A semiconductor structure and its manufacturing method
By introducing oxide semiconductor materials and improving contact plug materials into the semiconductor structure, the problems of increased GIDL and increased contact resistance caused by the reduction of word line size are solved, thereby improving the driving capability of transistors and the overall performance of semiconductor structures.
Patent Information
- Application Number
- CN202210620889.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-06-01
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2042-06-01
AI Technical Summary
With the miniaturization and high integration of semiconductor structures, the reduction in word line size leads to an increase in gate-induced drain leakage current (GIDL), which degrades the current driveability of transistors and reduces the performance of semiconductor structures. At the same time, the contact area between bit line plugs and memory node plugs decreases, resulting in increased contact resistance.
In a semiconductor structure, an oxide semiconductor material is introduced as a semiconductor layer and disposed between the word line structure and the inner wall of the groove. The oxide semiconductor material is used as a channel for transmitting charge. Combined with the setting of an insulating layer, leakage current is reduced, and contact resistance is reduced by improving the contact plug material.
It effectively alleviates or eliminates GIDL leakage current, improves the transistor's on/off current ratio and current driveability, reduces power consumption, and enhances the performance of the semiconductor structure.
Smart Images

Figure CN117219655B_ABST
Abstract
Description
Technical Field
[0001] This disclosure relates to the field of semiconductor manufacturing, and more particularly to a semiconductor structure and a method for manufacturing the same. Background Technology
[0002] Semiconductor structures, such as dynamic random access memory (DRAM), typically include transistors and embedded word lines that control the switching on and off of the transistors.
[0003] However, as semiconductor structures continue to evolve towards miniaturization and high integration, the size of word lines is further reduced, which leads to an increase in gate-induced drain leakage current (GIDL), degrading the current driveability of transistors and thus reducing the performance of semiconductor structures. Summary of the Invention
[0004] This disclosure provides a semiconductor structure, including: Substrate; Multiple grooves, the grooves being located within the substrate and extending along a first direction; Multiple character line structures, wherein the character line structures are located within the groove; A plurality of semiconductor layers, wherein at least partially located between the word line structure and the inner wall of the groove; wherein the semiconductor layers comprise an oxide semiconductor material.
[0005] In some embodiments, the oxide semiconductor material includes In x Ga y Zn 1-x-y O, where x is greater than or equal to 0 or less than or equal to 1, and y is greater than or equal to 0 or less than or equal to 1.
[0006] In some embodiments, the semiconductor structure further includes an insulating layer, the insulating layer being located at least between the substrate and the semiconductor layer.
[0007] In some embodiments, the substrate includes an isolation structure and a plurality of discrete active regions separated by the isolation structure, the extension direction of the active regions intersecting the first direction, two adjacent grooves separating the active regions into two ends and an intermediate region, the grooves exposing the active regions; wherein the orthographic projection of the semiconductor layer on the substrate plane at least partially overlaps with the orthographic projection of the active regions on the substrate plane.
[0008] In some embodiments, the insulating layer covers the bottom surface of the groove and a portion of the sidewalls, and the upper surface of the insulating layer on the sidewalls is lower than the upper surface of the substrate. The semiconductor layer covers the insulating layer and the area of the sidewalls of the groove not covered by the insulating layer, and contacts the exposed area.
[0009] In some embodiments, the semiconductor layer includes a first sublayer, a second sublayer, and a third sublayer, wherein the first sublayer covers the bottom surface and sidewalls of the groove, and the second and third sublayers are located on both sides of the groove and cover a portion of the upper surface of the substrate.
[0010] In some embodiments, the semiconductor structure further includes: a plurality of bit line structures located on the substrate, the plurality of bit line structures extending along a second direction intersecting the first direction; and a first contact plug located below the bit line structures and above the second sublayer, the first contact plug being electrically connected to the bit line structures and the second sublayer.
[0011] In some embodiments, the bit line structure includes: a bit line, a bit line capping layer, and a bit line sidewall layer, wherein the bit line capping layer covers the upper surface of the bit line, and the bit line sidewall layer covers the bit line capping layer, the bit line, and the sidewall of the first contact plug.
[0012] In some embodiments, it also includes: Multiple second contact plugs and multiple contact pads, wherein the second contact plugs are located below the contact pads and are in contact with the third sublayer.
[0013] This disclosure also provides a method for manufacturing a semiconductor structure, including: Provide substrate; A groove extending in a first direction is formed within the substrate; A semiconductor layer is formed, the semiconductor layer at least partially covering the inner wall of the groove; wherein the material of the semiconductor layer includes an oxide semiconductor material; A word line structure is formed, the word line structure being located within the groove and at least partially covering the semiconductor layer.
[0014] In some embodiments, forming a groove extending in a first direction within the substrate includes: The substrate is etched to form isolation trenches, which divide the substrate into multiple discrete active regions; A filling layer is formed within the isolation trench to create an isolation structure; The active region and the isolation structure are etched to form a plurality of grooves extending along a first direction, and each active region is separated into a middle region and two ends by two adjacent grooves.
[0015] In some embodiments, a semiconductor layer is formed that at least partially covers the sidewalls of the recess, including: A semiconductor material layer is formed, the semiconductor material layer covering the inner wall of the groove and the upper surface of the substrate; Remove the semiconductor material layer covering the upper surface of the substrate; A semiconductor material layer is etched onto the inner wall of the groove to form a plurality of discrete semiconductor layers, each of which covers the sidewall and bottom surface of the groove, and the projection of each semiconductor layer onto the substrate plane at least partially overlaps with the projection of the active region onto the substrate plane.
[0016] In some embodiments, prior to forming the semiconductor layer, the method further includes: An insulating layer is formed, which covers the inner wall of the groove and the upper surface of the substrate; Remove the insulating layer located on the upper surface of the substrate; The insulating layer covering the sidewall of the groove is etched such that the upper surface of the insulating layer on the sidewall of the groove is lower than the upper surface of the substrate.
[0017] In some embodiments, a semiconductor layer is formed that at least partially covers the sidewalls of the recess, including: A semiconductor material layer is formed, the semiconductor material layer covering the inner wall of the groove and the upper surface of the substrate; The semiconductor material layer is etched to form a plurality of discrete semiconductor layers, the projection of the semiconductor layer on the substrate plane at least partially overlapping the projection of the active region on the substrate plane, each semiconductor layer including a first sublayer, a second sublayer and a third sublayer, wherein the first sublayer covers the bottom surface and sidewalls of the groove, and the second sublayer and the third sublayer are located on both sides of the groove and cover the upper surface of the substrate portion.
[0018] In some embodiments, prior to forming the semiconductor layer, the method further includes: An insulating layer is formed, which covers the inner wall of the groove and the upper surface of the substrate.
[0019] In some embodiments, after forming the word line structure, the method further includes: Forming a dielectric layer; The dielectric layer is etched to form a first contact hole, which exposes the second sublayer. A first contact plug is formed in the first contact hole, and the first contact plug contacts the second sub-layer; Multiple bit line structures are formed extending along a second direction, and the bit line structures are in electrical contact with the top of the first contact plug.
[0020] In some embodiments, after forming the bit line structure, the method further includes: Multiple isolation fences are formed extending along a first direction, the multiple isolation fences and the multiple bit line structures forming multiple openings, and the third sublayer is exposed from the openings; A second contact plug is formed within the opening, and the second contact plug contacts the third sublayer.
[0021] The semiconductor structure and its manufacturing method provided in this disclosure include: a substrate; a plurality of grooves located within the substrate and extending along a first direction; a plurality of word line structures located within the grooves; and a plurality of semiconductor layers, at least partially located between the word line structures and the inner walls of the grooves; wherein the semiconductor layers comprise an oxide semiconductor material. The semiconductor structure provided in this disclosure includes a semiconductor layer disposed between the word line structures and the inner walls of the grooves. The material of the semiconductor layer comprises an oxide semiconductor material, which can serve as a channel for charge transport. The oxide semiconductor material has higher carrier mobility and lower leakage current, thus effectively mitigating or eliminating GIDL leakage, improving the transistor's on / off current ratio and current driveability, thereby improving the driving capability of the word line structures for transistors, reducing power consumption, and improving the performance of the semiconductor structure.
[0022] Details of one or more embodiments of this disclosure are set forth in the following drawings and description. Other features and advantages of this disclosure will become apparent from the accompanying drawings and claims. Attached Figure Description
[0023] To more clearly illustrate the technical solutions of the embodiments of this disclosure, the drawings used in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of this disclosure. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0024] Figure 1a This is a top view schematic diagram of a semiconductor structure provided in an embodiment of this disclosure. Figure 1b For along Figure 1a A schematic diagram of the cross-sectional structure taken by line A-A'. Figure 1c For along Figure 1a A schematic diagram of the cross-sectional structure taken by line B-B'; Figure 2a This is a top view schematic diagram of a semiconductor structure provided in another embodiment of the present disclosure. Figure 2b For along Figure 2a A schematic diagram of the cross-sectional structure taken by line A-A'. Figure 2c For along Figure 2a A schematic diagram of the cross-sectional structure taken by line B-B'; Figure 3 A flowchart illustrating a method for manufacturing a semiconductor structure according to an embodiment of this disclosure; Figures 4 to 16 The steps in the method for manufacturing the semiconductor structure provided in the embodiments of this disclosure are as follows: Figure 1a A schematic diagram of the cross-sectional structure taken by line A-A'; Figures 17 to 25 The steps in the method for manufacturing a semiconductor structure provided in another embodiment of this disclosure are as follows: Figure 2a A schematic diagram of the cross-sectional structure taken by line A-A'. Detailed Implementation
[0025] Exemplary embodiments of the present disclosure will now be described in more detail with reference to the accompanying drawings. While exemplary embodiments of the present disclosure are shown in the drawings, it should be understood that the present disclosure may be implemented in various forms and should not be limited to the specific embodiments set forth herein. Rather, these embodiments are provided so that this disclosure will be thorough and complete, and will fully convey the scope of the disclosure to those skilled in the art.
[0026] In the following description, numerous specific details are set forth in order to provide a more thorough understanding of this disclosure. However, it will be apparent to those skilled in the art that this disclosure may be practiced without one or more of these details. In other instances, to avoid confusion with this disclosure, certain technical features well-known in the art have not been described; that is, not all features of actual embodiments are described herein, nor are well-known functions and structures described in detail.
[0027] In the accompanying drawings, for clarity, the dimensions of layers, areas, and elements, as well as their relative dimensions, may be exaggerated. The same reference numerals denote the same elements throughout.
[0028] It should be understood that when an element or layer is referred to as "on," "adjacent to," "connected to," or "coupled to" other elements or layers, it may be directly on, adjacent to, connected to, or coupled to other elements or layers, or there may be intervening elements or layers. Conversely, when an element is referred to as "directly on," "directly adjacent to," "directly connected to," or "directly coupled to" other elements or layers, there are no intervening elements or layers. It should be understood that although the terms first, second, third, etc., may be used to describe various elements, components, areas, layers, and / or portions, these elements, components, areas, layers, and / or portions should not be limited by these terms. These terms are only used to distinguish one element, component, area, layer, or portion from another element, component, area, layer, or portion. Therefore, without departing from the teachings of this disclosure, the first element, component, area, layer, or portion discussed below may be referred to as a second element, component, area, layer, or portion. And the discussion of a second element, component, area, layer, or portion does not imply that the first element, component, area, layer, or portion necessarily exists in this disclosure.
[0029] Spatial relation terms such as “below,” “under,” “below,” “below,” “above,” “above,” etc., are used herein for convenience of description to describe the relationship between one element or feature shown in the figure and other elements or features. It should be understood that, in addition to the orientation shown in the figure, spatial relation terms are intended to also include different orientations of the device in use and operation. For example, if the device in the figure is flipped, then the element or feature described as “below” or “below” other elements or features will be oriented “above” other elements or features. Therefore, the exemplary terms “below” and “under” can include both upper and lower orientations. The device may be otherwise oriented (rotated 90 degrees or otherwise) and the spatial descriptive terms used herein will be interpreted accordingly.
[0030] The terminology used herein is for the purpose of describing particular embodiments only and is not intended to limit this disclosure. When used herein, the singular forms “a,” “an,” and “the” are also intended to include the plural forms unless the context clearly indicates otherwise. It should also be understood that the terms “comprise” and / or “comprising,” when used in this specification, identify the presence of the stated features, integers, steps, operations, elements, and / or components, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, components, and / or groups. When used herein, the term “and / or” includes any and all combinations of the associated listed items.
[0031] Semiconductor structures, such as dynamic random access memory (DRAM), typically include transistors, embedded word line structures, bit line structures, and information storage structures. The word line structures control the switching on and off of the transistors, the bit line structures are electrically connected to the drain of the transistors via bit line plugs, and the information storage structures are electrically connected to the source of the transistors via storage node plugs.
[0032] However, as semiconductor structures continue to evolve towards miniaturization and high integration, the size of word lines is further reduced, leading to an increase in gate-induced drain leakage current (GIDL), which degrades the current-driven capability of transistors and thus reduces the performance of the semiconductor structure. Simultaneously, with the shrinking of bit line plugs and memory node plugs, the contact area between the bit line plugs / memory node plugs and transistors decreases, resulting in increased contact resistance. Furthermore, in related technologies, the material for bit line plugs and memory node plugs is polycrystalline silicon, which has a relatively high contact resistance with the source and drain regions.
[0033] Based on this, the following technical solutions of the embodiments of this disclosure are proposed. The specific implementation methods of this disclosure will be described in detail below with reference to the accompanying drawings. In the detailed description of the embodiments of this disclosure, for ease of explanation, the schematic diagrams may be partially enlarged without adhering to general proportions, and the schematic diagrams are merely examples and should not limit the scope of protection of this disclosure.
[0034] Figure 1a This is a top view schematic diagram of a semiconductor structure provided in an embodiment of this disclosure. Figure 1b For along Figure 1a A schematic diagram of the cross-sectional structure taken by line A-A'. Figure 1c For along Figure 1a A schematic diagram of the cross-sectional structure taken by line B-B'; Figure 2a This is a top view schematic diagram of a semiconductor structure provided in another embodiment of the present disclosure. Figure 2b For along Figure 2a A schematic diagram of the cross-sectional structure taken by line A-A'. Figure 2c For along Figure 2a A schematic diagram of the cross-sectional structure taken by line B-B'. The following is combined with... Figures 1a to 2c The semiconductor structure provided in the embodiments of this disclosure will be further described.
[0035] As shown in the figure, the semiconductor structure includes: a substrate 10; a plurality of grooves 12 located within the substrate 10 and extending along a first direction; a plurality of word line structures 15 located within the grooves 12; and a plurality of semiconductor layers 14, at least partially located between the word line structures 15 and the inner walls of the grooves 12; wherein the semiconductor layers 14 comprise an oxide semiconductor material.
[0036] In practice, the semiconductor structure provided in this disclosure embodiment can be a three-dimensional dynamic random access memory (3DDRAM), but is not limited thereto. The semiconductor structure can also be any semiconductor structure with a buried gate.
[0037] The substrate may be a semiconductor substrate, and may include at least one elemental semiconductor material (e.g., a silicon (Si) substrate, a germanium (Ge) substrate), at least one III-V compound semiconductor material, at least one II-VI compound semiconductor material, at least one organic semiconductor material, or other semiconductor materials known in the art. In one specific embodiment, the substrate is a silicon substrate, which may be doped or undoped.
[0038] The plurality of grooves 12 are arranged along a second direction intersecting the first direction. In some embodiments, the first and second directions are perpendicular. However, this is not a limitation; the first direction may also be oblique to the second direction.
[0039] In one embodiment, the substrate 10 includes an isolation structure 11 and a plurality of discrete active regions AA separated by the isolation structure 11. The extending direction of the active regions AA intersects the first direction. Two adjacent grooves 12 separate the active regions AA into two ends and a middle region, and the grooves 12 expose the active regions AA. Specifically, as shown... Figures 1a to 1b As shown, the isolation structure 11 is disposed between the plurality of parallel active regions AA, and the groove 12 passes through the active regions AA and the isolation structure 11. The material of the isolation structure 11 includes one or more of oxides (e.g., silicon oxide), nitrides (e.g., silicon nitride), and oxynitrides (e.g., silicon oxynitride).
[0040] In one embodiment, the active region AA includes a first source / drain doped region d1 located at both ends and a second source / drain doped region d2 located in the middle region, the first source / drain doped region d1 and the second source / drain doped region d2 being separated by the groove 12. The first source / drain doped region d1 and the second source / drain doped region d2 may have the same doping type, and the doping type of the first source / drain doped region d1 and the second source / drain doped region d2 may be different from the doping type of the substrate 10.
[0041] In one embodiment, the orthographic projection of the semiconductor layer 14 onto the plane of the substrate 10 at least partially overlaps with the orthographic projection of the active region AA onto the plane of the substrate 10. In some embodiments, the semiconductor layer 14 covers at least a portion of the surface of the active region AA exposed by the recess 12, and the first source / drain doped region d1 and the second source / drain doped region d2 are located on opposite sides of the semiconductor layer 14 and in contact with the semiconductor layer 14. The upper surface of the semiconductor layer 14 is lower than the upper surface of the substrate 10, or the upper surface of the semiconductor layer 14 is flush with the upper surface of the substrate 10.
[0042] In this embodiment of the present disclosure, a semiconductor layer 14 is disposed between the word line structure 15 and the substrate 10. The semiconductor layer 14 is made of an oxide semiconductor material, which can serve as a channel for transmitting charge. The oxide semiconductor material has higher carrier mobility and lower leakage current, thus effectively alleviating or eliminating GIDL leakage phenomenon, improving the transistor's on / off current ratio and current driveability, thereby improving the driving capability of the word line structure 15 for the transistor, reducing power consumption, and improving the performance of the semiconductor structure.
[0043] In one embodiment, the oxide semiconductor material includes In x Ga y Zn 1-x-y O, where x is greater than or equal to 0 or less than or equal to 1, and y is greater than or equal to 0 or less than or equal to 1, such as materials with the chemical formula InGaZnO4. However, it is not limited to this; the oxide semiconductor material also includes at least one of the following: indium oxide, tin oxide, In-Zn oxides, Sn-Zn oxides, Al-Zn oxides, In-Ga oxides, In-Al-Zn oxides, In-Sn-Zn oxides, Sn-Ga-Zn oxides, Al-Ga-Zn oxides, and Sn-Al-Zn oxides.
[0044] However, the oxide semiconductor material may also include at least one of the following: In-Hf-Zn oxides, In-La-Zn oxides, In-Ce-Zn oxides, In-Pr-Zn oxides, In-Nd-Zn oxides, In-Sm-Zn oxides, In-Eu-Zn oxides, In-Gd-Zn oxides, In-Tb-Zn oxides, In-Dy-Zn oxides, In-Ho-Zn oxides, In-Er-Zn oxides, In-Tm-Zn oxides, In-Yb-Zn oxides, and In-Lu-Zn oxides; and quaternary metal oxides such as In-Sn-Ga-Zn oxides, In-Hf-Ga-Zn oxides, In-Al-Ga-Zn oxides, In-Sn-Al-Zn oxides, In-Sn-Hf-Zn oxides, and In-Hf-Al-Zn oxides.
[0045] Optionally, the oxide semiconductor material can be an undoped oxide semiconductor material or a doped oxide semiconductor material. Specifically, the dopant used to dope the oxide semiconductor material is one or more of boron, nitrogen, phosphorus, and arsenic, or one or more of helium, neon, argon, krypton, and xenon, or the dopant is hydrogen; but it is not limited to these, and the dopant can also be a combination of the above materials as needed.
[0046] In one embodiment, the semiconductor layer 14 is p-type doped. However, it is not limited thereto; the semiconductor layer 14 may also be n-type doped. It is understood that when the semiconductor layer 14 is p-type doped, the first source / drain doped region d1 and the second source / drain doped region d2 are n-type doped; conversely, when the semiconductor layer 14 is n-type doped, the first source / drain doped region d1 and the second source / drain doped region d2 are p-type doped.
[0047] In one embodiment, the semiconductor structure further includes an insulating layer 13, the insulating layer 13 being located at least between the substrate 10 and the semiconductor layer 14. Figure 1bAs shown, in some embodiments, the insulating layer 13 covers the bottom surface and part of the sidewalls of the groove 12, and the upper surface of the insulating layer 13 on the sidewalls is lower than the upper surface of the substrate 10. The semiconductor layer 14 covers the insulating layer 13 and the area of the sidewalls of the groove 12 not covered by the insulating layer 13, and contacts the exposed area. By providing the insulating layer 13 between the substrate 10 and the semiconductor layer 14, embodiments of this disclosure can effectively reduce channel leakage current and GIDL leakage current. The material of the insulating layer 13 includes oxides, such as silicon oxide. The insulating layer 13 can be formed using a thermal oxidation process, such as a furnace tube wet oxidation process or an in-situ steam generation (ISSG) process. It is understood that when the insulating layer 13 is formed using a thermal oxidation process, the insulating layer 13 covers at least a portion of the surface of the active region AA exposed by the groove 12. However, it is not limited to this; the insulating layer 13 can also be formed using a chemical vapor deposition (CVD) process.
[0048] The number of the character line structures 15 is multiple, and the multiple character line structures 15 are arranged along the second direction. For example... Figure 2b As shown, the word line structure 15 includes a conductive layer 152 and a gate dielectric layer 151 sandwiched between the conductive layer 152 and the semiconductor layer 14. The conductive layer 152 is made of materials including tungsten (W), copper (Cu), titanium (Ti), tantalum (Ta), titanium nitride (TiN), tantalum nitride (TaN), metal silicides, metal alloys, or any combination thereof, such as titanium nitride (TiN). The gate dielectric layer 151 can be made of a high dielectric constant material, such as tantalum oxide, hafnium oxide, zirconium oxide, niobium oxide, titanium oxide, barium oxide, strontium oxide, yttrium oxide, lanthanum oxide, praseodymium oxide, or barium strontium titanate. The use of a high dielectric constant material as the gate dielectric layer 151 in this embodiment can further improve the current driveability of the transistor.
[0049] In one embodiment, the upper surface of the word line structure 15 is lower than the upper surface of the substrate 10, and the semiconductor structure further includes a word line capping layer 16 that covers the word line structure 15. The material of the word line capping layer 16 includes titanium nitride.
[0050] like Figure 1b and Figure 1cAs shown, in one embodiment, the semiconductor structure further includes: a plurality of bit line structures 19 located on the substrate 10, the plurality of bit line structures 19 extending along a second direction and arranged along a first direction; and a first contact plug 18 located below the bit line structures 19 and above the second source / drain doped region d2, the first contact plug 18 electrically connecting the bit line 191 and the second source / drain doped region d2. Specifically, the bit line structure 19 includes: a bit line 191, a bit line capping layer 192, and a bit line sidewall layer 193, the bit line capping layer 192 covering the upper surface of the bit line 191, and the bit line sidewall layer 193 covering the bit line capping layer 192, the bit line 191, and the sidewalls of the first contact plug 18. The material of the first contact plug 18 includes polycrystalline silicon. The bit line 191 includes a titanium nitride layer and a tungsten layer located on the titanium nitride layer. The materials of the bit line capping layer 193 and the bit line sidewall layer 193 include silicon nitride.
[0051] In one embodiment, the semiconductor structure further includes: a dielectric layer 17, at least partially located between the bit line structure 19 and the substrate 10; and a trench S located below the bit line structure 19, the trench S being formed by removing a portion of the dielectric layer 17, a portion of a second source / drain doped region d2 located below the portion of the dielectric layer 17, a portion of a word line capping layer 16, and a portion of an isolation structure 11. A first contact plug 18 is located within the trench S, and the upper surface of the first contact plug 18 is flush with the upper surface of the trench S. A gap exists between the first contact plug 18 and the substrate 10 and the dielectric layer 17, and the bit line sidewall layer 192 fills the gap. The material of the dielectric layer 17 includes silicon nitride.
[0052] like Figures 1a to 1c As shown, in one embodiment, the semiconductor structure further includes a plurality of second contact plugs 23 and a plurality of contact pads 24. The second contact plugs 23 are located below the contact pads 24 and are connected to the first source / drain doped region d1. In some embodiments, the material of the second contact plugs 23 is titanium nitride, which has better conductivity than polycrystalline silicon mentioned in related technologies, resulting in lower contact resistance between the second contact plugs 23 and the first source / drain doped region d1. However, it is not limited to this; the material of the second contact plugs 23 can also be other materials with good conductivity, such as tungsten, tungsten nitride, titanium, etc. The material of the contact pads 24 includes tungsten. The material of the isolation barrier 21 includes silicon nitride.
[0053] In one embodiment, the semiconductor structure further includes: a plurality of isolation barriers 21 located above the substrate 10, the plurality of isolation barriers 21 extending along a first direction and arranged along a second direction, a plurality of bit line structures 19 intersecting with the plurality of isolation barriers 21 to define a plurality of openings 22, and a second contact plug 23 being at least partially located in one of these openings 22. Figure 1c As shown, the second contact plug 23 also covers a portion of the top and a portion of the sidewalls of the bit line structure 19, and the contact pad 24 covers the upper surface of the second contact plug 23. The material of the isolation barrier 21 includes silicon nitride.
[0054] Figures 1a to 1c The semiconductor layer 14 shown covers only the bottom surface and at least part of the sidewalls of the recess 12. In another embodiment of this disclosure, the semiconductor layer 14 also covers part of the upper surface of the substrate 10.
[0055] like Figures 2a to 2c As shown, specifically, the semiconductor layer 14 includes a first sublayer 141, a second sublayer 142, and a third sublayer 143. The first sublayer 141 covers the bottom surface and sidewalls of the groove 12. The second sublayer 142 and the third sublayer 143 are located on both sides of the groove 12 and cover the upper surface of the substrate 10. In some embodiments, each semiconductor layer 14 includes two first sublayers 141, one second sublayer 142, and two third sublayers 143. The two third sublayers 143 are located at both ends of the semiconductor layer 14, and the second sublayer 142 is located in the middle region of the semiconductor layer 14. The second sublayer 142 and the third sublayer 143 are spaced apart by the first sublayer 141, and both ends of the first sublayer 141 are connected to the second sublayer 142 and the third sublayer 143, respectively.
[0056] In this embodiment of the present disclosure, a first sub-layer 141 is disposed between the word line structure 15 and the substrate 10, and a second sub-layer 142 and a third sub-layer 143 are disposed on the substrate. The second sub-layer 142, the first sub-layer 141, and the third sub-layer 143 can form a current transmission path. The materials of the first sub-layer, the second sub-layer 142, and the third sub-layer 143 include oxide semiconductor materials. The oxide semiconductor materials have higher carrier mobility and lower leakage current. In this way, leakage current such as GIDL can be effectively reduced, the on / off current ratio and current driveability of the transistor can be improved, thereby improving the driving capability of the word line structure 15 for the transistor, reducing power consumption, and improving the performance of the semiconductor structure.
[0057] In one embodiment, the orthographic projection of the semiconductor layer 14 onto the plane of the substrate 10 at least partially overlaps with the orthographic projection of the active region AA onto the plane of the substrate 10. In some embodiments, the first sublayer 141 at least covers the portion of the surface of the active region AA exposed by the groove 12, the second sublayer 142 at least covers a portion of the upper surface of the two ends of the active region AA, and the third sublayer 143 at least covers a portion of the upper surface of the middle region of the active region AA.
[0058] In one embodiment, the first sublayer 141 is p-type doped, and the second sublayer 142 and the third sublayer 143 are n-type doped; or, the first sublayer 141 is n-type doped, and the second sublayer 142 and the third sublayer 143 are p-type doped.
[0059] In one embodiment, the insulating layer 13 is located between the first sub-layer 141 and the substrate 10, thereby effectively reducing channel leakage current and GIDL leakage current. Figure 2b and Figure 2c As shown, in some embodiments, the insulating layer 13 covers the inner wall of the groove 12 and the surface of the substrate 10, that is, the insulating layer 13 is also located between the second sub-layer 142, the third sub-layer 143 and the substrate 10, which can further reduce leakage current.
[0060] In this embodiment, the upper surface of the word line structure 15 is lower than the upper surfaces of the second sub-layer 142 and the third sub-layer 143, and the word line cover layer 16 covers the word line structure 15 and fills the gaps between the plurality of second sub-layers 142 and the plurality of third sub-layers 143.
[0061] In one embodiment, the semiconductor structure further includes: a plurality of bit line structures 19 located on the substrate 10, the plurality of bit line structures 19 extending along a second direction intersecting the first direction; and a first contact plug 18 located below the bit line structures 19 and above the second sub-layer 142, the first contact plug 18 electrically connecting the bit line structures 19 and the second sub-layer 142. Specifically, the bit line structure includes: a bit line 191, a bit line capping layer 192, and a bit line sidewall layer 193, the bit line capping layer 192 covering the upper surface of the bit line 191, and the bit line sidewall layer 193 covering the bit line capping layer 192, the bit line 191, and the sidewalls of the first contact plug 18. In one embodiment, the material of the first contact plug 18 is titanium nitride, which has better conductivity than polycrystalline silicon mentioned in related technologies, resulting in a lower contact resistance between the first contact plug 18 and the second sub-layer 142. The material of the bit line 191 includes tungsten.
[0062] like Figure 1cAs shown, in one embodiment, the semiconductor structure further includes a dielectric layer 17 located between the bit line 191 and the substrate 10, and the bit line sidewall layer 193 also covers the sidewalls of the dielectric layer 17.
[0063] In one embodiment, the semiconductor structure further includes a plurality of second contact plugs 23 and a plurality of contact pads 24, wherein the second contact plugs 23 are located below the contact pads 24 and are in contact with the third sublayer 143. In one embodiment, the material of the second contact plugs 23 is titanium nitride, which has better conductivity than polycrystalline silicon mentioned in related technologies, resulting in lower contact resistance between the second contact plugs 23 and the third sublayer 143. The material of the contact pads 24 includes tungsten.
[0064] In this embodiment, the first contact plug 18 contacts the second sub-layer 142 of the semiconductor layer 14, and the second contact plug 19 contacts the third sub-layer 143 of the semiconductor layer 14. The semiconductor layer 14 is made of an oxide semiconductor material, which has higher carrier mobility and lower leakage current. Compared with the embodiment in which the first contact plug 18 and the second contact plug 19 are in direct contact with the active region AA, this embodiment further reduces leakage current and contact resistance, and improves the performance of the semiconductor structure.
[0065] This disclosure also provides a method for manufacturing a semiconductor structure, such as... Figure 3 As shown, the method includes the following steps: Step 301: Provide a substrate; Step 302: Form a groove extending in a first direction within the substrate; Step 303: Form a semiconductor layer, the semiconductor layer at least partially covering the inner wall of the groove; wherein the material of the semiconductor layer includes an oxide semiconductor material; Step 304: Form a word line structure, wherein the word line structure is located within the groove and at least partially covers the semiconductor layer.
[0066] The following is combined with Figures 4 to 25 The method for manufacturing the semiconductor structure provided in the embodiments of this disclosure will be further described in detail.
[0067] First, perform step 301, such as... Figure 4 As shown, a substrate 10 is provided.
[0068] The substrate may be a semiconductor substrate, and may include at least one elemental semiconductor material (e.g., a silicon (Si) substrate, a germanium (Ge) substrate), at least one III-V compound semiconductor material, at least one II-VI compound semiconductor material, at least one organic semiconductor material, or other semiconductor materials known in the art. In one specific embodiment, the substrate is a silicon substrate, which may be doped or undoped.
[0069] Next, proceed to step 302, as follows: Figure 5 As shown, a groove 12 extending in a first direction is formed in the substrate 10.
[0070] Specifically, a groove 12 extending in a first direction is formed within the substrate 10, including: The substrate 10 is etched to form an isolation trench T, which divides the substrate 10 into a plurality of discrete active regions AA; An isolation structure 11 is formed by forming a filling layer within the isolation trench T; The active region AA and the isolation structure 11 are etched to form a plurality of grooves 12 extending along a first direction, and each active region AA is separated into a middle region and two ends by two adjacent grooves 12.
[0071] Multiple active regions AA are arranged in parallel, and multiple grooves 12 are arranged along a second direction intersecting the first direction. Each groove 12 passes through the active region AA and the isolation structure 11 and exposes the active region AA and the isolation structure 11. The material of the isolation structure 11 includes one or more of oxides (e.g., silicon oxide), nitrides (e.g., silicon nitride), and oxynitrides (e.g., silicon oxynitride). In some embodiments, the first direction and the second direction are perpendicular. However, this is not a limitation; the first direction may also be oblique to the second direction.
[0072] In one embodiment, the method further includes performing a doping process on the active region AA to form a first source / drain doped region d1 at both ends of the active region AA and a second source / drain doped region d2 in the middle region of the active region AA, wherein the first source / drain doped region d1 and the second source / drain doped region d2 are separated by the groove 12. The doping types of the first source / drain doped region d1 and the second source / drain doped region d2 may be the same, and the doping types of the first source / drain doped region d1 and the second source / drain doped region d2 may be different from the doping type of the substrate 10.
[0073] Next, proceed to step 303, as follows: Figures 8 to 9A semiconductor layer 14 is formed, which at least partially covers the inner wall of the groove 12; wherein the material of the semiconductor layer 14 includes an oxide semiconductor material.
[0074] Specifically, a semiconductor layer 14 is formed, which at least partially covers the sidewalls of the recess 12, including: A semiconductor material layer 14' is formed, which covers the inner wall of the groove 12 and the upper surface of the substrate 10, such as... Figure 8 As shown; Remove the semiconductor material layer 14' covering the upper surface of the substrate 10; etch the semiconductor material layer 14' remaining on the inner wall of the groove 12 to form a plurality of discrete semiconductor layers 14, each of the semiconductor layers 14 covering the sidewall and bottom surface of the groove 12, and the projection of each semiconductor layer 14 on the plane of the substrate 10 at least partially overlaps with the projection of the active region AA on the plane of the substrate 10.
[0075] The semiconductor layer 14 covers at least a portion of the surface of the active region AA exposed by the groove 12. The first source / drain doped region d1 and the second source / drain doped region d2 are located on opposite sides of the semiconductor layer 14 and are in contact with the semiconductor layer 14. The upper surface of the semiconductor layer 14 is lower than the upper surface of the substrate 10, or the upper surface of the semiconductor layer 14 is flush with the upper surface of the substrate 10. The oxide semiconductor material layer can be formed by sputtering, coating, printing, evaporation, PCVD, PLD, ALD, or MBE, etc.
[0076] In one embodiment, the oxide semiconductor material includes In x Ga y Zn 1-x-y O, where x is greater than or equal to 0 or less than or equal to 1, and y is greater than or equal to 0 or less than or equal to 1, such as materials with the chemical formula InGaZnO4. However, it is not limited to this; the oxide semiconductor material also includes at least one of the following: indium oxide, tin oxide, In-Zn oxides, Sn-Zn oxides, Al-Zn oxides, In-Ga oxides, In-Al-Zn oxides, In-Sn-Zn oxides, Sn-Ga-Zn oxides, Al-Ga-Zn oxides, and Sn-Al-Zn oxides.
[0077] However, the oxide semiconductor material may also include at least one of the following: In-Hf-Zn oxides, In-La-Zn oxides, In-Ce-Zn oxides, In-Pr-Zn oxides, In-Nd-Zn oxides, In-Sm-Zn oxides, In-Eu-Zn oxides, In-Gd-Zn oxides, In-Tb-Zn oxides, In-Dy-Zn oxides, In-Ho-Zn oxides, In-Er-Zn oxides, In-Tm-Zn oxides, In-Yb-Zn oxides, and In-Lu-Zn oxides; and quaternary metal oxides such as In-Sn-Ga-Zn oxides, In-Hf-Ga-Zn oxides, In-Al-Ga-Zn oxides, In-Sn-Al-Zn oxides, In-Sn-Hf-Zn oxides, and In-Hf-Al-Zn oxides.
[0078] Optionally, the oxide semiconductor material can be an undoped oxide semiconductor material or a doped oxide semiconductor material. Specifically, the dopant used to dope the oxide semiconductor material is one or more of boron, nitrogen, phosphorus, and arsenic, or one or more of helium, neon, argon, krypton, and xenon, or the dopant is hydrogen; but it is not limited to these, and the dopant can also be a combination of the above materials as needed.
[0079] In one embodiment, the semiconductor layer 14 is p-type doped. However, it is not limited thereto; the semiconductor layer 14 may also be n-type doped. It is understood that when the semiconductor layer 14 is p-type doped, the first source / drain doped region d1 and the second source / drain doped region d2 are n-type doped; conversely, when the semiconductor layer 14 is n-type doped, the first source / drain doped region d1 and the second source / drain doped region d2 are p-type doped.
[0080] like Figures 6 to 7 As shown, in one embodiment, before forming the semiconductor layer 14, the method further includes: An insulating layer 13 is formed, which covers the inner wall of the groove 12 and the upper surface of the substrate 10; Remove the insulating layer 13 located on the upper surface of the substrate 10; etch the insulating layer 13 covering the sidewall of the groove 12 such that the upper surface of the insulating layer 13 located on the sidewall of the groove 12 is lower than the upper surface of the substrate 10.
[0081] See you again Figure 9The semiconductor layer 14 covers the insulating layer 13 and at least a portion of the sidewalls of the recess 12 not covered by the insulating layer 13. By providing the insulating layer 13 between the substrate 10 and the semiconductor layer 14, embodiments of this disclosure can effectively reduce channel leakage current and GIDL leakage current. The insulating layer 13 is made of oxides, such as silicon oxide. The insulating layer 13 can be formed using thermal oxidation processes, such as furnace tube wet oxidation or in-situ steam generation (ISSG). It is understood that when the insulating layer 13 is formed using a thermal oxidation process, the insulating layer 13 covers at least a portion of the surface of the active region AA exposed by the recess 12. However, it is not limited to this; the insulating layer 13 can also be formed using a chemical vapor deposition (CVD) process.
[0082] Next, proceed to step 304, as follows: Figure 10 As shown, a word line structure 15 is formed, which is located within the groove 12 and at least partially covers the semiconductor layer 14.
[0083] Specifically, there are multiple word line structures 15, and these multiple word line structures 15 are arranged along a second direction. In some embodiments, each word line structure 15 includes a conductive layer 152 and a gate dielectric layer 151 sandwiched between the conductive layer 152 and the semiconductor layer 14. The material of the conductive layer 152 includes tungsten (W), copper (Cu), titanium (Ti), tantalum (Ta), titanium nitride (TiN), tantalum nitride (TaN), metal silicides, metal alloys, or any combination thereof, such as titanium nitride (TiN). The material of the gate dielectric layer 151 can be a high dielectric constant material, such as tantalum oxide, hafnium oxide, zirconium oxide, niobium oxide, titanium oxide, barium oxide, strontium oxide, yttrium oxide, lanthanum oxide, praseodymium oxide, or barium strontium titanate. The use of a high dielectric constant material as the material of the gate dielectric layer 151 in this embodiment can further improve the current driveability of the transistor.
[0084] See you again Figure 10 In one embodiment, the upper surface of the word line structure 15 is lower than the upper surface of the substrate 10; the method further includes forming a word line capping layer 16, the word line capping layer 16 covering the word line structure 15.
[0085] Next, as Figure 11 As shown, the method further includes: A dielectric layer 17 is formed on the substrate 10; A portion of the dielectric layer 17, a portion of the second source / drain doped region d2 located below the portion of the dielectric layer 17, and a portion of the word line capping layer 16 are removed to form a trench S; An initial first contact plug 18' is formed in the trench S, and the initial first contact plug 18' contacts the second source / drain doped region d2.
[0086] Next, as Figures 12 to 14 As shown, the method further includes: A bit line material layer 191' is formed on the substrate 10, and the bit line material layer 191' is in contact with the initial first contact plug 18'; an insulating material layer 192' is formed on the bit line material layer 191'; The insulating material layer 192' is etched to form a bit line capping layer 192, the bit line material layer 191' is etched to form a bit line 191, and the initial first contact plug 18' is etched to form a first contact plug 18. There is a gap between the first contact plug 18 and the substrate 10 and the dielectric layer 17. The bit line capping layer 192 and the bit line 191 both extend along the second direction and are arranged along the first direction.
[0087] A bit line sidewall layer 193 is formed, which covers the bit line cover layer 192, the bit line 191 and the sidewall of the first contact plug 18 and fills the gap; the bit line 191, the bit line cover layer 192 and the bit line sidewall layer 193 constitute multiple bit line structures 19 extending along the second direction and arranged along the first direction.
[0088] The first contact plug 18 is made of polysilicon. The bit line 191 includes a titanium nitride layer and a tungsten layer on the titanium nitride layer. The bit line capping layer 193 and the bit line sidewall layer 193 are made of silicon nitride.
[0089] Next, as Figures 15 to 17 , Figures 1b to 1c As shown, the method further includes: Multiple isolation fences 21 are formed, extending along a first direction and arranged along a second direction, and the multiple isolation fences 21 and the multiple bit line structures 19 form multiple openings 22; By removing a portion of the dielectric layer 17 in the opening 22 and a portion of the substrate 10 located below the portion of the dielectric layer 17, the first source / drain doped region d1 is exposed from the opening 22; A second contact plug 23 is formed within the opening 22, and the second contact plug 23 is connected to the first source / drain doped region d1.
[0090] See you again Figure 17 , Figures 1b to 1c The method further includes forming contact pads 24. Specifically, forming the first contact plug 23 and the contact pads 24 includes: A second contact plug material layer 23' is formed on the substrate 10, the second contact plug material layer 23' covering the opening 22, the bit line structure 19 and the isolation barrier 21; a contact pad material layer 24' is formed on the second contact plug material layer 23'; The second contact plug material layer 23' and the contact pad material layer 24' are etched to form a plurality of second contact plugs 23 and a plurality of contact pads 24. The second contact plugs 23 are at least partially located in the opening 22. The second contact plugs 23 also cover a portion of the top and a portion of the sidewall of the bit line structure 19. The contact pads 24 cover the upper surface of the second contact plugs 23.
[0091] In one embodiment, the second contact plug 23 is made of titanium nitride, which has better conductivity than polycrystalline silicon mentioned in related technologies, resulting in a lower contact resistance between the second contact plug 23 and the first source / drain doped region d1. However, this is not a limitation; the second contact plug 23 can also be made of other materials with good conductivity, such as tungsten, tungsten nitride, or titanium. The contact pad 24 is made of tungsten. The isolation barrier 21 is made of silicon nitride.
[0092] As can be seen, in this embodiment of the present disclosure, by providing the semiconductor layer 14 between the word line structure 15 and the substrate 10, and the material of the semiconductor layer 14 including an oxide semiconductor material, the oxide semiconductor material can serve as a channel for transmitting charge. The oxide semiconductor material has higher carrier mobility and lower leakage current, thus effectively alleviating or eliminating the GIDL leakage phenomenon, improving the transistor's on / off current ratio and current driveability, thereby improving the driving capability of the word line structure 15 for the transistor, reducing power consumption, and improving the performance of the semiconductor structure.
[0093] Figures 4 to 17 The semiconductor layer 14 shown only covers the bottom surface and at least part of the sidewalls of the recess 12. In another embodiment of this disclosure, the semiconductor layer 14 also covers part of the upper surface of the substrate 10, such as... Figures 18 to 25 As shown.
[0094] like Figures 19 to 20 As shown, specifically, a semiconductor layer 14 is formed, which at least partially covers the sidewalls of the recess 12, including: A semiconductor material layer 14' is formed, which covers the inner wall of the groove 12 and the upper surface of the substrate 10; The semiconductor material layer 14' is etched to form a plurality of discrete semiconductor layers 14. The projection of the semiconductor layer 14 on the plane of the substrate 10 at least partially overlaps with the projection of the active region AA on the plane of the substrate 10. Each semiconductor layer 14 includes a first sub-layer 141, a second sub-layer 142 and a third sub-layer 143. The first sub-layer 141 covers the bottom surface and sidewalls of the groove 12. The second sub-layer 142 and the third sub-layer 143 are located on both sides of the groove 12 and cover the upper surface of the active region AA.
[0095] In some embodiments, the first sublayer 141 at least covers the portion of the surface of the active region AA exposed by the groove 12, the second sublayer 142 at least covers a portion of the upper surface of the middle region of the active region AA, and the third sublayer 143 at least covers a portion of the upper surface of the two ends of the active region AA.
[0096] In one embodiment, the first sublayer 141 is p-type doped, and the second sublayer 142 and the third sublayer 143 are n-type doped; or, the first sublayer 141 is n-type doped, and the second sublayer 142 and the third sublayer 143 are p-type doped.
[0097] like Figure 18 As shown, in one embodiment, before forming the semiconductor layer 14, the method further includes forming an insulating layer 13, the insulating layer 13 covering the inner wall of the groove 12 and the upper surface of the substrate 10, thereby effectively reducing the channel leakage current and GIDL leakage current.
[0098] Next, as Figure 21 As shown, the word line structure 15 is formed in the groove 12, and the upper surface of the word line structure 15 is lower than the upper surface of the semiconductor layer 14; a word line capping layer 16 is formed, which covers the word line structure 15 and fills the gaps between the plurality of second sub-layers 142 and the plurality of third sub-layers 143.
[0099] Next, as Figures 22 to 24 As shown, after forming the word line structure 15, the method further includes: A dielectric layer 17 is formed; the dielectric layer 17 is etched to form a first contact hole V, the first contact hole V exposing the second sublayer 142; a first contact plug 18 is formed in the first contact hole V, the first contact plug 18 contacting the second sublayer 142. A plurality of bit line structures 19 are formed extending along a second direction, the bit line structures 19 being in electrical contact with the top of the first contact plug 18.
[0100] See you again Figures 23 to 24The bitline structure 19 is formed by: A bit line material layer 191' is formed on the substrate 10, and the bit line material layer 191' is in contact with the first contact plug 18; an insulating material layer 192' is formed on the bit line material layer 191'; The insulating material layer 192' is etched to form a plurality of bit line capping layers 192, and the bit line material layer 191' is etched to form a plurality of bit lines 191 extending along a second direction; the dielectric layer 17 between the plurality of bit lines 191 is removed; the plurality of bit lines 191 and the plurality of bit line capping layers 192 both extend along the second direction and are arranged along the first direction; A bit line sidewall layer 193 is formed, which covers the bit line cover layer 192, the bit line 191, and the sidewall of the first contact plug 18; the bit line 191, the bit line cover layer 192, and the bit line sidewall layer 193 constitute the bit line structure 19.
[0101] In one embodiment, the first contact plug 18 is made of titanium nitride. Titanium nitride has better conductivity than polycrystalline silicon mentioned in related technologies, resulting in lower contact resistance between the first contact plug 18 and the second sublayer 142. However, it is not limited to this; the first contact plug 18 can also be made of other materials with good conductivity, such as tungsten, tungsten nitride, titanium, etc. The bit line 191 is made of tungsten, copper, titanium, tantalum, titanium nitride, tantalum nitride, metal silicides, metal alloys, or any combination thereof.
[0102] Next, see Figure 25 and Figures 2b to 2c After forming the bit line structure 19, the method further includes: A plurality of isolation fences 22 are formed extending along a first direction, the plurality of isolation fences 22 and the plurality of bit line structures 19 forming a plurality of openings 24, and the third sub-layer 143 is exposed from the openings 22; A second contact plug 23 is formed within the opening 22, and the second contact plug 23 contacts the third sub-layer 143.
[0103] The method further includes forming contact pads 24, and the method for forming the contact pads 24 and the second contact plug 23 is the same as in the previous embodiments, and will not be repeated here.
[0104] In one embodiment, the second contact plug 23 is made of titanium nitride, which has better conductivity than polycrystalline silicon mentioned in related technologies, resulting in lower contact resistance between the second contact plug 23 and the third sublayer 143. However, this is not a limitation; the second contact plug 23 can also be made of other materials with good conductivity, such as tungsten, tungsten nitride, and titanium. The bit line 191 is made of tungsten, copper, titanium, tantalum, titanium nitride, tantalum nitride, metal silicides, metal alloys, or any combination thereof.
[0105] In this embodiment, the first contact plug 18 contacts the second sub-layer 142 of the semiconductor layer 14, and the second contact plug 23 contacts the third sub-layer 143 of the semiconductor layer 14. The semiconductor layer 14 is made of an oxide semiconductor material, which has higher carrier mobility and lower leakage current. Compared with the embodiment in which the first contact plug 18 and the second contact plug 23 are in direct contact with the active region AA, the leakage current and contact resistance are further reduced, and the performance of the semiconductor structure is improved.
[0106] It should be noted that those skilled in the art can change the order of the above steps without departing from the scope of protection of this disclosure. The above description is only an optional embodiment of this disclosure and is not intended to limit the scope of protection of this disclosure. Any modifications, equivalent substitutions and improvements made within the spirit and principles of this disclosure should be included within the scope of protection of this disclosure.
Claims
1. A semiconductor structure, characterized in that, include: Substrate; the substrate includes an isolation structure and a plurality of discrete active regions separated by the isolation structure; Multiple grooves are located within the substrate and extend along a first direction; the extension direction of the active region intersects the first direction, and two adjacent grooves separate the active region into two ends and a middle region, and the grooves expose the active region; Multiple character line structures, wherein the character line structures are located within the groove; A plurality of semiconductor layers, wherein the semiconductor layers are at least partially located between the word line structure and the inner wall of the groove, and the orthographic projection of the semiconductor layers on the substrate plane at least partially overlaps with the orthographic projection of the active region on the substrate plane; wherein the semiconductor layers comprise an oxide semiconductor material.
2. The semiconductor structure according to claim 1, characterized in that, The oxide semiconductor material includes In x Ga y Zn 1-x-y O, where x is greater than or equal to 0 or less than or equal to 1, and y is greater than or equal to 0 or less than or equal to 1.
3. The semiconductor structure according to claim 1, characterized in that, The semiconductor structure further includes an insulating layer, which is located at least between the substrate and the semiconductor layer.
4. The semiconductor structure according to claim 3, characterized in that, The insulating layer covers the bottom surface of the groove and part of the sidewalls, and the upper surface of the insulating layer on the sidewalls is lower than the upper surface of the substrate. The semiconductor layer covers the insulating layer and the area of the sidewalls of the groove not covered by the insulating layer, and is in contact with the exposed area.
5. The semiconductor structure according to claim 1, characterized in that, The semiconductor layer includes a first sublayer, a second sublayer, and a third sublayer. The first sublayer covers the bottom surface and sidewalls of the groove, and the second and third sublayers are located on both sides of the groove and cover a portion of the upper surface of the substrate.
6. The semiconductor structure according to claim 5, characterized in that, The semiconductor structure further includes: a plurality of bit line structures located on the substrate, the plurality of bit line structures extending along a second direction intersecting the first direction; and a first contact plug located below the bit line structures and above the second sub-layer, the first contact plug being electrically connected to the bit line structures and the second sub-layer.
7. The semiconductor structure according to claim 6, characterized in that, The bit line structure includes: a bit line, a bit line cover layer, and a bit line sidewall layer. The bit line cover layer covers the upper surface of the bit line, and the bit line sidewall layer covers the bit line cover layer, the bit line, and the sidewall of the first contact plug.
8. The semiconductor structure according to claim 5, characterized in that, Also includes: Multiple second contact plugs and multiple contact pads, wherein the second contact plugs are located below the contact pads and are in contact with the third sublayer.
9. A method for manufacturing a semiconductor structure, characterized in that, include: Provide substrate; A groove extending in a first direction is formed within the substrate; Forming a groove extending along a first direction within the substrate includes: etching the substrate to form an isolation trench, the isolation trench dividing the substrate into a plurality of discrete active regions; forming a filling layer within the isolation trench to form an isolation structure; etching the active regions and the isolation structure to form a plurality of grooves extending along the first direction, each active region being divided into an intermediate region and two ends by two adjacent grooves; A semiconductor layer is formed, the semiconductor layer at least partially covering the inner wall of the groove, and the orthographic projection of the semiconductor layer onto the substrate plane at least partially overlaps with the orthographic projection of the active region onto the substrate plane; wherein the material of the semiconductor layer includes an oxide semiconductor material; A word line structure is formed, the word line structure being located within the groove and at least partially covering the semiconductor layer.
10. The manufacturing method according to claim 9, characterized in that, Forming a semiconductor layer, the semiconductor layer at least partially covering the sidewalls of the groove, including: A semiconductor material layer is formed, the semiconductor material layer covering the inner wall of the groove and the upper surface of the substrate; Remove the semiconductor material layer covering the upper surface of the substrate; A semiconductor material layer is etched onto the inner wall of the groove to form a plurality of discrete semiconductor layers, each of which covers the sidewall and bottom surface of the groove.
11. The manufacturing method according to claim 10, characterized in that, Before forming the semiconductor layer, the method further includes: An insulating layer is formed, which covers the inner wall of the groove and the upper surface of the substrate; Remove the insulating layer located on the upper surface of the substrate; The insulating layer covering the sidewall of the groove is etched such that the upper surface of the insulating layer on the sidewall of the groove is lower than the upper surface of the substrate.
12. The manufacturing method according to claim 9, characterized in that, Forming a semiconductor layer, the semiconductor layer at least partially covering the sidewalls of the groove, including: A semiconductor material layer is formed, the semiconductor material layer covering the inner wall of the groove and the upper surface of the substrate; The semiconductor material layer is etched to form a plurality of discrete semiconductor layers, the projection of the semiconductor layer on the substrate plane at least partially overlapping the projection of the active region on the substrate plane, each semiconductor layer including a first sublayer, a second sublayer and a third sublayer, wherein the first sublayer covers the bottom surface and sidewalls of the groove, and the second sublayer and the third sublayer are located on both sides of the groove and cover a portion of the upper surface of the substrate.
13. The manufacturing method according to claim 12, characterized in that, Before forming the semiconductor layer, the method further includes: An insulating layer is formed, which covers the inner wall of the groove and the upper surface of the substrate.
14. The method according to claim 12, characterized in that, After forming the word line structure, the method further includes: Forming a dielectric layer; The dielectric layer is etched to form a first contact hole, which exposes the second sublayer. A first contact plug is formed in the first contact hole, and the first contact plug contacts the second sub-layer; Multiple bit line structures are formed extending along a second direction, and the bit line structures are in electrical contact with the top of the first contact plug.
15. The method according to claim 14, characterized in that, After forming the bit line structure, the method further includes: Multiple isolation fences are formed extending along a first direction, the multiple isolation fences and the multiple bit line structures forming multiple openings, and the third sublayer is exposed from the openings; A second contact plug is formed within the opening, and the second contact plug contacts the third sublayer.
Citation Information
Patent Citations
Semiconductor device and manufacturing method thereof
US20120187475A1