A strontium-rich soil conditioner and its preparation method and application
By using the skeleton material formed by calcining mussel shells from different temperatures and aqueous strontium chloride solution, a strontium rich soil conditioner was prepared, which solved the problem of high concentration of strontium in tea trees to inhibit calcium absorption, and achieved stable and high yields of tea and soil improvement.
Patent Information
- Application Number
- CN202211539114.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-12-01
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2042-12-01
AI Technical Summary
During the cultivation of strontium-rich tea, tea trees inhibit calcium absorption due to the absorption of high concentration of strontium, resulting in limited plant growth and problems such as soil slab formation and acidification are difficult to solve.
Mussel shells are crushed and calcined at different temperatures to form a variety of skeleton materials, combined with strontium chloride aqueous solution for strontium sustained release, synchronous release of calcium elements, forming a strontium-rich soil conditioner, used for tea tree soil improvement, alleviating plate bonding, acidification and heavy metal pollution .
The continuous, slow and quantitative absorption of strontium by tea trees is achieved, the antagonistic effect of strontium on calcium is avoided, the quality and yield of tea is improved, and the soil structure and environment are improved.
Smart Images

Figure BDA0003976360940000091
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of soil conditioning, and in particular to a strontium-enriched soil conditioner and a preparation method and application thereof. Background Art
[0002] Strontium is one of the 14 essential trace elements for humans and animals. It has physiological effects such as preventing tooth decay, stimulating bone formation, treating osteoporosis, preventing cardiovascular diseases and atherosclerosis. The optimal daily intake of strontium for the human body is 2.0 mg / kg. The strontium content in most foods is very low. The strontium content in meat, potatoes, fruits and dairy products is less than 1 mg / kg. The strontium content in root vegetables and seafood is slightly higher, about 1-4 mg / kg. At present, people mainly supplement strontium through strontium-containing mineral water or strontium-containing drugs. Adding strontium-containing soil conditioners is one of the effective ways to increase the strontium content in food, but the research and development of strontium-containing soil conditioners has not been reported.
[0003] Tea is one of the three major beverages in the world, and more than 2 billion people drink tea worldwide. Cultivating strontium-enriched tea will be an important way to enrich the variety of strontium-enriched foods. The nutrient content in the tea tree soil will have a significant impact on the growth of tea trees and the quality of tea. Therefore, improving the soil and creating a strontium-containing environment is a key link in achieving the cultivation and production of strontium-enriched tea.
[0004] Studies have shown that low concentrations of strontium can promote plant growth and increase the nutritional value and yield of crops. Low concentrations of strontium promote plant growth mainly by increasing plants' tolerance to CO 2 This is achieved by increasing the fixation capacity of calcium, accelerating the electron transfer and photosynthetic oxygen release of PSII, and improving the photosynthetic efficiency of plants. However, high concentrations of strontium will inhibit the absorption of calcium by plants, reduce the calcium content in plant cell walls, and thus inhibit plant growth. Summary of the invention
[0005] The purpose of the present invention is to solve the key problems encountered in the cultivation process of strontium-enriched tea, and to provide a strontium-enriched soil conditioner and a method for using the same. The soil conditioner has the function of continuously, slowly and quantitatively releasing the strontium element, and can also release the calcium element synchronously, so as to avoid the tea tree antagonizing calcium due to strontium absorption. In addition, the conditioner can also alleviate the functions of soil compaction, acidification, heavy metal pollution, etc. The soil conditioner has low cost and is easy to use. In addition to being used for tea tree cultivation, it can also be used for strontium-enriched cultivation of other crops by adjusting the dosage.
[0006] To achieve the above object, the technical solution adopted by the present invention is:
[0007] In a first aspect, the present invention provides a method for preparing a strontium-enriched soil conditioner, the method comprising the following steps:
[0008] (1) crushing mussel shells to obtain mussel shell powder;
[0009] (2) calcining the mussel shell powder obtained in step (1) at 300-400°C (e.g., 310°C, 320°C, 330°C, 340°C, 350°C, 360°C, 370°C, 380°C, 390°C) to obtain a mussel shell skeleton a, calcining the mussel shell powder obtained in step (1) at 500-700°C (e.g., 525°C, 550°C, 575°C, 600°C, 625°C, 650°C, 675°C) to obtain a mussel shell skeleton b, and calcining the mussel shell powder obtained in step (1) at 800-1000°C (e.g., 825°C, 850°C, 875°C, 900°C, 925°C, 950°C, 975°C) to obtain a mussel shell skeleton c;
[0010] (3) After the mussel shell skeleton b obtained in step (2) is crushed, KHCO is added 3 , mixed and then calcined to obtain mussel shell skeleton d;
[0011] (4) immersing the mussel shell skeleton d obtained in step (3) in an aqueous solution of strontium chloride, and then drying and calcining in sequence to obtain a strontium sustained-release agent;
[0012] (5) Take the mussel shell skeleton a and mussel shell skeleton c obtained in step (2) and the strontium sustained-release agent obtained in step (4), and mix them in a mass ratio of the mussel shell skeleton a: the mussel shell skeleton c: the strontium sustained-release agent of (1-3):(1-2):1 (for example, 1.5:1.5:1, 2:1.5:1, 2.5:1.5:1) to obtain the strontium-rich soil conditioner.
[0013] In the present invention, mussel shells are used as raw materials. Compared with other types of shells, mussel shells have a higher organic matter content. After calcination, a mussel shell skeleton material with relatively higher porosity can be obtained. The present invention also uses strontium chloride with better water solubility as a source of strontium. Through the above step (4), while strontium is fixed on the mussel shell skeleton d, the organic matter in the mussel shell skeleton d is further volatilized, and the mussel shell skeleton d is activated and modified.
[0014] In the above-mentioned method for preparing the strontium-enriched soil conditioner, as a preferred embodiment, in step (1), the mussel shells are first washed with tap water to remove the mud and sand, and then dried in the sun, and then crushed.
[0015] In the preparation method of the above-mentioned strontium-enriched soil conditioner, as a preferred embodiment, in step (2), the calcination is carried out in a muffle furnace; preferably, the calcination is carried out in an inert gas; preferably, the inert gas is nitrogen; preferably, the calcination temperature is 500-700°C (for example, 525°C, 550°C, 575°C, 600°C, 625°C, 650°C, 675°C), and the calcination time is 2-5 hours (for example, 2.5 hours, 3 hours, 3.5 hours, 4 hours, 4.5 hours).
[0016] In the present invention, oxygen-free calcination can retain elements such as C, N, and S in the shells, which play an important role in the functional groups on the pore surface of the material.
[0017] In the preparation method of the strontium-rich soil conditioner, as a preferred embodiment, in step (3), the mussel shell skeleton b is crushed, sieved and then KHCO is added to the sieved material. 3 Preferably, the KHCO 3 The specification is chemically pure; preferably, the sieving is through a 100-mesh sieve; preferably, the mussel shell skeleton b and KHCO 3 The mass ratio of is (0.9-1.1):1, more preferably 1:1; preferably, the calcination temperature in step (3) is 500-700°C (e.g., 525°C, 550°C, 575°C, 600°C, 625°C, 650°C, 675°C); preferably, the calcination time in step (3) is 1-3h (e.g., 1.5h, 2h, 2.5h); preferably, the calcination is carried out in a tubular furnace.
[0018] In the present invention, KHCO 3 As an activator / pore former, it can further form pores in the organic framework through the volatilization of potassium. KHCO 3 If the dosage is too small, the porosity will be insufficient, affecting the sustained release effect. If the dosage is too large, the reaction efficiency will be reduced.
[0019] In the preparation method of the above-mentioned strontium-rich soil conditioner, as a preferred embodiment, in step (4), the concentration of the strontium chloride aqueous solution is 20-60mmol / L (for example, 25mmol / L, 30mmol / L, 35mmol / L, 40mmol / L, 45mmol / L, 50mmol / L, 55mmol / L); preferably, the impregnation adopts an equal volume impregnation method; preferably, the amount of the mussel shell skeleton d and the strontium chloride aqueous solution is a volume ratio of 1:1; preferably, the impregnation time is 12-24 hours (for example, 13 hours, 14 hours, 15 hours, 16 hours, 17 hours, 18 hours, 19 hours, 20 hours, 21 hours, 22 hours, 23 hours, 24 hours, 25 hours, 26 hours, 27 hours, 28 hours, 29 hours, 30 hours, 31 hours, 32 hours, 33 hours, 34 hours, 35 hours, 36 hours, 37 hours, 38 hours, 39 hours, 40 hours, 41 hours, 42 hours, 43 hours, 44 hours, 45 hours, 46 hours, 47 hours, 48 hours, 49 hours, 50 hours, 51 hours, 52 hours, 53 hours, 54 hours, 55 hours, 56 hours, 57 hours, 58 hours, 59 hours, 60 hours, 61 hours, 62 hours, 63 hours, 64 hours, 65 hours, 66 hours, 67 hours, 68 hours, 69 hours, 70 hours, 71 hours, 72 hours, 73 hours, 74 hours, 75 hours, 76 hours, 77 hours, 78 hours, 79 hours, 80 hours, 8 8 hours, 19 hours, 20 hours, 21 hours, 22 hours, 23 hours); preferably, the drying temperature is 80-120°C (for example 85°C, 90°C, 95°C, 100°C, 105°C, 110°C, 105°C); preferably, the calcination is carried out in a tube furnace; preferably, the calcination is carried out in an inert gas; preferably, the inert gas is nitrogen; preferably, the calcination temperature is 200-400°C (for example 250°C, 300°C, 350°C, 380°C); preferably, the calcination time is 1-4 hours (for example 1.5 hours, 2 hours, 2.5 hours, 3 hours, 3.5 hours).
[0020] In a second aspect, the present invention provides a strontium-rich soil conditioner prepared by the above preparation method.
[0021] The third invention provides the use of the above-mentioned strontium-enriched soil conditioner in the cultivation of strontium-enriched crops.
[0022] In the above application, as a preferred embodiment, the crop is tea tree.
[0023] In the above application, as a preferred embodiment, the method of the application is:
[0024] Digging trenches between rows of tea trees to a depth of 20-40 cm (e.g., 25 cm, 30 cm, 35 cm), and applying the strontium-rich soil conditioner into the trenches;
[0025] Alternatively, the application method is: mixing the strontium-rich soil conditioner with water in a mass ratio of 1:(10-50) (for example, 1:15, 1:20, 1:25, 1:30, 1:35, 1:40, 1:45) to prepare a strontium-rich soil conditioner suspension and spraying it on the soil at the roots of tea trees.
[0026] In the above application, as a preferred embodiment, the conditioning agent is used 2-3 months before each tea tree budding period.
[0027] In the present invention, after the tea leaves are harvested after the first use of the conditioner, the conditioner can be reused before the next harvesting season (2-3 months before the budding period of the tea trees), and the application method is the same as the first application method. It is applied 4-6 times a year to obtain strontium-rich tea leaves with stable quality.
[0028] In the above application, as a preferred embodiment, the usage of the strontium-rich conditioner is 30-60 kg / mu (for example, 35 kg / mu, 40 kg / mu, 45 kg / mu, 50 kg / mu, 55 kg / mu).
[0029] The strontium-rich soil conditioner mentioned in the present invention has the following characteristics:
[0030] (1) The mussel shells were carbonized (calcined) at different temperatures to effectively retain the organic skeleton and calcium skeleton in the mussel shells. After being treated at different temperatures, they also had different compositions and functions. When carbonized at 300-400℃, the organic matter in the mussel shells thermally denatured and decomposed to form an organic-calcium carbonate skeleton material, which can effectively alleviate soil compaction, increase soil porosity, and adsorb soil heavy metals; at 500-700℃, the calcium carbonate in the mussel shells thermally denatured and decomposed to form an organic-calcium carbonate-calcium oxide skeleton material. The material has rich and uniform pores and can serve as a good slow-release carrier for strontium; after carbonization at 800-1000℃, the mussel shells mainly become organic-calcium oxide skeleton materials, which can adjust soil pH, slow down acidification, provide calcium ions, increase soil cation exchange capacity, and passivate heavy metals in the soil. After mixing the above three materials, a complete functional system with multiple functions can be formed.
[0031] (2) Mussel shells contain a variety of trace metal elements, such as K, Na, Zn, Mn, Fe, Sr, Mg, etc., which can provide trace metal ions from the ocean for plant growth and promote growth.
[0032] (3) Strontium-rich soil conditioners have the function of slow-release strontium. Strontium exists in the pores of shell skeleton materials. With watering and the passage of time, strontium and calcium in shell skeleton materials slowly dissociate into the soil and can be gradually absorbed by plants. The slow-release function can avoid the stress of high strontium concentration in the soil environment on plant growth, and also avoid the inhibition of calcium absorption by plants by high strontium concentration. DETAILED DESCRIPTION
[0033] In order to make the purpose, technical scheme and advantages of the present invention clearer, the technical scheme in the embodiment of the present invention will be clearly and completely described in conjunction with the embodiments of the present invention. It should be understood by those skilled in the art that the embodiments are only to help understand the present invention and should not be regarded as specific limitations of the present invention. Based on the embodiments in the present invention, all other embodiments obtained by ordinary technicians in the field without making creative work are within the scope of protection of the present invention.
[0034] The embodiments of the present invention are implemented on the premise of the technical solution of the present invention, and detailed implementation methods and processes are given, but the protection scope of the present invention is not limited to the following embodiments. The process parameters of the following embodiments that do not specify specific conditions are usually based on conventional conditions.
[0035] The endpoints and any values of the ranges disclosed in the present invention are not limited to the precise ranges or values, and these ranges or values should be understood to include values close to these ranges or values. For numerical ranges, the endpoint values of each range, the endpoint values of each range and the individual point values, and the individual point values can be combined with each other to obtain one or more new numerical ranges, which should be regarded as specifically disclosed in the present invention.
[0036] The following examples are provided to facilitate a better understanding of the present invention, but are not intended to limit the present invention. The experimental methods in the following examples are conventional methods unless otherwise specified. The experimental materials used in the following examples are purchased from conventional chemical reagent companies unless otherwise specified. The quantitative tests in the following examples were repeated three times, and the results were averaged.
[0037] The content and effect of the strontium-enriched soil conditioner and the use method thereof of the present invention are further described by specific examples. The following examples are only used to illustrate the content of the present invention and are not used to limit the protection scope of the present invention.
[0038] The tea tree varieties used in the embodiments of the present invention are: Taishun high mountain tea, 5 years old;
[0039] Soil pH was measured using a pH meter (water / soil = 2.5 / 1);
[0040] Strontium content was determined by atomic absorption spectrometry;
[0041] Chlorophyll content determination: After chlorophyll is extracted with acetone, it is detected and calculated using a spectrophotometer;
[0042] The total activity of SOD was determined by the nitroblue tetrazolium method, the total activity of POD was determined by the guaiacol method; the content of tea polyphenols was determined by ultraviolet spectrophotometry.
[0043] Example 1
[0044] The mussel shells were washed with tap water, and after removing the mud and sand, they were dried, crushed, and divided into three equal parts. They were calcined in a muffle furnace at 300°C, 500°C, and 800°C, respectively, and high-purity nitrogen was introduced. The calcinations were carried out for 3 hours to obtain mussel shell skeleton a, mussel shell skeleton b, and mussel shell skeleton c.
[0045] Take mussel shell skeleton b, according to mussel shell skeleton b: KHCO 3 At a mass ratio of 1:1, add KHCO 3 After mixing, the mixture was calcined in a tubular furnace at a temperature of 600°C for 2 hours to obtain a mussel shell skeleton d.
[0046] The mussel shell skeleton d was immersed in a 20 mmol / L strontium chloride solution for 12 h at a volume ratio of 1:1. After the immersion, it was dried at 100 °C and then transferred to a tube furnace for drying at N 2 Under atmospheric conditions, the strontium sustained-release agent was obtained by calcining at 200°C for 2 hours without oxygen.
[0047] The mussel shell skeleton a, the mussel shell skeleton c and the prepared strontium slow-release agent were mixed in a mass ratio of 1:1:1 to obtain a strontium-rich soil conditioner.
[0048] Two months before tea picking (two months before the tea trees germinate), prepare a strontium-rich soil conditioner suspension in a mass ratio of 1:10 between strontium-rich conditioner and water. Spray the strontium-rich soil conditioner suspension onto the soil at the roots of the tea trees at an application rate of 50 kg / mu (i.e. 550 kg / mu of strontium-rich soil conditioner suspension), and wait for tea to be picked two months later.
[0049] Example 2
[0050] The mussel shells were washed with tap water, and after removing the mud and sand, they were dried, crushed, and divided into three equal parts. They were calcined in a muffle furnace at 300°C, 500°C, and 800°C, respectively, and high-purity nitrogen was introduced. The calcinations were carried out for 3 hours to obtain mussel shell skeleton a, mussel shell skeleton b, and mussel shell skeleton c.
[0051] Take mussel shell skeleton b, according to mussel shell skeleton b: KHCO 3 At a mass ratio of 1:1, add KHCO 3 After mixing, the mixture was calcined in a tubular furnace at a temperature of 600°C for 2 hours to obtain a mussel shell skeleton d.
[0052] The mussel shell skeleton d was immersed in a 40 mmol / L strontium chloride solution for 12 h at a volume ratio of 1:1. After the immersion, it was dried at 100 °C and then transferred to a tube furnace for drying at N 2 Under atmospheric conditions, the strontium sustained-release agent was obtained by calcining at 200°C for 2 hours without oxygen.
[0053] The mussel shell skeleton a, the mussel shell skeleton c and the prepared strontium slow-release agent were mixed in a mass ratio of 1:1:1 to obtain a strontium-rich soil conditioner.
[0054] Two months before tea picking (two months before the tea trees germinate), prepare a strontium-rich soil conditioner suspension in a mass ratio of 1:10 between strontium-rich conditioner and water. Spray the strontium-rich soil conditioner suspension onto the soil at the roots of the tea trees at an application rate of 50 kg / mu (i.e. 550 kg / mu of strontium-rich soil conditioner suspension), and wait for tea to be picked two months later.
[0055] Example 3
[0056] The mussel shells were washed with tap water, and after removing the mud and sand, they were dried, crushed, and divided into three equal parts. They were calcined in a muffle furnace at 400°C, 700°C, and 1000°C, respectively, and high-purity nitrogen was introduced. The calcinations were carried out for 4 hours to obtain mussel shell skeleton a, mussel shell skeleton b, and mussel shell skeleton c.
[0057] Take mussel shell skeleton b, according to mussel shell skeleton b: KHCO 3 At a mass ratio of 1:1, add KHCO 3 After mixing, the mixture was calcined in a tubular furnace at a temperature of 600°C for 2 hours to obtain a mussel shell skeleton d.
[0058] The mussel shell skeleton d was immersed in a 40 mmol / L strontium chloride solution for 12 h at a volume ratio of 1:1 to the strontium chloride aqueous solution. After the immersion, it was dried at 100 °C and then transferred to a tube furnace for drying at N 2 Under atmospheric conditions, the strontium sustained-release agent was obtained by calcining at 400°C for 2 hours without oxygen.
[0059] The mussel shell skeleton a, the mussel shell skeleton c and the prepared strontium slow-release agent were mixed in a mass ratio of 2:1:1 to obtain a strontium-rich soil conditioner.
[0060] Two months before tea picking (two months before the tea trees germinate), prepare a strontium-rich conditioner suspension according to a mass ratio of 1:20 between strontium-rich conditioner and water. Spray the strontium-rich soil conditioner suspension onto the soil at the roots of the tea trees at an application rate of 50 kg / mu (that is, 1050 kg / mu of strontium-rich soil conditioner suspension), and wait for tea to be picked two months later.
[0061] Example 4
[0062] The mussel shells were washed with tap water, and after removing the mud and sand, they were dried, crushed, and divided into three equal parts. They were calcined in a muffle furnace at 400°C, 700°C, and 1000°C, respectively, and high-purity nitrogen was introduced. The calcinations were carried out for 4 hours to obtain mussel shell skeleton a, mussel shell skeleton b, and mussel shell skeleton c.
[0063] Take mussel shell skeleton b, according to mussel shell skeleton b: KHCO 3 At a mass ratio of 1:1, add KHCO 3 After mixing, the mixture was calcined in a tubular furnace at a temperature of 600°C for 2 hours to obtain a mussel shell skeleton d.
[0064] The mussel shell skeleton d was immersed in a 40 mmol / L strontium chloride solution for 12 h at a volume ratio of 1:1 to the strontium chloride aqueous solution. After the immersion, it was dried at 100 °C and then transferred to a tube furnace for drying at N 2 Under atmospheric conditions, the strontium sustained-release agent was obtained by calcining at 400°C for 2 hours without oxygen.
[0065] The mussel shell skeleton a, the mussel shell skeleton c and the prepared strontium slow-release agent were mixed in a mass ratio of 2:1:1 to obtain a strontium-rich soil conditioner.
[0066] Two months before tea picking (two months before the tea trees germinate), dig furrows between the rows of tea trees with a depth of 30 cm. Apply strontium-rich soil conditioner powder at a rate of 50 kg / mu into the furrows and turn the soil over appropriately. The tea leaves can be picked two months later.
[0067] Comparative Example 1
[0068] The mussel shells were washed with tap water, and after removing the mud and sand, they were dried, crushed, and divided into three equal parts. They were calcined in a muffle furnace at 400°C, 700°C, and 1000°C, respectively, and high-purity nitrogen was introduced. The calcinations were carried out for 4 hours to obtain mussel shell skeleton a, mussel shell skeleton b, and mussel shell skeleton c.
[0069] The improver does not add strontium chloride, and directly mixes mussel shell skeleton a, mussel shell skeleton b and mussel shell skeleton c in a mass ratio of 2:1:1 to prepare the soil conditioner.
[0070] Two months before tea picking (two months before the tea trees germinate), prepare a soil conditioner suspension by suspending the soil conditioner in water at a mass ratio of 1:20. Spray the soil conditioner suspension onto the soil at the roots of the tea trees at an application rate of 50 kg / mu (that is, 1050 kg / mu of soil conditioner suspension), and wait for tea to be picked two months later.
[0071] A blank control group was set up at the same time, and no soil conditioner was applied. Other growth conditions were consistent with those in Example 3 and Control Example 1.
[0072] Comparative Example 2
[0073] This comparative example is basically the same as Example 2, the only difference being that the concentration of the strontium chloride solution in this comparative example is 80 mmol / L, and the strontium content of the strontium-rich soil conditioner prepared in this comparative example is too high, which inhibits the growth of tea trees, resulting in a tea yield of 9 kg / mu using the strontium-rich soil conditioner in this comparative example.
[0074] Comparative Example 3
[0075] The strontium sustained-release agent prepared in Example 2 was used as a strontium-rich soil conditioner. Two months before tea picking, a strontium-rich soil conditioner suspension was prepared according to a mass ratio of 1:10 between the strontium-rich conditioner and water. The strontium-rich soil conditioner suspension was sprayed onto the soil at the roots of the tea trees at an application rate of 16.67 kg / mu (i.e., 183.37 kg / mu of strontium-rich soil conditioner). Tea leaves were picked two months later.
[0076] The strontium-rich soil conditioner in this comparative example does not contain mussel shell skeleton a or mussel shell skeleton c. Instead, the strontium sustained-release agent is directly diluted as a strontium-rich conditioner and then sprayed on the roots of the tea trees. Compared with the soil conditioner in Example 2 to which mussel shells carbonized (calcined) at different temperatures are added, this comparative example only contains mussel shells treated at a single temperature, which results in a decrease in the sustained-release ability of the strontium-rich soil conditioner and a reduction in the absorption efficiency of the tea trees for the strontium element.
[0077] The soil pH of each group of tea trees in the above Examples 1-4 and Comparative Examples 1-3, and the strontium content, chlorophyll content, POD activity, SOD activity, tea polyphenol content and tea yield in the picked tea leaves are shown in Table 1 below.
[0078] Table 1 Effects of conditioners on soil pH, strontium content in tea leaves and physiological indicators
[0079]
[0080] Finally, it should be noted that the above are only preferred embodiments of the present invention and are not intended to limit the present invention. Although the present invention has been described in detail with reference to the embodiments, it is still possible for those skilled in the art to modify the technical solutions described in the aforementioned embodiments or to replace some of the technical features therein with equivalents. However, any modifications, equivalent replacements, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A method for preparing a strontium-rich soil conditioner, It is characterized in that The method comprises the following steps in sequence: (1) crushing mussel shells to obtain mussel shell powder; (2) calcining the mussel shell powder obtained in step (1) at 300-400° C. to obtain a mussel shell skeleton a, calcining the mussel shell powder obtained in step (1) at 500-700° C. to obtain a mussel shell skeleton b, and calcining the mussel shell powder obtained in step (1) at 800-1000° C. to obtain a mussel shell skeleton c; the calcinations are all carried out in an inert gas, wherein the inert gas is nitrogen; and the calcinations are all carried out for 2-5 hours; (3) After the mussel shell skeleton b obtained in step (2) is crushed, KHCO is added 3 , mixing and calcining to obtain a mussel shell skeleton d; the calcination temperature is 500 to 700° C.; the calcination time is 1 to 3 hours; (4) immersing the mussel shell skeleton d obtained in step (3) in an aqueous solution of strontium chloride, and then drying and calcining in sequence to obtain a strontium sustained-release agent; the calcination is carried out in an inert gas, which is nitrogen; the calcination temperature is 200 to 400° C., and the calcination time is 1 to 4 hours; (5) Take the mussel shell skeleton a and mussel shell skeleton c obtained in step (2) and the strontium sustained-release agent obtained in step (4), and mix them in a mass ratio of (1-3): (1-2): 1 to obtain the strontium-rich soil conditioner.
2. The preparation method according to claim 1, It is characterized in that In step (1), the mussel shells are first washed with tap water, the sand is removed, the shells are dried, and then crushed; In step (2), the calcination is carried out in a muffle furnace; In step (3), the mussel shell skeleton b is crushed, sieved and then KHCO is added to the sieved material. 3 ; In step (3), the KHCO 3 The specification is chemically pure; In step (3), the mussel shell skeleton b and KHCO 3 The mass ratio is (0.9~1.1):1; In step (3), the calcination is carried out in a tubular furnace; In step (4), the concentration of the strontium chloride aqueous solution is 20 to 60 mmol / L; In step (4), the impregnation adopts an equal volume impregnation method; In step (4), the volume ratio of the mussel shell skeleton d to the strontium chloride aqueous solution is 1:1; In step (4), the immersion time is 12 to 24 hours; In step (4), the drying temperature is 80 to 120° C. In step (4), the calcination is carried out in a tubular furnace.
3. The preparation method according to claim 2, It is characterized in that In step (3), the sieving is through a 100-mesh sieve; And / or, in step (3), the mussel shell skeleton b and KHCO 3 The mass ratio is 1:
1.
4. A strontium-rich soil conditioner prepared by the preparation method according to any one of claims 1 to 3.
5. Use of the strontium-enriched soil conditioner according to claim 4 or the preparation method according to any one of claims 1 to 3 in the cultivation of crops enriched with strontium.
6. The use according to claim 5, It is characterized in that The crop is tea tree.
7. The use according to claim 6, It is characterized in that The application method is as follows: digging trenches between rows of tea trees with a depth of 20-40 cm, and applying the strontium-rich soil conditioner into the trenches; Alternatively, the application method is: mixing the strontium-rich soil conditioner with water in a mass ratio of 1:(10-50) to prepare a strontium-rich soil conditioner suspension, and spraying the suspension on the soil at the roots of tea trees.
8. The use according to claim 7, It is characterized in that The conditioning agent is used 2 to 3 months before each tea tree budding period.
9. The use according to any one of claims 5 to 8, It is characterized in that The usage of the strontium-rich conditioner is 30 to 60 kg / mu.