such as Figure 7 Layer 54 or Figure 8 of layer 66. In other configurations, thin glass layers such as layer 54 and layer 66 may be replaced by a polymer layer having textured areas and smooth areas.

[0056] exist Fig. 9 In the example of FIG. 1 , layer 72 has an outer surface that is textured in region 38. The inner surface of layer 72 may be textured in regions 38 and 38'. Thus, textured region 38 will have a rougher appearance than the appearance of textured region 38'. Layer 72 may be made of a thin glass layer (see, e.g., Figure 7 Layer 54 and Figure 8 The coating 70 may be formed on the inner surface of the layer 72, and an optically transparent adhesive layer 68 may be used to attach the layer 72 and the coating 70 on the layer 72 to the outer surface 30. The coating 70 may be a thin film interference filter, a metal layer, or an ink layer. There is no texture on the layer 72 or the coating 70 in the region 40, so the region 40 will not have a rough appearance. Because the region 38 and the region 38 'have different appearances, the region 38 and / or 38 ' may have the shape of text, logos, decorative patterns and / or other patterns, and may be visually distinguished by the observer 42.

[0057] Fig.10 Another exemplary arrangement is shown. Fig.10As shown, the inner surface 32 of the glass layer 24 can be textured to provide an overall rough appearance to the layer 24. A coating 74 (e.g., a thin film interference filter coating, a metal coating, and / or an ink coating) can be used to help prevent the user 42 from viewing the internal components. A layer 80 (e.g., a polymer film or a thin glass layer) can have an outer surface that is textured in the region 38 to enhance the rough appearance of the glass layer 24 in the region 38. In the region 40, the outer surface of the layer 80 can be smooth. The coating 78 can be selectively formed in the region 38 on the inner surface of the layer 80 to adjust the color, reflectivity, and / or other optical properties in the region 38 relative to the region 40. An optically clear adhesive 76 can be used to attach the layer 80 to the outer surface 30 of the layer 24.

[0058] exist Fig.11 and Fig.12 In the exemplary configuration of , a first texture is formed in region 38 and a second texture (e.g., a texture of a logo, text, or other pattern) or no texture is formed in region 40. A coating 82 (e.g., a thin film interference filter coating, a metal coating, and / or an ink coating) may be formed on the inner surface 32. Fig.11 In the example of FIG. 1 , outer surface 30 of glass layer 24 is textured (e.g., having a first texture in region 38 and a second, different texture or no texture in region 40 ). Fig.12 In the example of FIG. 4 , inner surface 32 of glass layer 24 is selectively textured in this manner.

[0059] Fig.13 24. It is shown how the inner surface 32 of the glass layer 24 may have a groove (e.g., a groove with an inclined sidewall, a vertical sidewall, or other sidewall profile). A protruding layer 88 (e.g., a glass or polymer layer having a thickness T of about 50-150 microns, at least 75 microns, less than 500 microns, etc.) may have a protrusion that is placed in the groove in the inner surface 32 and has a shape that matches the groove. Optional layers such as layer 90 (e.g., a thin film interference filter coating, a metal coating, and / or an ink coating, and / or an adhesive layer) may be interposed between layer 88 and layer 24.

[0060] exist Fig.14In the example of , the glass layer 24 has been formed by a mating first layer and a second layer such as an outer layer 24A and an inner layer 24B. The inner surface 32' of the outer layer 24A and / or the outer surface 30' of the inner layer 24B may have grooves, protrusions and / or other non-planar portions to create a visual contrast between the regions 38 and 40. For example, the inner surface 32' may have a groove 90, and the outer surface 30' may have a groove that overlaps completely or partially, such as a groove 92 (e.g., a mating groove). If desired, the inner surfaces of the grooves 90 and 92 may have corresponding coatings 94 and 96 (e.g., a thin film interference filter coating, a metal coating and / or an ink coating). The grooves 90 and 92 may be filled with air, liquid, polymer, glass inserts or inserts formed of other materials, and / or other materials. The outer layer 24A and the inner layer 24B may be coupled using an adhesive 98. In some configurations, the grooves 90 or the grooves 92 may be omitted. If desired, the glass layer 24 may also be formed only by the layer 24A instead of the layer 24B.

[0061] If desired, laser processing techniques may be used to form visible structures on glass layer 24. For example, a high-power laser beam may be focused into an interior portion of glass layer 24. This may produce laser-damaged regions embedded within layer 24, such as Fig.15 100. Laser processing to form these visible laser processed structures may occur in region 40 but not in region 38 (or vice versa) to provide regions 38 and 40 of glass layer 24 with a visually distinguishable appearance. An optional coating 102 (e.g., a thin film interference filter coating, a metal coating, and / or an ink coating) may be formed on inner surface 32 of layer 24.

[0062] like Fig.16 As shown, the inner surface 32 of the glass layer 24 can be coated with a polymer layer such as layer 106. Layer 106 can include particles such as particles 108. Particles 108 can have a different refractive index than the polymer binder that constitutes layer 106, and can have a diameter sufficient to cause reflection of light. Particles 108 can be, for example, glass particles having a diameter of 20-100 microns, at least 10 microns, at least 30 microns, less than 200 microns, etc., and can provide the glass layer 24 with a pearlescent appearance.

[0063] If necessary, Figures 4 to 16 One or more of the polymer layers coupled to glass layer 24 may be formed of glass instead of polymer, and / or one or more of the glass layers coupled to glass layer 24 may optionally be formed of a polymer coating or polymer film. Glass layer 24 may be replaced by a polymer layer or a layer of other material (sapphire or other crystalline material, ceramic, etc.). Figures 4 to 16Exemplary structures may be formed on glass layer 24, which forms a portion of a rear housing wall, a window structure for optical components, a display cover layer, a button member, a keyboard key, a trackpad surface, or any other suitable structure in device 10. Figures 4 to 16 The examples are illustrative only, and the coatings, glass layers, films, textures, and other structures of these examples may be used together if desired (e.g., by stacking layers of one configuration on top of another, laterally spacing structures from different configurations on a common glass layer, etc.).

[0064] According to one embodiment, an electronic device having opposite front and back sides and an interior is provided, comprising: a display on the front side; a first glass layer forming a housing wall on the back side, the first glass layer having an inner surface facing the interior and an opposite outer surface; a second glass layer, the second glass layer being thinner than the first glass layer and having an outer surface and an inner surface opposite to the outer surface facing the first glass layer; and an adhesive layer between the first glass layer and the second glass layer, the adhesive layer coupling the second glass layer to the first glass layer.

[0065] According to another embodiment, the second glass layer has a smooth region and has a textured region, the textured region having a greater surface roughness than the smooth region.

[0066] According to another embodiment, the textured region is formed on the outer surface of the second glass layer.

[0067] According to another embodiment, the textured region is formed on the inner surface of the second glass layer.

[0068] According to another embodiment, the electronic device includes a first thin film interference filter coating, which is on the second glass layer and overlaps the smooth area and does not overlap the textured area; and a second thin film interference filter coating, which is on the second glass layer and overlaps the smooth area and the textured area.

[0069] According to another embodiment, the electronic device includes a thin film interference filter coating on the inner surface of the first glass layer and overlapping the smooth area and not overlapping the textured area.

[0070] According to another embodiment, the second glass layer has a first region and a second region with different respective surface roughness values, and the electronic device includes a coating on the second glass layer overlapping the first region.

[0071] According to another embodiment, the first region is a smooth region, the second region is a textured region, and the coating comprises a thin film interference coating having a dielectric layer stack.

[0072] According to one embodiment, an electronic device having opposite front and back sides and an interior is provided, comprising: a display on the front side; a first glass layer forming a housing wall on the back side, the first glass layer having an inner surface facing the interior and an opposite outer surface; and a second glass layer, the second glass layer being thinner than the first glass layer, the second glass layer having an outer surface and an inner surface opposite to the outer surface facing the first glass layer, and the inner surface of the second glass layer having a smooth area and a textured area, the textured area having a greater surface roughness than the smooth area.

[0073] According to another embodiment, the electronic device includes a coating on the inner surface of the second glass layer.

[0074] According to another embodiment, the electronic device includes an adhesive layer interposed between the coating on the inner surface of the second glass layer and the outer surface of the first glass layer, the adhesive layer attaching the second glass layer to the first glass layer.

[0075] According to another embodiment, the coating comprises a thin film interference coating having a dielectric layer stack.

[0076] According to another embodiment, the second glass layer has a thickness of 20 micrometers to 250 micrometers.

[0077] According to one embodiment, an electronic device is provided, comprising: a display on the front side; a glass layer forming a housing wall on the back side, the glass layer having an inner surface facing inward and an opposite outer surface, and the glass layer having a surface including a smooth area and a textured area having a surface roughness greater than the smooth area; and a thin-film interference filter coating formed by a stack of dielectric layers on the inner surface of the glass layer.

[0078] According to another embodiment, the smooth area and the textured area are formed by respective smooth and textured surfaces on the outer surface.

[0079] According to another embodiment, the smooth area and the textured area are formed by respective smooth and textured surfaces on the inner surface.

[0080] According to one embodiment, an electronic device is provided, comprising: a display on the front side; a coupled first glass layer and a second glass layer, the coupled first glass layer and the second glass layer forming a housing wall on the back side, the first glass layer having a first area and a second area, the first area and the second area having different appearances and having a groove in the first area.

[0081] According to another embodiment, the electronic device includes a coating that overlaps the first region and does not overlap the second region.

[0082] According to another embodiment, the electronic device includes an adhesive layer interposed between the first glass layer and the second glass layer, the adhesive layer coupling the first glass layer and the second glass layer together.

[0083] According to another embodiment, the second glass layer has a groove that at least partially overlaps the groove of the first glass layer.

[0084] The foregoing is merely illustrative and various modifications may be made to the embodiments described. The foregoing embodiments may be implemented independently or in any combination.

Claims

1. An electronic device having opposite front and back sides and an interior, the electronic device comprising: a display, the display being on the front surface; a first glass layer forming a housing wall on the back surface, wherein the first glass layer has an inner surface facing the interior and an opposing outer surface; as well as A second glass layer, the second glass layer being thinner than the first glass layer, wherein the second glass layer has an outer surface and an opposing inner surface facing the outer surface of the first glass layer, and wherein the second glass layer has a first region and a second region having different appearances. 2 . The electronic device of claim 1 , wherein the first region is a laser damaged region embedded within the second glass layer, and wherein the second region is protected from laser damage.

3. The electronic device according to claim 1, further comprising: A polymer layer is coupled to the inner surface of the first glass layer, wherein the polymer layer has particles embedded in a polymer binder. 4 . The electronic device of claim 3 , wherein the particles have a first refractive index, and wherein the polymer binder has a second refractive index different from the first refractive index.

5. The electronic device according to claim 1, wherein: The first region is a smooth region, and wherein the second region is a textured region having a greater surface roughness than the first region.

6. The electronic device according to claim 5, wherein: The textured region is formed on the outer surface of the second glass layer.

7. The electronic device according to claim 5, wherein: The textured region is formed on the inner surface of the second glass layer.

8. The electronic device according to claim 1, further comprising: A thin film interference filter coating comprising a dielectric layer stack on the second glass layer.

9. The electronic device according to claim 8, wherein: The thin film interference filter coating overlaps the first region and the second region of the second glass layer.

10. The electronic device according to claim 8, wherein: The thin film interference filter coating overlaps the first region of the second glass layer and does not overlap the second region of the second glass layer.

11. An electronic device having opposite front and back sides and an interior, the electronic device comprising: a display, the display being on the front surface; a glass layer forming a housing wall on the back surface, wherein the glass layer has an inner surface facing the interior and an opposing outer surface, and wherein the glass layer has a smooth region and a textured region; an additional glass layer having an outer surface facing the inner surface of the glass layer and an opposing inner surface, wherein the glass layer is thinner than the additional glass layer; as well as A coating is provided on the inner surface of the glass layer.

12. The electronic device according to claim 11, wherein: The coating is a polymer coating comprising particles having a first refractive index embedded in a polymer binder having a second refractive index different from the first refractive index.

13. The electronic device according to claim 11, wherein: The coating is a thin film interference filter coating formed by a stack of dielectric layers.

14. The electronic device defined in claim 11 wherein the textured region is a laser damaged region embedded within the glass layer, and wherein the smooth region is immune to laser damage.

15. The electronic device according to claim 11, wherein: The smooth region and the textured region are formed on a surface of the glass layer.

16. An electronic device having opposite front and back sides and an interior, the electronic device comprising: a display, the display being on the front side; a layer forming a housing wall on the back surface, wherein the layer has an inner surface facing the interior and an opposing outer surface, and wherein the layer has a surface having smooth areas and textured areas; as well as An additional layer having an outer surface facing the inner surface of the layer and an opposing inner surface, wherein the layer is thinner than the additional layer.

17. The electronic device according to claim 16, wherein: The smooth region and the textured region are formed by respective smooth and textured surfaces on the outer surface of the layer.

18. The electronic device according to claim 16, wherein: The smooth region and the textured region are formed by respective smooth and textured surfaces on the inner surface of the layer.

19. The electronic device according to claim 16, wherein: Each of the layer and the additional layer is formed of a material selected from the group consisting of: glass, sapphire, ceramic and polymer.