A packaging method for micro-led chip

Through charged treatment and electrostatic adsorption technology, micro-led chips are adsorbed under an inert gas atmosphere, combining vibration and leveling processes, the problems of high cost and high difficulty in the existing technology are solved, and low-cost and efficient micro-light emitting diode chip packaging is achieved. , expanding its application scope.

CN117153959BActive Publication Date: 2024-11-01SUNSHINE GLOBAL CIRCUITS CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202311323923.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-10-13
Publication Date
2024-11-01
Estimated Expiration
2043-10-13

AI Technical Summary

Technical Problem

The existing micro-led chip packaging technology requires high-precision equipment, which is costly and difficult to operate, limiting the widespread application of micro-light emitting diode display technology.

Method used

Using the principles of live treatment and electrostatic adsorption, the micro-led chip is adsorbed to the packaging area of ​​the carrier plate under an inert gas atmosphere. Through vibration and leveling processes, the chip and the packaging area are installed one by one, reducing the packaging cost.

Benefits of technology

The packaging process of micro-light emitting diode chips is simplified, the equipment cost and operation difficulty is reduced, and the application range is expanded.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117153959B_ABST
    Figure CN117153959B_ABST
Patent Text Reader

Abstract

The present invention discloses a packaging method for a micro-led chip, comprising: subjecting a packaging area in a carrier board to a charged state; placing the carrier board in a mounting chamber, and in an inert gas atmosphere, inputting the micro-led chip into the mounting chamber so that the micro-led chip is adsorbed in the packaging area. The packaging method for a micro-led chip provided by the present application is simple to operate, has low equipment cost, can effectively reduce the packaging cost of the micro-led chip, and expand the application scope of the micro-led display technology.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of micro-led chip packaging, and in particular to a packaging method for a micro-led chip. Background Art

[0002] With the advancement of LCD screen backlight technology, the display effect brought by traditional LED backlight can no longer meet consumers' demand for higher display effects. For this reason, micro-led (micro-light emitting diode) technology came into being.

[0003] Micro-LED display technology refers to a display technology that uses self-luminous micron-sized LEDs as light-emitting pixel units and assembles them on a drive panel to form a high-density LED array. Due to the small size, high integration and self-luminescence of micro-LED chips, it has greater advantages in brightness, resolution, contrast, energy consumption, service life, response speed and thermal stability compared to LCD and OLED in terms of display.

[0004] In order to improve the production efficiency and product yield of micro-led, the existing technology uses a mass transfer method to transfer the device chip to the carrier. Mass transfer refers to the transfer of a large number of micro-led grains, chips or devices to the target carrier or circuit through specific high-precision equipment. Mass transfer mainly includes physical transfer, chemical transfer and laser transfer technology. Among them, the physical transfer method is mainly electrostatic adsorption transfer technology; the chemical transfer method is mainly micro transfer printing technology (μTP technology); the laser transfer method uses laser lift-off technology (LLO) to separate the finished μLED from the sapphire growth wafer; and then the μLED is moved from the donor to the substrate through mass transfer (LIFT).

[0005] The mass transfer in the existing technology requires specific high-precision equipment, which is expensive and difficult to operate, resulting in high packaging costs. In order to promote the widespread use of micro-led display technology, it is necessary to find a packaging method that can replace mass transfer. Summary of the invention

[0006] The present invention aims to solve at least one of the problems in the related art to a certain extent. To this end, the purpose of the present invention is to provide a packaging method for a micro-led chip, which is simple to operate and has low equipment cost, can effectively reduce the packaging cost of the micro-led chip, and expand the application scope of the micro-led display technology.

[0007] In order to achieve the above-mentioned purpose, the present application adopts the following technical solution: a packaging method of a micro-led chip, comprising:

[0008] Conducting electrification on the packaging area of ​​the carrier board;

[0009] Place the carrier board inside the mounting chamber, and in an inert gas atmosphere, input the micro-led chip into the mounting chamber so that the micro-led chip is adsorbed on the packaging area.

[0010] Furthermore, the installation chamber includes an air inlet, and the micro-led chip is wrapped in nitrogen to form a suspension of the micro-led chip; the suspension of the micro-led chip enters the installation chamber from the air inlet.

[0011] Furthermore, the micro-led chip and / or carrier board inside the installation chamber is in a vibrating state.

[0012] Furthermore, the charged treatment includes: subjecting the carrier to a treatment by electrifying the carrier, or subjecting the carrier to a treatment by using charged plasma.

[0013] Furthermore, it also includes: leveling the micro-led chip adsorbed on the packaging area so that the micro-led chip corresponds to the packaging area one by one.

[0014] Furthermore, the micro-led chip adsorbed on the packaging area is leveled, including: using a soft board to scrape the adsorbed micro-led chip so that the micro-led chip corresponds to the packaging area one by one.

[0015] Furthermore, the micro-led chip includes a first chip, a second chip and a third chip, and the packaging area in the carrier includes a first packaging area, a second packaging area and a third packaging area; the first chip, the second chip and the third chip are sequentially adsorbed on the first packaging area, the second packaging area and the third packaging area.

[0016] Further, including:

[0017] S1: Covering the carrier with a dry film, exposing and developing it, so that the first packaging area is exposed;

[0018] S2: performing a charging process on the first packaging area in the carrier so that the first packaging area is charged and other areas are not charged;

[0019] S3: placing the carrier board inside the mounting chamber, and in an inert gas atmosphere, inputting the first chip into the mounting chamber so that the first chip is adsorbed on the first packaging area;

[0020] S4: etching away the dry film in the second packaging area, and repeating steps S2-S3 so that the second chip is adsorbed in the second packaging area;

[0021] S5: Etching away the dry film in the third packaging area, and repeating steps S2-S3, so that the third chip is adsorbed in the third packaging area.

[0022] Furthermore, step S3 also includes welding the first chip and the first packaging area;

[0023] Step S4 also includes welding the second chip and the second packaging area;

[0024] Step S5 also includes welding the third chip and the third packaging area.

[0025] Furthermore, the first chip, the second chip and the third chip are an R chip, a G chip and a B chip respectively.

[0026] The above technical solution provided by the embodiment of the present application has the following advantages compared with the prior art: the present application performs a charging treatment on the packaging area in the carrier; then the carrier is placed inside the installation chamber, and under an inert gas atmosphere, the micro-led chip is input into the installation chamber so that the micro-led chip is adsorbed in the packaging area. In the present application, the position of the packaging area in the carrier is first defined. After the charging treatment, the packaging area is charged, and other areas are not charged; when the carrier is placed inside the installation chamber, the micro-led chip can be adsorbed in the charged area. The present application utilizes the principle of electrostatic adsorption to adsorb and install the micro-led chip in the packaging area. Compared with the mass transfer solution in the prior art, the method of the present application is simpler, less difficult to operate, and less costly, which effectively reduces the packaging cost of micro-led chips and expands the application scope of micro-led display technology. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] The accompanying drawings, which are incorporated in and constitute a part of this specification, illustrate embodiments consistent with the invention and, together with the description, serve to explain the principles of the invention.

[0028] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, for ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative labor.

[0029] In the attached figure:

[0030] Figure 1 Flow chart of the preparation method in Example 3. DETAILED DESCRIPTION

[0031] In order to have a clearer understanding of the technical features, purposes and effects of the present invention, the specific embodiments of the present invention are now described in detail with reference to the accompanying drawings. In the following description, it should be understood that the directions or positional relationships indicated by "front", "back", "up", "down", "left", "right", "longitudinal", "horizontal", "vertical", "horizontal", "top", "bottom", "inside", "outside", "head", "tail", etc. are based on the directions or positional relationships shown in the accompanying drawings, are constructed and operated in a specific direction, and are only for the convenience of describing the present technical solution, rather than indicating that the mechanism or element referred to must have a specific direction, and therefore cannot be understood as a limitation to the present invention.

[0032] It should also be noted that, unless otherwise clearly specified and limited, the terms such as "installed", "connected", "connected", "fixed", "set" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral one; it can be a mechanical connection or an electrical connection; it can be directly connected or indirectly connected through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. When an element is referred to as being "on" or "under" another element, the element can be "directly" or "indirectly" located on the other element, or there may be one or more intermediate elements. The terms "first", "second", "third", etc. are only for the convenience of describing the present technical solution, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first", "second", "third", etc. can explicitly or implicitly include one or more of the features. For those of ordinary skill in the art, the specific meanings of the above terms in the present invention can be understood according to the specific circumstances.

[0033] In the following description, specific details such as specific system structures, technologies, etc. are provided for the purpose of illustration rather than limitation, so as to provide a thorough understanding of the embodiments of the present invention. However, it should be clear to those skilled in the art that the present invention may be implemented in other embodiments without these specific details. In other cases, detailed descriptions of well-known systems, mechanisms, circuits, and methods are omitted to prevent unnecessary details from obstructing the description of the present invention.

[0034] Example 1

[0035] The present application provides a method for packaging a micro-led chip, comprising: subjecting a packaging area in a carrier to a charging treatment; placing the carrier inside an installation chamber, and in an inert gas atmosphere, inputting the micro-led chip into the installation chamber so that the micro-led chip is adsorbed on the packaging area.

[0036] In the present application, before performing electrification treatment on the packaging area in the carrier board, the packaging area needs to be defined first. A protective film can be used to cover other areas outside the packaging area, exposing only the packaging area, which makes it easier to perform electrification treatment on the packaging area.

[0037] In the present application, the size of the micro-led chip is relatively small, and it may be uncharged or carry a charge opposite to that of the packaging area, so that the micro-led chip can be adsorbed within the packaging area in the installation chamber.

[0038] In this application, the position of the packaging area in the carrier is first defined. After the charging treatment, the packaging area is charged and other areas are not charged. When the carrier is placed inside the installation chamber, the micro-led chip can be adsorbed in the charged area. This application uses the principle of electrostatic adsorption to adsorb and install the micro-led chip in the packaging area. Compared with the mass transfer solution in the prior art, the method of this application is simpler, less difficult to operate, and requires lower costs, which effectively reduces the packaging cost of the micro-led chip and expands the application scope of the micro-led display technology.

[0039] Example 2

[0040] The present application provides a method for packaging a micro-led chip, comprising:

[0041] S1: Perform electrification on the package area in the carrier; the specific operations include but are not limited to the following three:

[0042] The first method is to energize the carrier. The carrier is a silicon wafer containing potassium impurities and is a semiconductor material. After the carrier is energized, only the packaging area is exposed because other areas are covered by a protective film, so that the surface of the packaging area can be charged, while other areas will not be charged because of the insulating protective film on the surface.

[0043] The second method is to use charged plasma to etch the carrier, and the plasma carries both positive and negative charges. When the plasma used in the present application treats the surface of the carrier, the charged plasma remains in the packaging area, making the packaging area charged, while other areas will not be charged due to the insulating protective film on the surface.

[0044] The third method is to place the carrier in air containing charged particles. Since the air contains charged particles, and the charges carried by the charged particles in the air are all positive or all negative, only the package area of ​​the carrier is exposed, and the other areas are covered by a protective film. The charged particles in the air are adsorbed on the package area, making the package area charged, while the other areas will not be charged due to the insulating protective film on the surface.

[0045] S2: Place the carrier board inside the mounting chamber, and in an inert gas atmosphere, input the micro-led chip into the mounting chamber so that the micro-led chip is adsorbed on the packaging area.

[0046] The installation chamber includes an air inlet, and the micro-led chip is wrapped in nitrogen to form a suspension of the micro-led chip; the suspension of the micro-led chip enters the installation chamber from the air inlet. The size of the micro-led chip in this application is relatively small, and the micro-led chip can be suspended in the nitrogen to form a suspension of the micro-led chip by controlling the output pressure of the nitrogen. In this way, the suspension of the micro-led chip can be input into the installation chamber by inputting a nitrogen flow through the input port of the installation chamber.

[0047] The installation chamber also includes an air outlet. By controlling the air intake and air outlet of the air inlet and the air outlet, it is ensured that the internal pressure of the installation chamber remains constant.

[0048] In order to prevent the micro-led chips from stacking in the packaging area, the present application can make the micro-led chips and / or the carrier board inside the installation chamber in a vibrating state. In the vibrating state, the micro-led chips and the charged packaging area can be assembled one by one. The vibration is equivalent to the external force. If multiple micro-led chips are adsorbed in the same packaging area, then under the action of vibration, multiple micro-led chips will fall and be adsorbed in the exposed packaging area.

[0049] In the present application, there are multiple packaging areas, each packaging area needs to adsorb a micro-led chip, the charge carried by the packaging area is uniform, the micro-led chip can be free of static electricity or carry a charge opposite to that of the packaging area. In the present application, the vibration can be directed to the micro-led chip, the carrier board, or both the micro-led chip and the carrier board. At the same time, the intensity of the vibration needs to be controlled to ensure that the intensity of the vibration is less than the adsorption force of the micro-led chip and the packaging area, and greater than the adsorption force of other chips and the packaging area except the corresponding micro-led chip. The corresponding micro-led chip refers to a micro-led chip that is completely fitted and adsorbed in the packaging area.

[0050] For example: each packaging area only needs to absorb one micro-led chip. When multiple micro-led chips are absorbed in the same packaging area at the same time, only one micro-led chip can have the largest contact area with the packaging area and be absorbed most firmly. At this time, under the action of vibration, only one micro-led chip is absorbed by the packaging area, and the other micro-led chips are shaken off and absorbed in other packaging areas. Or multiple micro-led chips have a small contact area with the packaging area. At this time, multiple micro-led chips are shaken off and re-absorb a micro-led chip with a larger contact area with the packaging area. The micro-led chip with a larger contact area with the packaging area refers to the micro-led chip installed in the corresponding packaging area.

[0051] In the present application, vibration can also ensure that the micro-led chip is installed at the corresponding position of the packaging area. Preferably, the packaging area corresponds to the micro-led chip in size, or the size of the packaging area is slightly larger than the micro-led chip. When only part of the micro-led chip is adsorbed to the packaging area, the adsorption force between the two is weak. At this time, the micro-led chip is not adsorbed firmly. Under the action of vibration, the micro-led chip will fall off or be moved to a position that is completely in contact with the packaging area.

[0052] In the present application, the vibration of the carrier board can be achieved by setting a support base with a vibration function inside the installation chamber; the vibration of the micro-led chip can be achieved by setting multiple blowing holes inside the installation chamber so that the suspension of the micro-led chip moves continuously inside the installation chamber. The specific position of the blowing hole can be set according to the position of the carrier board and the position of the air inlet; and the blowing air pressure in the blowing hole needs to be smaller than the adsorption force between the micro-led chip and the packaging area to ensure that it will not affect the adsorption installation between the micro-led chip and the packaging area.

[0053] Furthermore, in the present application, after the carrier board is placed in the installation chamber, and the number of micro-led chips slightly more than the number of the packaging areas is input into the installation chamber, the micro-led chips are vibrated so that they are installed in a one-to-one correspondence with the packaging areas. After the installation is completed, it also includes: leveling the micro-led chips adsorbed on the packaging areas so that the micro-led chips are in a one-to-one correspondence with the packaging areas.

[0054] In the present application, the portion outside the packaging area is covered by a protective film, and the packaging area is a recessed structure relative to the protective film, or in other words, the packaging area is also a recessed structure relative to the carrier itself, and the micro-led chip corresponding to the packaging area is adsorbed and installed inside the recessed packaging area.

[0055] A micro-led chip is adsorbed and installed in each recessed packaging area. By controlling the height of the protective film, the recessed height of the packaging area relative to the protective film is equal to the thickness of the micro-led chip, ensuring that the micro-led chip fills the packaging area when adsorbed in the packaging area. In this way, the micro-led chip protruding from the packaging area can be moved to a position exactly located in the packaging area through the leveling process, and the excess micro-led chip adsorbed in the packaging area can also be removed.

[0056] In the present application, during the micro-led chip adsorption process, a vibration method is used to ensure that the micro-led chip is adsorbed and installed in a one-to-one correspondence with the packaging area; after the adsorption is completed, after the carrier is moved out of the installation chamber, the size design of the concave height of the packaging area relative to the protective film is equal to the thickness of the micro-led chip, and a leveling process is used to make the micro-led chip fit in the packaging area, and remove the excess adsorbed micro-led chip. The vibration and leveling processes cooperate with each other to ensure that the micro-led chip is adsorbed and installed in a one-to-one correspondence with the packaging area.

[0057] The specific leveling process can be: use a soft board to scrape the adsorbed micro-led chip. As mentioned above, the recessed height of the packaging area relative to the protective film is equal to the thickness of the micro-led chip. When the micro-led chip is not completely attached to the packaging area, or multiple micro-led chips are adsorbed in the same packaging area, use a soft board to scrape the surface of the carrier board so that the micro-led chip that is not completely adsorbed in the packaging area is attached to the packaging area, and the excess micro-led chip is scraped away, so as to achieve one-to-one adsorption and installation of the micro-led chip and the packaging area.

[0058] After leveling, spot welding and curing are required to fix the micro-led chip in the packaging area.

[0059] In the present application, the micro-led chip includes a first chip, a second chip and a third chip, and the packaging area in the carrier includes a first packaging area, a second packaging area and a third packaging area; the first chip, the second chip and the third chip are sequentially adsorbed on the first packaging area, the second packaging area and the third packaging area. That is to say, after the first chip is adsorbed on the first packaging area, the first chip and the first packaging area are welded and solidified, and then the second chip is adsorbed on the second packaging area, and the second chip and the second packaging area are welded and solidified; finally, after the third chip is adsorbed on the third packaging area, the third chip and the third packaging area are welded and solidified.

[0060] Example 3

[0061] The present application provides a packaging method for a micro-led chip, wherein the micro-led chip includes an R chip, a B chip and a G chip, and the packaging area includes an R packaging area, a B packaging area and a G packaging area; and the R chip, the B chip and the G chip are distributed in a Bayer array in a carrier board. Figure 1 As shown, specifically including:

[0062] S1: Cover the carrier with a dry film, expose and develop it, so that all R packaging areas corresponding to the R chips that need to be adsorbed and installed in the carrier are exposed.

[0063] S2: Conduct electrification treatment on the R package area in the carrier board, so that the R package area is electrified and other areas are not electrified. Specifically including:

[0064] Plasma is used to etch the carrier, and the plasma can carry positive or negative charge at the same time. When the plasma used in the present application treats the surface of the carrier, the charged plasma remains in the R packaging area, so that the R packaging area is charged, while other areas will not be charged due to the insulating protective film on the surface.

[0065] S3: Place the carrier board inside the mounting chamber, and in a nitrogen atmosphere, input the R chip into the mounting chamber so that the R chip is adsorbed on the R packaging area; and weld the R chip and the R packaging area. Specifically including:

[0066] S31: By controlling the output pressure of nitrogen, the R chip can be suspended in nitrogen to form a suspension of the R chip. A nitrogen flow is input through the input port of the installation chamber to input the suspension of the R chip into the interior of the installation chamber. The interior of the installation chamber of the present application is an inert gas atmosphere, free of dust and impurities, to prevent impurities from contaminating the carrier and the R chip.

[0067] S32: A plurality of blowing holes are arranged near the top of the carrier board inside the mounting chamber, so that the suspension of the R chip is continuously vibrated inside the mounting chamber.

[0068] S33: A support base with a vibration function is provided at the bottom of the installation chamber, and the carrier is placed on the support base. After the vibration function is turned on, the carrier is in a vibrating state. The R package area corresponds to the R chip in size, or the size of the R package area is slightly larger than the R chip. When only part of the R chip is adsorbed to the R package area, the adsorption force between the two is weak. At this time, the R chip is not adsorbed firmly. Under the action of vibration, the R chip will fall off, or be moved to a position where it is completely in contact with the R package area.

[0069] S34: The R packaging area is a recessed structure relative to the dry film, and an R chip is adsorbed and installed in each recessed R packaging area. By controlling the height of the dry film, the recessed height of the R packaging area relative to the dry film is equal to the thickness of the R chip. After the adsorption is completed, the carrier is moved out of the installation chamber, and a soft board is used to scrape the surface of the carrier, so that the R chip that is not completely adsorbed in the packaging area is attached to the R packaging area, and the excess R chip is scraped away, so that the R chip and the R packaging area are adsorbed and installed one by one.

[0070] S35: Use ultraviolet light to detect the R packaging area, control the electrostatic adsorption at the end of the robot arm to implant the R chip in the area where the R chip is missing. Control the electrostatic adsorption at the end of the robot arm to remove the defective R chip and implant a new R chip in the area where the R chip is defective.

[0071] In the present application, vibration and averaging are performed during the batch adsorption process of the R chips, with the aim of making the R chips and the R packaging areas adsorbed and installed one by one. In the present application, after the adsorption is completed, a part of checking for deficiencies and filling in gaps is also included, namely step S35, which controls the electrostatic charge at the end of the robotic arm to check for deficiencies and fill in gaps in the R packaging area, as well as the replacement of damaged chips. Specifically, the electrostatic charge at the end of the robotic arm is smaller than the electrostatic charge in the packaging area, ensuring that the end of the robotic arm can adsorb the R chip, and when the R chip is attached to the R packaging area, the adsorption force between the end of the robotic arm and the R chip is smaller than the adsorption force between the R chip and the R packaging area, thereby achieving precise transfer of the R chip.

[0072] S36: Solder and fix the R chip in the R packaging area. For example, solder paste is first applied to the R chip and the R packaging area, and the R chip and the R packaging area are soldered and fixed by solder paste welding.

[0073] S4: the dry film in the B package area is etched away without repeating the exposure and development process, and steps S2-S3 are repeated so that the B chip is adsorbed on the B package area; and the B chip and the B package area are welded;

[0074] S5: the dry film in the G package area is etched away without repeating the exposure and development process, and steps S2-S3 are repeated to make the G chip adsorbed on the G package area; and the G chip and the G package area are welded.

[0075] The present application can realize batch adsorption installation of micro-led chips and packaging areas in the carrier board inside the installation chamber. In actual operation, multiple carrier board placement positions can be set inside the installation chamber, which can realize the simultaneous adsorption installation of the same type of chips in multiple carrier boards. Compared with the mass transfer technology in the prior art, the installation chamber structure of the present application is simple, easy to operate, and has high adsorption installation efficiency and low cost. When the R chip, B chip and G chip are distributed in the Bayer array in the carrier board, only three adsorption installations are required to realize the installation of micro-led chips in multiple carrier boards. The cost required for the entire packaging process is also low, which effectively reduces the packaging cost of micro-led chips and expands the application scope of micro-led display technology.

[0076] During the adsorption installation process, the present application uses vibration to ensure that the micro-led chip and the packaging area are adsorbed one-to-one. After the adsorption installation is completed, the leveling method is used to ensure that the micro-led chip and the packaging area are one-to-one and completely fitted. After the carrier is removed from the installation chamber, ultraviolet rays are used again to check for defects and fill gaps in the packaging area, so that the micro-led chip in the vacant packaging area can be installed and the defective micro-led chip can be replaced. The quality of the final adsorbed micro-led chip and the stability of the product are ensured.

[0077] It can be understood that the above embodiments only express the preferred implementation modes of the present invention, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the patent scope of the present invention. It should be pointed out that, for ordinary technicians in this field, the above technical features can be freely combined without departing from the concept of the present invention, and several deformations and improvements can be made, which all belong to the protection scope of the present invention. Therefore, all equivalent changes and modifications made to the scope of the claims of the present invention should belong to the coverage of the claims of the present invention.

Claims

1. A method for packaging a micro-led chip, characterized in that: include: Conducting electrification on the packaging area of ​​the carrier board; The part outside the packaging area is covered by a protective film. The packaging area is a recessed structure relative to the protective film, and the recessed height of the packaging area relative to the protective film is equal to the thickness of the micro-led chip. The carrier is placed inside the mounting chamber, and the micro-led chip is input into the mounting chamber under an inert gas atmosphere, so that the micro-led chip is adsorbed on the packaging area; the micro-led chip and the carrier inside the mounting chamber are in a vibrating state, wherein a plurality of blowing holes are arranged near the top of the carrier inside the mounting chamber, so that the suspension of the micro-led chip is constantly vibrated inside the mounting chamber, and the blowing air pressure in the blowing holes is less than the adsorption force between the micro-led chip and the packaging area; a support seat with a vibration function is arranged at the bottom of the mounting chamber, and the carrier is placed on the support seat; Use a soft board to scrape the adsorbed micro-led chip so that the micro-led chip corresponds to the packaging area one by one.

2. A method for packaging a micro-led chip according to claim 1, characterized in that: The installation chamber includes an air inlet, and the micro-led chip is wrapped in nitrogen to form a suspension of the micro-led chip; the suspension of the micro-led chip enters the interior of the installation chamber from the air inlet.

3. The packaging method of a micro-led chip according to claim 1, characterized in that: The charged treatment includes: subjecting the carrier to a charged treatment, or subjecting the carrier to a charged plasma treatment.

4. The packaging method of a micro-led chip according to claim 1, characterized in that: The micro-led chip includes a first chip, a second chip and a third chip, and the packaging area in the carrier includes a first packaging area, a second packaging area and a third packaging area; the first chip, the second chip and the third chip are sequentially adsorbed on the first packaging area, the second packaging area and the third packaging area.

5. A method for packaging a micro-led chip according to claim 4, characterized in that: include: S1: Covering the carrier with a dry film, exposing and developing it, so that the first packaging area is exposed; S2: performing a charging process on the first packaging area in the carrier so that the first packaging area is charged and other areas are not charged; S3: placing the carrier board inside the mounting chamber, and in an inert gas atmosphere, inputting the first chip into the mounting chamber so that the first chip is adsorbed on the first packaging area; S4: etching away the dry film in the second packaging area, and repeating steps S2-S3 so that the second chip is adsorbed in the second packaging area; S5: Etching away the dry film in the third packaging area, and repeating steps S2-S3, so that the third chip is adsorbed in the third packaging area.

6. A method for packaging a micro-led chip according to claim 5, characterized in that: Step S3 also includes welding the first chip and the first packaging area; Step S4 also includes welding the second chip and the second packaging area; Step S5 also includes welding the third chip and the third packaging area.

7. The packaging method of a micro-led chip according to claim 5, characterized in that: The first chip, the second chip and the third chip are respectively an R chip, a G chip and a B chip.

Citation Information

Patent Citations

  • Transfer method of Micro-LED chip

    CN110767582A

  • Rapid and precise chip mass transfer process

    CN112289907A

  • Micro LED chip mass transfer method, Micro LED display screen and display equipment

    CN113948617A

  • Chip mass transfer method, chip substrate and positioning plate

    CN115566115A