Crop processor and crop processor manufacturing method

By using asymmetric tooth configuration and laser cladding technology on the crushing roller of the feed harvester, a wear-resistant layer with differentiated hardness is formed, which solves the problem of serious wear of the crushing roller and achieves longer service life and lower maintenance. cost.

CN115151129BActive Publication Date: 2024-10-29CNH IND MASCH (HARBIN) CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202180013943.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-01-05
Publication Date
2024-10-29
Estimated Expiration
2041-01-05

AI Technical Summary

Technical Problem

The crushing rollers of existing feed harvester crop processors are severely worn during the process of breaking grains, resulting in increased maintenance costs. Existing hardening treatment methods such as induction hardening and chrome plating technology have problems with material deformation and the use of toxic substances.

Method used

The asymmetric tooth configuration of the first crushing roller and the second crushing roller is used, and a wear-resistant layer with differentiated hardness is formed on the leading and trailing edges of the teeth through laser cladding and air hardening technology, and the areas with higher hardness are used to wear preferentially. Extend the life of the roller and deposit a tungsten carbide wear-resistant layer on the tooth surface.

Benefits of technology

It effectively extends the service life of the crushing roller, reduces maintenance costs, avoids problems with material deformation and the use of toxic substances, and at the same time improves the wear resistance of the crushing roller.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115151129B_ABST
    Figure CN115151129B_ABST
Patent Text Reader

Abstract

A crop processor for breaking grains in a forage harvester, the crop processor comprising: a shell having an inlet and an outlet; and a first crushing roller and a second crushing roller installed in the shell, the first crushing roller and the second crushing roller being arranged in parallel to define an opening between the first crushing roller and the second crushing roller, the first crushing roller and the second crushing roller being configured to rotate in opposite directions of rotation to each other during use to convey a harvested crop flow received from the inlet toward the outlet via the opening, wherein the first crushing roller is configured to rotate at a faster speed than the second crushing roller; wherein the first crushing roller and the second crushing roller each include a plurality of teeth arranged on a circumferential surface of the crushing roller, each of the plurality of teeth including a leading edge facing a rotation direction of the corresponding crushing roller; wherein the leading edge of the teeth of the second crushing roller includes a hard region having a greater hardness than the leading edge of the teeth of the first crushing roller.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of forage harvesters, and more particularly to a crop processor for rupturing crop grain in such harvesters. The present invention also relates to a method for manufacturing a crop processor for a forage harvester. Background Art

[0002] A forage harvester is used to harvest crops from a field, then pulverize the harvested crops and discharge them through a nozzle into a trailer traveling next to the forage harvester. The forage harvester is usually equipped with a crop processor that breaks or pulverizes the grains in the harvested crops. Usually, the crop processor includes a pair of crop pulverizing rollers, each of which has a plurality of teeth on its circumference; the teeth have a height in the radial direction and extend in the axial direction of the roller.

[0003] Both crop crushing rollers are mounted in a housing that includes an inlet and an outlet. The crushing rollers are arranged so that there is a small opening between their peripheries. During use, the crop crushing rollers rotate in opposite circumferential directions to each other (i.e., one roller rotates in a clockwise direction and the other roller rotates in a counterclockwise direction) so as to convey the harvested crop fed to the rollers via the inlet through the small opening between the rollers, thereby breaking the grains by the teeth. The harvested crop stream is then discharged from the housing via the outlet.

[0004] Irregular openings between the rollers can also result from wear caused by the kernel breaking process itself, for example when material flow is uneven along the length of the roller. Wear on the teeth inhibits the crop processor's ability to consistently break up the crop kernels. As a result, the comminution rollers must be replaced more regularly, increasing the maintenance costs of the forage harvester.

[0005] In order to enable the teeth to withstand the wear caused by the cracking of the seeds, it is known to configure the teeth of the milling roller so that the leading and trailing edges of the teeth show a uniform hardness. For example, the milling roller is subjected to an induction hardening treatment, which involves inducing an alternating magnetic field on the surface of the milling roller to locally heat the peripheral surface of the roller to a temperature above the transformation range of the constituent alloys. The local heating causes the peripheral surface to harden, thereby producing the same hardening effect on the leading and trailing edges of the teeth.

[0006] To further improve the wear resistance of the milling rollers, a thin hard chrome layer can be plated on the surface of the teeth after induction hardening. This chrome plating technology usually requires the use of hexavalent chromium, which is a toxic substance and its use is increasingly restricted by government regulations.

[0007] The disadvantage of induction hardening is that it tends to concentrate the energy in the tooth tip area, which can cause local melting of the tooth tip area. Hardening can also cause deformation of the roller due to metallurgical phase changes of the material. In addition, the disadvantage of electrochromization is that it causes indiscriminate hardening of the leading and trailing edges of the teeth, which can lead to irregular wear of the crushing roller during operation of the crop processor. In particular, uniform hardening can cause the teeth of the crushing roller to become gradually but irreversibly blunted during operation of the crop processor.

[0008] It is desirable to improve the wear resistance of chopping rollers used in crop processors for forage harvesters. Summary of the invention

[0009] According to a first aspect of the present invention, a crop processor is provided for breaking grains in a forage harvester, the crop processor comprising: a shell having an inlet and an outlet; and a first crushing roller and a second crushing roller installed in the shell, the first crushing roller and the second crushing roller being arranged in parallel to define an opening between the first crushing roller and the second crushing roller, the first crushing roller and the second crushing roller being configured to rotate in opposite directions of rotation to each other during use to convey a harvested crop flow received from the inlet toward the outlet via the opening, wherein the first crushing roller is configured to rotate at a faster speed than the second crushing roller; wherein the first crushing roller and the second crushing roller each include a plurality of teeth arranged on a circumferential surface of the crushing roller, each of the plurality of teeth including a leading edge facing a rotation direction of the corresponding crushing roller; wherein the leading edge of the teeth of the second crushing roller includes a hard region having a greater hardness than the leading edge of the teeth of the first crushing roller.

[0010] During operation of the crop processor, the crop material is squeezed between the leading edge of the faster moving first shredding roller and the trailing edge of the slower moving second shredding roller. Advantageously, the leading edge of the teeth of the first shredding roller is worn relative to the trailing edge, which causes the teeth of the first shredding roller to be sharpened by the crop material, thereby extending the life of the crop processor.

[0011] The teeth of the first comminuting roller may include a trailing edge facing away from the rotation direction of the first comminuting roller, the trailing edge including a hard region with a greater hardness than the leading edge of the teeth of the first comminuting roller.

[0012] The hardness of the hard area of ​​the leading edge of the teeth of the second pulverizing roller may be greater than the hardness of the trailing edge of the teeth of the second pulverizing roller arranged away from the rotation direction of the second pulverizing roller. Similar to the first pulverizing roller, the trailing edge of the second pulverizing roller will wear faster than the hard area of ​​the leading edge, which will cause the teeth of the second pulverizing roller to sharpen during operation of the crop processor.

[0013] The hard area of ​​the trailing edge of the teeth of the first pulverizing roller can be configured to be harder than the trailing edge of the teeth of the second pulverizing roller. The hard area of ​​the leading edge of the teeth of the second pulverizing roller can be configured to be harder than the leading edge of the teeth of the first pulverizing roller.

[0014] The plurality of teeth of the first comminuting roller may include a substantially flat top edge. The substantially flat top edge may include a hard region having a greater hardness than a leading edge of the teeth of the first comminuting roller.

[0015] The plurality of teeth of the second comminuting roller may include a substantially flat top edge. The substantially flat top edge may include a hard region having a greater hardness than a trailing edge of the teeth of the second comminuting roller.

[0016] The hard region may comprise a wear resistant layer deposited by laser cladding.The wear resistant layer may comprise tungsten carbide.

[0017] The plurality of teeth may include an air hardened surface region.The plurality of teeth may be made of steel or any suitable material having sufficient hardenability to enable the tooth surface to be air hardened.

[0018] At least one edge of the tooth may include a laser hardened surface region.The laser hardened surface region may be formed on the edge of the tooth that is not clad with wear resistant material.

[0019] The plurality of teeth may have an asymmetric profile in an axial section of the pulverizing roller. The axial section is defined as a cross section obtained by cutting the pulverizing roller along a plane intersecting the longitudinal axis of the roller at right angles. The axial plane may be defined as a cross section of the roller.

[0020] According to a second aspect of the present invention, there is provided a forage harvester comprising a crop processor according to any of the preceding paragraphs.

[0021] According to a third aspect of the present invention, there is provided a method for manufacturing a crop processor for cracking grains in a forage harvester, the method comprising: manufacturing a first crushing roller and a second crushing roller; and assembling the first crushing roller and the second crushing roller into a shell having an inlet and an outlet, the first crushing roller and the second crushing roller being arranged in parallel to define an opening between the first crushing roller and the second crushing roller, the first crushing roller and the second crushing roller being configured to rotate in opposite directions to each other during use to convey a harvested crop flow received from the inlet toward the outlet via the opening, wherein the first crushing roller is configured to rotate at a faster speed than the second crushing roller; wherein manufacturing the first crop crushing roller and the second crop crushing roller comprises: providing a pair of generally cylindrical rollers; machining a plurality of teeth in the generally cylindrical rollers, each of the plurality of teeth comprising a leading edge arranged to face the direction of rotation of the first crop crushing roller and the second crop crushing roller during use; and forming a hard area on the leading edge of the tooth of the second crushing roller, the hardness of the hard area being greater than the hardness of the leading edge of the tooth of the first crushing roller.

[0022] The method may include forming a hard area on a trailing edge of the teeth of the first pulverizing roller arranged away from a rotation direction of the first pulverizing roller, the hard area having a harder hardness than a leading edge of the teeth of the first pulverizing roller.

[0023] The method may include forming a hard area on a leading edge of the teeth of the second pulverizing roller having a harder hardness than a trailing edge of the teeth of the second pulverizing roller, the trailing edge being arranged away from a rotational direction of the second pulverizing roller.

[0024] The method may include laser cladding a wear-resistant layer on a leading edge or a trailing edge of teeth of the first pulverizing roller or the second pulverizing roller.

[0025] The method may further include air hardening at least one edge of the teeth of the first and second pulverizing rollers. The at least one edge of the teeth may be air hardened before or after laser cladding the wear resistant layer. For example, manufacturing the first and second pulverizing rollers may include air hardening the cylindrical rollers before laser cladding the wear resistant layer. Air hardening may be achieved after the wear resistant layer is deposited due to the heat input of the laser cladding process.

[0026] Manufacturing the first and second pulverizing rollers may include laser hardening the edges of the teeth that are not clad with the wear-resistant layer. Laser hardening may include heating the edges of the teeth using a laser source and then cooling the heat-treated teeth in air to cause air hardening of the edges of the teeth. Laser hardening of the unclad edges of the teeth may be performed before or after the teeth are laser-clad with the wear-resistant layer.

[0027] Within the scope of the present application, it is explicitly intended that the various aspects, embodiments, examples and alternatives, especially the various features, listed in the preceding paragraphs, the claims and / or the following description and drawings may be taken independently or in any combination. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] One or more embodiments of the present invention will now be described, by way of example only, with reference to the accompanying drawings, in which:

[0029] Figure 1 is a side view of a forage harvester according to the present invention;

[0030] Figure 2 yes Figure 1 Schematic diagram of the crop flow path of a forage harvester;

[0031] Figure 3 is a cross-sectional view of a crop processor according to the present invention;

[0032] Figure 4 yes Figure 3 A perspective view of a pair of crop crushing rollers of a crop processor in an assembled state;

[0033] Figure 5 yes Figure 4 A plan view of a pair of crop pulverizing rollers showing an opening between the crop pulverizing rollers;

[0034] Figure 6 yes Figure 3a cross-sectional view of a plurality of teeth of a first crop pulverizing roller;

[0035] Figure 7a and Figure 7b yes Figure 4 a cross-sectional view of a crop chopping roller showing wear on a plurality of teeth of the crop chopping roller during use of a crop processor;

[0036] Figure 8 is a schematic diagram of a method for depositing a wear-resistant layer on the plurality of teeth of a crop pulverizing roller;

[0037] Fig. 9 is a flow chart showing method steps suitable for use in a method of manufacturing a crop processor according to the present invention; and

[0038] Fig.10 and Fig.11 is a perspective view of a plurality of teeth of a comminution roller, showing the tooth profiles before and after the grinding process, respectively. DETAILED DESCRIPTION

[0039] In the following detailed description, reference is made to the accompanying drawings which constitute an integral part of the specification and which illustrate specific embodiments of the invention. These embodiments are described in sufficient detail to enable one skilled in the art to make and use them. Figures 1 to 9 Various aspects of the invention are described.

[0040] Figure 1 A harvesting vehicle 100 is shown in the form of a forage harvester 100. The forage harvester 100 is configured to harvest crops C such as corn and grass, which may be used, for example, for animal feed production.

[0041] To this end, the front end 102 of the forage harvester 100 includes a header 104, a crop processor 10, and a nozzle 106. The header 104 is configured to cut and collect crops C from the field as the forage harvester 100 moves forward. Figure 2 As shown, a set of feed rollers 108 are arranged to pull the cut crop into a crop flow path 110. In the crop flow path 110, the crop is processed and then directed into the spray tube 106. The spray tube 106 discharges the crop material from the forage harvester 100 into a trailer (not shown) adjacent to or behind the forage harvester 100.

[0042] For example, to harvest corn, the crop flow path 110 includes a chopper 112, a crop processor 10, and a blower 114, with the crop processor 10 being arranged between the chopper 112 and the accelerator 114. The chopper 112 cuts the crops pulled into the crop flow path 110 into small pieces. The crop processor 10 then grinds and presses the chopped crops (including corn kernels) in order to obtain all available nutrients therefrom. To this end, the crop processor 10 is composed of two toothed rollers with a very small gap between the two toothed rollers. The accelerator 114 then accelerates the (mostly) processed crops and pushes them into the nozzle 106 for discharge. The feed roller 108, the chopper 112, the crop processor 10, the accelerator 114, and the nozzle 106 are as shown in FIG. Figure 2 shown.

[0043] Figure 3 A crop processor 10 according to the present invention is shown. The crop processor 10 is arranged to be mounted in a forage harvester, which is well known in the art. During use, harvested crops are fed through the crop processor 10, where they are broken apart and then discharged from the harvester via a spray pipe.

[0044] The crop processor 10 includes a housing 12 having an inlet 14 and an outlet 16 and a pair of crop crushing rollers 18 disposed in a path (indicated by arrows 20) between the inlet 14 and the outlet 16. Each crushing roller 18 has a plurality of teeth 22 disposed along the circumference of the crushing roller 18. Figure 4 As shown, Figure 4 Shown is a perspective view of the crop crushing roller 18 detached from the housing 12, wherein the plurality of teeth 22 extend axially along the length of the crushing roller. In this way, the plurality of teeth 22 are arranged to cover at least a portion of the circumferential surface of each crushing roller 18.

[0045] The crop crushing rollers 18 are mounted parallel to one another in the housing 12 of the crop processor 10. As such, the crop crushing rollers 18 are arranged such that their respective longitudinal axes are generally aligned with one another. The crop crushing rollers 18 are spaced apart so as to define an opening between the rollers 18. The opening 30 between the crop crushing rollers 18 includes a depth or spacing (S), such as Figure 5 As shown, Figure 5 A plan view of the crop crushing roller 18 is shown disengaged from the housing 12. Because the crushing rollers 18 are aligned parallel within the housing 12, the openings 30 have a generally equal depth along the length of the rollers 18.

[0046] The crop crushing roller 18 used in the crop processor 10 according to the present invention has a diameter between 200 mm and 450 mm and has a plurality of teeth along its circumference, the number of which is 90 to 300. The pair of crop crushing rollers 18 includes a first crushing roller 24 and a second crushing roller 26. The first crushing roller 24 is arranged to rotate in a counterclockwise direction, while the second crushing roller 26 is arranged to rotate in a clockwise direction (e.g., Figure 3 , Figure 4 , Figure 6 , Figure 7a and Figure 7b 28 in FIG.

[0047] During operation of the crop processor 10 , the harvested crop flow entering the crop processor 10 through the inlet 14 is guided or conveyed by the plurality of teeth 22 , is forced to flow through the openings 30 between the cylindrical peripheries of the rollers 18 , further flows toward the outlet 16 , and then is discharged from the crop processor 10 through the outlet 16 .

[0048] The plurality of teeth 22 on each comminuting roller 24, 26 have a generally triangular profile, such as Figure 6 The plurality of teeth 22 have an asymmetrical profile when viewed in an axial section of the comminuting rollers 24, 26. The axial section is defined as a cross section obtained by cutting the comminuting rollers 24, 26 along a plane intersecting the longitudinal axis of the rollers at right angles.

[0049] Each tooth has a height (H) measured in a generally radial direction of the roller on which the teeth are arranged. Each of the plurality of teeth 22 also includes a length (L) measured in an axial direction of the pulverizing roller 18, such as Figure 4 According to the arrangement currently described, the length (L) of the plurality of teeth 22 is equal to the length of the comminuting roller 18 on which the teeth are arranged. Each tooth also includes a width C measured in the generally circumferential direction of the respective roller.

[0050] As the comminuting rollers 24, 26 rotate, the teeth 22 are functionally defined to include leading edges 32, 42 and trailing edges 34, 44, such as Figure 6 , Figure 7a and Figure 7b The leading edge 32, 42 of each tooth is defined as the edge facing or arranged to face the direction of movement of the pulverizing rollers 24, 26 (as shown by arrow 28). The trailing edge 34, 44 of each tooth 22 is defined as the tooth edge facing in the opposite direction opposite to the direction of rotation of the crop pulverizing roller on which the teeth are arranged (i.e., arranged to face in the opposite direction opposite to the corresponding leading edge 32, 42).

[0051] Each of the plurality of teeth 22 of the first pulverizing roller 24 further includes a substantially flat top edge 36. Thus, the top region 38 of each tooth is not point-shaped, but has a flat outer or peripheral surface. Each flat top edge 36 includes a width (W) measured in the circumferential direction of the respective pulverizing roller on which the teeth are formed, such as Figure 6 As shown. Figure 7a As shown, the teeth 22 of the second comminuting roller 26 are also configured with a flat top edge 46 having the same dimensions as the teeth of the first comminuting roller 24 .

[0052] The asymmetric profile or shape of the teeth 22 is arranged so that each tooth can be described as including a "steep slope" side and a "shallow slope" side. For example, each tooth 22 of the first comminuting roller 24 has a first side (also referred to as a steep slope side) including a steep slope and a second side (also referred to as a shallow slope side) having a shallow slope. According to the exemplary arrangement described herein, the first comminuting roller 24 is configured so that the steep slope side is the leading edge 32, and the shallow slope side is the trailing edge 34. The second comminuting roller 26 is arranged so that the steep slope side of the tooth is the trailing edge 44, and the shallow slope side is the leading edge 42.

[0053] Due to the asymmetric profile of the teeth, the multiple teeth can be defined as having an inherent directionality based on the sharp edge facing direction. In addition, the multiple teeth 22 of the first pulverizing roller and the second pulverizing roller are arranged with the same directionality. For the case of the first pulverizing roller 24, the multiple teeth 22 are arranged so that they point to the direction of rotation of the roller. In contrast, the teeth 22 of the second pulverizing roller 26 point to the direction opposite to the second pulverizing roller 26 direction of rotation.

[0054] During operation of the crop processor 10, the crushing rollers 24, 26 are arranged so that the harvested crop entering the crop processor 10 via the inlet 14 is initially engaged by the steeply sloped sides of the teeth of the first crushing roller 24 and the shallowly sloped sides of the teeth of the second crushing roller 26. The majority of the seed breakage occurs between the steeply sloped sides of the roller teeth of the first and second crushing rollers 24, 26, primarily due to the relative speed difference between the rollers. As the crop passes through the opening 30, the crop is further engaged by the other edges of the teeth, including the trailing edges, the leading edge, and the flat top edge.

[0055] It will be appreciated that while the crop pulverizing rollers 18 according to the presently described embodiment each have a plurality of teeth 22 having an asymmetrical profile, the pulverizing rollers 24, 26 may alternatively be configured with symmetrically shaped teeth having leading edges, trailing edges and flat top edges as described above.

[0056] During use, the pulverizing rollers 24, 26 are configured to rotate at different speeds. According to the exemplary arrangement described herein, the first pulverizing roller 24 is arranged to rotate at a faster speed than the second pulverizing roller 26, such as Figure 7aand Figure 7b As shown by the double arrow 28 shown in FIG. 1 , during operation of the crop processor 10, crop grains passing through the opening 30 between the rollers are squeezed between the leading edge 32 of the teeth of the first (faster rotating) pulverizing roller 24 and the trailing edge 44 of the second (slower rotating) pulverizing roller 26. The speed difference between the first and second pulverizing rollers 24, 26 is at least 10% and no more than 50% to effect rupturing of the crop grains.

[0057] During use, the irregular flow of the harvested crop causes irregular wear over the length of each comminuting roller. In particular, the flow of harvested crop material through the center of the roller is greater than the flow at the sides, which causes greater wear in the center than on the sides, resulting in uneven openings between the rollers. Therefore, the effectiveness of the grain rupture process of the harvested crop deteriorates over time. Due to the irregular wear of the comminuting rollers, the comminuting rollers must be replaced more regularly, increasing the maintenance costs of the forage harvester. It is to be understood that the above-mentioned wear process also occurs when a symmetrical tooth profile is applied to the comminuting rollers. In addition, the rupture process itself also causes tooth wear, resulting in irregularly enlarged openings between the rollers.

[0058] In order to enable the teeth to withstand the wear caused by seed breakage, it is known to configure the teeth of the milling roller so that the leading and trailing edges of the teeth exhibit a relatively high uniform hardness. For example, the milling roller may be manufactured from a material having or configured to have a uniform surface hardness. First, the milling roller is subjected to an induction hardening treatment, which involves inducing an alternating magnetic field on the surface of the milling roller so as to locally heat the peripheral surface to a temperature above the transformation range of the constituent alloys. The local heating causes the surface of the milling roller to be hardened, while the core thereof is substantially unaffected by the treatment. The heat treatment so produced has the same hardening effect on the leading and trailing edges of the teeth.

[0059] To further improve the wear resistance of the milling rollers, the tooth surfaces (i.e. the leading and trailing edges) can also be plated with a thin hard chrome layer after induction hardening. This chrome plating technology usually requires the use of hexavalent chromium, which is a toxic substance and its use is increasingly restricted by government regulations.

[0060] A disadvantage of induction hardening is that it tends to concentrate energy in the tooth tip area, which can cause local melting of the tooth tip area. Hardening can also cause deformation of the roller due to metallurgical phase changes in the material. In addition, electrochroming can cause the leading and trailing edges of the teeth to harden indiscriminately, resulting in irregular wear of the crushing roller during operation of the crop processor as described above. In particular, uniform hardening can cause the teeth of the crushing roller to become gradually but irreversibly blunted during operation of the crop processor.

[0061] According to the present invention, an alternative configuration of the first and second comminuting rollers 24, 26 is proposed which is less susceptible to wear. This is achieved by configuring the second (slower moving) comminuting roller 26 so that the leading edge 42 of the plurality of teeth has a hard region 50 which is harder than the leading edge 32 of the teeth of the first (faster moving) comminuting roller 24.

[0062] like Figure 7a and Figure 7b As shown, the advantageous benefits of the hard region 50 can be understood by considering the operation of the crop processor 10. During operation of the crop processor 10, crop material flows from below toward the shredding rollers 24, 26. The rotation of the shredding rollers causes the crop material to be engaged by the leading edge 32, 42 of each shredding roller 24, 26. The movement of the leading edge 32, 42 of the teeth directs the crop material in a generally upward direction toward the opening 30. As the crop material approaches the narrowest point of the opening 30, the relative speed difference between the shredding rollers 24, 26 causes the opposing sets of teeth to clamp the crop material, effectively tearing it apart.

[0063] The above-described grinding process causes the leading edges 32 of the teeth of the first pulverizing roller 24 to wear at a higher rate relative to the leading edges 42 of the teeth of the second pulverizing roller 26. This is due to the increased hardness of the hard region 50 on the second pulverizing roller 26 and, in particular, its enhanced ability to withstand the grinding forces associated with the grain rupture process. The preferential wear of the leading edge 32 causes the teeth of the first pulverizing roller 24 to sharpen, as shown in FIG. Figure 7b Advantageously, this sharpening effect helps extend the life of the shredder roller 24, thereby reducing maintenance costs associated with the crop processor 10.

[0064] Another hard area 48 is provided on the trailing edge 34 of the first pulverizing roller 24. The hard area 48 is provided to have a hardness greater than the hardness of the leading edge 32 of the teeth of the first pulverizing roller 24. The hard area 48 of the teeth 22 of the first pulverizing roller 24 further causes the leading edge 32 and trailing edge 44 of the teeth of the first and second pulverizing rollers 24, 26 to wear preferentially, respectively. Similar to the first pulverizing roller 24, the trailing edge 44 of the second pulverizing roller 26 wears faster than the hard area 50 of the leading edge 42, which will cause the teeth 22 of the second pulverizing roller 26 to sharpen during operation of the crop processor 10. Therefore, the hard areas 48, 50 are provided to have a hardness greater than the hardness of the trailing edge 44 of the teeth of the second pulverizing roller 26.

[0065] The flat top edges 36, 46 of the teeth are also provided with a hard region 52, the hardness of which is greater than the hardness of the leading edge 32 of the teeth of the first comminuting roller 24 and the trailing edge 44 of the teeth of the second comminuting roller 26. The hard region 52 defines the continuation of the hard regions 48, 50 of the leading edge 42 and trailing edge 34 of the teeth of the first comminuting roller 24, 26, respectively. Figure 6 and Figure 7a shown.

[0066] Each of the hard regions 48, 50, 52 is arranged to cover at least a portion of the base surface at which the edges of these hard regions are provided. Figure 6 As shown, the hard region 48 is arranged to extend over a portion (P) of the trailing edge 34 of the teeth of the comminuting roller 24. As will be appreciated by those skilled in the art, the proportion of the tooth surface covered by the hard region is determined according to the wear requirements of the roller.

[0067] The laser cladding process can selectively deposit a wear-resistant layer onto one of the leading and trailing edges of the tooth, thereby achieving the sharpening effect described above. Figure 8 To describe the laser cladding process, Figure 8 The first shredder roller 24 is shown separated from the crop processor 10 for laser cladding processing.

[0068] The laser cladding system is used to deposit wear-resistant material onto the edge of the tooth to be hardened. The laser source of the cladding system is configured to direct a laser beam onto the surface of the tooth, thereby forming a molten pool. The nozzle 52 of the cladding system provides a flow of powder precursors that interacts with the molten pool to form a metal-to-metal bond between the wear-resistant material and the base surface of the tooth. To achieve this, the nozzle 52 is linearly translated along the length of the pulverizing roller 24 in a direction substantially parallel to the axis of rotation of the pulverizing roller, while continuously depositing a narrow track of molten material along the trailing edge 34 (i.e., the less abrupt tooth edge) of a single tooth 22 of the first pulverizing roller 24.

[0069] Once the nozzle 52 reaches one end of the pulverizing roller 24, the pulverizing roller 24 will be rotated incrementally to align the nozzle 52 with the trailing edge 34 of the next adjacent tooth of the roller 24. The nozzle 52 is then translated in the opposite direction along the length of the roller 24 to deposit the molten wear resistant layer as the nozzle is translated. This process is then continued until each trailing edge 34 of each tooth 22 of the first pulverizing roller 24 is clad with the wear resistant material. The laser cladding process is then applied to the second pulverizing roller 26.

[0070] According to another alternative cladding process, a pulverized roller is mounted on a lathe-type machine and rotated during deposition of the wear-resistant material. Specifically, the roller rotates while the nozzle 52 is configured to move longitudinally from one end of the roller to the other. Thus, the wear-resistant layer is applied in a densely packed spiral pattern along the length of the roller. The rotational speed of the roller and the transverse speed of the nozzle are controlled separately to produce a continuous wear-resistant layer along the length of each tooth.

[0071] The dispensing nozzle 52 is configured to deposit a narrow track of molten wear-resistant material so that it covers only a portion (P) of the trailing edge 34, such as Figure 6 Translating the nozzle 52 along the length of the roller 24 causes the molten pool to solidify, thereby producing a continuous layer of solid material.

[0072] Laser cladding of the hard region 48 increases the wear resistance of the coated tooth due to the high tungsten carbide content of the wear-resistant material. The resulting wear-resistant layer has a tungsten carbide content.

[0073] The wear layer is melt-bonded to the teeth at high temperatures so as to form a strong bond between the wear layer and the base roller surface. This is in contrast to known chrome plating techniques which, due to the electrolytic process, mean that there is no real metallic bond between the base material and the hard chrome layer. The wear material of the hard areas 48, 50, 52 is therefore able to withstand the impact of hard stones without the risk of the wear material layer being peeled off from the teeth, as is common with electroplated chrome layers.

[0074] Laser cladding is capable of depositing wear resistant material between the individual features (i.e., between the individual teeth) of the finely serrated outer peripheral surface of the roller. The heat input of the laser cladding process is small and localized to the surface of the roller, so that the base material does not melt, thereby minimizing deformation of the roller. Therefore, the above-described laser cladding process is suitable for the milling roller 18 formed of an induction hardened alloy composition.

[0075] The pulverizing rollers 24, 26 are made of a material configured to provide a hardened surface when subjected to an air hardening process. Air hardening involves allowing the cast metal alloy to cool over a relatively long cooling period. This is typically achieved by allowing the metal alloy rollers to cool in air. The air hardening method is different from alternative methods of forming metal alloy parts, which involve quenching in a fluid (e.g., water). The cooling rate caused by air hardening causes heat energy to slowly dissipate from small molten areas on the roller surface to the rest of the material, resulting in a hard surface layer formed on each pulverizing roller 24, 26. Air hardening advantageously reduces the need to employ additional surface treatments, such as induction hardening, which can result in localized deformation of the teeth, particularly in the tooth tip region 38.

[0076] Once the teeth are machined into the rollers, the teeth are subjected to a hardening process. According to a first hardening process, the cylindrical rollers are heated to a suitable hardening temperature and then allowed to cool in air. Specifically, the first and second grinding rollers 24, 26 are air hardened to form a surface having a hardness sufficient to withstand the grinding of crop grain during operation of the crop processor 10. The air hardening of the rollers is performed prior to the deposition of the wear resistant material. To facilitate the air hardening process, the teeth are made of steel or any suitable material having sufficient hardenability to enable the tooth surface to be air hardened.

[0077] Alternatively, the tooth can be air hardened due to the heat input of the laser cladding process. Specifically, the laser source of the cladding system is configured to form a molten pool on the surface of the tooth during the laser cladding process. The molten pool defines a heat-treated area of ​​the tooth that air hardens as it cools. Therefore, air hardening can be achieved after the wear-resistant layer is deposited.

[0078] According to an alternative hardening process, the tooth may be laser hardened. In this case, the heat for performing the hardening process is provided by a high power laser configured to direct a laser beam to the edge of the tooth. Once the laser treated edge has been heated, it may be cooled in air. In this way, the laser treated edge is air hardened.

[0079] Laser hardening is used to harden the unclad surface of each tooth, i.e., the edge of the tooth that is not clad with wear resistant material. Laser hardening creates a heated area below the laser treated edge of the tooth. The heated area exhibits increased hardness relative to the rest of the tooth. Advantageously, laser hardening enables individual edges of the tooth to be targeted without affecting other areas of the tooth. Laser hardening can be performed before or after the wear resistant layer is clad. To facilitate laser hardening, the teeth should be made of steel or any suitable material that is sufficiently hardenable to enable the tooth surface to be air hardened.

[0080] The air-hardened tooth surface causes preferential wear of those tooth edges that have not been laser clad, resulting in a sharpening effect as described above. Advantageously, each steel composition is capable of forming an air-hardened tooth surface region having a hardness rating within a specified hardness range. Advantageously, the selective deposition of hard regions 48, 50 when combined with the base air-hardening alloy of the milling rollers 24, 26 can produce a sharpening effect on the untreated edges of the teeth 22 (i.e., the tooth edges that do not have laser clad hard regions), such as Figure 7b shown.

[0081] Laser hardening treatment may be selectively applied to the teeth 22 to improve the wear resistance of the unclad edges of the teeth 22. The wear resistance of the laser treated edges is still lower than the wear resistance of the wear layer formed on the teeth 22 of the opposing pulverizing rollers. Therefore, due to the relative difference in wear resistance or hardness between the clad edges and the unclad edges of the teeth 22 disposed on the opposing pulverizing rollers 24, 26, the self-sharpening effect is maintained.

[0082] Manufacturing the crop processor 10 according to the present invention requires manufacturing the crop crushing roller 18 as described above. The crop crushing roller is made of metal, usually ferrous metal. Starting from a cylindrical roller, various processes are performed, such as machining teeth and hardening the machined roller, to obtain a roller that can be used in the crop processor 10. Reference will now be made in particular to Figure 8 and Fig. 9 A method 80, 180 of manufacturing a crop processor 10 according to an aspect of the present invention will now be described.

[0083] The manufacturing method 80 begins by manufacturing the first and second pulverizing rollers 24, 26. In the first method step 82, 182, a pair of generally cylindrical rollers are provided. As described above, the pulverizing rollers 24, 26 are made of a material that can be configured to provide a hard surface when subjected to air hardening to achieve a sharpening effect of the untreated edges of the teeth 22. In order to achieve a self-sharpening effect, the untreated edges of the teeth 22 must be softer than the treated edges. The plurality of teeth can be made of at least one steel alloy.

[0084] In the second method step 84, 184, the plurality of teeth 22 are formed by machining the plurality of teeth into a generally cylindrical roller, thereby leaving a portion of the outer surface of the roller unaffected. As described above, each tooth 22 produced includes a leading edge 32, 42 arranged toward the direction of rotation of the pulverizing rollers 24, 26 during use and a trailing edge 34, 44 away from the direction of rotation of the crop pulverizing rollers 24, 26. The roller is machined so that the roller retains a flat surface on the outer diameter of the roller. The flat edge defines a flat top edge 36, 46 of the teeth 22 of the pulverizing rollers 24, 26. Alternatively, according to a variation of the second method step 184, the roller can be machined so that the roller does not retain a flat top surface on the outer diameter of the roller. Therefore, the teeth formed using this method do not yet include a flat top edge, which can be provided in a later manufacturing step.

[0085] In a third method step 86, 186, a hardened surface 48 is formed on the trailing edge 34 of the teeth of the first pulverizing roller 24. In a fourth step 88, 188, a hardened surface 50 is formed on the leading edge 42 of the teeth 22 of the second pulverizing roller 26. It is to be understood that method steps 86, 186 and 88, 188 may be performed in any order. Forming each hardened surface 48, 50 includes laser cladding a wear resistant layer on the trailing edge 34 and the leading edge 42 of the teeth 22 of the first and second pulverizing rollers 24, 26, respectively. Prior to forming the wear resistant layer, the pulverizing rollers may be subjected to an air hardening process. Alternatively, air hardening may be achieved after the wear resistant layer is deposited due to the heat input from the laser cladding process. Optionally, as described above, the teeth may be subjected to a separate laser hardening process.

[0086] According to a variant of the second method step 182 described above, the roller is machined to have a plurality of teeth without forming an outer flat surface at the roller diameter. The roller machined in this way is now subjected to an additional method step 190, in which a substantially flat top edge is machined or ground on the plurality of teeth. The grinding process of the flat top edge is arranged after the deposition of the hard areas 48, 50. The effect of the grinding process is as follows Fig.10 and Fig.11 As shown, Fig.10 and Fig.11 The teeth 22 of the comminution roller are shown before and after grinding.

[0087] The grinding process ensures that the finished rollers 24, 26 are cylindrical after laser cladding. The grinding process also creates sharp edges at the hard regions 48, 50 towards the tip regions of the teeth 22. It also defines a flat top edge 36, 46 at the outer diameter of the crushing rollers 24, 26. The effect of the grinding process reduces the shape changes of the deposited hard regions 48, 50 caused by the surface tension of the molten phase during deposition. Fig.10 As shown, surface tension can cause rounded outer edges in the crest regions 38 of the teeth 22. The resulting variations in the hard regions 48, 50 can cause a non-uniform reduction in the roller diameter. This rounding can cause the opening 30 between the comminuting rollers 24, 26 to be non-uniform.

[0088] Advantageously, the grinding process eliminates the rounding of the hard regions 48, 50, thereby producing a sharp edge at the flat top edges 36, 46 of the teeth 22, as shown in FIG. Fig.11 The grinding process also helps to reverse the degradation of the cylindricity of the grinding rollers 24, 26 that may be caused by slight variations in the thickness of the hard regions 48, 50. Figure 5 As shown, the flat top edge also helps maintain the spacing between the crushing rollers 24, 26 when they are installed in the crop processor. The crushing rollers 24, 26 require precise and consistent cylindricity to achieve proper narrow alignment of the rollers 24, 26. In particular, the combined laser cladding process and the grinding process can configure the openings 30 to within 1 mm of the gap over the entire length of the roller.

[0089] In the final method steps 92, 192, the pulverizing rollers 24, 26 are assembled into the crop processor housing 12. The pulverizing rollers 24, 26 are arranged in parallel to define an opening 30 between the pulverizing rollers 24, 26. The pulverizing rollers 24, 26 are configured to rotate in opposite directions to each other during use to convey a stream of harvested crop grain received from the inlet 14 through the opening 30 toward the outlet 16. The first pulverizing roller 24 is configured to rotate at a faster speed than the second pulverizing roller 26.

[0090] Reference numerals list

[0091] Crop Processor 10

[0092] Housing 12

[0093] Shell inlet 14

[0094] Shell outlet 16

[0095] Crushing roller 18

[0096] Tooth 22

[0097] First crushing roller 24

[0098] Second crushing roller 26

[0099] Direction of rotation 28

[0100] Tooth front edge 32, 42

[0101] Tooth rear edge 34, 44

[0102] Flat top edge 36, 46

[0103] Tip area 38

[0104] Hard area 48, 50, 52

[0105] Nozzle 52

[0106] Forage Harvester 100

[0107] Frontend 102

[0108] Cutting table 104

[0109] Nozzle 106

[0110] Feeding roller 108

[0111] Runner 110

[0112] Chopper 112

[0113] Accelerator 114

Claims

1. A crop processor (10) for cracking grains in a forage harvester (100), the crop processor (10) comprising: A housing (12) having an inlet (14) and an outlet (16); and A first pulverizing roller and a second pulverizing roller (24, 26) mounted within the housing (12), the first pulverizing roller and the second pulverizing roller (24, 26) being arranged in parallel to define an opening (30) between the first pulverizing roller and the second pulverizing roller (24, 26), the first pulverizing roller and the second pulverizing roller (24, 26) being configured to rotate in opposite directions of rotation to each other during use to convey a harvested crop stream received from the inlet (14) toward the outlet (16) via the opening (30), wherein the first pulverizing roller (24) is configured to rotate at a faster speed than the second pulverizing roller (26); The first pulverizing roller and the second pulverizing roller (24, 26) include a plurality of teeth (22) arranged on the circumferential surface of the first pulverizing roller and the second pulverizing roller (24, 26), and each of the plurality of teeth (22) includes a leading edge (32, 42) facing the rotation direction of the corresponding pulverizing roller; Characterized in that, in the same axial section of the first pulverizing roller and the second pulverizing roller, the leading edge (42) of each tooth of the second pulverizing roller (26) includes a hard area (50) having a harder hardness than the leading edge (32) of each tooth of the first pulverizing roller (24), wherein the axial section is defined as a cross section obtained by cutting the first pulverizing roller and the second pulverizing roller along the same plane intersecting the longitudinal axes of the first pulverizing roller and the second pulverizing roller at right angles.

2. The crop processor (10) according to claim 1, wherein: The trailing edge (34) of the teeth of the first comminuting roller (24) includes a hard region (48) having a greater hardness than the leading edge (32) of the teeth of the first comminuting roller (24).

3. The crop processor (10) according to claim 1 or 2, wherein: The hardness of the hard area (50) of the leading edge (42) of the teeth of the second comminuting roller (26) is greater than the hardness of the trailing edge (44) of the teeth of the second comminuting roller (26).

4. The crop processor (10) according to claim 1, wherein: The plurality of teeth of the first comminuting roller (24) include a generally flat top edge (36); wherein the generally flat top edge (36) of the teeth of the first comminuting roller includes a hard region (52) that is harder than the leading edge (32) of the teeth of the first comminuting roller (24).

5. The processor (10) according to claim 1, wherein: The plurality of teeth of the second comminuting roller (26) include a generally flat top edge (46); wherein the generally flat top edge (46) of the teeth of the second comminuting roller includes a hard region (52) having a greater hardness than a trailing edge (44) of the teeth of the second comminuting roller (26).

6. The crop processor (10) according to any one of claims 1, 2, 4 and 5, wherein: The hard area comprises a wear resistant layer deposited by laser cladding.

7. The crop processor (10) according to claim 1, wherein: The teeth include an air hardened surface area.

8. The crop processor (10) according to claim 1, wherein: At least one edge of the tooth (22) includes a laser hardened surface region.

9. The crop processor (10) according to claim 1, wherein: The plurality of teeth (22) have an asymmetric profile in an axial section of the first pulverizing roller and the second pulverizing roller.

10. A forage harvester comprising a crop processor (10) according to any one of the preceding claims.

11. A method of manufacturing a crop processor (10) for cracking grain in a forage harvester (100), the method comprising: Manufacturing a first pulverizing roller and a second pulverizing roller (24, 26); and Assembling a first pulverizing roller and a second pulverizing roller (24, 26) into a housing (12) having an inlet (14) and an outlet (16), the first pulverizing roller and the second pulverizing roller (24, 26) being arranged in parallel to define an opening (30) between the first pulverizing roller and the second pulverizing roller (24, 26), the first pulverizing roller and the second pulverizing roller (24, 26) being configured to rotate in opposite directions to each other during use to convey a harvested crop stream received from the inlet (14) toward the outlet (16) via the opening (30), wherein the first pulverizing roller (24) is configured to rotate at a faster speed than the second pulverizing roller (26); The manufacturing of the first crushing roller and the second crushing roller (24, 26) comprises: providing a pair of generally cylindrical rollers; a plurality of teeth (22) machined into the generally cylindrical roller, each of the plurality of teeth (22) including a leading edge (32, 42) arranged to face in the direction of rotation of the first and second comminuting rollers (24, 26) during use; and In the same axial section of the first pulverizing roller and the second pulverizing roller, a hard area (50) is formed on the leading edge (42) of each tooth of the second pulverizing roller (26), and the hardness of the hard area (50) is greater than the hardness of the leading edge (32) of each tooth of the first pulverizing roller (24), wherein the axial section is defined as a cross section obtained by cutting the first pulverizing roller and the second pulverizing roller along the same plane intersecting the longitudinal axes of the first pulverizing roller and the second pulverizing roller at right angles.

12. The method according to claim 11, wherein: The method includes forming a hard area (48) on a trailing edge (34) of a tooth of a first pulverizing roller (24) arranged away from a rotation direction of the first pulverizing roller (24), wherein the hardness of the hard area (48) of the trailing edge of the tooth of the first pulverizing roller is greater than the hardness of the leading edge (32) of the tooth of the first pulverizing roller (24).

13. The method according to claim 11, wherein: The method includes forming a hard area (50) on the leading edge (42) of the teeth of the second comminuting roller (26) having a greater hardness than the trailing edge (44) of the teeth of the second comminuting roller (26) arranged away from the rotation direction of the second comminuting roller (26).

14. The method according to any one of claims 11 to 13, wherein: Forming the hard area includes laser cladding a wear-resistant layer on the tooth edge of at least one of the first pulverizing roller and the second pulverizing roller (24, 26).

15. The method according to claim 14, wherein: The first and second comminution rollers (24, 26) are manufactured to also include air hardening at least one edge of the teeth.

Citation Information

Patent Citations

  • Stalk Roll With Coating

    US20100043371A1

  • Toothed crushing disk for a grain processor and method for producing the toothed crushing disk

    US20170118917A1

  • Transport and processing roller for a harvester

    US20180116117A1

  • Crop processor, manufacturing process for a crop processor and crop processor roll

    WO2015075157A1