A 222 nanometer excimer light board and its manufacturing method

By setting the dielectric plate and coval alloy dam in parallel, combining mesh or plate-shaped electrodes and optical filter membranes, the radiation uneven and life problems of existing DBD excimer lamps are solved, achieving an efficient and low-cost 222 nanometers Ultraviolet luminescent tablet, suitable for a variety of application scenarios.

CN116053112BActive Publication Date: 2024-11-01SUNNYVALE NEW MATERIAL TECH (NANJING) CO LTD
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
CN202211642817.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-12-20
Publication Date
2024-11-01
Estimated Expiration
2042-12-20

AI Technical Summary

Technical Problem

The existing 222-nanometer DBD excimer lamps are mostly designed in the shape of a lamp tube, resulting in uneven radiation intensity and it is difficult to create non-circular luminescent flat plates, affecting the application scenarios and life of the equipment.

Method used

Using parallel dielectric plates, the edges of the two dielectric plates are sealed and connected by a Kva alloy dam to form a cavity for discharge gas, and a mesh or plate-shaped electrode is provided on the surface of the dielectric plate, and an optical filter membrane is added to achieve uniform radiation. and improve lifespan.

Benefits of technology

It realizes a 222-nanometer excimer lamp plate with uniform irradiation intensity and high life. It has a simple process and low cost. It can produce luminescent flat plates of any shape, avoiding ozone production and enhancing the applicability and reliability of the equipment.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116053112B_ABST
    Figure CN116053112B_ABST
Patent Text Reader

Abstract

The present invention provides a 222-nanometer excimer lamp panel and a manufacturing method thereof. A 222-nanometer excimer lamp panel includes parallel dielectric plates, the dielectric plates are capable of transmitting 222-nanometer ultraviolet light; two opposite inner surfaces of the dielectric plates are provided with a tempered layer; the edges of the two dielectric plates are sealed and connected by a dam to form a cavity for accommodating discharge gas, and a vent is provided on the side wall of the dam; the outer surface of at least one dielectric plate is provided with a mesh electrode for emitting 222-nanometer ultraviolet light, and the outer surface of the dielectric plate for light transmission is plated with an optical filter film for filtering light with a wavelength other than 222 nanometers. The present invention adopts a lamp panel structure that is more likely to produce a uniform irradiation intensity effect, and the process of manufacturing electrodes on the lamp panel is simple and low-cost; the manufacturing process of the closed discharge cavity formed by the dielectric plate and the dam is highly controllable; the tempering treatment of the inner surface of the dielectric plate increases the life of the excimer lamp.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of ultraviolet sterilization and relates to a 222 nanometer excimer lamp panel and a manufacturing method thereof. Background Art

[0002] Currently, there is a demand for killing bacteria and viruses. Ultraviolet rays, especially the UVC band (100-280 nanometers), destroy the molecular structure of DNA (deoxyribonucleic acid) or RNA (ribonucleic acid) of bacteria or viruses, causing growth death and / or regenerative death, thereby killing bacteria and viruses. The purine and pyrimidine rings of nucleic acid molecules contain conjugated double bonds, which have strong absorption in the ultraviolet band of 240 to 280 nanometers, with the maximum absorption value near 260 nanometers.

[0003] However, ultraviolet radiation with a wavelength of around 260 nanometers is harmful to the human body, especially the eyes. Recent studies have shown that ultraviolet light of 222 nanometers is harmless to the human body and eyes. The basic principle of harmlessness is that the shorter the wavelength of ultraviolet light, the shallower its penetration depth into human skin. At a wavelength of 222 nanometers, ultraviolet radiation can only penetrate the stratum corneum on the surface of the skin, causing no harm to the human body, but can penetrate bacteria and viruses on the stratum corneum. Experimental data from multiple scientific research units show that 222-nanometer ultraviolet radiation can kill bacteria and viruses but does not harm the eyes of mice (David Welch, Manuela Buonanno, Veljko Grilj, Igor Shuryak, Connor Crickmore, Alan W. Bigelow, Gerhard Randers-Pehrson, Gary W. Johnson & David J. Brenner, "Far-UVC light: A new tool to control the spread of airborne-mediated microbial diseases", Scientific Reports | (2018) 8:2752 | DOI:10.1038 / s41598-018-21058-w., Nozomi Yamano, Makoto Kunisada1 , Sachiko Kaidzu, Kazunobu Sugihara, Aiko Nishiaki-Sawada, Hiroyuki Ohashi, Ai Yoshioka, Tatsushi Igarashi, Akihiro Ohira, Masaki Tanito and Chikako Nishigori, "Long-term Effects of 222-nm Ultraviolet Radiation C Sterilizing Lamps on Mice Susceptible to Ultraviolet Radiation",Photochemistry and Photobiology, 2020, 96: 853–862., Manuela Buonanno, BrianPonnaiya, David Welch, Milda Stanislauskas, Gerhard, Randers-Pehrson, Lubomir Smilenov, Franklin D. Lowy. David M.Owens, and David J. Brenner, "Germicidal Efficacy and Mammalian Skin Safety of 222-nm UV Light", RadiatRes. 2017 April ; 187(4): 483–491. doi:10.1667 / RR0010CC.1.), so the 222-nm ultraviolet radiation sterilization and virus removal device is considered to be able to "coexist with humans and machines". .

[0004] A device that produces ultraviolet radiation with a wavelength of 222 nanometers is a krypton chloride excimer lamp. One of the two components of the excimer is an inert element (here krypton). In the plasma state, that is, when electrons collide, the inert element is ionized, and the ionized inert element and the other component of the excimer, the halogen atom (here chlorine), form an excimer. The spontaneous decay of the excimer produces ultraviolet radiation. The ultraviolet radiation of the excimer is generally single-wavelength, and the wavelength of the krypton chloride excimer lamp here is 222 nanometers.

[0005] The common method for ionizing a mixture of chlorine and krypton is dielectric barrier discharge (DBD). In the structure of a DBD excimer lamp, there is a dielectric isolation between the electrode and the discharge gas, and the electrode does not directly contact the active discharge gas, thereby avoiding corrosion of the electrode by the discharge gas and contamination of the discharge gas by the electrode material. Compared with other methods of exciting and generating excimers, the DBD structure greatly increases the life of the excimer lamp.

[0006] At present, 222nm DBD excimer lamps are all in the form of lamp tubes. US 7800308B2 discloses an excimer lamp, which is composed of a single sealed circular lamp tube filled with luminescent gas, and two or three electrodes are arranged on the outside of the lamp tube. The high frequency and high voltage between the electrodes cause the luminescent gas in the lamp tube cavity to ionize and emit light. However, such a design, because the lamp tube is circular, the distance between the two electrodes attached to the outside of the lamp tube is inconsistent, and the discharge effect is uneven.

[0007] CN 213294766 and CN 213698044 use a sleeve formed by two quartz glass tubes of different diameters arranged coaxially. The two ends of the annular quartz sleeve are sealed to form an annular closed space between the two quartz tubes, which is filled with discharge gas. The outer electrode is wound on the outer surface of the quartz glass tube with a larger diameter, and the inner electrode is wound on the inner surface of the quartz tube with a smaller diameter. A high-frequency voltage is applied between the two electrodes for capacitive coupling discharge. This discharge setting between the two quartz tube sleeves is the current mainstream structure of 222 nanometer DBD excimers. However, many application scenarios require uniform radiation intensity, and flat-plate luminous bodies are more suitable than tubular luminous bodies.

[0008] CN104081496 discloses a light-emitting tube, whose cross-sectional shape is a flat, roughly quadrangular shape, and a pair of electrodes are arranged on the outer surface of the flat wall of the tube wall. The patent also discloses a method for manufacturing such a lamp tube with a flat, roughly quadrangular cross-sectional shape. The process starts with a cylindrical quartz glass tube, and a first flat wall is heated and pressed from a first direction by a blowtorch to form a first flat wall, and then a second flat wall is heated and pressed from a second direction opposite to the first direction by a blowtorch. However, this heating and pressure forming process is difficult to produce a very flat structure.

[0009] CN112820625 discloses a 222 nanometer excimer lamp with a flat tube wall. Two electrodes are arranged on the outer walls of the first tube wall and the second tube wall. The patent also discloses a method for manufacturing such a lamp tube. The process is very similar to CN104081496, starting with a single cylindrical quartz glass tube, which is heated and softened, and then extruded by a roller assembly to form a first tube wall and a second tube wall that are parallel to each other. This processing method is also difficult to produce a very flat structure. The patent document also mentions that "concave" is easily produced during the extrusion process, and the inside of the lamp tube must be inflated during the extrusion process.

[0010] The commonality between CN104081496 and CN112820625 is that they start with a quartz lamp tube, and produce two opposite planes on the surface of the circular lamp tube through heating and pressure forming, and then lay electrodes on the opposite planes. The softening temperature of quartz is about 1750°C. Not to mention the difficulty of pressure forming at such a high temperature, this process only produces a flat lamp tube in the shape of a long strip. The problem that this method solves is the problem of unequal distances between the two electrodes of the single-tube circular lamp tube in US 7800308B2; or it simplifies the double-tube lamp tube in CN 213294766 and CN 213698044 to make it a single-tube lamp tube, but it cannot produce light-emitting panels of any shape, such as round light-emitting panels or square light-emitting panels. Summary of the invention

[0011] In view of the problems in the prior art, the present invention provides a 222-nanometer excimer lamp panel and a manufacturing method thereof, which has uniform irradiation intensity, long service life, simple manufacturing process and low cost.

[0012] In order to achieve the purpose of the present invention, the technical solution adopted by the present invention is:

[0013] The present invention provides a 222-nanometer excimer lamp panel, comprising parallel dielectric plates, the dielectric plates being capable of transmitting 222-nanometer ultraviolet light; two opposite inner surfaces of the dielectric plates being provided with a tempered layer; the edges of the two dielectric plates being sealed and connected by a dam to form a cavity for accommodating discharge gas, the side walls of the dam being provided with a vent; the outer surface of at least one dielectric plate being provided with a mesh electrode for emitting 222-nanometer ultraviolet light, and the outer surface of the dielectric plate for transmitting light being plated with an optical filter film for filtering light having a wavelength other than 222 nanometers.

[0014] Preferably, a plate-shaped electrode is disposed on the outer surface of one of the dielectric plates, and the plate-shaped electrode is light-proof and can reflect 222 nanometer ultraviolet light.

[0015] More preferably, the planar size of the plate-shaped electrode is smaller than the planar size of the dielectric plate and the interface between the plate-shaped electrode and the dielectric plate is covered with a sealing layer.

[0016] More preferably, the plate-shaped electrode is provided with a power interface for connecting to a power source.

[0017] Preferably, a planar size of the mesh electrode is smaller than a planar size of the dielectric plate.

[0018] Preferably, the mesh electrode is provided with a power interface for connecting to a power source.

[0019] More preferably, the dielectric plate is made of quartz, and the dam is made of Kovar alloy dam, wherein the outer surface of one quartz plate is provided with a vacuum evaporated mesh metal electrode, and the plane size of the mesh metal electrode is smaller than the plane size of the quartz plate, and the surface of the other quartz plate is covered with aluminum foil with a plane size smaller than the plane size of the quartz plate, and sealing silicone is provided at the junction of the edge of the aluminum foil and the quartz plate.

[0020] The present invention also provides a method for manufacturing the above-mentioned 222 nanometer excimer light panel, comprising:

[0021] Tempering the inner surface of the opposite side of the dielectric plate;

[0022] The edges of the two dielectric plates are sealed and connected by a dam to form a cavity for containing discharge gas, and a vent is provided on the side wall of the dam;

[0023] An optical filter film is plated on the outer surface of a dielectric plate for light transmission and a mesh electrode is made.

[0024] Preferably, the method further comprises manufacturing a plate-shaped electrode on the outer surface of one of the dielectric plates and covering the interface between the plate-shaped electrode and the dielectric plate with a sealing material.

[0025] Preferably, the dielectric plate is a quartz plate, the dam is a Kovar dam, and the Kovar dam and the quartz plate are sealed by pre-oxidizing the Kovar in water vapor or a mixture of nitrogen and water vapor, and then melting and sealing the oxide layers on the surfaces of the quartz and Kovar; or a metal welding layer is plated on the quartz surface by vacuum evaporation or silver paste sintering, and then brazing is performed in an atmosphere furnace using silver-copper eutectic solder.

[0026] The present invention provides a 222 nanometer excimer light board and a manufacturing method thereof. The beneficial effects of the present invention include:

[0027] (1) The present invention uses a light board instead of a light bar, which is convenient for use in many application scenarios that require uniform radiation density. The plane shape of the light board can be any, including but not limited to round, square, annular, etc., as long as the quartz glass plate can be processed into a plane shape.

[0028] (2) One of the important factors affecting the life of the excimer lamp is the microcracks and their extension formed on the inner surface of the quartz tube due to long-term discharge and frequent thermal shocks. The present invention adds a dielectric plate quenching process in the production process of the excimer lamp, similar to the surface "tempering" treatment of glass, to form compressive stress on the surface of the dielectric plate, thereby increasing the life of the excimer lamp.

[0029] (3) When the dielectric plate is made of quartz plate, the structure of the dam composed of two pieces of quartz glass and Kovar alloy is simple. The brazing technology of quartz glass and Kovar alloy has a long history, perfect technology and controllable cost. The sealing treatment of the electrode avoids the generation of ozone. The optical filtering coating on the outer surface of the transparent quartz plate blocks the ultraviolet radiation of 250-280 nanometers that is harmful to the human body.

[0030] (4) The relevant manufacturing process is simple. Compared with the lamp tube, it is relatively easy to make mesh electrodes and optical filter coatings on the lamp board, which reduces the corresponding manufacturing cost. BRIEF DESCRIPTION OF THE DRAWINGS

[0031] Figure 1 It is a schematic diagram of the overall structure of a 222 nanometer excimer lamp panel of the present invention.

[0032] Figure 2 Shows the relationship between the reflection efficiency of various metals to ultraviolet light and the wavelength.

[0033] Figure 3 It is a schematic diagram of the structure of the surface electrode of the first dielectric plate.

[0034] Figure 4 It is a schematic diagram of the structure of the surface electrode of the second dielectric plate.

[0035] Figure 5 The diagram is a schematic diagram of the single-sided luminescence (A) and double-sided luminescence (B) structures of a 222-nanometer excimer lamp panel of the present invention.

[0036] In the figure:

[0037] 11. First dielectric plate, 111. First tempered layer; 12. Second dielectric plate, 121. Second tempered layer, 122. Optical filter membrane; 31. Plate electrode, 311. First power interface, 312. Sealing layer; 32. Mesh electrode, 321. Second power interface; 4. Dam, 41. Vent. DETAILED DESCRIPTION

[0038] In order to explain the present invention more clearly, the present invention is further described in detail below in conjunction with embodiments and with reference to the accompanying drawings. It should be understood by those skilled in the art that the content described below is illustrative rather than restrictive, and should not be used to limit the scope of protection of the present invention. Example

[0039] The present invention provides a 222 nanometer excimer lamp panel, referring to Figure 1 , including a first dielectric plate 11 and a second dielectric plate 12 arranged in parallel. In the present invention, the first dielectric plate 11 and the second dielectric plate 12 are both two transparent dielectric materials. "Transparent" means that the optical transmittance to a wavelength of 222 nanometers is high. Optional materials include magnesium fluoride (MgF2), lithium fluoride (LiF), calcium fluoride (CaF2), sapphire (Sapphire, single crystal Al2O3), and quartz (SiO2). Quartz is preferred here for cost considerations.

[0040] The first dielectric plate 11 and the second dielectric plate 12 have the same shape, which can be round, square, rectangular, or any shape. Simple quartz plates, such as round, square, and rectangular, can be easily purchased on the market. The plane size of the dielectric plate can be determined according to the application needs. The thickness has a great influence on the transmittance of 222 nanometer ultraviolet light. The literature reports that the quartz thickness ranges from 1.2 to 2.0 mm, and the transmittance is between 85% and 67%. The thinner the thickness, the more light it transmits. However, long-term discharge will produce microcracks on the quartz surface, and too thin quartz glass will affect the life of the lamp tube. In addition, quartz sheets with larger plane dimensions naturally choose thicker sizes. Here, the thickness is selected between 1 and 4 mm. For example, a circular quartz plate produced by Lianyungang Guangwei Quartz Products Co., Ltd. can be used, with a diameter of 30 mm and a thickness of 3 mm. Of course, it is not limited to this.

[0041] The first dielectric plate 11 and the second dielectric plate 12 are provided with a first tempered layer 111 and a second tempered layer 121 on two opposite inner surfaces, respectively. The excimer lamp of the present invention is made based on the principle of dielectric barrier discharge. The discharge is directly generated from the dielectric surface, resulting in a continuous high temperature on the dielectric surface. Long-term thermal stress will produce microcracks on the quartz surface. Microcracks are one of the main reasons for the failure of excimer lamps. The surface compressive stress layer (i.e., the tempered layer) formed by the tempering treatment can close the surface microcracks and reduce the crack propagation speed.

[0042] The edges of the two dielectric plates are connected by a dam seal. Figure 1 As shown, the function of the dam 4 is to connect the first dielectric plate 11 and the second dielectric plate 12 mentioned above at their edges to form a closed space with a thickness equal to the height of the dam 4, which is used to encapsulate the discharge gas. In the present invention, the dam 4 preferably adopts a Kovar alloy dam. Kovar alloy is an iron-cobalt-nickel alloy, and its thermal expansion coefficient is close to that of glass. The sealing of Kovar alloy and glass is widely used in microelectronic metal packaging, relays, connectors, solar vacuum collectors and other occasions that require vacuum airtightness. The dam 4 can be a ring or a square or a rectangle, depending on the shape of the dielectric plate.

[0043] The dam 4 has a vent 41 on the side wall for vacuuming and filling discharge gas, and a valve is provided at the end of the vent. The Kovar alloy dam and the two quartz plates can be sealed by flame sealing or high frequency induction heating, or brazed with solder.

[0044] In the present invention, the encapsulated discharge gas is high-purity chlorine and krypton. The total gas pressure and the partial pressure of chlorine and krypton have a significant effect on the luminous efficiency of the molecular lamp. The total gas pressure reported in the literature ranges from 100Pa to 1 atmosphere (101,000Pa). The choice here is 100-5000Pa, preferably 2000Pa. The ratio of krypton to chlorine is 200:1 to 50:1, and the optimal choice here is 100:1. The resulting luminous efficiency is 5%-10%.

[0045] Before filling the chlorine and krypton gases, the cavity is repeatedly evacuated and filled with chlorine because the price of chlorine is much lower than that of krypton. After cleaning the impurity gases in the cavity, high-purity chlorine and krypton are filled in respectively. The evacuation and filling of gas are completed through the vent 41 on the Kovar alloy dam. After the filling process is completed, the valve is sealed.

[0046] In the present invention, at least one dielectric plate has a mesh electrode on its outer surface for emitting 222 nm ultraviolet light. Figure 5As shown, one of the two dielectric plates can use a plate electrode 31 and the other can use a mesh electrode 32. This arrangement makes one side of the excimer lamp plate emit light while the other side does not. The two dielectric plates can also use mesh electrodes 32. This arrangement makes both sides of the excimer lamp plate emit light.

[0047] Figure 3 and Figure 4 3 is a structural diagram of the electrode on the surface of the dielectric plate. The planar size of the electrode, whether it is the plate electrode 31 or the mesh electrode 32, is smaller than the planar size of the dielectric plate. The consideration of this design is that the discharge area will not extend to the edge of the dielectric. Since the two dielectric plates are sealed together at the edge by the Kovar alloy dam, the planar size of the electrode is smaller than the planar size of the discharge dielectric, in order to avoid the interaction between the discharge gas and the Kovar alloy dam.

[0048] The plate-shaped electrode 31 is opaque and has high reflectivity to 222 nm ultraviolet light. The high reflectivity may be derived from aluminum or aluminum plating. The relationship between the reflectivity of various metals to ultraviolet light and the wavelength is as follows: Figure 2 As shown. It can be seen that aluminum is the only metal that can achieve 90% reflection at a wavelength of 222nm. Another method to obtain a high reflective layer is a dielectric multilayer film, which is formed by alternating evaporation of two materials with high and low refractive indices, such as alternating stacks of magnesium fluoride and lithium fluoride. The optical thickness of each layer is one-fourth of the wavelength of 222 nanometers, that is, the thickness of each layer is 55.5 nanometers. The high reflective performance of the dielectric multilayer film is based on the principle of mutual interference extinction of multiple layers of reflected light beams. The base metal material of the dielectric reflective film or aluminum film is preferably a material with good thermal conductivity, such as copper, silver, and gold. In the present invention, the plate-shaped electrode 31 is preferably aluminum foil or a metal material with aluminum coating on the surface.

[0049] The gap between the electrode and the dielectric material of the DBD excimer lamp will produce ozone. Ozone, or O3, itself has strong oxidizing properties and can kill bacteria and viruses. However, excessive ozone is harmful to human health. The National Ambient Air Quality Standards (NAAQS) proposes that the maximum concentration of ozone that a person can accept within one hour is 260μg / m 3 Being in an ozone environment exceeding this limit for one hour will cause coughing, breathing difficulties and decreased lung function.

[0050] In order to avoid excessive ozone, the present application covers the sealing layer 312 at the junction of the plate-shaped electrode 31 on the surface of the first dielectric plate 11 and the first dielectric plate 11. The material of the sealing layer 312 can be a mixed slurry of dielectric material powder such as silicon dioxide and an organic carrier, or it can be silica gel. The silica gel can be a two-component AB solidified by heating, or a single component solidified by heating and moisture. Silica gel is preferred here.

[0051] The plate-shaped electrode 31 is provided with a first power interface 311 for connecting to a power source.

[0052] The mesh electrode 32 is light-transmissive. The mesh electrode can be simply a mesh woven from metal wires, but the metal wire mesh is difficult to adhere to the surface of the dielectric, which affects the discharge, and the oxygen in the gap between the wire mesh and the surface of the dielectric may become ozone under high voltage. Excessive ozone will have adverse effects on the human body. Another method for manufacturing a mesh electrode is to form a mesh electrode on the surface of the discharge dielectric by printing, electroplating, evaporation, and sputtering. From a cost perspective, printing or evaporation is preferred here. Printing mixes metal powder, low-melting-point glass powder, and organic slurry and prints them on the surface of quartz glass. After high-temperature sintering, the organic slurry volatilizes, the low-melting-point glass melts, and finally the metal powder is sintered on the surface of the discharge dielectric. The thickness of the metal film formed after sintering is between 5 and 20 microns, generally 10 microns thick. The material of the metal powder can be gold, silver, platinum, nickel, and cobalt. Silver is preferred here. Silver paste can be purchased on the market, and there are many choices.

[0053] Theoretically, the Krypton Chloride Excimer Lamp has a single wavelength of 222 nanometers, but in reality, the spectrum of the DBD Krypton Chloride Excimer Lamp contains a very low energy wavelength of about 250 nanometers, and wavelengths near this wavelength are harmful to the human eye and body. Figure 5 The outer surfaces (the surfaces away from the cavity) of the second dielectric plates 12 for single-sided light emission (A) and double-sided light emission (B) are both coated with optical filter films 122 for filtering wavelengths other than 222 nanometers.

[0054] The mesh electrode 32 has a second power interface 321 for connecting to a power source, which may be a metal wire welded on the mesh electrode.

[0055] In the present application, the power supply adopts a pulse power supply with a frequency of 50-150 Hz and a voltage of 8-12 KV. The pulse waveform has a higher electro-optical conversion efficiency than the sine waveform.

[0056] The present invention also provides a method for manufacturing the above-mentioned 222 nanometer excimer light panel, comprising:

[0057] a. After the size of the quartz glass is completed, the inner surface of the opposite side of the dielectric plate (especially the surface in contact with the discharge gas) is tempered.

[0058] Tempering is to heat the glass to its softening temperature (quartz is close to 1700℃) and then quench it at high temperature to rearrange its molecular structure, forming a compressive stress layer on the surface of the glass and a tensile stress layer in the middle. The tempering process of quartz can be completed by adding a quenching process to the production process of quartz glass. Or the cut and formed quartz glass plate is heated in a high-temperature furnace to above its softening temperature. The softening temperature of quartz glass varies due to its production process. The softening point of quartz glass produced by electric melting is higher than that of quartz glass produced by gas refining. Generally, the softening point of quartz is 1600 degrees Celsius. Quenching can be done by blowing high-speed cold air.

[0059] b. The edges of the two dielectric plates are sealed and connected by a dam to form a cavity for accommodating the discharge gas, and a vent is opened on the side wall of the dam.

[0060] The sealing connection between the Kovar alloy dam and two pieces of quartz glass is an important step in the manufacturing process of the present invention. Kovar alloy is widely used for sealing connection with glass because its thermal expansion coefficient is close to that of glass. The connection methods of Kovar alloy and quartz glass can be divided into two categories: direct welding without solder; solder connection.

[0061] Direct welding without solder: Kovar and glass do not wet each other, so Kovar must be pre-oxidized before welding. The chemical bond of quartz glass is an ionic-covalent mixed chemical bond. According to the principle that similar chemical bonds or similar chemical bonds are mutually affinity, glass materials have good adhesion with glass and ceramic materials. However, since Kovar is a material mainly based on metal bonds, Kovar and quartz glass cannot be directly fused. After Kovar is pre-oxidized, a multi-layer oxide layer FeO / Fe3O4 / Fe2O3 is formed on its surface, which becomes a bridge between glass and metal.

[0062] The oxides required for pre-oxidation of Kovar alloy should be Fe3O4 and FeO, and Fe2O3 is not desired. The iron oxide layer has a cubic structure, which is similar to the structure of Kovar metal, so it can be firmly bonded to it; while Fe3O4 has a spinel structure, and the chemical bond type is similar to that of quartz glass, so it can be firmly bonded to it. In order to obtain Fe3O4 and FeO and avoid Fe2O3, the pre-oxidation process is set to be carried out in water vapor, or a mixed gas of nitrogen and water vapor, at a temperature between 500-550 degrees Celsius, and the heat treatment time is 30-100 minutes, preferably 60 minutes. The thickness of the oxide film should be controlled within a certain range; if the oxide film is too thin, the oxide will completely dissolve in the glass, resulting in direct sealing of the glass and the metal substrate surface, which reduces the sealing strength; if the oxide film is too thick, the oxide on the metal surface will be rough and loose, and the sealing part will easily leak. The thickness of the oxide layer on the surface of Kovar alloy described here is approximately equal to 1.0-2.0 μm.

[0063] The connection between the pre-oxidized Kovar alloy and the quartz glass can be flame sealing, high-frequency induction sealing, or laser sealing.

[0064] Solder connection: Solderable metals are plated on the surface of quartz glass and the surface of Kovar alloy respectively, and then solder is placed between the surfaces of quartz glass and Kovar alloy, and then heated to the melting temperature of the solder to form a sealed connection between quartz glass and Kovar alloy.

[0065] There are two methods to plate solderable metals on quartz surfaces: vacuum evaporation and silver paste sintering.

[0066] Vacuum evaporation can adopt a three-layer metal structure. The transition layer chromium (Cr) or titanium (Ti) is combined with quartz glass. Cr and Ti have strong bonding with quartz glass. The thickness of Cr or Ti should be greater than 30 nanometers. Adjacent to Cr or Ti is nickel (Ni). The outermost layer is gold. The thickness of Ni should be greater than 400 nanometers; the thickness of gold should be greater than 400 nanometers. Gold does not oxidize at room temperature and is the best interface for bonding with solder. If the thickness of the gold layer is less than 400 nanometers, defects may appear on the surface, such as pinholes. The nickel under the gold layer will perforate and form nickel oxide on the surface of the gold, affecting the connection quality with the solder. The role of nickel is a barrier layer. Gold and chromium (or titanium) react quickly with liquid solder. If there is no nickel, the liquid solder will quickly "eat" the gold and chromium (or titanium), resulting in direct contact between the solder and the quartz glass.

[0067] The process of silver paste sintering is to apply silver paste on the surface of quartz glass by screen printing. The main components of silver paste are silver powder, low-temperature glass powder and organic carrier. During the high-temperature sintering process, the organic carrier is vaporized, the low-temperature glass powder is melted, and the silver powder and quartz glass are sintered together to form a weldable silver metal surface. The cost of silver paste sintering process is relatively low, and silver paste sintering is preferred here.

[0068] The nickel / gold coating is produced on the surface of the kovar alloy by electroplating or chemical plating. Electroless Ni / immersion Au is a commonly used nickel / gold coating process. The thickness of the nickel layer should be greater than 2 microns. The thickness of the surface gold is theoretically 1 atomic layer thick, because the chemical process of gold plating is that gold atoms replace nickel atoms, and the gold plating stops when the surface of the nickel layer is covered with gold atoms; in fact, the thickness of the gold layer is less than 500 nanometers.

[0069] The solder can be silver-copper alloy, especially silver-copper eutectic alloy Ag72-Cu28 (weight ratio), with a eutectic temperature of 779°C. The solder can be customized into a solder piece of a certain shape and thickness, with a plane shape similar to the shape of the Kovar alloy dam, and a thickness between 0.05-0.5 mm, preferably 0.1 mm. The solder piece is placed between the metal solder layer of the quartz glass and the Kovar alloy, and heated to above the melting point of the solder, such as 800°C, and the atmosphere of the heating furnace is controlled to be nitrogen.

[0070] In addition to the heating furnace, high-frequency induction heating is also one of the heating methods for the sealing welding of quartz plates and Kovar alloy dams. Kovar alloy / solder sheet / quartz plate metal welding surface are aligned and stacked together and placed in a high-frequency current coil; the high-frequency current changes the magnetic field to generate an induced current, and the resistance heating of the current generates heat. The generated heat is localized and concentrated on the surface of the Kovar alloy and the solder sheet.

[0071] c. An optical filter film is plated on the outer surface of the dielectric plate used for light transmission and a mesh electrode is made.

[0072] When a plate-shaped electrode is disposed on the outer surface of one of the dielectric plates, the manufacturing method further comprises:

[0073] d. A plate-shaped electrode is made on the outer surface of one of the dielectric plates and a sealing material is covered at the interface between the plate-shaped electrode and the dielectric plate.

[0074] Obviously, the above embodiments of the present invention are merely examples to more clearly illustrate the present invention, and are not limitations on the implementation methods of the present invention. For ordinary technicians in the relevant field, other different forms of changes or modifications can be made on the basis of the above description. It is impossible to list all the implementation methods here. All obvious changes or modifications derived from the technical solution of the present invention are still within the protection scope of the present invention.

Claims

1. A 222-nanometer excimer lamp panel, comprising parallel dielectric plates, the dielectric plates being capable of transmitting 222-nanometer ultraviolet light; tempered layers being provided on two opposite inner surfaces of the dielectric plates; the edges of the two dielectric plates being sealed and connected by a dam to form a cavity for accommodating discharge gas, the side walls of the dam being provided with vents; the outer surface of at least one dielectric plate being provided with a mesh electrode for emitting 222-nanometer ultraviolet light, the outer surface of the dielectric plate for transmitting light being plated with an optical filter film for filtering light of a wavelength other than 222 nanometers, the plane size of the mesh electrode being smaller than the plane size of the dielectric plate, the outer surface of one of the dielectric plates being provided with a plate electrode, the plate electrode being opaque and capable of reflecting 222-nanometer ultraviolet light, the plane size of the plate electrode being smaller than the plane size of the dielectric plate, and the interface between the plate electrode and the dielectric plate being covered with a sealing layer to prevent ozone from exceeding the standard, the dielectric plate being made of a quartz plate, and the dam being made of a kovar alloy dam.

2. A 222 nanometer excimer light panel according to claim 1, characterized in that: The plate-shaped electrode is provided with a power interface for connecting to a power source.

3. A 222 nanometer excimer light panel according to claim 1, characterized in that: The mesh electrode is provided with a power interface for connecting to a power source.

4. A 222 nanometer excimer light panel according to claim 1, characterized in that: The outer surface of one of the quartz plates is provided with a vacuum-evaporated mesh metal electrode, and the plane size of the mesh metal electrode is smaller than the plane size of the quartz plate. The surface of the other quartz plate is covered with an aluminum foil with a smaller plane size than the plane size of the quartz plate, and a sealing silicone is provided at the junction of the edge of the aluminum foil and the quartz plate.

5. The method for manufacturing the 222 nanometer excimer light panel according to any one of claims 1 to 4, comprising: Tempering the inner surface of the opposite side of the dielectric plate; The edges of the two dielectric plates are sealed and connected by a dam to form a cavity for containing discharge gas, and a vent is provided on the side wall of the dam; An optical filter film is plated on the outer surface of a dielectric plate for light transmission and a mesh electrode is made; The invention also includes forming a plate-shaped electrode on the outer surface of one of the dielectric plates and covering the interface between the plate-shaped electrode and the dielectric plate with a sealing material; The dielectric plate is a quartz plate, the dam is a Kovar alloy dam, and the Kovar alloy dam and the quartz plate are sealed by pre-oxidizing the Kovar alloy in water vapor or a mixed gas of nitrogen and water vapor, and then melting and sealing the oxide layers on the surfaces of the quartz and Kovar alloy; or a metal welding layer is plated on the quartz surface by vacuum evaporation or silver paste sintering, and then brazing is performed in an atmosphere furnace using silver-copper eutectic solder.

Citation Information

Patent Citations

  • 222nm excimer lamp tube and manufacturing method thereof

    CN112820625A

  • 222nm excimer sterilizing lamp

    CN213294766U

  • Silk screen type 222nm excimer sterilizing lamp

    CN213698044U

  • Excimer lamp

    US7800308B2

  • Eximer discharging lamp and method of manufacturing eximer discharging lamp

    CN101740317A