Secondary batteries
By designing separation grooves on the electrode leads of the secondary battery, the safety problem caused by expansion is solved, enabling rapid breakage and blocking of the current path under high temperature and high pressure, thus enhancing the safety of the battery.
Patent Information
- Application Number
- CN202280011610.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2021-10-12
- Filing Date
- 2022-10-11
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2042-10-11
AI Technical Summary
Existing secondary batteries are prone to localized short circuits, fires, or explosions due to expansion under conditions such as overcharging or internal short circuits, lacking effective safety guarantees.
Separation grooves are designed on the electrode leads. These grooves are located in areas that do not correspond to the lead film and are not exposed outside the housing. They enhance safety by breaking and blocking the current path under high temperature and high pressure.
The separation groove through the electrode leads breaks rapidly under high temperature and high pressure, blocking the current path, improving the safety of the secondary battery, and preventing fire or explosion.
Smart Images

Figure CN116802923B_ABST
Abstract
Description
Technical Field
[0001] This disclosure relates to secondary batteries, and more specifically, to secondary batteries whose safety is improved by modifying the structure of the electrode leads. This application claims priority to Korean Patent Application No. 10-2021-0135349, filed on October 12, 2021, the disclosure of which is incorporated herein by reference. Background Technology
[0002] Secondary batteries, due to their product mix and electrical characteristics such as high energy density, are highly practical and therefore widely used not only in portable devices but also in electric vehicles (EVs) or hybrid electric vehicles (HEVs) powered by electric power sources. These secondary batteries are gaining attention as a new energy source that improves environmental friendliness and energy efficiency because they not only offer the major advantage of significantly reducing fossil fuel use but also produce no byproducts of energy consumption.
[0003] Generally, a secondary battery consists of a positive electrode, a negative electrode, a separator separating them, an electrolyte that carries lithium ions through the separator, a casing that houses them, and electrode leads that serve as paths for current to leave the casing. Typically, lead films are used to seal the electrode leads and the casing, while also preventing short circuits between the electrode leads and the casing by being bonded to such electrode leads.
[0004] In this type of secondary battery, when the internal temperature rises due to overcharging exceeding the allowable current or voltage, internal short circuits, or other reasons, the internal pressure increases due to electrolyte vaporization, resulting in a phenomenon known as expansion. When expansion occurs, partial short circuits may occur due to battery deformation, and in extreme cases, the battery may catch fire or explode.
[0005] Therefore, when expansion occurs due to overcharging, there is a need to develop technologies that can fundamentally eliminate the risks associated with overcharging and greatly improve safety by limiting the flow of current. Summary of the Invention
[0006] Technical issues
[0007] This disclosure aims to address the problems in the related technology, and therefore aims to provide a secondary battery that can ensure safety by implementing a current blocking function based on an increase in internal pressure.
[0008] Technical solution
[0009] A secondary battery according to one aspect of the present disclosure for solving the above-mentioned problems includes: an electrode assembly to which electrode leads are attached; a housing that houses the electrode assembly such that a portion of the electrode leads is exposed to the outside; a sealing portion formed in the housing to seal the electrode assembly; and a lead membrane that covers a portion of the outer surface of the electrode leads and is inserted between the electrode leads and the sealing portion, wherein the electrode leads include a first region that does not correspond to the lead membrane and is exposed to the outside of the housing, a second region that corresponds to the lead membrane, and a third region that does not correspond to the lead membrane and is not exposed to the outside of the housing, wherein a separation groove is located in the third region.
[0010] The separation tank may be additionally located in the first region.
[0011] In this case, the separation groove in the third region and the separation groove in the first region can be located on opposite sides of the electrode leads, respectively.
[0012] The separation groove can be formed as a strip that spans the width of the electrode leads.
[0013] The separation channel can have a dashed line shape.
[0014] In this case, the width of the dashed line can be 5% to 50% of the width of the electrode lead.
[0015] The length between the points on the dashed line can be 5% to 50% of the width of the electrode lead.
[0016] The ratio of the width of the dashed line to the length between the points of the dashed line is 5:1 to 1:5.
[0017] The cross-section of the separation tank can be any of the following: wedge-shaped, circular, or square.
[0018] The separation tank can be filled with an insulating film.
[0019] The separation tank can be covered with an insulating film.
[0020] In this case, there can be empty space inside the separation tank.
[0021] The insulating film may include polypropylene, polyethylene, polyimide, or two or more of them.
[0022] Preferably, the lead film comprises polyethylene.
[0023] The secondary battery can be a pouch-type secondary battery.
[0024] In the secondary battery according to this disclosure, the third region may not correspond to the sealing portion, and the width of the lead film may be wider than the width of the sealing portion.
[0025] The separation groove can be formed to connect one end of the electrode lead to the other end in a direction orthogonal to the extension direction of the electrode lead.
[0026] The separation groove can be a region in which a portion of the thickness of the electrode lead decreases along the width direction of the electrode lead.
[0027] The separation groove can be a groove that is recessed in the thickness direction from the surface of the electrode lead.
[0028] The separation tank does not have to be formed by connecting one end of the electrode lead to the other end, but can be divided into multiple parts, and there may be no continuity between the separation tanks.
[0029] Technical effect
[0030] In the secondary battery according to an embodiment of the present disclosure, the separation groove is located on the electrode leads that do not correspond to the lead film and are not exposed to the outside of the casing, so that the electrode leads break rapidly when the internal pressure of the battery increases, thereby ensuring safety.
[0031] According to this disclosure, the separation groove located on the electrode leads of the secondary battery can be designed to break when high temperature and high pressure are applied to the secondary battery. Therefore, when the temperature of the secondary battery runs out or the internal pressure of the secondary battery increases, the electrode leads can be cut at the separation groove. When the electrode leads break at the separation groove, the current path to the electrode assembly is completely blocked. Therefore, battery safety can be enhanced by forcibly decoupling the electrical connection structure.
[0032] In a secondary battery according to another embodiment of the present disclosure, the internal pressure at the time of electrode lead breakage can be controlled by adjusting the position and number of separation grooves. Specifically, when two separation grooves are located on opposite sides of the electrode lead, a stronger stress can be applied to the separation grooves, thus making the electrode lead more likely to break quickly.
[0033] According to this disclosure, an advantage lies in providing a thermal safety device even in pouch cells by placing a separation groove on the electrode leads and forcibly detaching the electrical connection at the separation groove. Pouch cells do not have a PTC or CID that operates during cell temperature runaway as is the case with cylindrical cells, but if a separation groove is formed on the electrode leads according to this disclosure, it can operate as a safety device in the event of cell temperature runaway. Therefore, preparations can be made for the risk of fire. Attached Figure Description
[0034] The accompanying drawings illustrate preferred embodiments of the present disclosure and, together with the foregoing disclosure, are intended to provide a further understanding of the technical features of the present disclosure. Therefore, the present disclosure should not be construed as being limited to the drawings.
[0035] Figure 1This is a plan view showing a secondary battery according to an embodiment of the present disclosure.
[0036] Figure 2 This is an enlarged plan view showing the electrode leads in a secondary battery according to an embodiment of the present disclosure.
[0037] Figure 3 This is an enlarged plan view showing the electrode leads in a secondary battery according to another embodiment of the present disclosure.
[0038] Figure 4 This is an enlarged perspective view showing the electrode leads in a secondary battery according to yet another embodiment of the present disclosure.
[0039] Figure 5 This is an enlarged perspective view showing the electrode leads in a secondary battery according to yet another embodiment of the present disclosure.
[0040] Figure 6 This is an enlarged exploded perspective view showing the electrode leads in a secondary battery according to yet another embodiment of the present disclosure.
[0041] Figure 7 This is an enlarged exploded perspective view showing the electrode leads in a secondary battery according to another embodiment of the present disclosure.
[0042] Figures 8 to 12 This is a graph showing the results of stress analysis when internal pressure is applied to the electrode lead portion of a secondary battery according to an example.
[0043] Figures 13 to 16 This is a graph showing the results of stress analysis when internal pressure is applied to the electrode lead portion of the secondary battery according to the comparative example. Detailed Implementation
[0044] Preferred embodiments of the present disclosure will be described in detail below with reference to the accompanying drawings. Before the description, it should be understood that the terminology used in the specification and appended claims should not be construed as limited to its general and dictionary meaning, but rather interpreted based on the meaning and concepts corresponding to the technical aspects of the present disclosure, on the basis of allowing the inventors to appropriately define the terminology for the best interpretation.
[0045] Therefore, the description presented herein is merely a preferred example for illustrative purposes only and is not intended to limit the scope of this disclosure. It should be understood that other equivalent substitutions and modifications may be made thereto without departing from the scope of this disclosure.
[0046] A secondary battery according to one aspect of the present disclosure includes: an electrode assembly with attached electrode leads; a housing housing the electrode assembly such that a portion of the electrode leads is exposed to the outside; a sealing portion formed in the housing to seal the electrode assembly; and a lead membrane covering a portion of the outer surface of the electrode leads and inserted between the electrode leads and the sealing portion, wherein the electrode leads include a first region not corresponding to the lead membrane and exposed to the outside of the housing, a second region corresponding to the lead membrane, and a third region not corresponding to the lead membrane and not exposed to the outside of the housing, wherein a separation groove is located in the third region.
[0047] Figure 1 This is a plan view showing a secondary battery according to an embodiment of the present disclosure.
[0048] Reference Figure 1 According to an embodiment of the present disclosure, the secondary battery 10 includes an electrode assembly 12 with electrode leads 11 attached and a housing 13.
[0049] The electrode assembly 12 includes a positive electrode plate, a negative electrode plate, and a separator. The electrode assembly 12 can be formed by sequentially stacking the positive and negative electrode plates and inserting the separator between them.
[0050] The positive electrode plate can be formed as a positive current collector made of a thin metal plate (e.g., aluminum (Al) foil) with excellent conductivity and a layer of positive active material coated on at least one surface thereon. Additionally, the positive electrode plate may include a positive electrode connector at one end made of a metallic material such as aluminum. The positive electrode connector may extend and protrude from one end of the positive electrode plate, or it may be soldered to one end of the positive electrode plate or bonded using a conductive adhesive.
[0051] The negative electrode plate may include a negative current collector made of a thin conductive metal plate (e.g., copper (Cu) foil) and a layer of negative active material coated on at least one surface thereon. Additionally, the negative electrode plate may include a negative electrode connector at one end made of a metallic material such as copper or nickel (Ni). The negative electrode connector may extend and protrude from one end of the negative electrode plate, or it may be soldered to one end of the negative electrode plate or bonded using a conductive adhesive.
[0052] A separator is inserted between the positive and negative electrode plates to electrically insulate them from each other, and can be formed into a porous membrane shape to allow lithium ions to pass through between the positive and negative electrode plates. The separator may comprise a porous membrane using, for example, polyethylene (PE), polypropylene (PP), or composites thereof.
[0053] An inorganic coating layer can be formed on the surface of the diaphragm. The inorganic coating layer can have a structure in which inorganic particles are bonded together by a binder to form interstitial volumes between the particles.
[0054] The electrode assembly 12 includes: a wound electrode assembly having a structure in which long sheet-shaped positive and negative electrodes are wound with a separator inserted between them; a stacked electrode assembly in which a plurality of positive and negative electrodes cut in units of predetermined size are stacked sequentially with a separator inserted between them; and a stacked / folded electrode assembly having a structure in which a predetermined unit of positive and negative electrodes is stacked with a separator inserted between them, and a dual-cell or full-cell wound structure.
[0055] The housing 13 includes a receiving portion 13a for accommodating the electrode assembly 12, a sealant resin, and a sealing portion 13b formed to seal the electrode assembly 12.
[0056] The sealing portion 13b refers to the portion that is melted along the outer peripheral surface of the receiving portion 13a to seal the electrode assembly 12. The melting can be thermal melting, ultrasonic melting, etc., but there are no particular restrictions as long as the sealing portion can be melted.
[0057] In embodiments of this disclosure, the housing 13 may be configured as a membrane with a multilayer structure having an outer layer for external impact protection, a metal barrier layer for blocking moisture, and a sealant layer for sealing the housing.
[0058] The outer layer may include polyester-based films such as polyethylene terephthalate (PET), polybutylene terephthalate, polyethylene naphthalate, polybutylene naphthalate, copolyester, polycarbonate, nylon, etc., and may consist of a single layer or multiple layers.
[0059] Metal barrier layers can include aluminum, copper, etc.
[0060] The sealant layer may include a sealant resin and may consist of a single layer or multiple layers.
[0061] The sealant resin may include polypropylene, acid-modified polypropylene (PPa), atactic polypropylene, ethylene-propylene copolymer, or two or more thereof. Ethylene-propylene copolymer may include, but is not limited to, ethylene-propylene rubber, ethylene-propylene block copolymer, etc.
[0062] In embodiments of this disclosure, the housing 13 may be in the form of a bag.
[0063] In embodiments of this disclosure, when the housing 13 is in the form of a bag, it may include an upper bag and a lower bag. When the housing 13 includes an upper bag and a lower bag, the outer peripheral surfaces of the upper bag and the lower bag can be melted together by heat and pressure, thereby sealing the battery.
[0064] When the housing is in the form of a bag, the sealing portion 13b can be sealed on four or three sides at the edge of the housing 13. The three-side sealing structure refers to the following structure: the edges of the three sides other than the bent portion are sealed when the upper and lower bags are formed into a single bag sheet, and then the boundary surfaces of the upper and lower bags are bent to overlap with the receiving portion 13a formed in the upper and lower bags. Figure 1 The figure can be described as showing the receiving portion 13a formed in the lower bag before the upper bag is covered.
[0065] Electrode leads 11 serve as current paths and are made of metallic material. As for the material, any metal that is conductive can be used.
[0066] Electrode leads 11 can be attached to electrode assembly 12 by connecting to negative and positive terminals. Electrode leads 11 can be housed in housing 13, with a portion of them exposed outside housing 13.
[0067] The electrode lead 11 connected to the negative terminal is called the negative lead, and the electrode lead 11 connected to the positive terminal is called the positive lead. These electrode leads 11 can extend in the same direction or in opposite directions. In this embodiment, the electrode leads 11 are arranged in the same direction relative to the length direction (X direction) of the battery and extend along the length direction of the battery. In addition, they are positioned side by side along the width direction (Y direction) of the battery.
[0068] Electrode lead 11 can be a rectangular component, wherein the length L along the length direction of the battery is greater than the width W along the width direction of the battery. Electrode lead 11 extends along the length direction. Electrode lead 11 can have a thickness (Z direction, see...) Figure 3 d) is a sheet-like member with a width W and a length L smaller than the sheet-like member. Finally, electrode leads 11 are electrically connected to external terminals.
[0069] The positive and negative leads can be made of different materials. That is, the positive lead can be made of the same aluminum material as the positive plate, and the negative lead can be made of the same copper material or nickel-plated copper material as the negative plate.
[0070] The lead film 14 covers a portion of the outer surface of the electrode lead 11 and is inserted between the electrode lead 11 and the sealing portion 13b of the protruding part of the electrode lead 11. The lead film 14 is inserted between the electrode lead 11 and the sealing portion 13b of the protruding part of the electrode lead to help bond the electrode lead 11 to the sealing portion 13b. The lead film 14 can be thermally fused to the housing 13.
[0071] The lead film 14 not only prevents short circuits between the electrode lead 11 and the metal layer (e.g., aluminum sheet) of the housing 13, but also prevents leakage of electrolyte and the like by increasing the sealing force of the housing 13.
[0072] In embodiments of this disclosure, the lead film 14 may comprise polyimide (PI), polypropylene, polyethylene, polyethylene terephthalate, or two or more of these. Specifically, when the lead film 14 comprises polyethylene, polyethylene has a low melting point and therefore can melt rapidly at high temperatures. Polypropylene has a melting point of about 160°C, and polyethylene has a melting point of about 120°C to 130°C. Therefore, the electrode lead 11 with the separation groove 15, described later, may be more prone to breakage.
[0073] When expansion occurs due to overcharging or other factors in related technologies, local short circuits may occur as the battery deforms, and in extreme cases, the battery may catch fire or explode.
[0074] The inventors of this disclosure have discovered that this risk can be greatly reduced by disconnecting the electrode lead itself to block the path of receiving current from the outside, thus completing this disclosure. The electrode lead 11 is designed to break when high temperature and high pressure are applied to the secondary battery 10. To this end, a separation groove 15 is formed in the electrode lead 11 to pre-cut a portion of the electrode lead 11. Thus, when the temperature of the secondary battery 10 runs out or the internal pressure of the secondary battery 10 increases, the electrode lead 11 can be cut at the separation groove 15 portion.
[0075] Figure 2 This is an enlarged plan view showing the electrode leads in a secondary battery according to an embodiment of the present disclosure.
[0076] Reference Figure 2 The electrode lead 11 includes a first region 100 that does not correspond to the lead film 14 and is exposed outside the housing 13, a second region 200 that corresponds to the lead film 14, and a third region 300 that does not correspond to the lead film 14 and is not exposed outside the housing 13. The third region 300, the second region 200, and the first region 100 are arranged in the length direction of the electrode lead 11 (i.e., along the extension direction of the electrode lead 11) in order from the portion closest to the electrode assembly 12 to the portion furthest from the portion closest to the electrode assembly 12.
[0077] In embodiments of this disclosure, the third region 300 may not correspond to the lead film 14, may not correspond to the sealing portion 13b of the housing 13, and may be a region not exposed to the outside of the housing 13. For example, the third region 300 may be a region whose width w_LF of the lead film 14 is wider than the width w_S of the sealing portion 13b, and which does not correspond to the lead film 14, does not correspond to the sealing portion 13b of the housing 13, and is not exposed to the outside of the housing 13. Here, the width w_LF of the lead film 14 refers to the maximum value of the distance between one end of the lead film 14 and the other end in the extension direction of the electrode lead 11. The width w_S of the sealing portion 13b refers to the maximum value of the distance between one end of the sealing portion 13b and the other end in the extension direction of the electrode lead 11.
[0078] Reference Figure 2 Separation groove 15 is located in the third region 300. Separation groove 15 is designed to prevent breakage when an external force, such as deformation of the housing 13, is applied, as the force accumulates at the interface where the separation groove 15 is formed. In other words, when the cell temperature runs out, the electrode lead 11 can be more easily broken and separated by the force applied while the housing 13 is expanding, thereby blocking further current flow and preventing extreme conditions, thus improving safety.
[0079] A separation groove 15 is formed along the width direction of the electrode lead 11. The separation groove 15 is formed in a straight line along a direction orthogonal to the extending direction of the electrode lead 11. The separation groove 15 can be formed from one end of the electrode lead 11 to the other end along a direction orthogonal to the extending direction of the electrode lead 11. The separation groove 15 is a region where the thickness of the electrode lead 11 decreases along the width direction of the electrode lead 11. For example, the separation groove 15 can be a recess from the surface of the electrode lead 11 in the thickness direction to a predetermined depth (see [link to documentation]). Figure 3 The groove of H in the separation groove 15. Therefore, when the electrode lead 11 breaks in the separation groove 15, the current path to the electrode assembly 12 is completely blocked.
[0080] In the secondary battery according to the embodiments of the present disclosure, unlike the conventional case where only a portion of the electrode connector breaks, the electrode lead 11 can be completely separated from the electrode assembly 12 when expansion occurs. Since the electrode lead 11 is completely separated from the electrode assembly 12, the current can be completely blocked.
[0081] On the other hand, since the lead film 14 is used to bond the electrode lead 11 and the sealing portion 13b of the housing 13, the electrode lead 11 is difficult to break quickly when the separation groove 15 is located at the part where the lead film 14 and the electrode lead 11 are in contact with each other.
[0082] In addition, since the electrode lead 11 and the sealing portion 13b form an adhesive force at the part where the electrode lead 11 contacts the sealing portion 13b, the electrode lead 11 is difficult to break quickly when the separation groove 15 is located at the part where the electrode lead 11 contacts the sealing portion 13b.
[0083] Therefore, when the separation groove 15 is located in the area where the lead film 14 and the electrode lead 11 do not correspond to each other and the electrode lead 11 is not exposed to the outside (e.g., the third region 300 corresponding to the interior of the battery compared to the sealed portion 13b), the electrode lead 11 can break quickly.
[0084] Furthermore, when the separation groove 15 is located in the third region 300, the region S1 between the separation groove 15 and the electrode lead 11, where the electrode lead 11 connects to the lower end of the electrode assembly 12, becomes narrower. Therefore, stronger stress can be concentrated in the separation groove 15, thus the electrode lead 11 can easily and quickly break.
[0085] By placing the separation groove 15 on the electrode lead 11 as described above, when the electrode lead 11 breaks at the separation groove 15, the electrical connection structure is forcibly released, thereby helping to enhance battery safety.
[0086] Figure 3 This is an enlarged plan view showing the electrode leads in a secondary battery according to another embodiment of the present disclosure.
[0087] Reference Figure 3 The separation groove 15 may also be additionally located in the first region 100. In embodiments of this disclosure, the first region 100 may be the area where the electrode lead 11 does not correspond to the lead film 14, does not correspond to the sealing portion 13b, and is exposed to the outside of the housing 13. When the separation groove 15 is located in the first region 100 in addition to being located in the third region 300, compared to the case where the separation groove 15 is only located in the third region 300, the stress can be more concentrated in the narrow region S2 between the separation groove 15 located in the first region 100 and the separation groove 15 located in the third region 300. Therefore, compared to the case where the separation groove 15 is only located in the third region 300, the electrode lead 11 can break more quickly.
[0088] In embodiments of this disclosure, the separation groove 15 located in the third region 300 and the separation groove 15 located in the first region 100 may be located on the same side of the electrode lead 11, respectively.
[0089] Here, "the same side of the electrode lead" refers to the surface of the electrode lead corresponding to the same side when the surface of the electrode lead 11 in contact with the housing 13 is taken as a reference. For example, the separation groove 15 located in the third region 300 and the separation groove 15 located in the first region 100 can be located on the upper surface of the electrode lead 11. Here, the upper surface can refer to the surface that is placed closer to the housing 13 along the thickness direction.
[0090] Figure 4 This is an enlarged perspective view showing the electrode leads in a secondary battery according to yet another embodiment of the present disclosure.
[0091] Reference Figure 4 The separation groove 15 located in the third region 300 and the separation groove 15 located in the first region 100 can be located on opposite sides of the electrode lead 11. For example, the separation groove 15 located in the third region 300 can be located on the lower surface of the electrode lead 11, while the separation groove 15 located in the first region 100 can be located on the upper surface of the electrode lead 11. Here, the upper surface can refer to the surface placed close to the housing 13 along the thickness direction, and the lower surface can refer to the surface located on the opposite side. When the separation groove 15 located in the third region 300 and the separation groove 15 located in the first region 100 are located on opposite sides of the electrode lead 11, the maximum stress applied near one separation groove 15 is not easily distributed to the other separation groove 15. Therefore, stronger stress can be applied to the separation groove 15, thereby making it easier for the electrode lead 11 to break quickly.
[0092] Here, "opposite side of the electrode lead" refers to the surface of the electrode lead that corresponds to the side of the electrode lead that is opposite to each other, when the surface of the electrode lead 11 in contact with the housing 13 is taken as a reference.
[0093] The separation tank 15 may have a shape suitable for separation so that physical and electrical barriers can be reliably implemented.
[0094] For example, such as Figures 2 to 4 As shown, the separation groove 15 can be formed as a strip that spans the width of the electrode lead 11. When the separation groove 15 is formed as a strip that spans the width of the electrode lead 11, the maximum stress is applied uniformly along the strip, so the electrode lead 11 can break more easily and quickly. In addition, the cutting area of the electrode lead 11 is very wide, which makes the electrode lead 11 easier to break quickly.
[0095] Alternative locations, such as Figure 5As shown, the separation groove 15 can have a dashed shape. Here, a dashed shape can mean that the separation groove 15 is not formed to connect one end of the electrode lead 11 to the other, but is divided into several sections, and there is no continuity between the separation grooves 15 due to the absence of intermediate separation grooves 15. When the separation groove 15 has a dashed shape, the electrode lead 11 can have greater stiffness under internal pressure under normal battery operating conditions, and the electrode lead 11 can easily and quickly break during abnormal battery operation. Furthermore, this can be used as a pressure sensing method to determine whether the battery is functioning properly.
[0096] Reference Figure 5 When the separation groove 15 has a dashed shape, the width a of the dashed line can be 5% to 50% of the width w of the electrode lead 11. When the width a of the dashed line meets the above-defined range, the electrode lead 11 can easily and quickly break, while maintaining rigidity under higher internal pressure.
[0097] In addition, refer to Figure 5 When the separation groove 15 has a dashed shape, the length b between the points of the dashed line can be 5% to 50% of the width w of the electrode lead 11. When the length b between the points of the dashed line meets the above-defined range, the electrode lead 11 can easily and quickly break, while maintaining rigidity under higher internal pressure.
[0098] In embodiments of this disclosure, when the separation groove 15 has a dashed line shape, the ratio of the width a of the dashed line to the length b between each point of the dashed line can be from 5:1 to 1:5. When the ratio of the width a of the dashed line to the length b between each point of the dashed line can satisfy the above-defined range, the electrode lead 11 can easily and quickly break, while maintaining rigidity under higher internal pressure.
[0099] Figure 6 This is an enlarged exploded perspective view showing the electrode leads in a secondary battery according to yet another embodiment of the present disclosure.
[0100] Reference Figure 6 The cross-section of the separation groove 15 along the extension direction of the electrode lead 11 can be square. The cross-section of the separation groove 15 can be wedge-shaped or circular, but there are no particular restrictions on the cross-sectional shape of the separation groove 15, as long as the electrode lead 11 can be broken quickly.
[0101] Reference Figure 6The separation groove 15 can be filled with an insulating film 16. Because the separation groove 15 is filled with an insulating film 16, the surface of the electrode lead 11 can be kept smooth. When the separation groove 15 is filled with an insulating film 16, foreign matter can be prevented from entering, and the electrode lead 11 can maintain rigidity under higher internal pressures under normal battery operating conditions. Additionally, the housing 13 can be protected from damage to the surface of the electrode lead 11 that may occur during the formation of the separation groove 15. Furthermore, since the separation groove 15 is located within the housing 13, the electrode lead 11 is protected when exposed to the electrolyte.
[0102] Figure 7 This is an enlarged exploded perspective view showing the electrode leads in a secondary battery according to another embodiment of the present disclosure.
[0103] Reference Figure 7 An insulating film 16 can be used to cover the separation tank 15. When the insulating film 16 covers the separation tank 15, it can partially cover the surface of the electrode leads 11 on both sides of the separation tank 15. Covering the separation tank 15 with the insulating film 16 can prevent foreign matter from flowing in, and the electrode leads 11 can maintain rigidity under higher internal pressures under normal battery operating conditions. In addition, the housing 13 can be protected from damage to the surface of the electrode leads 11 that may occur during the formation of the separation tank 15. Furthermore, since the separation tank 15 is located inside the housing 13, the electrode leads 11 can be protected when exposed to the electrolyte.
[0104] Reference Figure 7 When the insulating film 16 covers the separation groove 15, the insulating film 16 does not fill the interior of the separation groove 15, so there can be empty space inside the separation groove 15. Since the separation groove 15 is not filled, the stress concentration effect is excellent, and the separation groove 15 can break quickly.
[0105] In embodiments of this disclosure, the insulating film 16 may comprise polypropylene, polyethylene, polyimide, or two or more of these. Specifically, when the insulating film 16 is polypropylene, polyethylene, etc., it has a low melting point and can therefore melt rapidly at high temperatures. Consequently, the electrode leads can break more easily and quickly when the internal pressure of the battery increases.
[0106] Methods for forming the separation groove 15 include, for example, using a roller with a cutter on its surface, or using a frame equipped with a cutter, but are not limited thereto. When the electrode lead 11 is formed by a die-making method, the separation groove 15 may be included from the outset.
[0107] When forming the separation groove 15, the current path is ensured, and the depth H of the separation groove 15 can be adjusted to take into account the degree to which the battery may break rapidly when the internal pressure of the battery increases.
[0108] In embodiments of this disclosure, for example, Figure 3 The separation groove 15 can be formed to have a depth of more than 30% compared to the thickness d of the electrode lead 11. For example, when the thickness d of the electrode lead 11 is 0.4 mm, the depth H of the separation groove 15 can be 0.3 mm.
[0109] When forming the separation groove 15, the current path is ensured, and the width c of the separation groove 15 can be determined to account for the degree to which it can quickly break when the internal pressure of the battery increases. For example, the width c of the separation groove 15 can be 0.5 mm.
[0110] In this way, by adjusting the shape, size, number, and position of the separation grooves 15, the electrode leads 11 can be short-circuited under a desired internal pressure, and the internal pressure of the short circuit can be controlled. For example, if the shape of the separation grooves 15 is designed to have a stress concentration shape, it can cause more rapid breakage. If the depth H of the separation grooves 15 is increased, the separation grooves 15 may break even under lower internal pressure. This can also be used as a pressure sensing method to check whether the battery cell is normal, or it can also be used to perform battery cell inspection.
[0111] The separation groove 15 can be formed on at least one of the positive lead and the negative lead.
[0112] The separation groove 15 can be formed on either one of the surfaces of the electrode lead 11 that are in contact with the housing 13, or it can be formed on both one and the other surfaces of the electrode lead 11.
[0113] In embodiments of this disclosure, the secondary battery can be cylindrical, prismatic, or pouch-shaped. Among these, the secondary battery can be a pouch-shaped secondary battery. Pouch-shaped secondary batteries are easy to increase the volume ratio, but the disadvantage is that the pouch itself makes it difficult to hold the cell. Unlike cylindrical batteries with PTC or CID, pouch-shaped secondary batteries do not have thermal stability when the cell temperature runs out. According to this disclosure, an advantage is that a safety device is provided even in pouch-shaped secondary batteries by including a separation groove in the electrode leads and allowing the electrode leads to break at the separation groove portion to forcibly decouple the electrical connection.
[0114] When a secondary battery explodes, expansion typically occurs first. Furthermore, because secondary batteries pose a high risk of ignition due to significant temperature increases during operation, preparations must be made for this. According to this disclosure, preparations for the ignition risk can be made by including separation grooves in the electrode leads and allowing the electrode leads to break at the separation groove portion in the event of thermal runaway of the secondary battery.
[0115] In the following detailed description, with reference to examples, this disclosure will be readily understood. However, the following examples may be embodied in many different forms and should not be construed as limiting oneself to the exemplary embodiments set forth herein. Rather, these exemplary embodiments are provided so that this disclosure will be thorough and complete, and will fully convey the scope of this disclosure to those skilled in the art. As in this disclosure, the stress applied to the electrode leads is analyzed through simulation experiments for cases with and without separation channels. For ease of analysis, the analysis is performed under the assumption of a relatively short battery length. Embodiments and comparative examples are prepared under the following conditions.
[0116] Example 1
[0117] The electrode assembly, stacked in the order of positive electrode / separator / negative electrode, is inserted between two laminates composed of polyethylene terephthalate (PET) / aluminum / polypropylene, exposing the electrode leads to the outside. Polypropylene is then used as a lead film and inserted between the electrode leads and the housing. In this case, the width of the lead film is wider than the width of the sealing portion.
[0118] Consider the following scenario: A separation groove is formed by cutting a strip across the width of the electrode lead into an area that does not correspond to the sealing portion of the housing, nor to the lead film, and is not exposed to the outside of the housing. The electrode lead thickness is 0.4 mm, the separation groove depth is 0.3 mm, and the separation groove width is 0.5 mm. For example, this is a scenario where the separation groove is located in a third region, such as... Figure 2 As shown.
[0119] Example 2
[0120] Except for additionally forming a separation groove by further cutting one side of the electrode lead in a strip that spans the width of the electrode lead, exposing the exterior of the housing and not corresponding to either the lead film or the sealing portion of the housing, the same conditions as in Example 1 are set. For example, this is a scenario where the separation groove is located in the first and third regions, as... Figure 3 As shown.
[0121] Example 3
[0122] Except for forming a separation groove by cutting a strip across the width of the electrode lead on one side, exposing the exterior of the housing and not corresponding to either the sealing portion of the lead film or the housing, and forming a separation groove by cutting a strip across the width of the electrode lead on the other side, not corresponding to either the sealing portion of the lead film or the housing and not exposed to the exterior of the housing, the same conditions as in Example 1 are set. For example, this is a scenario where the separation groove is located in the first region and the third region but on opposite sides of each other, such as... Figure 4 As shown.
[0123] Example 4
[0124] Except that the polyethylene film is filled into the separation groove cut in Example 1, the same conditions as in Example 1 are set. For example, it is the same as... Figure 6 The implementation methods shown are the same.
[0125] Example 5
[0126] Except for covering the outer periphery of the separation groove cut in Example 1 with a polyethylene film, the same conditions as in Example 1 are set. For example, it is the same as... Figure 7 The implementation methods shown are the same.
[0127] Comparative Example 1
[0128] Except for forming the separation groove by cutting one side of the electrode lead in a strip that spans the width of the electrode lead, exposing it to the outside of the housing, and not corresponding to either the lead film or the sealing portion of the housing, the same conditions as in Example 1 are set. For example, this is a scenario where the separation groove is only located in the first region.
[0129] Comparative Example 2
[0130] Except that the separation groove is formed by cutting a strip across the width of the electrode lead on one side, exposing the outside of the housing, and corresponding to the lead film but not the sealing portion of the housing, the conditions are the same as in Example 1. For example, this is a scenario where the separation groove is located in the second region, outside the sealing portion, directly below the lead film located outside the housing.
[0131] Comparative Example 3
[0132] Except that the separation groove is formed by cutting a strip across the width of the electrode lead on one side of the sealed portion corresponding to the lead film and the housing, the same conditions as in Example 1 are set. For example, this is a scenario where the separation groove is located in the middle of the second region and is embedded in the lead film.
[0133] Comparative Example 4
[0134] Except that the separation groove is formed by cutting a strip across the width of the electrode lead inside the battery into a region corresponding to the lead film but not to the sealing portion of the housing and not exposed to the outside of the housing, the conditions are the same as in Example 1. For example, this is a scenario where the separation groove is located in the portion inside the sealing portion of the second region, directly below the lead film inside the housing.
[0135] Experimental Example: Measurement of Stress on Electrode Leads
[0136] Assuming a pressure of 0.1 MPa is applied to the interior of the casing of the secondary batteries according to Examples 1 to 5 and Comparative Examples 1 to 4, and when a temperature of 180°C is applied, the stresses applied to the electrode leads are measured by simulation experiments, such as... Figures 8 to 16 As shown. At this point, the lower end of the electrode housing is fixed. It is assumed that the electrode leads are made of aluminum, and plastic deformation stress-strain curve data are applied to the electrode leads and the bag. Plastic deformation occurs in the electrode leads when a stress above 87 MPa is applied. The lead film is made of polypropylene. Analysis boundary conditions are performed under the assumption that the electrode leads are welded to the busbar.
[0137] Figures 8 to 12 This is a graph showing the results of stress analysis when internal pressure is applied to the electrode lead portion of a secondary battery according to an example. Figures 13 to 16 This is a graph showing the stress analysis results when internal pressure is applied to the electrode lead portion of the secondary battery according to the comparative example. Figures 8 to 16 In the middle, the indices used to estimate stress are shown together on the lower right side, and as the indices move from bottom to top (from blue to red in the case of color plots) (for easy reference in the case of black and white plots), the larger the stress, the smaller the stress, the part with relatively small stress is denoted as ①, the part with relatively medium stress is denoted as ②, and the part with relatively large stress is denoted as ③.
[0138] Reference Figures 8 to 12 Based on the secondary batteries of Examples 1 to 5, the maximum stress in the separation tank section is the greatest, and the maximum stress acts uniformly throughout the entire separation tank. Therefore, in the case of the secondary batteries according to Examples 1 to 5, it can be inferred that the electrode leads can break rapidly when the internal pressure of the battery increases.
[0139] Specifically, it can be seen that according to Figure 10 Example 3 secondary battery and according to Figure 8 Example 1 Figure 9 Example 2 Figure 11 Example 4 and Figure 12 The secondary battery in Example 5 exhibits the highest maximum stress in the separation tank section compared to the secondary battery in Example 3. Therefore, in the case of the secondary battery according to Example 3, it can be deduced that the electrode leads can break most rapidly when the internal pressure of the battery increases.
[0140] Specifically, the maximum stress in Example 1 is 93.31267 MPa, while the maximum stress in Example 2 is 96.33443 MPa. In the case of Example 2, the maximum stress distribution can be said to be more suitable for high-voltage short circuits in both parts of the separation tank. Furthermore, since the separation tank does not overlap with the lead film or the sealing section, Examples 1 and 2 have the advantage of being prone to electrode lead breakage.
[0141] In Example 2, the separation groove formed in the third region has a greater maximum stress than the separation groove formed in the first region. In the separation groove formed in the third region, there is an additional region below the cut portion (see...). Figure 2 The S1 region in the third region is very narrow, while in the separation groove formed in the first region, the electrode lead region is wide on both sides of the upper and lower regions. Therefore, the separation groove formed in the third region has a larger maximum stress than the separation groove formed in the first region, and a high stress range is clearly shown around the separation groove.
[0142] The maximum stress in Example 3 is 96.55101 MPa, which is slightly higher than the maximum stress in Example 2. This is because when two separation grooves are formed on different sides of the electrode lead, the lead-side supports are misaligned, and therefore the stress is difficult to rise along the length of the electrode lead, thus increasing the stress.
[0143] The maximum stress in Example 4 was simulated as 96.55061 MPa, while the maximum stress in Example 5 was simulated as 96.34644 MPa. When the separation tank is covered with an insulating film as in Example 5, the maximum stress is slightly lower than in Example 3. However, it is higher than the maximum stress in Example 2. Furthermore, when the separation tank is filled with an insulating film as in Example 4, the maximum stress is shown as a value between Example 5 and Example 3. In this way, the location and number of separation tanks, as well as whether to add an insulating film, can be determined so that the desired maximum stress is appropriately generated as in Examples 1 to 5.
[0144] Next, refer to Figures 13 to 16 The maximum stresses of the secondary batteries according to Comparative Examples 1 to 4 were 93.13268 MPa, 96.01526 MPa, 94.54169 MPa, and 95.85877 MPa, respectively, and it was confirmed that all of them could cause plastic deformation of the electrode leads. However, when observing the stress distribution in the separation tank, it can be seen that, unlike the secondary batteries according to Examples 1 to 5, the maximum stress was not uniformly applied to the entire separation tank. Therefore, in the case of the secondary batteries according to Comparative Examples 1 to 4, it can be inferred that the electrode leads are slightly less likely to break quickly when the internal pressure of the battery increases.
[0145] While this disclosure has been described above with reference to a limited number of embodiments and accompanying drawings, it is not limited thereto, and it will be apparent to those skilled in the art that various modifications and variations can be made thereto within the technical aspects of this disclosure and within the equivalent scope of the appended claims.
[0146] [Figure Labels]
[0147] 10: Secondary batteries
[0148] 11: Electrode leads
[0149] 12: Electrode assembly
[0150] 13: Battery casing
[0151] 13a: Retaining part
[0152] 13b: Sealing part
[0153] 14: Lead wire film
[0154] 15: Separation tank
[0155] 16: Insulating film
[0156] 100: First Zone
[0157] 200: Second Zone
[0158] 300: Third Zone
Claims
1. A secondary battery, the secondary battery comprising: Electrode assembly, with electrode leads attached to the electrode assembly; A housing that houses the electrode assembly, such that a portion of the electrode leads is exposed to the outside, the housing including a sealing portion formed in the housing to seal the electrode assembly; as well as A lead film, which covers a portion of the outer surface of the electrode lead and is inserted between the electrode lead and the sealing portion. The electrode lead includes a first region that does not correspond to the lead film and is exposed to the outside of the housing, a second region that corresponds to the lead film, and a third region that does not correspond to the lead film and is not exposed to the outside of the housing. The separation tank is located in the third region. The separation tank is additionally located in the first region.
2. The secondary battery according to claim 1, in, The separation groove located in the third region and the separation groove located in the first region are respectively located on opposite sides of the electrode leads.
3. The secondary battery according to claim 1, in, The separation groove located in the third region and the separation groove located in the first region are respectively located on the same side of the electrode lead.
4. The secondary battery according to claim 1, in, The separation groove is formed as a strip that spans the width of the electrode lead.
5. The secondary battery according to claim 1, in, The separation groove has a dashed line shape.
6. The secondary battery according to claim 5, in, The width of the dashed line is 5% to 50% of the width of the electrode lead.
7. The secondary battery according to claim 5, in, The length between the dots of the dashed line is 5% to 50% of the width of the electrode lead.
8. The secondary battery according to claim 5, in, The ratio of the width of the dashed line to the length between the points of the dashed line is 5:1 to 1:
5.
9. The secondary battery according to claim 1, in, The cross-section of the separation groove has any one of the following shapes: wedge-shaped, circular, and square.
10. The secondary battery according to claim 1, in, The separation tank is filled with an insulating film.
11. The secondary battery according to claim 1, in, The separation tank is covered with an insulating film.
12. The secondary battery according to claim 11, in, There is an empty space inside the separation tank.
13. The secondary battery according to claim 10 or 11, in, The insulating film includes polypropylene, polyethylene, polyimide, or two or more of the above.
14. The secondary battery according to claim 1, wherein, The separation groove is formed to have a depth of more than 30% compared to the thickness of the electrode lead.
15. The secondary battery according to claim 1, in, The lead film comprises polyethylene.
16. The secondary battery according to claim 1, The secondary battery is a pouch-type secondary battery.
17. The secondary battery according to claim 1, in, The third region does not correspond to the sealing portion, and the width of the lead film is wider than the width of the sealing portion.
18. The secondary battery according to claim 1, in, The separation groove is formed to connect one end of the electrode lead to the other end of the electrode lead in a direction orthogonal to the extension direction of the electrode lead.
19. The secondary battery according to claim 1, in, The separation groove is a region in which the thickness of the electrode lead decreases along the width direction of the electrode lead.
20. The secondary battery according to claim 1, in, The separation groove is a groove of predetermined depth recessed in the thickness direction from the surface of the electrode lead.
21. The secondary battery according to claim 1, in, The separation groove is not formed to connect one end of the electrode lead to the other end, but is divided into multiple parts, and there is no continuity between the separation grooves.
Citation Information
Patent Citations
Electronic appliance
KR1020210135349A
Pouch-type secondary battery including electrode lead having electrical current limiting function
CN107534098A
Battery cell
US20170117515A1