Acid filling method for AGM lead-acid batteries

By using clamping fixtures and repeated acid filling before filling AGM lead-acid batteries, the problem of inconsistent pressure between the edge and middle cells was solved, the consistency of plate acid immersion was improved, the risk of internal battery temperature and separator dendrite short circuit was reduced, and the battery's service life and performance uniformity were ensured.

CN117374425BActive Publication Date: 2026-11-17FENGFAN
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202311488047.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-11-09
Publication Date
2026-11-17
Estimated Expiration
2043-11-09

AI Technical Summary

Technical Problem

During the acid filling process of AGM lead-acid batteries, the pressure in the edge cells and the middle cells is inconsistent, resulting in uneven battery performance and lifespan after formation, especially the edge cells are prone to failure.

Method used

Before acid filling, use a clamping fixture to fix the battery end face. Repeat acid filling and vacuum treatment multiple times to ensure the pressure and space consistency of each cell. Use cold acid and appropriate immersion time. Finally, remove the clamping fixture.

Benefits of technology

This solves the problem of inconsistent pressure between the edge and middle cells, improves the consistency of acid immersion on the plates, reduces the risk of internal battery temperature and short circuit due to separator dendrites, and ensures the battery's lifespan and performance uniformity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117374425B_ABST
    Figure CN117374425B_ABST
Patent Text Reader

Abstract

This invention provides a method for filling AGM lead-acid batteries with acid, belonging to the field of lead-acid battery production technology. The method includes the following steps: S1, clamping treatment before acid filling; S2, repeatedly filling the semi-finished battery with acid until an excess of acid is added; S3, using an acid-absorbing device to extract the excess acid from the semi-finished battery and removing the clamping fixture. The clamping fixture includes several connecting rods and two clamping plates movably mounted on the connecting rods. Each clamping plate has a limiting component on its opposite side, which cooperates with the connecting rods to press the clamping plate against the end face of the semi-finished battery. This method for filling AGM lead-acid batteries adds a clamping fixture before acid filling, fixing the end face of the semi-finished battery and preventing it from bulging outwards during acid filling, thus avoiding pressure in the outer cells and resolving the inconsistency between the pressure in the outer and inner cells.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of lead-acid battery production technology, and more specifically, relates to an acid filling method for AGM lead-acid batteries. Background Technology

[0002] After the positive and negative electrode plates of a lead-acid battery are cured, the composition of the raw positive and negative electrode plates is the same, both containing divalent lead compounds (3BS, 4BS, PbO) and some elemental Pb. Directly assembling these raw electrode plates into a battery cannot generate an electromotive force; therefore, electrode plate formation or battery formation is required. The formation process transforms the cured lead paste into porous positive and negative electrode materials PbO2 and Pb, which possess electrochemical properties.

[0003] Currently, over 90% of batteries utilize battery formation technology. The acid filling and immersion processes during battery formation are crucial. The immersion time and the consistency of acid immersion for the positive and negative plates significantly affect the quality and consistency of the plates after formation. This is especially true for AGM valve-regulated batteries, where the acid filling process is quite complex due to the pressure applied to the electrode groups. First, after acid filling, a series of chemical reactions occur between the sulfuric acid and the plates, releasing heat that causes the battery temperature to rise, potentially exceeding 60°C during immersion. Second, during the curing process, the lead carbonate generated from the partial carbonization of the positive and negative plates reacts with sulfuric acid, releasing CO2.

[0004] Currently, AGM battery structural designs take electrode group pressure into account, thickening the casing in the pressure release direction and employing vacuum cold acid filling. However, due to the pressure difference between the two edge cells and the four central cells, the acid immersion effect of the edge cells differs during the acid immersion process. This leads to differences in the performance and water consumption of the two edge cell electrode groups during battery formation, resulting in the problem of edge cell failure during use after formation, thus ending the battery's lifespan. Summary of the Invention

[0005] The purpose of this invention is to provide an acid filling method for AGM lead-acid batteries, which aims to solve the problem of inconsistent pressure between the side cells and the middle cells.

[0006] To achieve the above objectives, the technical solution adopted by the present invention is: to provide an acid filling method for AGM lead-acid batteries, comprising the following steps:

[0007] S1. Clamping treatment before acid filling; install clamping fixture on the semi-finished battery, with the two working surfaces of the clamping fixture respectively attached to the two end faces of the semi-finished battery in the length direction;

[0008] S2. Repeatedly fill the semi-finished battery with acid until the acid content is excessive; vacuuming is carried out in conjunction with the acid filling process.

[0009] S3. Set up an acid suction device to extract excess acid from the semi-finished battery and remove the clamping fixture.

[0010] The clamping fixture includes several connecting rods arranged along the length of the semi-finished battery and two clamping plates movably mounted on the connecting rods. Each clamping plate has a limiting member on its back side, and the limiting member cooperates with the connecting rod to press the clamping plate against the end face of the semi-finished battery.

[0011] In another embodiment of this application, there are multiple connecting rods, which are arranged in pairs on both sides of the semi-finished battery; the connecting rods are threaded rods, and each end of the connecting rod is provided with at least one limiting member, which is a nut; the clamping plate is provided with multiple connecting holes, and the clamping plate slides with the connecting rods through the connecting holes.

[0012] In another embodiment of this application, the clamping plate includes a main board, an abutment plate, and a fine-tuning assembly; the main board is slidably disposed on the connecting rod; the abutment plate is located inside the main board and is arranged parallel to the main board; the fine-tuning assembly includes a plurality of adjusting rods connecting the abutment plate and the main board, the adjusting rods being perpendicular to the main board and movable along its length direction on the main board, and the adjusting rods causing the abutment plate to move closer to or away from the main board.

[0013] In another embodiment of this application, the adjusting rod is a threaded rod, and one end of the adjusting rod is fixedly connected to the abutment plate; the other end of the adjusting rod passes through the main board and is threadedly connected to the main board; the pitch of the adjusting rod is smaller than the pitch of the connecting rod.

[0014] In another embodiment of this application, an elastic element is provided between the abutment plate and the main plate, the elastic element including a first compression spring connected to the middle of the abutment plate.

[0015] In another embodiment of this application, the fine-tuning component further includes a wedge block, which is slidably disposed on the side of the main board near the abutment plate. The side of the wedge block near the abutment plate has an inclined surface, which is in contact with the abutment plate.

[0016] In another embodiment of this application, in step S2, the inner cavity of the semi-finished battery needs to be evacuated before acid filling, and cold acid at -10℃ to 5℃ is used during acid filling.

[0017] In another embodiment of this application, a pickling time of 10 to 20 minutes is provided between step S2 and step S3.

[0018] As another embodiment of this application, the following steps are also included:

[0019] S4. The semi-finished battery is installed with the formation connection clip in the water bath and then formed and charged.

[0020] In another embodiment of this application, a conveyor track is provided between each workstation where each step is located.

[0021] The beneficial effects of the acid filling method for AGM lead-acid batteries provided by this invention are as follows: Compared with the prior art, the acid filling method for AGM lead-acid batteries of this invention adds a clamping fixture before acid filling, which fixes the end face of the semi-finished battery and avoids the problem of it bulging outward during acid filling, affecting the pressure of the side cells, and solving the problem of inconsistent pressure between the side cells and the middle cells; In addition, the use of multiple injections of excess acid during the acid filling process accelerates the acid immersion process of the AGM electrode groups, reduces the internal temperature of the battery after acid immersion and the risk of short circuit due to dendrites in the separator caused by low electrolyte density. Attached Figure Description

[0022] To more clearly illustrate the technical solutions in the embodiments of the present invention, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0023] Figure 1 A flowchart of an acid filling method for AGM lead-acid batteries provided in an embodiment of the present invention;

[0024] Figure 2 This is a schematic diagram of the clamping fixture provided in the first embodiment of the present invention;

[0025] Figure 3 This is a schematic diagram showing the connection between the clamping fixture and the semi-finished battery provided in the first embodiment of the present invention;

[0026] Figure 4 This is a schematic diagram of the clamping fixture provided in the second embodiment of the present invention;

[0027] Figure 5 This is a schematic diagram of the clamping fixture provided in the third embodiment of the present invention;

[0028] Figure 6 This is a schematic diagram of the structure of a semi-finished battery in a comparative embodiment of the present invention.

[0029] In the diagram: 1. Conveying track; 2. Clamping fixture; 3. Acid filling device; 4. Acid suction equipment; 5. Battery formation water bath; 6. Semi-finished battery; 7. Electrode group; 8. Battery case; 9. Main board; 10. Connecting rod; 11. Limiting component; 12. Adjusting rod; 13. Abutment plate; 14. Elastic component; 15. Wedge block; 16. Fixing rod; 17. Fixing seat. Detailed Implementation

[0030] To make the technical problems to be solved, the technical solutions, and the beneficial effects of the present invention clearer, the present invention will be further described in detail below with reference to the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are merely illustrative of the present invention and are not intended to limit the present invention.

[0031] Please see Figures 1 to 5 The present invention will now describe the method for filling AGM lead-acid batteries with acid. The method for filling AGM lead-acid batteries with acid includes the following steps:

[0032] S1. Clamping treatment before acid filling; Install clamping fixture 2 on the semi-finished battery 6, with the two working surfaces of clamping fixture 2 respectively attached to the two end faces of the semi-finished battery 6 along its length.

[0033] S2. Repeatedly fill the semi-finished battery 6 with acid until the acid content is excessive; vacuuming is carried out in conjunction with the acid filling process.

[0034] S3. Set up acid suction equipment 4 to extract excess acid from the semi-finished battery 6 and remove clamping fixture 2;

[0035] The clamping fixture 2 includes several connecting rods 10 arranged along the length of the semi-finished battery 6 and two clamping plates movably disposed on the connecting rods 10. Each clamping plate is provided with a limiting member 11 on its back side. The limiting member 11 cooperates with the connecting rods 10 to press the clamping plate against the end face of the semi-finished battery 6.

[0036] For the acid filling process of the battery, firstly, a clamping fixture 2 is installed on the semi-finished battery 6. The working surface of the clamping fixture 2 is attached to the two end faces along the length of the semi-finished battery 6. The clamping fixture 2 is used to limit the side wall of the semi-finished battery 6 to prevent it from bulging outwards during acid filling, which would affect the volume and pressure of the cell. After clamping, acid is repeatedly filled into the semi-finished battery 6 through the acid filling device 3. The amount of acid filled is an excess of acid exceeding the design value. During the acid filling process, a vacuum device is required. The excess acid filling accelerates the acid immersion process of the AGM electrode group, reduces the internal temperature of the battery after acid immersion, and reduces the risk of short circuit due to dendrites in the separator caused by low electrolyte density. Finally, after acid immersion, the excess acid in the semi-finished battery 6 is sucked out by the acid suction device 4 to avoid the problem of acid overflow caused by excessive acid during battery formation. Finally, the clamping fixture 2 is removed.

[0037] The clamping fixture 2 includes several connecting rods 10. The connecting rods 10 are all arranged along the length direction of the semi-finished battery 6 and are evenly distributed on both sides of the semi-finished battery 6. Both ends of the connecting rods 10 are connected to clamping plates. The clamping plates move along the length direction of the connecting rods 10 and abut against the end face of the semi-finished battery 6 with the help of the limiting member 11.

[0038] The acid filling method for AGM lead-acid batteries provided by this invention, compared with the prior art, adds a clamping fixture 2 before acid filling. The clamping fixture 2 fixes the end face of the semi-finished battery 6, preventing it from bulging outward during acid filling and affecting the pressure of the side cells, thus solving the problem of inconsistent pressure between the side cells and the middle cells. In addition, the acid filling process uses multiple injections of excess acid, which accelerates the acid immersion process of the AGM electrode groups, reduces the internal temperature of the battery after acid immersion, and reduces the risk of short circuits caused by dendrites in the separator due to low electrolyte density.

[0039] The clamping fixture 2 ensures that the pressure of the battery side cells and the middle cells is consistent, ensures that the movement trajectory and speed of the acid during the acid filling process in each cell are consistent, ensures the consistency of the acid immersion process of the green plate, improves the consistency of the green plate after acid immersion, and thus ensures the consistency of the plate, the electrode group 7 and the cell after formation.

[0040] The AGM semi-finished battery 6 is clamped. It is required to design clamping fixtures 2 of different sizes and clamping pressures according to the different AGM battery dimensions, so as to achieve consistent pressure and space in each cell, thereby eliminating pressure differences in each cell, especially the two side cells, and ensuring consistent acid immersion in each cell and the plates in each cell after acid filling.

[0041] Specifically, AGM lead-acid batteries have an automated production line system for the acid filling process, with fixed workstations at each step, such as: pretreatment workstation, vacuum acid filling workstation, acid suction workstation, tooling removal workstation, and formation workstation. Conveyor tracks 1 are provided between adjacent workstations.

[0042] An acid injection device 3, such as a V12 liquid injection vacuum machine, is installed at the vacuum acid injection station.

[0043] An acid suction device 4, such as the Jialihang battery acid suction machine, is installed at the acid suction station.

[0044] In some possible embodiments, please refer to Figure 1 For the clamping fixture 2, the clamping fixture 2 includes a connecting rod 10 and two clamping plates. The two clamping plates are respectively attached to the two ends of the semi-finished battery 6 in the length direction and are fixed to the connecting rod 10 to limit the deformation of the wall surface of the end of the semi-finished battery 6.

[0045] In the first embodiment, such as Figure 2 and Figure 3 As shown, there are multiple connecting rods 10, which are arranged in pairs on both sides of the semi-finished battery 6. The connecting rods 10 are threaded rods, and each end of the connecting rod 10 is provided with at least one limiting member 11, which is a nut. The clamping plate is provided with multiple connecting holes, and the clamping plate slides with the connecting rods 10 through the connecting holes.

[0046] Specifically, multiple connecting rods 10 are spaced apart on one side of the semi-finished battery 6, and at least two connecting rods 10 are located at the upper and lower parts of the semi-finished battery 6 respectively; the connecting rod 10 is a threaded rod with threaded parts at both ends, and a nut is provided at both ends of the connecting rod 10, and the nut is threadedly engaged with the connecting rod 10.

[0047] The nut is located on the outside of the clamping plate, and the outer diameter of the nut is larger than the inner diameter of the connecting hole on the clamping plate. Under the action of the nut, the nut presses the clamping plate against the end face of the semi-finished battery 6. Optionally, nuts are provided on both sides of the clamping plate, and the nuts on both sides clamp and fix the clamping plate to ensure that the clamping plate will not shift after being fixed.

[0048] Optionally, the semi-finished battery 6 has two connecting rods 10 on each side, which are respectively connected to the upper and lower parts of the clamping plate. The four connecting rods 10 are respectively connected to the four corners of the clamping plate to fix the clamping plate.

[0049] In the second embodiment, as Figure 4 As shown, the clamping plate includes a main plate 9, an abutment plate 13, and a fine-tuning assembly; the main plate 9 is slidably mounted on the connecting rod 10; the abutment plate 13 is located inside the main plate 9 and is parallel to the main plate 9; the fine-tuning assembly includes several adjusting rods 12 that connect the abutment plate 13 and the main plate 9. The adjusting rods 12 are perpendicular to the main plate 9 and move along its length direction on the main plate 9. The adjusting rods 12 drive the abutment plate 13 to move closer to or away from the main plate 9.

[0050] The side of the motherboard 9 closest to the semi-finished battery 6 is the inner side. An adjustment rod 12 is connected to the inner side of the motherboard 9. The adjustment rod 12 is horizontally set and extends inward. An abutment plate 13 is connected to the end of the adjustment rod 12. The area of ​​the abutment plate 13 is smaller than the area of ​​the motherboard 9. The abutment plate 13 is located inside the motherboard 9.

[0051] The adjusting rod 12 is a threaded rod, and one end of the adjusting rod 12 is fixedly connected to the abutment plate 13; the other end of the adjusting rod 12 passes through the main plate 9 and is threadedly connected to the main plate 9; the pitch of the adjusting rod 12 is less than the pitch of the connecting rod 10.

[0052] When clamping the semi-finished battery 6, the adjusting rod 12 is threadedly connected to the main board 9, and the adjusting rod 12 is movably engaged with the abutment plate 13. When it is necessary to fine-tune the fit between the abutment plate 13 and the semi-finished battery 6, simply rotate the adjusting rod 12. The rotation of the adjusting rod 12 causes the abutment plate 13 to move along the length of the semi-finished battery 6, moving closer to or further away from the main board 9, thereby adjusting the fit between the abutment plate 13 and the end face of the semi-finished battery 6.

[0053] Furthermore, an elastic element 14 is provided between the abutment plate 13 and the main plate 9. The elastic element 14 includes a first compression spring connecting the middle part of the abutment plate 13. The elastic element 14 also includes a second compression spring sleeved on the outside of the adjusting rod 12, with its two ends abutting against the abutment plate 13 and the main plate 9, respectively. Under the action of the first spring and the second spring, the abutment plate 13, without being subjected to external force, is always located at the end of the adjusting rod 12 away from the main plate 9.

[0054] The second compression spring applies a force to the abutment plate 13 in the direction of the semi-finished battery 6. The force of the second compression spring on the abutment plate 13 corresponds to the force applied by the semi-finished battery 6 to the abutment plate 13.

[0055] In the third embodiment, as Figure 5 As shown, the fine-tuning component also includes a wedge block 15, which is slidably disposed on the side of the main board 9 near the abutment plate 13. The side of the wedge block 15 near the abutment plate 13 has an inclined surface, which is in contact with the abutment plate 13.

[0056] The abutment plate 13 is located inside the main board 9 with the help of the adjusting rod 12, and the abutment plate 13 and the adjusting rod 12 are in sliding engagement. Under the action of the main board 9, the abutment plate 13 is attached to the end face of the semi-finished battery 6, and the abutment strength between the abutment plate 13 and the end face of the semi-finished battery 6 needs to be adjusted with the help of the wedge block 15.

[0057] A fixing seat 17 is provided on any edge of the main board 9 near the abutment plate 13. A fixing rod 16 is connected to one end of the wedge block 15 that extends out of the abutment plate 13. The fixing rod 16 passes through the fixing seat 17 and is threadedly connected to the fixing seat 17. The thickness of the wedge block 15 gradually increases from one side of the abutment plate 13 toward the fixing seat 17.

[0058] The end of the fixing rod 16 is rotatably connected to the thicker end of the wedge block 15. Rotating the fixing rod 16 adjusts the length of the fixing rod 16 extending out of the fixing seat 17, which in turn adjusts the length of the wedge block 15 extending between the abutment plate 13 and the main plate 9. Due to the change in the thickness of the wedge block 15, the movement of the fixing rod 16 along its length direction can adjust the length between the abutment plate 13 and the main plate 9 through the wedge block 15.

[0059] In step S2, the inner cavity of the semi-finished battery 6 needs to be evacuated before acid filling, and cold acid at -10℃ to 5℃ is used during acid filling.

[0060] The clamped AGM semi-finished battery 6 is then filled with acid. The sulfuric acid temperature for filling the acid must be between -10℃ and 5℃. The larger the battery, the lower the sulfuric acid temperature. Generally, for batteries ≤70Ah, the sulfuric acid temperature is between -3℃ and 5℃, and for batteries >70Ah, it is between -10℃ and -4℃. The amount of acid to be filled is designed based on the battery size and the acid capacity of each cell after installation into the electrode group. Specifically, the amount of acid to be filled is first weighed quantitatively, then the battery is vacuum-sealed for acid filling. This process is repeated 2 to 4 times until all the sulfuric acid is filled. This repeated vacuum-sealing and acid filling accelerates the acid immersion speed and increases the acid density in the middle of the electrode plates, preventing dendrite short circuits caused by low acid density.

[0061] A pickling time of 10 to 20 minutes is allowed between steps S2 and S3. Please refer to [link / reference]. Figure 1 The battery, which is filled with acid through the vacuum acid filling device 3, is transported to the battery acid removal device 4 via a transport track. The transport time between the acid filling device 3 and the acid removal device 4 is between 10 minutes and 20 minutes depending on the size of the battery, so as to ensure that the plates are immersed in acid at the same time along the same trajectory.

[0062] The method for filling AGM lead-acid batteries with acid also includes the following steps:

[0063] S4. The semi-finished battery 6 is installed with a formation connection clip in a water bath and then formed and charged.

[0064] like Figure 1 and Figure 2 As shown, after 10-20 minutes of acid filling, the battery reaches the acid absorption device 4. After acid absorption is completed according to the different amounts of acid required for different batteries, the clamping fixture 2 is removed, and the battery is transported to the battery formation water bath 5 via a transport track. Compared with the existing equipment, the addition of the acid absorption device 4 increases the amount of cold acid poured in. After soaking in the acid for a certain period of time, the acid is removed, which can effectively reduce the internal temperature of the battery after acid filling. Furthermore, the acid density after soaking will not be too low, which could cause dendrite short circuits in the separators, and the consistency of the plate acid soaking is also ensured.

[0065] Example 1, as Figure 2As shown, the clamped AGM semi-finished battery 6, with electrode groups 7 inserted into the battery cell under certain pressure, is shown in the cross-sectional view as 7-1, 7-2, and 7-3 representing different individual cell electrode groups 7. 7-1 and 7-2 are the middle cell electrode groups 7, and 7-3 is the edge cell electrode group 7. Since 7-1 and 7-2 are both in the middle cells, they experience consistent pressure. However, 7-3, being an edge cell, experiences pressure release not only from the battery cell wall but also from the clamping action of the clamping fixture 2. Therefore, the pressure on both sides of 7-3 is consistent, and the battery cell wall does not deform under the action of the clamping fixture 2. This ensures that the pressure and space size of 7-3 are consistent with 7-1 and 7-2, guaranteeing consistent acid movement trajectory and speed during the acid filling process in each cell, ensuring consistency in the acid immersion process of the green plates, improving the consistency of the green plates after acid immersion, and ultimately ensuring the consistency of the plates, electrode groups 7, and individual cells after formation.

[0066] Comparative embodiments, such as Figure 6 As shown, the unclamped AGM semi-finished battery 6, because the electrode groups 7 are installed into the battery cell under certain pressure, 7-1, 7-2, and 7-3 in the cross-sectional view are electrode groups 7 of different individual cells, where 7-1 and 7-2 are the middle cell electrode groups 7, and 7-3 is the edge cell electrode group 7. Since 7-1 and 7-2 are both in the middle cells, they are under the same pressure; while 7-3 is in the edge cell, and the pressure release in the edge cell direction is only due to the constraint of the battery cell wall. Under the action of its internal pressure, the battery cell wall bulges in the direction of the arrow, which results in less pressure and more space in the edge cell electrode group 7-3. This ultimately causes differences in acid impregnation, formation, and performance of individual cells, leading to premature termination of life due to inconsistency among individual cells.

[0067] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, and improvements made within the spirit and principles of the present invention should be included within the protection scope of the present invention.

Claims

1. An acid filling method for AGM lead-acid batteries, characterized in that, Includes the following steps: S1. Clamping treatment before acid filling; Install clamping fixture (2) on the semi-finished battery (6), and attach the two working surfaces of clamping fixture (2) to the two end faces of the semi-finished battery (6) in the length direction respectively; S2. Repeatedly fill the semi-finished battery (6) with acid until the acid is excessive; vacuum treatment is carried out in conjunction with the acid filling process. S3. Set up an acid suction device (4) to extract excess acid from the semi-finished battery (6) and remove the clamping fixture (2); The clamping fixture (2) includes several connecting rods (10) arranged along the length direction of the semi-finished battery (6) and two clamping plates movably arranged on the connecting rods (10). Each clamping plate has a limiting member (11) on its back side. The limiting member (11) cooperates with the connecting rod (10) to press the clamping plate against the end face of the semi-finished battery (6).

2. The method for filling AGM lead-acid batteries as described in claim 1, characterized in that, There are multiple connecting rods (10), and the multiple connecting rods (10) are arranged in pairs on both sides of the semi-finished battery (6); the connecting rod (10) is a threaded rod, and each end of the connecting rod (10) is provided with at least one limiting member (11), and the limiting member (11) is a nut; the clamping plate is provided with multiple connecting holes, and the clamping plate slides with the connecting rod (10) through the connecting holes.

3. The method for filling AGM lead-acid batteries as described in claim 2, characterized in that, The clamping plate includes a main board (9), an abutment plate (13), and a fine-tuning assembly; the main board (9) is slidably disposed on the connecting rod (10); the abutment plate (13) is located inside the main board (9) and is arranged parallel to the main board (9); the fine-tuning assembly includes a plurality of adjusting rods (12) connecting the abutment plate (13) and the main board (9), the adjusting rods (12) are perpendicular to the main board (9) and are moved along its length direction on the main board (9), and the adjusting rods (12) drive the abutment plate (13) to move closer to or away from the main board (9).

4. The method for filling AGM lead-acid batteries as described in claim 3, characterized in that, The adjusting rod (12) is a threaded rod, and one end of the adjusting rod (12) is fixedly connected to the abutment plate (13); the other end of the adjusting rod (12) passes through the main plate (9) and is threadedly connected to the main plate (9); the pitch of the adjusting rod (12) is less than the pitch of the connecting rod (10).

5. The method for filling AGM lead-acid batteries as described in claim 4, characterized in that, An elastic element (14) is provided between the abutment plate (13) and the main plate (9), the elastic element (14) including a first compression spring connected to the middle of the abutment plate (13).

6. The method for filling AGM lead-acid batteries as described in claim 3, characterized in that, The fine-tuning component also includes a wedge block (15), which is slidably disposed on the side of the main board (9) near the abutment plate (13). The side of the wedge block (15) near the abutment plate (13) has an inclined surface, which is in contact with the abutment plate (13).

7. The method for filling AGM lead-acid batteries as described in claim 1, characterized in that, In step S2, the inner cavity of the semi-finished battery (6) needs to be evacuated before acid filling, and cold acid at -10℃ to 5℃ is used during acid filling.

8. The method for filling AGM lead-acid batteries as described in claim 1, characterized in that, Between steps S2 and S3, a soaking time of 10 to 20 minutes is allowed.

9. The method for filling AGM lead-acid batteries as described in claim 8, characterized in that, It also includes the following steps: S4. The semi-finished battery (6) is installed with a formation connection clip in a water bath and then formed and charged.

10. The method for filling AGM lead-acid batteries as described in claim 1, characterized in that, Each step is connected to a conveyor track (1).

Citation Information

Patent Citations

  • Flexible membrane battery unit and storage battery

    CN116314848A

  • Capacity-increasing bipolar storage battery stack

    WO2022257297A1