A display panel, its manufacturing method and display device

By introducing an auxiliary electrode layer into the composite cathode structure of the OLED display panel, the problem of uneven brightness caused by voltage drop is solved, higher conductivity and light extraction efficiency are achieved, and display uniformity and optical performance are improved.

CN115696980BActive Publication Date: 2026-11-10BOE TECHNOLOGY GROUP CO LTD +1
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202211021031.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-08-24
Publication Date
2026-11-10
Estimated Expiration
2042-08-24

AI Technical Summary

Technical Problem

In OLED display panels, uneven voltage drop due to varying distances between pixels and the driving chip results in poor brightness uniformity.

Method used

An auxiliary electrode layer is introduced into the composite cathode structure of the display panel. The auxiliary electrode layer has a second opening at each light-emitting sub-pixel and is formed by inkjet printing and thermal annealing. The material of the auxiliary electrode layer is a metallic conductive material or a transparent conductive material with a reflectivity greater than 90%, which increases conductivity and reflectivity.

Benefits of technology

It improves the conductivity and light emission efficiency of the display panel, avoids uneven brightness caused by voltage drop, and enhances display uniformity and optical performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115696980B_ABST
    Figure CN115696980B_ABST
Patent Text Reader

Abstract

This invention provides a display panel, its manufacturing method, and a display device. The display panel includes: a substrate, a plurality of light-emitting sub-pixels arranged in an array on the substrate, a pixel delimiting structure having a first opening at each light-emitting sub-pixel, and a composite cathode structure located on the side of the pixel delimiting structure and each light-emitting sub-pixel away from the substrate. Along the light emission direction of each light-emitting sub-pixel, the composite cathode structure includes a main electrode layer and an auxiliary electrode layer arranged sequentially. The auxiliary electrode layer has a second opening at each light-emitting sub-pixel, and the orthographic projection of the first opening on the substrate completely falls within the area of ​​the orthographic projection of the second opening on the substrate.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of display technology, and in particular to a display panel, its manufacturing method, and a display device. Background Technology

[0002] Active-matrix organic light-emitting diode (AMOLED) display panels are widely used in mobile phones, wearable devices and other fields due to their advantages such as being flexible and foldable.

[0003] Because the distance between pixels and the driver chip varies in a display panel, the voltage drop of pixels farther from the driver chip is generally greater than that of pixels closer to the chip, resulting in poor brightness uniformity of the display panel. Improving the display panel's performance has become an urgent technical problem to solve. Summary of the Invention

[0004] The present invention provides a display panel, a method for manufacturing the same, and a display device for improving display uniformity.

[0005] In a first aspect, embodiments of the present invention provide a display panel, comprising:

[0006] The substrate has a plurality of light-emitting sub-pixels arranged in an array on the substrate, a pixel defining structure having a first opening at each light-emitting sub-pixel, and a composite cathode structure located on the side of the pixel defining structure and each light-emitting sub-pixel away from the substrate.

[0007] Along the light emission direction of each light-emitting sub-pixel, the composite cathode structure includes a main electrode layer and an auxiliary electrode layer arranged sequentially. The auxiliary electrode layer has a second opening at each light-emitting sub-pixel, and the orthogonal projection of the first opening on the substrate falls completely within the area of ​​the orthogonal projection of the second opening on the substrate.

[0008] In one possible implementation, the thickness of the auxiliary electrode layer is greater than the thickness of the main electrode layer.

[0009] In one possible implementation, the cross-sectional area of ​​the auxiliary electrode layer decreases along a direction away from the substrate, parallel to the plane containing the substrate.

[0010] In one possible implementation, the cross-sectional shape of the auxiliary electrode layer along the corresponding thickness direction is any one of trapezoidal, arc-shaped, or rectangular.

[0011] In one possible implementation, the auxiliary electrode layer is made of a metallic conductive material with a reflectivity greater than 90%.

[0012] In one possible implementation, the auxiliary electrode layer is composed of aggregates of silver nanoparticles.

[0013] In one possible implementation, the auxiliary electrode layer is made of a transparent conductive material.

[0014] In one possible implementation, the transparent conductive material includes at least one material selected from MoO3, ZnO, and ITO.

[0015] In one possible implementation, an organic common layer is further included on the side of the main electrode layer near the substrate. The organic common layer includes a first portion that overlaps with the orthographic projection of the auxiliary electrode layer onto the substrate, and a second portion other than the first portion. The density of the first portion is greater than that of the second portion.

[0016] Secondly, embodiments of the present invention provide a display device, comprising:

[0017] Display panel as described in any of the above items.

[0018] Thirdly, embodiments of the present invention provide a method for manufacturing a display panel, comprising:

[0019] The first opening of the pixel-defining structure is formed on the substrate using a patterning process;

[0020] Multiple light-emitting sub-pixels are formed within the first opening;

[0021] A main electrode layer is formed on the side of the plurality of light-emitting sub-pixels and the pixel defining structure opposite to the substrate.

[0022] Using inkjet printing and thermal annealing processes, an auxiliary electrode layer pattern is formed on the side of the main electrode layer away from the substrate. The auxiliary electrode layer has a second opening at each light-emitting sub-pixel. The orthogonal projection of the first opening on the substrate falls completely within the area of ​​the orthogonal projection of the second opening on the substrate.

[0023] A composite cathode structure comprising the main electrode layer and the auxiliary electrode layer is formed.

[0024] In one possible implementation, the use of inkjet printing and thermal annealing processes to form a pattern of an auxiliary electrode layer on the side of the main electrode layer facing away from the substrate includes:

[0025] An auxiliary processing body is formed on the side of the main electrode layer opposite to the substrate using an inkjet printing process;

[0026] The auxiliary material is thermally annealed under patterned UV light using a thermal annealing process. Nanoparticles corresponding to the metallic conductive material with a reflectivity greater than 90% agglomerate to form a pattern of the auxiliary electrode layer.

[0027] In one possible implementation, after forming the auxiliary processing body on the side of the main electrode layer opposite to the substrate using an inkjet printing process, the method further includes:

[0028] The auxiliary material is thermally annealed under patterned UV light using a thermal annealing process, which causes the nanoparticles of the transparent conductive material to agglomerate and form a patterned auxiliary electrode layer.

[0029] In one possible implementation, the heating temperature in the thermal annealing process ranges from 100°C to 200°C, the heating time ranges from 0.2 min to 2 min, and the UV light intensity ranges from 50 mw / cm². 2 -500mw / cm 2 .

[0030] In one possible implementation, prior to employing the thermal annealing process, the method further includes:

[0031] The auxiliary body is preheated and annealed for a duration ranging from 0.5 min to 3 min.

[0032] The beneficial effects of this invention are as follows:

[0033] This invention provides a display panel, its manufacturing method, and a display device. The display panel includes a substrate, a plurality of light-emitting sub-pixels arranged in an array on the substrate, a pixel defining structure with a first opening at each light-emitting sub-pixel, and a composite cathode structure located on the side of the pixel defining structure and each light-emitting sub-pixel facing away from the substrate. Along the light emission direction of each light-emitting sub-pixel, the composite cathode structure includes a main electrode layer and an auxiliary electrode layer sequentially disposed. The auxiliary electrode layer has a second opening at each light-emitting sub-pixel, and the orthographic projection of the first opening onto the substrate completely falls within the area of ​​the orthographic projection of the second opening onto the substrate. In this way, the conductivity of the entire composite cathode structure is improved by adding an auxiliary electrode layer. Furthermore, the auxiliary electrode layer can increase the reflectivity of the composite cathode structure to a certain extent, thereby improving the light emission efficiency, avoiding brightness unevenness caused by voltage drop, and improving display uniformity. Attached Figure Description

[0034] Figure 1 This is a characteristic curve of pixel driving in OLED display panels in related technologies;

[0035] Figure 2A top view schematic diagram of one embodiment of a display panel provided by the present invention;

[0036] Figure 3 For along Figure 2 A schematic diagram of one type of cross-sectional structure in the direction shown in MM;

[0037] Figure 4 For along Figure 2 A schematic diagram of one type of cross-sectional structure in the direction shown in MM;

[0038] Figure 5 For along Figure 2 A schematic diagram of one type of cross-sectional structure in the direction shown in MM;

[0039] Figure 6 This is a schematic diagram of one structure of a display device provided in an embodiment of the present invention;

[0040] Figure 7 A flowchart illustrating a method for manufacturing a display panel according to an embodiment of the present invention;

[0041] Figure 8 for Figure 7 Flowchart of one method for step S104;

[0042] Figure 9 This is a SEM image of the organic common layer before the heat annealing process;

[0043] Figure 10 This is a SEM image of the organic common layer after the heat annealing process;

[0044] Figure 11 The effect of UV light irradiation time on the temperature of the auxiliary electrode layer;

[0045] Figure 12 The effect of UV light irradiation time on the temperature of surrounding sub-pixels;

[0046] Figure 13 The transverse conductivity of the composite cathode structure before and after the preparation of the auxiliary electrode layer.

[0047] Explanation of reference numerals in the attached figures:

[0048] 10-Substrate; 20-Light-emitting sub-pixel; 30-First opening; 40-Pixel defining structure; 50-Composite cathode structure; 51-Main electrode layer; 52-Auxiliary electrode layer; 53-Second opening; 60-Auxiliary light-emitting layer; 70-Thin film encapsulation layer; 80-Organic common layer; 100-Display panel. Detailed Implementation

[0049] To make the objectives, technical solutions, and advantages of the embodiments of the present invention clearer, the technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some, not all, of the embodiments of the present invention. Furthermore, the embodiments and features in the embodiments of the present invention can be combined with each other without conflict. Based on the described embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0050] Unless otherwise defined, the technical or scientific terms used in this invention shall have the ordinary meaning as understood by one of ordinary skill in the art to which this invention pertains. The terms "comprising" or "including," or similar terms as used in this invention, mean that the element or object preceding the word encompasses the elements or objects listed following the word and their equivalents, without excluding other elements or objects.

[0051] It should be noted that the dimensions and shapes of the figures in the accompanying drawings do not reflect actual proportions and are intended only to illustrate the content of the invention. Furthermore, the same or similar reference numerals denote the same or similar elements or elements having the same or similar functions throughout.

[0052] In related technologies, the voltage drop of pixels farther from the driver chip in an OLED display panel is generally greater than that of pixels farther from the driver chip. Combined with... Figure 1 As shown in the characteristic curve of the pixel driving of the OLED display panel, the voltage difference Vds between the source and drain of the driving transistor of the pixel farther away from the driving chip is smaller than that between the source and drain of the driving transistor of the pixel closer to the driving chip. As a result, the current Ids of the pixel farther away from the driving chip is smaller than that of the pixel closer to the driving chip, which in turn leads to the problem of abnormal brightness uniformity of the display panel.

[0053] In view of this, embodiments of the present invention provide a display panel, a method for manufacturing the same, and a display device for improving display uniformity.

[0054] Combination Figure 2 and Figure 3 As shown, where, Figure 2 This is a top view schematic diagram of one embodiment of a display panel provided by the present invention. Figure 3 For along Figure 2 A schematic diagram of one type of cross-sectional structure in the direction shown in the middle MM. Still combined with... Figure 2 and Figure 3 As shown, the display panel provided in this embodiment of the invention includes:

[0055] The substrate 10 includes a plurality of light-emitting sub-pixels 20 arranged in an array on the substrate 10, a pixel defining structure 40 having a first opening 30 at each light-emitting sub-pixel 20, and a composite cathode structure 50 located on the side of the pixel defining structure 40 and each light-emitting sub-pixel 20 away from the substrate 10.

[0056] Along the light emission direction of each light-emitting sub-pixel 20, the composite cathode structure 50 includes a main electrode layer 51 and an auxiliary electrode layer 52 arranged sequentially. The auxiliary electrode layer 52 has a second opening 53 at each light-emitting sub-pixel 20. The orthographic projection of the first opening 30 on the substrate 10 completely falls within the area of ​​the orthographic projection of the second opening 53 on the substrate 10.

[0057] In specific implementation, the substrate 10 can be a flexible substrate or a rigid substrate, and no limitation is made here. The display panel also includes a plurality of light-emitting sub-pixels 20 arranged in an array on the substrate 10, wherein the plurality of light-emitting sub-pixels 20 can be sub-pixels including multiple colors. Figure 2 In one exemplary embodiment, the luminous pixel may be composed of luminous sub-pixels 20 of three colors, including red, green, and blue sub-pixels. In another exemplary embodiment, the luminous pixel may be composed of luminous sub-pixels 20 of four colors, including red, green, blue, and white sub-pixels. Figure 2 and Figure 3 This illustration only shows the arrangement of some of the luminous sub-pixels 20 in the display panel and does not mean that the display panel can only be arranged in this way. Of course, the number and arrangement of the luminous sub-pixels 20 can be set according to the actual application needs, and are not limited here.

[0058] Furthermore, the display panel also includes a pixel defining structure 40 with a first opening 30 at each light-emitting sub-pixel 20, and a composite cathode structure 50 located on the side of the pixel defining structure 40 and each light-emitting sub-pixel 20 facing away from the substrate 10. Along the light emission direction of each light-emitting sub-pixel 20, the composite cathode structure 50 includes a main electrode layer 51 and an auxiliary electrode layer 52 sequentially disposed. In one exemplary embodiment, the orthographic projection of each light-emitting sub-pixel 20 onto the substrate 10 can completely fall within the area of ​​the orthographic projection of the main electrode layer 51 onto the substrate 10, and the main electrode layer 51 can be a single, continuous structure. Moreover, the auxiliary electrode layer 52 has a second opening 53 at each light-emitting sub-pixel 20, and the orthographic projection of the first opening 30 onto the substrate 10 completely falls within the area of ​​the orthographic projection of the second opening 53 onto the substrate 10. In practical applications, the composite cathode structures 50 corresponding to each light-emitting sub-pixel 20 can be connected in series through the auxiliary electrode layer 52 and the main electrode layer 51. On the one hand, the auxiliary electrode layer 52 increases the overall thickness of the composite cathode structure 50 to a certain extent, thereby increasing the conductivity of the corresponding structure. On the other hand, the auxiliary electrode layer 52 of a certain thickness reduces the light transmittance of the pixel defining structure 40 on the side away from the substrate 10, and increases the reflectivity of the composite cathode structure 50 at the corresponding position. In this way, the light that was originally emitted from the side view is reflected and refracted, and part of it is emitted from the front view, which to a certain extent makes up for the efficiency reduction caused by the voltage drop, thereby avoiding the abnormal optical performance of the display panel caused by the voltage drop and ensuring the display effect.

[0059] In this embodiment of the invention, the thickness of the auxiliary electrode layer 52 is greater than the thickness of the main electrode layer 51.

[0060] In the specific implementation process, the thickness of the main electrode layer 51 ranges from 100nm to 200nm, and the thickness of the auxiliary electrode layer 52 ranges from 500nm to 2000nm.

[0061] The inventors discovered that, according to the sheet resistance formula for metals: R = ρ / d, where ρ represents the resistivity of the cathode and d represents the thickness of the cathode, the resistance can be reduced and the conductivity increased by increasing the cathode thickness. However, once the cathode thickness increases, the light transmittance decreases accordingly. This means that achieving the same brightness as conventional devices requires a larger voltage, leading to increased power consumption. Furthermore, increasing the cathode thickness also increases the optical path difference between the front and side viewing angles, resulting in poor color shift. Balancing cathode transmittance and conductivity is crucial for improving display performance. Therefore, in this embodiment, a thicker auxiliary electrode layer 52 is added to the main electrode layer 51. This improves the conductivity of the composite cathode structure 50. Additionally, since the auxiliary electrode layer 52 is located outside the first opening 30 in the pixel defining structure 40, it increases the reflectivity of the composite cathode structure 50. Light that would normally exit from the side viewing angle is partially reflected and refracted, exiting from the front viewing angle, thus mitigating the efficiency reduction caused by voltage drop and preventing abnormal optical performance of the display panel due to voltage drop, ensuring optimal display performance. In addition, the linewidth of the auxiliary electrode layer 52 can be in the range of 2μm-10μm, and the corresponding sheet resistance can be less than 2.0Ω / □, thereby improving the display abnormality caused by voltage drop in the display panel.

[0062] In embodiments of the present invention, the auxiliary electrode layer 52 can have various structural configurations. In one exemplary embodiment, it is still combined with... Figure 3 As shown, along the direction away from the substrate 10, the cross-sectional area of ​​the auxiliary electrode layer 52 decreases along the plane parallel to the substrate 10. Of course, the auxiliary electrode layer 52 can be configured according to actual application needs, and is not limited to this.

[0063] In one exemplary embodiment, the cross-sectional shape of the auxiliary electrode layer 52 along the corresponding thickness direction is any one of trapezoidal, arc-shaped, or rectangular. In one exemplary embodiment, Figure 4 For along Figure 2 A schematic diagram of one type of cross-sectional structure in the direction shown in the middle MM. Still combined with... Figure 4 As shown, the cross-sectional shape of the auxiliary electrode layer 52 along the corresponding thickness direction is arc-shaped. Of course, the cross-sectional shape of the auxiliary electrode layer 52 along the corresponding thickness direction can also be set according to the actual application needs, and is not limited here.

[0064] It should be noted that after the auxiliary electrode layer 52 is provided on the main electrode layer 51, the transmission path of light from the light-emitting sub-pixel 20 can be as follows: Figure 3 and Figure 4The direction indicated by the middle arrow. Light from the light-emitting sub-pixel 20, after reflection and refraction by the auxiliary electrode layer 52, increases the light output efficiency at the positive viewing angle. This reduces the power consumption of the display panel in this embodiment of the invention while maintaining the same brightness. Furthermore, the actual light transmission path is not limited to... Figure 3 and Figure 4 The situation shown is not limited here.

[0065] In this embodiment of the invention, the auxiliary electrode layer 52 can be prepared using several exemplary methods. In specific implementations, the material of the auxiliary electrode layer 52 is a metallic conductive material with a reflectivity greater than 90%. In one exemplary embodiment, the auxiliary electrode layer 52 is formed by the aggregation of silver nanoparticles. Taking the preparation of the auxiliary electrode layer 52 by the aggregation of silver nanoparticles as an example, an inkjet printing process can be used to print a solution containing silver nanoparticles onto the side of the main electrode layer 51 facing away from the substrate 10, thereby forming an auxiliary processed body; then, the auxiliary processed body is subjected to thermal annealing under patterned ultraviolet (UV) light, causing the silver nanoparticles to aggregate and form a structure such as... Figure 3 or Figure 4 The auxiliary electrode layer 52 is solidified. In addition, the solution including silver nanoparticles can be an organic polar solvent that is insoluble in the organic materials being evaporated. In this way, the solution including silver nanoparticles will not dissolve the light-emitting layer related to the evaporation process. Accordingly, the preparation of the auxiliary electrode layer 52 will not affect the light-emitting layer of the evaporation process, nor will it affect the device performance such as the lifespan of the device, thereby ensuring the manufacturing efficiency of the display panel.

[0066] In one exemplary embodiment, the auxiliary electrode layer 52 is made of a transparent conductive material. This transparent conductive material has a high refractive index, and can be a material with a refractive index greater than 1. In specific implementations, the transparent conductive material includes at least one of MoO3, ZnO, and ITO. In actual fabrication, an inkjet printing method can be used to print a solution of nanoparticles containing the transparent conductive material onto the side of the main electrode layer 51 facing away from the substrate 10, thereby forming an auxiliary processing body. Then, this auxiliary body is subjected to thermal annealing under patterned UV light, causing the nanoparticles of the transparent conductive material to aggregate, reducing their surface energy. Depending on the heating method, the auxiliary electrode layer 52 of the desired shape is formed. Furthermore, the solution containing the transparent conductive material can be an organic polar solvent that will not dissolve the vapor-deposited light-emitting layer. Consequently, the fabrication process of the auxiliary electrode layer 52 will not affect the light-emitting layer of the vapor deposition process, nor will it affect the device's lifespan or other device performance, thus ensuring the fabrication efficiency of the display panel.

[0067] Furthermore, the inventors discovered that after setting the auxiliary electrode layer 52 on the display panel, the white light efficiency (WEff) gain of the display panel can reach 19%, and the specific gains are shown in Table 1, where "ref" represents reference data, "Effi" represents efficiency, and "EL power@450nit" represents the light-emitting power consumption of the light-emitting sub-pixel at a brightness of 450nit.

[0068]

[0069] Table 1

[0070] Existing Efficiency Enhancement Structure (EES) technology requires the integration of high-refractive-index and low-refractive-index optical synthesis, involving processes such as inkjet printing, exposure, and development. As shown in Table 1, the display panel provided in this embodiment, compared to existing EES technology, only requires an auxiliary electrode layer 52 with the desired structure, formed by the agglomeration of silver nanoparticles after inkjet printing and heating. This auxiliary electrode layer 52 can serve as a reflective layer, improving the light extraction efficiency at the front viewing angle of the display panel. The display panel has lower power consumption and lower cost, and has broad application prospects.

[0071] It should be noted that the light-emitting sub-pixels 20 involved in the embodiments of the present invention may include at least one of: Organic Light Emitting Diode (OLED) and Quantum Dot Light Emitting Diodes (QLED). In specific implementation, in addition to the aforementioned film layers, the display panel in the embodiments of the present invention uses... Figure 3 Taking the display panel shown as an example, as Figure 5As shown, the display panel also includes an auxiliary light-emitting layer 60 disposed on the side of the main electrode layer 51 facing away from the substrate 10 and located within the second opening 53. The orthographic projection of the auxiliary light-emitting layer 60 onto the substrate 10 completely falls within the area of ​​the orthographic projection of the corresponding sub-pixel onto the substrate 10. In this way, the light emission efficiency of the corresponding light is increased during the light emission process of each sub-pixel, improving the display effect of the display panel. In addition, the display panel also includes a thin film encapsulation (TFE) 70 located on the side of the auxiliary electrode layer 52 facing away from the substrate 10. Along the light emission direction of the light-emitting sub-pixel 20, the thin film encapsulation layer 70 includes overlapping inorganic and organic layers. It should be noted that, regardless of the structure of the thin film encapsulation layer 70, the topmost layer of the thin film encapsulation layer 70 is always an inorganic layer to effectively block water and oxygen, improving the performance of the display panel. The inorganic layer can be made of at least one of silicon oxide, silicon nitride, and silicon oxynitride, and the organic layer can be made of an organic material suitable for inkjet printing.

[0072] In the embodiments of the present invention, it is still combined with Figure 5 As shown, the display panel also includes an organic common layer 80 located on the side of the main electrode layer 51 near the substrate 10. The organic common layer 80 includes a first portion that overlaps with the orthographic projection of the auxiliary electrode layer 52 on the substrate 10, and a second portion other than the first portion. The density of the first portion is greater than the density of the second portion.

[0073] Still combined Figure 5 As shown, the display panel also includes an organic common layer 80 located on the side of the main electrode layer 51 near the substrate 10. Along the light emission direction of each light-emitting sub-pixel 20, the organic common layer 80 includes a hole blocking layer, an electron transport layer, and an electron injection layer located between the light-emitting sub-pixel 20 and the main electrode layer 51, as well as a hole injection layer, a hole transport layer, and an electron blocking layer located between the light-emitting sub-pixel 20 and the substrate 10. Figure 5 The specific film structure of the organic common layer 80 is not illustrated in the diagram; however, the specific film structure is implemented according to relevant technologies. Furthermore, the organic common layer 80 includes a first portion overlapping the orthographic projection of the auxiliary electrode layer 52 onto the substrate 10, and a second portion excluding the first portion. This reduces the lateral conductivity of the organic common layer 80, avoids lateral carrier mobility issues between adjacent light-emitting pixels 20 corresponding to the organic common layer 80, effectively prevents lateral crosstalk, and improves the display effect.

[0074] In one exemplary embodiment, the display panel further includes a polarizer located on the side of the thin-film encapsulation layer 70 facing away from the substrate 10. This polarizer not only reduces the reflection of ambient light from the display panel, improving the user experience, but also prevents the influence of ambient light on the organic light-emitting materials, ensuring the lifespan of the organic light-emitting materials and improving the performance of the display panel. In addition, the display panel also includes an adhesive layer and a cover plate disposed on the side of the polarizer facing away from the substrate 10. The adhesive layer can be optically clear adhesive (OCA), ensuring both transparent display and structural stability. The cover plate not only protects the display panel from damage, but also improves the performance of the display device by providing a coating with specific functions. This coating can be one or more of an anti-glare (AG) protective film, an anti-fingerprint (AF) film, and an anti-ultraviolet (UV) protective film, and is not limited here. Of course, other films can be provided according to actual application needs, which can be implemented with reference to relevant technologies, and will not be detailed here.

[0075] In one exemplary embodiment, the display panel further includes a color filter located on the side of the thin-film encapsulation layer 70 facing away from the substrate 10. In this case, a color filter on encapsulation (COE) technology can be employed, ensuring a thinner and lighter display panel design compared to a thicker polarizer. In this exemplary embodiment, the display panel also includes an adhesive layer and a cover plate disposed on the side of the color filter facing away from the substrate 10. The arrangement of the adhesive layer and cover plate can be found in related technologies and will not be detailed here.

[0076] In one exemplary embodiment, the display panel further includes a touch structure (Flexible Multi-Layer On Cell, FMLOC) located on the side of the thin-film encapsulation layer 70 opposite to the substrate 10. Accordingly, the various film layers of the touch structure can be directly fabricated on the thin-film encapsulation layer 70, and the touch structure is disposed within the film layer structure. Therefore, there is no need to separately provide a touch substrate, thereby ensuring the touch functionality of the display panel while maintaining a thin and lightweight design. Specific details regarding the touch structure can be found in related technologies and will not be elaborated here. Of course, in addition to the aforementioned film layer structure, the display panel may also include other film layer structures, which can be found in related technologies and will not be elaborated here.

[0077] Based on the same inventive concept, such as Figure 6As shown, this embodiment of the invention also provides a display device. The principle of this display device in solving the problem is similar to that of the aforementioned display panel 100. Therefore, the implementation of this display device can refer to the implementation of the aforementioned display panel 100, and the repeated parts will not be described again.

[0078] In specific implementations, the display device provided in the embodiments of the present invention can be any product or component with display function, such as a mobile phone, tablet computer, television, monitor, laptop computer, digital photo frame, or navigator. Other essential components of this display device are understood by those skilled in the art and will not be described in detail here, nor should they be construed as limiting the present invention.

[0079] Based on the same inventive concept, such as Figure 7 As shown, this embodiment of the invention also provides a method for manufacturing a display panel as described above, the method comprising:

[0080] S101: The first opening of the pixel definition structure is formed on the substrate using a patterning process;

[0081] S102: Multiple light-emitting sub-pixels are formed within the first opening;

[0082] S103: A main electrode layer is formed on the side of the plurality of light-emitting sub-pixels and the pixel defining structure opposite to the substrate.

[0083] S104: Using inkjet printing and thermal annealing processes, an auxiliary electrode layer pattern is formed on the side of the main electrode layer away from the substrate. The auxiliary electrode layer has a second opening at each light-emitting sub-pixel. The orthogonal projection of the first opening on the substrate falls completely within the area of ​​the orthogonal projection of the second opening on the substrate.

[0084] S105: Form a composite cathode structure including the main electrode layer and the auxiliary electrode layer.

[0085] In the specific implementation process, steps S101 to S105 are implemented as follows:

[0086] First, a first opening 30 of the pixel defining structure 40 is formed on the substrate 10 using a patterning process. This "patterning process" primarily involves exposure, development, and etching to form a pattern for the corresponding film layer. Then, a plurality of light-emitting sub-pixels 20 can be formed within the first opening 30. In one exemplary embodiment, the plurality of light-emitting sub-pixels 20 can be formed within the first opening 30 using a vacuum evaporation process. In another exemplary embodiment, the plurality of light-emitting sub-pixels 20 can also be formed within the first opening 30 using an inkjet printing process; of course, any process required for the actual application can be used to form the plurality of light-emitting sub-pixels 20 within the first opening 30. After the plurality of light-emitting sub-pixels 20 are formed within the first opening 30, a main electrode layer 51 can be formed on the side of the plurality of light-emitting sub-pixels 20 and the pixel defining structure 40 facing away from the substrate 10. In one exemplary embodiment, the main electrode layer 51 can be formed on the side of the plurality of light-emitting sub-pixels 20 and the pixel defining structure 40 facing away from the substrate 10 using a vacuum evaporation process. Then, inkjet printing and thermal annealing processes can be used to form the pattern of the auxiliary electrode layer 52 on the side of the main electrode layer 51 facing away from the substrate 10. The specific implementation process can be found in the description below and will not be detailed here. The pattern of the formed auxiliary electrode layer 52 satisfies the condition that a second opening 53 is formed at each light-emitting sub-pixel 20, and the orthographic projection of the first opening 30 on the substrate 10 completely falls within the area of ​​the orthographic projection of the second opening 53 on the substrate 10, thereby forming a composite cathode structure 50 including the main electrode layer 51 and the auxiliary electrode layer 52. In this way, the conductivity of the entire composite cathode structure 50 is improved by adding the auxiliary electrode layer 52. Furthermore, the auxiliary electrode layer 52 can increase the reflectivity of the composite cathode structure 50 to a certain extent, thereby improving the light extraction efficiency, avoiding brightness unevenness caused by voltage drop, and improving display uniformity.

[0087] In the embodiments of the present invention, the auxiliary electrode layer 52 can be prepared by the following exemplary implementation methods, but is not limited to the following methods.

[0088] In one exemplary embodiment, the auxiliary electrode layer 52 is made of a metallic conductive material with a reflectivity greater than 90%, such as... Figure 8 As shown, step S104: using inkjet printing and thermal annealing processes, a pattern of an auxiliary electrode layer is formed on the side of the main electrode layer facing away from the substrate, including:

[0089] S201: An auxiliary processing body is formed on the side of the main electrode layer away from the substrate using inkjet printing technology;

[0090] S202: The auxiliary material is thermally annealed under patterned UV light using a thermal annealing process. Nanoparticles corresponding to the metal conductive material with a reflectivity greater than 90% agglomerate to form a pattern of the auxiliary electrode layer.

[0091] In the specific implementation process, steps S201 to S202 are implemented as follows:

[0092] First, an inkjet printing process is used to form a patterned auxiliary material on the side of the main electrode layer 51 facing away from the substrate 10. Then, a thermal annealing process can be used to anneal the auxiliary material under patterned UV light. This causes the nanoparticles corresponding to the metallic conductive material with a reflectivity greater than 90% to aggregate, forming the pattern of the cured auxiliary electrode layer 52. In practical applications, the desired pattern of the auxiliary electrode layer 52 can be formed by the aggregation of silver nanoparticles. The metallic conductive material can be silver. Of course, any metallic conductive material with a reflectivity greater than 90% can be selected according to the actual application requirements; this is not limited here. Taking silver as an example... Figure 9 The image shown is a scanning electron microscope (SEM) image of the organic common layer before the thermal annealing process. Figure 10 The image shown is a SEM image of the first overlapping portion of the orthographic projection of the organic common layer 80 and the auxiliary electrode layer 52 onto the substrate after the thermal annealing process. Based on Figure 9 and Figure 10 As shown, Figure 10 The density of the first part of the organic common layer 80 is significantly improved. This reduces the overall lateral conductivity of the organic common layer 80, avoids the lateral mobility of charge carriers between adjacent light-emitting pixels 20 corresponding to the organic common layer 80, effectively avoids the problem of lateral crosstalk, and improves the display effect.

[0093] In one exemplary embodiment, the auxiliary electrode layer 52 is made of a transparent conductive material. After step S201: forming the auxiliary processing body on the side of the main electrode layer away from the substrate using an inkjet printing process, the method further includes:

[0094] The auxiliary material is thermally annealed under patterned UV light using a thermal annealing process, which causes the nanoparticles of the transparent conductive material to agglomerate and form a patterned auxiliary electrode layer.

[0095] In this exemplary embodiment, after forming an auxiliary processing body on the side of the main electrode layer 51 away from the substrate 10 using inkjet printing, a thermal annealing process can be employed. This process involves annealing the auxiliary processing body under patterned UV light, causing the nanoparticles of the transparent conductive material to aggregate and form the pattern of the auxiliary electrode layer 52. The transparent conductive material includes at least one material selected from MoO3, ZnO, and ITO. An inkjet printing process can be used to print a solution of nanoparticles containing the transparent conductive material onto the side of the main electrode layer 51 away from the substrate 10. This nanoparticle solution is an organic solvent and has no solubility for the vapor-deposited organic light-emitting material, thus not affecting the device's lifespan.

[0096] Furthermore, the inventors discovered in their actual research that heat is generated during UV light irradiation of the auxiliary processing substrate, leading to an increase in the temperature of the sub-pixels and consequently affecting the performance of the sub-pixel OLED device. Generally, the temperature of the sub-pixels surrounding the auxiliary electrode layer 52 in a display panel should be controlled below 80°C. Combined with... Figure 11 and Figure 12 As shown, where, Figure 11 The effect of UV light irradiation time on the temperature of auxiliary electrode layer 52. Figure 12 This describes the effect of UV light irradiation time on the temperature of surrounding sub-pixels. (Still combined with...) Figure 11 and Figure 12 It can be seen that at 300mw / cm 2 Under illumination of 400mW / cm² light intensity for approximately 160s, the temperature of the auxiliary electrode layer 52 reached about 145℃, but the temperature of the surrounding sub-pixels reached about 100℃. 2 Under illumination of 400mw / cm² for approximately 120 seconds, the temperature of the auxiliary electrode layer 52 reached approximately 152℃, while the temperature of the surrounding sub-pixels reached approximately 80℃. Based on this, it can be concluded that under the above conditions, at 400mw / cm²... 2 When the light intensity is irradiated for about 120 seconds, the temperature of the surrounding sub-pixels reaches about 80℃, which has little impact on the lifespan performance of the sub-pixels surrounding the auxiliary electrode layer 52.

[0097] In the specific implementation process, the heating temperature range is 100℃-200℃, the heating time ranges from 0.2min to 2min, and the UV light intensity ranges from 50mw / cm². 2 -500 mw / cm 2 In this way, while ensuring the uniformity of the display panel's appearance, the lifespan of the display panel is also guaranteed.

[0098] In this embodiment of the invention, before employing the hot annealing process, the method further includes:

[0099] The auxiliary body is preheated and annealed for a duration ranging from 0.5 min to 3 min.

[0100] In the specific implementation process, before performing the thermal annealing process on the auxiliary processing body, a higher temperature can be used to preheat and anneal the auxiliary processing body, thereby ensuring that the nanoparticles move faster at high temperature, reducing defects, and making the structure of the obtained auxiliary electrode layer 52 more compact, thus improving the performance of the display panel.

[0101] Furthermore, the inventors discovered through testing the lateral conductivity before and after the fabrication of the auxiliary electrode layer 52 that, combined with Figure 13 The current density and voltage curves shown indicate that, under a test environment of 25°C, when the preparation conditions of 150°C and 120s are applied to the auxiliary substrate, the lateral conductivity of the organic common layer 80 decreases to 10% of its original value. -5 This reduces the lateral mobility of charge carriers between adjacent photonic pixels 20 and their corresponding organic common layers 80 by orders of magnitude, effectively avoiding lateral crosstalk and improving the display effect.

[0102] This invention provides a display panel, its manufacturing method, and a display device. The display panel includes a substrate 10, a plurality of light-emitting sub-pixels 20 arranged in an array on the substrate 10, a pixel defining structure 40 with a first opening 30 at each light-emitting sub-pixel 20, and a composite cathode structure 50 located on the side of the pixel defining structure 40 and each light-emitting sub-pixel 20 facing away from the substrate 10. Along the light emission direction of each light-emitting sub-pixel 20, the composite cathode structure 50 includes a main electrode layer 51 and an auxiliary electrode layer 52 arranged sequentially. The auxiliary electrode layer 52 has a second opening 53 at each light-emitting sub-pixel 20, and the orthographic projection of the first opening 30 onto the substrate 10 completely falls within the area of ​​the orthographic projection of the second opening 53 onto the substrate 10. In this way, the conductivity of the entire composite cathode structure 50 is improved by adding the auxiliary electrode layer 52. Furthermore, the auxiliary electrode layer 52 can increase the reflectivity of the composite cathode structure 50 to a certain extent, thereby improving the light emission efficiency, avoiding brightness unevenness caused by voltage drop, and improving display uniformity.

[0103] Although preferred embodiments of the invention have been described, those skilled in the art, upon learning the basic inventive concept, can make other changes and modifications to these embodiments. Therefore, the appended claims are intended to be interpreted as including both the preferred embodiments and all changes and modifications falling within the scope of the invention.

[0104] Obviously, those skilled in the art can make various modifications and variations to this application without departing from the spirit and scope of this application. Therefore, if such modifications and variations fall within the scope of the claims of this application and their equivalents, this application also intends to include such modifications and variations.

Claims

1. A display panel, characterized in that, include: The substrate has a plurality of light-emitting sub-pixels arranged in an array on the substrate, a pixel defining structure having a first opening at each light-emitting sub-pixel, and a composite cathode structure located on the side of the pixel defining structure and each light-emitting sub-pixel away from the substrate. Along the light emission direction of each light-emitting sub-pixel, the composite cathode structure includes a main electrode layer and an auxiliary electrode layer arranged sequentially. The auxiliary electrode layer has a second opening at each light-emitting sub-pixel, and the orthogonal projection of the first opening on the substrate completely falls within the area of ​​the orthogonal projection of the second opening on the substrate. The formation of the auxiliary electrode layer includes: using a thermal annealing process to perform thermal annealing on the auxiliary processing body under patterned UV light. The display panel further includes an organic common layer located on the side of the main electrode layer near the substrate. The organic common layer includes a first portion that overlaps with the orthographic projection of the auxiliary electrode layer on the substrate, and a second portion other than the first portion. The density of the first portion of the organic common layer after patterned UV photothermal annealing is greater than the density of the second portion. The thickness of the main electrode layer ranges from 100nm to 200nm, the thickness of the auxiliary electrode layer ranges from 500nm to 2000nm, and the thickness of the auxiliary electrode layer is greater than the thickness of the main electrode layer. The linewidth of the auxiliary electrode layer ranges from 2μm to 10μm.

2. The display panel as described in claim 1, characterized in that, Along the direction away from the substrate, the cross-sectional area of ​​the auxiliary electrode layer decreases along the plane parallel to the substrate.

3. The display panel as described in claim 2, characterized in that, The cross-sectional shape of the auxiliary electrode layer along the corresponding thickness direction is any one of trapezoidal, arc, or rectangular.

4. The display panel as described in any one of claims 1-3, characterized in that, The auxiliary electrode layer is made of a metallic conductive material with a reflectivity greater than 90%.

5. The display panel as described in claim 4, characterized in that, The auxiliary electrode layer is composed of aggregated silver nanoparticles.

6. The display panel as described in any one of claims 1-3, characterized in that, The auxiliary electrode layer is made of a transparent conductive material.

7. The display panel as described in claim 6, characterized in that, The transparent conductive material includes at least one of MoO3, ZnO, and ITO.

8. A display device, characterized in that, include: The display panel as described in any one of claims 1-7.

9. A method for manufacturing a display panel, characterized in that, include: The first opening of the pixel-defining structure is formed on the substrate using a patterning process; Multiple light-emitting sub-pixels are formed within the first opening; A main electrode layer is formed on the side of the plurality of light-emitting sub-pixels and the pixel defining structure opposite to the substrate. An auxiliary electrode layer pattern is formed on the side of the main electrode layer away from the substrate using inkjet printing and thermal annealing processes. The auxiliary electrode layer has a second opening at each light-emitting sub-pixel, and the orthogonal projection of the first opening on the substrate completely falls within the area of ​​the orthogonal projection of the second opening on the substrate. The formation of the auxiliary electrode layer includes: thermal annealing the auxiliary processing body under patterned UV light. A composite cathode structure including the main electrode layer and the auxiliary electrode layer is formed; wherein, the display panel further includes an organic common layer located on the side of the main electrode layer near the substrate, the organic common layer including a first portion overlapping the orthographic projection of the auxiliary electrode layer on the substrate, and a second portion other than the first portion; the density of the first portion in the organic common layer after patterned UV photothermal annealing is greater than the density of the second portion; wherein, the thickness of the main electrode layer is in the range of 100nm-200nm, the thickness of the auxiliary electrode layer is in the range of 500nm-2000nm, and the thickness of the auxiliary electrode layer is greater than the thickness of the main electrode layer, and the linewidth of the auxiliary electrode layer is in the range of 2μm~10μm.

10. The manufacturing method as described in claim 9, characterized in that, The process employs inkjet printing and thermal annealing to form a pattern for an auxiliary electrode layer on the side of the main electrode layer facing away from the substrate, including: An auxiliary processing body is formed on the side of the main electrode layer away from the substrate using an inkjet printing process; The auxiliary material is thermally annealed under patterned UV light using a thermal annealing process. Nanoparticles corresponding to the metallic conductive material with a reflectivity greater than 90% agglomerate to form a pattern of the auxiliary electrode layer.

11. The manufacturing method as described in claim 10, characterized in that, After forming the auxiliary processing body on the side of the main electrode layer opposite to the substrate using inkjet printing technology, the method further includes: The auxiliary material is subjected to a thermal annealing process under patterned UV light, which causes the nanoparticles of the transparent conductive material to agglomerate and form a pattern for the auxiliary electrode layer.

12. The manufacturing method as described in claim 9, characterized in that, In the aforementioned hot annealing process, the heating temperature range is 100℃-200℃, the heating time ranges from 0.2min to 2min, and the UV light intensity ranges from 50 mw / cm². 2 -500 mw / cm 2 .

13. The manufacturing method as described in claim 10, characterized in that, Prior to employing the aforementioned hot annealing process, the method further includes: The auxiliary body is preheated and annealed for a duration ranging from 0.5 min to 3 min.

Citation Information

Patent Citations

  • Display substrate and manufacturing method thereof, and display device

    CN109301078A

  • Display panel and manufacturing method thereof, and display device

    CN109817825A

  • Display panel and preparation method thereof

    CN110931653A

  • Display substrate, preparation method thereof and display device

    CN112928150A