A plastic modified particle for hose and preparation method thereof

By combining polyvinyl chloride, polystyrene resin and acrylonitrile-styrene resin, and using flake fillers to optimize the filler components, the problem of liquid flow resistance caused by the high roughness of PVC plastic hoses is solved and a lower friction coefficient is achieved and better mechanical properties, reducing material transfer costs.

CN117924854BActive Publication Date: 2024-10-01浙江富华新材料科技有限公司
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410163935.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-02-05
Publication Date
2024-10-01
Estimated Expiration
2044-02-05

AI Technical Summary

Technical Problem

Due to its high roughness, PVC plastic hoses have greater resistance when liquid flows and increase energy consumption. There is an urgent need for a plastic material with high smoothness to reduce the cost of material transmission.

Method used

By combining polyvinyl chloride, polystyrene resin and acrylonitrile-styrene resin, and adding flake fillers such as talc powder and mica powder, the filler components are optimized to form a flatter surface, reduce the surface friction coefficient, and maintain the appropriate Extrusion preparation is carried out at melting temperature to form plastic modified particles with a lower friction coefficient.

Benefits of technology

It effectively reduces the resistance to liquid flow inside the hose, while maintaining good mechanical properties, such as wear resistance and impact resistance, and improving the flatness and processing performance of the plastic surface.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
  • Figure SMS_2
    Figure SMS_2
  • Figure SMS_3
    Figure SMS_3
Patent Text Reader

Abstract

The present application relates to the field of plastic polymer technology, and specifically to a plastic particle for a hose and a preparation method thereof, wherein the material comprises a plastic material mainly composed of PVC, polystyrene resin and acrylonitrile styrene resin, and fillers are added. By controlling the mass fraction of flaky materials in the fillers within a certain range, a plastic system with a smooth surface after melt extrusion can be obtained, which can effectively reduce the flow resistance of liquid in the hose.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of plastic polymer technology, and in particular to plastic particles for hoses and a preparation method thereof. Background Art

[0002] PVC plastic is a common component used to prepare plastic hoses. It is inexpensive, has good resistance to chemical corrosion, aging and wear, and has good flexibility and tensile and impact resistance. It is widely used in industrial production.

[0003] PVC plastic is soft in texture and therefore has strong resistance to deformation. It can maintain good sealing performance under external forces. However, PVC plastic currently has a common problem, that is, it has high roughness. Since hoses are used to transport liquid substances in most cases, the smoothness of their inner walls will have a great impact on the resistance to liquid flow, thereby increasing the energy and driving force required for mass transfer. In the case of large-scale material transmission, the smoother the inner wall of the plastic hose, the lower its energy consumption. Therefore, there is an urgent need for a plastic material with high smoothness under extrusion to reduce the cost of material transmission. Summary of the invention

[0004] The present application relates to a plastic modified particle for a hose and a preparation method thereof. Specifically, by adjusting the formula of the plastic particles, the processed hose can have a smoother inner wall structure, thereby reducing the resistance of the hose when transmitting liquid.

[0005] In the present application, a plastic modified particle for a hose is first provided, and the raw materials include the following components by mass:

[0006] PVC 100 copies;

[0007] 25-30 parts of polystyrene resin;

[0008] 5-8 parts of acrylonitrile-styrene resin;

[0009] 10-15 parts of plasticizer;

[0010] Lubricant 0.6~1 part

[0011] 20-30 parts of filler;

[0012] Colorant 0-1 part;

[0013] 1-2 parts of heat stabilizer;

[0014] Antioxidant 0-2 parts;

[0015] Wherein, the polymerization degree of the PVC is 900 to 1200;

[0016] The melt index of the acrylonitrile-styrene resin is not less than 2.5 g / 10 min;

[0017] The filler comprises flaky materials accounting for 50-60% of the filler mass, the average particle size of which is no greater than 50 μm, and the average particle size of the remaining part is no greater than 200 μm.

[0018] In the above scheme, a combination of polyvinyl chloride, polystyrene resin and acrylonitrile-styrene resin is firstly used. Among the above three resins, polyvinyl chloride is the main component, and the polymerization degree of polyvinyl chloride is controlled within the range of 900-1200. With the cooperation of plasticizer, it provides the most basic structure of the hose, with just the right hardness and good anti-bending performance. On the basis of the above, the polyester polyurethane tree provides good cohesion, so that the three-phase system can be mixed more evenly, while the acrylonitrile-styrene resin provides good surface strength. It can form a relatively flat system through the phenyl macromolecular group on the surface, which greatly reduces the surface friction coefficient at a higher processing temperature.

[0019] On the basis of the above, the components of the filler are optimized in the present application. First, among the fillers, flaky silicate materials are selected. Under the action of the polyurethane system, the flaky system is easier to form support on the surface than the needle-like structure and traditional spherical particles verified in the experiment, so that the plastic surface has a smoother structure. At the same time, controlling the overall average particle size of the system also helps to improve the surface flatness. Overall, the more small-sized flaky materials there are, the smaller the overall average particle size, and the system has a smoother surface, but the corresponding cost will also be higher. When the flaky material accounts for more than 50% of the mass fraction of the filler, it has a good effect.

[0020] Preferably, the sheet material is any number of talc, mica or wollastonite.

[0021] Any one of talcum powder, mica and wollastonite has good supporting performance, and due to its low hardness, it is not easy to have adverse effects on processing equipment, and the surface formed by it has high flatness.

[0022] Preferably, the oil absorption value of the sheet material is 25 to 50 g / 100 g.

[0023] Within the range of oil absorption values, the compatibility between the sheet material and the organic system is relatively high. On the one hand, it is not easy to produce agglomeration, making the system more uniform and less likely to produce cracks on the surface during bending. At the same time, too high an oil absorption value will cause the filler to have an excessively strong ability to adsorb the resin system, resulting in a decrease in the flow properties of the system under hot melt, which in turn leads to a rough surface.

[0024] Preferably, among the fillers, except for the sheet material, the Mohs hardness of the remaining fillers is 5-7.

[0025] In the system, in addition to the filler including some flaky materials, the remaining components can be selected from a filler system with a slightly higher hardness, such as silica. In this state, there is less wear on the processing equipment, and the surface can maintain good wear and impact resistance, which significantly improves the overall mechanical strength of the system.

[0026] Preferably, except for the flake material, the rest of the filler is made of silicon dioxide particles or magnesium oxide powder.

[0027] In this system, the relatively low content of silicon dioxide particles and magnesium oxide powder has a better effect of improving mechanical properties, and the prepared plastic system has moderate hardness and good bending and wear resistance.

[0028] Preferably, it also includes 1 to 4 parts by weight of polyethylene wax.

[0029] Polyethylene wax can improve the processing performance on the basis of the above fillers and reduce the wear effect of the overly hard components in the fillers on the system.

[0030] Preferably, the raw material further comprises 1.5 to 2 parts by weight of rosin-modified phenolic resin.

[0031] In the above scheme, the addition of rosin-modified phenolic resin can improve the cohesion of the system without significantly increasing the difficulty of system processing, and enhance the coating performance of the resin on the filler. In the case of good coating, the filler can be further prevented from being located on the plastic surface and thus increasing the friction coefficient. The viscosity of the rosin-modified phenolic resin is preferably 3000-3600 mpa*s.

[0032] Preferably, the melt index of the polystyrene resin is 4 to 5 g / 10 min.

[0033] The polystyrene resin within this range has slightly poor fluidity, but its leveling performance is better. Within the above melt index range, better flatness can be achieved by processing the plastic system at a higher temperature.

[0034] In addition, on the basis of the above, the present application also relates to a method for preparing the above-mentioned plastic modified particles for the hose. Under this method, the plastic modified particles are prepared by melt extrusion, and the melting temperature is 170 to 180°C. Extruding the plastic within this range can, on the one hand, reduce the friction coefficient and achieve a smooth surface, and on the other hand, reduce the damage to the polymer system caused by excessively high temperatures.

[0035] In summary, in the present application, a modified particle of a plastic structure having a lower surface friction coefficient is provided. After the particle is used to prepare a plastic hose, it can effectively reduce the resistance to the flow of liquid inside it, and also has good mechanical properties. DETAILED DESCRIPTION

[0036] The solution of the present application is further described through the following specific implementation methods.

[0037] In this application, the parameter selection categories of PVC are as follows:

[0038] PVC-1 label average degree of polymerization 900;

[0039] PVC-2 average degree of polymerization 760;

[0040] PVC-3 label average degree of polymerization 1050;

[0041] PVC-4 label average degree of polymerization 1180;

[0042] PVC-5 label average degree of polymerization 1475.

[0043] The grades of polystyrene resin are selected as follows:

[0044] PS-1: High impact resistance, melt index 4.7 g / 10min;

[0045] PS-2: High impact resistance, melt index 4.0 g / 10min;

[0046] PS-3: High impact resistance, melt index 5.2 g / 10min;

[0047] PS-4: Ordinary type. Melt index 7.4 g / 10min;

[0048] PS-5: Ordinary type, melt index 5.0 g / 10min;

[0049] PS-6: Ordinary type, melt index 3.8 g / 10min

[0050] PS-7: Ordinary type, melt index 14.0 g / 10min.

[0051] The grades of acrylonitrile-styrene resin are as follows:

[0052] AS-1: Melt index 2.5g / 10min;

[0053] AS-2: Melt index 2.8g / 10min;

[0054] AS-3: Melt index 3.8g / 10min;

[0055] AS-4: Melt index 2.2g / 10min.

[0056] The grades of rosin modified phenolic resin are selected as follows:

[0057] SX-1: bisphenol A type, softening temperature 173℃, viscosity 3340mpa*s;

[0058] SX-2: bisphenol A type, softening temperature 178°C, viscosity 3583mpa*s;

[0059] SX-3: bisphenol A type, softening temperature 173°C, viscosity 3004mpa*s;

[0060] SX-4: bisphenol A type, softening temperature 169°C, viscosity 2754mpa*s;

[0061] SX-5: tert-octylphenol type, softening temperature 104°C, viscosity 3441mpa*s;

[0062] SX-6: tert-octylphenol type, softening temperature 109℃, viscosity 4037mpa*s.

[0063] The grades of some materials in the filler are as follows:

[0064] Talc A, 18 μm, oil absorption value 38 g / 100 g;

[0065] Talc B, 45 μm, oil absorption value 16 g / 100 g;

[0066] Talc C, 70 μm, oil absorption value 5.4 g / 100 g;

[0067] Mica powder A, 50μm, oil absorption value 25g / 100g;

[0068] Mica powder B, 3μm, oil absorption value 50g / 100g;

[0069] Heavy calcium carbonate A: particle size 18μm, oil absorption value 22g / 100g;

[0070] Heavy calcium carbonate B: particle size 48μm, oil absorption value 20g / 100g;

[0071] Wollastonite: particle size 18μm, oil absorption value 26g / 100g;

[0072] Magnesium oxide A: average particle size 160 μm;

[0073] Magnesium oxide B: average particle size 250 μm;

[0074] Silica particles A: average particle size 200 μm;

[0075] Silica particles B: average particle size 125 μm;

[0076] Silica particles C: average particle size 40 μm;

[0077] Alumina powder: average particle size 160 μm;

[0078] Glass fiber A: average length is about 200 μm;

[0079] Glass fiber B: average length is about 500 μm;

[0080] Kaolin: particle size distribution is mainly between 0.5 and 5 μm, oil absorption value is 59 g / 100 g;

[0081] Cotton fiber: average length is about 140μm.

[0082] Among them, the Mohs hardness of talc is approximately 1, the Mohs hardness of mica powder is 2-3, the hardness of heavy calcium carbonate is about 3, the Mohs hardness of wollastonite is about 4.5, the Mohs hardness of magnesium oxide is approximately 5-6, the Mohs hardness of silica particles is 7, the Mohs hardness of alumina powder is about 9, the Mohs hardness of glass fiber is about 6.5, the Mohs hardness of kaolin is about 2.5, and cotton fiber is too soft, so its Mohs hardness is less than 1.

[0083] In the following examples, the prepared plastic modified particles are first prepared into corresponding samples by melt extrusion, and then the samples are subjected to wear resistance test, heat aging impact resistance test and surface flatness test, wherein the wear resistance test is measured by a wear tester, with the amount of wear as the measurement standard. Under the same conditions, the lower the amount of wear, the better the wear resistance. The aging impact resistance test measures the impact resistance of the plastic after aging it at 80°C for 120 hours. The above two measurement experiments are to verify the mechanical properties of the prepared hose, so as to reduce the phenomenon of the hose bursting under a large liquid pressure after the surface is damaged due to wear and impact during use. The surface flatness experiment refers to the roughness obtained by the "GB / T10610-2009 Product Geometry Technical Specification (GPS) Surface Structure Profile Method for Surface Structure Assessment" for determination.

[0084] Among them, a combination of PVC-1, PS-1, and AS-1 is selected, and different filler components are tested to obtain Example 1. The specific material components in Example 1 are selected as follows:

[0085] PVC 100 pieces

[0086] 25 parts of polystyrene resin

[0087] 5 parts of acrylonitrile-styrene resin

[0088] 15 parts of plasticizer;

[0089] 0.8 parts of lubricant;

[0090] 25 parts of filler;

[0091] 1 part colorant

[0092] 1 part of heat stabilizer;

[0093] 1 part antioxidant;

[0094] Specifically, the lubricant is paraffin, and calcium stearate, oxidized polyethylene wax and other components can also be used as lubricants. It mainly plays a role in lubricating processing equipment such as screws to reduce adhesion. It can be optionally adjusted and added between 0.6 and 1 parts according to the ratio of materials. The heat stabilizer is a calcium zinc stabilizer, and the antioxidant is antioxidant 264. When the addition amount does not exceed 2 parts, the two have no obvious effect on the mechanical properties of the system, and can be added according to the actual weather resistance required. The plasticizer is DEHP, and other plasticizers with alternative properties can also be used. The increase or decrease of the amount of plasticizer has a certain effect on the softness and hardness of the prepared hose. At the same time, the increase in the amount of addition will also affect the processing flowability of the plastic. It can adjust its amount according to the actual hardness of the hose required. It is reasonable to add it within the range of 10 to 15 parts by mass. In this embodiment, taking the addition of 15 parts of plasticizer as an example, a hose with a certain hardness is prepared. The colorant can be selected from various masterbatches, or it can be added without addition. Its small amount of addition has no obvious effect on the overall. After the above raw materials are mixed, they are extruded at 170-180° C. using a device (such as a single-screw extruder or a twin-screw extruder) to obtain a hose material.

[0095] In this example, the different filler components used are shown in Table 1.

[0096]

[0097] The experimental results of Example 1 are shown in Table 2.

[0098]

[0099] Through the above experimental results, it is not difficult to find that in this embodiment, compared with the granular filler system such as heavy calcium carbonate, wollastonite, kaolin, etc., the use of flaky, low-hardness inorganic fillers, such as talcum powder and mica powder, and medium-high hardness inorganic fillers with larger particles, such as silica particles and magnesium oxide, can better take into account the mechanical strength, processing performance and surface smoothness of the material, and there is no excessive wear on the equipment. In this system, on the one hand, the small particle system should be flaky, which can form a relatively flat structure on the outside of the plastic system. On the other hand, the large particle system is easier to fill in the inside of the plastic system to produce better support performance, so that the impact resistance and flatness are both high without obvious changes in hardness. And for the ratio of the two, the mass of the flaky material should account for 50-60% of the mass of the filler.

[0100] In addition, on the basis of the above, the mass proportion of filler can be adjusted relatively freely within 20 to 30 parts. On the whole, increasing the amount of filler will increase the hardness and enhance the wear resistance and impact resistance, but it will also cause a slight decrease in surface flatness and a decrease in the processing performance of the system. On the whole, within the range of 20 to 30 parts, the above properties do not change significantly, and simple experiments can be carried out according to the specific formula to determine the best ratio.

[0101] On the basis of the above, on the basis of Example 1-1, different PVC, polystyrene resin and acrylonitrile-styrene resin are used, and their dosages are adjusted to obtain Example 2, as shown in Table 3.

[0102]

[0103] The examples in Table 3 were tested and the results are shown in Table 4.

[0104]

[0105] From the above table, it is not difficult to find that on the basis of the PVC-PS-AS blend system, the PVC with a polymerization degree of 900-1200 is selected. It has better compatibility, coating and heat shock resistance overall, and has a strong capacity for filling. Compared with PVC with a lower polymerization degree, its performance in all aspects is better, but the high polymerization degree of PVC will lead to its processing difficulties and the problem of reduced surface smoothness. At the same time, the too long molecular chain will also increase the difficulty of processing. AS should not use too low melt index. AS with a high melt index helps to improve the overall smoothness. The improvement of its flatness is positively correlated with the increase of melt index. However, when the melt index reaches 2.5g / 10min, the overall surface smoothness reaches an acceptable level. Continuing to increase the melt index of the AS used can improve the smoothness slightly (but the amplitude is small), which will also affect the processing performance. On the basis of the above, the selection of a PS system with a melt index in the range of 4-5g / 10min is also helpful to improve the smoothness, but the effect of PS on the smoothness is small, and its increased dosage will affect the mechanical properties of the system. It is not feasible to completely not use PS, because AS itself will cause a significant increase in hardness when added to the PVC system in large quantities, and not adding AS will result in poor compatibility between PVC and PS phases. Therefore, both Example 20 and Example 21 are not advisable.

[0106] It should be noted that, due to the limitation of length and amount of data, the embodiments involved in Table 3 are not all experimental embodiments, but only representative ones. On the whole, the trend of material selection has a relatively obvious regularity. For example, with the increase of the mass of PS and AS, the rigidity of the system will gradually increase and tend to be stable, but the wear resistance, tensile resistance and impact resistance will show a trend of first increasing and then decreasing.

[0107] Furthermore, on the basis of Example 1-1, different rosin-modified resins and different amounts of polyethylene wax were added to obtain examples as shown in Table 5.

[0108]

[0109] Experiments were conducted on each experimental group in Example 3, and the results are shown in Table 6.

[0110]

[0111] In the above experimental scheme, through data comparison, it can be seen that in this application, adding rosin-modified phenolic resin can improve the smoothness and wear resistance of the system, but its addition will also lead to a decrease in fluidity, and the general addition amount is preferably in the range of 1.5 to 2 parts by mass. Adding polyethylene wax can further improve the processing performance and make the processing process easier. When the polyethylene wax is added in an amount of no more than four parts, there is no obvious effect on the mechanical properties of the system.

[0112] This specific embodiment is merely an explanation of the present application and is not a limitation of the present application. After reading this specification, those skilled in the art may make modifications to the present embodiment without any creative contribution as needed, but such modifications are protected by the patent law as long as they are within the scope of the claims of the present application.

Claims

1. A plastic modified particle for a hose, characterized in that: The raw materials include the following components by mass: PVC 100 copies; 25-30 parts of polystyrene resin; 5-8 parts of acrylonitrile-styrene resin; 10-15 parts of plasticizer; Lubricant 0.6~1 part 20-30 parts of filler; Colorant 0-1 part; 1-2 parts of heat stabilizer; Antioxidant 0-2 parts; Wherein, the polymerization degree of the PVC is 900 to 1200; The melt index of the acrylonitrile-styrene resin is not less than 2.5 g / 10 min; The filler comprises a sheet material accounting for 50-60% of the filler mass, the average particle size of which is not greater than 50 μm, and the average particle size of the remaining part is not greater than 200 μm; The oil absorption value of the sheet material is 25 to 50 g / 100 g.

2. The plastic modified particles for hose according to claim 1, characterized in that: The sheet material can be any number of talc, mica or wollastonite.

3. The plastic modified particles for hose according to claim 1, characterized in that: Among the fillers, except for the sheet material, the Mohs hardness of the remaining fillers is 5-7.

4. The plastic modified particles for hose according to claim 3, characterized in that: Among the fillers, except for the flake material, the rest of the fillers are selected from silicon dioxide particles or magnesium oxide powder.

5. The plastic modified particles for hose according to claim 3, characterized in that: The filler also includes 1 to 4 parts by weight of polyethylene wax.

6. The plastic modified particles for hose according to claim 1, characterized in that: The raw materials also include rosin-modified phenolic resin in an amount of 1.5 to 2 parts by weight.

7. The plastic modified particles for hose according to claim 6, characterized in that: The viscosity of the rosin-modified phenolic resin is 3000-3600 mpa*s.

8. The plastic modified particles for hose according to claim 1, characterized in that: The melt index of the polystyrene resin is 4 to 5 g / 10 min.

9. The method for preparing modified plastic particles for hoses according to any one of claims 1 to 8, characterized in that: It is prepared by extrusion, and the extrusion temperature is 170-180°C.