fuel cell stack
By setting a sacrificial electrolytic corrosion zone in the coolant manifold area of the fuel cell stack, using stainless steel baffles designed with flat and uneven contacts, the problem of coolant manifold electrolytic corrosion was solved, extending the life of the fuel cell stack and reducing costs.
Patent Information
- Application Number
- CN202310319424.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2022-05-16
- Filing Date
- 2023-03-29
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2043-03-29
AI Technical Summary
Electrolytic corrosion in the coolant manifold of existing fuel cell stacks leads to shortened lifespan, and the use of highly corrosion-resistant materials or the addition of sacrificial components increases costs.
Sacrificial electrolytic corrosion zones are set up in the coolant manifold area of the fuel cell stack. Stainless steel baffles are used, and the coolant inlet or outlet areas are designed to be flat and in contact with the insulating sheet, while other areas are uneven to promote electrolytic corrosion reaction and extend life.
By using inexpensive stainless steel materials and design, the lifespan of fuel cell stacks has been extended while costs have been reduced.
Smart Images

Figure CN117080477B_ABST
Abstract
Description
Technical Field
[0001] This disclosure relates to fuel cell stacks. Background Technology
[0002] Various studies have been conducted on fuel cells.
[0003] For example, Japanese Patent No. 4901169 discloses the following technology: a sacrificial member is separately provided to treat electrolytic corrosion generated in the coolant manifold by the sacrificial member.
[0004] For example, Japanese Unexamined Patent Application Publication No. 2016-096033 (JP 2016-096033 A) discloses a fuel cell stack capable of suppressing the corrosion of the separator.
[0005] For example, Japanese Unexamined Patent Application Publication No. 2008-016216 (JP 2008-016216 A) discloses a fuel cell system that effectively suppresses corrosion, especially on the separator and the like, on the high-potential side.
[0006] For example, Japanese Unexamined Patent Application Publication No. 2010-113864 (JP 2010-113864 A) discloses a fuel cell having a mechanism for suppressing corrosion of the separator plate caused by coolant recovering heat from the fuel cell.
[0007] For example, Japanese Unexamined Patent Application Publication No. 2010-113863 (JP 2010-113863 A) discloses a fuel cell having a mechanism for suppressing corrosion of fuel cell stack components (such as conductive separators) caused by coolant recovering heat from the fuel cell. Summary of the Invention
[0008] In the coolant inlet or outlet area of the coolant manifold of the fuel cell stack, especially on its outlet side, high-temperature coolant flows out, which increases the ionic conductivity of the coolant, decreases the ionic resistance of the coolant, and concentrates electrolytic corrosion, thus shortening the life of the fuel cell stack.
[0009] A separate sacrificial component is used to treat the electrolytic corrosion that occurs in the coolant manifold, and this increases the number of components that make up the fuel cell stack, thereby increasing the cost of the fuel cell stack.
[0010] Furthermore, to address the electrolytic corrosion that occurs in the coolant manifold, changing the battery separator substrate where electrolytic corrosion occurs from inexpensive stainless steel materials (such as SUS (steel-use-stainless)) to highly corrosion-resistant materials such as titanium increases the cost of fuel cell stacks.
[0011] This disclosure provides a fuel cell stack that can have a long lifespan through an inexpensive construction.
[0012] One aspect of this disclosure provides a fuel cell stack. The fuel cell stack has a battery stack comprising multiple cell units stacked together, each cell unit including a separator made of stainless steel.
[0013] The cell unit includes a cathode separator, an anode separator, and an insulating sheet disposed between the cathode separator and the anode separator.
[0014] In at least one of the cell units, in a region adjacent to the coolant manifold of the cell unit along the planar direction, at least one of the cathode separator and the anode separator includes a sacrificial electrolytic corrosion region and a sealing region, wherein the sacrificial electrolytic corrosion region is not bonded to the insulating sheet in the lamination direction, and the sealing region is adjacent to the sacrificial electrolytic corrosion region and bonded to the insulating sheet in the planar direction.
[0015] The sacrificial electrolytic corrosion region includes a coolant inlet or outlet region and a region outside the coolant inlet or outlet region. The baffle in the coolant inlet or outlet region is flat and contacts the insulating sheet, and the baffle in the region outside the coolant inlet or outlet region is convex and concave, at least partially not in contact with the insulating sheet.
[0016] In the fuel cell stack according to the above scheme, when the width of the sacrificial electrolytic corrosion region in the planar direction, starting from the end of the coolant manifold on the coolant inlet or outlet side, is defined as the sacrificial electrolytic corrosion distance W, the sacrificial electrolytic corrosion surface area W×D, which is the product of the sacrificial electrolytic corrosion distance W and the thickness D of the separator, can be 0.25 mm. 2 above.
[0017] In a fuel cell stack according to the above scheme, at least one type of separator may include a sacrificial electrolytic corrosion region protrusion that protrudes further toward a portion of the coolant manifold in the planar direction than the insulating sheet adjacent to the separator. The type of separator is selected from the group consisting of: a cathode separator of the highest potential cell that contributes to power generation and has the highest potential in the cell, a cathode separator of an end cell that is adjacent to the highest potential cell and does not contribute to power generation, and an anode separator of the end cell.
[0018] In the fuel cell stack according to the above scheme, the cathode separator of the highest potential cell may include the sacrificial electrolytic corrosion region protrusion.
[0019] In the fuel cell stack according to the above scheme, the sacrificial electrolytic corrosion distance W can be from 2.1 mm to 13 mm, and the thickness D of the separator can be from 0.08 mm to 0.12 mm.
[0020] The fuel cell stack disclosed herein can have a long lifespan through an inexpensive construction. Attached Figure Description
[0021] The features, advantages, and technical and industrial significance of exemplary embodiments of the invention will be described below with reference to the accompanying drawings, wherein like reference numerals denote like elements, and wherein:
[0022] Figure 1 A schematic cross-sectional view illustrating an example near the coolant discharge manifold of a fuel cell stack according to a first embodiment of the present disclosure;
[0023] Figure 2 A schematic cross-sectional view illustrating an example of the sacrificial electrolytic corrosion distance W and the separator thickness D of a fuel cell stack according to a second embodiment of the present disclosure near the coolant discharge manifold;
[0024] Figure 3 A graph illustrating an example of the relationship between the sacrificial electrolytic corrosion distance W of separators with different ionic conductivity in a fuel cell stack according to a second embodiment of the present disclosure and the lifespan of the fuel cell stack; and
[0025] Figure 4 A schematic cross-sectional view is provided to illustrate an example of a fuel cell stack near a coolant discharge manifold according to a third embodiment of the present disclosure. Detailed Implementation
[0026] Embodiments according to this disclosure will be described below. Note that matters other than those specifically described in this specification but necessary for implementing this disclosure (e.g., the common construction and manufacturing process of fuel cell stacks, which are not features of this disclosure) should be understood as matters designed by those skilled in the art based on prior art. This disclosure can be implemented based on the disclosures in this specification and common technical knowledge in the art.
[0027] Furthermore, the dimensional relationships (length, width, thickness, etc.) in the attached drawings do not affect the actual dimensional relationships.
[0028] In this specification, the term "to" used to indicate a range of values is used in the sense of including the values described before and after it as lower and upper limits.
[0029] It can use any combination of the upper and lower limits of the numerical range.
[0030] This disclosure provides a fuel cell stack having a battery stack in which multiple cell units, each having a separator made of stainless steel, are stacked together.
[0031] Each cell includes a cathode separator, an anode separator, and an insulating sheet arranged between the cathode separator and the anode separator.
[0032] In at least one of a plurality of cell units, at least one of the cathode separator and the anode separator includes a sacrificial electrolytic corrosion region and a sealing region in the region adjacent to the coolant manifold of the cell unit in the planar direction, the sacrificial electrolytic corrosion region not bonded to the insulating sheet adjacent in the lamination direction, and the sealing region adjacent to the sacrificial electrolytic corrosion region in the planar direction and bonded to the insulating sheet.
[0033] In the sacrificial electrolytic corrosion region, the coolant inlet or outlet area of the partition is flat and in contact with the insulating sheet, and the area outside the coolant inlet or outlet area in the sacrificial electrolytic corrosion region of the partition can be convex and concave, at least partially not in contact with the insulating sheet.
[0034] In this disclosure, in a battery where electrolytic corrosion occurs, a predetermined area starting from the end of the coolant manifold is defined as a sacrificial electrolytic corrosion area using inexpensive stainless steel material, and a sealing area is set outside this area.
[0035] In this disclosure, the coolant manifold of a fuel cell using stainless steel separators has a sacrificial electrolytic corrosion region. Within the coolant inlet or outlet region of this sacrificial electrolytic corrosion region, the separator is flat, with only one side of the separator in contact with the coolant. Simultaneously, the separator outside the coolant inlet or outlet region of the sacrificial electrolytic corrosion region has an uneven surface, with areas not in contact with the insulating sheet, and a structure where both sides of the separator are in contact with the coolant during electrolytic corrosion. The electrolytic corrosion reaction in the sacrificial electrolytic corrosion region is further promoted by increasing the surface area and by providing an uneven surface.
[0036] According to this disclosure, in the area of the sacrificial electrolytic corrosion region that is not in contact with the insulating sheet, electrolytic corrosion occurs on both sides of the separator, thus promoting the electrolytic corrosion reaction. Therefore, the effect of sacrificial electrolytic corrosion in this area is increased, and the concentration of electrolytic corrosion in the coolant inlet or outlet areas is reduced, thereby extending the lifespan of the fuel cell stack. Furthermore, stainless steel separators can be used to achieve an inexpensive construction.
[0037] The fuel cell stack according to this disclosure has a battery stack in which multiple cell units, each having a separator made of stainless steel, are stacked together.
[0038] In this disclosure, both a single cell and a fuel cell stack consisting of multiple single cells may be referred to as a fuel cell.
[0039] In this disclosure, a unit cell may be referred to as a battery.
[0040] A battery stack is a stack obtained by stacking multiple cell units together.
[0041] The number of cells stacked in a battery stack is not particularly limited and can range from two to several hundred.
[0042] A fastening load can be applied to the battery stack via fastening components.
[0043] Examples of fastening components include shaft components (such as bolts and nuts with threads at both ends), spring components, etc.
[0044] A fuel cell stack may have a pair of end plates at both ends in the stacking direction of the battery stack.
[0045] Examples of fastening battery stacks include methods of applying fastening load by threaded fastening using end plates arranged at both ends of the battery stack in the stacking direction, using shaft members (such as bolts and nuts with threads at both ends), and methods of applying fastening load by using spring members, etc.
[0046] A fuel cell unit includes a cathode separator, an anode separator, and an insulating sheet disposed between the cathode separator and the anode separator, and typically includes a membrane electrode gas diffusion layer assembly (MEGA).
[0047] The membrane electrode gas diffusion layer assembly comprises, in the following order, an anode-side gas diffusion layer, an anode catalyst layer, an electrolyte membrane, a cathode catalyst layer, and a cathode-side gas diffusion layer.
[0048] The cathode (oxidant electrode) includes a cathode catalyst layer and a cathode-side gas diffusion layer.
[0049] The anode (fuel electrode) includes an anode catalyst layer and an anode-side gas diffusion layer.
[0050] The cathode catalyst layer and the anode catalyst layer will be collectively referred to as the "catalyst layer".
[0051] For example, the catalyst layer may include a catalyst metal that promotes electrochemical reactions, an electrolyte with proton conductivity, a support with electronic conductivity, etc.
[0052] Examples of catalyst metals include platinum (Pt), alloys made of Pt and another metal (e.g., Pt alloys including cobalt, nickel, etc.).
[0053] The electrolyte can be a fluoropolymer, etc. Examples of solutions that can use fluoropolymers include Nafion solutions.
[0054] The catalyst metal is supported on a support, and in each catalyst layer, the support supporting the catalyst metal (catalyst support) can be mixed with the electrolyte.
[0055] Examples of supports for catalyst metals include carbon materials such as carbon, which are commercially available.
[0056] The cathode-side gas diffusion layer and the anode-side gas diffusion layer will be collectively referred to as the "gas diffusion layer".
[0057] The diffusion layer can be a breathable conductive component, etc.
[0058] Examples of conductive components include porous carbon materials such as carbon cloth and carbon paper, and porous metals such as metal mesh and foam metal.
[0059] The electrolyte membrane can be a solid polymer electrolyte membrane. Examples of solid polymer electrolyte membranes include fluorine-based electrolyte membranes such as water-containing perfluorosulfonic acid films, hydrocarbon-based electrolyte membranes, etc. Examples of electrolyte membranes can include Nafion membranes (manufactured by DuPont), etc.
[0060] An insulating sheet is positioned between the cathode separator and the anode separator. The insulating sheet can also be positioned on the outer periphery of the membrane electrode gas diffusion layer assembly.
[0061] Insulating sheets may have a frame portion, an opening portion, and holes.
[0062] The frame section is the main part that connects the insulating sheet to the membrane electrode gas diffusion layer assembly.
[0063] The opening is the holding area of the membrane electrode gas diffusion layer assembly, and is a region that extends through a portion of the frame portion to accommodate the membrane electrode gas diffusion layer assembly. It is sufficient for the opening to be positioned within the insulating sheet, around the frame portion (in the outer periphery of the membrane electrode gas diffusion layer assembly), and it can also be located in the middle of the insulating sheet.
[0064] The holes in the insulating sheet allow fluids such as reactive gases and coolants to flow along the stacking direction of the cell units. The holes in the insulating sheet can be arranged and positioned to communicate with holes in the separator.
[0065] The insulating sheet may include a frame-shaped core layer and two frame-shaped shell layers disposed on two sides of the core layer, namely, a first shell layer and a second shell layer.
[0066] The first and second shell layers can be arranged in a frame-like manner on both sides of the core layer, in the same way as the core layer.
[0067] The core layer only needs to be a structural component with airtightness and insulation, and it can be made of a material whose structure does not change under temperature conditions during hot pressing in the fuel cell manufacturing process. Specifically, materials used for the core layer include resins such as polyethylene, polypropylene, polycarbonate (PC), polyphenylene sulfide (PPS), polyethylene terephthalate (PET), polyethylene naphthalate (PEN), polyamide (PA), polyimide (PI), polystyrene (PS), polyphenylene ether (PPE), polyetheretherketone (PEEK), cycloalkenes, polyethersulfone (PES), polyphenylene sulfone (PPSU), liquid crystal polymer (LCP), and epoxy resin. The core layer material can also be a rubber material such as ethylene propylene diene monomer (EPDM), fluororubber, and silicone rubber.
[0068] From the perspective of ensuring insulation, the thickness of the core layer can be 5μm or more, or 20μm or more, while from the perspective of reducing the thickness of the battery, it can be less than 200μm, or less than 150μm.
[0069] The first and second shell layers can have high adhesion to other materials, soften under temperature conditions during hot pressing, and have lower viscosity and melting point than the core layer, in order to bond the core layer to the anode and cathode separators and ensure sealing performance. Specifically, the first and second shell layers can be thermoplastic resins such as polyester-based thermoplastic resins, modified olefin-based thermoplastic resins, or thermosetting resins as modified epoxy resins.
[0070] The resin constituting the first shell layer and the resin constituting the second shell layer can be the same type of resin, or they can be different types of resin. Having shell layers on both sides of the core layer facilitates bonding the insulating sheet and the two separators together via hot pressing.
[0071] The thickness of each of the first and second housing layers can be greater than 5 μm or greater than 30 μm from the viewpoint of ensuring adhesion, while it can be less than 100 μm or less than 40 μm from the viewpoint of reducing battery thickness.
[0072] In the insulating sheet, the first shell layer and the second shell layer can be disposed only on the portions (sealing areas of the separators) to which they will be bonded to the anode separator and the cathode separator, respectively. The first shell layer disposed on one side of the core layer can be bonded to the cathode separator. The second shell layer disposed on the other side of the core layer can be bonded to the anode separator. The insulating sheet can be held between a pair of separators.
[0073] The fuel cell stack may have a manifold communicating with each port, such as a supply manifold communicating with each supply port and an exhaust manifold communicating with each exhaust port.
[0074] Examples of supply manifolds include fuel gas supply manifolds, oxidizer gas supply manifolds, and coolant supply manifolds.
[0075] Examples of exhaust manifolds include fuel gas exhaust manifolds, oxidizer gas exhaust manifolds, and coolant exhaust manifolds.
[0076] In this disclosure, the coolant supply manifold and the coolant discharge manifold will be collectively referred to as the "coolant manifold".
[0077] Fuel cell stacks can have gaskets placed between adjacent cells. The gaskets serve as sealing components to prevent reactant gases from leaking from each reactant gas system.
[0078] Washers can be made of ethylene propylene diene monomer (EPDM) rubber, silicone rubber, thermoplastic elastomer resin, etc.
[0079] A single cell includes a pair of separators.
[0080] The separator holds the insulating sheet and typically also holds the membrane electrode gas diffusion layer assembly.
[0081] In the partition, one is an anode partition and the other is a cathode partition. In this disclosure, the anode partition and the cathode partition will be collectively referred to as "partition".
[0082] The separator may have orifices such as supply and discharge ports for fluids such as reactant gases and coolants flowing in the stacking direction of the cell units. Examples of coolants that can be used include a mixture of ethylene glycol and water to suppress freezing at low temperatures.
[0083] Examples of supply ports include fuel gas supply ports, oxidizer gas supply ports, coolant supply ports, etc.
[0084] Examples of discharge ports include fuel gas discharge ports, oxidizer gas discharge ports, coolant discharge ports, etc.
[0085] For convenience, these holes may be referred to as "manifolds" in this disclosure.
[0086] The separator may have reactant gas channels on the surface in contact with the gas diffusion layer. The separator may also have coolant channels on the surface opposite to the gas diffusion layer to maintain a constant temperature in the fuel cell.
[0087] The anode separator may have fuel gas channels on the surface that contacts the anode-side gas diffusion layer. Furthermore, the anode separator may have coolant channels on the surface opposite to the surface that contacts the anode-side gas diffusion layer to maintain a constant temperature in the fuel cell.
[0088] The cathode separator may have an oxidant gas channel on the surface in contact with the cathode-side gas diffusion layer. Furthermore, the cathode separator may have a coolant channel on the surface opposite to the surface in contact with the cathode-side gas diffusion layer to maintain a constant temperature in the fuel cell.
[0089] The partition can be a sheet made of stainless steel such as SUS.
[0090] The shape of the partition can be rectangular, horizontally elongated hexagon, horizontally elongated octagon, circular, elliptical, etc.
[0091] In this disclosure, fuel gas and oxidant gas will be collectively referred to as "reactant gas". The reactant gas supplied to the anode is fuel gas, while the reactant gas supplied to the cathode is oxidant gas. The fuel gas is a gas mainly containing hydrogen, and may be hydrogen gas. The oxidant gas is a gas containing oxygen, and may be oxygen, air, dry air, etc.
[0092] The baffle has a coolant inlet or outlet area between the coolant supply hole or coolant outlet hole that constitutes the coolant manifold and the coolant passage.
[0093] Specifically, the baffle has a coolant inlet area between the coolant supply hole and the coolant passage that constitute the coolant supply manifold, and a coolant outlet area between the coolant outlet hole and the coolant passage that constitute the coolant outlet manifold.
[0094] The term "coolant inlet or outlet area" means either the coolant inlet area or the coolant outlet area.
[0095] The area of the separator adjacent to the coolant manifold (coolant supply port or coolant discharge port constituting the coolant manifold) of the cell in the planar direction has a coolant inlet or outlet area, and an area outside the coolant inlet or outlet area.
[0096] Specifically, the area of the separator adjacent to the coolant supply manifold of the cell in the planar direction has a coolant inlet area and an area other than the coolant inlet area, while the area of the separator adjacent to the coolant outlet manifold of the cell in the planar direction has a coolant outlet area and an area other than the coolant outlet area.
[0097] The area outside the coolant inlet or outlet area can be the area of the separator adjacent to the coolant manifold of the cell in the planar direction, and can be the area not connected to the coolant channel.
[0098] (1) First embodiment
[0099] In at least one of the multiple cell units of a fuel cell stack according to a first embodiment of the present disclosure, at least one of the cathode separator and the anode separator has a sacrificial electrolytic corrosion region and a sealing region in a region adjacent to the coolant manifold of the cell unit in a planar direction, the sacrificial electrolytic corrosion region not bonded to an insulating sheet adjacent in a lamination direction, and the sealing region adjacent to the sacrificial electrolytic corrosion region in a planar direction and bonded to the insulating sheet.
[0100] In other words, the sacrificial electrolytic corrosion zone is the area of the partition that is adjacent to the coolant manifold in the planar direction and is not bonded to the insulating sheet.
[0101] Furthermore, the sealing area is the area of the partition that is adjacent to the sacrificial electrolytic corrosion area in the planar direction and is bonded to the insulating sheet.
[0102] It is sufficient to place the sacrificial electrolytic corrosion zone on at least one of the cathode and anode partitions, and the sacrificial electrolytic corrosion zone can be placed on two partitions.
[0103] It is sufficient to place the sacrificial electrolytic corrosion region in at least one of the multiple cell units, and the sacrificial electrolytic corrosion region can be placed in all cell units.
[0104] In the sacrificial electrolytic corrosion zone, the coolant inlet or outlet area of the baffle is shaped as a flat plate that contacts the insulating sheet.
[0105] In the sacrificial electrolytic corrosion zone, it is sufficient for the area outside the coolant inlet or outlet area of the partition to have an uneven shape that at least partially does not contact the insulating sheet, and if the shape is uneven, the area outside the coolant inlet or outlet area does not need to contact the insulating sheet at all.
[0106] In the sacrificial electrolytic corrosion region, the coolant inlet area of the partition is flat and in contact with the insulating sheet, while the area outside the coolant inlet area in the sacrificial electrolytic corrosion region can be irregularly shaped, at least partially not in contact with the insulating sheet.
[0107] In the sacrificial electrolytic corrosion region, the coolant outlet area of the partition is flat and in contact with the insulating sheet, while the area outside the coolant outlet area in the sacrificial electrolytic corrosion region can be convex and concave, at least partially not in contact with the insulating sheet.
[0108] Figure 1 This is a schematic cross-sectional view illustrating an example of a fuel cell stack near a coolant discharge manifold according to a first embodiment of the present disclosure.
[0109] like Figure 1 As shown, in each cell of a fuel cell stack according to a first embodiment of the present disclosure, the cathode separator and the anode separator have sacrificial electrolytic corrosion regions and sealing regions in the areas adjacent to the coolant discharge manifold of the cell in the planar direction, the sacrificial electrolytic corrosion regions not bonded to the insulating sheet adjacent in the stacking direction, and the sealing regions adjacent to the sacrificial electrolytic corrosion regions in the planar direction and bonded to the insulating sheet.
[0110] In the sacrificial electrolytic corrosion zone, the coolant outlet area of the partition is flat and in contact with the insulating sheet, while the area in the sacrificial electrolytic corrosion zone other than the coolant outlet area is uneven and partially not in contact with the insulating sheet.
[0111] exist Figure 1 It should be noted that the diagram shows an example of a coolant drain manifold, but the same construction can be used when the coolant manifold supplies coolant to the coolant manifold.
[0112] (2) Second embodiment
[0113] In the fuel cell stack according to the second embodiment of this disclosure, the width of the coolant manifold in the planar direction, starting from the end of the sacrificial electrolytic corrosion region at the coolant inlet or outlet side, is defined as the sacrificial electrolytic corrosion distance W (mm). The sacrificial electrolytic corrosion surface area W×D, which is the product of the sacrificial electrolytic corrosion distance W (mm) and the thickness D (mm) of the separator, can be 0.25 mm. 2 Furthermore, considering the balance between the size (energy density) of the fuel cell stack and its lifespan, the upper limit can be 1.00 mm. 2 the following.
[0114] The sacrificial electrolytic etching distance W (mm) can be from 2.1mm to 13mm, with a lower limit of 2.5mm or more, or 3mm or more, and an upper limit of 6mm or less, or 4mm or less.
[0115] The thickness D (mm) of the partition can be from 0.08mm to 0.12mm, and the lower limit can be above 0.1mm.
[0116] In particular, the ionic conductivity of the separator is not limited and can be 1 μS / cm. 2 Up to 8 μS / cm 2 And it can be 2μS / cm 2 Up to 6 μS / cm 2 .
[0117] The sacrificial electrolytic corrosion zone at the end of the coolant inlet or outlet side of the coolant manifold can be the coolant inlet or outlet zone of the baffle at the end of the coolant manifold side.
[0118] The sacrificial electrolytic corrosion zone at the end of the coolant inlet side of the coolant supply manifold can be the coolant inlet zone of the baffle at the end of the coolant supply manifold side.
[0119] The sacrificial electrolytic corrosion zone at the end of the coolant outlet side of the coolant discharge manifold can be the coolant outlet zone of the baffle at the end of the coolant discharge manifold side.
[0120] Figure 2 This is a schematic cross-sectional view illustrating an example of the sacrificial electrolytic corrosion distance W and the separator thickness D of a fuel cell stack according to a second embodiment of the present disclosure near the coolant discharge manifold.
[0121] exist Figure 2 It should be noted that the diagram shows an example of a coolant drain manifold, but the same construction can be used when the coolant manifold supplies coolant to the coolant manifold.
[0122] Figure 3 A graph illustrating an example of the relationship between the sacrificial electrolytic corrosion distance W of separators with different ionic conductivity in a fuel cell stack according to the second embodiment and the lifespan of the fuel cell stack.
[0123] For example, the sacrificial electrolytic corrosion volume V (mm) of the partition can be used as a basis. 3 The electrolytic corrosion rate S (mol / s) and ionic conductivity (μS / cm) of the separator are also considered. 2 The relationship between the two factors is considered, and rules of thumb are taken into account to estimate the lifespan of the fuel cell stack.
[0124] In this disclosure, the sacrificial electrolytic corrosion volume V (mm²) of the partition is... 3 The value is D×W×L, which is the product of the thickness D (mm) of the baffle, the sacrificial electrolytic corrosion distance W (mm) which is the width of the coolant manifold in the planar direction starting from the end of the coolant inlet or outlet, and the circumference L (mm) of the coolant manifold.
[0125] In this disclosure, the electrolytic corrosion rate S (mol / s) of the baffle is L×d×v, where L (mm) is the circumference of the coolant manifold, d (mm) is the length of the electrolytic corrosion reaction zone of the baffle, and v (mol / s·mm) is the reaction rate per unit surface area. 2 The product of ).
[0126] According to a second embodiment of this disclosure, the electrolytic corrosion of the separator in the coolant manifold is limited to a sacrificial electrolytic corrosion region. Therefore, even after the separator dissolves in the sacrificial electrolytic corrosion region, the sealing structure of the cell is not damaged, the sealing function of the cell is maintained, and the lifespan of the fuel cell stack is extended.
[0127] Moreover, setting the sacrificial electrolytic corrosion surface area below a predetermined value can improve the balance between fuel cell stack lifespan and energy density.
[0128] (3) Third embodiment
[0129] In a fuel cell stack according to a third embodiment of the present disclosure, at least one type of separator may have a sacrificial electrolytic corrosion region protrusion that protrudes in the planar direction toward a portion of the coolant manifold more than the insulating sheet adjacent to the separator. The at least one type of separator is selected from the group consisting of: a cathode separator of the highest potential cell that contributes to power generation among a plurality of cell units and has the highest potential, a cathode separator of an end cell that is adjacent to the highest potential cell unit and does not contribute to power generation, and an anode separator of the end cell unit unit.
[0130] In the fuel cell stack according to the third embodiment, at least the cathode separator of the highest potential cell may have a sacrificial electrolytic corrosion region protrusion, and further, the cathode separator of the end cell adjacent to the highest potential cell and not contributing to power generation, and the anode separator of the end cell may have a sacrificial electrolytic corrosion region protrusion.
[0131] The sacrificial electrolytic corrosion region protrusion can protrude further toward the coolant supply manifold in the planar direction than the insulating sheet, can protrude toward the coolant discharge manifold in the planar direction, and can protrude toward both the coolant supply manifold and the coolant discharge manifold in the planar direction.
[0132] It is sufficient for the protruding portion of the sacrificial electrolytic corrosion zone to protrude further toward the coolant manifold in the planar direction than the insulating sheet, and it can protrude so as not to block the coolant manifold.
[0133] Figure 4 A schematic cross-sectional view is provided to illustrate an example of a fuel cell stack near a coolant discharge manifold according to a third embodiment of the present disclosure.
[0134] like Figure 4 As shown, in the fuel cell stack of the third embodiment of this disclosure, the cathode separator of the highest potential cell, which contributes to power generation among multiple cell units and has the highest potential, has a sacrificial electrolytic corrosion region protrusion that protrudes in the planar direction toward a portion of the coolant discharge manifold more than the insulating sheet adjacent to the cathode separator.
[0135] exist Figure 4 It should be noted that the diagram shows an example of a coolant drain manifold, but the same construction can be used when the coolant manifold supplies coolant to the coolant manifold.
[0136] In a third embodiment of this disclosure, in the separators of the stacked power generation cells, only at the cathode separator having the highest potential and closest to the negative electrode side, or at the separator of the adjacent end cell, the separator protrudes further toward the coolant manifold side than the adjacent insulating sheet.
[0137] Therefore, the partition is subjected to electrolytic corrosion from the protruding edge of the partition, thereby protecting other components.
[0138] In addition, one to three partitions protrude further from the insulating sheet, thus eliminating concerns about dielectric breakdown due to contact with other partitions of different potentials.
Claims
1. A fuel cell stack, characterized in that... A battery stack comprising multiple cell units stacked together, each cell unit including a separator made of stainless steel, wherein: The cell unit includes a cathode separator, an anode separator, and an insulating sheet disposed between the cathode separator and the anode separator; In at least one of the cell units, in a region adjacent to the coolant manifold of the cell unit along the planar direction, at least one of the cathode separator and the anode separator includes a sacrificial electrolytic corrosion region and a sealing region. The sacrificial electrolytic corrosion region is the region of the separator that is adjacent to the coolant manifold in the planar direction and is not bonded to the insulating sheet in the lamination direction. The sealing region is adjacent to the sacrificial electrolytic corrosion region in the planar direction and is bonded to the insulating sheet. The sacrificial electrolytic corrosion zone includes the coolant inlet or outlet area and the area outside the coolant inlet or outlet area; The baffle in the coolant inlet or outlet area is a flat plate that contacts the insulating sheet; The baffle plate in the region outside the coolant inlet or outlet area has an uneven shape that at least partially does not contact the insulating sheet; and At least one type of separator includes a sacrificial electrolytic corrosion region protrusion that protrudes further toward a portion of the coolant manifold in the planar direction than the insulating sheet adjacent to the separator. The at least one type of separator is selected from the group consisting of: a cathode separator of the highest potential cell that contributes to power generation and has the highest potential in the cell, a cathode separator of an end cell that is adjacent to the highest potential cell and does not contribute to power generation, and an anode separator of the end cell.
2. The fuel cell stack according to claim 1, characterized in that, When the width of the sacrificial electrolytic corrosion region in the planar direction, starting from the end of the coolant manifold on the coolant inlet or outlet side, is defined as the sacrificial electrolytic corrosion distance W, the sacrificial electrolytic corrosion surface area W×D, which is the product of the sacrificial electrolytic corrosion distance W and the thickness D of the baffle, is 0.25 mm. 2 above.
3. The fuel cell stack according to claim 1, characterized in that, The cathode separator of the highest potential cell includes the protrusion of the sacrificial electrolytic corrosion region.
4. The fuel cell stack according to claim 2, characterized in that: The sacrificial electrolytic corrosion distance W is 2.1 mm to 13 mm; and The thickness D of the partition is from 0.08 mm to 0.12 mm.
Citation Information
Patent Citations
JP1974001169A
Fuel cell system
JP2008016216A
Fuel cell
JP2010113863A
Fuel cell
JP2010113864A
Fuel cell stack
JP2016096033A