Method for decoking a rotary kiln
By controlling the temperature and rotation speed inside the rotary kiln, the coke flow is made out and a coking layer is formed, which solves the problem of coking in the rotary kiln, extends its service life, reduces the frequency of maintenance, and improves operating efficiency and cost-effectiveness.
Patent Information
- Application Number
- CN202310617168.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-29
- Publication Date
- 2026-07-03
- Estimated Expiration
- 2043-05-29
AI Technical Summary
Severe coking occurs during rotary kiln combustion, leading to frequent unit shutdowns for maintenance and affecting service life and operational stability.
By controlling the temperature and rotation speed inside the rotary kiln, the coking material becomes fluid and flows out of the kiln, while a uniform coking layer is formed inside the kiln to protect the refractory bricks and avoid damage from mechanical cleaning.
It extended the operating cycle of the rotary kiln, reduced the frequency of maintenance, improved the processing capacity of the unit, and saved production costs.
Abstract
Description
Technical Field
[0001] This invention relates to the field of rotary kiln incineration technology, and more specifically, to a method for removing coke from a rotary kiln. Background Technology
[0002] A rotary kiln incinerator is a cylindrical, continuously rotating device lined with refractory bricks. Its axis is installed at a slight angle to the horizontal. Typically, the kiln head is equipped with accessories such as a burner and a solid waste feed inlet. By controlling the burner and the solid waste feed rate, the waste inside the rotary kiln is incinerated.
[0003] Most hazardous waste incineration plants in China adopt a "rotary kiln + secondary combustion chamber" incineration mode. The rotary kiln can be used to process solid waste containing liquids or large volumes of solid waste. Solid waste, waste gas, and liquid waste can be fed into the rotary kiln. Utilizing the tilt angle and rotation characteristics of the rotary kiln, the solid waste entering the kiln slides downwards, causing the organic matter within to be incinerated. In the "rotary kiln + secondary combustion chamber" incineration mode, the secondary combustion chamber ensures the complete combustion of volatile organic compounds and organic matter entrained by suspended particulate matter in the gas.
[0004] The main residues left in the rotary kiln after combustion are ash and other non-combustible materials, primarily empty cans and the metal outer shells of solid waste packaging. These ash and other non-combustible materials are cooled and packaged after entering a slag cooler from the kiln tail due to the kiln's tilt angle and rotation.
[0005] Coking on the inner wall of a rotary kiln is a common phenomenon during the disposal of hazardous waste using this method. There are three main types of coking in rotary kilns: first, coking from low-melting-point salts; second, coking caused by incomplete combustion due to insufficient sealing at the kiln head leading to low kiln head temperature caused by excessive cold air or combustion air; and third, coking mainly at the kiln tail, primarily caused by insufficient sealing at the kiln tail allowing cold air to enter and evaporation of cooling water from the slag cooler.
[0006] Generally, the temperature at the center of a rotary kiln incinerator can reach 1100℃. The hazardous waste generated during industrial production is complex in composition, containing various low-melting-point salts and other substances. When these low-melting-point salts burn at this temperature, they form molten and semi-molten states. As the rotary kiln moves, they still exhibit viscosity or a molten state when in contact with the wall. Due to the different combustion positions within the rotary kiln, there are differences in the temperature of the inner wall of the rotary kiln. When the flue gas temperature of the surrounding wall is lower, the substances in the molten and semi-molten states will gradually adhere to the wall, forming a relatively dense layer of ash, i.e., coking.
[0007] Solid waste treatment systems using a rotary kiln + secondary combustion chamber share a common characteristic: the types of solid waste being treated are diverse and complex, making it impossible to guarantee the stability of the solid waste composition and calorific value. This leads to coking in the rotary kiln, a common problem in the industry. Severe coking in the rotary kiln necessitates a shutdown for maintenance. During maintenance, external force is required to clean the internal coking material. Because the hardness and other properties of refractory bricks or refractory mortar change after high-temperature calcination, they will inevitably be damaged by external force, significantly shortening their service life and affecting the stability and operating costs of the system. Summary of the Invention
[0008] The main objective of this invention is to provide a method for decoking rotary kilns, in order to solve the problem that the post-coking treatment of rotary kilns is difficult and affects the service life of rotary kilns in the prior art.
[0009] To achieve the above objectives, according to one aspect of the present invention, a method for decoking a rotary kiln is provided, the method comprising: step S1, heating and melting the coke in the rotary kiln to raise the temperature inside the rotary kiln to a first temperature to make the coke fluid; step S2, raising the temperature of the rotary kiln to a second temperature to allow the coke to flow out of the rotary kiln; and step S3, lowering the temperature of the rotary kiln and controlling the rotation speed of the rotary kiln to a third rotation speed to form a uniform coking layer inside the rotary kiln.
[0010] Furthermore, the softening temperature of the coke is T1℃, based on the kiln tail temperature of the rotary kiln, with the first temperature being (T1-15)℃~(T1+15)℃.
[0011] Furthermore, in step S1, the rotational speed of the rotary kiln is a first rotational speed, which is 0.2 to 0.3 r / min.
[0012] Furthermore, the hemispherical temperature of the coke is T2℃, based on the kiln tail temperature of the rotary kiln, and the second temperature is (T2-25)℃~(T2+25)℃.
[0013] Furthermore, in step S2, the coking material is cooled by a slag cooler to obtain solid waste residue.
[0014] Furthermore, in step S2, the rotational speed of the rotary kiln is the second rotational speed. The second rotational speed is adjusted according to the slag discharge speed. When the slag discharge speed is 3-4 t / h, the second rotational speed is adjusted to 0.2-0.25 r / min. When the slag discharge speed is greater than 4 t / h, the second rotational speed is adjusted to 0.25-0.3 r / min. When the slag discharge speed is less than 3 t / h, the second rotational speed is adjusted to 0.15-0.2 r / min.
[0015] Furthermore, taking the kiln tail temperature of the rotary kiln as the standard, the temperature reduction rate of the rotary kiln is 15-30℃ / h.
[0016] Furthermore, in step S3, the rotational speed of the rotary kiln is the third rotational speed, which is 0.35-0.45 r / min.
[0017] Furthermore, the thickness of the coking layer is H, and H satisfies 10%*L*sinα≤H≤25%*L*sinα, where L represents the length of the rotary kiln in meters; and α represents the angle between the rotary kiln and the horizontal plane in degrees.
[0018] Furthermore, before proceeding to step S3, the slag output from the rotary kiln is 75% to 90% of the coking material, preferably 85% to 90%.
[0019] By utilizing the tilt and rotational characteristics of the rotary kiln, and controlling the heating temperature, the coke inside the kiln melts and flows out. Through a specific cooling method, a portion of the molten coke is retained inside the kiln after decoking, forming a uniform coke layer to protect the refractory bricks of the kiln wall. This decoking method is not only easy to implement but also avoids the damage to the refractory bricks or refractory mortar caused by mechanical decoking, which could affect the service life of the rotary kiln. Furthermore, the decoking method of this application can significantly extend the operating cycle of the rotary kiln, shorten routine shutdowns for maintenance, and greatly increase the processing capacity of the equipment. In addition, the thermal expansion and contraction of the refractory bricks inside the rotary kiln during start-up and shutdown due to maintenance reduces the frequency of maintenance, effectively extending the service life of the rotary kiln refractory bricks and significantly saving production costs. Detailed Implementation
[0020] It should be noted that, unless otherwise specified, the embodiments and features described in this application can be combined with each other. The present invention will now be described in detail with reference to the embodiments.
[0021] As analyzed in the background section of this application, the existing technology suffers from difficulties in processing coking material in rotary kilns, which affects their service life. To solve this problem, this application provides a method for decoking rotary kilns. The method includes: step S1, raising the temperature inside the rotary kiln to a first temperature to heat-dissolve the coking material inside the rotary kiln until the coking material becomes fluid; step S2, raising the temperature of the rotary kiln to a second temperature to allow the coking material to flow out of the rotary kiln; and step S3, uniformly lowering the temperature of the rotary kiln and controlling the rotation speed of the rotary kiln to a third rotation speed to form a uniform coking layer inside the rotary kiln.
[0022] The aforementioned rotary kiln decoking method utilizes the kiln's inclination and rotational characteristics. By controlling the heating temperature, the coke inside the kiln melts and flows out. Through a specific cooling method, a portion of the molten coke is retained inside the kiln after decoking, forming a uniform coke layer that protects the refractory bricks of the kiln wall. This decoking method is not only easy to implement but also avoids the damage to the refractory bricks or refractory mortar caused by mechanical decoking methods, which could affect the service life of the rotary kiln. Furthermore, the decoking method of this application can significantly extend the rotary kiln's operating cycle, shorten routine shutdowns for maintenance, and greatly release the unit's processing capacity. Additionally, the thermal expansion and contraction of the refractory bricks inside the rotary kiln during start-up and shutdown due to maintenance reduces the frequency of maintenance, effectively extending the service life of the rotary kiln's refractory bricks and significantly saving production costs.
[0023] In step S1 above, the coke in the rotary kiln is heated to melt it and make it fluid. The heating method can be selected from existing technologies, such as introducing fuel, such as natural gas or coal, into the rotary kiln for combustion to provide heat and raise the temperature of the coke. In some typical embodiments of this application, the softening temperature of the coke is T1℃, based on the kiln tail temperature of the rotary kiln. The aforementioned first temperature is (T1-15)℃~(T1+15)℃. For example, if the softening temperature T1 of the coke is 1100℃, then the aforementioned first temperature is 1085℃~1115℃. Preferably, the first temperature is the softening temperature of the coke, which helps to improve the decoking efficiency and reduce energy consumption.
[0024] If the coking material at the kiln tail cancels out the tilt angle of the rotary kiln, it will prevent normal slag discharge. Therefore, priority should be given to dissolving the coking material at the kiln tail to avoid the accumulation of molten coking material inside the kiln due to the inability to discharge slag normally. For the same reason, the first temperature mentioned above and the second temperature introduced later are based on the temperature at the kiln tail of the rotary kiln, that is, it is preferable to ensure that the coking material at the kiln tail can flow out of the rotary kiln.
[0025] During the process, the tilt angle of the rotary kiln can be adjusted according to the site conditions, without any special requirements.
[0026] In some embodiments of this application, the rotational speed of the rotary kiln in step S1 is a first rotational speed. In order to take into account the uniformity of heating of each part of the rotary kiln and to save energy, the first rotational speed is 0.2 to 0.3 r / min.
[0027] In step S2 above, the process continues under heating to allow the coke to flow out of the rotary kiln. In some typical embodiments of this application, in order to ensure the fluidity of the coke and its smooth flow out of the rotary kiln, the hemispherical temperature of the coke is T2℃, and based on the kiln tail temperature of the rotary kiln, the second temperature is (T2-25)℃~(T2+25)℃.
[0028] The softening temperature and hemispherical temperature of the coke can be obtained by testing samples of the coke from the brick kiln, or by relevant indicators such as the type of incinerated material.
[0029] The coking material flowing out of the rotary kiln has a very high temperature. In order to improve the safety of the process, the coking material is cooled down first. In some embodiments of this application, the coking material in step S2 is cooled by a slag cooler to obtain solid waste slag.
[0030] In the decoking process described in step S2, the rotational speed of the rotary kiln can be adjusted according to the slag discharge rate to further improve the decoking efficiency. In some embodiments of this application, the rotational speed of the rotary kiln is a second rotational speed. When the slag discharge rate is 3-4 t / h, the second rotational speed is adjusted to 0.2-0.25 r / min; when the slag discharge rate is greater than 4 t / h, the second rotational speed is adjusted to 0.25-0.3 r / min; and when the slag discharge rate is less than 3 t / h, the second rotational speed is adjusted to 0.15-0.2 r / min. This can effectively improve the decoking efficiency of the rotary kiln while also considering energy consumption.
[0031] Step S3 above involves retaining a portion of the molten coke after decoking to a certain extent. By lowering the temperature and controlling the rotary kiln rotation speed, a uniform coke layer is formed inside the rotary kiln to protect the refractory bricks. In some preferred embodiments of this application, the kiln tail temperature is used as the benchmark, and the temperature reduction rate of the rotary kiln is 15–30 °C / h. At this rate of cooling, the coke layer retained on the rotary kiln is more uniform and has higher strength, further improving the protective effect on the refractory bricks. In step S3, the rotary kiln rotation speed is the third rotation speed, preferably 0.35–0.45 r / min, resulting in a more uniform coke layer.
[0032] In some embodiments of this application, after the above treatment, the thickness H of the coking layer is such that H satisfies 10%*L*sinα≤H≤25%*L*sinα, where L represents the length of the rotary kiln (m) and α represents the angle between the rotary kiln and the horizontal plane (°). The coking material inside the rotary kiln is effectively removed, and the remaining small amount of coking material is uniformly attached to the inner wall of the rotary kiln, protecting the refractory bricks and significantly improving the service life of the rotary kiln.
[0033] The rotary kiln is decoked using the method described above, and there are no special requirements regarding the amount of coke buildup. However, excessively high decoking frequency will reduce the operating efficiency of the rotary kiln, while prolonged neglect of decoking will lead to coke blockage in the furnace, hindering the flow of combustion products. Those skilled in the art can determine whether the coke buildup in the rotary kiln is affecting its normal operation based on specific circumstances, thus deciding whether decoking is necessary. In some embodiments of this application, when the amount of coke buildup before decoking has reached a level affecting the normal operation of the rotary kiln, the slag discharge from the rotary kiln before step S3 is 75%–90% of the weight of the coke material. This retains an appropriate amount of coke, protecting the refractory bricks on the inner wall of the rotary kiln while maintaining its operating efficiency. Preferably, the slag discharge from the rotary kiln is 85%–90% of the weight of the coke material, which better balances the service life and operating efficiency of the rotary kiln.
[0034] The amount of coke deposited can be calculated based on the feed rate, ash content, and fly ash production of the rotary kiln. The feed rate is the total solid waste treated by the rotary kiln from the end of the previous coke melting process to the current coke melting process. The ash content is the ash content (%) in the feed measured using the total ash content determination method. The fly ash production is obtained by weighing the fly ash generated by the bag filter from the end of the previous coke melting process to the current coke melting process. In some embodiments of this application, a total of 567 tons of solid waste was treated from the previous coke melting process to the current coke melting process, of which the ash content was 9.68% and the fly ash generated by the bag filter was 5.63 tons. Before this decoking treatment, the amount of coke deposited was 567 tons * 9.68% - 5.63 tons = 49.26 tons. The amount of slag discharged after treatment was 75-85 wt% of the total coke deposits. Operating according to this method can reduce the rotary kiln's operating cycle from once every 3 months to once every 9 months, significantly increasing the unit's processing capacity. Furthermore, the reduced maintenance frequency effectively extends the service life of the rotary kiln's refractory bricks, greatly saving production costs.
[0035] The beneficial effects that this application can achieve will be further illustrated below with reference to embodiments and comparative examples.
[0036] Example 1
[0037] This facility primarily handles hazardous waste classified as HW04 and HW11 in the National Hazardous Waste Catalogue. The ash melting points of the slag, measured using a closed furnace method, are: deformation temperature 1129℃, softening temperature 1139℃, hemispherical temperature 1193℃, and flow temperature 1206℃. The rotary kiln has a length L = 16m and an inclination angle α = 3°.
[0038] Heating: Adjust the frequency converter of the rotary kiln trolley motor to reduce the rotary kiln speed to 0.3 r / min, so that the coking material inside can store heat. At the same time, raise the temperature of the tail of the rotary kiln to the softening temperature of 1139℃ so that the coking material inside the kiln can be melted and have a certain fluidity. The flow is ensured by the tilt of the rotary kiln and the rotation characteristics of the rotary kiln itself.
[0039] Coking removal: Control the fuel flow rate to keep the temperature at the tail end of the rotary kiln at around 1192℃ to ensure the fluidity of the coking material. After the coking material flows out, use a slag cooler to remove the waste residue. The slag output is 4.2t / h. Adjust the rotary kiln speed by 0.25r / min in a timely manner according to the slag output to control the outflow rate of the hot-melt coking material.
[0040] Coke application: 1) Estimated slag output: After the last coke melting, the unit processed a total of 500t, with an ash content of 9.21%. The fly ash generated by the bag filter was 4.98t, and the estimated slag output was 30.80-34.91t. The actual slag output this time was 31.21t, and the coking material was retained to form an 8-9cm coking layer; 2) Coke application speed adjustment: Adjust the fuel flow rate to control the rotary kiln cooling rate to 30℃ / h, and at the same time adjust the rotary kiln speed to 0.45r / min to form a uniform coking layer inside the rotary kiln to protect the refractory bricks.
[0041] The rotary kiln, which is regularly treated by this decoking method, is overhauled every 9 months. The rotary kiln has been in normal use for 15 months.
[0042] Example 2
[0043] The difference from Example 1 is that in the coking process, the coking layer thickness is 7-8 cm. After the coking process is completed, it is found that the temperature of the rotary kiln head shell rises by 32-40°C, which leads to a high temperature of the rotary kiln shell and affects normal operation.
[0044] Rotary kilns that undergo regular decoking should be inspected every 4 months, and the service life of the rotary kiln is 12 months.
[0045] Example 3
[0046] The difference from Example 1 is that in the coking process, the coking layer thickness is 22-25cm. Compared with Example 1, the interval between coking in the rotary kiln is shortened from 12 days / time to 7 days / time. The frequency of coking in the rotary kiln is increased. The softening temperature and hemispherical temperature of the coking material continue to rise to the maximum tolerance temperature of the rotary kiln refractory bricks, making high-temperature coking impossible. Compared with Example 1, the maintenance time is reduced from once in September to once in May.
[0047] Rotary kilns that undergo regular decoking should be inspected every 5 months, and the service life of the rotary kiln is 10 months.
[0048] Example 4
[0049] The difference from Example 1 is that in the coke-coating process, a second rotation speed of 0.25 r / min is used for coke coating. The formation of spherical coke deposits inside the rotary kiln results in the formation of an uneven coking layer, and the spherical coke deposits cause the surface of the refractory bricks to be in a worn state.
[0050] Rotary kilns that undergo regular decoking should be inspected every 4 months, and the service life of the rotary kiln is 8 months.
[0051] Comparative Example 1
[0052] The slag ash is the same as in Example 1.
[0053] Heating: Adjust the frequency converter of the rotary kiln trolley motor to reduce the rotary kiln speed to 0.3 r / min, so that the coking material inside can store heat. At the same time, raise the temperature of the tail of the rotary kiln to the softening temperature of 1139℃ so that the coking material inside the kiln can be melted and have a certain fluidity. The flow is ensured by the tilt of the rotary kiln and the rotation characteristics of the rotary kiln itself.
[0054] Coking removal: Control the fuel flow rate to maintain the rotary kiln tail temperature at approximately 1192℃, ensuring the fluidity of the coke. After the coke flows out, use a slag cooler to remove the waste residue at a rate of 4 t / h. Adjust the rotary kiln speed by 0.25 r / min based on the slag output to control the outflow rate of the hot-melt coke. Stop coking removal when no more coke flows out of the rotary kiln; no further coke adhering treatment is required.
[0055] Rotary kilns that undergo regular decoking should be inspected every 4 months, and the service life of the rotary kiln is 9 months.
[0056] Comparative Example 2
[0057] The slag ash is the same as in Example 1.
[0058] The difference from Example 1 is that the rotary kiln was not subjected to high-temperature coking according to the technical solution of this application. The rotary kiln was inspected once a month and mechanical external force was used for coking removal. The service life of the rotary kiln was 4 months.
[0059] As can be seen from the above description, the embodiments of the present invention achieve the following technical effects: Utilizing the tilt angle and rotational characteristics of the rotary kiln, by controlling the heating temperature, the coke inside the kiln melts and flows out of the rotary kiln. Through a specific cooling method, after decoking, a portion of the molten coke is retained inside the rotary kiln, forming a uniform coke layer to protect the refractory bricks of the kiln wall. The above decoking method is not only easy to implement, but also avoids the damage to the refractory bricks or refractory mortar of the kiln wall caused by mechanical decoking, which would affect the service life of the rotary kiln. Furthermore, the decoking method of this application can significantly extend the operating cycle of the rotary kiln, shorten routine shutdowns for maintenance, and greatly release the processing capacity of the device. In addition, during the start-up and shutdown processes caused by maintenance, the refractory bricks inside the rotary kiln will experience thermal expansion and contraction. The reduced maintenance frequency can effectively extend the service life of the rotary kiln refractory bricks and greatly save production costs.
[0060] The above description is merely a preferred embodiment of the present invention and is not intended to limit the invention. Various modifications and variations can be made to the present invention by those skilled in the art. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of the present invention should be included within the scope of protection of the present invention.
Claims
1. A method of decoking a rotary kiln, characterized in that, include: Step S1: The coking material in the rotary kiln is heated and melted to raise the temperature in the rotary kiln to a first temperature, making the coking material fluid; the softening temperature of the coking material is T1℃, based on the kiln tail temperature of the rotary kiln, the first temperature is (T1-15)℃~(T1+15)℃; the rotation speed of the rotary kiln is a first rotation speed, the first rotation speed is 0.2~0.3r / min; Step S2: The temperature of the rotary kiln is raised to a second temperature, causing the coke to exit the rotary kiln. The coke is cooled by a slag cooler to obtain solid waste. The hemispherical temperature of the coke is T2℃, based on the kiln tail temperature of the rotary kiln. The second temperature is (T2-25)℃~(T2+25)℃. The rotation speed of the rotary kiln is the second rotation speed, which is adjusted according to the slag discharge rate. When the slag discharge rate is 3~4t / h, the second rotation speed is adjusted to 0.2~0.25r / min; when the slag discharge rate is greater than 4t / h, the second rotation speed is adjusted to 0.25~0.3r / min; when the slag discharge rate is less than 3t / h, the second rotation speed is adjusted to 0.15~0.2r / min. Step S3: Reduce the temperature of the rotary kiln and control the rotation speed of the rotary kiln to a third rotation speed of 0.35-0.45 r / min to form a uniform coking layer inside the rotary kiln; based on the kiln tail temperature, the temperature reduction rate of the rotary kiln is 15~30℃ / h.
2. The decoking method of a rotary kiln according to claim 1, characterized in that, The thickness of the coking layer is H, and H satisfies 10%*L*sinα≤H≤25%*L*sinα, where L represents the length of the rotary kiln in meters and α represents the angle between the rotary kiln and the horizontal plane in degrees.
3. The rotary kiln decoking method according to claim 1, characterized in that, Before performing step S3, the slag output of the rotary kiln is 75% to 90% of the coking material.
4. The rotary kiln decoking method according to claim 3, characterized in that, Before performing step S3, the slag output of the rotary kiln is 85% to 90% of the coking material.
Citation Information
Patent Citations
Wear-resistant protective layer structure of circulating fluidized bed boiler cyclone targeting area