A flexible automated molding method for composite materials
Through the combination of laser rangefinder and machine vision inspection system, the flexible automated molding method solves the problem of insufficient diaphragm stretching in thermal diaphragm molding, achieves more efficient and accurate composite material molding, and ensures the quality of finished products.
Patent Information
- Application Number
- CN202211430763.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-11-15
- Publication Date
- 2024-10-25
- Estimated Expiration
- 2042-11-15
AI Technical Summary
In thermal separator molding technology, the insufficient stretch of the separator for different products results in poor molding effect, and there is a lack of closed-loop feedback of the product after molding, which affects molding accuracy and efficiency.
A flexible automated molding method is used to adjust the diaphragm area through a laser range finder, and a machine vision inspection system is used to monitor and adjust the molding process in real time to ensure the fit between the mold and the diaphragm. Material testing is performed after molding to ensure quality standards.
It improves the molding accuracy and efficiency, enhances the degree of mechanical automation, and ensures high-quality molding of composite materials.
Smart Images

Figure CN115709573B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of fiber composite material laying, in particular to a flexible automatic molding method for composite materials. Background Art
[0002] With the continuous advancement of aviation manufacturing technology, the use of composite materials has continued to increase. Its application has gradually expanded from secondary load-bearing components to primary load-bearing components, and its application has also expanded from the tail to the wing and even to the fuselage. Its use has become an important symbol of the advancement of aviation structures. The main load-bearing components of composite materials are mainly large reinforced wall panels, and a large number of composite long stringer parts will be used. Composite long stringers have the characteristics of large aspect ratio, complex cross-sectional shape, and high processing precision requirements, which puts higher requirements on the molding process.
[0003] Hot diaphragm molding is a typical composite material preforming technology, which is to place the prepreg on the mold, evacuate and heat it through a diaphragm made of special materials, and the diaphragm is stretched and deformed to press the prepreg against the mold, and finally the desired preform shape is obtained. Compared with the traditional layering method, it has high molding efficiency and high part precision. At present, the hot diaphragm molding technology has the problem of insufficient diaphragm stretching for different products, resulting in poor molding effect, and no corresponding closed-loop feedback for the molded products. Summary of the invention
[0004] In view of the above technical problems, a preparation method for flexible automatic molding of composite materials is provided.
[0005] The technical means adopted by the present invention are as follows:
[0006] A composite material flexible automatic molding method comprises the following steps:
[0007] S1. placing the mold containing the material in the diaphragm device;
[0008] An automatic conveying device can be used to transport the mold carrying the material to the diaphragm device;
[0009] S2, using hot air to heat the diaphragm in the diaphragm device, and at the same time heat the mold and the material in the mold;
[0010] During the heating process, a temperature sensor is used to timely feedback the temperature, and the diaphragm, mold and material are accurately controlled to reach the preset temperature value based on the feedback temperature, and the error range is accurately controlled within 0.5℃.
[0011] S3, calculating the shape of the mold cavity by a laser rangefinder, and adjusting the diaphragm area corresponding to the mold accordingly;
[0012] The diaphragm area is adjusted by a pair of rollers. The pair of rollers adjusts the amount of overhang deformation of the diaphragm in the diaphragm frame according to the shape of the mold cavity, so that the size of the diaphragm used to compact the prepreg is compatible with the prepreg. The pair of rollers includes two groups of rollers, each group of rollers includes two rollers, one of which is an active roller connected to a pair of rollers motor, and the other is a driven roller. The diaphragm is located in the gap between the active roller and the driven roller, and the movement is achieved through the cooperation of the active roller and the driven roller, thereby adjusting its overhang deformation in the diaphragm frame.
[0013] S4, after the mold and the diaphragm frame of the diaphragm device are molded together, the mold and the diaphragm frame are fixed by clamping claws;
[0014] The clamping jaws can be electromagnetic clamping jaws, which can make the overall equipment more automated. When designing the clamping jaws, it should be ensured that the taper between the clamping jaws and the clamping block is greater than the Morse taper, so that the strength between them can be guaranteed from a structural point of view.
[0015] S5. Vacuum the space below the diaphragm in blocks according to the shape of the mold;
[0016] The area that needs to be deformed is deformed first by vacuuming in blocks, and the corresponding vacuum holes are opened or closed according to the difficulty of deformation of the diaphragm. The vacuum holes are covered with a polytetrafluoroethylene breathable film to ensure that the vacuum holes will not be blocked by the diaphragm during vacuuming.
[0017] S6, applying positive pressure to the diaphragm from above the diaphragm;
[0018] The pressure of the positive pressure is P, the area of the diaphragm frame is S, and the minimum pressure value F1 that the clamp can withstand should be: F1>P×S+E, where E is the safety factor, and the value of E is determined by the actual situation on site.
[0019] S7. Observe the vacuum degree in the mold cavity and maintain the pressure for 3 minutes;
[0020] S8. Test the material after diaphragm molding. If the material meets the standard, separate the diaphragm frame from the mold and take out the material. If the material does not meet the standard, re-diaphragm mold the material until it meets the standard.
[0021] In step S8, the material is inspected using a machine vision inspection system;
[0022] Furthermore, the specific machine vision inspection system includes:
[0023] (1) Grayscale processing: converting the color image taken by the industrial camera into a grayscale image;
[0024] (2) Perform histogram equalization and median filtering on the grayscale image;
[0025] (3) The image obtained in step (2) is filtered using a Gabor filter based on scale transformation, and the filtered images in multiple directions are fused to obtain an image with clearer texture.
[0026] (4) Texture compression, compressing the pixels in an image with clearer texture;
[0027] Identify the number of fibers in the image obtained in step (3), divide it into regions that match the number of fibers, calculate the average pixel value of each region, and perform binarization according to the threshold to obtain a texture compressed image. D ( x, y );
[0028] (5) Defect area analysis
[0029] Compressed texture image D ( x, y ) Divide the template image into several regions according to its size, and then compare each region with the target template using the following formula;
[0030]
[0031] in d ( x , y ) is the calculated image, N is the template image, and a threshold for identifying defects is set based on the calculated percentage of defects in each area. d ( x , y ) is compared with the threshold value. If it is higher than the threshold value, the area number is output, and then the part that does not meet the standard after the diaphragm is formed is obtained.
[0032] Compared with the prior art, the present invention has the following advantages:
[0033] The present invention takes a hot diaphragm forming machine as a research object, analyzes the mold surface through equipment such as a laser rangefinder, obtains the basic morphology of the mold, and adjusts the roller device according to the basic morphology to make the overhang of the diaphragm match the concave cavity of the mold. At the same time, the corresponding quality analysis of the formed material is performed through machine vision technology, so that the machine automation level is higher and the material forming is better.
[0034] Based on the above reasons, the present invention can be widely promoted in the fields of thermal diaphragm molding and the like. BRIEF DESCRIPTION OF THE DRAWINGS
[0035] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0036] Figure 1 It is a schematic diagram of the structure of the roller mechanism in a specific implementation manner of the present invention. DETAILED DESCRIPTION
[0037] It should be noted that, in the absence of conflict, the embodiments of the present invention and the features in the embodiments can be combined with each other. The present invention will be described in detail below with reference to the accompanying drawings and in combination with the embodiments.
[0038] In order to make the purpose, technical solutions and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. The following description of at least one exemplary embodiment is actually only illustrative and is by no means intended to limit the present invention and its application or use. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0039] It should be noted that the terms used herein are only for describing specific embodiments and are not intended to limit exemplary embodiments according to the present invention. As used herein, unless the context clearly indicates otherwise, the singular form is also intended to include the plural form. In addition, it should be understood that when the terms "comprising" and / or "including" are used in this specification, it indicates the presence of features, steps, operations, devices, components and / or combinations thereof.
[0040] Unless otherwise specifically stated, the relative arrangement, numerical expressions and numerical values of the parts and steps set forth in these embodiments do not limit the scope of the present invention. Meanwhile, it should be clear that, for ease of description, the sizes of the various parts shown in the accompanying drawings are not drawn according to the actual proportional relationship. The technology, method and equipment known to those of ordinary skill in the relevant art may not be discussed in detail, but in appropriate cases, the technology, method and equipment should be considered as a part of the specification. In all examples shown and discussed here, any specific value should be interpreted as being merely exemplary, rather than as a limitation. Therefore, other examples of exemplary embodiments may have different values. It should be noted that similar reference numerals and letters represent similar items in the following drawings, and therefore, once a certain item is defined in an accompanying drawing, it does not need to be further discussed in subsequent drawings.
[0041] In the description of the present invention, it is necessary to understand that the directions or positional relationships indicated by directional words such as "front, back, up, down, left, right", "lateral, vertical, perpendicular, horizontal" and "top, bottom" are usually based on the directions or positional relationships shown in the drawings. They are only for the convenience of describing the present invention and simplifying the description. Unless otherwise specified, these directional words do not indicate or imply that the device or element referred to must have a specific direction or be constructed and operated in a specific direction. Therefore, they cannot be understood as limiting the scope of protection of the present invention: the directional words "inside and outside" refer to the inside and outside relative to the contours of each component itself.
[0042] For ease of description, spatially relative terms such as "above", "above", "on the upper surface of", "above", etc. may be used here to describe the spatial positional relationship between a device or feature and other devices or features as shown in the figure. It should be understood that spatially relative terms are intended to include different orientations of the device in use or operation in addition to the orientation described in the figure. For example, if the device in the accompanying drawings is inverted, the device described as "above other devices or structures" or "above other devices or structures" will be positioned as "below other devices or structures" or "below their position devices or structures". Thus, the exemplary term "above" may include both "above" and "below". The device may also be positioned in other different ways (rotated 90 degrees or in other orientations), and the spatially relative descriptions used here are interpreted accordingly.
[0043] In addition, it should be noted that the use of terms such as "first" and "second" to limit components is only for the convenience of distinguishing the corresponding components. If not otherwise stated, the above terms have no special meaning and therefore cannot be understood as limiting the scope of protection of the present invention.
[0044] A composite material flexible automatic molding method comprises the following steps:
[0045] S1. placing the mold containing the material in the diaphragm device;
[0046] An automatic conveying device can be used to transport the mold carrying the material to the diaphragm device;
[0047] S2, using hot air to heat the diaphragm in the diaphragm device, and at the same time heat the mold and the material in the mold;
[0048] During the heating process, a temperature sensor is used to timely feedback the temperature, and the diaphragm, mold and material are accurately controlled to reach the preset temperature value based on the feedback temperature, and the error range is accurately controlled within 0.5℃.
[0049] S3, calculating the shape of the mold cavity by a laser rangefinder, and adjusting the diaphragm area corresponding to the mold accordingly;
[0050] The diaphragm area can be adjusted by using a roller mechanism (such as Figure 1 As shown), the roller mechanism adjusts the overhang deformation of the diaphragm in the diaphragm frame according to the shape of the mold cavity, so that the size of the diaphragm used to compact the prepreg is compatible with the prepreg; the roller mechanism includes two groups of rollers, each group of rollers includes two rollers, one of which is an active roller connected to a roller motor, and the other is a driven roller. The diaphragm is located in the gap between the active roller and the driven roller, and the movement is achieved through the cooperation of the active roller and the driven roller, thereby adjusting its overhang deformation in the diaphragm frame.
[0051] S4, after the mold and the diaphragm frame of the diaphragm device are molded together, the mold and the diaphragm frame are fixed by clamping claws;
[0052] The clamping jaws can be electromagnetic clamping jaws, which can make the overall equipment more automated. When designing the clamping jaws, it should be ensured that the taper between the clamping jaws and the clamping block is greater than the Morse taper, so that the strength between them can be guaranteed from a structural point of view.
[0053] S5. Vacuum the space below the diaphragm in blocks according to the shape of the mold;
[0054] The area that needs to be deformed is deformed first by vacuuming in blocks, and the corresponding vacuum holes are opened or closed according to the difficulty of deformation of the diaphragm. The vacuum holes are covered with a polytetrafluoroethylene breathable film to ensure that the vacuum holes will not be blocked by the diaphragm during vacuuming.
[0055] S6, applying positive pressure to the diaphragm from above the diaphragm;
[0056] The pressure of the positive pressure is P, the area of the diaphragm frame is S, and the minimum pressure value F1 that the clamp can withstand should be: F1>P×S+E, where E is the safety factor, and the value of E is determined by the actual situation on site.
[0057] S7. Observe the vacuum degree in the mold cavity and maintain the pressure for 3 minutes;
[0058] S8. Test the material after diaphragm molding. If the material meets the standard, separate the diaphragm frame from the mold and take out the material. If the material does not meet the standard, re-diaphragm mold the material until it meets the standard.
[0059] In step S8, the material is inspected using a machine vision inspection system;
[0060] Specific machine vision inspection systems include:
[0061] (1) Grayscale processing: converting the color image taken by the industrial camera into a grayscale image; grayscale processing can effectively reduce the calculation time and eliminate the influence of light on the image to a certain extent.
[0062] (2) The grayscale image is subjected to histogram equalization and median filtering to obtain image I. Median filtering is often used to filter out impulse noise. It can protect the edge information of the signal while filtering out impulse noise, so that the edge is not blurred.
[0063] (3) The image I obtained in step (2) is filtered by a scale-transformed Gabor filter, and the filtered images in multiple directions are fused to obtain an image with a clearer texture. Texture features can be obtained through a set of multi-channel Gabor filters.
[0064] Gabor filter can well balance the resolution of signals in both spatial and frequency domains.
[0065] The mathematical expression of the two-dimensional Gabor filter function used in this embodiment is:
[0066] Plural expression:
[0067]
[0068] The real part of a complex expression:
[0069]
[0070] Imaginary part of complex expression:
[0071]
[0072] in:
[0073]
[0074]
[0075] Where x, y represent the pixel coordinates, λ represents the wavelength of the filter; (the larger the wavelength, the larger the interval between black and white, θ represents the tilt angle of the Gabor kernel image; ψ represents the phase offset, ranging from -180 to 180; (when ψ=0, the white bar is the center, when ψ=180, the black bar is the center), σ represents the standard deviation of the Gaussian function; (the larger σ, the more stripes), γ represents the aspect ratio, which determines the ellipticity of the Gabor kernel image. (The smaller γ, the higher the kernel image will be)
[0076] Implementation of Gabor filter
[0077] For the defect image of carbon fiber prepreg, after being processed by a set of Gabor filters with different radial center frequencies and different directions, the defects will have different manifestations under the action of different filters. Finally, by fusing the filtering results under different radial center frequencies and different directions into the final processing result, the defects can be clearly highlighted. For the defect image of carbon fiber prepreg obtained by Gabor filter, a Gabor filter group (12 filters in total) with 3 center frequencies (64, 32, 16) and 4 directions (0, 45, 90, 135) is used to process the defect image of carbon fiber prepreg. The process is as follows:
[0078] The image and Gabor filter are converted to the frequency domain using Fourier transform, the discrete Fourier transform of the image is multiplied by the frequency response of the Gabor filter, and then the discrete Fourier inverse transform is performed and the modulus is taken to obtain the filtered result image G, where G is the image I and the filter convolution.
[0079]
[0080] 2) According to the difference between the obtained standard carbon fiber prepreg image and the filtered result image of the sample carbon fiber prepreg image, take its absolute value to obtain the deviation image; then compare the deviation image with the threshold, and assign the deviation image value to 0 when it is less than the threshold, and the deviation image value remains unchanged when it is greater than the threshold, where m 0 is the preset threshold. K(x,y) is the image obtained after convolution.
[0081]
[0082] The deviation images in the four directions are fused, and the fused images are binarized to obtain the carbon fiber prepreg defect detection result image, where Ki (i = 1, 2, 3, 4) (x, y) is the processed image in the four directions, and H (x, y) is the fused image.
[0083]
[0084] (4) Texture compression: compressing the pixels in an image with clearer texture. The structure pattern of the carbon fiber woven prepreg includes a large number of pixels in both the horizontal and vertical fibers. If the calculation is done directly, the amount of calculation is too large. The present invention calculates the average value of the pixels in each bundle of the horizontal and vertical fibers, and replaces the numerous pixels in the bundle with the average value, which can greatly reduce the amount of calculation. The method is as follows:
[0085] According to the number of horizontal and vertical fibers in the image obtained in step (3), the image is divided into regions that match the number of horizontal and vertical fibers, and the average pixel value of each region is calculated. P(x, y) is the image after the average pixel value of H(x, y) is calculated. The texture compressed image is obtained by binarization according to the threshold. D ( x, y );
[0086] The threshold is binarized as follows:
[0087]
[0088] D(x,y) is the pixel point obtained after binarization processing, where m is the average value of the pixel value in each area, τ is the adjustment parameter, and n is the preset threshold;
[0089] (5) Defect area analysis
[0090] The image is divided into several regions according to the size of the template image, and then each region is compared with the target template using the following formula; if the image template in this embodiment is 10*10, then the formula obtained in step (4) is D ( x, y ) is also divided into 10*10, each area is compared with the target template, the defect percentage value is calculated, and this value is compared with the set defect threshold, and then the defect area can be output as follows:
[0091]
[0092] in d ( x , y ) is the calculated image, N is the template image, and a threshold for identifying defects is set based on the calculated percentage of defects in each area. d ( x , y ) are summed up and compared with the sum of the pixels in the image template, and the result is compared with the threshold. If it is higher than the threshold, the area number is output.
[0093] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.
Claims
1. A composite material flexible automated molding method, characterized in that: The steps include: S1. placing the mold containing the material in the diaphragm device; S2, using hot air to heat the diaphragm in the diaphragm device, and at the same time heat the mold and the material in the mold; S3. Calculate the shape of the mold cavity by a laser rangefinder, and adjust the diaphragm area corresponding to the mold accordingly; the diaphragm area is adjusted by a roller mechanism, and the roller mechanism adjusts the drape deformation of the diaphragm in the diaphragm frame according to the shape of the mold cavity, so that the size of the diaphragm used to compact the prepreg is compatible with the prepreg; the roller mechanism includes two groups of rollers, each group of rollers includes two rollers, one of which is an active roller connected to a roller motor, and the other is a driven roller. The diaphragm is located in the gap between the active roller and the driven roller, and the movement is achieved through the cooperation of the active roller and the driven roller, thereby adjusting its drape deformation in the diaphragm frame; S4, after the mold and the diaphragm frame of the diaphragm device are molded together, the mold and the diaphragm frame are fixed by clamping claws; S5. Vacuum the space below the diaphragm in blocks according to the shape of the mold; The area that needs to be deformed is deformed first by vacuuming the air in blocks, and the vacuum holes corresponding to the area are opened or closed according to the difficulty of deformation of the diaphragm; S6. Apply positive pressure to the diaphragm above the diaphragm; the pressure of the positive pressure is P, the area of the diaphragm frame is S, and the minimum pressure value F1 that the clamp can withstand should meet the following conditions: F1>P×S+E, where E is the safety factor, and the value of E is determined by the actual situation on site; S7. Observe the vacuum degree in the mold cavity and maintain the pressure for 3 minutes; S8. Test the material after diaphragm molding. If the material meets the standard, separate the diaphragm frame from the mold and take out the material. If the material does not meet the standard, re-diaphragm mold the material until it meets the standard.
2. A composite material flexible automated molding method according to claim 1, characterized in that: In step S2, a temperature sensor is used to timely feedback the temperature, and the diaphragm, mold and material are accurately controlled to reach a preset temperature value according to the feedback temperature, and the error range is accurately controlled within 0.5°C.
3. A composite material flexible automated molding method according to claim 1, characterized in that: The air-exhaust hole is covered by a polytetrafluoroethylene breathable film to ensure that the air-exhaust hole will not be blocked by the diaphragm during air extraction.
4. A composite material flexible automated molding method according to claim 1, characterized in that: In step S8, the material is inspected using a machine vision inspection system; Furthermore, the specific machine vision inspection system includes: (1) Grayscale processing: converting the color image taken by the industrial camera into a grayscale image; (2) Perform histogram equalization and median filtering on the grayscale image; (3) The image obtained in step (2) is filtered using a Gabor filter based on scale transformation, and the filtered images in multiple directions are fused to obtain an image with clearer texture. (4) Texture compression, compressing the pixels in an image with clearer texture; Identify the number of fibers in the image obtained in step (3), divide it into regions that match the number of fibers, calculate the average pixel value of each region, and perform binarization according to the threshold to obtain a texture compressed image. D ( x,y ); (5) Defect area analysis Compressed texture image D ( x,y ) Divide the template image into several regions according to its size, and then compare each region with the target template using the following formula; in d ( x , y ) is the calculated image, N is the template image, and a threshold for identifying defects is set based on the calculated percentage of defects in each area. d ( x , y ) is compared with the threshold value. If it is higher than the threshold value, the area number is output, and then the part that does not meet the standard after the diaphragm is formed is obtained.