A high-concentration continuous coupling preparation method for azo disperse dyes

By adopting the continuous coupling process of ultra-fine coupling component suspension and aromatic amine diazonium salt double salt in the production of azo disperse dyes, the problem of high-concentration coupling preparation is solved, efficient and environmentally friendly dye production is achieved, and waste water and The use of acid improves production efficiency and product purity.

CN116478559BActive Publication Date: 2024-10-11DONGHUA UNIV +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310374536.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-04-10
Publication Date
2024-10-11
Estimated Expiration
2043-04-10

AI Technical Summary

Technical Problem

It is difficult to achieve high-concentration coupling preparation of azo disperse dyes with existing technology, resulting in large amounts of wastewater, low production efficiency, and serious environmental pollution. Moreover, traditional processes are difficult to perform coupling reactions at high concentrations.

Method used

The ultra-fine coupling component suspension and the aromatic amine diazonium salt double salt are continuously coupled in a tubular reactor. The pH value is adjusted through online detection, and the temperature is heated and crystallized in the crystallization kettle, combined with grinding and filtration to achieve high performance. Concentrated liquid disperse dye production.

Benefits of technology

It achieves high-concentration green and efficient synthesis of azo disperse dyes, reduces the use of acid and washing water, improves reaction efficiency and product purity, and reduces resource consumption and environmental pollution.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0004169866590000051
    Figure BDA0004169866590000051
  • Figure BDA0004169866590000061
    Figure BDA0004169866590000061
Patent Text Reader

Abstract

The present invention relates to a high-concentration continuous coupling preparation method of azo disperse dyes, comprising the following steps: (1) adding coupling component, dispersant, water and zirconium oxide beads to a grinder for grinding, filtering, and obtaining an ultrafine coupling component suspension; (2) continuously adding the above-mentioned ultrafine coupling component suspension and aromatic amine diazonium salt double salt to a batching kettle for mixing, flowing into a tubular reactor through an overflow port, detecting the reaction state through an online detection device, and transferring to a crystallization kettle after adjusting pH to 6-7; (3) heating and crystallizing in a crystallization kettle, transferring to a grinder for grinding to obtain liquid disperse dyes; or through filter pressing and washing, obtaining a disperse dye filter cake. The method of the present invention can avoid the acid dilution heat effect when the external acid dissolves during coupling and the diazo component is added, greatly reducing the water consumption and blowdown of the coupling process, improving the reaction efficiency, realizing the high-concentration coupling of azo disperse dyes, and having a broad application prospect.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of disperse dyes, and particularly relates to a high-concentration continuous coupling preparation method of azo disperse dyes. Background Art

[0002] Disperse dyes are mainly used for dyeing polyester fibers. In my country, the annual output is 300,000 to 400,000 tons, accounting for more than 40% of the total output of dyes. According to the chemical structure, disperse dyes mainly include azo, anthraquinone, non-azo heterocyclic, etc., among which azo production accounts for more than 70%, with complete color spectrum, good application performance, simple production process and low cost. The production of azo disperse dyes involves three processes: diazotization, coupling and commercialization. In the coupling reaction, since the coupling components are difficult to dissolve in water, high-concentration and large-quantity acid or alkali is usually added to promote dissolution; at the same time, since the aromatic amine diazonium salt added during coupling contains concentrated acid solution, acid dilution heat effect is generated after mixing, and a large amount of ice water is required for cooling. Therefore, after the coupling reaction is completed, the solid content is only 4-5%, that is, 95-96 tons of water are used to produce 4-5 tons of azo compounds. After the reaction is completed, a large amount of acid-containing wastewater and washing wastewater are generated, which brings serious environmental problems. In addition, since the generated dye is insoluble in water, it is difficult for the traditional intermittent stirred tank reactor to achieve uniform mixing of the solid-liquid heterogeneous system materials, and side reactions are prone to occur, resulting in long reaction times and low production efficiency. Therefore, developing a high-concentration coupling process for azo disperse dyes, reducing wastewater generation and improving production efficiency is of great significance to achieving the industry development goals of energy conservation, emission reduction, and ecological protection.

[0003] In order to realize energy-saving production of coupling reaction, CN102093756A proposes to prepare the original dye by coupling under the condition of dispersant, and the solid content of the coupling reaction product can reach 10% or more, but below 20%, and the coupling component still needs to be dissolved by acid or alkali. CN103450699B proposes to disperse and emulsify the coupling material first, and add diazonium salt for coupling under stirring and grinding state, which can reduce the amount of acid and water consumption during coupling, but grinding is a non-continuous process, and heat is generated when the material is ground. In addition, the heat generated by the coupling reaction needs to be dissipated in time, making the reaction process difficult to control; in addition, the solid content after the coupling reaction is still less than 20%. CN104059377B also heats the aqueous solution containing the coupling component and then adds a dispersant, then cools it with ice water and disperses it with a homogenizing emulsifier pump, and then couples it with a diazonium salt, which can reduce the amount of acid used, reduce production costs, and reduce the pressure of wastewater treatment. However, the efficiency of the homogenizing emulsifier pump in reducing solid particles is low, the particle size distribution is wide, and the diazonium salt is synthesized by a conventional method and has a high acid content, making the coupling reaction difficult to carry out at high concentrations. CN105385185B has made further improvements on this, that is, coupling the fine particle dispersion of the coupling component with the aromatic amine diazonium salt complex salt, which does not have the acid dilution heat effect, can save acid and washing water, but there are problems such as large dispersion particle size, low concentration of the coupling component dispersion, and easy viscosity of the coupling product. CN111303653A continuously injects the ground and dispersed coupling components and diazonium salt solution into a supergravity machine, realizing continuous production of the coupling process, which can effectively reduce the amount of wastewater and improve the reaction efficiency. However, the particle size of the liquid after the coupling components are emulsified is large and the content is low, so that the coupling reaction is only carried out at a low concentration. Therefore, there is no method and process that can achieve high-concentration coupling of disperse dyes. Summary of the invention

[0004] The technical problem to be solved by the present invention is to provide a high-concentration continuous coupling preparation method for azo disperse dyes, which has the advantages of easy industrial implementation, ecological and environmental protection, wide adaptability to dye synthesis, high yield, and the like.

[0005] The present invention provides a high-concentration continuous coupling preparation method of azo disperse dyes, comprising the following steps:

[0006] (1) adding a coupling component, a dispersant A, water and zirconium oxide beads into a grinder, grinding and filtering to obtain an ultrafine coupling component suspension; wherein the average particle size (D50) of the ultrafine coupling component suspension is 0.1-1 μm; wherein the mass ratio of the coupling component to water is 1:1-2.5, and the mass of the dispersant A is 5-15% of the mass of the coupling component;

[0007] (2) adding the above-mentioned ultrafine coupling component suspension and aromatic amine diazonium salt complex salt into the batching kettle continuously and mixing them evenly, and then flowing into the tubular reactor through the overflow port, detecting the reaction state through the online detection device, adjusting the pH to 6-7 and then transferring to the crystallization kettle;

[0008] (3) Heating and crystallizing in a crystallization kettle, and then transferring the mixture to a grinder for grinding to obtain a liquid disperse dye; or filtering and washing with water to obtain a disperse dye filter cake.

[0009] The coupling component in step (1) is one or more of N,N-diethyl-3-acetamidoaniline, N,N-diethyl-2-methoxy-5-acetamidoaniline, N,N-biscyanoethylaniline, N-cyanoethyl-N-acetoxyethylaniline, N-cyanoethyl-N-benzylaniline, N,N-diacetoxyethyl-2-methoxy-5-acetamidoaniline and N,N-diallyl-2-methoxy-5-acetamidoaniline.

[0010] The dispersant A in the step (1) is one or more of sodium methyl naphthalene sulfonate formaldehyde condensate, sodium methylene dinaphthalene sulfonate, sodium naphthalene sulfonate formaldehyde polymer sodium salt, and phenol condensate sulfonate.

[0011] The particle size of the zirconia beads in step (1) is 0.1-1 mm, and the mass ratio of the zirconia beads to the coupling component is 7:1-5.

[0012] The rotation speed of the grinding machine in the steps (1) and (3) is 400-1000 rpm, and the grinding time is 2-10 hours.

[0013] The aromatic amine diazonium salt complex salt in the step (2) is a diazonium complex salt formed by diazotizing at least one of p-nitroaniline, 2,4-dinitro-6-chloroaniline, 2,4-dinitro-6-bromoaniline, 2-chloro-4-nitroaniline, 2,6-dichloro-4-nitroaniline, 2,6-dibromo-4-nitroaniline, 2-cyano-4-nitroaniline, 2-cyano-4,6-dinitroaniline and 2,6-dicyano-4-nitroaniline with 1,5-naphthalenesulfonic acid.

[0014] In the present invention, the aromatic amine diazonium double salt solid is a diazonium double salt solid obtained by diazotization in an organic solvent in the presence of 1,5-naphthalenesulfonic acid and then filtering.

[0015] The molar ratio of the aromatic amine diazonium salt to the coupling component in step (2) is 1:0.9-1.1, the residence time in the tubular reactor is 5-60 minutes, and the reaction temperature is 10-40°C.

[0016] In the step (2), the coupling component suspension and the aromatic amine diazonium salt double salt are continuously fed through a metering pump and a vibrating weight loss scale respectively, and the temperature of the batching kettle is maintained at 0-5°C.

[0017] The temperature of the heating and crystallization in step (3) is 50-100° C. and the time is 1-2 hours.

[0018] In the step (3), after being transferred into the crystallization kettle, the solid content of the material is 20-50%, and the dye content is 10-40%.

[0019] The grinding in step (3) may be supplemented with dispersant B in an amount of 3-10% of the original dye mass.

[0020] The dispersant B is one or more of sodium methyl naphthalene sulfonate formaldehyde condensate, sodium methylene dinaphthalene sulfonate, naphthalene sulfonate formaldehyde polymer sodium salt, phenol condensate sulfonate, peregal, OP-10, and NP-30.

[0021] Beneficial Effects

[0022] (1) The present invention uses a stable ultrafine coupling component suspension with a relatively high concentration, a solid aromatic amine diazonium salt complex salt and a tubular reactor during coupling to achieve high-concentration coupling of disperse dyes, thereby achieving green and efficient synthesis of azo disperse dyes.

[0023] (2) The present invention grinds and disperses the coupling components into stable ultrafine particles before coupling. On the one hand, it can completely eliminate the need to add sulfuric acid or hydrochloric acid during pulping in the traditional process. On the other hand, it increases the contact area between the diazonium salt and the coupling components, thereby improving the reaction efficiency. At the same time, due to the presence of the dispersant, the product particle size is small and is not viscous even at high concentrations. In addition, the grinding time of the subsequent dye can also be shortened.

[0024] (3) The present invention uses a solid double salt of aromatic amine diazonium salt, which can avoid the excessive concentrated sulfuric acid used to dissolve the diazonium salt in the traditional process and add the coupling component to dilute and release heat, and can also avoid the environmental problems caused by the use of excessive acid.

[0025] (4) The present invention fully mixes the diazonium salt and the coupling component and then uses a tubular reactor for continuous synthesis. Compared with the traditional intermittent production process, the mixing is more sufficient, and the heat generated by the coupling can be dissipated in time, which effectively inhibits the decomposition of the unreacted diazonium salt and improves the product purity and yield.

[0026] (5) Since the product after crystallization of the present invention has a high concentration of disperse dye and contains few impurities (mainly including original dye and dispersant), it can be directly subjected to subsequent grinding process to prepare liquid dye without traditional pressure filtration and water washing process, which greatly reduces resource consumption and reduces environmental pollution from the source. DETAILED DESCRIPTION

[0027] The present invention will be further described below in conjunction with specific embodiments. It should be understood that these embodiments are only used to illustrate the present invention and are not intended to limit the scope of the present invention. In addition, it should be understood that after reading the content taught by the present invention, those skilled in the art can make various changes or modifications to the present invention, and these equivalent forms fall within the scope limited by the appended claims of the application equally.

[0028] Example 1

[0029] (1) Preparation of ultrafine coupling component suspension: N,N-diacetyloxyethyl-2-methoxy-5-acetamidoaniline, sodium methylnaphthalenesulfonate formaldehyde condensate (MF), water and 0.3-0.4 mm zirconia beads were added into a grinder in a mass ratio of 50:5:55:70, and ground at a speed of 600 rpm for 6 hours. The suspension was filtered to obtain an ultrafine coupling component suspension with an average particle size (D50) of 0.45 μm.

[0030] (2) Continuous coupling reaction: The ultrafine coupling component suspension obtained above and the diazonium double salt formed by 2,4-dinitro-6-chloroaniline and 1,5-naphthalenesulfonic acid were continuously added into a batching kettle maintained at a temperature of 0-5°C (suspension feed rate 4.2 L / h, diazonium double salt feed rate 3.0 kg / h) at a molar ratio of 1:1.03. The temperature and residence time of the coupling reaction were 25°C and 20 min, respectively. Subsequently, the pH was adjusted to 6-7 with 10% liquid caustic soda and then transferred into a crystallization kettle.

[0031] (3) Post-treatment: The temperature was raised to 60°C in a crystallization kettle and crystallized for 2 h to obtain a suspension with an average particle size of less than 10 μm, a solid content of 45.4%, and a dye content of 30%. The suspension was transferred to a grinder and ground with 0.3-0.4 mm zirconium oxide beads at a speed of 600 rpm for 8 h to obtain CI Disperse Blue 79:1 liquid dye with an average particle size (D50) of 0.48 μm.

[0032] Example 2

[0033] (1) Preparation of ultrafine coupling component suspension: same as in Example 1.

[0034] (2) Continuous coupling reaction: Same as Example 1.

[0035] (3) Post-treatment: The same as Example 1, except that the suspension after crystallization was filtered and washed with water to obtain CI Disperse Blue 79:1 filter cake with a yield of 98%.

[0036] Example 3

[0037] (1) Preparation of ultrafine coupling component suspension: N,N-diethyl-3-acetamidoaniline, naphthalenesulfonic acid formaldehyde polymer sodium salt, water and 0.4-0.6 mm zirconia beads were added into a grinder in a mass ratio of 30:4.5:65.5:70, and ground at a speed of 600 rpm for 8 hours. The suspension was filtered to obtain an ultrafine coupling component suspension with an average particle size (D50) of 0.42 μm. (2) Continuous coupling reaction: The ultrafine coupling component suspension obtained above and the diazonium double salt formed by 2,4-dinitro-6-bromoaniline and 1,5-naphthalenesulfonic acid were continuously added into a batching kettle maintained at 0-5°C in a molar ratio of 1:1 (suspension feed rate 4.0 L / h, diazonium double salt feed rate 3.6 kg / h). The temperature and residence time of the coupling reaction were 30°C and 15 min, respectively. Subsequently, the pH was adjusted to 6-7 with 15% liquid caustic soda and then transferred into a crystallization kettle.

[0038] (3) Post-treatment: The temperature was raised to 70°C in a crystallization kettle and crystallized for 1 hour to obtain a suspension with a particle size of less than 10 μm, a solid content of 47.5%, and a dye content of 25%. The suspension was transferred to a grinder and 10% naphthalenesulfonic acid formaldehyde polymer sodium salt solution was added to make the total solid content 40%. The suspension was ground with 0.4-0.6 mm zirconia beads at a speed of 800 rpm for 6 hours to obtain CI Disperse Violet 93 liquid dye with an average particle size (D50) of 0.45 μm.

[0039] Example 4

[0040] (1) Preparation of ultrafine coupling component suspension: N,N-diethyl-2-methoxy-5-acetamidoaniline, sodium methylnaphthalenesulfonate formaldehyde condensate (MF), water and 0.3-0.4 mm zirconia beads were added into a grinder in a mass ratio of 40:4:56:70, and ground at a speed of 450 rpm for 6 hours. The mixture was filtered to obtain an ultrafine coupling component suspension having an average particle size (D50) of 0.51 μm.

[0041] (2) Continuous coupling reaction: The ultrafine coupling component suspension obtained above and the diazonium double salt formed by 2,4-dinitro-6-chloroaniline and 1,5-naphthalenesulfonic acid were continuously added into a batching kettle maintained at 0-5°C in a molar ratio of 1:1.04 (suspension feed rate 3.4 L / h, diazonium double salt feed rate 3.14 kg / h). The temperature and residence time of the coupling reaction were 30°C and 20 min, respectively. Subsequently, the pH was adjusted to 6-7 with 10% liquid caustic soda and then transferred into a crystallization kettle.

[0042] (3) Post-treatment: The temperature was raised to 65°C in a crystallization kettle and crystallized for 1 hour. After filter pressing and water washing, CI Disperse Blue 291:1 filter cake was obtained with a yield of 97%.

[0043] Comparative Example 1

[0044] This comparative example is a traditional intermittent coupling process of CI Disperse Blue 79:1. N,N-diacetoxyethyl-2-methoxy-5-acetamidoaniline, 98% sulfuric acid, and water (containing crushed ice) were added to a reactor in a mass ratio of 1:1:15 for slurrying, and then 30% 2,4-dinitro-6-chloroaniline diazonium sulfate solution was added dropwise, and the molar ratio of diazonium salt to coupling component in the added material was controlled to be 1.03:1, the time was 2.5-3h, and the temperature was controlled below 5°C. After the coupling was completed, the temperature was raised to crystallize, and then the CI Disperse Blue 79:1 filter cake was obtained by filter pressing and washing with water, with a yield of 94%.

[0045] Comparative Example 2

[0046] This comparative example is a low-concentration coupling process of a CI disperse blue 79:1 aromatic amine diazonium salt complex salt and a coupling component fine particle dispersion. N,N-diacetoxyethyl-2-methoxy-5-acetamidoaniline, water, sodium methylnaphthalenesulfonate formaldehyde condensate (MF) and Φ0.3-0.4mm zirconium oxide beads were added to a grinder in a mass ratio of 1:5:0.01:3, and ground at a speed of 500 rpm for 2.5 hours to obtain a coupling component suspension with an average particle size (D50) of 4.61μm. The suspension was diluted to a solid content of 9%, stirred at room temperature, and a diazonium complex salt formed by 2,4-dinitro-6-bromoaniline and 1,5-naphthalenesulfonic acid (the molar ratio of the coupling component to the diazonium complex salt was 1.03:1) was added within half an hour. The mixture was reacted at 30°C for 2 hours. After the reaction was completed, the temperature was raised for crystallization, and then filtered and washed with water to obtain a CI Disperse Blue 79:1 filter cake with a yield of 98%.

[0047] Table 1 Comparison of acid and water usage in each embodiment and comparative example

[0048]

[0049]

[0050] As can be seen from Table 1, the use of the scheme of the present invention has obvious advantages in reducing the amount of acid and water used in the coupling reaction, and less or even no washing water can be used. The amount of acid used in the traditional intermittent coupling process (Comparative Example 1) in Table 1 does not include the acid brought in by the aromatic amine diazonium sulfate solution. In order to reduce the heat release effect of the acid and the influence of the exothermic coupling reaction and maintain the system temperature, a large amount of water and ice are required in the coupling reaction; after the reaction is completed, the system contains a large amount of acid, and the amount of washing water is greatly increased. Although the raw materials in Comparative Example 2 are consistent with Examples 1 and 2, the amount of water used in the low-concentration coupling process is increased, and the acid in the system is not neutralized after the reaction is completed, resulting in a significant increase in the amount of washing water.

Claims

1. A high-concentration continuous coupling preparation method of azo disperse dyes, comprising the following steps: (1) adding coupling component, dispersant A, water and zirconium oxide beads into a grinder, grinding, filtering, and obtaining an ultrafine coupling component suspension; wherein: The average particle size of the ultrafine coupling component suspension is 0.1-1 μm, and the particle size of the zirconium oxide beads is 0.1-1 mm; wherein the mass ratio of the coupling component to water is 1:1-2.5, and the mass of the dispersant A is 5-15% of the mass of the coupling component; (2) adding the above-mentioned ultrafine coupling component suspension and aromatic amine diazonium salt complex salt into the batching kettle continuously and mixing them evenly, and then flowing into the tubular reactor through the overflow port, detecting the reaction state through the online detection device, adjusting the pH to 6-7 and then transferring to the crystallization kettle; (3) Heating and crystallizing in a crystallization kettle, and then transferring the mixture to a grinder for grinding to obtain a liquid disperse dye; or filtering and washing with water to obtain a disperse dye filter cake.

2. The preparation method according to claim 1, characterized in that: The coupling component in step (1) is one or more of N,N-diethyl-3-acetamidoaniline, N,N-diethyl-2-methoxy-5-acetamidoaniline, N,N-biscyanoethylaniline, N-cyanoethyl-N-acetoxyethylaniline, N-cyanoethyl-N-benzylaniline, N,N-diacetoxyethyl-2-methoxy-5-acetamidoaniline and N,N-diallyl-2-methoxy-5-acetamidoaniline.

3. The preparation method according to claim 1, characterized in that: The dispersant A in step (1) is one or more of sodium methyl naphthalene sulfonate formaldehyde condensate, sodium methylene dinaphthalene sulfonate, naphthalene sulfonate formaldehyde polymer sodium salt, and phenol condensate sulfonate.

4. The preparation method according to claim 1, characterized in that: The mass ratio of the zirconium oxide beads to the coupling components in the step (1) is 7:1-5.

5. The preparation method according to claim 1, characterized in that: The rotation speed of the grinding machine in the steps (1) and (3) is 400-1000 rpm, and the grinding time is 2-10 hours.

6. The preparation method according to claim 1, characterized in that: The aromatic amine diazonium salt complex salt in the step (2) is a diazonium complex salt formed by diazotizing at least one of p-nitroaniline, 2,4-dinitro-6-chloroaniline, 2,4-dinitro-6-bromoaniline, 2-chloro-4-nitroaniline, 2,6-dichloro-4-nitroaniline, 2,6-dibromo-4-nitroaniline, 2-cyano-4-nitroaniline, 2-cyano-4,6-dinitroaniline and 2,6-dicyano-4-nitroaniline with 1,5-naphthalenesulfonic acid.

7. The preparation method according to claim 1, characterized in that: The molar ratio of the aromatic amine diazonium salt to the coupling component in step (2) is 1:0.9-1.1, the residence time in the tubular reactor is 5-60 minutes, and the reaction temperature is 10-40°C.

8. The preparation method according to claim 1, characterized in that: The temperature of the heating and crystallization in step (3) is 50-100° C. and the time is 1-2 hours.

9. The preparation method according to claim 1, characterized in that: After being transferred into the crystallization kettle in step (3), the solid content of the material is 20-50%, and the dye content is 10-40%.

10. The preparation method according to claim 1, characterized in that: The grinding in step (3) further comprises adding dispersant B in an amount of 3-10% of the original dye mass.