Semiconductor structure and its fabrication method
By setting grooves in the substrate of the semiconductor structure and filling them with gradient layers, the lattice mismatch problem between the doped structure and the substrate is solved, the carrier mobility is improved and leakage current is reduced, thereby enhancing the stability and conductivity of the semiconductor structure.
Patent Information
- Application Number
- CN202210047626.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-01-17
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2042-01-17
AI Technical Summary
In existing semiconductor structures, lattice mismatch between the doped structure and the substrate leads to uneven growth morphology and leakage current, affecting the stability of the device.
A groove is formed in the substrate of a semiconductor structure, and a gradient layer is filled in the groove. The doping concentration of the gradient layer gradually changes from the bottom of the groove upwards. The gradient doping concentration is achieved through multiple structural layers. Combined with conductive and metal layers, the carrier mobility is improved and leakage current is reduced.
By matching the gradient layer with the groove wall, the carrier mobility is improved while the leakage current problem caused by lattice mismatch is reduced, thereby enhancing the stability and conductivity of the semiconductor structure.
Smart Images

Figure CN116487410B_ABST
Abstract
Description
Technical Field
[0001] This disclosure relates to the field of semiconductor technology, and in particular to a semiconductor structure and a method for fabricating the same. Background Technology
[0002] In the fabrication of semiconductor structures, in order to improve carrier mobility, doped structures can be embedded in the substrate of the semiconductor structure, thereby improving the device performance of the semiconductor structure.
[0003] In the aforementioned semiconductor structures, the doped structure and the original substrate will have a lattice mismatch problem, which will not only cause uneven growth morphology, but also leakage current, affecting the stability of the device. Summary of the Invention
[0004] The following is an overview of the subject matter described in detail in this disclosure. This overview is not intended to limit the scope of the claims.
[0005] This disclosure provides a semiconductor structure and a method for fabricating the same.
[0006] A first aspect of this disclosure provides a semiconductor structure, the semiconductor structure comprising: A substrate, the substrate including doped regions; A groove, the groove being located within the doped region; A gradient layer fills the groove, and the doping concentration of the gradient layer gradually changes from the bottom of the groove upwards.
[0007] According to some embodiments of this disclosure, the gradient layer includes a multilayer structure layer and a protective layer stacked sequentially, with adjacent structure layers having different doping concentrations.
[0008] According to some embodiments of this disclosure, the doping concentration of the multilayer structure increases first and then decreases from the bottom of the groove upwards.
[0009] According to some embodiments of this disclosure, the multilayer structure layer is a multilayer silicon-germanium layer, and the protective layer is a silicon layer.
[0010] According to some embodiments of this disclosure, the thickness of each of the structural layers is 2-10 nm.
[0011] According to some embodiments of this disclosure, the semiconductor structure further includes a conductive layer and a metal layer, the protective layer includes a via, the conductive layer fills the via, and the metal layer is disposed on the conductive layer and electrically connected to the conductive layer.
[0012] According to some embodiments of this disclosure, the material of the conductive layer includes cobalt silicide or nickel silicide; The material of the metal layer includes tungsten, copper, gold, or aluminum.
[0013] According to some embodiments of this disclosure, the doped region includes a heavily doped region and a lightly doped region, both of which are located around the periphery of the groove, with the heavily doped region being closer to the bottom of the groove.
[0014] A second aspect of this disclosure provides a transistor comprising the semiconductor structure described above, the semiconductor structure being located in the source region and drain region of the transistor.
[0015] A third aspect of this disclosure provides a method for fabricating a semiconductor structure, the method comprising: A substrate is provided, the substrate having doped regions; Grooves are formed in the doped region of the substrate; A gradient layer is formed, which fills the groove, and the doping concentration of the gradient layer gradually changes from the bottom of the groove upwards.
[0016] According to some embodiments of this disclosure, forming the gradient layer includes: A stacked structure is formed within the groove, the stacked structure comprising multiple stacked structural layers with different doping concentrations among adjacent structural layers; A protective layer is formed, which covers the stacked structure and fills the groove.
[0017] According to some embodiments of this disclosure, the doping concentration of the multilayer structure increases first and then decreases from the bottom of the groove upwards.
[0018] According to some embodiments of this disclosure, forming a stacked structure within the groove includes: Multiple rounds of epitaxial growth are performed within the groove, with each round of epitaxial growth forming one layer of the structure.
[0019] According to some embodiments of this disclosure, the multilayer structure is a multilayer silicon-germanium layer.
[0020] According to some embodiments of this disclosure, the difference in germanium content between adjacent silicon-germanium layers is 1 wt% to 5 wt%.
[0021] According to some embodiments of this disclosure, in the multilayer silicon-germanium layer, the germanium content in the silicon-germanium layer near the bottom of the groove is 25wt% to 30wt%, the germanium content in the silicon-germanium layer with the highest germanium content is 35wt% to 40wt%, and the germanium content in the silicon-germanium layer near the top of the groove is 25wt% to 30wt%.
[0022] According to some embodiments of this disclosure, after forming the gradient layer... A portion of the protective layer is removed to form a through-hole, which exposes a portion of the top surface of the stacked structure. The through-hole is filled with metal material, and a high-temperature annealing process is used to bond the metal material with the material of the protective layer to form a conductive layer. A metal layer is formed on the conductive layer.
[0023] According to some embodiments of this disclosure, before forming the gradient layer, ions are used to dope a second region located near the bottom of the groove to form a heavily doped region.
[0024] According to some embodiments of this disclosure, the ion includes at least one of germanium, carbon, and helium.
[0025] According to some embodiments of this disclosure, before forming a groove on the substrate, a first region located on the surface of the substrate is doped to form a lightly doped region, and the heavily doped region is located below the lightly doped region.
[0026] In the semiconductor structure and its fabrication method provided in the embodiments of this disclosure, a groove is formed in the doped region of the substrate, and a gradient layer is filled in the groove. The doping concentration of the gradient layer gradually changes from the bottom of the groove upward. The gradient layer with gradually changing doping concentration can better match the groove wall, thereby improving the carrier mobility and reducing leakage problems caused by lattice mismatch between the groove wall and the gradient layer.
[0027] After reading and understanding the accompanying diagrams and detailed descriptions, the other aspects can be understood. Attached Figure Description
[0028] The accompanying drawings, which are incorporated in and constitute a part of this specification, illustrate embodiments of the present disclosure and, together with the description, serve to explain the principles of these embodiments. In these drawings, similar reference numerals are used to denote similar elements. The drawings described below are some embodiments of the present disclosure, but not all embodiments. Other drawings will be readily available to those skilled in the art based on these drawings without inventive effort.
[0029] Figure 1 This is a schematic diagram of the semiconductor structure in related technologies; Figure 2 This is a schematic diagram of a semiconductor structure according to an exemplary embodiment; Figure 3 This is a schematic diagram of a semiconductor structure according to an exemplary embodiment; Figure 4 This is a schematic diagram of a semiconductor structure according to an exemplary embodiment; Figure 5This is a flowchart illustrating a method for fabricating a semiconductor structure according to an exemplary embodiment; Figure 6 This is a flowchart illustrating a method for fabricating a semiconductor structure according to an exemplary embodiment; Figure 7 This is a flowchart illustrating a method for fabricating a semiconductor structure according to an exemplary embodiment; Figure 8 This is a schematic diagram of a substrate provided in a method for fabricating a semiconductor structure according to an exemplary embodiment; Figure 9 This is a schematic diagram illustrating the formation of a groove in a method for fabricating a semiconductor structure according to an exemplary embodiment; Figure 10 This is a schematic diagram illustrating the formation of heavily doped regions in a method for fabricating a semiconductor structure according to an exemplary embodiment; Figure 11 This is a schematic diagram illustrating the formation of a first structural layer in a method for fabricating a semiconductor structure according to an exemplary embodiment; Figure 12 This is a schematic diagram illustrating the formation of a multilayer structure in a method for fabricating a semiconductor structure according to an exemplary embodiment; Figure 13 This is a schematic diagram illustrating the formation of a protective layer in a method for fabricating a semiconductor structure according to an exemplary embodiment; Figure 14 This is a schematic diagram illustrating the formation of a through-hole in a method for fabricating a semiconductor structure according to an exemplary embodiment; Figure 15 This is a schematic diagram illustrating the formation of a conductive layer in a method for fabricating a semiconductor structure according to an exemplary embodiment.
[0030] Figure label: 100, Substrate; 110, Heavily doped region; 120, Lightly doped region; 130, Halo region; 200, Groove; 300, Gradient layer; 310, Structural layer; 311, First structural layer; 312, Second structural layer; 313, Third structural layer; 320, Protective layer; 321, Via; 400, Conductive layer; 500, Metal layer; 10. Substrate; 11. Semiconductor substrate; 12. Well region; 20. Gate oxide layer; 30. Gate; 40. Dielectric layer sidewall; 10', Substrate; 20', Gate oxide layer; 30', Gate; 40', Doped structure. Detailed Implementation
[0031] To make the objectives, technical solutions, and advantages of the embodiments of this disclosure clearer, the technical solutions in the disclosed embodiments will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some, not all, of the embodiments of this disclosure. All other embodiments obtained by those skilled in the art based on the embodiments of this disclosure without creative effort are within the scope of protection of this disclosure. It should be noted that, unless otherwise specified, the embodiments and features in the embodiments of this disclosure can be arbitrarily combined with each other.
[0032] In existing semiconductor structures, to improve carrier mobility, doped structures are embedded in the substrate, for example, such as... Figure 1 As shown, the semiconductor structure is a transistor structure, which includes a substrate 10' having a source region, a drain region, and a channel region. A gate oxide layer 20' is formed on the channel region, and a gate 30' is formed on the gate oxide layer 20'. A doped structure 40' is embedded in the source and drain regions, such as a silicon-germanium structure. The applicant has discovered that since the material of the substrate 10' is typically silicon, a lattice mismatch exists between silicon and the silicon-germanium structure, resulting in uneven growth morphology and leakage current, thus affecting the stability of the transistor structure.
[0033] Based on this, an exemplary embodiment of this disclosure provides a semiconductor structure, such as... Figure 2 As shown, the semiconductor structure includes: a substrate 100, a recess 200 disposed on the substrate 100, and a gradient layer 300 filling the recess 200. The substrate 100 is made of, for example, silicon, and includes doped regions, which are used, for example, to form source / drain regions of a transistor. The recess 200 is disposed in the doped regions, and the gradient layer fills the recess 200. The doping concentration of the gradient layer 300 gradually changes from the bottom of the recess 200 upwards. Here, the doping concentration refers to the proportion of dopant to the total material. For example, when the gradient layer 300 is a silicon-germanium structure, the doping concentration is the germanium content in the silicon-germanium structure. The gradual change here can be a gradual decrease, a gradual increase, a decrease followed by an increase, or an increase followed by a decrease; this embodiment does not impose any limitations on this.
[0034] In the semiconductor structure of this embodiment, a groove 200 is provided in the doped region of the substrate 100, and a gradient layer 300 is filled in the groove 200. The doping concentration of the gradient layer 300 gradually changes from the bottom of the groove 200 upwards. The gradient layer 300 with gradually changing doping concentration can better match the groove wall of the groove 200, thereby improving the carrier mobility and reducing leakage problems caused by lattice mismatch between the groove wall of the groove 200 and the gradient layer 300.
[0035] In some embodiments, the gradient layer 300 is a monolithic structure in which the doping concentration gradually changes from the bottom of the groove 200 upwards. In other embodiments, the gradient layer 300 is a multilayer structure, and the gradual change in doping concentration of the gradient layer 300 from the bottom of the groove 200 upwards is achieved by setting different doping concentrations for different layers in the multilayer structure.
[0036] According to an exemplary embodiment, such as Figure 2 As shown, the gradient layer 300 includes multiple stacked structural layers 310. Adjacent structural layers 310 have different doping concentrations; that is, each structural layer 310 itself has the same doping concentration, but adjacent structural layers 310 have different doping concentrations, thus achieving the desired doping concentration variation. The number of structural layers 310 is not limited and can be set according to specific needs. For example, in... Figure 2 In the illustrated embodiment, from the bottom of the groove 200 upwards, the multilayer structure layer 310 sequentially includes a first structure layer 311, a second structure layer 312, and a third structure layer 313. The first structure layer 311 and the second structure layer 312 have different doping concentrations, the second structure layer 312 and the third structure layer 313 have different doping concentrations, and the doping concentrations of the first structure layer 311 and the third structure layer 313 can be equal or different. In an embodiment where the doping concentration of the gradient layer 300 gradually increases from the bottom of the groove 200 upwards, the doping concentration of the multilayer structure layer 310 also gradually increases from the bottom of the groove 200 upwards. For example, in... Figure 2 In the illustrated embodiments, the doping concentration of the third structural layer 313 is greater than the doping concentration of the second structural layer 312, and the doping concentration of the second structural layer 312 is greater than the doping concentration of the first structural layer 311. In embodiments where the doping concentration of the gradient layer 300 gradually decreases from the bottom of the groove 200 upwards, the doping concentration of the first structural layer 311 is greater than the doping concentration of the second structural layer 312, and the doping concentration of the second structural layer 312 is greater than the doping concentration of the third structural layer 313. In embodiments where the doping concentration of the gradient layer 300 first increases and then decreases, the doping concentration of the second structural layer 312 is greater than the doping concentration of the first structural layer 311 and greater than the doping concentration of the third structural layer 313. In embodiments where the doping concentration of the gradient layer 300 first decreases and then increases, the doping concentration of the second structural layer 312 is less than the doping concentration of the first structural layer 311 and less than the doping concentration of the third structural layer 313.
[0037] The gradient layer 300 also includes a protective layer 320 disposed on the multilayer structure layer 310, which provides good protection for the multilayer structure layer 310. In this embodiment, the doping concentration of the multilayer structure layer 310 increases and then decreases from the bottom of the groove 200 upwards. That is, the doping concentration of the structure layer 310 near the protective layer 320 is lower to achieve a good match with the protective layer 320, the doping concentration of the structure layer 310 near the substrate 100 is lower to achieve a good match with the substrate 100, and the doping concentration of the structure layer 310 far from the protective layer 320 and the substrate 100 is higher, thereby improving the carrier mobility of the gradient layer 300. By increasing and then decreasing the doping concentration of the multilayer structure layer 310 from the bottom of the groove 200 upwards, the device performance of the semiconductor structure can be guaranteed, leakage current caused by lattice mismatch can be avoided, and the conductivity of the gradient layer 300 can be improved at the same time.
[0038] In one embodiment, the thickness of each structural layer 310 is 2-10 nm, thereby ensuring the reliability of the formation process of each structural layer 310 and ensuring that the number of structural layers 310 in the gradient layer 300 is controllable.
[0039] According to an exemplary embodiment, the multilayer structure layer 310 is a multilayer silicon-germanium layer, that is, each structure layer 310 is a structure layer 310 obtained by doping germanium material in silicon, and the protective layer 320 is a silicon layer. The germanium content in the multilayer structure layer 310 first increases and then decreases from the bottom of the groove 200 upwards. That is, in the multilayer structure layer 310, the germanium content in the upper structure layer 310 is relatively small, the germanium content in the lower structure layer 310 is relatively small, and the germanium content in the middle structure layer 310 is relatively large. As an example, the multilayer structure layer 310 sequentially includes a first structure layer 311, a second structure layer 312, and a third structure layer 313. The germanium content in the second structure layer 312 is greater than the germanium content in the first structure layer 311, and is also greater than the germanium content in the third structure layer 313.
[0040] In this embodiment, the structural layer 310 is a silicon-germanium layer, and the protective layer 320 is a silicon layer. The upper structural layer 310 has a smaller germanium content, which allows it to be well matched with the silicon layer (protective layer 320) above it. The lower structural layer 310 also has a smaller germanium content, which allows it to be well matched with the silicon layer (substrate 100) below it. The middle structural layer 310 has a larger germanium content. Since the middle structural layer 310 is not in contact with the silicon layer (protective layer 320 and substrate 100), more germanium can be doped into the middle structural layer 310 to improve its carrier mobility and thus improve its conductivity.
[0041] In one embodiment, in the multilayer silicon-germanium layers, the germanium content in the silicon-germanium layer near the bottom of the groove 200 is 25wt% to 30wt%, the germanium content in the silicon-germanium layer with the highest germanium content is 35wt% to 40wt%, and the germanium content in the silicon-germanium layer near the top of the groove 200 is 25wt% to 30wt%. The difference in germanium content between adjacent silicon-germanium layers is 1wt% to 5wt%. This ensures that the germanium content difference between silicon-germanium layers is not too large, which would affect the mismatch between the silicon-germanium layers, while also preventing the difference in germanium content between silicon-germanium layers from being too small, which would affect the germanium content in the intermediate silicon-germanium layers. This balances the reliability and conductivity of the semiconductor structure.
[0042] According to an exemplary embodiment, such as Figure 2 As shown, the semiconductor structure also includes a conductive layer 400 and a metal layer 500. The protective layer 320 includes a via 321. The conductive layer 400 fills the via 321, and the metal layer 500 is disposed on the conductive layer 400 and electrically connected to it. By setting the metal layer 500 and the conductive layer 400 and contacting the structural layer 310 through the via 321, the structural layer 310 is electrically connected to other layers. The conductive layer 400 is made of a metal compound, such as cobalt silicide or nickel silicide. The metal silicide enables conductivity between the metal layer 500 and the structural layer 310, reducing contact resistance and improving the device performance of the semiconductor structure. The metal layer 500 can be made of materials such as tungsten, copper, gold, or silver.
[0043] In this embodiment, the protective layer 320 can also help form the metal compound, i.e., the conductive layer 400. For example, the through-hole 321 of the protective layer 320 can be filled with metal materials such as cobalt and nickel. After high-temperature annealing, the metal material in the through-hole 321 reacts with the material of the protective layer 320 to generate a metal compound for reducing contact resistance.
[0044] According to an exemplary embodiment, such as Figure 3As shown, the doped regions include a heavily doped region 110 and a lightly doped region 120. Both regions are located around the periphery of the trench, with the heavily doped region 110 closer to the bottom of the trench 200. The lightly doped (LDD) region 120 is a structure adopted by the MOSFET to reduce the drain field and improve the hot carrier injection effect. It involves placing a lightly doped region near the source and drain regions, allowing this region to bear a portion of the voltage, thus effectively preventing the hot carrier injection effect. The heavily doped region 110 is closer to the bottom of the trench 200; for example, the bottom of the trench 200 is higher than the lowest point of the heavily doped region 110. This results in the formation of the heavily doped region 110 on the bottom wall of the trench 200 and the sidewalls near the bottom wall. The ion-doped region 110 forms vacancies or defects, which release the stress of lattice mismatch and achieve a better match between the trench wall of the trench 200 and the gradient layer 300. (Continue to refer to...) Figure 3 A heavily doped Halo region 130 is provided below the lightly doped region 120 to reduce the short-channel effect of the device and suppress the threshold voltage drop.
[0045] According to an exemplary embodiment of this disclosure, this embodiment provides a transistor, such as... Figure 4 As shown, the transistor structure includes: a substrate 10, a channel disposed in the substrate 10, and a gate oxide layer 20 and a gate electrode 30 located above the channel. Dielectric sidewalls 40 are disposed on both sides of the gate oxide layer 20 and the gate electrode 30. The semiconductor structure described above is disposed in the source and drain regions of the substrate 10, that is, a groove 200 is disposed in both the source and drain regions, and a gradient layer 300 is filled in the groove 200. The doping concentration of the gradient layer 300 gradually changes from the bottom of the groove 200 upwards. By providing the gradient layer 300 in the source and drain regions, the gradient layer 300 with gradually changing doping concentration can better match the groove walls of the groove 200, thereby improving the carrier mobility and reducing leakage problems caused by lattice mismatch between the groove walls of the groove 200 and the gradient layer 300, thus improving the device performance of the transistor.
[0046] For example, such as Figure 4 As shown, the substrate 10 includes a semiconductor substrate 11 and a well region 12 on the semiconductor substrate 11 having a first conductivity type, such as an N-type well region or a P-type well region. In this embodiment, the lightly doped region 120 is formed by doping with ions of the first conductivity type, and the Halo region 130 is formed by doping with ions of the second conductivity type. That is, the first conductivity type and the second conductivity type are opposite. If the ions of the first conductivity type are N-type ions, then the ions of the second conductivity type are P-type ions; if the ions of the first conductivity type are P-type ions, then the ions of the second conductivity type are N-type ions.
[0047] This disclosure provides a method for fabricating a semiconductor structure in exemplary embodiments, such as... Figure 5 As shown, Figure 5 A flowchart illustrating a method for fabricating a semiconductor structure according to an exemplary embodiment of the present disclosure is shown. Figures 8-15 The diagram below illustrates the various stages of semiconductor structure fabrication. Figures 8-15 The methods for fabricating semiconductor structures are introduced.
[0048] like Figure 5 As shown, an exemplary embodiment of this disclosure provides a method for fabricating a semiconductor structure, comprising the following steps: Step S10: Provide a substrate having doped regions.
[0049] For example, such as Figure 8 As shown, the substrate 100 serves as a support component for supporting other components disposed thereon. The substrate 100 may be made of a semiconductor material, which may be one or more of silicon, germanium, silicon-germanium compounds, and silicon-carbon compounds.
[0050] According to an exemplary embodiment, such as Figure 8 As shown, a lightly doped (LDD) region 120 is formed in the first region on the surface of the substrate 100. For example, the first region is doped with ions of a first conductivity type to form the lightly doped region 120. A heavily doped region 110 is located below the lightly doped region 120. A trench 200 is formed at least partially in the heavily doped region 110 and the lightly doped region 120, and the bottom of the trench 200 is higher than the lowest point of the heavily doped region 110. The lightly doped region 120 is a structure adopted by the MOSFET to reduce the drain field and improve the hot carrier injection effect. Specifically, a lightly doped region is set near the source and drain regions, allowing this region to bear a portion of the voltage, thereby effectively preventing the hot carrier injection effect.
[0051] Furthermore, a heavily doped Halo region 130 can be formed below the lightly doped region 120. For example, the Halo region 130 is formed by doping with ions of a second conductivity type. That is, the first conductivity type is opposite to the second conductivity type; if the first conductivity type ion is an N-type ion, then the second conductivity type ion is a P-type ion; if the first conductivity type ion is a P-type ion, then the second conductivity type ion is an N-type ion. By setting the Halo region 130, the short-channel effect of the device can be reduced, and threshold voltage drops can be suppressed.
[0052] Step S20: Form a groove in the doped region of the substrate.
[0053] In this step, the groove 200 can be formed in the doped region of the substrate 100 using methods such as photolithography (Litho) and etching (ETCH). For example... Figure 9 As shown, the groove 200 is at least partially formed in the heavily doped region 110 and the lightly doped region 120, and the bottom of the groove 200 is higher than the lowest point of the heavily doped region 110.
[0054] Step S30: Form a gradient layer that fills the groove, and the doping concentration of the gradient layer gradually changes from the bottom of the groove upwards.
[0055] In this step, a doped semiconductor material can be deposited to form a gradient layer 300, or an undoped semiconductor material can be deposited to fill the trench 200 to form a semiconductor material layer. Then, doped impurities are injected into the semiconductor material layer through a thermal diffusion process or an ion implantation process to form the gradient layer 300.
[0056] In this embodiment, a semiconductor structure is formed in which a groove 200 is formed in the doped region of the substrate 100, and a gradient layer 300 is formed in the groove 200. The doping concentration of the gradient layer 300 gradually changes from the bottom of the groove 200 upwards. The gradient layer 300 with gradually changing doping concentration can better match the groove wall of the groove 200, thereby improving the carrier mobility and reducing leakage problems caused by lattice mismatch between the groove wall of the groove 200 and the gradient layer 300.
[0057] According to an exemplary embodiment of this disclosure, this embodiment is a further explanation of step S30 in the above embodiment.
[0058] like Figure 6 As shown, forming the gradient layer includes: S31. A stacked structure is formed in the groove. The stacked structure includes multiple stacked structural layers with different doping concentrations in adjacent structural layers.
[0059] In this step, such as Figure 12 As shown, by setting different doping concentrations for different structural layers 310 in the multilayer structure 310, the doping concentration of the gradient layer 300 gradually changes from the bottom of the groove 200 upwards. Adjacent structural layers 310 have different doping concentrations; that is, for each structural layer 310 itself, its doping concentration is the same, but the doping concentrations of adjacent structural layers 310 are different, thus achieving the desired doping concentration variation. The number of structural layers 310 is not limited and can be set according to specific needs. For example, in... Figure 12In the illustrated embodiment, with the bottom of the groove 200 facing upwards, the multilayer structure layer 310 sequentially includes a first structure layer 311, a second structure layer 312, and a third structure layer 313. The first structure layer 311 and the second structure layer 312 have different doping concentrations, the second structure layer 312 and the third structure layer 313 have different doping concentrations, and the doping concentrations of the first structure layer 311 and the third structure layer 313 can be equal or different.
[0060] As an example, a semiconductor material layer can be deposited using processes such as atomic layer deposition (ALD) and chemical vapor deposition (CVD), and then doped within the semiconductor material layer to form a structural layer 310. In another embodiment, in step S31, multiple rounds of epitaxial growth are performed within the groove 200, with each round forming a structural layer 310. By controlling the material content during the epitaxial growth process, the desired doping concentration is achieved. Using epitaxial growth to form the structural layer 310 allows for more precise control of the doping concentration of each structural layer 310, thereby improving process controllability.
[0061] S32. A protective layer is formed, which covers the stacked structure and fills the groove.
[0062] In this step, such as Figure 13 As shown, the protective layer 320 can be formed by processes such as atomic layer deposition (ALD) and chemical vapor deposition (CVD), or by epitaxial growth. By forming the protective layer 320 on the laminated structure, the laminated structure is well protected, and the protective layer 320 is used to fill the groove 200 to ensure flatness.
[0063] In this embodiment, the doping concentration of the multilayer structure layer 310 first increases and then decreases from the bottom of the groove 200 upwards. That is, in the multilayer structure layer 310, the doping concentration of the structure layer 310 near the protective layer 320 is smaller to form a good match with the protective layer 320, the doping concentration of the structure layer 310 near the substrate 100 is smaller to form a good match with the substrate 100, and the doping concentration of the structure layer 310 far away from the protective layer 320 and the substrate 100 is larger, thereby improving the carrier mobility of the gradient layer 300. By increasing and then decreasing the doping concentration of the multilayer structure layer 310 from the bottom of the groove 200 upwards, the device performance of the formed semiconductor structure can be guaranteed, leakage current caused by lattice mismatch can be avoided, and the conductivity of the gradient layer 300 can be improved at the same time.
[0064] According to an exemplary embodiment, the structural layer 310 is a silicon-germanium layer, and the protective layer 320 is a silicon layer. Thus, the germanium content in the upper structural layer 310 is relatively small, thereby achieving a good match with the silicon layer (protective layer 320) above it. The germanium content in the lower structural layer 310 is also relatively small, thereby achieving a good match with the silicon layer (substrate 100) below it. The germanium content in the middle structural layer 310 is relatively large. Since the middle structural layer 310 is not in contact with the silicon layer (protective layer 320 and substrate 100), more germanium can be doped in the middle structural layer 310 to improve its carrier mobility and thus improve its conductivity.
[0065] In this embodiment, step 31 includes: S311. Under conditions of 400°C to 1000°C, silicon-germanium is selectively epitaxially grown in a groove, and by controlling the germanium content in the silicon-germanium, a first structural layer with the desired doping concentration is obtained. See [link to documentation]. Figure 11 ; S312. On top of the first structural layer, multiple rounds of selective epitaxy are performed, with the thickness of silicon-germanium growth controlled within the range of 2-10nm in each round, thereby forming a multilayer structural layer.
[0066] As an example, such as Figure 12 As shown, a second structural layer 312 is selectively epitaxially formed on the first structural layer 311, and a third structural layer 313 is selectively epitaxially formed on the second structural layer 312. The doping concentration of the second structural layer 312 is greater than that of the first structural layer 311 and greater than that of the third structural layer 313.
[0067] In this embodiment, the germanium content in the silicon-germanium layer near the bottom of the groove 200 is 25wt% to 30wt%, the germanium content in the silicon-germanium layer with the highest germanium content is 35wt% to 40wt%, and the germanium content in the silicon-germanium layer near the top of the groove 200 is 25wt% to 30wt%. The difference in germanium content between adjacent silicon-germanium layers is 1wt% to 5wt%. This ensures that the germanium content difference between silicon-germanium layers is not too large, which would affect the mismatch between the silicon-germanium layers, and also avoids that the difference in germanium content between silicon-germanium layers is too small, which would affect the germanium content in the intermediate silicon-germanium layer. This balances the reliability and conductivity of the semiconductor structure.
[0068] According to an exemplary embodiment, such as Figure 7 As shown, after forming the gradient layer, the following steps are performed: S40. Remove part of the protective layer to form a through-hole, which exposes part of the top surface of the stacked structure.
[0069] In this step, such as Figure 14As shown, vias 321 can be formed on the protective layer 320 using methods such as photolithography and etching. As an example, a BARC layer (Bottom Anti-Reflective Coatings) is formed on the upper surface of the protective layer 320, a patterned photoresist layer is formed on the BARC layer, and the pattern in the patterned photoresist layer is transferred to the protective layer 320 using dry etching to form vias 321 in the protective layer 320.
[0070] S50. Fill the through hole with metal material and use a high-temperature annealing process to bond the metal material with the material of the protective layer to form a conductive layer.
[0071] In this embodiment, as Figure 15 As shown, a metal material is filled into the through-hole 321, and a high-temperature annealing process is used to bond the metal material in the through-hole with the protective layer 320 to form a metal compound. The metal compound enables conductivity between the structural layer 310 and the metal layer 500 formed in subsequent processes, which can reduce contact resistance and thus improve the device performance of the semiconductor structure. The metal material is, for example, cobalt or nickel, which can bond with silicon in the protective layer 320 to form cobalt silicide or nickel silicide.
[0072] S60. A metal layer is formed on the conductive layer.
[0073] In this step, the material of the metal layer 500 is, for example, tungsten, copper, gold, or silver, and the metal layer 500 can be deposited using processes such as atomic layer deposition (ALD) or chemical vapor deposition (CVD).
[0074] According to an exemplary embodiment, before forming the gradient layer 300, such as Figure 6 As shown, the following steps are also performed: S70, using ion pairs to dope the second region located near the bottom of the groove to form a heavily doped region.
[0075] In this step, such as Figure 9 As shown, before forming the gradient layer 300, ion doping is performed in the region near the bottom of the groove 200 to form a heavily doped region 110. The heavily doped region 110 constitutes the bottom wall of the groove 200 and part of the sidewall near the bottom. Vacancies or defects are formed in the heavily doped region 110 formed by ion doping, thereby releasing the stress of lattice mismatch and achieving a better match between the groove wall of the groove 200 and the gradient layer 300. The ions used for ion doping include at least one of germanium, carbon, and helium.
[0076] In one embodiment, the heavily doped region 110 is in contact with the first structural layer 311. For example, the bottom surface of the first structural layer 311 is in contact with the bottom of the heavily doped region 110, and the side surface of the first structural layer 311 is in contact with the side surface of the heavily doped region 110, thereby releasing the stress caused by lattice mismatch during the formation of the first structural layer 311.
[0077] According to an exemplary embodiment of this disclosure, after forming the heavily doped region 110 and before forming the gradient layer 300, the following steps are also performed: S80 uses ion doping to form a stress-relieving region in the third region near the side of the groove.
[0078] In this step, ions are used to dope the third region, thereby creating vacancies or defects in the sidewalls of the groove 200. This releases the stress caused by lattice mismatch during the formation of subsequent structural layers 310, resulting in a better match between the groove walls of the groove 200 and the gradient layer 300. The ions forming the heavily doped region 110 can be the same as or different from the ions forming the stress-relieving region. For example, the ions used for ion doping include at least one of germanium, carbon, and helium.
[0079] The stress relief region can be a monolithic cylindrical structure, thereby completely enclosing all structural layers above the first structural layer 311 in the gradient layer 300, for example, in Figure 3 In the illustrated embodiment, the stress relief region surrounds the second structural layer 312 and the third structural layer 313. In another embodiment, the stress relief region may be a plurality of regions arranged upward from the bottom of the groove 200, with each stress relief region corresponding to one structural layer 310, that is, each stress relief region contacts the sidewall of a structural layer 310.
[0080] The doping concentration of the stress relief region can be the same as or different from that of the heavily doped region 110. In some embodiments, the doping concentration of the heavily doped region 110 matches the doping concentration of the structural layer 310 it contacts, and the doping concentration of the stress relief region matches the doping concentration of the structural layer 310 it contacts. For example, the stress relief region corresponding to a structural layer with a higher doping concentration has a correspondingly higher doping concentration, and the stress relief region corresponding to a structural layer with a lower doping concentration has a correspondingly lower doping concentration.
[0081] For example, the multilayer structure 310 of the gradient layer 300 includes a first structure layer 311, a second structure layer 312, and a third structure layer 313 stacked sequentially. The doping concentration of the second structure layer 312 is greater than that of the first structure layer 311 and greater than that of the third structure layer 313. The stress relief region includes a first stress relief region corresponding to the second structure layer 312 and a second stress relief region corresponding to the third structure layer 313. That is, the first stress relief region is in contact with the sidewall of the second structure layer 312, and the second stress relief region is in contact with the sidewall of the third structure layer 313. The doping concentration of the first stress relief region is greater than that of the heavily doped region and greater than that of the second stress relief region.
[0082] Because the second structural layer 312 has a high doping concentration, the lattice mismatch between it and the sidewalls of the trench is relatively severe. Correspondingly, the doping concentration of the first stress relief region in contact with the second structural layer 312 is set to be relatively high, thereby forming more vacancies or defects in the first stress relief region, and thus releasing the stress generated by the formation of the second structural layer 312. Because the doping concentration of the first structural layer 311 and the third structural layer 313 is relatively low, the lattice mismatch between them and the bottom wall and sidewalls of the trench is relatively mild. Correspondingly, the doping concentration of the heavily doped region in contact with the first structural layer 311 and the second stress relief region in contact with the third structural layer 313 is set to be relatively low. This ensures stress relief (the stress generated when forming the first structural layer 311 and the stress generated when forming the third structural layer 313) while avoiding excessive vacancies or defects that could affect the reliability of the semiconductor structure.
[0083] Of course, it is understandable that the stress relief region can also be formed by doping after the formation of the first structural layer. When there are multiple stress relief regions, the formation steps of each stress relief region can also be interspersed between the structural layer formation steps. As an example, when the stress relief region includes a first stress relief region in contact with the second structural layer 312 and a second stress relief region in contact with the third structural layer 313, the first stress relief region can be formed by doping after the formation of the first structural layer 311, and the second stress relief region can be formed by doping after the formation of the second structural layer 312, and then the third structural layer 313 can be formed.
[0084] According to an exemplary embodiment of this disclosure, a method for fabricating a semiconductor structure is provided for fabricating a transistor. In this method, a gate oxide layer and a gate electrode are formed on a substrate. Before forming a trench, ion implantation is performed on the substrate on both sides of the gate oxide layer and the gate electrode to form the source electrode and the gate electrode. In another embodiment, ion implantation may be performed on the gradient layer after the gradient layer is formed to form the source electrode and the gate electrode.
[0085] In the semiconductor structure and its fabrication method provided in the embodiments of this disclosure, a groove is formed in the doped region of the substrate, and a gradient layer is filled in the groove. The doping concentration of the gradient layer gradually changes from the bottom of the groove upward. The gradient layer with gradually changing doping concentration can better match the groove wall, thereby improving the carrier mobility and reducing leakage problems caused by lattice mismatch between the groove wall and the gradient layer.
[0086] The various embodiments or implementation methods described in this specification are presented in a progressive manner. Each embodiment focuses on the differences from other embodiments, and the same or similar parts between the embodiments can be referred to each other.
[0087] In the description of this specification, references to the terms "embodiment," "exemplary embodiment," "some implementation," "illustrated implementation," "example," etc., refer to specific features, structures, materials, or characteristics described in connection with an implementation or example that are included in at least one implementation or example of this disclosure.
[0088] In this specification, the illustrative expressions of the terms used do not necessarily refer to the same implementation or example. Furthermore, the specific features, structures, materials, or characteristics described may be combined in any suitable manner in one or more implementations or examples.
[0089] In the description of this disclosure, it should be noted that the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inner", "outer", etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are only for the convenience of describing this disclosure and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this disclosure.
[0090] It is understood that the terms "first," "second," etc., as used in this disclosure may be used to describe various structures, but these structures are not limited by these terms. These terms are only used to distinguish one structure from another.
[0091] In one or more accompanying drawings, the same elements are represented by similar reference numerals. For clarity, many parts in the drawings are not drawn to scale. Furthermore, certain well-known parts may not be shown. For simplicity, a structure obtained after several steps may be depicted in a single drawing. Many specific details of this disclosure, such as the structure, materials, dimensions, processing methods, and techniques of the devices, are described below to provide a clearer understanding of the disclosure. However, as those skilled in the art will understand, this disclosure may be implemented without adhering to these specific details.
[0092] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of this disclosure, and are not intended to limit them. Although this disclosure has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some or all of the technical features therein. Such modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of this disclosure.
Claims
1. A semiconductor structure, characterized in that, The semiconductor structure includes: A substrate, the substrate including doped regions; A groove, the groove being located within the doped region; A gradient layer that fills the groove, wherein the doping concentration of the gradient layer gradually changes from the bottom of the groove upwards; The doped region includes a heavily doped region and a lightly doped region, both of which are located around the periphery of the groove, with the heavily doped region being closer to the bottom of the groove. The heavily doped regions are doped with at least one of germanium, carbon, and helium.
2. The semiconductor structure according to claim 1, characterized in that, The gradient layer comprises multiple stacked structural layers and a protective layer, with adjacent structural layers having different doping concentrations.
3. The semiconductor structure according to claim 2, characterized in that, The doping concentration of the multilayer structure increases first and then decreases from the bottom of the groove upwards.
4. The semiconductor structure according to claim 2, characterized in that, The multilayer structure is a multilayer silicon-germanium layer, and the protective layer is a silicon layer.
5. The semiconductor structure according to claim 2, characterized in that, The thickness of each of the structural layers is 2-10 nm.
6. The semiconductor structure according to claim 2, characterized in that, The semiconductor structure further includes a conductive layer and a metal layer. The protective layer includes a via. The conductive layer fills the via. The metal layer is disposed on the conductive layer and electrically connected to the conductive layer.
7. The semiconductor structure according to claim 6, characterized in that, The material of the conductive layer includes cobalt silicide or nickel silicide; The material of the metal layer includes tungsten, copper, gold, or aluminum.
8. A transistor, characterized in that, The transistor includes a semiconductor structure as described in any one of claims 1 to 7, wherein the semiconductor structure is located in the source region and the drain region of the transistor.
9. A method for fabricating a semiconductor structure, characterized in that, The method for fabricating the semiconductor structure includes: A substrate is provided, the substrate having doped regions; Grooves are formed in the doped region of the substrate; A gradient layer is formed, which fills the groove, and the doping concentration of the gradient layer gradually changes from the bottom of the groove upwards; Before forming the gradient layer, ions are used to dope a second region located near the bottom of the groove to form a heavily doped region; The ion includes at least one of germanium, carbon, and helium.
10. The manufacturing method according to claim 9, characterized in that, The formation of the gradient layer includes: A stacked structure is formed within the groove, the stacked structure comprising multiple stacked structural layers with different doping concentrations among adjacent structural layers; A protective layer is formed, which covers the stacked structure and fills the groove.
11. The manufacturing method according to claim 10, characterized in that, The doping concentration of the multilayer structure increases first and then decreases from the bottom of the groove upwards.
12. The manufacturing method according to claim 10, characterized in that, The formation of a stacked structure within the groove includes: Multiple rounds of epitaxial growth are performed within the groove, with each round of epitaxial growth forming one layer of the structure.
13. The manufacturing method according to claim 10, characterized in that, The multilayer structure is a multilayer silicon-germanium layer.
14. The manufacturing method according to claim 13, characterized in that, The difference in germanium content between adjacent silicon-germanium layers is 1 wt% to 5 wt%.
15. The manufacturing method according to claim 13, characterized in that, In the multilayer silicon-germanium layer, the germanium content in the silicon-germanium layer near the bottom of the groove is 25wt% to 30wt%, the germanium content in the silicon-germanium layer with the highest germanium content is 35wt% to 40wt%, and the germanium content in the silicon-germanium layer near the top of the groove is 25wt% to 30wt%.
16. The manufacturing method according to claim 10, characterized in that, After the gradient layer is formed A portion of the protective layer is removed to form a through-hole, which exposes a portion of the top surface of the stacked structure. The through-hole is filled with metal material, and a high-temperature annealing process is used to bond the metal material with the material of the protective layer to form a conductive layer. A metal layer is formed on the conductive layer.
17. The manufacturing method according to claim 9, characterized in that, Before forming a groove on the substrate, a lightly doped region is formed by doping a first region on the surface of the substrate, and the heavily doped region is located below the lightly doped region.
Citation Information
Patent Citations
Method for forming semiconductor structure and method for forming P-channel metal oxide semiconductor (PMOS) transistor
CN102931058A
