A method for distinguishing rail surface damage leakage magnetic detection signals

By setting up multiple magnetic sensitive sensors on the surface of the rail, measuring and calculating the leakage magnetic field distribution, and using the correlation coefficient to judge the damage signal, the problems of lifting and misjudgment are solved, and the accuracy and safety of damage detection on the surface of the rail are improved. sex.

CN114965676BActive Publication Date: 2024-11-01JINLING INST OF TECH
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202210526418.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-05-16
Publication Date
2024-11-01
Estimated Expiration
2042-05-16

AI Technical Summary

Technical Problem

In the existing magnetic detection technology for surface damage leakage of rails, the error rate of removal and other factors leads to a high error rate, making it difficult to accurately determine the damage signal, affecting the detection rate and safety.

Method used

Multiple magnetic sensitive sensors are installed along the surface of the rail to measure the magnetic fields in the x and z directions, calculate the damage depth and width, calculate the leakage magnetic field distribution, and judge whether the sampling point is a damage signal through the correlation coefficient to reduce interference effects.

Benefits of technology

Effectively reduce the false alarm rate, improve the injury detection rate, enhance the accuracy of detection signals, and is suitable for surface damage detection of rails and other ferromagnetic materials.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114965676B_ABST
    Figure CN114965676B_ABST
Patent Text Reader

Abstract

The present invention discloses a method for distinguishing rail surface damage leakage magnetic detection signals, comprising the following steps: arranging a magnetic sensor under a magnetic yoke and detecting x , z Directional magnetic field, the sensor output is sampled. x Direction data, if a sampling point is the front and back M The maximum value among the sampling points is used to infer the depth and width of the damage based on the leakage magnetic field intensity at that point, and further calculate the damage at x , z The theoretical leakage magnetic field distribution in the direction, and then the calculated x , z Direction Theoretical Leakage Magnetic Field and Actual x , z The correlation coefficient of the measurement results of the direction is calculated. If x , z If the correlation coefficients of the directions are all greater than the threshold, the sampling point is considered to be a damage signal, otherwise the sampling point is considered to be interference. The present invention can effectively distinguish damage signals from interference, increase the detection rate of damage, reduce the false alarm rate, and is suitable for magnetic leakage detection of rail surface damage.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of nondestructive testing, relates to digital signal processing technology, and specifically relates to a method for distinguishing rail surface damage and magnetic leakage detection signals. Background Art

[0002] Rails are an important part of the rail transit system. When trains run on rails, they will constantly cause various forces such as squeezing and bending on the rails. In addition, the rails will suffer various damages such as fatigue cracks. Early damage often appears on the top surface of the rail head. If it is not handled in time, it will further expand and develop into a larger damage, and even cause the rails to break, seriously affecting the driving safety of the train.

[0003] The magnetic flux leakage nondestructive testing method means that when the ferromagnetic material is magnetized, if there is damage on the surface, due to the distortion of the magnetic flux in the magnetic circuit, the magnetic induction line changes, causing part of the magnetic flux to leak out of the material surface, forming a leakage magnetic field. By detecting the magnetic field change on the surface of the test piece with a magnetic sensor, it can be determined whether there is damage. Its basic principle is as follows: Figure 1 As shown in the figure. Magnetic flux leakage detection has high sensitivity, fast speed, low requirements on the surface cleanliness of the workpiece, low cost, and simple operation. It is widely used in non-destructive testing of surface damage of ferromagnetic materials such as rails and steel pipes. Due to the long inspection distance of rails, it is difficult to manually judge whether there is damage through the detection data, and an intelligent judgment method is needed.

[0004] The vertical distance between the magnetic sensor and the workpiece being measured is called lift-off. When the probe is patrolling the surface of the workpiece for inspection, the lift-off will change due to factors such as vibration. Due to the different distribution of the damage leakage magnetic field under different lift-offs, the lift-off change will cause the output of the magnetic sensor to change, which is called lift-off interference. Since the amplitude of lift-off interference is similar to that of smaller damage, the spectrum often overlaps with the damage signal, which is difficult to filter out effectively and easily causes misjudgment. Factors such as inspection speed, rail residual magnetism, alignment between the probe and the rail, and random interference will also affect the detection signal, which further increases the difficulty of distinguishing the leakage magnetic detection signal of rail surface damage. In short, in order to eliminate the influence of various interferences in leakage magnetic detection, improve the detection rate of rail surface damage, and reduce the false alarm rate, a suitable damage discrimination method is needed. Summary of the invention

[0005] Purpose of the invention: In order to overcome the deficiencies in the prior art, a method for distinguishing magnetic flux leakage detection signals of rail surface damage is provided, which can effectively overcome various interferences during the inspection process, accurately determine whether there is damage, and is suitable for magnetic flux leakage detection of rail damage.

[0006] Technical solution: To achieve the above purpose, the present invention provides a method for distinguishing rail surface damage magnetic leakage detection signals, comprising the following steps:

[0007] S1: Several magnetic sensors are arranged along the lower edge of the magnetic yoke. Each magnetic sensor measures the magnetic field in the x and z directions simultaneously. The measurement results of each magnetic sensor in the x and z directions are sampled respectively. 1 to N sampling points are obtained in each direction, with a total of N sampling points.

[0008] S2: For the sampling data of a magnetic sensor in the x direction, process them one by one starting from the first sampling point. If the value X(i) of the i-th sampling point is the maximum value among the iM-th to i+M-th sampling points (if iM<1, then the 1st to i+M-th sampling points are taken; if i+M>N, then the iM-th to N-th sampling points are taken), then enter S3; otherwise, continue to process the next sampling point. 2a min is the minimum damage width required to be detected, k is the sampling speed, and v is the inspection speed.

[0009] S3: Calculate the depth and width of the damage based on X(i), that is, solve the following equation to obtain a, with a as the depth of the damage and 2a as the width of the damage. If a positive number solution cannot be obtained, set a = 0.001 meter.

[0010]

[0011] z0 is the lift-off of the magnetic sensor, that is, the vertical distance from the magnetic sensor to the rail surface. ms is the surface magnetic charge density of the damaged side, which can be calculated by the following formula:

[0012]

[0013] Where μ is the magnetic permeability of the rail, H α is the strength of the external magnetic field.

[0014] S4: Based on the damage depth a and width 2a calculated in S3, calculate the leakage magnetic field distribution H of the damage in the x and z directions x (j) and H z (j), j = -20a min ,

[0015]

[0016]

[0017] S5: Compare the actual x-direction sampling results from the iMth to the i+Mth sampling points with the x-direction leakage magnetic field H calculated in S4 x (j) Calculate the correlation coefficient by comparing the actual z-direction sampling results from the iMth to the i+Mth sampling points with the z-direction leakage magnetic field H calculated in S4. z(j) Calculate the correlation coefficient. If iM < ​​1, then take the 1st to i+Mth sampling points to calculate the correlation coefficient; if i+M > N, then take the iMth to Nth sampling points to calculate the correlation coefficient. If the correlation coefficients in the x and z directions are both greater than the threshold, the sampling point is considered to be a damaged signal; otherwise, the sampling point is considered to be interference.

[0018] Beneficial effects: The scheme of the present invention can be used alone or in combination with various existing filtering methods. Compared with the prior art, the present invention effectively reduces the influence of various interferences on damage identification during magnetic flux leakage detection, improves the detection rate of damage, and reduces the false alarm rate. It is suitable for the detection of surface damage of ferromagnetic materials such as rails and steel pipes. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] Figure 1 This is a schematic diagram of the magnetic flux leakage detection principle;

[0020] Figure 2 It is a schematic diagram of the flow chart of the identification method of the present invention;

[0021] Figure 3 This is a schematic diagram of damage size and coordinates;

[0022] Figure 4 is the magnetic field distribution diagram of the damage in the x and z directions (the damage center is at the horizontal axis 0);

[0023] Figure 5 Schematic diagram of the distribution of leakage magnetic field of damage of different sizes (the damage center is at the position of 15 on the horizontal axis);

[0024] Figure 5 (a) Leakage magnetic field in the x direction at different damage depths; Figure 5 (b) Leakage magnetic field in z direction at different damage depths; Figure 5 (c) Leakage magnetic field in the x direction of damage with different widths; Figure 5 (d) Leakage magnetic field in the z direction for damages of different widths. DETAILED DESCRIPTION

[0025] The present invention is further explained below in conjunction with the accompanying drawings and specific embodiments. It should be understood that these embodiments are only used to illustrate the present invention and are not used to limit the scope of the present invention. After reading the present invention, various equivalent forms of modifications to the present invention by those skilled in the art all fall within the scope defined by the claims attached to this application.

[0026] The present invention provides a method for distinguishing rail surface damage leakage magnetic field detection signals, the flow chart of which is as follows: Figure 2 As shown, the following steps are included:

[0027] S1: Several magnetic sensors are arranged along the lower edge of the magnetic yoke. Each magnetic sensor measures the magnetic field in the x and z directions simultaneously. The measurement results of each magnetic sensor in the x and z directions are sampled respectively. 1 to N sampling points are obtained in each direction, with a total of N sampling points.

[0028] S2: For the sampling data of a magnetic sensor in the x direction, process them one by one starting from the first sampling point. If the value X(i) of the i-th sampling point is the maximum value among the iM-th to i+M-th sampling points (if iM<1, then the 1st to i+M-th sampling points are taken; if i+M>N, then the iM-th to N-th sampling points are taken), then enter S3; otherwise, continue to process the next sampling point. 2a min is the minimum damage width required to be detected, k is the sampling speed, and v is the inspection speed.

[0029] S3: Calculate the depth and width of the damage based on X(i), that is, solve the following equation to obtain a, with a as the depth of the damage and 2a as the width of the damage. If a positive number solution cannot be obtained, set a = 0.001 meter.

[0030]

[0031] z0 is the lift-off of the magnetic sensor, that is, the vertical distance from the magnetic sensor to the rail surface. ms is the surface magnetic charge density of the damaged side, which can be calculated by the following formula:

[0032]

[0033] Where μ is the magnetic permeability of the rail, H α is the strength of the external magnetic field.

[0034] S4: Based on the damage depth a and width 2a calculated in S3, calculate the leakage magnetic field distribution H of the damage in the x and z directions x (j) and H z (j), j = -20a min ,

[0035]

[0036]

[0037] S5: Compare the actual x-direction sampling results from the iMth to the i+Mth sampling points with the x-direction leakage magnetic field H calculated in S4 x (j) Calculate the correlation coefficient by comparing the actual z-direction sampling results from the iMth to the i+Mth sampling points with the z-direction leakage magnetic field H calculated in S4. z(j) Calculate the correlation coefficient. If iM < ​​1, then take the 1st to i+Mth sampling points to calculate the correlation coefficient; if i+M > N, then take the iMth to Nth sampling points to calculate the correlation coefficient. If the correlation coefficients in the x and z directions are both greater than the threshold, the sampling point is considered to be a damaged signal; otherwise, the sampling point is considered to be interference.

[0038] Based on the above scheme, the present invention is analyzed as follows in combination with the existing method:

[0039] The basic idea of ​​the present invention is to first find the sampling point of suspected damage according to the amplitude of the leakage magnetic signal in the x direction; then estimate the depth and width of the damage according to the amplitude of this point; then calculate the leakage magnetic field of the damage in the theoretical x and z directions according to the estimated depth and width; finally, calculate the correlation coefficient between the calculated theoretical leakage magnetic field in the x and z directions and the actual measurement results in the x and z directions respectively. If the correlation coefficients in the x and z directions are both greater than the threshold, the sampling point is considered to be a damage signal, otherwise the sampling point is considered to be interference.

[0040] like Figure 3 As shown in the figure, if the damage width is 2a and the depth is b, the leakage magnetic field intensity at a point P(x, z) above the damage is H(x, z), and its x-direction component is H x (x, z), the z-direction component is H z (x, z), can be obtained by equations (1) and (2) respectively. The change trend of damage is as follows: Figure 4 shown.

[0041]

[0042]

[0043] σ ms is the surface magnetic charge density of the damaged side, which can be calculated by the following formula:

[0044]

[0045] Where μ is the magnetic permeability of the material and H is the strength of the applied magnetic field.

[0046] from Figure 4 It can be seen that the positive peak value in the x direction appears just above the damage, that is, at x=0. Therefore, if the value X(i) of the i-th sampling point is the maximum value among the iM-th to i+M-th sampling points (if iM<1, then the 1st to i+M-th sampling points are taken; if i+M>N, then the iM-th to N-th sampling points are taken), then it is likely to be a damage signal.

[0047] from Figure 4It can also be seen that the leakage magnetic field of the damage has a certain distribution range, which is generally more than 20 times the width of the damage. However, the farther away from the damage center, the smaller the leakage magnetic field is, and the more easily it is disturbed by various factors, which is not conducive to the judgment of the damage. The present invention takes the damage center as the origin and takes [-20a min , 20a min ] to process the leakage magnetic field within 2a min is the minimum damage width required to be detected, k is the sampling speed, and v is the inspection speed.

[0048] from Figure 5 It can be seen that for damages of different depths or widths, although their x- and z-direction signal peaks are different, the leakage magnetic field variation trends are basically the same. Therefore, when calculating the correlation coefficient between the theoretical leakage magnetic field and the actual measurement result, even if the calculated results of the damage width 2a and the depth b have large errors with the actual values, it will not significantly affect the calculated results of the correlation coefficient. Considering that the rail inspection distance is long and the amount of data is large, in order to simplify the calculation, the present invention uses a=b for calculation, that is, (0, X(i)) and a=b are substituted into formula (1) to obtain formula (3). The equation is solved to obtain a, which is used as the depth a and width 2a of the damage. If a positive number solution cannot be obtained, a=0.001 meter is set.

[0049]

[0050] Substitute the calculated damage depth a and width 2a into equations (1) and (2) to calculate the leakage magnetic field distribution H of the damage in the x and z directions. x (j) and H z (j), j = -20a min ,

[0051]

[0052]

[0053] Compare the actual x-direction sampling results from the iMth to the i+Mth sampling points with the calculated x-direction leakage magnetic field H x (j) Calculate the correlation coefficient by comparing the actual z-direction sampling results from the iMth to the i+Mth sampling points with the calculated z-direction leakage magnetic field H z (j) Calculate the correlation coefficient. If iM < ​​1, then take the 1st to i+Mth sampling points to calculate the correlation coefficient; if i+M > N, then take the iMth to Nth sampling points to calculate the correlation coefficient. If the correlation coefficients in the x and z directions are both greater than the threshold, the sampling point is considered to be a damaged signal; otherwise, the sampling point is considered to be interference.

[0054] Based on the above analysis, this embodiment describes the above filtering method in detail and provides a method for distinguishing rail surface damage magnetic flux leakage detection signals, which includes the following steps:

[0055] Step 1: Set up several magnetic sensors under the magnetic yoke. Each magnetic sensor measures the magnetic field in the x and z directions at the same time. Sample the measurement results of each magnetic sensor in the x and z directions respectively. Obtain 1 to N sampling points in each direction, with a total of N sampling points. N is determined according to the actual sampling situation.

[0056] Step 2: The minimum damage width required to be detected is 2mm, that is, a min =0.001m, sampling speed k is 10000, inspection speed v is 2m / s, then For the sampling data of a magnetic sensor in the x direction, process them one by one starting from the first sampling point. If the value X(i) of the i-th sampling point is the maximum value among the i-100th to i+100th sampling points (if i-100 < 1, then take the 1st to i+100th sampling points; if i+100 > N, then take the i-100th to Nth sampling points), then go to step 3; otherwise, continue to process the next sampling point.

[0057] Step 3: Solve the following equation to obtain a, with a as the depth of the damage and 2a as the width of the damage. If a positive solution cannot be obtained, set a = 0.001 meters.

[0058]

[0059] The magnetic sensor lift-off z0 is 0.001m, and the surface magnetic charge density σ on the damaged side ms Calculated by the following formula:

[0060]

[0061] Where the magnetic permeability μ of the rail is 1000, and the applied magnetic field strength H α It is 8000A / m.

[0062] Step 4: Based on the damage depth a and width 2a calculated in step 3, calculate the leakage magnetic field distribution H of the damage in the x and z directions x (j) and H z (j), j=-0.0200, -0.0198, -0.0196,…, -0.0002, 0.0000, 0.0002,…, 0.0196, 0.0198, 0.0200m:

[0063]

[0064]

[0065] Step 5: Compare the actual x-direction sampling results from the i-100th to the i+100th sampling points with the x-direction leakage magnetic field H calculated in step 4. x (j) Calculate the Pearson correlation coefficient by comparing the actual z-direction sampling results from the i-100th to the i+100th sampling points with the z-direction leakage magnetic field H calculated in step 4. z (j) Calculate the Pearson correlation coefficient. If i-100 < 1, then take the 1st to i+100th sampling points to calculate the correlation coefficient; if i+100 > N, then take the i-100th to Nth sampling points to calculate the correlation coefficient. If the correlation coefficients in the x and z directions are both greater than the threshold value of 0.85, then the sampling point is considered to be a damaged signal, otherwise the sampling point is considered to be interference. The threshold can be selected according to actual needs. The larger the threshold, the higher the missed detection rate and the lower the false alarm rate; the smaller the threshold, the lower the missed detection rate and the higher the false alarm rate. Generally, it is set to about 0.85.

Claims

1. A method for distinguishing rail surface damage leakage magnetic detection signals, characterized in that: The steps include: S1: Several magnetic sensors are set at the lower edge of the magnetic yoke, and each magnetic sensor measures simultaneously x and z Direction of magnetic field, for each magnetic sensor x and z The direction measurement results are sampled separately, and each direction obtains 1~ N ,common N sampling points; S2: For a magnetic sensor x The sampling data in the direction are processed one by one starting from the first sampling point. i The value of the sampling point X ( i ) is the i - M To i + M If the maximum value among the sampling points is found, then the process goes to S3; otherwise, the process continues to the next sampling point. , 2 a min is the minimum damage width required to be detected, k is the sampling speed, v is the inspection speed; S3: According to X ( i ) to estimate the depth and width of the damage, that is, to solve the following equation, we can get a ,by a As the depth of the damage, 2 a As the width of the damage, if a positive solution cannot be obtained, let a = 0.001 m, ; z 0 is the lift-off of the magnetic sensor, that is, the vertical distance from the magnetic sensor to the rail surface. σ ms is the surface magnetic charge density of the damaged side, which can be calculated by the following formula: ; In the formula, μ is the magnetic permeability of the rail, H α is the strength of the applied magnetic field; S4: Damage depth calculated in S3 a and width 2 a , calculate the damage in x , z The leakage magnetic field distribution in the direction H x ( j )and H z ( j ); S5: The actual x The sampling results of the direction i - M To i + M The sampling points are compared with the ones calculated in S4 x Direction of leakage magnetic field H x ( j ) to find the correlation coefficient, and convert the actual z The sampling results of the direction i - M To i + M The sampling points are compared with the ones calculated in S4 z Direction of leakage magnetic field H z ( j )Calculate the correlation coefficient.

2. A rail surface damage leakage magnetic detection signal discrimination method according to claim 1, characterized in that: In step S2, if i - M <1, then take the first to the i + M sampling points; like i + M > N , then take the i - M To N sampling points.

3. A rail surface damage leakage magnetic detection signal discrimination method according to claim 1, characterized in that: In step S5, if i - M <1, then take the first to the i + M The correlation coefficient is calculated for each sampling point. i + M > N , then take the i - M To N The correlation coefficient is calculated for each sampling point; if x , z If the correlation coefficients of the directions are all greater than the threshold, the sampling point is considered to be a damaged signal, otherwise it is considered to be interference.

4. A rail surface damage leakage magnetic detection signal discrimination method according to claim 3, characterized in that: The threshold is 0.85.

Citation Information

Patent Citations

  • Ferromagnetic material large-range damage low-frequency electromagnetic detection method based on wideband excitation

    CN110196276A

  • Filtering method for inhibiting lift-off interference in magnetic flux leakage detection of steel rail

    CN113671018A

  • Flaw detection device and flaw detection method

    JP2017150904A

  • Wide-band excitation-based low-frequency electromagnetic testing method for wide-range damage of ferromagnetic material

    WO2020259070A1