Joining method

By pressing the uncoated portion of the electrode assembly with a clamp and bending the end with a curved track, combined with laser welding, the problem of insufficient welding surface quality between the current collector and the electrode assembly was solved, achieving high quality and stability of the battery.

CN117355989BActive Publication Date: 2026-11-10PANASONIC INTELLECTUAL PROPERTY MANAGEMENT CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202280037023.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2021-05-27
Filing Date
2022-04-12
Publication Date
2026-11-10
Estimated Expiration
2042-04-12

AI Technical Summary

Technical Problem

In the existing technology, the method of forming the welding surface between the current collector and the electrode assembly has not been able to fully improve the quality of the battery, and there is room for improvement.

Method used

The uncoated portion of the electrode assembly is pressed by a clamp, and the end is moved and bent by a curved track. Combined with laser welding, a high-quality connection between the electrode assembly and the current collector is achieved.

Benefits of technology

This improved the welding quality of the electrode assembly and current collector, enhanced the overall performance of the battery, avoided the generation of cutting debris from uncoated areas, and ensured the high quality and stability of the battery.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117355989B_ABST
    Figure CN117355989B_ABST
Patent Text Reader

Abstract

The joining method of the wound electrode group (2) with the spacer and electrode plate being stacked and wound together and the current collector includes: pressing the clamp (32) against multiple ends of the electrode plates arranged in the radial direction of the electrode group (2), moving the clamp (32) along a curved track in such a way that the displacement in the direction close to the electrode group (2) gradually increases and the displacement in the radial direction gradually decreases, bending the multiple ends, and joining the bent multiple ends with the current collector.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This disclosure relates to a method for joining an electrode assembly to a current collector. Background Technology

[0002] Batteries containing wound electrode assemblies and electrolyte in a cylindrical outer casing are known in the past. Regarding such batteries, Patent Document 1 discloses a method in which slits are radially provided at both ends of the electrode assembly, in the uncoated portion, and the uncoated portion is bent outward in the radial direction of the electrode assembly to form a flat welding surface, which is then welded to a current collector.

[0003] Existing technical documents

[0004] Patent documents

[0005] Patent Document 1: Japanese Patent Application Publication No. 2007-227137 Summary of the Invention

[0006] The technical problem that the invention aims to solve

[0007] The inventors of this invention conducted repeated and in-depth research on the method of joining the current collector to the welded surface formed by the bent uncoated portion, and finally discovered that there was still room for improvement in the previous method in terms of further improving the quality of the battery.

[0008] This disclosure was made in view of the circumstances, and one of its purposes is to provide a technology for improving the quality of batteries.

[0009] Methods for solving technical problems

[0010] One aspect of this disclosure is a method for joining a wound electrode assembly and a current collector, wherein spacers and electrode plates are stacked and wound together. The joining method includes: pressing a clamp against multiple ends of electrode plates arranged radially in the electrode assembly; moving the clamp along a curved path with a gradually increasing displacement in the direction approaching the electrode assembly and a gradually decreasing displacement in the radial direction; bending the multiple ends; and joining the bent ends with the current collector.

[0011] Any combination of the above-mentioned constituent elements, or any scheme that transforms the present disclosure into methods, apparatus, systems, etc., is also valid as a scheme of the present disclosure.

[0012] Invention Effects

[0013] According to this disclosure, it is possible to improve battery quality. Attached Figure Description

[0014] Figure 1 This is a cross-sectional view of the battery.

[0015] Figure 2 (A) is a diagram showing the formation process of the electrode assembly. Figure 2 (B) is a diagram showing the processing steps of the electrode assembly.

[0016] Figure 3 (A) is a diagram showing the state of the ends of the bent electrode assembly. Figure 3 (B) is a diagram showing the state after the electrode assembly and current collector are joined. Detailed Implementation

[0017] The present disclosure will now be described with reference to the accompanying drawings based on preferred embodiments. These embodiments are not intended to limit the present disclosure but are illustrative, and all features or combinations thereof described in the embodiments do not necessarily represent the essential content of the present disclosure. For the same or equivalent constituent elements, components, and processes shown in the various drawings, the same reference numerals are used, and repeated descriptions are omitted where appropriate. Furthermore, the scales or shapes of the parts shown in the various drawings are set for ease of explanation and are not intended to be limiting unless specifically mentioned. Additionally, when terms such as "first" and "second" are used in this specification or claims, unless specifically mentioned, these terms do not indicate any order or importance, but are used to distinguish one configuration from other configurations. Furthermore, in the various drawings, parts of less important components are omitted when describing the embodiments.

[0018] Figure 1 This is a cross-sectional view of battery 1. Battery 1 is, for example, a rechargeable secondary battery such as a lithium-ion battery, a nickel-metal hydride battery, or a nickel-cadmium battery. As an example, battery 1 has a structure in which electrode assembly 2 and electrolyte (not shown) are housed together in an outer container 4. Electrode assembly 2, as an example, is cylindrical and has a spiral-wound structure consisting of a strip-shaped first electrode plate 6 and a strip-shaped second electrode plate 8 sandwiched between strip-shaped spacers 10. Figure 2 (A)). In this embodiment, the first electrode plate 6 is used as the positive electrode plate, and the second electrode plate 8 is used as the negative electrode plate.

[0019] The first electrode plate 6 and the second electrode plate 8 have a structure in which electrode active material layers are stacked on the current collector. In a typical lithium-ion secondary battery, the current collector, which is the positive electrode, is made of aluminum foil or the like, and the negative electrode is made of copper foil or the like. The electrode active material layer can be formed by coating the surface of the current collector with an electrode composite material using a known coating apparatus, followed by drying and rolling. The electrode composite material is obtained by mixing electrode active materials, binder materials, conductive materials, etc., in a dispersion medium and dispersing them uniformly. In the case of a typical lithium-ion secondary battery, the positive electrode active material is lithium cobalt oxide or lithium iron phosphate, etc., and the negative electrode is graphite or the like.

[0020] The first electrode plate 6 has a first uncoated portion 12 of uncoated electrode composite material at its end on one side of the width direction A (the direction intersecting the length direction of the strip). The first uncoated portion 12 is the exposed portion in the current collector of the first electrode plate 6 where no layer of electrode active material is laminated. Furthermore, the second electrode plate 8 has a second uncoated portion 14 of uncoated electrode composite material at its end on the other side of the width direction A, i.e., the side opposite to the side protruding from the first uncoated portion 12. The second uncoated portion 14 is the exposed portion in the current collector of the second electrode plate 8 where no layer of electrode active material is laminated.

[0021] As described above, the electrode assembly 2 has a structure in which the first electrode plate 6 and the second electrode plate 8 are wound around each other. Therefore, the ends of the first electrode plate 6 and the second electrode plate 8 in the width direction A are arranged in a plurality of portions in the radial direction B of the electrode assembly 2. Thus, the electrode assembly 2 has a plurality of first uncoated portions 12 arranged in the radial direction B and a plurality of second uncoated portions 14 arranged in the radial direction B. Each first uncoated portion 12 has a curved portion 16 at its front end that bends in a curved shape toward the winding center C of the electrode assembly 2. Each second uncoated portion 14 has a curved portion 18 at its front end that bends in a curved shape toward the winding center C. Alternatively, the electrode assembly 2 may have only either the curved portion 16 or the curved portion 18.

[0022] As an example, the spacer 10 is made of a microporous membrane composed of polypropylene resin or the like, and is located between the first electrode plate 6 and the second electrode plate 8.

[0023] A first current collector 20 is disposed on the protruding side of the first uncoated portion 12 in the electrode assembly 2. The first current collector 20 is made of, for example, aluminum. At least a portion of each bent portion 16 is in contact with the surface of the first current collector 20. That is, the bent portions 16 are formed, thereby increasing the contact area between each first uncoated portion 12 and the first current collector 20. Moreover, each bent portion 16 and the first current collector 20 are joined together by laser welding or the like. Thus, the current collectors of each wound layer in the first electrode plate 6 are electrically connected to the first current collector 20.

[0024] A second current collector 22 is disposed on the protruding side of the second uncoated portion 14 in the electrode assembly 2. The second current collector 22 is made of, for example, copper, nickel, nickel-plated copper, or nickel-plated iron. At least a portion of each bent portion 18 is in contact with the surface of the second current collector 22. That is, by forming the bent portion 18, the contact area between each second uncoated portion 14 and the second current collector 22 is increased. Moreover, each bent portion 18 is joined to the second current collector 22 by laser welding or the like. Thus, the current collectors of each wound layer in the second electrode plate 8 are electrically connected to the second current collector 22.

[0025] The electrode assembly 2, with the first current collector 20 and the second current collector 22 attached, is housed together with the electrolyte in a bottomed cylindrical outer container 4. The outer container 4 is made of, for example, copper, nickel, iron, or alloys thereof. The second current collector 22 is joined to the inner bottom surface of the outer container 4 by welding or the like. A metal sealing plate 26 is embedded in the opening of the outer container 4 via an insulating gasket 24. Thus, the electrode assembly 2 and the electrolyte are sealed inside the outer container 4. The first current collector 20 is joined to the sealing plate 26 by welding or the like.

[0026] Next, the formation of electrode group 2, the processing of the ends of electrode group 2, and the joining of electrode group 2 and current collector plate will be explained. Figure 2 (A) is a diagram showing the formation process of electrode assembly 2. Figure 2 In (A), the illustrations of the first uncoated portion 12 and the second uncoated portion 14 are omitted. Figure 2 (B) is a diagram showing the processing steps of electrode assembly 2. Figure 2 In (B), a cross-section is shown for a portion of the end of electrode group 2. Figure 3 (A) is a diagram showing the state in which the end of electrode assembly 2 is bent. Figure 3 (B) is a diagram showing the state after the electrode group 2 and the current collector plate are joined. Figure 3 In (B), the first collector board 20 is shown as an example.

[0027] First, such as Figure 2 As shown in (A), a strip-shaped first electrode plate 6, a second electrode plate 8, and a spacer 10 are prepared respectively. Then, the spacer 10, the first electrode plate 6, the spacer 10, and the second electrode plate 8 are stacked in this order. The resulting stack is wound in a spiral shape to form a wound electrode assembly 2.

[0028] Next, as Figure 2 As shown in (B), the electrode assembly 2 is placed on the processing apparatus 28. The processing apparatus 28 includes a stage 30, a pair of clamps 32, a cam mechanism 34, and a frame 36. The stage 30 has a mounting surface 30a for mounting the electrode assembly 2. As an example, the mounting surface 30a has a circular groove (not shown) for inserting the end of the electrode assembly 2 into the groove, thereby fixing the electrode assembly 2. Furthermore, the method of fixing the electrode assembly 2 is not particularly limited. The electrode assembly 2 is positioned such that it extends in the normal direction of the mounting surface 30a around the center C. Figure 2 The electrode assembly 2 shown in (B) is positioned such that the second uncoated portion 14 faces the mounting surface 30a and the first uncoated portion 12 faces the side opposite to the mounting surface 30a. The mounting stage 30 is capable of rotating the electrode assembly 2 around the winding center C.

[0029] A pair of clamps 32 are positioned opposite the mounting surface 30a while clamping the electrode assembly 2. Each clamp 32 has a pressing surface 32a opposite to the electrode assembly 2. The pressing surface 32a abuts against a plurality of uncoated portions facing the mounting surface 30a opposite to the electrode assembly 2. Figure 2 (B) The first uncoated portion 12). Each clamp 32 is supported by the frame 36 in a state where it can move forward and backward relative to the electrode group 2. In addition, a drive unit (not shown) is supported at the frame 36 to move each clamp 32 forward and backward relative to the electrode group 2.

[0030] The cam mechanism 34 is positioned further away from the electrode assembly 2 than the pressing surface 32a and is supported by the frame 36. The cam mechanism 34 has a plate 38, a pair of cam grooves 40, and a pair of cam followers 42. The plate 38 is fixed to the frame 36. The pair of cam grooves 40 are provided on the plate 38. Viewed from the direction extending from the winding center C (i.e., the width direction A), the pair of cam grooves 40 are arranged to clamp the winding center C. One end of each of the pair of cam followers 42 is connected to a respective clamp 32. The other end of one cam follower 42 is slidably inserted into one cam groove 40. The other end of the other cam follower 42 is slidably inserted into the other cam groove 40.

[0031] Each cam groove 40 extends at an angle toward the electrode group 2 from the outer side of the radial direction B toward the inner side. Furthermore, each cam groove 40 bends with an increasing displacement toward the inner side of the radial direction B toward the electrode group 2.

[0032] The cam mechanism 34 moves each clamp 32. That is, with each clamp 32 pressed against the plurality of first uncoated portions 12 arranged in the radial direction B of the electrode assembly 2, each clamp 32 moves in and out toward the electrode assembly 2 via the drive unit. Thus, the cam follower 42 slides along the cam groove 40, and each clamp 32 moves toward the winding center C while approaching the electrode assembly 2. Figure 3 As shown in (A), each clamp 32 moves along a curved track with a gradually increasing displacement (displacement per unit time) in the direction approaching the electrode group 2 and a gradually decreasing displacement in the radial direction B of the electrode group 2. As a result, the front ends of the plurality of first uncoated portions 12 bend inward in the radial direction B, forming a plurality of curved portions 16.

[0033] In the initial stage of displacement, each clamp 32 shifts a greater extent toward the winding center C than toward the direction approaching electrode group 2. Furthermore, during the displacement process, the displacement amount toward the direction approaching electrode group 2 gradually increases, while the displacement amount in the radial direction B of electrode group 2 gradually decreases. As a result, in the later stage of displacement, each clamp 32 shifts a greater extent toward the direction approaching electrode group 2 than toward the direction towards the winding center C. That is, the displacement state of each clamp 32 shifts from a state where the displacement amount in the radial direction B is greater than the displacement amount in the direction approaching electrode group 2, to a state where the displacement amount in the direction approaching electrode group 2 is greater than the displacement amount in the radial direction B.

[0034] In this way, by moving each clamp 32 along a curved track, in the initial stage of the movement of each clamp 32, a force that pours in towards the inner radial direction B can be preferentially applied to each of the first uncoated portions 12 compared to the force of pushing in. Then, in the later stage of the movement, each of the guided first uncoated portions 12 can be pressed more firmly to pour in towards the inner radial direction B. As a result, the direction of pouring can be made consistent, and the front end of each of the first uncoated portions 12 can be bent.

[0035] Furthermore, each clamp 32 bends multiple first uncoated portions 12 in a portion of the circumferential region of the electrode assembly 2. In this embodiment, as the first stage of the processing step, the pair of clamps 32 press each first uncoated portion 12 in a straight line passing through the winding center C when viewed from the direction extending from the winding center C. Next, as the second stage, the electrode assembly 2 rotates 90° around the winding center C, and the pair of clamps 32 again press each first uncoated portion 12 in a straight line passing through the winding center C. Thus, a bend 16 is formed in a cross shape on the electrode assembly 2.

[0036] After the cross-shaped bend 16 is formed, as shown Figure 3 As shown in (B), laser welding or the like is performed on the locations where the multiple first uncoated portions 12, i.e., the multiple bent portions 16, overlap with the first current collector 20 to form a joint 44. This joins the electrode assembly 2 and the first current collector 20. The electrode assembly 2, with the first current collector 20 joined to it, is positioned such that the second uncoated portions 14 face the side opposite to the mounting surface 30a and is fixed to the mounting stage 30. Furthermore, the second uncoated portions 14 are subjected to the aforementioned processing using a pair of clamps 32. As a result, a cross-shaped bent portion 18 is formed in the electrode assembly 2. Then, the multiple bent portions 18 and the second current collector 22 are joined by laser welding or the like.

[0037] The electrode assembly 2, which is joined with the first current collector 20 and the second current collector 22, is contained in the outer can 4 along with the electrolyte. Next, processes such as joining the second current collector 22 to the outer can 4, joining the first current collector 20 to the sealing plate 26, and inserting the sealing plate 26 into the opening of the outer can 4 are performed to obtain the battery 1.

[0038] As explained above, the method for joining the electrode assembly 2 and the current collector in this embodiment includes: pressing the clamp 32 against multiple ends (at least one of the first uncoated portion 12 and the second uncoated portion 14) of the electrode plates arranged in the radial direction of the electrode assembly 2; moving the clamp 32 along a curved track in such a way that the displacement amount in the direction approaching the electrode assembly 2 gradually increases and the displacement amount in the radial direction of the electrode assembly 2 gradually decreases; bending the multiple ends; and joining the bent multiple ends with the current collector (at least one of the first current collector 20 and the second current collector 22).

[0039] The inventors of this invention discovered that when bending multiple uncoated portions, if the clamp 32 is moved linearly to apply load to each uncoated portion, the bending position or direction of each uncoated portion is inconsistent, making it difficult to bend each uncoated portion uniformly in the same direction. If the bending methods of each uncoated portion are inconsistent, the welding quality of the electrode assembly 2 and the current collector may be reduced. In contrast, in this embodiment, the clamp 32 is moved along a curved track to apply load to each uncoated portion. As a result, a uniformly shaped bent portion bending in the same direction can be formed at the front end of each uncoated portion. Therefore, the welding quality of the electrode assembly 2 and the current collector can be improved, and the quality of the battery 1 can be enhanced.

[0040] Furthermore, as a method to easily bend the uncoated portions, it is conceivable to provide slits in the uncoated portions, as is the case in the prior art. However, in this case, cutting debris from the uncoated portions may be generated when forming the slits. If this cutting debris gets mixed into the electrode assembly 2, it may lead to a decrease in the quality of the battery 1, thus requiring a strategy to deal with the cutting debris. In this regard, the joining method according to this embodiment can form a uniformly shaped curved portion without providing slits in the uncoated portions. Therefore, it is possible to further improve the quality of the battery 1.

[0041] Furthermore, in the bonding method of this embodiment, the uncoated portion is bent in a region of the circumferential direction of the electrode assembly 2. This allows the circumferential deflection caused by the bending of the uncoated portion to be absorbed by the unbent region. Therefore, the welding quality between the electrode assembly 2 and the current collector can be improved, thereby enhancing the quality of the battery 1.

[0042] Furthermore, in the joining method of this embodiment, the clamp 32 is moved by the cam mechanism 34. This allows for high-precision movement of the clamp 32 with a simple structure. Consequently, the quality of the battery 1 can be further improved.

[0043] The embodiments of this disclosure have been described in detail above. The foregoing embodiments are merely specific examples of implementing this disclosure. The content of the embodiments does not limit the technical scope of this disclosure; various design changes, such as alterations, additions, and deletions of constituent elements, are possible without departing from the inventive concept defined in the claims. New embodiments with design changes combine the effects of both combined and modified embodiments. In the foregoing embodiments, the phrases "in this embodiment" and "in this embodiment" are used to emphasize the possibility of such design changes; design changes are permitted even without such phrases. Furthermore, any combination of constituent elements included in each embodiment is valid as a solution of this disclosure. The shading lines in the cross-sectional annotations of the drawings are not limited to the material of the objects shaded.

[0044] The implementation method can also be determined by the items described below.

[0045] [Item 1] A bonding method is a bonding method for a wound electrode assembly (2) in which spacers (10) and electrode plates (6, 8) are stacked and wound together with current collector plates (20, 22), comprising:

[0046] The clamp (32) is pressed against multiple ends (12, 14) of the electrode plates (6, 8) arranged radially in the electrode group (2). The clamp (32) is moved along a curved track and the multiple ends (12, 14) are bent in such a way that the displacement in the direction close to the electrode group (2) gradually increases and the displacement in the radial direction gradually decreases.

[0047] The multiple bent ends (12, 14) are joined with the current collector (20, 22).

[0048] [Item 2] The joining method as described in Item 1

[0049] In a portion of the circumferential region of the electrode assembly (2), multiple ends (12, 14) are bent.

[0050] [Item 3] The joining method as described in Item 1 or 2

[0051] The clamp (32) is moved by the cam mechanism (34).

[0052] Industrial availability

[0053] This disclosure can be used in the method of joining electrode groups and current collectors.

[0054] Explanation of reference numerals in the attached figures

[0055] 1 Battery, 2 Electrode group, 6 First electrode plate, 8 Second electrode plate, 10 Spacer, 12 First uncoated part, 14 Second uncoated part, 20 First current collector, 22 Second current collector, 32 Fixture, 34 Cam mechanism.

Claims

1. A bonding method, comprising bonding a wound electrode assembly (in which spacers and electrode plates are stacked and wound) to a current collector plate, comprising: The clamp is pressed against multiple ends of the electrode plates arranged radially in the electrode group, and the clamp is moved along a curved path to bend the multiple ends in a manner that gradually increases the displacement in the direction close to the electrode group and gradually decreases the displacement in the radial direction. The multiple bent ends are joined to the current collector.

2. The joining method according to claim 1, wherein, The plurality of ends are bent in a portion of the circumferential region of the electrode assembly.

3. The joining method according to claim 1 or 2, wherein, The clamp is moved by a cam mechanism.

Citation Information

Patent Citations

  • Sealed storage battery

    JP2007227137A

  • Secondary battery

    CN101771141A

  • Cell and its making method

    JP2003036834A